Metal mask manufacturing method, metal mask

The method addresses mask deformation issues by preheating components and using a laminated adhesive structure, resulting in a more precise and stable metal mask for vapor deposition.

JP7573003B2Active Publication Date: 2024-10-24MAXELL LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2022162062
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-10-07
Publication Date
2024-10-24
Estimated Expiration
2037-08-28

AI Technical Summary

Technical Problem

Conventional vapor deposition masks face challenges in maintaining high precision and stability due to mask deformation, especially as masks become thinner and hole patterns become finer, leading to decreased positional accuracy of vapor-deposited products.

Method used

A method for manufacturing a metal mask involves preheating the mother mold, exposure device, and photomask to a predetermined temperature before exposure, and using a laminated structure with a specific adhesive layer to stabilize the mask body and frame, reducing thermal expansion effects.

Benefits of technology

This method enables the production of a metal mask with improved precision and stability, ensuring accurate alignment and reducing deformation during the vapor deposition process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573003000001
    Figure 0007573003000001
  • Figure 0007573003000002
    Figure 0007573003000002
  • Figure 0007573003000003
    Figure 0007573003000003
Patent Text Reader

Abstract

A method for manufacturing a metal mask that can stably and accurately form a mask body is provided. [Solution] A method for manufacturing a metal mask having a mask body with a large number of through holes and a frame body for reinforcing the mask body, comprising a mask body forming process for forming the mask body and a joining process for joining the mask body and the frame body, and the mask body forming process includes a preheating process for preheating to a predetermined preheating temperature.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a metal mask used in processes such as vapor deposition, printing, and solder ball mounting, and to a metal mask manufactured by the method. [Background technology]

[0002] The deposition mask method is often used to form the light-emitting layer of an organic EL (Electroluminescence) element. In this deposition mask method, a deposition mask with holes removed at the locations of the substrate corresponding to the deposition sites is used to deposit organic light-emitting materials at desired locations on a substrate made of a transparent material such as glass. Such deposition masks must be thin and must have a large number of deposition through-holes for passing the deposition material formed with high precision. In recent years, it has been proposed to form the deposition masks by electroforming.

[0003] In forming a mask by electroforming, a resist is placed in advance at many locations on the surface of the mother mold that will become the deposition holes, and then an electrodeposition layer made of an electroformable metal such as nickel that forms a mask is formed on the mother mold surface by electroforming, simultaneously forming a state in which many deposition holes are provided in a predetermined pattern. If necessary, a reinforcing frame is integrated by plating or the like to obtain the desired mask structure, and the mother mold is separated to complete the deposition mask. An example of a conventional deposition mask manufactured using electroforming is disclosed in Japanese Patent Application Laid-Open No. 2005-15908. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2005-15908 A Summary of the Invention [Problem to be solved by the invention]

[0005] Conventional deposition masks have the configurations shown in the above-mentioned patent documents, and the frame is appropriately integrated with the mask body by electroforming, thereby suppressing relative deformation between the mask and the substrate when heat is applied during the deposition process, and preventing deterioration of the positional accuracy of the deposition formation.

[0006] However, in recent years, there has been a demand in the market for even higher precision in deposition formation, leading to thinner masks and finer through-hole patterns, and as a result, the impact of mask deformation has become extremely large.

[0007] The present invention has been made to solve the above-mentioned problems, and has an object to provide a method for manufacturing a metal mask that can form a mask body stably and with high precision, and a metal mask manufactured by the manufacturing method. [Means for solving the problem]

[0008] The method for manufacturing a metal mask disclosed in the present invention is a method for manufacturing a metal mask having a mask body with a number of through holes and a frame body for reinforcing the mask body, and includes a mask body formation process for forming the mask body and a joining process for joining the mask body and the frame body, and the mask body formation process includes a preheating process for preheating to a predetermined preheating temperature.

[0009] The mask body forming process also includes a resist layer forming process for forming a resist layer on a matrix, and an exposure process for exposing the resist layer to light, and includes a matrix preheating process for preheating the matrix to a predetermined preheat temperature before the exposure process.

[0010] In the exposure step, exposure is performed in an exposure device, and a matrix device preheating step is performed before the exposure step, in which the inside of the exposure device is preheated to a predetermined preheat temperature.

[0011] In the exposure step, exposure is performed using a photomask having a predetermined pattern corresponding to the mask body, and a photomask preheating step of preheating the photomask to a predetermined preheating temperature is performed before the exposure step.

[0012] In addition, the matrix, the inside of the exposure tool, and the photomask are preheated to the same temperature.

[0013] In addition, the maximum temperature that can be reached inside the exposure device is set as the preheat temperature.

[0014] In addition, the mask body forming process further includes, after the exposure process, a primary pattern resist forming process in which unexposed portions of the resist are removed to form a primary pattern resist, and a primary electrodeposition layer forming process in which a primary electrodeposition layer is formed by electroforming on the surface of the mother mold that is not covered with the primary pattern resist, and the maximum temperature among the exposure temperature in the exposure process, the electroforming temperature in the primary electrodeposition layer forming process, and the deposition temperature in the deposition process using a metal mask is set as the preheat temperature.

[0015] The present invention also provides a metal mask manufactured by the above-mentioned method for manufacturing a metal mask. [Brief description of the drawings]

[0016] [Figure 1] FIG. 1 is a schematic cross-sectional view of an electroforming master mold according to a first embodiment of the present invention. [Diagram 2] FIG. 1 is a schematic plan view of a deposition mask manufactured using an electroforming master according to a first embodiment of the present invention. [Diagram 3] FIG. 2 is an explanatory view of the configuration of a main part of a deposition mask manufactured using the electroforming master according to the first embodiment of the present invention. [Figure 4] FIG. 2 is an explanatory diagram of an outer frame resist formation process in the manufacture of an electroforming master die according to the first embodiment of the present invention. [Diagram 5] FIG. 2 is an explanatory view of a conductive layer forming step in the manufacture of an electroforming master according to the first embodiment of the present invention. [Figure 6] FIG. 4 is an explanatory view of the first half of the adhesive layer forming step in the manufacture of an electroforming master according to the first embodiment of the present invention. [Figure 7] FIG. 4 is an explanatory view of the latter half of the adhesive layer forming step in the manufacture of an electroforming master according to the first embodiment of the present invention. [Figure 8] FIG. 4 is an explanatory diagram of a transfer step of an adhesive layer and a conductive layer onto a base portion in the manufacture of an electroforming master according to the first embodiment of the present invention. [Figure 9] FIG. 2 is an explanatory diagram of a primary pattern resist formation process in a deposition mask manufacturing process using an electroforming mother mold according to the first embodiment of the present invention. [Figure 10] FIG. 2 is an explanatory diagram of a primary electrodeposition layer forming process in a deposition mask manufacturing process using an electroforming mother mold according to the first embodiment of the present invention. [Figure 11] FIG. 2 is an explanatory diagram of a secondary pattern resist formation process in a deposition mask manufacturing process using an electroforming mother mold according to the first embodiment of the present invention. [Figure 12] FIG. 2 is an explanatory diagram of a frame bonding and electrodeposited metal layer forming process in a deposition mask manufacturing process using an electroforming mother mold according to the first embodiment of the present invention. [Figure 13] 4A to 4C are explanatory views of a process of separating a base portion of a matrix and a part of a conductive layer in a deposition mask manufacturing process using an electroforming matrix according to the first embodiment of the present invention. [Figure 14] 4A to 4C are explanatory views of a process of separating a remaining conductive layer of a mold and a state of removing unnecessary parts from a deposition mask in a deposition mask manufacturing process using an electroforming mold according to a first embodiment of the present invention. [Figure 15] 13A to 13C are explanatory views of a state in which formation of an adhesive layer is completed and a state in which transfer of an adhesive layer and a conductive layer to a base portion is completed in a manufacturing process for an electroforming mother die according to a second embodiment of the present invention. [Figure 16] 13 is an explanatory diagram showing another state where formation of an adhesive layer is completed and where transfer of an adhesive layer and a conductive layer to a base portion is completed in the manufacturing process of an electroforming mother die according to the second embodiment of the present invention. FIG. [Figure 17] 13A to 13C are explanatory views of a state in which formation of an adhesive layer is completed and a state in which transfer of an adhesive layer and a conductive layer to a base portion is completed in a manufacturing process for an electroforming mother die according to a third embodiment of the present invention. [Figure 18] 13A to 13C are explanatory views of another state in which formation of an adhesive layer is completed and a state in which transfer of an adhesive layer and a conductive layer to a base portion is completed in the manufacturing process of an electroforming master according to the third embodiment of the present invention. [Figure 19]13 is an explanatory diagram showing yet another state in which formation of an adhesive layer is completed and transfer of an adhesive layer and a conductive layer to a base portion is completed in the manufacturing process of an electroforming master according to the third embodiment of the present invention. FIG. [Figure 20] FIG. 13 is an explanatory view of an adhesive layer forming step in the manufacture of an electroforming master according to a fourth embodiment of the present invention. [Figure 21] 13A to 13C are explanatory views of a state in which formation of an adhesive layer is completed and a state in which transfer of an adhesive layer and a conductive layer to a base portion is completed in a manufacturing process for an electroforming mother die according to a fourth embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] (First embodiment of the present invention) Hereinafter, an electroforming matrix according to a first embodiment of the present invention will be described with reference to FIGS. In this embodiment, the present invention is applied to a master mold for forming a deposition mask for an organic EL element by electroforming. An example in which this was used will be described.

