Laminated sheet, packaging body, and method for manufacturing packaging body

The laminated sheet design with a propylene resin-based first film layer and adhesive layer facilitates recyclability by allowing separation of the barrier layer, addressing the recyclability challenges of coextrusion methods and reducing resin usage.

JP7574093B2Inactive Publication Date: 2024-10-28IDEMITSU UNITECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021015773
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-03
Publication Date
2024-10-28
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing laminated sheets with barrier layers formed by coextrusion methods face challenges in recyclability due to the difficulty in separating and recovering layers made of different materials, hindering environmental sustainability.

Method used

A laminated sheet structure with a barrier layer, a laminate adhesive layer, and a first film layer, where the first film layer contains propylene resin with smectica crystals, allowing the layers to be bonded via the adhesive layer for easier separation and recycling.

Benefits of technology

This structure reduces the amount of resin raw material used for the barrier layer and enhances recyclability by enabling the reuse of the first film layer after separating the barrier layer, thus improving environmental friendliness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007574093000004
    Figure 0007574093000004
  • Figure 0007574093000005
    Figure 0007574093000005
  • Figure 0007574093000001
    Figure 0007574093000001
Patent Text Reader

Abstract

To provide a laminate sheet with consideration to environment conservation which has high recyclability.SOLUTION: A laminate sheet includes a barrier layer 13, a laminate adhesive layer 14, and a first film layer 15 which are arranged in this order.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a laminated sheet, a package, and a method for producing the package. [Background technology]

[0002] Conventionally, as a laminate sheet forming a package excellent in visibility of contents and long-term storage, a laminate sheet formed by extruding a polyolefin resin and a resin constituting a barrier layer using a co-extrusion method has been known. Patent Document 1 discloses a laminate sheet having layers in the order of a polybutylene terephthalate resin layer, a polyethylene terephthalate resin layer, a gas barrier layer, and an antifogging agent-containing heat seal layer, with the aim of obtaining a laminate sheet with high gas barrier properties and antifogging properties. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-30255 A Summary of the Invention [Problem to be solved by the invention]

[0004] In recent years, there has been a demand for improving the recyclability of packaging materials from the viewpoint of environmental conservation. However, in the case of a sheet having a barrier layer laminated thereon by a co-extrusion method, it is difficult to separate and recover the barrier layer and the film layer, which are made of different materials, and there remains a problem in terms of recyclability.

[0005] Therefore, an object of the present invention is to provide a laminated sheet, a packaging body, and a method for producing a packaging body that are highly recyclable and environmentally friendly. [Means for solving the problem]

[0006] [1] A laminate sheet having, in this order, a barrier layer, a laminating adhesive layer, and a first film layer. [2] The laminate sheet according to [1], wherein the first film layer contains a propylene-based resin containing smectic crystals. [3] The laminate sheet according to [2], wherein the propylene-based resin has an isotactic pentad fraction of 85 mol % or more. [4] Propylene-based resins have a crystallization rate of 2.5 min at 130°C. -1 The laminate sheet according to [2] or [3], which is as follows: [5] The laminate sheet according to any one of [2] to [4], wherein the propylene-based resin has an exothermic peak of 1.0 J / g or more on the low-temperature side of the maximum endothermic peak in a differential scanning calorimetry curve. [6] A laminate sheet described in any one of [2] to [5], wherein the first film layer does not contain a nucleating agent. [7] The laminate sheet according to any one of [2] to [6], having a second film layer, a barrier layer, a laminating adhesive layer, and a first film layer in this order. [8] The laminate sheet according to [7], wherein the thickness of the second film layer is 10 μm or more. [9] The laminate sheet according to [7] or [8], wherein the ratio A / B of the thickness of the first film layer to the thickness of the second film layer is 2 or more, where A is the thickness of the first film layer and B is the thickness of the second film layer.

[10] A laminate sheet described in any one of [7] to [9], wherein the second film layer is primarily composed of unstretched polypropylene resin.

[11] The laminate sheet according to any one of [2] to

[10] , wherein the barrier layer contains a resin and an inorganic filler.

[12] The laminate sheet according to any one of [2] to

[11] , having a thickness of 0.2 mm or more and 1.5 mm or less.

[13] A laminate sheet according to any one of [2] to

[12] , wherein the lamination adhesive layer is formed from an ester-based adhesive or an ether-based adhesive.

[14] A packaging body using the laminated sheet described in any one of [1] to

[13] .

[15] A packaging body obtained by thermoforming the laminate sheet described in any one of [1] to

[13] .

