SUBSTRATE PROCESSING APPARATUS AND SUBSTRATE PROCESSING METHOD
The substrate processing apparatus and method address the challenge of substrate separation by using a laser absorption film and peel-promoting film to control peeling surfaces, enhancing edge trimming efficiency and throughput.
Patent Information
- Application Number
- JP2022575538
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-01-15
- Filing Date
- 2022-01-05
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-01-05
AI Technical Summary
Existing methods for separating bonded substrates in polymerized wafers face challenges when the thickness of the laser absorption layer is small, leading to inadequate energy absorption and storage, which complicates the edge trimming process.
A substrate processing apparatus and method that includes a laser absorption film, a peel-promoting film, and a control unit to control laser irradiation and movement, allowing selective peeling at different interfaces based on the thickness of the laser absorption film, using pulsed laser light to form an unbonded region and facilitate separation.
Enables effective separation of substrates regardless of the laser absorption film thickness, improving edge trimming efficiency and throughput by controlling the peeling surface position, ensuring consistent and efficient substrate separation.
Smart Images

Figure 0007577137000001 
Figure 0007577137000002 
Figure 0007577137000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a substrate processing apparatus and a substrate processing method. [Background technology]
[0002] Patent Document 1 discloses a substrate processing system having a modified layer forming device that forms a modified layer inside a first substrate along the boundary between the peripheral and central parts of a first substrate to be removed in a laminated substrate formed by bonding a first substrate and a second substrate, and a peripheral removal device that removes the peripheral part of the first substrate using the modified layer as a base point. Patent Document 1 also describes forming a modified surface inside a device layer formed on a non-processing surface of the first substrate, thereby reducing the bonding strength between the first substrate and the second substrate at the peripheral part of the first substrate. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2019 / 176589 Summary of the Invention [Problem to be solved by the invention]
[0004] The technique according to the present disclosure appropriately peels the first substrate from the second substrate in a laminated substrate in which the first substrate and the second substrate are bonded together. [Means for solving the problem]
[0005] One aspect of the present disclosure is a substrate processing apparatus for processing a polymerized substrate formed by stacking a first substrate, an interface layer including at least a laser absorbing film and a peeling-promoting film, and a second substrate, the substrate processing apparatus including: a substrate holding unit for holding the polymerized substrate; an interface laser irradiation unit for irradiating the laser absorbing film with pulsed laser light; a movement mechanism for relatively moving the substrate holding unit and the interface laser irradiation unit; and a control unit for controlling the movement mechanism, wherein the control unit selects a position of a peeling surface between the first substrate and the second substrate from between the first substrate and the laser absorbing film, or between the peeling-promoting film and the second substrate, based on a thickness of the laser absorbing film. Effect of the Invention
[0006] According to the present disclosure, in a laminated substrate in which a first substrate and a second substrate are bonded together, the first substrate can be appropriately peeled off from the second substrate. [Brief description of the drawings]
[0007] [Figure 1A] FIG. 2 is a side view showing a configuration example of an overlapped wafer according to an embodiment. [Figure 1B] FIG. 11 is a side view showing another configuration example of the overlapped wafer according to the embodiment. [Diagram 2] 1 is a plan view showing an outline of the configuration of a wafer processing system according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a side view showing the outline of the configuration of an interface modification device. [Figure 4] FIG. 2 is an explanatory diagram showing main steps of wafer processing in the wafer processing system. [Diagram 5] FIG. 2 is an explanatory diagram showing a state of a laminated wafer irradiated with laser light. [Figure 6] FIG. 2 is an explanatory diagram showing the position of the peeling surface of the first wafer. [Figure 7] 11 is a table showing the correlation between the thickness of the laser absorbing film and the irradiation interval of the laser light, and the position of the peeled surface of the first wafer. [Figure 8]FIG. 2 is a flow diagram showing main steps of wafer processing according to the embodiment. [Figure 9] 1 is a graph showing a tendency of the relationship between the thickness of a laser absorbing film and the pulse energy of a laser beam. [Figure 10] 11 is an explanatory diagram showing main steps of another wafer processing in the wafer processing system. FIG. [Figure 11] 11 is an explanatory diagram showing main steps of another wafer processing in the wafer processing system. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] In the manufacturing process of semiconductor devices, a first substrate (a silicon substrate such as a semiconductor substrate) having a plurality of electronic circuits or other devices formed on its surface and a second substrate are bonded together to form a laminated substrate. substrate In some cases, the peripheral portion of the semiconductor device is removed, which is called edge trimming.
[0009] The edge trim of the first substrate is performed, for example, by using a substrate processing system disclosed in Patent Document 1. That is, a modified layer is formed by irradiating the inside of the first substrate with a laser beam, and the peripheral portion is removed from the first substrate using the modified layer as a base point. According to the substrate processing system described in Patent Document 1, a modified surface is formed by irradiating the interface where the first substrate and the second substrate are bonded with a laser beam, and the bonding strength between the first substrate and the second substrate at the peripheral portion is reduced.
[0010] In such edge trimming, by irradiating a laser absorbing layer (e.g., an oxide film) formed between the first substrate and the second substrate with a laser beam, peeling may occur at the interface between the first substrate and the second substrate. However, when performing edge trimming of the first substrate by irradiating the laser absorbing layer with a laser beam in this manner, if the thickness of the laser absorbing layer is small, the amount of energy absorbed and stored in the absorbing layer by the irradiation of the laser beam becomes small, and there is a risk that the edge trimming of the first substrate cannot be performed appropriately.
