Glass base unit, cover glass assembly, and in-vehicle display device

A glass substrate with a thin and thick plate portion and a deforming device addresses impact resistance issues by ensuring higher protection in critical areas, maintaining visibility and functionality.

JP7571728B2Active Publication Date: 2024-10-23AGC INC
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
JP2021543700
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-09-03
Filing Date
2020-08-21
Publication Date
2024-10-23
Estimated Expiration
2040-08-21

AI Technical Summary

Technical Problem

Existing glass substrates for vehicle displays do not adequately ensure impact resistance, particularly in areas that require higher protection, such as the passenger side, due to uniform thickness that does not account for varying impact risk zones.

Method used

A glass substrate design with a thin plate portion and a thick plate portion, where the thin plate portion can be elastically deformed into a concave shape, ensuring higher impact resistance where needed, and a glass deforming device to switch between flat and concave shapes.

Benefits of technology

The design provides sufficient impact resistance in critical areas by localizing thicker glass where needed, enhancing protection without compromising visibility or functionality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007571728000001
    Figure 0007571728000001
  • Figure 0007571728000002
    Figure 0007571728000002
  • Figure 0007571728000003
    Figure 0007571728000003
Patent Text Reader

Abstract

A glass substrate unit according to the present invention has: a glass substrate provided with a thin plate section and a thick plate section; and a glass deformation apparatus for deforming the glass substrate. The thin plate section has a first main surface and a second main surface facing the first main surface. The thick plate section has a plate thickness greater than the plate thickness of the thin plate section, and has a first main surface and a second main surface facing the first main surface. The glass deformation apparatus deforms the glass substrate by moving one among the thin plate section and the thick plate section.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a glass base unit, a cover glass assembly, and an in-vehicle display device. [Background technology]

[0002] It is already known that the surface of a display device, including an in-vehicle display, is protected by a glass substrate (see, for example, Patent Document 1). On the other hand, it is also known that the display is movable (deformable) and the surface is covered with a glass substrate. For example, Patent Documents 2 to 4 disclose a configuration in which a plate-shaped glass substrate is attached to the movable portion (bent portion) and the non-movable portion of the surface of a bendable display. In such a configuration, the glass substrate can be moved (deformed) together with the display. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2018 / 129065 [Patent Document 2] Japanese Patent Publication No. 2017-120415 [Patent Document 3] Japanese Patent No. 6198194 [Patent Document 4] International Publication No. 2015 / 178391 Summary of the Invention [Problem to be solved by the invention]

[0004] In a glass base protecting a display or the like, when the glass base moves together with the display, a situation may be conceivable in which it is necessary to provide a portion within the glass base that has higher impact resistance than other portions. In particular, when an in-vehicle display is protected with a glass base as in Patent Document 1, for example, a higher impact resistance (head impact resistance) is required for the portion of the glass base that faces the vehicle occupant (specifically, the passenger in the passenger seat). In contrast, in the above-mentioned Patent Documents 2 to 4, the thickness of the glass substrate protecting the display is uniform, making it difficult to meet the above demands; particularly in the case of protective glass for in-vehicle displays, sufficient impact resistance is not ensured in areas that require impact resistance (head impact resistance).

[0005] Therefore, an object of the present invention is to provide a glass base unit, a cover glass assembly, and an in-vehicle display device in which impact resistance is ensured at a predetermined portion of the glass base in a structure in which the glass base is movable. [Means for solving the problem]

[0006] As a result of intensive research, the present inventors have found that the above object can be achieved by adopting the following configuration. That is, the present invention relates to the following [1] to

[16] . [1] A glass base unit comprising: a glass base; and a glass deformation device that deforms the glass base, wherein the glass base comprises a thin plate portion having a first main surface and a second main surface opposite the first main surface, and a thick plate portion having a thickness greater than the thickness of the thin plate portion and having the first main surface and the second main surface opposite the first main surface, and the glass deformation device deforms the glass base by moving one of the thin plate portion and the thick plate portion. [2] The glass base unit according to the above [1], wherein the shape of the glass base can be freely switched between a first shape in which the thin plate portion extends in a flat plate shape and a second shape in which the thin plate portion is elastically deformed. [3] The glass base unit according to [2], wherein the second shape is a shape in which the thin plate portion is elastically deformed into a concave shape. [4] The glass base unit according to any one of the above [1] to [3], wherein a display panel is attached to a first main surface of the thin plate portion, and the glass deformation device moves the thin plate portion together with the display panel. [5] The glass base unit according to any one of the above [1] to [4], wherein the glass base further comprises a connection portion having a first connection surface connecting the first main surface of the thin portion and the first main surface of the thick portion, and a second connection surface connecting the second main surface of the thin portion and the second main surface of the thick portion, wherein a starting point of deformation of the glass base is at the connection surface or on the thin portion side of the connection surface, and wherein the first connection surface is an arc-shaped curved surface and has a radius of curvature of 400 μm or more. [6] The glass base unit according to any one of the above [1] to [4], wherein the glass base further comprises a connection portion having a first connection surface connecting the first main surface of the thin portion and the first main surface of the thick portion and a second connection surface connecting the second main surface of the thin portion and the second main surface of the thick portion, wherein a starting point of deformation of the glass base is at the connection portion or on the thin portion side of the connection portion, and the thickness of the thinnest point of the connection portion is smaller than the thickness of the thin portion. [7] The glass base unit according to the above [6], wherein the thinnest part of the connection portion has a plate thickness of 0.5 mm or less. [8] The glass base unit according to any one of the above [5] to [7], wherein the connecting portion has an overhanging portion. [9] The glass base unit according to any of the above [1] to [4], wherein the glass base further comprises a connection portion having a first connection surface connecting a first main surface of the thin portion and a first main surface of the thick portion, and a second connection surface connecting a second main surface of the thin portion and a second main surface of the thick portion, wherein a starting point of deformation of the glass base is at the connection portion or on the thin portion side of the connection portion, wherein the first connection surface has a first adjacent surface adjacent to the first main surface of the thin portion and a second adjacent surface adjacent to the first main surface of the thick portion, wherein the first adjacent surface and the second adjacent surface are both arc-shaped curved surfaces and are connected to each other to form a first connection surface bent in an S shape.

[10] The glass base unit according to any one of the above [1] to [9], wherein the thickness of the thin portion is 0.05 mm or more and 0.8 mm or less, and the thickness of the thick portion is 0.5 mm or more and 2.5 mm or less.

[11] The glass base unit according to any one of the above [1] to

[10] , wherein the glass base is a chemically strengthened glass.

[12] The glass base unit according to any one of the above [1] to

[11] , wherein the glass deformation device is constituted by an actuator that applies an external force to one of the thin plate portion and the thick plate portion in the glass base.

[13] The glass base unit according to the above

[12] , further comprising a controller for controlling the operating state of the actuator.

[14] A cover glass assembly comprising the glass base unit according to any one of the above [1] to

[13] , wherein the glass base functions as a cover glass for a display panel.