[16] A packaging body obtained by thermoforming the laminate sheet according to any one of [2] to

[13] at a temperature equal to or lower than the melting point of the propylene-based resin.

[17] A method for producing a packaging body by thermoforming a laminate sheet described in any one of [1] to

[13] . Effect of the Invention

[0007] According to the laminate sheet of the present invention, the barrier layer and the first film layer are bonded via a laminating adhesive layer, so that the amount of resin raw material used for the barrier layer can be reduced and recyclability can be improved. In addition, when the laminate sheet has a second film layer, a barrier layer, a laminating adhesive layer, and a first film layer in that order, and the first film layer and the second film layer are made of different materials, the barrier layer and the first film layer are bonded via the laminating adhesive layer, and by separating the barrier layer and the first film layer, it becomes possible to reuse the first film after separating the barrier layer, thereby improving recyclability. [Brief description of the drawings]

[0008] [Figure 1] FIG. 2 is a schematic cross-sectional view showing a laminate structure of the laminate sheet according to the embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic diagram of a manufacturing device for manufacturing a second film constituting a laminate sheet according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings. In this specification and the drawings, components having substantially the same functional configurations are designated by the same reference numerals, and duplicated explanations will be omitted.

[0010] In this specification, the main component of the resin forming each layer of the laminate sheet means the resin component with the highest content among the resins forming that layer. Therefore, the resin may contain other components in addition to the main component. The main component can be confirmed, for example, by the IR method. In this specification, the content of the resin component forming each layer of the laminate sheet is expressed in mass% relative to the total resin forming that layer, unless otherwise specified.

[0011] FIG. 1 is a schematic cross-sectional view showing a laminate structure of a laminate sheet according to one embodiment of the present invention. 1, the laminate sheet 10 has, in this order, a second film layer 11, an anchor coat layer 12, a barrier layer 13, and a first film layer 15. The barrier layer 13 and the first film layer 15 are bonded via a laminating adhesive layer 14 formed of, for example, an ester-based adhesive or an ether-based adhesive. The laminate sheet 10 preferably has a thickness suitable for forming a container, with the lower limit being, for example, 0.15 mm, preferably 0.20 mm, and the upper limit being, for example, 1.5 mm, preferably 1.2 mm. The structure of each layer will now be described.

[0012] The second film layer 11 is a layer forming the surface of the laminate sheet 10, and is a layer formed of a film such as a retort compatible film, an antistatic film, or an easy peel film. The second film layer 11 is formed of a film mainly composed of a polyolefin resin. Specifically, the second film layer 11 is preferably mainly composed of a polypropylene resin, and more preferably mainly composed of a non-oriented polypropylene resin (CPP), but is not limited thereto, and may be formed of other polyolefin resins. The content of the polypropylene resin is, for example, 60% by mass or more, preferably 70% by mass or more, and more preferably 80% by mass or more. The upper limit of the content of the polypropylene resin is not particularly limited, but is, for example, 100% by mass.

[0013] The second film layer 11 may contain, in addition to polypropylene-based resin, nylon, polyethylene-based resin such as high density polyethylene (HDPE) or low density polyethylene (LDPE), polystyrene-based resin, polyester-based resin such as polyethylene terephthalate, or a mixture thereof. The melt flow rate of the polypropylene-based resin is preferably, for example, 0.1 g / 10 min to 6.0 g / 10 min, and more preferably 1.5 g / 10 min to 5.0 g / 10 min. This improves moldability. In the present invention, the melt flow rate of the polypropylene resin is measured in accordance with JIS-K7210 at a measurement temperature of 230° C. and a load of 2.16 kg. The polypropylene resin may contain a polypropylene resin having an isotactic pentad fraction of 85 mol% or more. The isotactic pentad fraction of the polypropylene resin is preferably 88 mol% or more, more preferably 90 mol% or more. The upper limit of the isotactic pentad fraction of the polypropylene resin is not particularly limited, but is, for example, 99 mol%. By increasing the isotactic pentad fraction of the polypropylene resin, the barrier property can be further improved. The content of the polypropylene resin in the second film layer 11 is, for example, 5% or more, preferably 15% or more, more preferably 30% or more. The upper limit of the content of the polypropylene resin having an isotactic pentad fraction of 85 mol% or more in the second film layer 11 is usually 100%.