[0011] The technology according to the present disclosure has been made in consideration of the above circumstances, and in a laminated substrate in which a first substrate and a second substrate are bonded together, the first substrate is appropriately peeled off from the second substrate. Hereinafter, a substrate processing system as a substrate processing apparatus and a substrate processing method according to the present embodiment will be described with reference to the drawings. In this specification and the drawings, elements having substantially the same functional configurations are denoted by the same reference numerals, and duplicated descriptions will be omitted.
[0012] In a wafer processing system 1 according to this embodiment, which will be described later, processing is performed on a laminated wafer T, which is a laminated substrate in which a first wafer W as a first substrate and a second wafer S as a second substrate are bonded together, as shown in Fig. 1A. Hereinafter, in the first wafer W, the surface to be bonded to the second wafer S is referred to as the front surface Wa, and the surface opposite the front surface Wa is referred to as the back surface Wb. Similarly, in the second wafer S, the surface to be bonded to the first wafer W is referred to as the front surface Sa, and the surface opposite the front surface Sa is referred to as the back surface Sb.
[0013] The first wafer W is a semiconductor wafer such as a silicon substrate, and a device layer (not shown) including a plurality of devices is formed on the front surface Wa side of the first wafer W. A laser absorbing film Fw as a laser absorbing film, a metal film Fm as a peeling promoting film, and a surface film Fe are further formed in a laminated manner on the front surface Wa side of the first wafer W, and the surface film Fe is bonded to the surface film Fs of the second wafer S. As the laser absorbing film Fw, for example, an oxide film (SiO2 film, TEOS film) or the like that can absorb the laser light from the laser irradiation system 110 described later is used. As the metal film Fm, for example, a film such as a tungsten film that has an adhesive force with the surface film Fe that is at least weaker than the adhesive force between the first wafer W and the laser absorbing film Fw is used. Also, the peripheral portion We of the first wafer W is a portion to be removed in the edge trim described later, and is, for example, in the range of 0.5 mm to 3 mm in the radial direction from the outer end of the first wafer W. As the surface film Fe, for example, an oxide film (THOX film, SiO2 film, TEOS film), a SiC film, a SiCN film, an adhesive, or the like is used.
[0014] The second wafer S is, for example, a wafer that supports the first wafer W. A surface film Fs is formed on the surface Sa of the second wafer S. Examples of the surface film Fs include an oxide film (THOX film, SiO2 film, TEOS film), a SiC film, a SiCN film, or an adhesive. The second wafer S is a wafer that supports the first wafer W. Device Layer The second wafer S functions as a protective material (support wafer) for protecting the first wafer W. The second wafer S does not need to be a support wafer, and may be a device wafer on which a device layer (not shown) is formed, similar to the first wafer W.
[0015] In the laminated wafer T according to the present embodiment, the laser absorbing film Fw, the metal film Fm, the surface film Fe, and the surface film Fs correspond to the "interface layer" according to the technique of the present disclosure.
[0016] In the following, an example will be described in which the wafer processing system 1 processes a laminated wafer T formed by stacking a laser absorbing film Fw, a metal film Fm, a surface film Fe, and a surface film Fs at the interface between the first wafer W and the second wafer S shown in FIG. 1A. However, the configuration of the laminated wafer T processed in the wafer processing system 1 is not limited to this. For example, in the wafer processing system 1, as shown in Fig. 1B, a laminated wafer T2 may be processed in which a surface film Fm2 as a second peeling-promoting film is further formed at the interface between the surface Wa of the first wafer W and the laser absorbing film Fw. As the surface film Fm2, a film (e.g., a SiN film) that has a smaller adhesion to the surface Wa of the first wafer W than the laser absorbing film Fw and can transmit a laser beam from a laser irradiation system 110 described later can be used. In this case, the adhesion between the metal film Fm and the surface film Fe is smaller than the adhesion between the surface Wa of the first wafer W and the surface film Fm2.
[0017] 2, the wafer processing system 1 has a configuration in which a loading / unloading station 2 and a processing station 3 are integrally connected. In the loading / unloading station 2, for example, a cassette C capable of accommodating a plurality of overlapped wafers T is loaded and unloaded between the loading / unloading station 2 and the outside. The processing station 3 is equipped with various processing devices that perform desired processing on the overlapped wafers T.
[0018] The loading / unloading station 2 is provided with a cassette mounting stage 10 on which a cassette C capable of accommodating a plurality of overlapped wafers T is mounted. A wafer transport device 20 is provided adjacent to the cassette mounting stage 10 on the positive side of the X-axis of the cassette mounting stage 10. The wafer transport device 20 moves on a transport path 21 extending in the Y-axis direction, and is configured to be able to transport the overlapped wafers T between the cassette C on the cassette mounting stage 10 and a transition device 30 described below.
[0019] In the loading / unloading station 2, a transition device 30 for transferring the overlapped wafer T between the processing station 3 and the wafer transfer device 20 is provided adjacent to the wafer transfer device 20 on the positive side of the X-axis of the wafer transfer device 20.
[0020] The processing station 3 is provided with a wafer transport device 40, an edge removal device 50 as an edge removal section, a cleaning device 60, an interface modification device 70 as an interface laser irradiation section, and an internal modification device 80 as an internal laser irradiation section.
[0021] The wafer transport device 40 is provided on the X-axis positive side of the transition device 30. The wafer transport device 40 is configured to be freely movable on a transport path 41 extending in the X-axis direction, and configured to be able to transport the overlapped wafer T to the transition device 30, the edge removing device 50, the cleaning device 60, the interface modifying device 70, and the internal modifying device 80 in the carry-in / out station 2.
