Cell culture component for forming cell sheets, manufacturing method of cell culture component for forming cell sheets, culture vessel, method for producing cultured cells, and cultured cells with cell culture component
The cell culture member with hydrophilic and hydrophobic regions and fine uneven structures addresses the challenge of controlling cell orientation and adhesion, facilitating efficient industrial production and improved cell adhesion.
Patent Information
- Application Number
- JP2021058006
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-30
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2041-03-30
AI Technical Summary
Existing cell culture members, such as those described in Patent Document 1, face challenges in controlling the orientation and adhesion area of cultured cells, and there is a need for improved industrial mass production capabilities.
A cell culture member with a base material featuring hydrophilic and hydrophobic regions, and a fine uneven structure region, where the ratio of hydrophobic area to total area is between 0.02 to 0.95, with height differences and uneven structures that facilitate controlled cell adhesion and orientation.
The solution allows for precise control of cell orientation and adhesion area, enhancing industrial mass production capabilities while improving cell adhesion and orientation control.
Smart Images

Figure 0007578043000001 
Figure 0007578043000002 
Figure 0007578043000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a cell culture component for forming a cell sheet, a method for producing a cell culture component for forming a cell sheet, a culture vessel, a method for producing cultured cells, and cultured cells attached to the cell culture component. [Background technology]
[0002] In recent years, cell culture techniques have been used in various industrial fields. For example, Patent Document 1 proposes a cell culture member for controlling the orientation of cultured cells. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2019-37220 A Summary of the Invention [Problem to be solved by the invention]
[0004] The cell culture component of Patent Document 1 has a plurality of flat portions and a plurality of uneven portions, and the extension direction of the cultured cells is aligned in these uneven portions to control the orientation of the cultured cells. However, according to the study by the present inventors, there is room for improvement in terms of controlling the orientation of cultured cells while limiting the adhesion area of the cultured cells in the cell culture component of Patent Document 1. In addition, the cell culture component for forming cell sheets is also required to be industrially mass-producible during production. The present invention provides a cell culture component for forming a cell sheet, which can control the orientation and adhesive area of cultured cells and has excellent industrial mass productivity; and a method for producing the same; a culture vessel equipped with the cell culture component for forming a cell sheet; a method for producing cultured cells using the cell culture component for forming a cell sheet; and cultured cells attached to the cell culture component equipped with the cell culture component for forming a cell sheet. [Means for solving the problem]
[0005] The present invention has the following aspects. [1] A cell culture component for forming a cell sheet, comprising a substrate; a hydrophilic region and a hydrophobic region formed on a surface of the substrate; the hydrophobic region is located at a position that is at a height difference relative to the hydrophilic region in the thickness direction of the substrate; at least a part of the hydrophobic region is formed with a fine concave-convex structure region including a plurality of convex portions or a plurality of concave portions; and the ratio of the area of the hydrophobic region to the sum of the area of the hydrophilic region and the area of the hydrophobic region when the cell culture component is viewed in a plane is 0.02 to 0.95. [2] The cell culture component for forming a cell sheet according to [1], wherein the height difference between the hydrophilic region and the hydrophobic region is 100 nm to 10 μm. [3] The cell culture component for forming a cell sheet according to [1] or [2], wherein the average height of the plurality of convex portions or the average depth of the plurality of concave portions is 100 nm or more. [4] A cell culture component for forming a cell sheet, comprising: a substrate; a hydrophilic region and a hydrophobic region are formed on a surface of the substrate; a fine concave-convex structure region including a plurality of convex portions or a plurality of concave portions is formed in at least a part of the hydrophobic region; the average height of the plurality of convex portions or the average depth of the plurality of concave portions is 100 nm or more; and a ratio of the area of the hydrophobic region to the sum of the area of the hydrophilic region and the area of the hydrophobic region when the cell culture component is viewed in a plane is 0.02 to 0.95. [5] The cell culture component for forming a cell sheet according to [4], wherein an absolute value of the difference in height between the hydrophilic region and the hydrophobic region is 0 to 10 μm. [6] The cell culture member for forming a cell sheet according to any one of [1] to [5], wherein the hydrophilic region is provided with a hydrophilic coating layer. [7] The cell culture component for forming a cell sheet according to any one of [1] to [6], wherein a hydrophilic coating layer is provided on both the hydrophilic region and the hydrophobic region. [8] The cell culture component for forming a cell sheet according to any one of [1] to [7], wherein the average height of the plurality of convex portions or the average depth of the plurality of concave portions is greater than the thickness of the hydrophilic coating layer. [9] The cell culture component for forming a cell sheet according to any one of [1] to [8], wherein a hydrophilic layer is formed in the recesses between the plurality of convex portions of the microrelief structure region of the hydrophobic region, or on the bottoms of the plurality of recesses.
[10] The cell culture component for forming a cell sheet according to any one of [1] to [9], wherein the base material contains at least one resin selected from the group consisting of polyethylene terephthalate, triacetyl cellulose, polycarbonate, cycloolefin polymer, cycloolefin copolymer, acrylic resin, polystyrene, and dimethylpolysiloxane.
[11] A method for producing a cell culture component having a substrate for forming a cell sheet, comprising: forming a hydrophilic region and a hydrophobic region on a surface of the substrate, the hydrophilic region being located at a position that is relatively higher than the hydrophilic region in the thickness direction of the substrate; and forming a finely textured structure region including a plurality of convex portions or a plurality of concave portions in the hydrophobic region; and then applying a hydrophilicity imparting liquid to the entire surface.
[12] The method for producing a cell culture component for forming a cell sheet according to
[11] , wherein the height difference between the hydrophilic region and the hydrophobic region is 100 nm to 10 μm in the thickness direction of the base material.
[13] The method for producing a cell culture component for forming a cell sheet according to
[11] or
[12] , wherein the average height of the plurality of convex portions or the average depth of the plurality of concave portions is 100 nm or more.
[14] A method for producing a cell culture component having a substrate for forming a cell sheet, comprising: dividing the surface of the substrate into a hydrophilic region and a hydrophobic region; forming a finely textured region in the hydrophobic region, the finely textured region including a plurality of convex portions having an average height of 100 nm or more or a plurality of concave portions having an average depth of 100 nm or more; and then applying a hydrophilicity-imparting liquid to the entire surface.