[15] An in-vehicle display device having an instrument cluster arranged in front of the driver's seat, a center information display arranged in front between the driver's seat and the passenger seat, and a glass base unit according to any one of [1] to

[13] above, wherein the instrument cluster is attached to a first main surface of the thin plate portion and the center information display is attached to a first main surface of the thick plate portion, and while a vehicle equipped with the in-vehicle display device is running, a glass deformation device elastically deforms the thin plate portion into a concave shape to move it together with the instrument cluster, thereby deforming the glass base.

[16] An in-vehicle display device having an instrument cluster arranged in front of the driver's seat, a center information display arranged in front of the driver's seat and a passenger seat, and a glass base unit according to any one of [1] to

[13] above, wherein the instrument cluster is attached to a first main surface of the thin plate portion, and the center information display is attached to a first main surface of the thick plate portion, and while a vehicle equipped with the in-vehicle display device is traveling, a glass deformation device brings the thick plate portion together with the center information display closer to the driver's seat, thereby deforming the glass base. Effect of the Invention

[0007] According to the present invention, in a structure in which the glass base is deformable, a portion of the glass base that requires higher impact resistance is made into a thick plate portion, thereby making it possible to sufficiently ensure the impact resistance of that portion. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a schematic cross-sectional view of a glass base unit according to a first embodiment. [Diagram 2] FIG. 2 is a schematic cross-sectional view of the glass substrate of the first embodiment. [Diagram 3] FIG. 3 is a schematic cross-sectional view showing the glass plate after etching. [Figure 4] FIG. 4 is a block diagram showing a control system for the glass base unit of the first embodiment. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing a modified example of the glass base unit of the first embodiment. [Figure 6] FIG. 6 is a schematic cross-sectional view showing a glass base according to the second embodiment. [Figure 7] FIG. 7 is a schematic cross-sectional view showing a glass base according to a third embodiment. [Figure 8] FIG. 8 is a schematic cross-sectional view showing the glass plate after polishing. [Figure 9] FIG. 9 is a schematic cross-sectional view showing the glass plate after etching. [Figure 10] FIG. 10 is a schematic cross-sectional view showing a glass base according to the fourth embodiment. [Figure 11] FIG. 11 is a schematic cross-sectional view for explaining how to determine the radius of curvature of the first connecting surface and the radius of curvature of the overhanging surface. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, specific embodiments of the present invention will be described with reference to the drawings. However, the present invention is not limited to the following embodiments. Various modifications and substitutions can be made to the following embodiments without departing from the scope of the present invention.

[0010] In the following description, ranges expressed using "~" include both ends of the range. For example, a range expressed as "A~B" includes A and B.

[0011] The glass sheet thickness (average sheet thickness) is determined by measurement using a micrometer.

[0012] How to determine the radius of curvature of the curved surface of the glass will be explained later with reference to FIG.

[0013] The compressive stress value (hereinafter, CS) of the compressive stress layer of the glass and the depth of the compressive stress layer (hereinafter, DOL) are determined by measuring with a surface stress meter (FSM-6000) manufactured by Orihara Seisakusho Co., Ltd. The central tension (hereinafter, CT) of the glass is calculated from CS, DOL and the sheet thickness t according to the following formula: CT=CS[MPa]×DOL[mm] / (t[mm]-2×DOL[mm])

[0014] The limit bending radius of glass is the minimum bending radius at which no cracks occur when the glass is bent, and the bending radius is determined by the following bending test. The bending test and the bending test device used in the bending test are in accordance with the test and device described in WO 2016 / 194785. The bending test procedure is as follows. (Bending test) The first support plate and the second support plate are arranged in parallel so that the support surface of the first support plate and the support surface of the second support plate face each other. The first support plate and the second support plate support the end of the glass, respectively. The distance between the support surface of the first support plate and the support surface of the second support plate is maintained at a distance D [mm] calculated by the following formula (1). In this state, the position of the second support plate relative to the first support plate is moved back and forth by 100 mm in a direction parallel to the support surface of the first support plate and the support surface of the second support plate and in a direction that does not change the curvature direction of the glass. It is checked whether cracks are formed in the glass to be curved between the first support plate and the second support plate. The bending radius R is calculated by the following formula (2). D = (A × E × t / σ) + t (1) R=D / 2 (2) D: Distance between the support surface of the first support plate and the support surface of the second support plate [mm] A=1.198 E: Young's modulus of glass [MPa] t: Glass thickness [mm] σ: Bending stress [MPa]

[0015] The surface strength of the glass plate is determined by the ball-on-ring (BOR) test described below. (Ball-on-ring test) First, the glass plate is placed horizontally on a stainless steel ring with a diameter of 30 mm and a curvature radius of 2.5 mm at the contact point with the glass plate. Next, a steel sphere with a diameter of 10 mm is brought into contact with the glass plate placed on the ring at the center of the ring. In this state, the sphere is lowered and pressed against the glass plate (descending speed of the sphere: 1.0 mm / min), applying a static load to the glass plate and destroying it. The load at which the glass plate breaks is measured, and the average of 20 measurements is regarded as the surface strength of the glass plate. However, if the starting point of the glass plate's breakage is more than 2 mm away from the position where the sphere was pressed, this is excluded from the measurements used to calculate the average value.

[0016] [First aspect] The first embodiment will be described with reference to FIGS. FIG. 1 is a schematic cross-sectional view of a glass base unit of a first embodiment (hereinafter, glass base unit 10). FIG. 2 is a schematic cross-sectional view of a glass base of a first embodiment (hereinafter, glass base 1). FIG. 3 is a diagram showing the manufacturing process of the glass base 1, specifically, a schematic cross-sectional view showing a glass plate 41 after etching. FIG. 4 is a block diagram showing a control system for the glass base unit 10. As shown in FIG.

[0017] As shown in FIG. 1, the glass substrate unit 10 includes a glass substrate 1 and a glass deformation device 6 that deforms the glass substrate 1. Moreover, the glass base unit 10 further includes a controller 7 for controlling the glass deformation device 6, as shown in FIG. The glass base 1, the glass deformation device 6, and the controller 7 will be described individually below. For ease of explanation, the thickness direction of the glass base 1 will be referred to as the "thickness direction." Also, the direction in which the thin plate portion 2, the connection portion 4, and the thick plate portion 3, which will be described later, are arranged in the glass base 1 will be referred to as the "arrangement direction."

[0018] <Glass Base> As shown in FIG. 1, the glass base 1 has a thin plate portion 2, a thick plate portion 3, and a connection portion 4. The thin plate portion 2 has a first main surface 2a and a second main surface 2b opposite to the first main surface 2a. The thick plate portion 3 has a first main surface 3a and a second main surface 3b opposite to the first main surface 3a. The plate thickness t3 of the thick plate portion 3 is greater than the plate thickness t2 of the thin plate portion 2. The connecting portion 4 is disposed between the thin plate portion 2 and the thick plate portion 3, and has a first connecting surface 4a and a second connecting surface 4b. The first connecting surface 4a connects the first main surface 2a of the thin plate portion 2 to the first main surface 3a of the thick plate portion 3. The second connecting surface 4b connects the second main surface 2b of the thin plate portion 2 to the second main surface 3b of the thick plate portion 3. In the first embodiment, the plate thickness of the connection portion 4 gradually increases from the thin plate portion 2 side toward the thick plate portion 3 side. However, this is not limited thereto, and the plate thickness of the connection portion 4 may increase in a stepped manner from the thin plate portion 2 side toward the thick plate portion 3 side. Alternatively, the connection portion 4 may not be provided, and the thickness of the glass base 1 may change discontinuously from the thickness t2 to the thickness t3 at the boundary between the thin portion 2 and the thick portion 3.