[0022] The peripheral removal device 50 removes the peripheral portion We of the first wafer W, i.e., performs edge trimming. The cleaning device 60 performs cleaning processing on the exposed surface of the second wafer S after the edge trimming, and removes particles on the exposed surface. The interface modification device 70 irradiates the interface between the first wafer W and the second wafer S with laser light (interface laser light, e.g., CO2 laser) to form an unbonded region Ae, which will be described later. The detailed configuration of the interface modification device 70 will be described later. The internal modification device 80 irradiates the inside of the first wafer W with laser light (interface laser light, e.g., YAG laser) to form a peripheral modified layer M1, which is a base point for peeling off the peripheral portion We, and a divided modified layer M2, which is a base point for dividing the peripheral portion We into small pieces.
[0023] The above-described wafer processing system 1 is provided with a control device 90 as a control unit. The control device 90 is, for example, a computer, and has a program storage unit (not shown). The program storage unit stores a program for controlling the processing of the laminated wafer T in the wafer processing system 1. The program storage unit also stores a program for controlling the operation of a drive system such as the above-described various processing devices and transport device to realize wafer processing in the wafer processing system 1, which will be described later. The above-described program may be recorded in a computer-readable storage medium H and installed in the control device 90 from the storage medium H.
[0024] Next, a detailed configuration of the interface modification device 70 will be described.
[0025] 3, the interface modification device 70 has a chuck 100 as a substrate holding part that holds the upper surface of the overlapped wafer T. The chuck 100 holds the back surface Sb of the second wafer S by suction.
[0026] The chuck 100 is supported by a slider table 102 via an air bearing 101. A rotation mechanism 103 is provided on the lower surface side of the slider table 102. The rotation mechanism 103 incorporates, for example, a motor as a drive source. The chuck 100 is configured to be rotatable around a θ-axis (vertical axis) via the air bearing 101 by the rotation mechanism 103. The slider table 102 is configured to be movable along a rail 105 extending in the Y-axis direction by a horizontal movement mechanism 104 provided on the lower surface side of the slider table 102. The rail 105 is provided on a base 106. The drive source of the horizontal movement mechanism 104 is not particularly limited, but for example, a linear motor is used. In this embodiment, the above-mentioned rotation mechanism 103 and horizontal movement mechanism 104 correspond to the "movement mechanism" according to the technology of the present disclosure.
[0027] A laser irradiation system 110 is provided above the chuck 100. The laser irradiation system 110 has a laser head 111 and a lens 112. The lens 112 may be configured to be movable up and down by an elevator mechanism (not shown).
[0028] The laser head 111 has a laser oscillator (not shown) that oscillates a laser beam in a pulsed manner. That is, the laser beam irradiated from the laser irradiation system 110 to the laminated wafer T held on the chuck 100 is a so-called pulsed laser, and its power repeatedly changes between 0 (zero) and a maximum value. In this embodiment, the laser beam is a CO2 laser beam, and the wavelength of the CO2 laser beam is, for example, 8.9 μm to 11 μm. The laser head 111 may have other devices besides the laser oscillator, such as an amplifier.
[0029] The lens 112 is a cylindrical member, and irradiates laser light onto the laminated wafer T held by the chuck 100. The laser light emitted from the laser irradiation system 110 passes through the first wafer W, and is irradiated onto and absorbed by the laser absorbing film Fw.
[0030] Next, a description will be given of wafer processing performed using the wafer processing system 1 configured as above. In this embodiment, as described above, a case will be described in which the peripheral portion We of the first wafer W is peeled off from the second wafer S (so-called edge trimming) in the wafer processing system 1. In this embodiment, the first wafer W and the second wafer S are bonded in a bonding device (not shown) outside the wafer processing system 1 to form an overlapped wafer T in advance.
[0031] First, a cassette C containing a plurality of overlapped wafers T is placed on a cassette placement table of the loading / unloading station 2. 10 It is placed on.
[0032] Next, the overlapped wafer T is taken out of the cassette C by the wafer transfer device 20 and transferred to the , by the wafer transfer device 40 The first wafer W is transported to the internal reforming device 80. In the internal reforming device 80, a laser beam is irradiated to the inside of the first wafer W as shown in FIG. 4(a) to form a peripheral modified layer M1 and a divided modified layer M2. The peripheral modified layer M1 serves as a base point for removing the peripheral portion We in the edge trimming described below. The divided modified layer M2 serves as a base point for breaking the peripheral portion We into small pieces to be removed. In the drawings used in the following explanation, the divided modified layer M2 may be omitted in order to avoid complicating the illustration.
[0033] The overlapped wafer T with the peripheral modified layer M1 and the divided modified layer M2 formed inside the first wafer W is then transferred to the interface modification device 70 by the wafer transfer device 40. In the interface modification device 70, the interface between the first wafer W and the second wafer S at the peripheral portion We (more specifically, the above-mentioned laser absorbing film Fw formed at the interface) is irradiated with pulsed laser light while rotating and moving the overlapped wafer T (first wafer W) in the Y-axis direction. As a result, peeling occurs at the interface between the first wafer W and the second wafer S, as shown in FIG. 4(b).
[0034] In the interface modification device 70, peeling occurs at the interface between the first wafer W and the second wafer S in this manner, and an unbonded area Ae is formed in which the bonding strength between the first wafer W and the second wafer S is reduced. As a result, an annular unbonded area Ae and a bonded area Ac in which the first wafer W and the second wafer S are bonded are formed at the interface between the first wafer W and the second wafer S, as shown in Fig. 5, on the radial inside of the unbonded area Ae. In edge trimming, which will be described later, the peripheral portion We of the first wafer W, which is the object of removal, is removed, and the presence of the unbonded area Ae in this manner allows the peripheral portion We to be appropriately removed.