[15] The method for producing a cell culture component for forming a cell sheet according to
[14] , wherein the absolute value of the height difference between the hydrophilic region and the hydrophobic region is 0 to 10 μm in the thickness direction of the base material.
[16] A culture vessel equipped with a cell culture component for forming a cell sheet according to any one of [1] to
[10] .
[17] A method for producing cultured cells, comprising culturing cells using the cell culture component for forming a cell sheet according to any one of [1] to
[10] , and then detaching the cultured cells from the cell culture component for forming a cell sheet.
[18] A cultured cell with a cell culture component, comprising: a cell culture component for forming a cell sheet according to any one of [1] to
[10] ; and cells attached to the cell culture component. Effect of the Invention
[0006] According to the present invention, there are provided a cell culture component for forming a cell sheet, which can control the orientation and adhesive area of cultured cells and has excellent industrial mass productivity; and a method for producing the same; a culture vessel equipped with the cell culture component for forming a cell sheet; a method for producing cultured cells using the cell culture component for forming a cell sheet; and cultured cells attached to the cell culture component equipped with the cell culture component for forming a cell sheet. [Brief description of the drawings]
[0007] [Figure 1] FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II of FIG. [Diagram 3] FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Figure 4] FIG. 4 is a cross-sectional view taken along line IV-IV of FIG. [Diagram 5] FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Figure 6] 6 is a cross-sectional view taken along line VI-VI of FIG. 5. [Figure 7] FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Figure 8] FIG. 8 is a cross-sectional view taken along line VIII-VIII of FIG. 7. [Figure 9] FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Figure 10] XX cross-sectional view of Figure 9. [Figure 11]FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Figure 12] FIG. 12 is a cross-sectional view taken along line XII-XII of FIG. [Figure 13] FIG. 2 is an enlarged plan view illustrating an example of a cell culture member for forming a cell sheet. [Figure 14] 14 is a cross-sectional view taken along the line XIV-XIV of FIG. 13. [Figure 15] 1 is an observation image of cultured cells obtained using the cell culture component for forming a cell sheet of Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] <Cell culture material for cell sheet formation> Hereinafter, a cell culture component for forming a cell sheet according to one embodiment will be described. Hereinafter, in this specification, the term "cell culture component for forming a cell sheet according to one embodiment" will be simply referred to as "cell culture component according to one embodiment."
[0009] The cell culture component according to one embodiment has a substrate. The material of the substrate is not particularly limited, but may be a resin substrate. Among them, a hydrophobic substrate is preferable from the viewpoint of industrial mass production, and a resin substrate is more preferable from the viewpoint of moldability and production cost.
[0010] Examples of the resin constituting the resin substrate include thermoplastic resins, cured products of thermosetting resins, cured products of photocurable resins, etc. For example, the substrate is preferably one containing at least one resin selected from the group consisting of polyethylene terephthalate (PET), triacetyl cellulose (TAC), polycarbonate (PC), cycloolefin polymer (COP), cycloolefin copolymer (COC), acrylic resin (polymethyl methacrylate (PMMA), etc.), polystyrene (PS), and dimethylpolysiloxane (PDMS).
[0011] The overall shape of the substrate is not particularly limited, and may be, for example, a film, a sheet, a plate, or a block. The overall shape of the substrate may be changed depending on the cultured cells and the application of the cultured cells. For example, when producing a cultured cell sheet, the overall shape of the substrate is preferably a sheet shape. A substrate having an overall sheet shape may be called a "sheet-shaped substrate."
[0012] The surface of the substrate is provided with hydrophilic and hydrophobic regions. The hydrophilic regions are regions on the surface of the cell culture component that exhibit hydrophilic properties. On the other hand, the hydrophobic regions are regions on the surface of the cell culture component that exhibit hydrophobic properties. The difference in surface properties between hydrophilic and hydrophobic regions results in differences in cell adhesion between the hydrophilic and hydrophobic regions. Therefore, according to one embodiment of the cell culture component, cells can be selectively collected in the hydrophobic regions, and the adhesion region and orientation can be controlled by adhering cultured cells to the hydrophobic regions.
[0013] In one embodiment of the cell culture component, the hydrophilic and hydrophobic regions can be defined as follows: When a water droplet is dropped onto a substrate, the contact angle formed between the droplet and the surface of the substrate increases, the surface is more hydrophobic, and decreases, the surface is more hydrophilic. In one embodiment, the contact angles of two surface regions on a substrate with different properties are measured, and the surface region with the relatively larger contact angle value is defined as the hydrophobic region, and the surface region with the smaller contact angle value is defined as the hydrophilic region. In one embodiment, when a fine unevenness structure is formed on the surface of a hydrophobic substrate, the contact angle of the surface may become larger than that of the original flat substrate, and the surface may be changed to exhibit hydrophobicity. In this case, the surface region on which the fine unevenness structure is formed is defined as a hydrophobic region, and the original flat surface region is defined as a hydrophilic region.
[0014] In one embodiment of the cell culture component, a hydrophilic coating layer is formed on the hydrophilic region. The hydrophilic coating layer is a layer of a hydrophilic material that imparts hydrophilicity to the surface of the cell culture component. The hydrophilic material is not particularly limited as long as it has a hydrophilic functional group such as a hydroxyl group, a carbonyl group, or a carboxyl group. For example, a biocompatible polymer such as an MPC polymer having a phospholipid-like structure can be mentioned. A biocompatible polymer is preferable because it has low cytotoxicity and can suppress nonspecific adhesion of cells. The type of biocompatible polymer is not particularly limited, but examples thereof include dimethylpolysiloxane (PDMS), polyethylene glycol (PEG), oligoethylene glycol (OED), 2-methacryloyloxyethyl phosphorylcholine (MPC), poly(MPC-co-butyl methacrylate) (PMB), poly(MPC-co-dodecyl methacrylate) (PMD), and the like. As the hydrophilic material, commercially available products such as PREVELEX (registered trademark, manufactured by Nissan Chemical Industries, Ltd.), LIPIDURE (registered trademark, manufactured by NOF Corporation), RX-6-GB series, and RX-6-GA series (registered trademark, manufactured by Nippon Shokubai Co., Ltd.) may be used.