[0018] In each of the above figures, the electroforming matrix 10 according to this embodiment is a conductive metal plate. A base portion 11, a sheet-like adhesive layer 12 disposed on the base portion 11, and A sheet-like conductive layer 1 having a multi-layer laminate structure is attached to a base portion 11 via an adhesive layer 12. The configuration includes:

[0019] The base portion 11 is made of a metal such as stainless steel (e.g., SUS430), brass, or steel. The thickness of the base portion is preferably about 1 mm. The base portion 11 may also be made of 42 alloy (42% nickel-iron alloy) or Invar (3 It can also be made of materials with low thermal expansion coefficients such as SUS430, 6% nickel-iron alloy, etc. The base portion 11 is made of an insulating substrate such as a glass plate or a resin plate, and a conductive material such as chromium or titanium is applied to the surface of the insulating substrate. It is also acceptable to use a metal film made of an electrically conductive metal.

[0020] The adhesive layer 12 has a two-layer structure consisting of a first resist 12a and a second resist 12b. Thus, the base portion 11 and the conductive layer 13 are bonded together to form an integral unit. The first resist 12a is a frame-shaped portion 12c of a predetermined range from the outer periphery, for example, The frame-shaped portion within the 20 mm width range is in an uncured state with adhesive properties, and the other intermediate portion 12d The base portion 11 is in a semi-cured state in which the adhesiveness and the volume change over time are smaller than those in the uncured state. The configuration is such that the sensor is disposed in contact with the sensor.

[0021] The second resist 12b is a frame-shaped resist having a predetermined area from the outer periphery, similar to the first resist 12a. The portion 12e is in an uncured state having adhesiveness, and the other intermediate portion 12f is in a state where the volume of the adhesive changes with time. The adhesive layer 14 is disposed in an uncured state in contact with the conductive layer 13.

[0022] Specifically, the first resist 12a and the second resist 12b are negative photosensitive resists. The liquid film resist is placed on the part to be bonded, and the frame-shaped part within a specified range from the outer edge is photoetched. The intermediate portion is exposed or partially exposed while covered with the masks 71 and 72. .

[0023] Dry film resist is adhesive when unexposed and hardens when exposed to light. It has the property of being non-sticky and transitioning to a stable state in which the volume does not change over time. Dry film resists limit the light transmittance through the photomask during exposure and If you do a half-exposure by shortening the time to reduce the amount of exposure, the curing will progress to a partially cured state. In this semi-cured state, the degree of change in viscosity and volume over time is greater than in the uncured state. As the adhesiveness decreases, the adhesive strength of the adhesive layer also decreases.

[0024] Dry film resist is a process in which a resist liquid is applied to the surface of a carrier film and then dried. A cover film is placed on the resist film. This dry film resist is supplied in a state where it is completely covered. After the resist film is removed, the resist film is placed in contact with the surface of the target area. After exposing the required areas through the carrier film to light to produce hardened areas, the carrier film is The film is also peeled off and removed.

[0025] The adhesive layer 12 has a two-layer structure consisting of a first resist 12a and a second resist 12b. Each resist is a photosensitive dry film resist, but it is in sheet form and has adhesive properties. Anything other than a dry film resist may be used as long as it has the above properties. The present invention provides a method for adjusting the state of a cured or semi-cured product from an uncured state to a cured state. This is preferable in terms of ease of handling.

[0026] The conductive layer 13 is made of thin sheets 13a, 13b, 13c made of a metal suitable for electroforming, such as nickel. It is made by stacking three pieces of 3c together. The thickness of each sheet 13a, 13b, 13c constituting the conductive layer 13 increases as it moves away from the adhesive layer 12. Therefore, the distance is set to be small, for example, 60 μm, 40 μm, and 20 μm from the side closer to the adhesive layer. It is said to be μm.

[0027] These sheets 13a, 13b, and 13c are each used for removing the matrix after the mask is completed. The boundary surface of the sheet is treated with a specific surface treatment to promote separation so that it can be peeled off from the mask side. do.

[0028] Although the conductive layer 13 has a laminated structure made up of three sheets, the present invention is not limited to this. It is also possible to use a multi-layer structure other than three sheets, such as two sheets or four or more sheets. Alternatively, the conductive layer may be in the form of a single sheet rather than a laminated structure.

[0029] The deposition mask 1 formed using the matrix 10 of this embodiment has a large number of deposition through-holes 8 formed at predetermined intervals. A plurality of mask bodies 2 are provided in a turn, and a frame body 3 is arranged around the mask body 2. This is a configuration that includes:

[0030] The mask body 2 is made of nickel, nickel alloys such as nickel-cobalt, or other electrodeposited metals. The metal is electroformed into a sheet shape and has numerous independent deposition passages through which the deposition material can pass. The holes 8 are arranged in a predetermined pattern.

[0031] The mask body 2 has an inner pattern forming area 2a in which a number of deposition through holes 8 are provided, and a plating and an outer peripheral edge 2b integrally joined to the frame 3 via a metal layer 7 formed by welding. In the pattern formation region 2a, a large number of vapor deposition through holes 8 are provided in the front and rear directions for forming a light emitting layer. A plurality of through-hole groups arranged linearly in the left-right direction are defined as rows, and a plurality of rows are arranged in parallel in the left-right direction. A matrix-shaped deposition pattern 9 is formed.

[0032] The frame 3 is a plate-like body having a thickness greater than that of the mask body 2 and having a rectangular frame shape. It is arranged around the outside of the mask body 2 to reinforce the main body 2 and is connected to the mask body 2. In detail, the frame body 3 is formed in a lattice shape as a whole, and has a plurality of The mask body 2 is positioned in each of the partitioned opening regions, and is aligned with the frame body 3 via the metal layer 7. It is a configuration that is embodied.

[0033] The frame 3 is made of a material with a low thermal expansion coefficient, for example, Invar, which is a nickel-iron alloy. It is made of materials such as Super Invar, which is a nickel-iron-cobalt alloy. The frame 3 has a metal layer 7 formed by plating, which is a metal layer that is formed on the mask body 2. The outer peripheral edge 2b of the hole forming region 2a is connected and integrated with the outer peripheral edge 2b so that they do not separate from each other.

[0034] When Invar or Super Invar is used as the material for the frame 3, its thermal expansion coefficient Since the thickness is extremely small, the dimensional change of the mask body 2 caused by the heat effect in the deposition process can be effectively prevented. That is, the mask body 2 is made of a material having a thermal expansion coefficient similar to that of the deposition substrate, such as nickel. Even if the thermal expansion coefficient is larger than that of the general glass plate (not shown), Due to the difference in thermal expansion coefficient due to high temperatures, when deposition mask 1 is aligned with the deposition substrate at room temperature, However, a deviation occurs between the position of the through hole relative to the substrate and the deposition position of the deposition material during actual deposition. The frame 3 that holds the mask body 2 has a small thermal expansion coefficient, The mask body 2 is kept from changing in size and shape due to expansion during use. The alignment accuracy in the deposition process can be maintained at a good level even when the temperature is increased during deposition.