[0035] The method for forming the unbonded region Ae in the interface modification apparatus 70 will be described in detail later.
[0036] The overlapped wafer T with the unbonded region Ae formed therein is then transferred by the wafer transfer device 40 to the edge removal device 50. In the edge removal device 50, as shown in FIG. 4(c), the edge We of the first wafer W is removed, i.e., edge trimming is performed. At this time, the edge We is peeled off from the center of the first wafer W using the edge modified layer M1 as a base point, and is also completely peeled off from the second wafer S using the unbonded region Ae as a base point. At this time, the removed edge We is also divided into small pieces using the divided modified layer M2 as a base point.
[0037] In removing the peripheral portion We, for example, a wedge-shaped blade may be inserted into the interface between the first wafer W and the second wafer S forming the overlapped wafer T. Alternatively, for example, an air blow or a water jet may be sprayed to strike and remove the peripheral portion We. In this manner, in edge trimming, an impact is applied to the peripheral portion We of the first wafer W, so that the peripheral portion We is peeled off from the peripheral modified layer M1 as a base point. As described above, the bonding strength between the first wafer W and the second wafer S is reduced due to the unbonded region Ae, so that the peripheral portion We is appropriately removed from the second wafer S.
[0038] The overlapped wafer T from which the peripheral portion We of the first wafer W has been removed is then transferred to the cleaning apparatus 60 by the wafer transfer apparatus 40. In the cleaning apparatus 60, as shown in FIG. 4(d), the peripheral portion of the second wafer S from which the peripheral portion We has been removed (hereinafter, sometimes referred to as the "exposed surface" after edge trimming) is cleaned.
[0039] In the cleaning apparatus 60, for example, a cleaning laser light (e.g., a CO2 laser) may be irradiated onto the exposed surface of the second wafer S to modify and remove the surface of the exposed surface, thereby removing (cleaning) particles and the like remaining on the exposed surface. For example, the exposed surface of the second wafer S may be spin-cleaned by supplying a cleaning liquid to the exposed surface of the second wafer S while rotating the laminated wafer T. In the cleaning apparatus 60, in addition to cleaning the exposed surface of the second wafer S, the back surface Sb of the second wafer S may also be cleaned.
[0040] Thereafter, the laminated wafer T on which all the processes have been performed is transferred by the wafer transfer device 20 to the cassette C on the cassette mounting table 10 via the transition device 30. In this manner, a series of wafer processes in the wafer processing system 1 is completed.
[0041] 4(a) and 4(b), the peripheral modified layer M1 and the divided modified layer M2 are formed in the internal reforming device 80, and then the unbonded region Ae is formed in the interface reforming device 70. However, the order of wafer processing in the wafer processing system 1 is not limited to this. In other words, the peripheral modified layer M1 and the divided modified layer M2 may be formed in the internal reforming device 80 after the unbonded region Ae is formed in the interface reforming device 70.
[0042] Here, in the interface modification device 70, a laser irradiation system 110 irradiates a laser beam onto the laser absorbing film Fw formed at the interface between the first wafer W and the second wafer S. The irradiated laser beam is absorbed by the laser absorbing film Fw. At this time, the laser absorbing film Fw accumulates energy by absorbing the laser beam, and the temperature rises, causing it to expand. As a result, shear stress is generated at the interface between the first wafer W and the laser absorbing film Fw (the interface between the first wafer W and the surface film Fm2, which has a small adhesive force, in the case of the laminated wafer T2 shown in FIG. 1B) due to the expansion of the laser absorbing film Fw, and this causes peeling at the interface between the first wafer W and the laser absorbing film Fw (the surface film Fm2). That is, at the irradiation position of the laser beam, an unbonded area Ae is formed in which the bonding force between the first wafer W and the second wafer S is reduced due to peeling.
[0043] In this way, in the interface modification apparatus 70, normally, an unbonded region Ae is formed at the interface between the laser absorbing film Fw (surface film Fm2) and the first wafer W, but as described above, when the thickness of the laser absorbing film Fw is small, the amount of energy absorbed and stored in the laser absorbing film Fw is small. That is, since the amount of expansion of the laser absorbing film Fw is reduced, the shear stress generated at the interface between the first wafer W and the laser absorbing film Fw (surface film Fm2) is reduced, and as a result, the interface between the first wafer W and the laser absorbing film Fw (surface film Fm2) cannot be properly peeled off, and there is a risk that the unbonded region Ae cannot be properly formed.
[0044] In this embodiment, as shown in Fig. 1, a metal film Fm is formed as a peeling promoting film at the interface between the first wafer W and the second wafer S. The metal film Fm is a film in which the adhesion between the metal film Fm and the surface film Fe is weaker than the adhesion between the first wafer W and the laser absorbing film Fw (surface film Fm2). In the following description, the interface between the first wafer W and the laser absorbing film Fw (the interface between the first wafer W and the surface film Fm2 in the case of the overlapped wafer T2 shown in Fig. 1B) may be referred to as "interface A", and the interface between the metal film Fm and the surface film Fe may be referred to as "interface B" (see Fig. 6).