[0015] In one embodiment of the cell culture component, a hydrophilic coating layer is provided on a part of the surface of the base material to form a hydrophilic region. When a hydrophilic coating layer is provided, the surface of the hydrophilic region is the surface of the hydrophilic coating layer. The thickness of the hydrophilic coating layer provided in the hydrophilic region is preferably 0.005 to 0.500 μm, more preferably 0.005 to 0.300 μm, and even more preferably 0.010 to 0.100 μm. When the thickness of the hydrophilic coating layer is equal to or greater than the lower limit of the above-mentioned numerical range, the hydrophilic region tends to exhibit sufficient hydrophilicity. When the thickness of the hydrophilic coating layer is equal to or less than the upper limit of the above-mentioned numerical range, production costs tend to be reduced.
[0016] The thickness of the hydrophilic coating layer is measured as the shortest distance between the base surface of the substrate and the top surface of the hydrophilic coating layer. In this specification, the "base surface of the substrate" refers to the flat surface of the substrate itself when the surface of the substrate in the hydrophilic or hydrophobic region is flat. When the surface of the substrate in the hydrophilic or hydrophobic region has a fine uneven structure, the "base surface of the substrate" refers to the surface excluding all the convex parts from the surface, or the surface formed by filling all the concave parts of the surface.
[0017] In one embodiment of the cell culture component, a hydrophilic coating layer may be formed on both the hydrophilic region and the hydrophobic region. In this case, the hydrophilic coating layer is formed on a surface of a part of the plurality of convex portions or the plurality of concave portions of the microrelief structure region so that the microrelief structure region in the hydrophobic region exhibits adhesiveness to cells.
[0018] In one embodiment of the cell culture component, the ratio (S2 / (S1+S2)) of the area S2 of the hydrophobic regions to the sum of the area S1 of the hydrophilic regions and the area S2 of the hydrophobic regions in a plan view is 0.02 to 0.95, preferably 0.10 to 0.80, more preferably 0.30 to 0.70, and even more preferably 0.40 to 0.60. Since the ratio (S2 / (S1+S2)) is equal to or greater than the lower limit, differences in adhesiveness to cells occur between the hydrophilic regions and the hydrophobic regions, making it possible to control the orientation and adhesive regions of the cultured cells. Furthermore, the proportion of the hydrophobic regions is sufficient, and the cell culture component has excellent adhesiveness to the cultured cells. When the ratio (S2 / (S1+S2)) is equal to or less than the upper limit, a difference in adhesiveness to cells occurs between the hydrophilic and hydrophobic regions, making it possible to control the orientation and adhesive region of cultured cells.
[0019] The area S1 of the hydrophilic region and the area S2 of the hydrophobic region when the cell culture component is viewed in a plan view can be calculated as follows. The hydrophobic region can be distinguished from the hydrophilic region because it is colored with optical interference colors caused by the fine uneven structure described below. The areas are calculated by taking a low-magnification microscope image of the substrate and measuring the area S1 of the transparent hydrophilic region and the area S2 of the optical interference colored hydrophobic region. In one embodiment of the cell culture component, when there are two or more hydrophilic regions, the sum of the areas of the hydrophilic regions is defined as area S1. When there are two or more hydrophobic regions, the sum of the areas of the hydrophobic regions is defined as area S2.
[0020] In a plan view of a cell culture component according to an embodiment, the shapes of the hydrophilic and hydrophobic regions are not particularly limited. The shapes of the hydrophilic and hydrophobic regions may be, for example, circular, elliptical, polygonal, striped, or irregular, and are not limited to these examples. Furthermore, the number of hydrophilic regions and hydrophobic regions is not particularly limited, as long as at least one hydrophilic region and at least one hydrophobic region are formed.
[0021] The cell culture component according to one embodiment is for forming a cell sheet. A cell sheet is a thin-film sheet in which cells adhere to the cell culture component in the hydrophobic regions and to each other. The cell sheet may be a single layer of cells or a stack of multiple cells. The shape of the sheet is not particularly limited, and may be a single continuous sheet or multiple strip-shaped sheets.
[0022] There may be a height difference between the hydrophilic region and the hydrophobic region, or there may be no height difference. The "height difference between the hydrophilic region and the hydrophobic region" refers to the difference in height between the base surfaces of the hydrophilic region and the hydrophobic region of each substrate. The definition of the base surface is as described above.
[0023] In one embodiment of the cell culture component, a microrelief structure region including a plurality of convex portions or a plurality of concave portions is formed in at least a part of the hydrophobic region. In the microrelief structure region including a plurality of convex portions, a plurality of concave portions are formed between the plurality of convex portions, and in the microrelief structure region including a plurality of concave portions, continuous convex portions are formed between the plurality of concave portions. A microrelief structure (so-called moth-eye structure) containing multiple convex portions and multiple concave portions can be a structure that supports cells during culture. Therefore, the microrelief structure can function as a scaffold for cells like an extracellular matrix. Therefore, the microrelief structure region can exhibit relatively high cell adhesiveness among hydrophobic regions.
[0024] The microrelief structure region may be formed in at least a part of the hydrophobic region, or may be formed in the entire hydrophobic region. The proportion of the microrelief structure region in the hydrophobic region is not particularly limited, and can be changed depending on the type, morphology, and properties of the cultured cells. When a microrelief structure region is formed in a part of the hydrophobic region, the adhesiveness to cells may differ depending on the presence or absence of the microrelief structure region, even in the hydrophobic region. In this case, it becomes easier to selectively gather cells in the microrelief structure region even in the hydrophobic region, and it becomes easier to control the adhesive region and orientation of the cultured cells.
[0025] The shape of the microrelief structure region is not particularly limited and can be changed according to the type, morphology, and properties of the desired cultured cells. For example, when culturing cells that express functions based on the directionality and morphology in biological tissue, it is considered preferable to reproduce the directionality and morphology of the cells in the living body with the shape of the microrelief structure region. For example, when culturing cells such as cardiac muscle cells, skeletal muscle cells, and nerve cells, it is considered preferable to make the shape of the microrelief structure region into a band or stripe shape.
[0026] The shapes of the convex and concave portions of the fine concave-convex structure region are not particularly limited. The shapes of the convex and concave portions may be conical, cylindrical, truncated conical, pyramidal, truncated pyramidal, or bell-shaped, and are not limited to these exemplified shapes.
[0027] The average pitch between a plurality of convex portions or a plurality of concave portions is preferably from 50 nm to 5 μm, more preferably from 100 nm to 2 μm, and further preferably from 200 nm to 1 μm. When the average pitch is equal to or greater than the lower limit of the numerical range, the fine relief region is easily formed, improving industrial mass productivity. When the average pitch is equal to or less than the upper limit of the numerical range, cell adhesion to the fine relief region is further improved.