[0014] The anchor coat layer 12 is preferably a layer containing one or more resins selected from the group consisting of urethane-based resins, acrylic-based resins, polyolefin-based resins, and polyester-based resins. In consideration of adhesion to other layers, urethane-based resins and polyolefin-based resins are preferred. The urethane resin is usually obtained by reacting at least a diisocyanate, a high molecular weight polyol, and a chain extender. The high molecular weight polyol may be a polyether polyol, a polycarbonate polyol, or a polyester polyol. The anchor coat layer may be made of one or more of the above-mentioned materials. The anchor coat layer 12 can be formed, for example, by applying the above-mentioned resin to the second film layer 11 with a gravure coater, kiss coater, bar coater, or the like, and drying it at 40° C. or higher and 100° C. or lower for 10 seconds to 10 minutes. The thickness of the anchor coat layer 12 is, for example, 35 nm or more, preferably 50 nm or more. The thickness of the anchor coat layer 12 is, for example, 3000 nm or less, preferably 2000 nm or less. When the thickness of the anchor coat layer 12 is 35 nm or more, the adhesion with other layers can be sufficiently ensured. When the thickness of the anchor coat layer is 3000 nm or less, the occurrence of blocking due to stickiness can be suppressed.

[0015] The barrier layer 13 is a layer having oxygen barrier properties and water vapor barrier properties. The barrier layer 13 can be formed, for example, by using an aqueous coating agent in which a resin or an inorganic filler is dispersed in a solvent. By forming the barrier layer 13 with the aqueous coating agent, it is possible to improve the conformability of the barrier layer 13 when the laminate sheet 10 is formed. The barrier layer 13 may contain additives and the like in addition to the aqueous coating agent.

[0016] The barrier layer 13 can be formed by applying a water-based coating agent containing resin and inorganic particles in water or alcohol, followed by heat treatment. By carrying out heat treatment, the inorganic particles are regularly arranged, resulting in a so-called labyrinth effect, which enhances the barrier properties. Examples of resins include polyvinyl alcohol (PVA), ethylene-vinyl alcohol copolymer (EVOH), polyvinylidene chloride, polyacrylonitrile, polysaccharides, polyacrylic acid and its esters, polymethacrylic acid and its esters, amide resins, imide resins, ester resins, resins having two or more types of functional groups in one molecule, urethane resins, epoxy resins, phenolic resins, and melamine resins. The inorganic particles are preferably inorganic layered compounds. Inorganic layered compounds have a layered structure formed by stacking unit crystal layers one on top of the other. Examples of inorganic layered compounds include graphite, phosphate derivative compounds (e.g., zirconium phosphate compounds), chalcogenides, hydrotalcite compounds, lithium aluminum composite hydroxides, and clay minerals. Examples of clay minerals include kaolinite-serpentine clay minerals such as kaolinite, talc-pyrophyllite clay minerals such as talc, smectite clay minerals such as montmorillonite, vermiculite clay minerals, mica clay minerals such as tetrasilylic mica, brittle mica clay minerals such as xanthophyllite, and chlorite clay minerals such as clinochlore. Moreover, as the water-based coating agent, commercially available materials can be used, such as EXCEVIER NOH1200 (trade name) and EXCEVIER NOH2200 (trade name) (manufactured by Sumitomo Chemical Co., Ltd.).

[0017] The laminating adhesive layer 14 is formed by a laminating process as described below, and is a layer formed from, for example, an ester-based or ether-based adhesive.

[0018] The first film layer 15 is a layer that functions as a base layer of the laminate sheet 10, and contains a propylene-based resin. The propylene-based resin may be a polymer containing at least propylene. Examples of the polymer containing propylene include homopolypropylene and a copolymer of propylene and an olefin. The copolymer of propylene and an olefin may be a block copolymer or a random copolymer. Alternatively, it may be a mixture of these. From the viewpoints of heat resistance and hardness, the propylene-based resin contained in the first film layer 15 in this embodiment is preferably homopolypropylene.

[0019] The propylene-based resin forming the first film layer 15 contains Smectic crystals as a crystal structure. Smectic crystals are a metastable intermediate phase, and each domain size is small, so they have excellent transparency. In addition, since they are in a metastable state, the laminated sheet 10 containing Smectic crystals softens with a lower amount of heat compared to a sheet containing α crystals in which crystallization has progressed, and therefore has excellent moldability. The first film layer 15 is preferably composed mainly of a propylene-based resin containing Smectic crystals.

[0020] The propylene-based resin forming the first film layer 15 may contain, in addition to Smectic crystals, other crystal forms such as β crystals, γ crystals, and amorphous portions. For example, 30% by mass or more, 50% by mass or more, 70% by mass or more, or 90% by mass or more of the propylene-based resin may be Smectic crystals, with the remainder being other crystal forms.