[0045] As a result, in this embodiment, even if the thickness of the laser absorbing film Fw is small and the shear stress generated at the A interface by the irradiation of the laser light is small, peeling can be caused at the B interface with weak adhesion, and the unbonded region Ae can be formed. Specifically, even if the shear stress generated due to the expansion of the laser absorbing film Fw is not sufficient to the stress required for peeling at the A interface, it can reach the stress required for peeling at the B interface, and as a result, the unbonded region Ae can be formed at the B interface instead of the A interface. In other words, in this embodiment, even when the thickness of the laser absorbing film Fw is small, which has conventionally made it difficult to properly peel the first wafer W from the second wafer S, it is possible to properly peel (edge trim) the first wafer W.
[0046] 1, when the laser absorbing film Fw is thick, if the laser absorbing film Fw is irradiated with laser light under the same conditions as in the case where the laser absorbing film Fw is thin, the unbonded region Ae may not be appropriately formed at the interface B. Specifically, when the laser absorbing film Fw is thick, the energy of the laser light irradiation does not reach the interface on the metal film Fm side, which is the surface opposite to the laser light incident surface, and as a result, the shear stress required for peeling off the interface B may not be generated.
[0047] That is, for example, when a plurality of overlapped wafers T that are processed successively are irradiated with laser light under similar processing conditions, if there is variation in the thickness of the laser absorbing film Fw among the overlapped wafers T, the edge trimming may not be performed appropriately on the overlapped wafer T having a large thickness of the laser absorbing film Fw, which may result in a reduced yield.
[0048] Therefore, the inventors conducted intensive research and found that it is possible to selectively determine the peeling surface position (the position where the unbonded region Ae is formed) of the first wafer W and the second wafer S by controlling the pulse pitch P, which is the irradiation interval of the laser light in the circumferential direction on the laser absorbing film Fw, and the index pitch Q, which is the irradiation interval of the laser light in the radial direction (see FIG. 5 : hereinafter, the pulse pitch P and the index pitch Q may be collectively referred to simply as the “irradiation interval”).
[0049] Specifically, it was found that narrowing the irradiation interval of the laser light to the laser absorbing film Fw causes peeling at the interface (A interface) between the first wafer W and the laser absorbing film Fw (surface film Fm2), and widening the irradiation interval of the laser light causes peeling at the interface (B interface) between the metal film Fm and the surface film Fe, as shown in Fig. 7. In the following description, the irradiation interval at which peeling occurs at the A interface may be referred to as the "A interface peeling pitch," and the irradiation interval at which peeling occurs at the B interface may be referred to as the "B interface peeling pitch," as shown in Fig. 7.
[0050] The inventors have also found that the laser light irradiation interval at which the peeling surface position of the first wafer W and the second wafer S switches between the A interface and the B interface (hereinafter referred to as the "conversion pitch Pq") changes depending on the thickness of the laser absorbing film Fw. Specifically, as shown in Fig. 7, the inventors have found that the conversion pitch Pq increases as the thickness of the laser absorbing film Fw increases. The inventors have also found that when the thickness of the laser absorbing film Fw increases (to 700 nm or more in the example of Fig. 7), peeling does not occur at the B interface and peeling occurs only at the A interface.
[0051] Next, a method for forming an unbonded region Ae at the interface between the first wafer W and the second wafer S, which is performed in the interface modification apparatus 70 based on the above findings, will be described.
[0052] In forming the unbonded region Ae in the interface modification device 70, first, the thickness of the laser absorbing film Fw is acquired as layer information of the overlapped wafer T on which the unbonded region Ae is to be formed (step E1 in FIG. 8). The acquired layer information of the overlapped wafer T is output to the control device 90. The layer information of the overlapped wafer T may be obtained by the interface modification apparatus 70, or may be obtained in advance outside the interface modification apparatus 70. Further, the method of obtaining the layer information of the overlapped wafer T is not particularly limited, and for example, the layer information may be measured by a sensor or the like, or may be obtained by capturing an image of the overlapped wafer T by a camera or the like.
[0053] The layer information of the overlapped wafer T to be acquired is not limited to only the thickness information of the laser absorbing film Fw, and other information, such as the thickness of a device layer not shown, and the tendency of the surface shapes of the first wafer W and the second wafer S (e.g., whether the shape is convex or concave, etc.) may be acquired.
[0054] When the layer information of the overlapped wafer T (thickness information of the laser absorbing film Fw) is acquired, the separation surface position between the first wafer W and the second wafer S is selected from the A interface or the B interface shown in FIG. 6 (step E2 in FIG. 8). Specifically, for example, the separation surface position may be determined based on the layer information of the overlapped wafer T acquired in step E1, or may be determined according to the purpose of the wafer processing. In addition, when the separation surface position is determined based on the layer information of the overlapped wafer T, it may be determined manually as appropriate based on the acquired layer information, or may be determined automatically using the desired thickness of the laser absorbing film Fw as a threshold value.
[0055] After the separation surface positions of the first wafer W and the second wafer S are selected, the irradiation interval (pulse pitch P and index pitch Q) of the laser light irradiated from the laser irradiation system 110 to the laser absorbing film Fw is then determined (step E3 in FIG. 8).
[0056] 7, in the overlapped wafer T, when the irradiation interval of the laser light is equal to or less than the conversion pitch Pq (A interface peeling pitch), an unbonded area Ae is formed at the A interface, and when the irradiation interval of the laser light is greater than the conversion pitch Pq (B interface peeling pitch), an unbonded area Ae is formed at the B interface. In other words, the position of the peeling surface at which the first wafer W is peeled from the second wafer S changes according to the irradiation interval of the laser light. Moreover, the conversion pitch Pq at which the peeling surface position is switched increases as the thickness of the laser absorbing film Fw formed on the front surface Wa side of the first wafer W increases.