[0028] The average pitch between the multiple convex portions is determined as follows: The cell culture component is observed in plan view using a scanning electron microscope (SEM), 20 convex portions are randomly selected from multiple images in a magnification range in which 50 to 100 multiple convex portions are captured, and the arithmetic mean value of the shortest distance between the centers of the circumscribing ellipses of two adjacent convex portions in plan view is determined as the average pitch between the multiple convex portions.
[0029] The average pitch between the recesses is determined in the same manner as the average pitch between the protrusions, except that the shortest distance between the centers of the circumscribing ellipses of two adjacent recesses in a plan view is measured. Details and preferred aspects of the average pitch between the recesses are the same as those described for the average pitch between the protrusions.
[0030] The average diameter of the plurality of convex portions or the plurality of concave portions is preferably 50 nm to 5 μm, more preferably 100 nm to 2 μm, and even more preferably 200 nm to 1 μm. When the average diameter is equal to or greater than the lower limit of the aforementioned numerical range, the formation of a fine concave-convex structure region is facilitated, improving industrial mass productivity. When the average diameter is equal to or less than the upper limit of the aforementioned numerical range, the adhesiveness of cells to the fine concave-convex structure region is further improved.
[0031] The average diameter of the multiple protrusions is determined as follows: The cell culture component is observed in plan view using a scanning electron microscope (SEM), 20 protrusions are randomly selected from multiple images in a magnification range in which 50 to 100 multiple protrusions are captured, the major and minor axes of the circumscribing ellipses in plan view of the 20 protrusions are measured, and the geometric mean value of the major and minor axes is determined to be the average diameter of the multiple protrusions.
[0032] The average diameter of the plurality of recesses is determined in the same manner as the average diameter of the protrusions, except that the major and minor axes of the circumscribing ellipses in a plan view of the recesses are measured. Details and preferred aspects of the average diameter of the plurality of recesses are the same as those described for the average diameter of the plurality of protrusions.
[0033] In one embodiment of the cell culture component, a hydrophilic layer may be formed in the recesses between the multiple protrusions in the microrelief structure region in the hydrophobic region or in the bottoms of the multiple recesses. The hydrophilic layer is a layer of a hydrophilic material. Details and preferred aspects of the hydrophilic material are the same as those described for the hydrophilic coating layer. The hydrophilic material in the hydrophilic layer may be the same as or different from the hydrophilic material in the hydrophilic coating layer. When the hydrophilic material in the hydrophilic layer is the same as the hydrophilic material in the hydrophilic coating layer, industrial mass productivity is further improved.
[0034] In one embodiment of the cell culture component, a layer of an adhesion factor may be provided on the surface of the hydrophobic region to enhance adhesion of cells. Examples of the adhesion factor include extracellular matrices such as laminin, collagen, gelatin, fibronectin, polylysine (PDL, PLL), and hyaluronic acid, polymers, gels, and the like.
[0035] (Action and effect) In one embodiment of the cell culture component, at least one hydrophilic region and at least one hydrophobic region are formed on the surface of the substrate, and a microrelief structure region is formed in at least a part of the hydrophobic region. Therefore, cells adhere relatively more easily to the hydrophobic region than to the hydrophilic region, and among the hydrophobic regions, cells adhere more easily to the microrelief structure region. In addition, since the area ratio of the hydrophobic regions (S2 / (S1+S2)) is sufficiently large, the adhesion of cultured cells to the hydrophobic region is improved, and the hydrophobic region can be used as an adhesion region for cells. In addition, since the area ratio of the hydrophobic regions (S2 / (S1+S2)) is not excessively large, there is a sufficient difference in adhesiveness to cells between the hydrophilic regions, the hydrophobic regions, and the fine uneven structure regions. Therefore, according to one embodiment of the cell culture component, the orientation and adhesive region of the cultured cells can be controlled.
[0036] The cell culture device according to one embodiment relates to the cell culture devices (P1) and (P2) according to the following two embodiments. Cell culture component according to the first embodiment (P1): A cell culture component in which a hydrophobic region is located at a position with a relative difference in height with respect to a hydrophilic region in the thickness direction of the base material. Cell culture member according to a second embodiment (P2): a cell culture member in which the average height of a plurality of convex portions or the average depth of a plurality of concave portions in a microrelief structure region is 100 nm or more.
[0037] (Cell culture component (P1) according to the first embodiment) In the cell culture member (P1) according to the first embodiment, the hydrophobic region is located at a height difference relative to the hydrophilic region in the thickness direction of the base material. Here, the height position of the hydrophobic region is the height position of the base surface of the fine concave-convex structure region. Therefore, in the cell culture member (P1), the base surface of the fine concave-convex structure region is located at a higher or lower position than the surface of the hydrophilic region in the thickness direction of the base material.
[0038] According to the cell culture component (P1), the hydrophobic region is located at a position that is relatively different in height from the hydrophilic region in the thickness direction of the substrate. In addition, since the hydrophobic region of the substrate has a microrelief structure region formed therein, after the hydrophilicity imparting liquid is applied to the entire surface of the substrate during manufacture, the hydrophilicity imparting liquid migrates from the high position to the low position of the microrelief structure of the hydrophobic region and simultaneously migrates from the high position region to the low position region in order to minimize the surface tension (surface area). Therefore, when forming the hydrophilic and hydrophobic regions, a hydrophilic liquid can be applied to the entire surface of the substrate in an integrated manner, which eliminates the need to selectively apply the hydrophilic liquid to only specific regions, improving the productivity of the cell culture device and improving industrial mass production.
[0039] In the cell culture member (P1), the height difference between the hydrophilic region and the hydrophobic region is preferably 100 nm to 10 μm, more preferably 300 nm to 5 μm, and even more preferably 400 nm to 1 μm. When the height difference is equal to or greater than the lower limit of the above-mentioned range, the hydrophilicity imparting liquid is more likely to migrate from the higher region to the lower region during production. This makes it easier to produce the cell culture member, and the industrial mass productivity is more excellent. When the height difference is equal to or less than the upper limit of the above-mentioned range, the migration of cells to the hydrophobic region is less likely to be hindered.