[0021] Whether or not the propylene-based resin contains smectic crystals can be determined by whether or not the sheet containing the propylene-based resin is obtained by cooling at 80°C / sec or more. Whether or not the sheet containing the propylene-based resin is obtained by cooling at 80°C / sec or more can be determined by calculating the scattering intensity distribution and long period by small-angle X-ray scattering analysis. The measurement is performed under the following conditions. The X-ray generator used is ultraX 18HF (manufactured by Rigaku Corporation), and an imaging plate is used to detect scattering. ·Light source wavelength: 0.154nm Voltage / Current: 50kV / 250mA Irradiation time: 60 minutes Camera length: 1.085m -Sample thickness: Stack the sheets so that the thickness is 1.5 mm to 2.0 mm. Stack the sheets so that the film formation (MD) direction is aligned. In order to shorten the measurement time, the sheets are stacked so that the thickness is 1.5 mm or more and 2.0 mm or less. However, if the measurement time is extended, it is possible to measure a single sheet without stacking the sheets.

[0022] The propylene-based resin forming the first film layer 15 preferably has an isotactic pendant fraction of 85 mol% or more, more preferably 88 mol% or more, and even more preferably 90 mol% or more. If the isotactic pendant fraction is 85 mol% or more, the laminate sheet 10 has excellent rigidity. If the isotactic pendant fraction is 99 mol% or less, the laminate sheet 10 has excellent transparency. The isotactic pendant fraction is the isotactic pendant fraction of pendant units (units in which five consecutive propylene monomers are isotactically bonded) in the molecular chain of the resin composition. The method for measuring this fraction is described, for example, in Macromolecules, Vol. 8 (1975), p. 687, 13 It can be measured by C-NMR.

[0023] The propylene-based resin forming the first film layer 15 has a crystallization rate of 2.5 min at 130° C. -1 It is preferable that the crystallization rate is 2.5 min -1 When the crystallization rate is equal to or less than this value, rapid hardening of the portion in contact with the mold during thermoforming can be suppressed, and deterioration of the design can be prevented. The crystallization rate is measured by the method described in the Examples.

[0024] The propylene-based resin forming the first film layer 15 preferably has an exothermic peak of 1.0 J / g or more on the low temperature side of the maximum endothermic peak in a differential scanning calorimetry curve. More preferably, it is 1.5 J / g or more. There is no particular upper limit. It is usually 10 J / g or less. The exothermic peak is measured using a differential scanning calorimeter. The melt flow rate of the polypropylene resin forming the first film layer 15 is preferably, for example, 0.1 g / 10 min to 6.0 g / 10 min, more preferably 1.5 g / 10 min to 5.0 g / 10 min, which can improve moldability.

[0025] The first film layer 15 may contain, in addition to the propylene-based resin, a resin other than the propylene-based resin, an additive, and the like. It is preferable that the first film layer 15 does not contain a nucleating agent. When the first film layer 15 does not contain a nucleating agent, the number of α crystals and spherulites does not increase, and the degree of crystallinity does not become high. Examples of the nucleating agent include sorbitol-based crystal nucleating agents, etc. Examples of commercially available products include Gelall MD (New Japan Chemical Co., Ltd.) and Rikemaster FC-2 (Riken Vitamin Co., Ltd.). When the thickness of the first film layer 15 is A and the thickness of the second film layer 11 is B, the ratio of the thicknesses of the first film layer 15 and the second film layer 11 (layer ratio) A / B is preferably 2 or greater.

[0026] [Method for producing laminated sheet] Next, a method for producing the laminate sheet 10 will be described. The manufacturing method of the laminated sheet 10 includes a first film manufacturing process for manufacturing a first film 15b constituting the first film layer 15, a barrier coated film manufacturing process for laminating an anchor coating agent and a barrier coating agent onto a second film 11a constituting the second film layer 11 to form a barrier coated film 16, and a lamination process for bonding the first film 15b and the barrier coated film 16 together by a lamination method.

[0027] (First film manufacturing process) The first film 15b constituting the first film layer 15 is manufactured using a manufacturing apparatus 20 shown in Fig. 2. The manufacturing apparatus 20 includes a T-die 21 for forming a molten resin into a film, a first cooling roll 22, a second cooling roll 23, a third cooling roll 24, a fourth cooling roll 25, a metallic endless belt 26, a cooling water spray nozzle 27, a water tank 28, a water absorbing roll 29, and a peeling roll 30.