[0057] Therefore, in this embodiment, the irradiation interval of the laser light irradiated to the laser absorbing film Fw is determined based on the layer information (thickness of the laser absorbing film Fw) of the overlapped wafer T acquired in step E1 and the peeling surface position selected in step E2. Specifically, when it is selected in step E2 to peel the first wafer W at the A interface, the irradiation interval is determined within the A interface peeling pitch that is equal to or smaller than the conversion pitch Pq. When it is selected to peel the first wafer W at the B interface, the irradiation interval is determined within the B interface peeling pitch that is larger than the conversion pitch Pq. It is preferable that the correlation between the thickness of the laser absorbing film Fw and the irradiation interval of the laser light, which are shown in FIG. 7, and the position of the peeled surface of the first wafer W is obtained in advance before starting the wafer processing in the wafer processing system 1, and is output to the control device 90.
[0058] Here, as described above, the position of the peeling surface of the first wafer W becomes the A interface when it is equal to or smaller than the conversion pitch Pq, and becomes the B interface when it is larger than the conversion pitch Pq. In other words, the irradiation interval of the laser light for the purpose of peeling the first wafer W at the A interface or the B interface can be arbitrarily selected within the A interface peeling pitch or the B interface peeling pitch.
[0059] Therefore, when determining the irradiation interval of the laser light in step E3, the irradiation interval of the laser light is determined to be, for example, the largest irradiation interval among the A interface peeling pitch and the B interface peeling pitch, thereby improving the throughput of the interface modification equipment 70. In addition, for example, by appropriately selecting the irradiation interval of the laser light among the A interface peeling pitch and the B interface peeling pitch, the throughput of the interface modification equipment 70 can be arbitrarily controlled, and it becomes easy to match the tact time with other processing equipment outside the interface modification equipment 70, for example.
[0060] As described above, when the irradiation interval of the laser light is widened, the position of the peeled surface of the first wafer W tends to be the interface (interface B) between the metal film Fm and the surface film Fe. From this viewpoint, when it is determined that the first wafer W can be peeled at the interface B based on the thickness of the laser absorbing film Fw acquired in step E1, the throughput of the interface modification device 70 can be improved by determining the position of the peeled surface of the first wafer W to be the interface B.
[0061] Once the irradiation interval of the laser light is determined, the laser absorbing film Fw of the overlapped wafer T held by the chuck 100 is irradiated with the laser light so as to achieve the determined irradiation interval (step E4 in FIG. 8). Specifically, the frequency of the laser light and the rotation speed of the chuck 100 (overlapped wafer T) are controlled so that the laser light is irradiated at the determined pulse pitch P, and the movement speed of the chuck 100 (overlapped wafer T) in the Y-axis direction is controlled so that the laser light is irradiated at the determined index pitch Q.
[0062] Thereafter, the entire surface of the laser absorbing film Fw in the peripheral edge portion We to be removed is irradiated with laser light, and when an unbonded area Ae is formed, a series of wafer processing steps in the interface modification apparatus 70 is completed.
[0063] As described above, according to this embodiment, when removing (edge trimming) the peripheral portion We of the first wafer W, the laser absorbing film Fw formed at the interface between the first wafer W and the second wafer S is irradiated with laser light to form an unbonded region Ae, thereby reducing the bonding strength at the interface between the first wafer W and the second wafer S. At this time, since the metal film Fm having a weaker adhesion to the surface film Fe than the adhesion between the first wafer W and the laser absorbing film Fw is formed at the interface between the first wafer W and the second wafer S, even if it is difficult to peel off the peripheral portion We at the interface (A interface) between the first wafer W and the laser absorbing film Fw, the peripheral portion We can be appropriately peeled off at the interface (B interface) between the metal film Fm and the surface film Fe.
[0064] Moreover, according to this embodiment, by controlling the irradiation interval (pulse pitch P and index pitch Q) of the laser light irradiated to the laser absorbing film Fw according to the thickness of the laser absorbing film Fw, it is possible to selectively determine whether the first wafer W is to be peeled off at the above-mentioned A interface or B interface. As a result, even if there is a variation in the thickness of the laser absorbing film Fw among a plurality of overlapped wafers T processed by the interface modification device 70, for example, it is possible to appropriately remove the peripheral portion We of the first wafer W in each overlapped wafer T. In particular, according to this embodiment, even if the thickness of the laser absorbing film Fw is small, which has conventionally made it difficult to peel off the peripheral portion We at the A interface, it is possible to appropriately peel off the peripheral portion We at the B interface.
[0065] Moreover, according to this embodiment, regardless of the thickness of the laser absorbing film Fw formed on the interface of the overlapped wafer T, the edge trimming of the first wafer W can be performed with a substantially constant pulse energy. Specifically, as shown in the comparative example of Fig. 9, in a conventional overlapped wafer T in which a metal film Fm is not formed at the interface, if the thickness of the laser absorbing film Fw is small, the volume that absorbs the pulse energy is small and the energy absorption efficiency is low, so the pulse energy required for peeling becomes large. In other words, the energy control related to the peeling of the first wafer W (the formation of the unbonded region Ae) becomes complicated, and there is room for improvement in terms of energy efficiency. In this regard, with the overlapped wafers T, T2 according to this embodiment in which the metal film Fm is formed at the interface, the first wafer W can be peeled off (the unbonded area Ae can be formed) with approximately constant pulse energy regardless of the thickness of the laser absorbing film Fw, as shown in Fig. 9. In other words, according to this embodiment, the first wafer W can be peeled off (the unbonded area Ae can be formed) with good energy efficiency and with simple control.