[0040] In the microrelief structure region of the cell culture member (P1), the average height of the plurality of convex portions or the average depth of the plurality of concave portions is preferably 100 nm or more, more preferably 200 nm to 2 μm, and even more preferably 400 nm to 1 μm. When the average height of the plurality of convex portions or the average depth of the plurality of concave portions is equal to or more than the lower limit of the above-mentioned numerical range, the convex portions and concave portions of the microrelief structure region are easily formed, and industrial mass productivity is further improved. In addition, the hydrophilicity imparting liquid applied during production is more likely to flow from high positions to low positions of the microrelief structure in the hydrophobic region, and the thickness of the applied layer of the hydrophilicity imparting liquid becomes thinner at the tops of the convex portions and the base surfaces of the concave portions of the microrelief structure, making it easier for cells to adhere. On the other hand, when the average height of the plurality of convex portions or the average depth of the plurality of concave portions is equal to or less than the upper limit of the aforementioned numerical range, the adhesiveness of cells to the microrelief structure region is further improved.
[0041] The average height of the plurality of convex portions or the average depth of the plurality of concave portions is preferably greater than the thickness of the hydrophilic coating layer, because it is presumed that the tops of the plurality of convex portions or the base surfaces of the plurality of concave portions have a thinner layer of the hydrophilicity imparting liquid applied during production, making it easier for cells to adhere to them.
[0042] The average height of the plurality of convex portions and the average depth of the plurality of concave portions are obtained as follows. The cell culture component is cut perpendicularly to the surface at an arbitrary position by a microtome or CP processing (ion milling), and the cross section is observed by a scanning electron microscope (SEM). 20 convex portions or concave portions are randomly selected from a plurality of images in a magnification range in which 20 to 50 convex portions or concave portions are captured, and the height of the convex portion or the depth of the concave portion are measured, and the arithmetic mean value is taken as the average height of the plurality of convex portions or the average depth of the plurality of concave portions. Here, the height of each convex portion is measured as the shortest distance in the thickness direction of the substrate between the apex of the convex portion and the base surface of the fine concave-convex structure region, and the height of each concave portion is measured as the shortest distance in the thickness direction of the substrate between the apex of the concave portion and the surface of the substrate.
[0043] In the cell culture member (P1), the aspect ratio of the average height of the multiple convex portions to the average diameter of the multiple convex portions, or the aspect ratio of the average depth of the multiple concave portions to the average diameter of the multiple concave portions, is preferably 0.5 to 5.0, more preferably 0.6 to 4.0, and even more preferably 0.8 to 3.0. When the aspect ratio is equal to or greater than the lower limit of the numerical range, the adhesiveness of cells to the microrelief structure region is improved.When the aspect ratio is equal to or less than the upper limit of the numerical range, the microrelief structure region is easily formed, and industrial mass productivity is improved.
[0044] (Cell culture component according to the second embodiment (P2)) In the cell culture member (P2) according to the second embodiment, the average height of the plurality of convex portions or the average depth of the plurality of concave portions in the microrelief structure region is 100 nm or more. In the cell culture component (P2), due to the presence of the fine uneven structure region, after a hydrophilicity imparting liquid is applied to the entire surface of the base material during production, the hydrophilicity imparting liquid is less likely to remain on the surface of the hydrophobic region and easily flows into the hydrophilic region. In addition, in the cell culture member (P2), the average height of the plurality of convex portions or the average depth of the plurality of concave portions in the microrelief structure region is 100 nm or more. Therefore, the hydrophilicity imparting liquid in the coating layer flows from the high position to the low position in the microrelief structure in the hydrophobic region, so that the thickness of the coating layer of the hydrophilicity imparting liquid becomes thin at the tops of the plurality of convex portions or the base surfaces of the plurality of concave portions, making it easier for cells to adhere. Therefore, when forming the hydrophilic region and the hydrophobic region, a hydrophilicity imparting liquid can be applied to the entire surface of the base material in an integrated process, which improves the productivity of the cell culture device and provides excellent industrial mass production.
[0045] In the cell culture member (P2), the average height of the plurality of convex portions is preferably 100 nm to 2 μm, more preferably 200 nm to 2 μm, and even more preferably 400 nm to 1 μm. When the average height of the plurality of convex portions or the average depth of the plurality of concave portions is equal to or greater than the lower limit of the aforementioned numerical range, it is easier to form the convex portions and concave portions in the microrelief structure region, which is advantageous in that industrial mass productivity is further improved. On the other hand, when the average height of the plurality of convex portions or the average depth of the plurality of concave portions is equal to or less than the upper limit of the aforementioned numerical range, the adhesiveness of cells to the microrelief structure region is further improved.
[0046] In the cell culture member (P2), too, the average height of the plurality of convex portions or the average depth of the plurality of concave portions is preferably greater than the thickness of the hydrophilic coating layer, because it is presumed that the tops of the plurality of convex portions or the base surfaces of the plurality of concave portions have a thinner layer of the hydrophilicity-imparting liquid applied during production, making it easier for cells to adhere to them. In the cell culture member (P2), the average height of the plurality of convex portions or the average depth of the plurality of concave portions is determined in the same manner as in the cell culture member (P1). In addition, the details and preferred modes of the aspect ratio of the plurality of convex portions or the plurality of concave portions in the cell culture member (P2) are also the same as in the cell culture member (P1).
[0047] In the cell culture member (P2), the positional relationship between the hydrophobic region and the hydrophilic region in the height direction (i.e., the thickness direction of the substrate) is not particularly limited. That is, in the cell culture member (P2), the hydrophobic region may be located higher than the hydrophilic region in the thickness direction of the substrate, may be located lower than the hydrophilic region, or may be located at the same height as the hydrophilic region.
[0048] To further improve the industrial mass productivity of the cell culture component (P2), it is preferable that the hydrophobic region is located at a position with a difference in height from the hydrophilic region in the thickness direction of the substrate, because after the hydrophilicity imparting liquid is applied to the entire surface of the substrate during production, the hydrophilicity imparting liquid easily migrates from the high position region to the low position region, making production easier.