[0028] First, a polypropylene resin is extruded as a sheet-like material 15a from a T-die 21 of an extruder, and the sheet-like material 15a is sandwiched between a metallic endless belt 26 and a fourth cooling roll 25 on a first cooling roll 22. In this state, the sheet-like material 15a is rolled and quenched by the first cooling roll 22 and the fourth cooling roll 25 in a circular arc portion corresponding to the central angle θ1 of the first cooling roll 22.

[0029] Next, the sheet-like material 15a is sandwiched between the metallic endless belt 26 and the fourth cooling roll 25 in a circular arc portion corresponding to approximately the lower half of the fourth cooling roll 25 and further rolled, and the sheet-like material 15a is further quenched by spraying cooling water onto the back side of the metallic endless belt 26 by a cooling water spray nozzle 27. The sprayed cooling water is collected in a water tank 28, and the collected water is discharged through a drainage groove 28a.

[0030] Next, the sheet-like material 15a is further rolled and cooled by the fourth cooling roll 25, and is then transported together with the metal endless belt 26 onto the second cooling roll 23. Here, the sheet-like material 15a is pressed against the second cooling roll 23 by the tension applied by the peeling roll 30, and is further cooled via the metal endless belt 26 in a circular arc portion corresponding to approximately the upper half of the second cooling roll 23. Note that water adhering to the back surface of the metal endless belt 26 is removed by a water absorbing roll 29 provided midway from the fourth cooling roll 25 to the second cooling roll 23.

[0031] Next, the sheet-like material 15 a cooled on the second cooling roll 23 is peeled off from the metallic endless belt 26 by a peeling roll 30 . In the manufacturing apparatus 20 as described above, the surface of the first cooling roll 22 is covered with an elastic material 21a made of nitrile-butadiene rubber (NBR). The surface of the second cooling roll 23 is also covered with an elastic material (not shown) made of nitrile-butadiene rubber (NBR). In addition, the temperature of the metallic endless belt 26 can be adjusted by a cooling means (not shown) such as a water-cooling type built into the third cooling roll 24 or the like.

[0032] An example of manufacturing conditions for first film 15b will be shown below, but the manufacturing conditions are not limited to the following. Molten resin: homopolypropylene F-300SP (Prime Polymer Co., Ltd.) (melting point: 160°C, isotactic pendant fraction: [mmmm] = 92 mol%) Extruder diameter: 150mm T-die 21 width (die edge size): 1400mm Thickness of the first film 15b: 0.3mm Take-up speed of first film 15b: 25 m / min Surface temperature of the fourth cooling roll 25 and the metal endless belt 26: 17°C ·Cooling rate: 10,800℃ / min (180℃ / sec) Nucleating agent: None

[0033] The melting point of the molten resin (polypropylene) was measured as follows. Using a differential scanning calorimeter (DSC) (Diamond DSC, manufactured by PerkinElmer Japan Co., Ltd.), the polypropylene was heated from 50° C. to 200° C. at 10° C. / min, held at 220° C. for 5 minutes, and cooled from 220° C. to 50° C. at 10° C. / min. The temperature showing the maximum value of the endothermic peak obtained at this time was taken as the melting point of the polypropylene.

[0034] The crystallization rate of the polypropylene used in the first film 15b was measured using a differential scanning calorimeter (DSC) (Diamond DSC manufactured by PerkinElmer Japan Co., Ltd.). Specifically, the polypropylene was heated from 50°C to 230°C at 10°C / min, held at 230°C for 5 minutes, cooled from 230°C to 130°C at 80°C / min, and then held at 130°C for crystallization. Measurement of the change in heat quantity was started when the temperature reached 130°C, and a DSC curve was obtained. The crystallization rate was calculated from the obtained DSC curve by the following steps (i) to (iv). (i) The baseline was determined by approximating the change in heat quantity from a point 10 times the time from the start of measurement to the peak top to a point 20 times the time by a straight line. (ii) The intersection points between the tangent line having a slope at the inflection point of the peak and the baseline were determined to determine the start and end times of crystallization. (iii) The time from the obtained crystallization start time to the peak top was measured as the crystallization time. (iv) The crystallization rate was calculated from the reciprocal of the obtained crystallization time.

[0035] (Barrier coat film manufacturing process) The barrier coat film 16 consisting of the second film layer 11, the anchor coat layer 12 and the barrier layer 13 is obtained by coating the second film 11a constituting the second film layer 11 with an anchor coat agent and a barrier agent. The barrier coat film 16 can be coated by, for example, a method using a bar coater, a gravure coating method, a spray coating method, a dip coating method or the like.