[0035] The material of the frame 3 is a material having a low thermal expansion coefficient similar to that of the glass substrate on which the deposition is to be performed, for example. Glass and ceramics can also be used. In this case, at least one of these materials In either case, the surface is made conductive.

[0036] The deposition mask 1 is provided on the surface of the matrix 10 in a manner corresponding to a non-positioned portion of the primary electrodeposition layer 15. After the next pattern resist 14 is provided, a primary electrodeposition layer is formed on the matrix 10 by electroforming a metal. A secondary pattern 15 is formed on the primary electrodeposition layer 15, which covers the portion of the primary electrodeposition layer 15 corresponding to the pattern forming region 2a. After the photoresist 16 is formed and the frame 3 is placed so as to surround the primary electrodeposition layer 15, Then, a metal layer 7 is formed by plating so as to cover the surface of the frame 3 and the surface of the outer periphery 2b of the primary electrodeposition layer 15. The primary electrodeposition layer 15 and the frame 3 are integrally connected via the metal layer 7 so as not to be separated. In the bonded state, the primary electrodeposition layer 15, the frame 3, and the metal layer 7 are separated from the matrix 10. The material is manufactured by

[0037] After the metal layer 7 is formed on the matrix 10 by plating (see FIG. 12(C)), the matrix 10 is The matrix 10 is separated and removed from the deposition mask 12 by applying force (see FIG. 13 and FIG. 14). Specifically, each layer of the matrix 10 is physically peeled off from the side. That is, the base portion 11 and the conductive layer 13 are separated from the mask side in that order. Each of the sheets 13a, 13b, and 13c constituting the sheet 13 is separated one by one from the side farthest from the mask side. This will be the case.

[0038] The primary electrodeposition layer 15 is made of nickel or a nickel alloy such as nickel-cobalt, which is suitable for electroforming. The pattern is formed by electroforming in the area where the primary pattern resist 14 is not present on the mold 10. In the deposition mask 1, the primary electrodeposition layer 15 is a layer for depositing a light-emitting layer or the like on a deposition substrate. A mask body 2 covers the surface of the substrate to be vapor-deposited, except for the vapor deposition through holes 8 corresponding to the target areas. It will be formed as a.

[0039] The primary pattern resist 14 is resistant to the electrolyte used in electroforming of the primary electrodeposition layer 15. A primary electrodeposition layer 15 made of a soluble insulating material and set in advance on the matrix 10. and is removed after the formation of the primary electrodeposition layer 15. (See Figures 9 and 10).

[0040] The primary pattern resist 14 is disposed on the matrix 10 prior to the formation of the primary electrodeposition layer 15. A photosensitive resist, for example a negative type photosensitive dry film resist, is applied to the matrix 1. 0 to a predetermined thickness, for example, about 20 μm, and the deposition mask 1 is The photomask has a predetermined pattern corresponding to the position of the main body 2, i.e., the position of the primary electrodeposition layer 15. With the screen 41 placed on the substrate, the resist is hardened by exposure to ultraviolet light, and the non-irradiated areas are removed. After undergoing processes such as development, the pattern is formed in a shape corresponding to the non-positioned portion of the primary electrodeposition layer 15.

[0041] The secondary pattern resist 16 is resistant to dissolution by the electrolytic solution used in plating the metal layer 7. The insulating material has a predetermined non-placement portion of the metal layer 7. The metal layer 7 is formed and the matrix 10 is separated, and is removed after the metal layer 7 is formed (FIG. 11, See Figures 12 and 14).

[0042] The secondary pattern resist 16 is a photosensitive resist, for example, a negative type photosensitive dry A film resist is applied onto the matrix 10 and the primary electrodeposition layer 15 already disposed thereon. Then, a photomask 42 having a predetermined pattern corresponding to the metal layer 7 and the frame 3 of the deposition mask 1 is formed. The series of steps of exposing the substrate to ultraviolet light with the substrate placed on the substrate is repeated once or multiple times. After the resist is formed to the required thickness, the photosensitive material in the non-irradiated areas is removed. After image processing, etc., the non-placement portion of the metal layer 7 (the pattern formation region 2a of the mask body 2) is The shape is formed according to the shape of the mold.

[0043] The secondary pattern resist 16 (resist layer 18) and the second layer forming the adhesive layer 12 are The first resist 12a (another resist 64) and the second resist 12b (one resist 63 ) and the primary pattern resist 14 (resist layer 17) are all made of the same resist. This is more preferable because it allows specification conditions (such as dimensional variations due to exposure) to be the same.

[0044] The metal layer 7 is formed by plating, and is typically made of nickel or nickel-cobalt. The secondary pattern is formed on the matrix 10, the primary electrodeposition layer 15 already arranged, and the frame 3. The conductive layer 14 is formed by plating on the exposed portion where the thermal resist 16 is not provided.

[0045] The metal layer 7 bonds the outer periphery 2b of the pattern forming region 2a of the mask body 2 to the frame body 3. The metal layer 7 is formed on the upper surface of the mask body 2 which is adjacent to the outer periphery 2b of the pattern forming region. In detail, the metal layer 7 is formed on the outer periphery 2b of the pattern forming region 2a by plating. the upper surface of the mask body 2, the upper surface of the frame 3 and the side surface of the pattern forming region 2a side, and the mask body 2 and the frame 3 This forms the gap between the outer periphery 2b of the pattern forming region 2a and the opening of the frame 3. It is connected to the periphery so that it does not come apart.

[0046] Next, a manufacturing process of the matrix according to this embodiment and a manufacturing process of the deposition mask using the matrix will be described. He explains. First, the manufacturing process of the matrix 10 will be described. A flat metal substrate suitable for electroforming (e.g., stainless steel such as SUS304) On the surface of 60, a resist 61, for example an unexposed negative dry film, is applied to a required thickness. The resist is then disposed so that the photomask 70 is disposed outside the predetermined peripheral area of ​​the resist. Then, the resist 61 is covered with a photomask 70 by an exposure process. The outer peripheral portion that is not hardened is hardened, and the portion other than the hardened outer peripheral portion is removed to form an outer frame resist 62 for electroforming. (See Figure 4.)

[0047] Then, sheets are sequentially formed by electroforming on the inner portion surrounded by the outer frame resist 62 on the substrate 60. This results in a conductive layer 13 consisting of three sheets 13a, 13b, and 13c (see FIG. 5). Each sheet 13a, 13b, 13c of the conductive layer 13 becomes thicker with each layer formed. The thickness of each sheet 13a, 13b, and 13c is changed so that the ... Each time a layer is formed, a surface treatment is applied to facilitate peeling when removing the matrix.

[0048] An adhesive layer 12 is formed on the obtained conductive layer 13. Specifically, an unexposed A first resist 63, which is a negative dry film resist, is placed on the substrate 61. A frame-shaped portion of a predetermined range is covered with a photomask 71. Then, one resist 6 The intermediate portion not covered by the photomask 71 of FIG. 3 is exposed to light to harden the intermediate portion. In this way, the outer peripheral frame-shaped portion 12e is exposed from one resist 63. Then, the second resist 12b is obtained in which the middle portion 12f surrounded by the frame portion 12e is hardened. (See Figure 6.)

[0049] On the second resist 12b whose intermediate portion 12f is hardened, a film having the same thickness as the first resist 63 is formed. Another resist 64, which is an unexposed negative dry film resist, is placed on the outer periphery of the resist. A frame-shaped portion of a predetermined range from the edge is covered with a photomask 72. The intermediate portion of the first resist 63 is not covered by the photomask 72 of the second resist 64. The exposure amount is reduced compared to the exposure for the first part, and the intermediate part is left in a semi-cured state. Thus, the outer peripheral frame-shaped portion 12c is left unexposed from the other resist 64, and the frame-shaped The first resist 12a is obtained in which the intermediate portion 12d surrounded by the portion 12c is in a semi-cured state. (See Figure 7.)

[0050] The half-exposure for the other resist 64 is less than half the exposure amount (integrated amount of light) during normal exposure. For example, the exposure amount is 200 mJ / cm 2 In contrast, half exposure is 1 / 20 the exposure amount of 10 mJ / cm 2 It is made to be as follows.