[0049] In the cell culture member (P2), the absolute value of the height difference between the hydrophilic region and the hydrophobic region is preferably 0 to 10 μm, more preferably 300 nm to 5 μm, and even more preferably 500 nm to 1 μm. When the height difference is within the above-mentioned numerical range, after the hydrophilicity imparting liquid is applied to the entire surface of the base material during production, the hydrophilicity imparting liquid is likely to migrate from the high-position region to the low-position region in order to minimize the surface tension (to minimize the surface area). This makes it easier to produce the cell culture member, and the industrial mass productivity is further improved. When the height difference is equal to or less than the upper limit of the above-mentioned numerical range, the migration of cells to the hydrophobic region is less likely to be hindered.
[0050] When the height difference between the hydrophilic region and the hydrophobic region is 0, the height of the surface of the substrate in the hydrophilic region coincides with the base surface of the microrelief region in the hydrophobic region. In this case, the height of the multiple convex portions in the microrelief region is preferably greater than the thickness of the hydrophilic coating layer.
[0051] (Example of embodiment) Hereinafter, a cell culture component according to an embodiment will be described by way of an example embodiment with reference to the drawings as appropriate. However, the cell culture component according to an embodiment is not limited to the following example embodiment. 1 to 14 are for the sake of convenience and may differ from the actual dimensions. In the following drawings, the same components are designated by the same reference numerals, and descriptions of overlapping components may be omitted.
[0052] [Embodiment Example 1] Fig. 1 is an enlarged plan view showing an example of a cell culture device, and Fig. 2 is a cross-sectional view taken along line II-II of Fig. 1. In a cell culture device 1A shown in FIGS. 1 and 2, a substrate 2 has a surface 2a on which hydrophilic regions 3A and hydrophobic regions 4A are formed.
[0053] In a plan view of the cell culture component 1A, the hydrophobic regions 4A are formed in a strip shape. A hydrophilic region 3A is formed outside each strip-shaped hydrophobic region, and a hydrophilic region 3A is also formed between the hydrophobic regions 4A.
[0054] Each of the hydrophilic regions 3A is covered with a hydrophilic coating layer 5A provided on the surface 2a of the substrate 2. Each of the hydrophilic regions 3A exhibits hydrophilicity due to this hydrophilic coating layer 5A. The thickness of the hydrophilic coating layer 5A is preferably from 0.005 to 0.500 μm, more preferably from 0.005 to 0.300 μm, and further preferably from 0.010 to 0.100 μm.
[0055] In the cell culture component 1A, the entire hydrophobic region 4A is a convex microrelief structure region 6A. The hydrophobic region 4A exhibits hydrophobicity due to the microrelief structure region 6A formed on the surface 2a of the base material 2. The fine concave-convex structure region 6A includes a plurality of cone-shaped convex portions 7A. A hydrophilic layer 8 is formed in concave portions 9A between the plurality of convex portions 7A of the fine concave-convex structure region 6A.
[0056] Due to the fine concave-convex structure in the fine concave-convex structure region 6A, the hydrophilicity imparting liquid used during production is less likely to remain on the surface of the fine concave-convex structure region 6A, and easily flows out into the hydrophilic region 3A. As a result, the coating layer of the hydrophilicity imparting liquid forms a thinner film on the tops of the multiple convex portions 7 A. Thereafter, when the hydrophilicity imparting liquid is solidified while partially filling the concave portions 9 A between the multiple convex portions 7 A, a hydrophilic layer 8 having a different thickness is formed between the tops of the multiple hydrophobic convex portions 7 A and the concave portions 9 A between the convex portions 7 A.
[0057] In this way, the hydrophilic layer 8 can be said to be the solidification of the hydrophilic imparting liquid that has been applied to the entire surface 2a of the substrate 2, and that has remained in the microrelief structure region 6A without migrating to the hydrophilic region 3A. The thickness of the hydrophilic layer 8 is smaller than the average height of the plurality of protrusions 7A. In the microrelief structure region 6A, the hydrophilic layer may not be attached to the upper 1 / 2 to 1 / 3 of the plurality of convex portions 7A and the plurality of concave portions 9A. The side surfaces of the convex portions 7A are thinly covered with the hydrophilic layer 8, and the hydrophilic layer 8 becomes thicker toward the bottoms of the concave portions 9A. The thickness of the hydrophilic layer 8 is preferably 80% or less, and more preferably 50% or less, of the average height of the plurality of convex portions 7A. The thickness of the hydrophilic layer 8 is the maximum thickness in the concave portions 9A.
[0058] Furthermore, the area ratio (S2 / (S1+S2)) of the hydrophobic region 4A is 0.02 to 0.95, preferably 0.10 to 0.80, more preferably 0.30 to 0.70, and even more preferably 0.40 to 0.60. Since the area ratio (S2 / (S1+S2)) is within the above range, a difference occurs in the adhesiveness of cells in the hydrophilic region 3A and the hydrophobic region 4A. As a result, it becomes possible to control the orientation and adhesive region of the cultured cells by controlling the elongation direction of the cultured cells with the hydrophobic region 4A. Additionally, in the cell culture member 1A, the cultured cells tend to gather on the surfaces of the protrusions 7 of the band-shaped microrelief structure region 6A. Therefore, the orientation of the cultured cells can be controlled to be band-shaped.
[0059] In the cell culture component 1A, the hydrophobic region 4A is located higher than the hydrophilic region 3A in the thickness direction of the substrate 2. Furthermore, since the microrelief structure region 6A is formed in the hydrophobic region of the substrate, after the hydrophilicity imparting liquid is applied to the entire surface of the substrate during production, the hydrophilicity imparting liquid migrates from the hydrophobic region 4A to the hydrophilic region 3A. Therefore, when forming the hydrophilic regions 3A and the hydrophobic regions 4A, a hydrophilicity imparting liquid can be applied to the entire surface 2a of the substrate 2 in an integrated process. As a result, productivity is improved, and the cell culture device 1A has excellent industrial mass productivity.
[0060] In the cell culture component 1A, the height difference h between the hydrophilic region 3A and the hydrophobic region 4A is preferably 100 nm to 10 μm, more preferably 300 nm to 5 μm, and even more preferably 500 nm to 1 μm. In the cell culture component 1A, the "height difference h" refers to the difference in height between the surface 2a of the base material 2 in the hydrophilic region 3A and the base surface of the microrelief structure region 6A in the hydrophobic region 4A.
[0061] The width W of the band-shaped microrelief structure region 6A is preferably 0.5 to 100 μm, more preferably 1 to 50 μm, and even more preferably 5 to 30 μm. When the width W is equal to or greater than the lower limit of the aforementioned numerical range, the band-shaped microrelief structure region 6A is easily formed, improving industrial mass productivity. When the width W is equal to or less than the upper limit of the aforementioned numerical range, the orientation of the cultured cells can be easily controlled.