[0036] (Lamination process) The lamination step is a step of bonding the first film 15b and the barrier coat film 16 by a lamination method such as adhesive lamination, extrusion lamination, or thermal lamination. Among the above lamination methods, the adhesive lamination method or thermal lamination method is preferred, the adhesive lamination method is more preferred, and the dry lamination method is even more preferred. The adhesive used in the lamination method may be, for example, an ester-based, ether-based or other adhesive, depending on the application of the container or the like.

[0037] In the lamination process, the surface of the barrier coat film 16 on the barrier layer 13 side is adhered to the first film layer 15b. As a result, a lamination adhesive layer 14 made of the adhesive as described above is formed between the barrier layer 13 and the first film layer 15. At the interface between the laminate adhesive layer 14 and the barrier layer 13, and at the interface between the laminate adhesive layer 14 and the first film 15b, the resins of both are not mixed by melting. In this specification, a layer having such characteristics is called a laminate adhesive layer. Because the laminate adhesive layer has the above characteristics, it is relatively easy to separate it from the barrier layer 13 or the first film 15b, for example, when recycling after use.

[0038] According to the laminated sheet 10 of the above embodiment, the barrier coated film 16 having the barrier layer 13 and the first film 15b are bonded via a lamination adhesive layer 14 formed through a lamination process, so that the amount of resin raw material used for the barrier layer 13 can be reduced and recyclability can be improved, compared to, for example, a co-extruded multilayer film. In addition, when the first film layer 15 and the second film layer 11 are made of different materials, the barrier layer 13 and the first film layer 15 are bonded together via a laminate adhesive layer 14, and by separating the barrier layer 13 and the first film layer 15, it becomes possible to reuse the first film 15b after separating the barrier coated film 16, thereby improving recyclability.

[0039] The barrier layer 13 may be formed of a polyvinylidene chloride resin, which is a barrier resin. The polyvinylidene chloride resin is not particularly limited as long as it mainly contains vinylidene chloride monomers as a constituent unit, and may be polyvinylidene chloride (PVDC) or a copolymer of vinylidene chloride and a monomer copolymerizable with vinylidene chloride.

[0040] An example of the copolymer is one having a vinylidene chloride content of 60% by mass or more and 99% by mass or less and a content of a monomer copolymerizable with vinylidene chloride of 1% by mass or more and 40% by mass or less. Examples of monomers copolymerizable with vinylidene chloride include one or more selected from vinyl chloride, acrylonitrile, acrylic acid, acrylic acid alkyl esters (alkyl group having 1 to 18 carbon atoms), methacrylic acid, methacrylic acid alkyl esters (alkyl group having 1 to 18 carbon atoms), maleic anhydride, itaconic acid, itaconic acid alkyl esters, vinyl acetate, ethylene, propylene, isobutylene, butadiene, and the like.

[0041] The polyvinylidene chloride resin can be produced by a known method, or various commercially available products can be used, such as the Saran Resin series manufactured by Asahi Kasei Corporation and the Saran Latex series manufactured by Asahi Kasei Corporation.

[0042] The barrier layer 13 made of polyvinylidene chloride resin can be formed by dispersing a polyvinylidene chloride resin in a solvent, coating the first film layer 15 with a resin liquid, and curing the liquid. The method for forming the polyvinylidene chloride resin is not limited to this, and the polyvinylidene chloride resin may be formed by a lamination method in which a resin film made of the polyvinylidene chloride resin is laminated on the first film layer 15. When forming the polyvinylidene chloride resin by the lamination method, it is preferable to coat it with an anchor coating agent as necessary.

[0043] The barrier layer 13 may be formed of polyvinyl alcohol (PVA). Like polyvinylidene chloride resins, polyvinyl alcohol can be formed on the first film layer 15 by coating or laminating.

[0044] When the barrier layer 13 is formed of a polyvinylidene chloride resin or polyvinyl alcohol, the laminate sheet 10 does not require the second film layer 11 and the anchor coat layer 12. In other words, when the barrier layer 13 is formed of a polyvinylidene chloride resin or polyvinyl alcohol, the laminate sheet 10 may have a configuration including the barrier layer 13 and the first film layer 15 in this order.

[0045] In the above embodiment, when the second film layer 11 is made of a polypropylene-based resin, it may have the same structure as the first film layer 15, for example, a polypropylene-based resin containing smectic crystals.