[0066] Furthermore, according to this embodiment, as described above, the irradiation interval of the laser light for the purpose of peeling the first wafer W at the A interface or the B interface can be arbitrarily determined within the A interface peeling pitch or the B interface peeling pitch, thereby making it possible to appropriately control the throughput in the interface modification apparatus 70. Specifically, for example, by irradiating the laser light at the widest irradiation interval among the A interface peeling pitch or the B interface peeling pitch, the throughput of the interface modification apparatus 70 can be improved to the maximum. Also, for example, by irradiating the laser light at any irradiation interval within the A interface peeling pitch or the B interface peeling pitch, the laser processing time in the interface modification device 70 can be adjusted to the laser processing time required by the wafer processing system 1, and this makes it easy to match the tact time with other processing devices. In other words, the wafer processing can be optimized in the entire wafer processing system 1, i.e., the throughput in the entire wafer processing system 1 can be improved.
[0067] In the above embodiment, the irradiation interval of the laser light to the laser absorbing film Fw is determined based on the thickness of the laser absorbing film Fw thus formed on the interface of the overlapped wafer T. However, instead of this, when it is necessary to control the irradiation interval of the laser light at a desired interval in the interface modification device 70, the thickness of the laser absorbing film Fw may be determined according to the irradiation interval to form the overlapped wafer T.
[0068] Similarly, when there is a requirement regarding the position of the peeled surfaces between the first wafer W and the second wafer S depending on the purpose of the wafer processing, etc., the thickness of the laser absorbing film Fw may be determined according to the required position of the peeled surfaces to form the overlapped wafer T.
[0069] In the above embodiment, an example has been described in which laser light is irradiated onto the laser absorbing film Fw at a position corresponding to the peripheral portion We of the first wafer W in the wafer processing system 1 to remove the peripheral portion We, i.e., perform edge trimming. However, the wafer processing performed in the wafer processing system 1 is not limited to edge trimming.
[0070] For example, as shown in FIG. 10, the technology disclosed herein can be applied even in a case where an internal surface modification layer M3 serving as a starting point for thinning a first wafer W is formed inside the first wafer W, and in so doing, the peripheral portion We is removed integrally with the back surface Wb side of the first wafer W.
[0071] 10(a), a peripheral modified layer M1 and an internal surface modified layer M3 are sequentially formed in the internal modification device 80, and then an unbonded region Ae is formed at a position corresponding to the peripheral portion We in the interface modification device 70. As a result, as shown in FIG 10(b), the first wafer W is thinned from the internal surface modified layer M3 as a base point, and the peripheral portion We is peeled off and removed together from the peripheral modified layer M1 and the unbonded region Ae as base points.
[0072] Even in such a case, as described above, the metal film is formed at the interface between the first wafer W and the second wafer S. Fm and by controlling the irradiation interval of the laser light to the laser absorbing film Fw, the peeling surface position of the peripheral portion We can be appropriately selected from interface A or interface B. In other words, the first wafer W can be appropriately peeled off from the second wafer S regardless of the thickness of the laser absorbing film Fw.
[0073] Furthermore, for example, as shown in FIG. 11, the technology disclosed herein can also be applied when a so-called laser lift-off is performed in which the entire surface of a first wafer W is peeled off from a second wafer S and a device layer (not shown) formed on the surface Wa of the first wafer W is transferred to the second wafer S.
[0074] Specifically, as shown in Fig. 11(a), a laser light is irradiated onto the laser absorbing film Fw on the entire surface of the overlapped wafer T in an interface modification device 70 to form an unbonded region Ae. This reduces the bonding force between the first wafer W and the second wafer S on the entire surface of the overlapped wafer T, and as shown in Fig. 11(b), the first wafer W can be appropriately peeled off from the second wafer S.
[0075] Even in such a case, as described above, the metal film is formed at the interface between the first wafer W and the second wafer S. Fm and by controlling the irradiation interval of the laser light to the laser absorbing film Fw, the peeling surface position of the first wafer W can be appropriately selected from interface A or interface B. In other words, the first wafer W can be appropriately peeled off from the second wafer S regardless of the thickness of the laser absorbing film Fw.
[0076] In the above embodiment, the example has been described in which the peel-promoting film formed at the interface between the first wafer W and the second wafer S is a metal film Fm (e.g., a tungsten film), but the type of the peel-promoting film is not limited to this. Specifically, it is sufficient that the adhesion force between at least the surface film Fe (or the laser absorbing film Fw) is different from the adhesion force between the first wafer W and the laser absorbing film Fw, and the position of the peeled surface can be selected when irradiating the laser absorbing film Fw with laser light.
[0077] 1, i.e., between the laser absorbing film Fw and the surface film Fe, and may be formed, for example, between the surface Wa and the laser absorbing film Fw of the first wafer W. In such a case, the peeling-promoting film needs to be transparent to the laser light from the laser irradiation system 110.
[0078] 4, after the peripheral modified layer M1 and the divided modified layer M2 are formed inside the first wafer W, the unbonded region Ae is formed at the interface between the first wafer W and the second wafer S, but the order of wafer processing in the wafer processing system 1 is not limited to this. That is, as described above, after the unbonded region Ae is formed at the interface between the first wafer W and the second wafer S, the peripheral modified layer M1 and the divided modified layer M2 may be formed inside the first wafer W.
[0079] Similarly, in the case where the peripheral portion We shown in FIG. 10 is removed integrally with the back surface Wb side of the first wafer W, an unbonded area Ae may be formed at the interface between the first wafer W and the second wafer S, and then a peripheral modification layer M1 and an internal surface modification layer M3 may be formed inside the first wafer W.