[0051] In addition, when forming the adhesive layer 12, a cap that covers the middle part of the first resist 63 is The rear film or other cover film is left to cover the middle part of the resist 64. A film is interposed between the first resist 12a and the second resist 12b. The film can be used to prevent the middle parts of the resist from adhering to each other, This makes it easier to separate the deposition layer 12 starting from the resist gap.

[0052] The laminated conductive layer 13 and adhesive layer 12 are then placed on a base portion 11, which is a metal plate, and the adhesive layer 1 is then placed on the base portion 11. The transfer step (see FIG. 8) is performed by attaching the substrate 60 to the substrate 60 using the adhesive strength of 2. After this process, the matrix 10 is completed.

[0053] In this matrix 10, an adhesive layer 12 consisting of a first resist 12a and a second resist 12b is formed. However, the intermediate portions 12d and 12e are surrounded by frame-like portions 12c and 12e in a predetermined range from the outer periphery of the frame. In the case of f, the volume change with time is made smaller than that of the unexposed frame-shaped portions 12c and 12e. Since the adhesive layer 12 is in a stable state, the adhesive layer 12 can be prevented from expanding over a long period of time during the electroforming process using the mold 10. It is possible to prevent the influence of time-dependent changes from reaching the primary electrodeposition layer 15 via the conductive layer 13. The adhesive layer 12 connects the base portion 11 and the conductive layer 13 at its intermediate portions 12d and 12f. By reducing the adhesive force, the base part 11 can be easily attached to the mold in the final process of separating the mold. This makes it easier to separate the conductive layer 13 from the conductive layer 13 .

[0054] Next, a manufacturing process of the deposition mask will be described. First, the deposition holes 8 of the mask body 2, which are set in advance on the matrix 10, i.e., the primary A resist layer 17 is provided on the matrix 10 so as to correspond to the non-positioned portion of the electrodeposition layer 15 (see FIG. 9). Specifically, on the surface side of the matrix 10, i.e., on the conductive layer 13, for example, a negative type The photosensitive dry film resist is applied to a predetermined thickness ( For example, one or several sheets are laminated to a thickness of about 20 μm, and the resist layer 17 is formed by thermocompression bonding. (See FIG. 9(A)).

[0055] The surface of the resist layer 17 is provided with a light transmitting hole 41a corresponding to the vapor deposition through hole 8. A photomask (e.g., a glass mask) having a predetermined pattern corresponding to the position where the primary electrodeposition layer 15 is to be disposed is used. After the mask 41 is attached, the mask 41 is exposed to ultraviolet light using an exposure device (ultraviolet light exposure device). Execute (see Figures 9(B) and (C)).

[0056] In the exposure process for this resist layer 17, before exposure with an exposure device, The matrix 10 on which the photoresist layer 17 is formed is exposed to light using, for example, a hot plate or a preheating furnace. A predetermined preheat temperature, for example, a temperature that can be reached in the exposure apparatus during the exposure process. Preheat to 27.0℃±0.3℃.

[0057] In addition, the photomask 41 to be placed on the surface of the resist layer 17 is also dummy before exposure. - Place the mold (mold + resist layer) on the exposure device and then operate the exposure device. By a dummy exposure in which the working conditions are the same as those of the exposure of the matrix 10, the preheating temperature, e.g. If necessary, preheat to 27.0°C ± 0.3°C.

[0058] In addition, the stage on which the matrix 10 is mounted in the exposure tool is also set before the official exposure. Do not place the object to be exposed such as a matrix inside the chamber, or place a dummy matrix on the stage before exposure. The same preheating as for the matrix 10 was performed by a dummy exposure in which the apparatus was in the same operating condition as the actual exposure. Preheat to a temperature of, for example, 27.0°C ± 0.3°C.

[0059] In this way, the matrix 10, the photomask 41, and the inside (stage) of the exposure device are preliminarily kept at the same temperature. After heating, a photomask 41 is placed on the surface of the resist layer 17 on the matrix 10, and these are exposed. The specimen is then placed on the stage of the optical device and the exposure is formally performed.

[0060] In this exposure, the matrix 10, the photomask 41, and the inside of the exposure device (stage) are exposed. The reason for preheating the master mold 10 and the laser beam to a temperature that can be reached during the laser beam work is as follows. The thermal expansion coefficients of the resist layer 17 and the photomask 41 are different from each other. These are exposed at a temperature lower than the internal temperature when the exposure is actually performed in the exposure device, such as room temperature. When the mold is placed in the exposure device and exposed to light, the heat generated in the exposure device due to ultraviolet light irradiation etc. As the mold 10 and the resist layer 17 expand due to heating, the relative positions of the mold 10, the resist layer 17, and the photomask 41 This will result in a deviation in the overall positional relationship.

[0061] Due to such a shift, the position of the primary pattern resist 14 obtained after exposure with respect to the matrix 10 The accuracy of the placement and the accuracy of the shape of the primary pattern resist 14 are reduced. If the positional accuracy of the resist 14 is reduced or the shape is defective, the primary electrodeposition layer 15 (mask This affects the process of forming the mask body 2, making it impossible to form the mask body 2 with the precision intended by the design. There is a risk.

[0062] In contrast, the matrix 10 (including the resist layer 17), the photomask 41, and the exposure device ( The stage is preheated to a temperature that can be reached during exposure work, and then exposed to light by the exposure device. By performing exposure, new thermal expansion of the matrix 10 etc. due to a temperature rise in the exposure device is prevented. In addition, the temperature inside the exposure device can be kept stable, and the temperature of the matrix 10 in the device can be kept constant. The exposure proceeds unaffected by the change.

[0063] As a result, the position and shape of the primary pattern resist 14 on the mold 10 after exposure can be determined. The accuracy of the primary pattern resist 14 is improved, and the primary electrodeposition layer 15 is formed based on the accuracy of the primary pattern resist 14. The mask body 2 can also be formed stably and with high precision, and the mask body 2 can reproduce the deposition layer with high precision. The lower the preheating temperature, the more the thermal expansion can be suppressed. , and preferably at standard temperature (23°C) or even lower (e.g. 0°C), Since heat is generated during exposure in the exposure device, there is a limit to how low the preheating temperature can be. When the main purpose is to avoid the effect of thermal expansion caused by heat generated during exposure, It is preferable to set the maximum temperature that can be reached inside the exposure device when exposed to light as the preheat temperature.

[0064] In addition, when considering the thermal expansion in each process after exposure, the exposure equipment (exposure temperature), plating The maximum temperature in the plating bath (plating temperature) and the deposition equipment (deposition temperature) is preset. Preferably at thermal temperature.

[0065] After exposure, the resist in the masked unexposed (non-irradiated) parts on the matrix 10 is removed. Then, the respective processes such as development and drying are carried out. In this way, the non-deposition portion of the primary electrodeposition layer 15 is A primary pattern resist 14 is obtained on the matrix 10 (see FIG. 10(A)).

[0066] Such a primary pattern resist 14 is a lithography process using a photoresist or the like. The forming method may be the feed method or any other method, but is not limited to the above. It is not.

[0067] The matrix 10 having this primary pattern resist 14 is placed in an electroforming tank prepared under predetermined conditions. The primary pattern resist 14 of the matrix 10 is formed within the range of the thickness of the primary pattern resist 14. For example, a nickel alloy or other metal is electroformed on the surface (exposed area) that is not covered with A primary electrodeposition layer 15 having a thickness of 12 μm, which will become the mask body 2, is formed (see FIG. 10(B)).

[0068] After this, the primary pattern resist 14 is dissolved and removed to form a predetermined deposition pattern 9 A primary electrodeposition layer 15 is obtained, which becomes the mask body 2 and has a large number of independent deposition through holes 8. (See FIG. 10(C)).

[0069] After the primary electrodeposition layer 15 is obtained, the entire surface of the matrix 10 including the portion where the primary electrodeposition layer 15 is to be formed is Specifically, a resist layer 18 is provided on the front surface of the matrix 10. The photosensitive dry film resist is cut to a preset thickness. Then, several sheets are laminated and subjected to thermocompression bonding to form a resist layer 18 (see FIG. 11(A)).