[0046] [Package and manufacturing method of package] The laminate sheet 10 of the above embodiment can be used as a packaging material. The packaging body can be produced, for example, by thermoforming the laminate sheet 10 of the above embodiment. In this case, it is preferable to carry out thermoforming at a temperature equal to or lower than the melting point of the propylene-based resin in the first film layer 15 of the laminate sheet 10. By thermoforming at a temperature equal to or lower than the melting point of the propylene-based resin, the fine crystal structure is maintained, resulting in a highly transparent laminate sheet 10. The packaging body can be used, for example, as a container body or a lid for a container for food or the like.

[0047] From the viewpoint of improving transparency, the internal haze of the package is preferably 15% or less. It is also preferable that the ratio of the internal haze of the package to the internal haze of the laminate sheet 10 before thermoforming is 1 or less. It is more preferable that the internal haze of the package is 15 percent or less, and the ratio of the internal haze of the package to the internal haze of the laminated sheet 10 before thermoforming is 1 or less. If the internal haze of the package is 15 percent or less, and the ratio of the internal haze of the package to the internal haze of the laminated sheet before thermoforming is 1 or less, the package will have higher transparency. The internal haze is the haze of the resin itself measured without the influence of the surface roughness of the sheet, etc. The internal haze is measured using a haze meter (NDH-2000, manufactured by Nippon Denshoku Industries Co., Ltd.) based on JIS K 7136. EXAMPLES

[0048] The present invention will now be described in more detail with reference to examples and comparative examples, but the present invention is not limited to the contents of these examples. In the examples, the laminate sheet 10 was produced by bonding the barrier coat film 16 and the first film 15b by a lamination method. On the other hand, in the comparative examples, a laminate sheet having a film layer and a barrier layer was produced by a co-extrusion method.

[0049] Example 1 A laminated sheet 10 in which the first film layer contained smectic crystals was produced so that the total thickness of the layers was 0.3 mm. The materials and thicknesses of the layers were as follows: <Second film layer> Non-oriented polypropylene resin (CPP), product name RT-610C (manufactured by Idemitsu Unitech Co., Ltd.) Thickness: 80μm <Barrier layer> Water-based coating agent, product name EXCEVIER NOH1200 (manufactured by Sumitomo Chemical Co., Ltd.) Thickness: 0.95μm <First film layer> Homopolypropylene resin, product name F-300SP (Prime Polymer, isotactic pendant fraction: 92 mol%, melt flow rate: 3.0 g / 10 min) Thickness: 200μm Crystallization rate at 130℃: 1.0min -1 below

[0050] Example 2 Except for the fact that the thickness of the barrier layer was 1.2 μm, the same procedure as in Example 1 was followed. The materials and thicknesses of the layers were as follows: <Second film layer> Non-oriented polypropylene resin (CPP), product name RT-610C (manufactured by Idemitsu Unitech Co., Ltd.) Thickness: 80μm <Barrier layer> Water-based coating agent, product name EXCEVIER NOH1200 (manufactured by Sumitomo Chemical Co., Ltd.) Thickness: 1.2μm <First film layer> Homopolypropylene resin, product name F-300SP (manufactured by Prime Polymer Co., Ltd.) Thickness: 200μm

[0051] Comparative Example 1 A laminated sheet having a film layer / adhesive layer / barrier layer / adhesive layer / film layer in this order was produced using a co-extruder so that the total layer thickness was 0.3 mm. The raw materials and thicknesses of each layer are as follows. The adhesive layer in Comparative Example 1 is a layer formed to improve the adhesion between the barrier layer and the film layer during the production of the laminated sheet using the co-extrusion method, and is formed of, for example, the following adhesive resin. The adhesive layer of Comparative Example 1 is formed by a co-extrusion method, and therefore, unlike a laminate adhesive layer, the resins of both layers are melted and mixed at the interfaces between the film layer and the adhesive layer, and between the adhesive layer and the barrier layer.

[0052] <Film layer> Homopolypropylene resin, product name F-300SP (manufactured by Prime Polymer Co., Ltd.) <Barrier layer> Ethylene-vinyl alcohol copolymer resin (EVOH), product name G-Soarnol (manufactured by Mitsubishi Chemical Corporation) <Adhesive layer> Adhesive resin, product name Modic P674V (manufactured by Mitsubishi Chemical Corporation)

[0053] Comparative Example 2 The procedure was the same as in Comparative Example 1, except that the film layer was made of a homopolypropylene resin, trade name PS412M (manufactured by SunAllomer Co., Ltd.).