[0062] In the cell culture component 1A, the average height of the plurality of convex portions 7A or the average depth of the plurality of concave portions 9A is preferably 100 nm or more, more preferably 200 nm to 2 μm, and even more preferably 400 nm to 1 μm.
[0063] [Embodiment Example 2] Fig. 3 is an enlarged plan view showing an example of the cell culture member, and Fig. 4 is a cross-sectional view taken along line IV-IV of Fig. 3. 3 and 4, a hydrophilic region 3B and a hydrophobic region 4B are formed on a surface 2a of a substrate 2. A hydrophilic region 3B is formed outside each of the hydrophobic regions 4B. In the cell culture component 1B, the "height difference h" refers to the difference in height between the surface 2a of the substrate 2 in the hydrophilic region 3B and the base surface of the microrelief structure region 6B in the hydrophobic region 4B.
[0064] In the cell culture component 1B, the area ratio (S2 / (S1+S2)) is also within a predetermined range, so that the extension direction of the cultured cells can be controlled by the hydrophobic region 4B, thereby controlling the orientation and adhesive region of the cultured cells. In addition, since the hydrophobic region 4B is located at a higher position than the hydrophilic region 3B in the thickness direction of the substrate 2 and the fine uneven structure region 6B is formed in the hydrophobic region 4B, after the hydrophilic imparting liquid is applied to the entire surface of the substrate during production, the hydrophilic imparting liquid migrates from the hydrophobic region 4B to the hydrophilic region 3B. Therefore, when forming the hydrophilic regions 3B and the hydrophobic regions 4B, a hydrophilicity imparting liquid can be applied to the entire surface 2a of the substrate 2 in an integrated process. As a result, productivity is improved, and the cell culture device 1B has excellent industrial mass productivity.
[0065] [Embodiment Example 3] Fig. 5 is an enlarged plan view showing an example of the cell culture member, and Fig. 6 is a cross-sectional view taken along line VI-VI of Fig. 5. The cell culture substrate 1C shown in FIGS. 5 and 6 differs from the cell culture substrate 1B in the following three points, and otherwise has a common configuration with the cell culture substrate 1B. The hydrophobic region 4C is located lower in the thickness direction of the substrate 2 than the surface 2a of the substrate 2. The average height of the plurality of convex portions 7C or the average depth of the plurality of concave portions 9C in the fine concave-convex structure region 6C is 100 nm or more. The thickness of the hydrophilic coating layer 5C is smaller than the thickness of the hydrophilic coating layer 5B (FIG. 4).
[0066] In the cell culture component 1C, the average height of the plurality of convex portions 7C or the average depth of the plurality of concave portions 9C in the microrelief structure region 6C is 100 nm or more. Therefore, the thickness of the coating layer of the hydrophilicity imparting liquid at the tops of the plurality of convex portions 7C during production is thin at the tops of the plurality of convex portions 7C. Therefore, when forming the hydrophilic and hydrophobic regions, an integrated process of coating the hydrophilicity imparting liquid over the entire surface of the substrate is possible. As a result, the productivity of the cell culture component is improved, and industrial mass production is excellent.
[0067] In the manufacture of the cell culture component 1C in which the hydrophobic region 4C is located lower in the thickness direction of the substrate 2 than the surface 2a of the substrate 2, the amount of hydrophilicity imparting liquid applied is less than that in the manufacture of the cell culture component 1B. As a result, the thickness of the hydrophilic coating layer 5C is smaller than that of the hydrophilic coating layer 5A.
[0068] In the cell culture component 1C, the height difference h between the hydrophilic region 3C and the hydrophobic region 4C is preferably 100 nm to 10 μm, more preferably 300 nm to 5 μm, and even more preferably 500 nm to 1 μm. In the cell culture component 1C, the "height difference h" refers to the difference in height between the surface 2a of the base material 2 in the hydrophilic region 3C and the base surface of the microrelief structure region 6C in the hydrophobic region 4C.
[0069] [Embodiment Example 4] Fig. 7 is an enlarged plan view showing a schematic diagram of one example of the cell culture member. Fig. 8 is a cross-sectional view taken along line VIII-VIII in Fig. 7. The cell culture member 1D shown in Figs. 7 and 8 differs from the cell culture member 1B in the following two points, but has a configuration in common with the cell culture member 1B in other points. The fine uneven structure region 6D is formed in the hydrophilic region 3D. The cell culture device 1D also provides the same effects as those of the cell culture device 1B.
[0070] The average height of the multiple convex portions 7D, the average depth of the concave portions 9D, the average diameter of the convex portions 7D and the concave portions 9D, and the average pitch of the microrelief structure region 6D may be the same as or different from those of the microrelief structure region 6B. However, the average height of the multiple convex portions 7D of the microrelief structure region 6D is smaller than the thickness of the hydrophilic coating layer 5D. Therefore, the microrelief structure region 6D is located inside the coating layer 5D.
[0071] In the cell culture component 1D, the height difference h between the hydrophilic region 3D and the hydrophobic region 4B is preferably 100 nm to 10 μm, more preferably 300 nm to 5 μm, and even more preferably 500 nm to 1 μm. In the cell culture component 1D, the "height difference h" refers to the difference in height between the base surface of the fine relief structure region 6D in the hydrophilic region 3D and the base surface of the fine relief structure region 6B in the hydrophobic region 4B.
[0072] The thickness of the hydrophilic coating layer 5D in the hydrophilic region 3D is preferably 0.005 to 1.000 μm, more preferably 0.050 to 0.700 μm, and further preferably 0.100 to 0.500 μm. The thickness of the hydrophilic coating layer 5D is the height between the surface of the hydrophilic region 3D and the base surface of the microrelief structure region 6D.
[0073] [Embodiment Example 5] Fig. 9 is an enlarged plan view showing an example of the cell culture member, and Fig. 10 is a cross-sectional view taken along line XX in Fig. 9. The cell culture substrate 1E shown in FIGS. 9 and 10 differs from the cell culture substrate 1A in the following two respects, and otherwise has a common configuration with the cell culture substrate 1A. A concave microrelief structure region 6E is formed. The hydrophilic layer 8 is formed between the multiple recesses 9E of the microrelief structure region 6E.