[0019] The thin plate portion 2 and the connection portion 4 are flexible and elastically deformable, that is, the glass base 1 can change its shape. Specifically, the shape of the glass base 1 can be freely switched between a first shape (shape shown by dashed lines in FIG. 1) in which the thin plate portion 2 extends in a flat plate shape, and a second shape (shape shown by solid lines in FIG. 1) in which the thin plate portion 2 is elastically deformed in a concave shape toward the rear side in the plate thickness direction. The concave elastic deformation of the thin plate portion 2 improves the visibility of devices (e.g., display panels 22, 23, 24 described below) attached to the thin plate portion 2. However, the present invention is not limited to this, and the thin plate portion 2 may be elastically deformed in a convex shape toward the front side in the plate thickness direction, or the thin plate portion 2 may be elastically deformed in an S-shape by using multiple actuators described below. 1, the starting point (bending starting point) of deformation of the glass base 1 is the connection portion 4. In this case, the thin plate portion 2 does not overlap with the device (for example, a center information display described below) protected by the thick plate portion 3, and the head impact resistance of the device is sufficiently satisfied. However, the bending starting point is not limited to the connection portion 4, and may be located closer to the thin plate portion 2 than the connection portion 4.

[0020] As shown in FIG. 1, a display panel is attached to each of a first main surface 2a of the thin plate portion 2 and a first main surface 3a of the thick plate portion 3. In detail, the three display panels 22, 23, 24 are attached to the first main surface 2a of the thin plate portion 2 in a state spaced apart from one another in the arrangement direction. Here, between the first main surface 2a of the thin plate portion 2 and the three display panels 22, 23, 24, a film-like optical clear adhesive (hereinafter, OCA) (not shown) is interposed. Moreover, one display panel 25 is attached to the first main surface 3a of the thick plate portion 3 via an OCA (not shown). Each of the display panels 22 to 25 is, for example, a liquid crystal panel. A backlight unit (not shown) is disposed on the rear side of each liquid crystal panel. Each of the display panels 22 to 25 may be, for example, an organic EL panel, a plasma display panel, or an electronic ink panel. Alternatively, each of the display panels 22 to 25 may have a touch panel or the like. As a modified example, in a display device in which each of the display panels 22 to 25 includes a liquid crystal panel, a housing portion of the display device and the glass base 1 may be bonded together.

[0021] The glass base 1 on which the above-mentioned display panels 22-25 are attached functions as a cover glass for each of the display panels 22-25. That is, in the first embodiment, the glass base 1 is used as a cover glass to cover each of the display panels 22-25. When used as a cover glass, the glass base 1 is preferably glass that has been subjected to a chemical strengthening treatment (chemically strengthened glass).

[0022] The glass substrate 1 on which the above-mentioned display panels 22 to 25 are attached is assembled into a frame 26 having a concave-convex structure 21 . The frame 26 has a flat portion in a portion that forms the protrusion 21a of the concave-convex structure 21. With the display panel 25 sandwiched between this flat portion and the thick plate portion 3 of the glass substrate 1, the thick plate portion 3 is fixed to the protrusion 21a of the frame 26. The portion of the frame 26 that forms the recess 21b of the concave-convex structure 21 has an isosceles trapezoidal recessed portion. With the display panels 22, 23, 24 positioned between this recessed portion and the thin plate portion 2 of the glass base 1, the thin plate portion 2 is disposed in a state in which it can freely deform with respect to the recess 21b. It should be noted that the display panels 22, 23, and 24 are not fixed to the frame 26, and when the thin plate portion 2 is deformed, the respective positions of the display panels 22, 23, and 24 change accordingly.

[0023] The glass base 1 is deformable while the thin plate portion 2 and the thick plate portion 3 are fixed to the frame 26, and can be switched between a first shape and a second shape. More specifically, when the glass base 1 has the first shape, the thin plate portion 2 extends in a flat plate shape in front of the recessed portion 21b of the frame 26 along the arrangement direction. On the other hand, when the glass base 1 is in the second shape, the thin plate portion 2 is elastically deformed along the recess 21b of the frame 26. In detail, the glass base 1 is bent from the connection portion 4 as a starting point so that the thin plate portion 2 fits into the recess 21b, and further, the thin plate portion 2 is bent at a position between the display panels 22 and 23 and a position between the display panels 23 and 24.

[0024] When the glass base 1 is in the second shape, the display panels 22, 23, and 24 are sandwiched between the inner wall surface of the recess 21b and the thin plate portion 2. In other words, when the direction when viewing frame 26 from glass base 1 is the back side, and the direction when viewing glass base 1 from frame 26 is the front side, the shape of glass base 1 becomes the first shape, and display panels 22, 23, and 24 are positioned closer to the front. Conversely, when the glass base 1 has the second shape, the display panels 22, 23, and 24 are positioned further back.

[0025] Incidentally, when switching the shape of the glass base 1 from the first shape to the second shape, it is necessary to bend the glass base 1 at the bending starting point (specifically, at the connection portion 4, or at a position closer to the thin plate portion 2 than the connection portion 4). At this time, if the glass base 1 is difficult to bend at the bending starting point (if the bending is insufficient), for example, problems such as the display panel 24 being easily peeled off from the first main surface 2a of the thin plate portion 2 may occur.

[0026] In contrast, in the first embodiment, as shown in FIG. 2, the first connecting surface 4a of the connecting portion 4 is an arc-shaped curved surface, and the radius of curvature r1 of the first connecting surface 4a is 400 μm or more. This makes the connection portion 4 easier to bend, and makes the display panel 24 less likely to peel off from the first main surface 2a of the thin plate portion 2. In addition, since the first connecting surface 4a is an arc-shaped curved surface, even if air bubbles get between the first connecting surface 4a and the film material when a film material such as OCA is adhered to the first connecting surface 4a, it is expected that the air bubbles will be easily removed.

[0027] In order to more effectively exert the above-mentioned effects, the radius of curvature r1 of the first connecting surface 4a is preferably 550 μm or more, and more preferably 700 μm or more. Furthermore, there is no particular upper limit to the radius of curvature r1 of the first connecting surface 4a, but it is preferably 1300 μm or less, more preferably 1100 μm or less, and even more preferably 900 μm or less.

[0028] Here, a method for determining the radius of curvature r1 of the first connecting surface 4a will be described with reference to Fig. 11. Fig. 11 is a schematic cross-sectional view for explaining a method for determining the radius of curvature r1 of the first connecting surface 4a and the radius of curvature r2 of an overhanging surface 5a, which will be described later. FIG. 11 is an enlarged view of FIG. 6, which will be referred to in a later section.