[0054] (Optical property evaluation) Using a haze meter (NDH-2000, manufactured by Nippon Denshoku Industries Co., Ltd.), the haze and gloss of the laminated sheets of the examples and comparative examples were measured based on JIS K 7136. In addition, the laminated sheets were molded in a mold with a flat surface (in Examples 1 and 2, the first film layer was the mold surface), and the haze and gloss of the mold side were measured. The optical property evaluation results are shown in Table 1.

[0055] [Table 1]

[0056] As shown in Table 1, it can be seen that the laminate sheets of Examples 1 and 2 are superior to the laminate sheets of Comparative Examples 1 and 2 in both transparency and glossiness.

[0057] (Oxygen permeability rating 1) The laminated sheets of the examples and comparative examples were molded into a vessel having a diameter of 76 mm, and the concentration of oxygen gas permeating from outside the vessel was measured in accordance with JIS K 7126-B under conditions of a measurement atmosphere having a temperature of 23° C. and a relative humidity of 50%. The results of oxygen permeability evaluation 1 are shown in Table 2.

[0058] [Table 2]

[0059] As shown in Table 2, it is apparent that the containers of Examples 1 and 2 are superior in oxygen barrier property compared to the containers of Comparative Examples 1 and 2.

[0060] (Oxygen permeability rating 2) The laminated sheets of the Examples and Comparative Examples were stretched on their flat surfaces in a mold, and the concentration of permeated oxygen gas was measured in accordance with JIS K 7126-B under conditions of a temperature of 23° C. and a relative humidity of 50% in the measurement atmosphere. The results of oxygen permeability evaluation 2 are shown in Table 3.

[0061] [Table 3]

[0062] As shown in Table 3, it is apparent that the laminate sheets of Examples 1 and 2 are superior to the laminate sheet of Comparative Example 1 in terms of oxygen barrier property. [Explanation of symbols]

[0063] 10... laminated sheet, 11... second film layer, 12... anchor coat layer, 13... barrier layer, 14... laminate adhesive layer, 15... first film layer, 20... manufacturing apparatus.

Claims

1. A barrier layer; A laminating adhesive layer; a first film layer, The first film layer is a laminate sheet containing a propylene-based resin containing smectic crystals.

2. The laminate sheet according to claim 1 , wherein the propylene-based resin has an isotactic pentad fraction of 85 mol % or more.

3. The propylene-based resin has a crystallization rate of 2.5 min at 130° C. -1 The laminate sheet according to claim 1 or claim 2, wherein:

4. The laminate sheet according to claim 1 , wherein the propylene-based resin has an exothermic peak of 1.0 J / g or more on the low-temperature side of a maximum endothermic peak in a differential scanning calorimetry curve.

5. The laminate sheet according to claim 1 , wherein the first film layer does not contain a nucleating agent.

6. The laminate sheet according to claim 1 , comprising, in this order, a second film layer, the barrier layer, the laminating adhesive layer, and the first film layer.

7. The laminate sheet according to claim 6 , wherein the second film layer has a thickness of 10 μm or more.

8. The laminate sheet according to claim 6 or claim 7, wherein the thickness ratio A / B of the first film layer to the second film layer is 2 or more, where A is the thickness of the first film layer and B is the thickness of the second film layer.

9. The laminate sheet according to claim 6 , wherein the second film layer is mainly composed of a non-oriented polypropylene resin.

10. The laminate sheet according to claim 1 , wherein the barrier layer contains a resin and an inorganic filler.

11. The laminate sheet according to any one of claims 1 to 10, having a thickness of 0.2 mm or more and 1.5 mm or less.

12. The laminate sheet according to claim 1 , wherein the lamination adhesive layer is formed from an ester-based adhesive or an ether-based adhesive.

13. A packaging body using the laminated sheet according to any one of claims 1 to 12.

14. A packaging body obtained by thermoforming the laminate sheet according to any one of claims 1 to 12.

15. A packaging body obtained by thermoforming the laminate sheet according to any one of claims 1 to 12 at a temperature equal to or lower than the melting point of the propylene-based resin.

16. A method for producing a package by thermoforming a laminate sheet according to any one of claims 1 to 12.

Citation Information

Patent Citations

  • Gas barrier laminate and package using the same

    JP2013159074A

  • Non-stretched coextrusion film for lid material and package

    JP2018030255A

  • Laminated film

    JP2018176670A

  • Package

    JP2021008324A

  • Oxygen absorber composition, oxygen-absorbing multilayer body, oxygen-absorbing packaging container, and method for storing article

    WO2017169036A1