[0070] Then, the pattern of the mask body 2 is formed on the surface of the resist layer 18 as shown in FIG. 11(B). After a photomask 42 having light transmitting holes 42a corresponding to the semiconductor device forming region 2a is attached to the semiconductor device, ultraviolet light is applied to the semiconductor device. The pattern is formed by irradiating the area with radiation (see Figs. 11B and 11C). The portion corresponding to 2a is a resist layer 18a that has been hardened by exposure, and the other portion is unexposed. This becomes the resist layer 18b. Thereafter, a process is carried out to dissolve and remove the unexposed resist layer 18b that is exposed on the surface. A secondary pattern resist 16 is formed to cover the pattern forming region 2a (see FIG. 12(A)). .

[0071] After the secondary pattern resist 16 is formed in this manner, the frame body is formed through a frame body forming process. The adhesive layer 19 is placed on the underside of the primary electrodeposition layer 15. The substrate is then aligned and placed at the designated location (see FIG. 12(B)).

[0072] In this state, the frame 3 does not easily move on the primary electrodeposition layer 15 due to the adhesiveness of the adhesive layer 19. It can be temporarily fixed in place. If necessary, a load is applied from above the temporarily fixed frame body 3 to press the frame body 3. It is also possible to carry out the above steps to make it even more difficult for the frame 3 to separate from the primary electrodeposition layer 15.

[0073] After this, the secondary pattern resist 16 is not covered and the outer periphery 2b of the pattern forming region 2a is The upper surface of the primary electrodeposition layer 15 exposed on the surface, the primary electrodeposition layer 15a on the lower side of the frame 3 and its lateral sides Each exposed surface of the matrix 10 and the surface of the frame 3 are plated with gold by electroplating. The metal layer 7 is formed (see FIG. 12(C)). The metal layer 7 is used to bond the primary electrodeposition layer 15 and the frame 3 together. They can be connected together so that they do not come apart.

[0074] In this case, the metal layer 7 is a primary layer exposed on the surface related to the outer periphery 2b of the pattern formation region 2a. On the upper surface of the electrodeposition layer 15 and on the surface of the matrix 10 exposed between the primary electrodeposition layer 15 and the frame 3, The thickness of the metal layer 7 on the surface of the frame 3 is formed thinner than the thickness at the base. The difference in thickness is due to the metal layer 7 being laminated in sequence from the surface of the matrix 10 or the primary electrodeposition layer 15. Only when the frame 3 exceeds the height dimension of the layer 19 and reaches the frame 3 does the frame 3 reach the matrix 10 and the primary electrodeposition layer 15 This is because the metal layer 7 starts to be formed on the surface of the frame 3 .

[0075] After the formation of the metal layer 7 is completed, the final step is to remove the integral primary electrodeposition layer 15, the frame 3 and the metal The matrix 10 is separated from the metal layer 7. This separation is carried out starting from the base part 11 of the matrix. Then, the base portion 11 is peeled off from the conductive layer 13. In this case, the first resist of the adhesive layer 12 is peeled off. The base portion 11 is peeled off from between the adhesive layer 12a and the second resist 12b. The middle portion 12c of the first resist 12a is in a semi-cured state, and the middle portion of the second resist 12b is in a semi-cured state. Since 12d is in a hardened state, this adhesive layer can be peeled off and separated without difficulty ( See Figure 13(A). When peeling off the base portion 11, the remaining portion including the primary electrodeposition layer 15 and the conductive layer 13 must be sufficiently removed. By having a sufficient thickness, the primary electrodeposition layer 15 is not adversely affected, such as by deformation.

[0076] After the base portion 11 (including the first resist 12a portion of the adhesive layer 12) is separated, the conductive layer The sheets 13 are separated one by one from the side away from the primary electrodeposition layer 15 (FIG. 13). (B, see Fig. 14(A)(B). Each layer of the sheet is surface-treated, When a force is applied to peel them off, they can be easily separated. a, 13b, and 13c become thinner as they approach the primary electrodeposition layer 15, etc. The load on the electrodeposition layer 15 is small, and the primary electrodeposition layer 15 can be separated without being deformed. Cut.

[0077] When the sheets 13a, 13b, and 13c constituting the conductive layer 13 are peeled off, the primary The remaining sheet of the conductive layer 13 is in contact with the adhesive layer 15 to form a reinforced state. The electrodeposition layer 15 is not adversely affected, such as being deformed.

[0078] In addition, the sheets 13a, 13b, and 13c constituting the conductive layer 13 approach the primary electrodeposition layer 15, etc. As the thickness of the conductive layer 13 increases, the thickness of the conductive layer 13 decreases. When separating the primary electrodeposition layer 15 from the other layers, the force applied to the primary electrodeposition layer 15 is kept to a minimum. Layer 15 can be separated without deformation.

[0079] All the sheets 13a, 13b, and 13c constituting the conductive layer 13 are peeled off, and the separation of the matrix 10 is completed. After this, the primary electrodeposition layer 15a present on the underside of the frame 3 is removed together with the adhesive layer 19, and then By removing the secondary pattern resist 16, the manufacturing of the deposition mask 1 is completed. If the adhesive layer 19 remains on the underside of the frame 3, when removing the secondary pattern resist 16, The secondary pattern resist 16 may be removed before the mother die 10 is separated. .

[0080] In this way, in the electroforming master according to the present embodiment, the adhesive layer 12 is The central portion other than the frame-shaped portion is in a state where the volume is unlikely to change over time, and the entire adhesive layer 12 is By stabilizing the structure as a base, the adhesive layer reduces the volume change over time. The conductive layer 13 and the base portion 11 can be stably fixed together, and the conductive layer 13 can be prevented from being damaged by the change in volume of the adhesive layer 12. 3 and the displacement of the primary electrodeposition layer 15 formed on the conductive layer 13 are suppressed. This makes it possible to prevent a decrease in accuracy of the mask body 2 formed using 10.

[0081] In addition, a sufficient adhesive strength is ensured in a frame-shaped portion within a predetermined range from the outer periphery of the adhesive layer 12, while By suppressing the adhesive strength of the middle portion of the adhesive layer 12, the matrix 10 can be formed in the electroforming process. The base portion 11 and the conductive layer 13 are securely integrated, and the adhesive layer is fixed to the substrate after electroforming is completed. The base portion 11 and the conductive layer 13 can be separated from each other with a smaller force starting from the position where the electroforming is performed. Then, the base portion 11 and the conductive layer 13 are sequentially separated from the mask side, and the matrix 10 is separated from the mask. The separation and removal can be easily and efficiently performed, and the force applied to the mask side during separation of the master mold is reduced. As a result, adverse effects such as deformation of the mask body 2 can be suppressed.

[0082] The electroforming mother mold according to the embodiment is a deposition mask for an organic EL element. The body 2 and the frame 3 are integrated with a metal layer 7 to form a deposition mask 1. However, the present invention is not limited to this structure, and metal masks of other structures, such as frames, may be used. There are masks that are just the mask body without a frame, and masks that have a mask body and a frame but are glued together. A mask with an integrated structure, which also has a mask body and a frame, but these are gauze (mesh) It can also be used to form a mask or the like having a structure in which the mask is bonded together via a vapor deposition method. A mother mold for forming masks other than masks, such as printing masks and masks for mounting solder balls. It's okay if there is.

[0083] (Second embodiment of the present invention) In the manufacturing method of the electroforming mold according to the first embodiment, the conductive layer 1 is formed in the adhesive layer forming step. The central portion of one resist 63 placed on the substrate 3 is exposed to light, and the resist 63 is The other resist 64 placed on the substrate is partially exposed to light to make the intermediate portion 12f sticky. The second resist 12b is in a hardened state and does not change in volume over time, and the intermediate portion 12d is The first resist 1 is in a semi-cured state, which has smaller viscosity and volume change over time than the unexposed portion. 2a, and the first resist 12a and the second resist 12b are bonded to an adhesive layer 12 However, the present embodiment is not limited to this, and as a second embodiment, as shown in FIG. In the adhesive layer forming step, the middle part of one resist 63 and the middle part of the other resist 64 are The first resist 12a and the second resist 12b forming the adhesive layer 12 are also exposed to light. In both cases, the intermediate portions 12d and 12f are in a cured state that is not tacky and does not change in volume over time. It is also possible to adopt a configuration in which

[0084] In this case, as in the above embodiment, the adhesive layer 12 is formed in a predetermined area from the outer periphery of the adhesive layer 12. The central portion of the outer shell is made in a state where the volume is unlikely to change over time, and the adhesive layer 12 is bonded to the base portion 11. In the state of the matrix 10 in which the conductive layer 13 is bonded and integrated, the conductive layer 1 3 and the positional deviation of the primary electrodeposition layer 15 (mask body 2) formed on the conductive layer 13. This suppresses the formation of a high-precision mask using the matrix 10. The frame-shaped area within a predetermined range is left unexposed to maintain adhesion and ensure sufficient adhesive strength. By reducing the adhesive strength of the middle part, the matrix 10 is formed in the electroforming process. The base portion 11 and the conductive layer 13 are securely integrated by the adhesive layer 12, and after electroforming is completed, The base portion 11 and the conductive layer 13 can be separated with a small force at the adhesive layer position, and the matrix 10 can be removed from the mask. Therefore, separation and removal of the particles can be easily and efficiently performed.