[0029] The radius of curvature r1 of the first connecting surface 4a of the connecting portion 4 is determined as follows. First, consider a straight line L1 that slopes from the first main surface 3a of the thick plate portion 3 toward the second connecting surface 4b of the connecting portion 4 and intersects with the first main surface 3a of the thick plate portion 3 at an angle θ1 (=45°). When the straight line L1 is moved from the thick plate portion 3 in the direction toward the connecting portion 4 and the straight line L1 first touches the first connecting surface 4a at a single point, the point of contact is defined as a point S1. Next, a point on the first connecting surface 4a that is a length W1 (=10 μm) away from point S1 along the straight line L1 is designated as point S2. Similarly, a point on the first connecting surface 4a that is a length W1 (=10 μm) away from point S1 along the straight line L1 on the opposite side to point S2 is designated as point S3. The radius of a perfect circle that passes through points S1, S2, and S3 is defined as the radius of curvature r1 of the first connecting surface 4a of the connecting portion 4.

[0030] Suitable values ​​for the dimensions and characteristic quantities of each portion of the glass base 1 will now be described in detail. The thickness t2 of the thin plate portion 2 is preferably 0.05 mm or more, and more preferably 0.2 mm or more, whereas the thickness t2 of the thin plate portion 2 is preferably 0.8 mm or less, and more preferably 0.6 mm or less. The compressive stress value (CS) of the compressive stress layer of the thin plate portion 2 is preferably 500 MPa or more, more preferably 650 MPa or more, and even more preferably 750 MPa or more. The depth of the compressive stress layer (DOL) of the thin plate portion 2 is preferably 10 μm or more, more preferably 15 μm or more, and further preferably 25 μm or more. The internal tensile stress (CT) of the thin plate portion 2 is preferably 160 MPa or less, more preferably 140 MPa or less, while the CT of the thin plate portion 2 is preferably 20 MPa or more, more preferably 30 MPa or more. The limit bending radius of the thin plate portion 2 is preferably 60 mm or less, more preferably 50 mm or less, and further preferably 40 mm or less.

[0031] The plate thickness t3 of the thick plate portion 3 is preferably 0.5 mm or more, and more preferably 0.7 mm or more. On the other hand, the plate thickness t3 of the thick plate portion 3 is preferably 2.5 mm or less, and more preferably 2.0 mm or less. If the plate thickness t3 of the thick plate portion 3 is within the above range, the thick plate portion 3 has excellent impact resistance. The compressive stress value (CS) of the compressive stress layer of the thick plate portion 3 is preferably 500 MPa or more, more preferably 650 MPa or more, and even more preferably 750 MPa or more, because the thick plate portion 3 has excellent impact resistance. The depth of the compressive stress layer (DOL) of the thick plate portion 3 is preferably 10 μm or more, more preferably 15 μm or more, and even more preferably 25 μm or more, because the thick plate portion 3 has excellent impact resistance. The internal tensile stress (CT) of the thick plate portion 3 is preferably 50 MPa or less, more preferably 30 MPa or less, because the thick plate portion 3 has excellent impact resistance. On the other hand, the CT of the thick plate portion 3 is preferably 1 MPa or more, more preferably 5 MPa or more.

[0032] The surface strength of the thick plate portion 3 is preferably 150 kgf or more, more preferably 200 kgf or more, and even more preferably 250 kgf or more, because the thick plate portion 3 has excellent impact resistance.

[0033] 25mm 2It is preferable that the number density (unit: pieces / (5 cm x 5 cm)) of crushed pieces having the above area (hereinafter simply referred to as "crushed pieces") is different between the thin plate portion 2 and the thick plate portion 3, and it is more preferable that there is a clear difference. Specifically, the difference in number density of crushed fragments between the thin plate portion 2 and the thick plate portion 3 is preferably 0.1 fragments / (5cm x 5cm) or more, more preferably 1 fragment / (5cm x 5cm) or more, even more preferably 5 fragments / (5cm x 5cm) or more, and particularly preferably 7 fragments / (5cm x 5cm) or more. If the difference in number density of the crushed pieces is within the above range, the crushing in the thin plate portion 2 and the crushing in the thick plate portion 3 will be discontinuous, and even if the thin plate portion 2 is crushed, the spread of the crushing to the thick plate portion 3 can be reduced.

[0034] Furthermore, the number of crushed pieces may be greater in the thin plate portion 2 than in the thick plate portion 3. In this case, there is a technical significance in that when an impact is applied to the thin plate portion 2 and the thin plate portion 2 is crushed, the propagation of cracks from the thin plate portion 2 to the thick plate portion 3 is reduced. In other words, it is preferable that the number of crushed pieces is greater in the thin plate portion 2 than in the thick plate portion 3, because this suppresses the progression of cracks from the thin plate portion 2 to the thick plate portion 3 at the connection portion 4. Specifically, it is preferable that the progression of one or more cracks is suppressed per 30 cm of the length of the connection portion 4, and it is more preferable that the progression of three or more cracks is suppressed.

[0035] The number density of the crushed pieces is determined as follows. First, a head impact test is carried out on each of the thin plate portion 2 and the thick plate portion 3. More specifically, a test specimen is prepared using the thin plate portion 2 or the thick plate portion 3 as a cover glass in accordance with a procedure similar to that described in paragraphs

[0081] to

[0088] of JP 2019-64874 A, and a rigid model is collided with the test specimen. However, the collision position of the rigid model is the center position of the main surface of the cover glass, and the rigid model is caused to collide with this main surface in a direction perpendicular to the center position. If the cover glass does not break due to the impact of the rigid body model, the height of the rigid body model is raised by 5 cm and the rigid body model is made to collide with the cover glass again. This process is repeated until the cover glass breaks. If the cover glass breaks, the number and area of ​​the broken pieces are measured in an area 10 cm or more away from the impact point on the rigid model, and the number density of the broken pieces is calculated.

[0036] The size and density of the crushed pieces can be adjusted by adjusting the conditions of the chemical strengthening treatment described below. For example, when the glass plate is cooled after being immersed in molten salt, cooling is promoted only for the portion that will become the thin plate portion 2 or the portion that will become the thick plate portion 3. By using such a method, the size and density of the crushed pieces can be precisely controlled.

[0037] The ratio of the CT of the thin plate portion 2 to the CT of the thick plate portion 3 (CT of the thin plate portion 2 / CT of the thick plate portion 3) is preferably 1.1 or more, more preferably 1.5 or more, and even more preferably 3.0 or more, in order to maintain the crack strength of the thick plate portion 3. On the other hand, in order to maintain the crack strength of the thin plate portion 2, the above ratio is preferably 20 or less, more preferably 10 or less, and even more preferably 7 or less.

[0038] As described above, the first connecting surface 4a of the connecting portion 4 is an arc-shaped curved surface. On the other hand, the second connection surface 4b of the connection part 4 is a projection surface of the first connection surface 4a when projected in a direction parallel to the plate thickness direction. Therefore, the plate thickness of the connection part 4 changes continuously in the arrangement direction, becoming thicker as it approaches the thick plate part 3 and becoming thinner as it approaches the thin plate part 2.