[0080] The embodiments disclosed herein should be considered as illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims. [Explanation of symbols]
[0081] 1. Wafer Processing System 70 Interface Modification Equipment 90 Control device 100 Chuck 103 Rotation mechanism 104 Horizontal movement mechanism Fm metal film Fw laser absorbing film P Pulse pitch Q Index Pitch S 2nd wafer T Polymer Wafer W First wafer
Claims
1. A substrate processing apparatus for processing a laminated substrate formed by stacking a first substrate, an interface layer including at least a laser absorbing film and a peeling-promoting film, and a second substrate, comprising: a substrate holder for holding the laminated substrate; an interface laser irradiation unit that irradiates the laser absorbing film with a pulsed laser beam; a moving mechanism that moves the substrate holding unit and the interface laser irradiation unit relatively; a control unit for controlling the interface laser irradiation unit and the movement mechanism, The control unit is and executing control to select a position of a peeling surface between the first substrate and the second substrate from between the first substrate and the laser absorbing film, or between the peeling promoting film and the second substrate, based on a thickness of the laser absorbing film.
2. The control unit is The substrate processing apparatus according to claim 1 , further comprising: a control for setting an interval of the laser light irradiated to the laser absorbing film in accordance with a selected position of the peeling surface.
3. The moving mechanism includes: a rotation mechanism that rotates the substrate holding unit and the interface laser irradiation unit relatively; a horizontal movement mechanism for relatively moving the substrate holding unit and the interface laser irradiation unit in a horizontal direction, The substrate processing apparatus according to claim 2 , wherein the control unit executes control to set a circumferential interval and a radial interval as the interval between the laser beams.
4. The substrate processing apparatus according to claim 2 , wherein the control unit executes control to set an interval between the laser beams based on a thickness of the laser absorbing film so that a laser processing time for the laminated substrate is minimized.
5. 4. The substrate processing apparatus according to claim 2, wherein the control unit executes control to set an interval of the laser light based on a thickness of the laser absorbing film so that a laser processing time for the laminated substrate becomes a laser processing time required for the substrate processing apparatus.
6. The substrate processing apparatus according to any one of claims 1 to 5, further comprising an internal laser irradiation unit that irradiates an interior of the first substrate with laser light to form a modified layer that serves as a starting point for peeling of the first substrate.
7. a peripheral removal unit that removes a peripheral portion of the first substrate that is a removal target; The substrate processing apparatus according to claim 6 , wherein the internal laser irradiation section forms a peripheral modified layer that serves as a starting point for peeling of a peripheral portion of the first substrate to be removed.
8. a second peeling-promoting film is formed between the first substrate and the laser absorbing film; The control unit is provided between the first substrate and the laser absorbing film, The substrate processing apparatus according to any one of claims 1 to 7, wherein the position of the peeling surfaces of the first substrate and the second substrate is selected from either between the first substrate and the second peeling-promoting film or between the peeling-promoting film and the second substrate.
9. 9. The substrate processing apparatus according to claim 1, wherein the peeling-promoting film is a tungsten film.
10. A substrate processing method for processing a laminated substrate formed by stacking a first substrate, an interface layer including at least a laser absorbing film and a peeling-promoting film, and a second substrate, comprising the steps of: Obtaining thickness information of the laser absorbing film; and selecting, based on the thickness information, positions of peeling surfaces of the first substrate and the second substrate from either between the first substrate and the laser absorbing film, or between the peeling-promoting film and the second substrate.
11. setting an interval of the laser light irradiated to the laser absorbing film according to the selected position of the peeling surface; 11. The substrate processing method according to claim 10, further comprising: irradiating the laser absorbing film with a pulsed laser beam so as to achieve a set interval between the laser beams.
12. the intervals of the laser beams include circumferential intervals and radial intervals, The laminated substrate and the laser light irradiation unit are rotated relative to each other so that the circumferential interval is the same, The substrate processing method according to claim 11 , wherein the laser absorbing film is irradiated with the laser light from the irradiation unit while the laminated substrate and the laser light irradiation unit are moved relatively in a horizontal direction so as to achieve the radial interval.
13. 13. The substrate processing method according to claim 11, further comprising: setting an interval between the laser beams based on a thickness of the laser absorbing film so that a laser processing time for the laminated substrate is minimized.
14. 13. The substrate processing method according to claim 11, further comprising: setting an interval between the laser beams so that a laser processing time for the laminated substrate is a required laser processing time based on a thickness of the laser absorbing film.
15. The substrate processing method according to any one of claims 10 to 14, further comprising irradiating an inside of the first substrate with laser light to form a modified layer that becomes a starting point for peeling of the first substrate.
16. removing a peripheral portion of the first substrate to be removed; 16. The substrate processing method according to claim 15, wherein the modified layer formed inside the first substrate includes a peripheral modified layer that becomes a starting point for peeling of a peripheral portion of the first substrate to be removed.
17. a second peeling-promoting film is formed between the first substrate and the laser absorbing film; The positions of the peeling surfaces of the first substrate and the second substrate are changed to between the first substrate and the laser absorbing film, The substrate processing method according to any one of claims 10 to 15, wherein the separation is selected from between the first substrate and the second release-promoting film, or between the release-promoting film and the second substrate.
Citation Information
Patent Citations
Separation method
JP1998125929A
Laser lift-off method and laser lift-off system
JP2012015150A
Wafer detachment using medium wavelength infrared ablation
JP2016525801A
Substrate processing system, substrate processing method, and computer storage medium
WO2019176589A1