[0085] In the adhesive layer forming step, the intermediate portions of the resists 63 and 64 are exposed to light. The present invention is not limited to a method in which the exposure is performed so that the cured state is completely cured, but may be performed in other ways. As shown in FIG. 16, in the adhesive layer forming step, the middle portion of one resist 63 and the other resist 6 The first and second portions of the adhesive layer 12 are partially exposed to a small amount of light. In both the first resist 12a and the second resist 12b, the intermediate portions 12d and 12f are The semi-transparent portion 12c and the semi-transparent portion 12e are less viscous and have a smaller change in volume over time than the unexposed outer frame-shaped portions 12c and 12e. It is also possible to configure the device to obtain a cured state.

[0086] (Third embodiment of the present invention) In the manufacturing method of the electroforming mold according to the first embodiment, in the adhesive layer forming step, After the first resist 63 is exposed to light, another resist 64 is placed on the first resist 63. By half-exposing the middle part of 64, the middle part 12d becomes more viscous than the unexposed frame-shaped part 12c. A configuration for obtaining a first resist 12a in a semi-cured state with small adhesion and small change in volume over time. However, the present invention is not limited to this. As a third embodiment, as shown in FIG. On the resist 63 after the exposure, an unexposed negative dry film resist is formed. After the other resist 64 is placed, the other resist 64 is not exposed to light. It is also possible to obtain the first resist 12a in an unexposed state.

[0087] In this case, the second resist 12b of the adhesive layer 12 has an intermediate portion 12f that is adhesive. Since the adhesive is in a cured state without any change in volume over time, the adhesive is in a cured state without any change in volume over time, as in the previous embodiment. As a whole layer, the central part is in a state where the volume is unlikely to change over time, and the adhesive layer In the state of the mother mold 10 in which the base portion 11 and the conductive layer 13 are bonded together at 12, the adhesive layer 12 The displacement of the conductive layer 13 due to the change in volume and the primary electrodeposition layer 15 (mass) formed on the conductive layer 13 In addition, the base portion 11 in the middle portion of the adhesive layer 12 is prevented from being displaced. The adhesive strength that integrates the conductive layer 13 with the electroforming portion is smaller than that of the outer frame-shaped portion. After completion of the process, the base portion 11 and the conductive layer 13 are easily and quickly bonded together starting from the adhesive layer 12. It can encourage separation.

[0088] After exposure, the intermediate portion 12f is in a cured state in which it has no tackiness and does not change in volume over time. The second resist 12b is in a state of being exposed to light, and the first resist 12a is in a state of being entirely unexposed. The combination of the adhesive layer 12 is as shown in FIG. 17, similar to the first embodiment. In addition to making the plates 12a and 12b thin (for example, a thickness of a few tens of μm) and having the same thickness, As shown in FIG. 1, the second resist 12b, the middle portion 12f of which is in a hardened state, is It may be arranged so that the thickness is larger than that of 2a (for example, several tens of μm), or as shown in FIG. As shown in FIG. 1, the first resist 12a and the second resist 12b are both made thicker than in the case of a thin resist. It is also possible to combine them in a large number (for example, several tens of μm thick). Regarding the sections 12a and 12b, the thinner the section, the greater the change in volume over time. Even in situations where this occurs, the amount of change can be kept relatively small, and the impact on the conductive layer, etc. is also suppressed. This is more preferable.

[0089] (Fourth embodiment of the present invention) In the manufacturing method of the electroforming mold according to the first embodiment, the conductive layer 1 is formed in the adhesive layer forming step. After exposing the central portion of one resist 63 placed on the substrate 3, The intermediate portion 12f of the other resist 64 placed on the substrate 12 is partially exposed to light. The second resist 12b is in a cured state, and the intermediate portion 12d is in a semi-cured state due to partial exposure. In the fourth embodiment, the first resist 12a is obtained by the above-mentioned method. As an embodiment, as shown in FIG. 20 and FIG. 21, a substrate is placed on the conductive layer 13 in the adhesive layer forming step. The first resist 63 is not exposed to light and is left in an unexposed state. Another resist 64 placed on the resist 63 is exposed or partially exposed in the middle portion. The first resist 12 is in a cured or semi-cured state after the exposure process. Alternatively, the second resist 12a may be obtained, and the second resist 12b may be obtained in a state where the whole of the resist is left unexposed. .

[0090] In this case, the first resist 12a of the adhesive layer 12 has an intermediate portion 12d that is adhesive. Since the composition is in a cured or semi-cured state in which the change in viscosity and volume over time is small, As with the morphology, the adhesive layer as a whole is in a state where the volume of the central part is unlikely to change over time. In the state of the mother mold 10 in which the base portion 11 and the conductive layer 13 are bonded and integrated with each other by the adhesive layer 12, The displacement of the conductive layer 13 due to the volume change of the adhesive layer 12 and the primary electrode formed on the conductive layer 13 The positional deviation of the adhesive layer 15 (mask body 2) can be suppressed. The adhesive strength that integrates the base portion 11 and the conductive layer 13 is smaller than that of the outer frame portion. After the electroforming is completed, the capacity of the base portion 11 and the conductive layer 13 is determined based on the adhesive layer 12. This can promote easy and rapid separation.

[0091] In the manufacture of the electroforming master according to each of the first to fourth embodiments, the adhesive layer type In the forming process, the first resist 63 and the second resist 64 are formed within a predetermined range from the outer periphery of the resist. The second resist 12b and the first resist 11 are exposed to light without exposing the frame-shaped portion of the photoresist. Each frame-shaped portion of 2a is configured to be maintained in an uncured state having adhesive properties. However, the present invention is not limited to this. For example, the frame-shaped portion of one resist 63 may be exposed or partially exposed to light to form a frame-shaped portion 1 2e to obtain a second resist 12b in a hardened or semi-hardened state, or The frame-shaped portion of the resist 64 is exposed to light or partially exposed to light, so that the frame-shaped portion 12c is in a cured or partially cured state. It is also possible to obtain the first resist 12a in a state where the resist is in a non-transparent state.

[0092] In this case, one resist 63 is exposed or partially exposed to a frame-shaped portion. The middle part of 3 may be exposed or semi-exposed, or may not be exposed. The intermediate portion 12f of the resulting second resist 12b may be in a cured or semi-cured state. On the other hand, the frame-shaped portion of the other resist 64 is exposed to light. When this is done, the intermediate portion of the other resist 64 is half-exposed or not exposed. The resulting intermediate portion 12d of the first resist 12a is in a semi-cured or uncured state. In addition, when the frame-shaped portion of the other resist 64 is partially exposed, The other resist 64 may be exposed or partially exposed in the middle. It is also possible to avoid performing the above step, and the resulting intermediate portion 12d of the first resist 12a is It may be in a cured, semi-cured, or uncured state.

[0093] In addition, the frame-shaped portion 12c of the first resist 12a and the frame-shaped portion 12b of the second resist 12b are There is no particular need to match the properties of the first resist 12a and the second resist 2e. For example, the frame shape of the first resist 12a may be the same as that of the second resist 2e. When the portion 12c is in a cured state, the frame-shaped portion 12e of the second resist 12b is in a semi-cured state. The adhesive may be in a different state, such as in a cured or uncured state.

[0094] The electroforming matrix and the method for manufacturing the matrix according to the present invention will now be described. When forming a mask by electroforming, it is usually difficult to separate the mask from the mother mold due to the thickness of the mask. Since the thickness of the matrix is ​​large, the force applied for separation causes the matrix to act as a mask. When deforming in a direction away from the electrodeposition, excessive force is applied to the electrodeposition, causing a part of it to become permanently deformed. This could potentially deteriorate the accuracy.