[0039] Here, by adjusting the plate thickness of the connection portion 4, it is possible to increase or decrease the progression of a crack from the thin plate portion 2 to the thick plate portion 3. Specifically, the thinner the plate thickness of the connection portion 4, the more the progression of a crack straddling the connection portion 4 can be suppressed. For the reasons mentioned above, the plate thickness of the connection portion 4 is preferably 0.5 mm or less, more preferably 0.3 mm or less, and even more preferably 0.2 mm or less. On the other hand, from the viewpoint of preventing the glass base 1 from breaking during transportation and installation, the plate thickness of the connection portion 4 is preferably 0.05 mm or more, more preferably 0.07 mm or more, and even more preferably 0.1 mm or more. In this specification, unless otherwise specified, the plate thickness of the connection portion 4 refers to the plate thickness at the thinnest portion of the connection portion 4.

[0040] The above-described method for producing the glass base 1 according to the first embodiment will be described with reference to FIG. First, a glass plate 41 having a first main surface 41a and a second main surface 41b is prepared. The thickness t 1 of the prepared glass plate 41 is the same as the thickness t 3 of the thick portion 3 of the completed glass base 1 . Examples of the glass type of the glass plate 41 include soda lime glass and aluminosilicate glass (SiO2-Al2O3-Na2O-based glass). Examples of the glass composition of the glass plate 41 include the glass composition described in paragraph

[0019] of JP 2019-006650 A. When performing a chemical strengthening treatment described later, for example, a chemically strengthened glass based on aluminosilicate glass (for example, "Dragontrail (registered trademark)") is preferably used.

[0041] Thereafter, the prepared glass plate 41 is slimmed. The slimming includes masking and etching. In the masking, the surface of the first main surface 41a of the glass plate 41 that will become the first main surface 3a of the thick plate portion 3 described above, and the entire second main surface 41b of the glass plate 41 are each covered with a mask material 45. The material of the mask material 45 is not particularly limited as long as it is a material that has resistance to the etching solution described below, and any conventionally known material can be appropriately selected and used. Alternatively, as the mask material 45, a resist pattern may be formed on the first main surface 41a of the glass plate 41.

[0042] In the etching, the glass plate 41 covered with the mask material 45 is immersed in a known etching solution to dissolve the portions not covered with the mask material 45 . The etching is not limited to a wet method using an etching solution, but may be a dry method using, for example, hydrogen fluoride gas. Dissolution by etching progresses gradually from the first main surface 41a that is not covered with the mask material 45 toward the second main surface 41b, and as a result, a portion of the glass plate 41 that will become the thin plate portion 2 is formed. The etching forms a smooth etched surface (curved surface) on the first main surface 41a of the glass plate 41. This curved surface becomes the first connecting surface 4a having a specific radius of curvature r1, and as a result, a portion of the glass plate 41 that becomes the connecting portion 4 is formed. On the other hand, the portion of the glass plate 41 that remains unmelted becomes the thick plate portion 3 . After etching, the mask material 45 is appropriately removed by a known method.

[0043] The slimmed glass plate 41 may be subjected to a chemical strengthening treatment. When chemical strengthening treatment is performed, glass for chemical strengthening is used as the glass plate 41 . In the chemical strengthening treatment, a conventionally known method can be adopted, and typically, the glass sheet 41 is immersed in a molten salt. As a result, a compressive stress layer is formed on the surface layer of the glass sheet 41, and the glass sheet 41 is strengthened. The treatment conditions, such as the temperature of the molten salt during the treatment and the immersion time, may be set so that the compressive stress value (CS) and the thickness (DOL) of the compressive stress layer become desired values. After being immersed in the molten salt, the glass plate 41 is pulled out of the molten salt and cooled. At this time, the glass plate 41 may be washed with industrial water or ion-exchanged water.

[0044] In the above-described manufacturing method, the glass base 1 is formed only by the glass plate 41, but the present invention is not limited to this. For example, a decorative layer may be laminated on the first main surface 41a side of the glass plate 41 to produce a laminate, and the glass base 1 may be formed by this laminate. The decorative layer is formed of, for example, a printed layer (ink layer) recorded by an inkjet method. In this case, by controlling the thickness of the printed layer according to the location of each part of the glass plate 41, the plate thickness of each part of the glass base 1 can be adjusted to the respective suitable ranges described above.

[0045] <Glass transformation equipment> The glass deformation device 6 is a device that deforms the glass base 1 by moving one of the thin plate portion 2 and the thick plate portion 3 in the glass base 1 . The glass deformation device 6 is constituted by, for example, an actuator that applies an external force to one of the thin plate portion 2 and the thick plate portion 3 in the glass base 1. Specifically, the actuator constituting the glass transformation device 6 is an electric actuator having a linear-acting rod 6a that can move forward and backward, a motor (not shown), and a power source (not shown). The tip of the rod 6a is connected to the first main surface 2a of the thin plate portion 2 via the display panel 23.

[0046] In the first embodiment, the glass deformation device 6 applies an external force to the thin plate portion 2 when the glass base 1 is deformed, and moves the thin plate portion 2 together with the display panels 22, 23, and 24. In detail, when the motor is driven by power supplied from the power source, the rod 6a moves and applies an external force from the first main surface 2a side to the thin plate portion 2. At this time, when the rod 6a advances, the thin plate portion 2 is pushed forward by the rod 6a. As a result, the thin plate portion 2 moves together with the display panels 22, 23, 24, and extends in a flat plate shape in front of the recesses 21b in the concave-convex structure 21 of the frame 26 along the arrangement direction. In other words, the shape of the glass base 1 becomes the first shape. Conversely, when the rod 6a retracts, the thin plate portion 2 is pulled toward the rear by the rod 6a. As a result, the thin plate portion 2 moves together with the display panels 22, 23, 24, and is elastically deformed into a concave shape along the recess 21b. In other words, the shape of the glass base 1 becomes the second shape.

[0047] In the first embodiment, the glass deformation device 6 applies an external force to the thin plate portion 2 in the glass base 1 to move the thin plate portion 2, thereby deforming the glass base 1, but is not limited to this. For example, the glass deformation device 6 may apply an external force to the thick plate portion 3 in the glass base 1 to move the thick plate portion 3. In this case, the thick plate portion 3 itself does not bend, and the glass base 1 deforms so as to bend starting from the connection portion 4.

[0048] The actuator constituting the glass deformation device 6 is not limited to an electric actuator using a linear-type rod, and may be an actuator of another type. Examples of other types of actuators include an actuator consisting of a cam link mechanism, an actuator consisting of a power cylinder driven by hydraulic or pneumatic pressure, an actuator that uses a piezoelectric element such as a piezo element, or an electromagnetic solenoid actuator.

[0049] Furthermore, the glass deforming device 6 is not limited to an actuator, and may be any device that can apply a sufficient external force to one of the thin plate portion 2 and the thick plate portion 3 in the glass base 1 to deform the glass base 1. For example, a shape memory alloy may be arranged along the glass base 1, and the glass base 1 may be deformed by utilizing the shape change of the shape memory alloy caused by a change in temperature.

[0050] <controller> The controller 7 is a device that controls the operating state of the actuator that constitutes the glass deformation device 6. The controller 7 is configured, for example, by a drive control circuit (not shown). The drive control circuit includes a memory and a processor that executes a program stored in the memory. As the processor, a general-purpose CPU (Central Processing Unit) can be used. In addition to CPUs, programmable logic devices (PLDs), such as field programmable gate arrays (FPGAs), which are processors whose circuit configuration can be changed after manufacture, can also be used. It is also possible to use dedicated electrical circuits, such as ASICs (Application Specific Integrated Circuits), which are processors having a circuit configuration designed specifically for performing specific processing. Furthermore, the control circuit may be configured using one of the various processors mentioned above, or may be configured using a combination of two or more processors of the same or different types, for example, a combination of multiple FPGAs, or a combination of an FPGA and a CPU, etc. Also, a processor may be used that realizes the functions of an entire system including a plurality of control circuits in a single IC (Integrated Circuit) chip, as typified by a system on chip (SoC).

[0051] The controller 7 automatically switches the operating state of the actuator when a predetermined condition is met. In detail, the controller 7 receives a signal output from a predetermined sensor 8, and switches the operating state of the actuator based on the output signal. The operating state of the actuator switches between a normal state and a state when a certain condition is met, specifically, between a state in which the aforementioned rod 6a is advanced and a state in which the rod 6a is retreated. As the operating state of the actuator is switched, the shape of the glass base 1 is switched from the first shape to the second shape, or from the second shape to the first shape.

[0052] In the first embodiment, the operating state of the actuator is controlled by the controller 7, but the operating state of the actuator may be manually switched by an operator. For example, the operator may operate a handle and a driving force may be transmitted from the handle to the rod 6a, thereby moving the rod 6a.

[0053] <Applications of glass base unit> The above-mentioned glass base 1, display panels 22 to 25, frame 26, glass transformation device 6, and controller 7 constitute a glass base unit 10. As described above, the glass base 1 functions as a cover glass for the display panels 22 to 25. In other words, the glass base unit 10 forms a cover glass assembly in which the cover glass is assembled. A cover glass assembly including the glass base unit 10 is used, for example, as a display device, and a specific example of such a display device is an in-vehicle display device that is mounted on a vehicle for use. Specifically, the glass substrate unit 10 is used as an in-vehicle display device having an instrument cluster (cluster) located in front of the driver's seat, and a center information display (CID) located in front of the driver's seat and between the driver's seat and the passenger seat.

[0054] In the above case, in the glass base unit 10 assembled as an in-vehicle display device, the display panels 22, 23, and 24 arranged on the side of the recess 21b in the concave-convex structure 21 of the frame 26 correspond to a cluster. Moreover, the display panel 25 arranged on the side of the convex portion 21a in the concave-convex structure 21 of the frame 26 corresponds to a CID. Furthermore, the thin plate portion 2 in the glass base 1 is used as a cover glass for the cluster, and the thick plate portion 3 in the glass base 1 is used as a cover glass for the CID. That is, the cluster is attached to the first main surface 2a of the thin plate portion 2, and the CID is attached to the first main surface 3a of the thick plate portion 3.

[0055] Since the cover glass of the CID does not have a steering wheel that the driver operates, it is likely to be hit directly by the head of the occupant in the event of a vehicle collision. For this reason, the portion of the glass base 1 located on the CID side is required to have higher impact resistance (head impact resistance), and by making this portion into the thick plate portion 3, sufficient impact resistance is ensured for this portion. Note that the thick plate portion 3 preferably has an impact resistance sufficient to prevent it from breaking when hit by the head of the occupant in the event of a vehicle collision.

[0056] On the other hand, the thin plate portion 2 used as the cover glass of the cluster is positioned further back than the steering wheel, so there is a low possibility that the occupant's head will hit it directly, and therefore it does not require the same level of impact resistance as the thick plate portion 3. In addition, while the driver is operating the steering wheel to drive the vehicle, it is preferable to elastically deform the thin plate portion 2 into a concave shape along the recess 21b in the uneven structure 21 of the frame 26 and move it toward the rear together with the display panels 22, 23, and 24 in order to improve the visibility of the cluster. Conversely, when the steering wheel is not being operated (for example, when the vehicle is stopped for a certain period of time), visibility of the cluster is not required, so there is no need to elastically deform the thin plate portion 2 into a concave shape, and it is preferable for the thin plate portion 2 to extend in a flat plate shape.

[0057] In order to prevent the visibility of the cluster and the like from being impaired by the reflection of external light, it is also preferable to move the thin plate portion 2 together with the display panels 22, 23, and 24. For example, the interior space of the vehicle is photographed by a camera (not shown) installed in the vehicle, the photographed image is analyzed to identify the position of the external light (irradiation position) and the position of the driver, and the thin plate portion 2 and the display panels 22, 23, and 24 are moved so that these positions are out of the positional relationship of regular reflection with respect to at least one surface of the cluster.

[0058] For the above reasons, in the in-vehicle display device incorporating the glass base unit 10, while the vehicle equipped with the in-vehicle display device is traveling, more specifically, while the steering wheel is being operated, the glass deformation device 6 elastically deforms the thin plate portion 2 in the glass base 1. At this time, the thin plate portion 2 elastically deforms into a convex, concave, S-shape, etc., but from the viewpoint of improving the visibility of the cluster, it is more preferable for the thin plate portion 2 to deform into a concave shape. In such a case, the thin plate portion 2 moves toward the rear together with the cluster, and the glass base 1 deforms and switches from the first shape to the second shape.

[0059] When the controller 7 receives the detection signal output from the sensor 8, it controls the operating state of the actuator that constitutes the glass deformation device 6. The controller 7 is configured as an on-board controller, such as an ECU (Electric Control Unit). In this case, the controller 7 receives the above-mentioned detection signal from the sensor 8 via, for example, an in-vehicle LAN, and controls the glass deformation device 6. The glass deformation device 6 operates under the control of the controller 7, and presses the thin plate portion 2 forward to extend it into a flat plate shape. As a result, the thin plate portion 2 moves toward the front together with the cluster, and the glass base 1 deforms and switches from the second shape to the first shape.

[0060] As described above, in the vehicle-mounted display device incorporating the glass base unit 10, the shape of the glass base 1 can be changed by moving the thin plate portion 2 in accordance with switching of the mode related to the cluster position. This improves the convenience of the in-vehicle display device; more specifically, the position of the cluster can be adjusted to a position convenient for the driver depending on the current mode.

[0061] In the vehicle-mounted display device in which the glass base unit 10 is incorporated, the thin plate portion 2 in the glass base 1 is not limited to being moved, and the thick plate portion 3 may be moved. Specifically, for example, as shown in Fig. 5, when the steering wheel is operated, the glass deformation device 6 may push the thick plate portion 3 toward the driver. This causes the thick plate portion 3 to move (strictly speaking, rotate) toward the driver's seat together with the CID, starting from the connection portion 4, and the glass base 1 is bent and deformed starting from the connection portion 4. FIG. 5 is a schematic cross-sectional view showing a glass base unit according to a modified example (hereinafter, glass base unit 10X).

[0062] In the vehicle-mounted display device incorporating the above-described glass base unit 10X, the thick plate portion 3 together with the CID can be brought closer to the driver's seat when the driver is operating the steering wheel, improving convenience for the driver.