[0095] For this reason, the master mold used in electroforming has a laminated structure, and each layer of the master mold is By separating the layers one by one from the farthest side of the electrodeposition layer, excessive force is applied to the electrodeposition layer, causing it to deform. In recent years, there have been proposals for preventing this.

[0096] In such a laminated structure, each layer of the mold is formed by forming a mask and then attaching the mask and the mold. The adhesive must be maintained until the parts are separated. If a general adhesive is used to bond each layer of such a mold, the thickness of the adhesive layer cannot be controlled uniformly. It is difficult to control the flatness of the primary electrodeposition layer (mask) formed on the matrix. This could adversely affect the accuracy of the mask. It has been proposed to use a dry film resist having a certain adhesive strength in such a case.

[0097] Dry film resist is a sheet with a uniform thickness. When used for adhesion, The flatness of the next electrodeposition layer can be ensured without any problems. However, the dry film layer is The resist is used unexposed, and the dry film resist is placed between each layer of the matrix. Since the resin is not in a stable cured state after exposure to light, it will retain the shape of the master mold as time passes. For example, volume changes such as shrinkage due to the outflow of volatile components may occur, and the mold may become There is a problem that the primary electrodeposition layer (mask) formed on the substrate may be adversely affected, such as being misaligned. The company had a problem.

[0098] Therefore, the electroforming master mold disclosed in the present invention is used for electroforming to manufacture a mask having a large number of through holes, and comprises a plate-shaped base portion having at least one flat surface, a sheet-shaped adhesive layer arranged on top of the flat surface of the base portion, and a sheet-shaped conductive layer having electrical conductivity, either in a single layer or in a multi-layered structure, and bonded to the base portion via the adhesive layer, and an intermediate portion of the adhesive layer, surrounded by a frame-shaped portion within a predetermined range from the outer periphery of the adhesive layer, has a smaller change in volume over time than the frame-shaped portion, and has a smaller adhesive force bonding the base portion and the conductive layer.

[0099] Thus, according to the disclosure of the present invention, by maintaining a state in which the volume of the adhesive layer is less likely to change over time in the central part other than the frame-shaped part within a predetermined range from the outer peripheral edge, while maintaining a state in which adhesive force is generated at least in the frame-shaped part, and stabilizing the structure of the adhesive layer as a whole, the base part and the conductive layer can be stably fixed together by an adhesive layer that has small volumetric changes over time, thereby suppressing displacement of the conductive layer due to volumetric changes in the adhesive layer and misalignment of the electrochemical layer formed on this conductive layer, and preventing a decrease in accuracy of the mask formed using the master mold.

[0100] Furthermore, by ensuring sufficient adhesive strength in a frame-shaped portion within a specified range from the outer peripheral edge of the adhesive layer, while suppressing the adhesive strength in the middle portion of the adhesive layer, it is possible to reliably maintain the integration of the base portion and conductive layer that form the master mold during the electroforming process, while allowing the base portion and conductive layer to be separated with less force at the adhesive layer position after electroforming is completed.After electroforming, the base portion and conductive layer can be separated sequentially from the mask side, making it easy and efficient to separate and remove the master mold from the mask, and by reducing the force applied to the mask side when separating the master mold, adverse effects such as deformation of the mask body can be suppressed.

[0101] Furthermore, the electroforming master mold disclosed in the present invention, as necessary, comprises a first resist arranged in contact with the base portion, the adhesive layer having a frame-shaped portion in an uncured state and adhesive properties over at least a predetermined range from the outer peripheral edge, and a second resist arranged in contact with the conductive layer, the frame-shaped portion in an uncured state and adhesive properties over at least a predetermined range from the outer peripheral edge, and an intermediate portion surrounded by the frame-shaped portion in at least one of the first resist and second resist is in a cured state that is not adhesive and does not change in volume over time.

[0102] Thus, according to the disclosure of the present invention, by setting the middle part of at least one of the two layers of resist forming the adhesive layer in a hardened state and bringing the middle part of the adhesive layer closer to a stable state in which the volume is unlikely to change over time, even if time has passed since the base part and the conductive layer are fixed and integrated by the adhesive layer, the volume change in the adhesive layer is suppressed, and the displacement of the conductive layer and the associated positional shift of the electrodeposition layer on the conductive layer are prevented, and a high-precision mask can be manufactured. Also, by setting the middle part of at least one of the two layers of resist forming the adhesive layer in a hardened state so that the adhesive force is not exerted, the separation of the base part and the conductive layer after the completion of electroforming can be performed with a smaller force starting from the adhesive layer, and the separation and removal of the mother mold from the mask can be smoothly carried out.

[0103] Furthermore, the electroforming master mold disclosed in the present invention, as necessary, comprises a first resist arranged in contact with the base portion, and a frame-shaped portion of at least a predetermined range from the outer periphery, which is in an uncured state and adhesive, and a second resist arranged in contact with the conductive layer, and a frame-shaped portion of at least a predetermined range from the outer periphery, which is in an uncured state and adhesive, and an intermediate portion surrounded by the frame-shaped portion in at least one of the first resist and second resist is in a semi-cured state with less adhesiveness and less change in volume over time than the frame-shaped portion.

[0104] Thus, according to the disclosure of the present invention, by making the middle part of at least one of the two resist layers forming the adhesive layer semi-cured and making the middle part of the adhesive layer less susceptible to volumetric changes over time, even if time has passed since the base part and the conductive layer are fixed and integrated by the adhesive layer, the volumetric changes in the adhesive layer are suppressed, and the displacement of the conductive layer and the associated positional shift of the electrodeposition layer on the conductive layer are prevented, and a high-precision mask can be manufactured. Also, by making the middle part of at least one of the two resist layers forming the adhesive layer semi-cured and making the adhesive force weak, the separation of the base part and the conductive layer after electroforming can be performed with a smaller force starting from the adhesive layer, and the separation and removal of the mother mold from the mask can be smoothly carried out.

[0105] Furthermore, in the electroforming master mold disclosed in the present invention, as necessary, the first resist in the adhesive layer has the frame-shaped portion in an uncured state and the middle portion surrounded by the frame-shaped portion in a semi-cured state, and the second resist in the adhesive layer has the frame-shaped portion in an uncured state and the middle portion surrounded by the frame-shaped portion in a cured state.

[0106] Thus, according to the disclosure of the present invention, the intermediate portion of the first resist of the two layers of resist forming the adhesive layer is in a semi-cured state, and the intermediate portion of the second resist is in a cured state, and the intermediate portion of the adhesive layer is in a stable state in which the volume is unlikely to change over time. This makes it possible to appropriately suppress the volume change in the adhesive layer even after time has passed since the base portion and the conductive layer are fixed and integrated by the adhesive layer, and prevents the conductive layer and the electrodeposition layer thereon from shifting, thereby obtaining a highly accurate mask. In addition, the intermediate portion of the two layers of resist forming the adhesive layer is in a state in which almost no adhesive force is exerted, so that the base portion and the conductive layer can be separated from each other starting from the adhesive layer after electroforming is completed without difficulty, and the efficiency of the separation work between the mask and the matrix is ​​greatly improved.

[0107] In addition, the manufacturing method of an electroforming mother mold disclosed in the present invention is a manufacturing method of an electroforming mother mold used for electroforming a mask having a large number of through holes, and includes a conductive layer formation step of forming one or more sheet-like conductive layers at predetermined positions on a predetermined flat metal substrate, an adhesive layer formation step of forming an adhesive layer having an adhesive function on the conductive layer, and a transfer step of affixing and arranging the formed conductive layer and adhesive layer on a flat surface of a plate-shaped base portion by the adhesive force of the adhesive layer and separating them from the substrate, wherein in the adhesive layer formation step, an intermediate portion of the adhesive layer surrounded by a frame-shaped portion within a predetermined range from the outer periphery of the adhesive layer is formed so as to have a smaller change in volume over time than the frame-shaped portion and to have a smaller adhesive force bonding the base portion and the conductive layer.

[0108] As described above, according to the disclosure of the present invention, a conductive layer is formed on a metal substrate, an adhesive layer is formed on this conductive layer, the integrated conductive layer and adhesive layer are attached to a base portion by the adhesive force of this adhesive layer, and the conductive layer and adhesive layer are separated from the substrate to manufacture a master mold consisting of the conductive layer, adhesive layer, and base portion. In this process, the adhesive layer is formed so that the intermediate portion of the adhesive layer other than the frame-shaped portion within a predetermined range from the outer peripheral edge is less likely to change in volume over time and has a small adhesive force. This makes it possible to stably fix and integrate the base portion and the conductive layer with the adhesive layer that has small volume change over time, suppressing displacement of the conductive layer due to volume change in the adhesive layer and misalignment of the electrochemical layer formed on this conductive layer, and preventing a decrease in accuracy of the mask formed using the manufactured master mold.

[0109] Furthermore, by ensuring adhesive strength in a frame-shaped portion within a predetermined range from the outer peripheral edge of the adhesive layer, while suppressing adhesive strength in the middle portion of the adhesive layer, it is possible to reliably maintain the integration of the base portion and conductive layer that constitute the mother mold in the electroforming process using the manufactured mother mold, while easily separating the base portion and conductive layer with less force at the adhesive layer position after electroforming is completed.This allows the mother mold to be separated and removed efficiently by sequentially separating the base portion and conductive layer from the mask side after electroforming, and also suppresses adverse effects such as deformation of the mask body by reducing the force applied to the mask side when separating the mother mold.

[0110] In addition, in the method for manufacturing an electroforming mold disclosed in the present invention, if necessary, in the adhesive layer formation step, one resist, which is an unexposed negative dry film resist, is placed on the conductive layer, and a frame-shaped portion within a predetermined range from the outer peripheral edge of the one resist is not exposed and left unexposed, while a middle portion of the one resist surrounded by the frame-shaped portion is exposed to harden the middle portion, and another resist, which is an unexposed negative dry film resist, is placed on the one resist with the hardened middle portion, and a frame-shaped portion within a predetermined range from the outer peripheral edge of the other resist is not exposed and left unexposed, while a half-exposure with a smaller amount of exposure than the exposure for the middle portion of the one resist is performed on the one resist, and the one resist and the other resist form the adhesive layer.

[0111] Thus, according to the disclosure of the present invention, in the adhesive layer forming step, one resist, which is a dry film resist forming an adhesive layer, and another resist are laminated and arranged, and for the one resist placed on the conductive layer, a frame-shaped portion within a predetermined range from its outer periphery is left unexposed, while the middle portion is hardened by exposure, and for the other resist placed on the one resist, a frame-shaped portion within a predetermined range from its outer periphery is left unexposed, while the middle portion is subjected to half exposure with a small amount of exposure, so that the middle portion of the formed adhesive layer is in a stable state in which the volume is unlikely to change over time, and even if time has passed since the base portion and the conductive layer are integrated by the adhesive layer, the volume change in the adhesive layer can be appropriately suppressed, and the conductive layer is prevented from being affected, and a highly accurate mask can be electroformed with the manufactured mother mold. In addition, by obtaining a state in which almost no adhesive force is exerted in the middle portion of the adhesive layer, the separation work of the formed mask and the mother mold can be efficiently carried out after the manufactured mother mold is used for electroforming. [Explanation of symbols]

[0112] 1. Deposition mask (metal mask) 2 Mask body 2a Pattern formation area 2b Outer edge 3 Frame 7 metal layer 8 Vapor deposition hole (through hole) 9 Deposition pattern (pattern) 10. Matrices 11 Base 12 Adhesive layer 12a First Resist 12b Second Resist 12c, 12e frame-shaped part 12d, 12f middle part 13 Conductive layer 13a Sheet 13b Sheet 13c sheet 14 Primary pattern resist 15, 15a Primary electrodeposition layer 16 Secondary pattern resist 17 Resist layer 18 Resist layer 18a, 18b Resist layer 19 Adhesive layer 41 Photomask 41a Transparent hole 42 Photomask 42a Transparent hole 60 Substrates 61 Resist 62 Outer frame resist 63, 64 Resist 70 Photomask 71, 72 Photomask

Claims

1. A method for manufacturing a metal mask including a mask body having a large number of through holes and a frame for reinforcing the mask body, comprising: a mask body forming step of forming the mask body by electroforming using a matrix having a laminated structure; a joining step of joining the mask body and the frame body, the mask body forming step includes a resist layer forming step of forming a resist layer on a matrix and an exposure step of exposing the resist layer to light, The mask body forming step includes a preheating step of preheating to a predetermined preheating temperature before the exposure step, the mother die includes a plate-shaped base portion, a sheet-shaped adhesive layer disposed on the base portion, and a conductive layer adhered to the base portion via the adhesive layer; the adhesive layer has a property of being tacky in an uncured state, but transitioning to a state in which it is no longer tacky and in which its volume does not change over time as curing progresses; In the adhesive layer, an intermediate portion surrounded by a frame-shaped portion in a predetermined range from the outer periphery of the adhesive layer, which is in an uncured state, is in a predetermined cured state in which the degree of change in volume over time is smaller than that of the frame-shaped portion. A method for manufacturing a metal mask.

2. the adhesive layer of the matrix is ​​a dry film resist arranged in two layers, and at least a frame-shaped portion within a predetermined range from an outer periphery is in the uncured state; The intermediate portion of at least one of the two layers of dry film resist constituting the adhesive layer is in a semi-cured state in which the adhesiveness is less than that of the frame-shaped portion and the degree of change in volume over time is small, or in a cured state in which the adhesiveness is not present and the volume does not change over time. The method for manufacturing a metal mask according to claim 1 .

3. A method for manufacturing a metal mask as described in claim 1 or 2, characterized in that it includes a master mold preheating process of preheating the master mold to a predetermined preheating temperature prior to the exposure process.

4. In the exposure step, exposure is performed by an exposure device, 4. The method for manufacturing a metal mask according to claim 3, further comprising an exposure device preheating step of preheating the inside of the exposure device to a predetermined preheat temperature before the exposure step.

5. In the exposure step, exposure is performed using a photomask having a predetermined pattern corresponding to the mask body, 5. The method for producing a metal mask according to claim 4, further comprising a photomask preheating step of preheating the photomask to a predetermined preheating temperature before the exposure step.

6. 6. The method for manufacturing a metal mask according to claim 5, wherein the matrix, the interior of the exposure device, and the photomask are preheated to the same temperature.

7. 7. The method for manufacturing a metal mask according to claim 6, wherein a maximum temperature that can be reached inside the exposure device is set to a preheating temperature.

8. the mask body forming step further includes a primary pattern resist forming step of forming a primary pattern resist by removing an unexposed portion of the resist after the exposure step, and a primary electrodeposition layer forming step of forming a primary electrodeposition layer by electroforming on a surface of the mother mold that is not covered with the primary pattern resist, 8. The method for manufacturing a metal mask according to claim 3, wherein the preheating temperature is set to the maximum temperature among the exposure temperature in the exposure step, the electroforming temperature in the primary electrodeposition layer formation step, and the deposition temperature in the deposition step using a metal mask.

9. A metal mask having a mask body with a large number of through holes and a frame for reinforcing the mask body, the mask body is a metal plate-like body formed by electroforming in an exposed area of ​​a matrix having a pattern resist; the mother die has a laminated structure including a plate-shaped base portion, a sheet-shaped adhesive layer disposed on the base portion, and a conductive layer adhered to the base portion via the adhesive layer; the adhesive layer has a property of being tacky in an uncured state, but transitioning to a state in which it is no longer tacky and in which its volume does not change over time as curing progresses; an intermediate portion of the adhesive layer, which is surrounded by a frame-shaped portion that is in an uncured state and extends from an outer periphery of the adhesive layer, is in a predetermined cured state in which the degree of change in volume over time is smaller than that of the frame-shaped portion; The pattern resist is formed by exposing the resist layer to light in a state where the mother mold on which an unexposed resist layer has been formed is preheated to a predetermined preheating temperature, and then curing the resist layer. A metal mask that features

Citation Information

Patent Citations

  • Method for exposing

    JP1997246178A

  • Vapor deposition mask, and its production method

    JP2005015908A

  • Aligner

    JP2005243771A

  • Substrate temperature adjusting unit, stage unit, exposure unit, and manufacturing method of device

    JP2006080357A

  • Vapor deposition mask structural body manufacturing method

    JP2006152339A