[0063] [Second aspect] The second embodiment will be described with reference to FIG. FIG. 6 is a schematic cross-sectional view showing a glass base of a second embodiment (hereinafter, glass base 1X). In addition, the second embodiment differs from the first embodiment in the structure of the glass substrate, but is otherwise common to the first embodiment. Therefore, in Fig. 6, the same parts as those in the first embodiment are indicated by the same reference numerals, and the description thereof is omitted.

[0064] In the second embodiment, as shown in FIG. 6, a glass base 1X has an overhang portion 5 at a connection portion 4. The overhang portion 5 is a part of the connection portion 4, and is a portion that protrudes from the thick plate portion 3 toward the thin plate portion 2. The overhang portion 5 has an overhang surface 5a that is a part of the first connection surface 4a of the connection portion 4, and a surface 5b that forms the same plane as the first main surface 3a of the thick plate portion 3. The overhang portion 5 is formed when dissolution of the glass plate 41 due to etching proceeds excessively during slimming in the method for producing a glass base according to the first embodiment described above.

[0065] The radius of curvature r2 of the overhang surface 5a shown in FIG. 6 is preferably 150 μm or more, and more preferably 300 μm or more, because when the glass base 1X is viewed from the first main surface 2a and the first main surface 3a side, the boundary portion between the thin plate portion 2 and the thick plate portion 3 looks sharp, which is preferable in terms of appearance. On the other hand, in order to protect the connection portion 4 and make it difficult for it to break when the glass base 1X is transported or processed, the radius of curvature r2 of the overhanging surface 5a is preferably 1100 μm or less, and more preferably 900 μm or less.

[0066] Here, a method for determining the radius of curvature r2 of the overhanging surface 5a will be described with reference to Fig. 11. The radius of curvature r2 of the overhanging surface 5a is determined as follows. First, consider the line L2 that is perpendicular to the line L1 described above. When the straight line L2 is moved from the thick plate portion 3 in the direction of the overhang portion 5 and the straight line L2 first touches the overhang surface 5a at a single point, the point of contact is designated as a point S4. Next, a point on the overhang surface 5a is defined as point S5, which is located along the straight line L2 from point S4 by a length W2 (=10 μm) toward the thick plate portion 3. A point on the opposite side of point S5 along the straight line L2 from point S4 by a length W2 (=10 μm) is defined as point S6, which is symmetrical to point S5. Point S6 may or may not be a point on the overhang surface 5a. The radius of a perfect circle that passes through points S4, S5, and S6 is defined as the radius of curvature r2 of the overhanging surface 5a.

[0067] [Third aspect] Next, a third embodiment will be described with reference to FIGS. FIG. 7 is a schematic cross-sectional view showing a glass base of a third embodiment (hereinafter, glass base 1Y). 8 and 9 are diagrams showing the manufacturing process of the glass base 1Y. Fig. 8 is a schematic cross-sectional view showing a glass plate 41 after polishing. Fig. 9 is a schematic cross-sectional view showing a glass plate 41 after etching. The third embodiment differs from the first embodiment in the structure of the glass base, but is otherwise common to the first embodiment. Therefore, in Figs. 7 to 9, the same parts as those in the first embodiment are denoted by the same reference numerals, and the description thereof will be omitted.

[0068] In the third embodiment, the plate thickness of the connection portion 4 at the thinnest portion in the glass base 1Y is defined as the plate thickness t4 of the connection portion 4. In the glass base 1Y, the plate thickness t4 of the connection portion 4 is smaller than the plate thickness t2 of the thin plate portion 2. This makes the connection portion 4 more easily bendable. Because the above-mentioned effects can be more effectively exerted and because the progression of cracks across the connection portion 4 can be suppressed as described above, the plate thickness t4 of the connection portion 4 is preferably 0.5 mm or less, more preferably 0.3 mm or less, and even more preferably 0.2 mm or less. On the other hand, the lower limit of the plate thickness t4 of the connection portion 4 is not particularly limited, but is preferably 0.05 mm or more, and more preferably 0.1 mm or more.

[0069] Next, a method for manufacturing the glass base 1Y will be described with reference to FIGS. In the method for manufacturing the glass base 1Y, the steps other than slimming are the same as those in the first embodiment, so the description will be omitted and only the slimming will be described below. The slimming in the manufacturing method of the glass base 1Y includes polishing, masking and etching.

[0070] 8, the portions of the glass plate 41 that will become the thin plate portion 2 and the connection portion 4 are polished from the first main surface 41a to the second main surface 41b so as to reduce the plate thickness t1. The portions that will become the thick plate portion 3 are left unpolished. By polishing, a polished surface 41c is formed on the glass plate 41 at a position lower than the first main surface 41a. At the boundary between the first main surface 41a and the polished surface 41c, a polished end surface 41d is formed as a step between both surfaces. The polishing method is not particularly limited, and a conventionally known polishing pad or the like can be appropriately used.

[0071] In the masking after polishing, the entire first and second main surfaces 41a and 41b of the glass plate 41 and the polished surface 41c are covered with a mask material 45 as shown in FIG. At this time, only the surface of the polished surface 41c that will become the first main surface 2a of the thin plate portion 2 is covered with the mask material 45. In addition, the first main surface 41a may be covered with the mask material 45 while exposing the surface of the end of the polished end surface 41d.

[0072] In the etching after masking, the glass plate 41 covered with the mask material 45 is etched with an etching solution. As a result, dissolution by the etching solution gradually progresses toward the inside of the glass plate 41 in the parts not covered with the mask material 45, specifically, in the parts of the polished surface 41c, the polished end surface 41d, and the first main surface 41a. By etching, a portion that becomes the connection portion 4 is formed between the portion of the polished surface 41c that is covered with the mask material 45 and the first main surface 41a of the glass plate 41. Moreover, a smooth etched surface (curved surface) is formed in the portion that becomes the connection portion 4. The portions of the glass plate 41 that remain unmelted become the thin plate portion 2 and the thick plate portion 3. After etching, the mask material 45 is appropriately removed by a known method.

[0073] [Fourth aspect] Next, a fourth embodiment will be described with reference to FIG. FIG. 10 is a schematic cross-sectional view showing a glass base of a fourth embodiment (hereinafter, glass base 1Z). In addition, the fourth embodiment differs from the first embodiment in the structure of the glass substrate, but is otherwise common to the first embodiment. Therefore, in Fig. 10, the same parts as those in the first embodiment are indicated by the same reference numerals, and the description thereof is omitted.

[0074] In the fourth embodiment, as shown in FIG. 10 , a first connecting surface 4a of a connecting portion 4 in a glass base 1Z has a first adjacent surface 4c adjacent to the first main surface 2a of the thin plate portion 2 and a second adjacent surface 4d adjacent to the first main surface 3a of the thick plate portion 3. The first adjacent surface 4c is a curved surface having a circular arc shape that is convex toward the second connecting surface 4b of the connecting portion 4. The second adjacent surface 4d is an arc-shaped curved surface that is convex toward the opposite side to the second connecting surface 4b. As shown in FIG. 10, the first adjacent surface 4c and the second adjacent surface 4d are connected to each other to form a first connecting surface 4a that is bent in an S-shape. The S-shaped bent first connecting surface 4a is formed in the manufacturing method of the glass substrate in the third aspect described above by polishing, after etching, the end portion of the first main surface 41a that is covered with the mask material 45 during etching, which is closer to the polished surface 41c, into an arc shape.

[0075] In the glass base 1Z, the first connecting surface 4a of the connecting portion 4 is gently curved in an S-shape, so that when a film material such as OCA is adhered to the first connecting surface 4a, if any air bubbles are trapped between the first connecting surface 4a and the film material, the air bubbles can be more easily removed. In the fourth embodiment, the radius of curvature of the first adjacent surface 4c corresponds to the radius of curvature r1 of the first connecting surface 4a of the connecting portion 4.

[0076] Although the present invention has been described in detail and with reference to specific embodiments, it will be apparent to those skilled in the art that various changes and modifications can be made without departing from the spirit and scope of the invention. This application is based on Japanese Patent Application No. 2019-160236 filed on September 3, 2019, the contents of which are incorporated herein by reference. [Explanation of symbols]

[0077] 1: Glass substrate 1X: Glass substrate 1Y: Glass substrate 1Z: Glass substrate 2: Thin plate part 2a: 1st main surface 2b: 2nd principal surface 3: Thick plate section 3a: 1st main surface 3b: 2nd principal surface 4: Connection part 4a: First connection surface 4b: Second connection surface 4c: First adjacent surface 4d: 2nd adjacent surface 5: Overhang 5a: Overhang surface 5b: Face 6: Glass transformation equipment 6a: Rod 7: Controller 8: Sensor 10: Glass substrate unit (cover glass assembly) 10X: Glass base unit 21: Uneven structure 21a: Convex 21b: Recess 22: Display panel 23: Display panel 24: Display panel 25: Display panel 26: Frame 41: Glass plate 41a: First main surface 41b: Second main surface 41c: Polished surface 41d: Polished end face 45: Masking material r1: Radius of curvature of the first connecting surface r2: Radius of curvature of the overhang surface t1: thickness of glass plate t2: thickness of thin plate t3: Thickness of the thick plate t4: Plate thickness of connection part L1, L2: Straight line W1, W2: Length θ1: Angle S1, S2, S3, S4, S5, S6: points P1:Position D1, D2: distance

Claims

1. A glass substrate and a glass deformation device for deforming the glass substrate, The glass substrate is A thin plate portion having a first main surface and a second main surface opposite to the first main surface; a thick plate portion having a plate thickness greater than a plate thickness of the thin plate portion, and having a first main surface and a second main surface opposite to the first main surface; The glass deformation device is a glass base unit configured by an actuator that applies an external force, and the glass base is deformed by moving one of the thin plate portion and the thick plate portion by the external force.

2. 2. The glass base unit according to claim 1, wherein the shape of the glass base is freely switchable between a first shape in which the thin plate portion extends in a flat plate shape and a second shape in which the thin plate portion is elastically deformed.

3. The glass base unit according to claim 2 , wherein the second shape is a shape in which the thin plate portion is elastically deformed into a concave shape.

4. A display panel is attached to a first main surface of the thin plate portion, The glass base unit according to any one of claims 1 to 3, wherein the glass deformation device moves the thin plate portion together with the display panel.

5. the glass base further includes a connection portion having a first connection surface connecting a first main surface of the thin plate portion and a first main surface of the thick plate portion, and a second connection surface connecting a second main surface of the thin plate portion and a second main surface of the thick plate portion, a starting point of deformation of the glass base is located at the connection portion or on the thin plate portion side relative to the connection portion, The first connection surface is an arc-shaped curved surface, 5. The glass base unit according to claim 1, wherein the first connecting surface has a radius of curvature of 400 μm or more.

6. the glass base further includes a connection portion having a first connection surface connecting a first main surface of the thin plate portion and a first main surface of the thick plate portion, and a second connection surface connecting a second main surface of the thin plate portion and a second main surface of the thick plate portion, a starting point of deformation of the glass base is located at the connection portion or on the thin plate portion side relative to the connection portion, 5. The glass base unit according to claim 1, wherein the plate thickness at the thinnest point in the connection portion is smaller than the plate thickness of the thin plate portion.

7. 7. The glass base unit according to claim 6, wherein the thinnest portion of the connection portion has a plate thickness of 0.5 mm or less.

8. The glass base unit according to any one of claims 5 to 7, wherein the connecting portion has an overhang portion.

9. the glass base further includes a connection portion having a first connection surface connecting a first main surface of the thin plate portion and a first main surface of the thick plate portion, and a second connection surface connecting a second main surface of the thin plate portion and a second main surface of the thick plate portion, a starting point of deformation of the glass base is located at the connection portion or on the thin plate portion side relative to the connection portion, the first connecting surface has a first adjacent surface adjacent to the first main surface of the thin plate portion and a second adjacent surface adjacent to the first main surface of the thick plate portion, The glass base unit according to any one of claims 1 to 4, wherein the first adjacent surface and the second adjacent surface are both arc-shaped curved surfaces and are connected to each other to form the first connecting surface that is curved in an S-shape.

10. The plate thickness of the thin plate portion is 0.05 mm or more and 0.8 mm or less, 10. The glass base unit according to claim 1, wherein the thick portion has a thickness of 0.5 mm or more and 2.5 mm or less.

11. The glass base unit according to any one of claims 1 to 10, wherein the glass base is a chemically strengthened glass.

12. The glass substrate unit according to claim 11, further comprising a controller for controlling an operating state of the actuator.

13. The glass substrate unit according to any one of claims 1 to 12, A cover glass assembly, wherein the glass substrate serves as a cover glass for a display panel.

14. An in-vehicle display device comprising: an instrument cluster arranged in front of a driver's seat; a center information display arranged in front of a vehicle between the driver's seat and a passenger seat; and the glass base unit according to any one of claims 1 to 12, The instrument cluster is attached to a first main surface of the thin plate portion, The center information display is attached to a first main surface of the thick plate portion, While a vehicle equipped with the in-vehicle display device is traveling, the glass deformation device elastically deforms the thin plate portion into a concave shape and moves it together with the instrument cluster, thereby deforming the glass base.

15. An in-vehicle display device comprising: an instrument cluster arranged in front of a driver's seat; a center information display arranged in front of a vehicle between the driver's seat and a passenger seat; and the glass base unit according to any one of claims 1 to 12, The instrument cluster is attached to a first main surface of the thin plate portion, The center information display is attached to a first main surface of the thick plate portion, The in-vehicle display device, wherein while a vehicle equipped with the in-vehicle display device is traveling, the glass deformation device moves the thick plate portion together with the center information display toward a driver's seat, thereby deforming the glass base.

Citation Information

Patent Citations

  • Controller for pulse motor

    JP1986098194A

  • Method for manufacturing phase shift mask

    JP2001142194A

  • Glass for electronic apparatus

    JP2015099171A

  • Cover member, portable information terminal having the same, display device, and method for producing cover glass

    JP2016145968A

  • Glass substrate and method for producing the same, cover glass and method for producing the same, portable information terminal, and display device

    JP2017001940A