[0074] In the microrelief structure region 6E, no hydrophilic layer is attached to the upper 1 / 2 to 1 / 3 of the plurality of convex portions 7 and the plurality of concave portions 9E. In addition, the side surfaces of the convex portions are thinly covered with the hydrophilic layer 8, and the hydrophilic layer 8 becomes thicker toward the bottoms of the concave portions.
[0075] In the cell culture component 1E, the "height difference h" refers to the difference in height between the surface 2a of the substrate 2 in the hydrophilic region 3A and the base surface of the microrelief structure region 6E in the hydrophobic region 4E. The base surface of the microrelief structure region 6E is a surface formed by filling all of the multiple recesses 9E. The cell culture device 1E also provides the same effects as those of the cell culture device 1A.
[0076] [Embodiment Example 6] Fig. 11 is an enlarged plan view showing an example of the cell culture member, and Fig. 12 is a cross-sectional view taken along line XII-XII of Fig. 11. The cell culture component 1F shown in FIGS. 11 and 12 differs from the cell culture component 1B in the following two respects, and otherwise has a common configuration with the cell culture component 1B. The concave microrelief structure region 6F is formed. The hydrophilic layer 8 is formed between the multiple recesses 9F of the microrelief structure region 6F.
[0077] In the cell culture component 1F, the "height difference h" refers to the difference in height between the surface 2a of the substrate 2 in the hydrophilic region 3B and the base surface of the microrelief structure region 6F in the hydrophobic region 4F. The base surface of the microrelief structure region 6F is a surface formed by filling all of the multiple recesses 9F. The cell culture device 1F also provides the same effects as those of the cell culture device 1B.
[0078] [Embodiment Example 7] Fig. 13 is an enlarged plan view showing an example of the cell culture member, and Fig. 14 is a cross-sectional view taken along line XIV-XIV of Fig. 13. The cell culture substrate 1G shown in FIGS. 13 and 14 differs from the cell culture substrate 1D in the following two respects, and otherwise has a common configuration with the cell culture substrate 1D. The concave microrelief structure region 6G is formed. The hydrophilic layer 8 is formed between the multiple recesses 9 of the microrelief structure region 6G.
[0079] In the cell culture component 1G, the "height difference h" refers to the difference in height between the base surface of the microrelief structure region 6G in the hydrophilic region 3G and the base surface of the microrelief structure region 6G in the hydrophobic region 4G. The base surface of the microrelief structure region 6G is a surface formed by filling all of the multiple recesses 9G. The cell culture device 1G also provides the same effects as those of the cell culture device 1D.
[0080] Although not further illustrated, in other embodiment examples, the shape of the fine relief structure region 6 may be any geometric shape such as a polygonal shape or an irregular shape.
[0081] <Method of manufacturing cell culture components> Hereinafter, a cell culture component according to one embodiment will be described. The method for producing a cell culture component according to one embodiment is a method for producing a cell culture component having a substrate. Details and preferred aspects of the substrate are the same as those described in the section on the cell culture component according to one embodiment.
[0082] A method for producing a cell culture component according to one embodiment is characterized in that a hydrophilicity imparting liquid is applied to the entire surface of a substrate. When the applied layer of the hydrophilicity imparting liquid dries and solidifies, a hydrophilic coating layer is provided on the surface of the substrate, and the surface of the hydrophilic coating layer becomes the surface of the hydrophilic region. At this time, a hydrophilic layer is formed between the recesses between the multiple protrusions of the microrelief structure region of the hydrophobic region. The hydrophilicity imparting liquid is a liquid containing at least a hydrophilic material. The hydrophilicity imparting liquid may further contain components other than the hydrophilic material as long as the hydrophilicity can be imparted to the surface of the substrate. Details of the hydrophilic material are the same as those described in the section on the cell culture component according to one embodiment.
[0083] In the method for producing a cell culture component according to one embodiment, when the hydrophilicity imparting liquid is applied to the entire surface of the substrate, it is preferable to adjust the amount of the hydrophilicity imparting liquid applied so that the thickness of the applied layer of the hydrophilicity imparting liquid is smaller than the average height of the plurality of convex portions, because the thickness of the applied layer on the tops of the plurality of convex portions or the base surfaces of the plurality of concave portions becomes thinner.
[0084] The coating method is not particularly limited as long as the hydrophilicity-imparting liquid can be applied to the entire surface of the substrate. For example, spin coating, bar coating, slit coating, die coating, dip coating, spray coating, and various printing methods such as microcontact printing and screen printing can be used. However, the coating method is not limited to these examples. After application of the hydrophilicity-imparting liquid, the hydrophilicity-imparting liquid may be dried by natural drying or by heat drying, and the drying method is not particularly limited.
[0085] The method for producing a cell culture component according to one embodiment relates to the method for producing a cell culture component according to the following two embodiments. A method for producing a cell culture component according to a first embodiment: A method for producing a cell culture component (Q1), comprising the steps of: forming a hydrophilic region and a hydrophobic region on the surface of a substrate, the hydrophilic region being located at a height difference in the thickness direction of the substrate from the hydrophilic region; and forming a fine concave-convex structure region including a plurality of convex portions or a plurality of concave portions in the hydrophobic region; and then applying a hydrophilicity imparting liquid to the entire surface of the substrate. A method for producing a cell culture component according to a second embodiment: A method for producing a cell culture component (Q2), characterized in that the surface of a substrate is divided into a hydrophilic region and a hydrophobic region, and a fine concave-convex structure region including a plurality of convex portions having an average height of 100 nm or more is formed in the hydrophobic region; and then a hydrophilicity imparting liquid is applied to the entire surface of the substrate.
[0086] (Method for manufacturing a cell culture component according to the first embodiment) In the method for producing a cell culture component according to the first embodiment, a hydrophilic region and a hydrophobic region that is located at a position with a relative difference in height from the hydrophilic region in the thickness direction of the substrate are formed on the surface of the substrate, and a fine uneven structure region including multiple convex portions or multiple concave portions is formed in the hydrophobic region. Therefore, after applying a hydrophilicity imparting liquid to the entire surface of the substrate, the hydrophilicity imparting liquid migrates from the high-positioned region to the low-positioned region in the thickness direction. Therefore, when forming the hydrophilic region and the hydrophobic region, a hydrophilicity imparting liquid can be applied to the entire surface of the base material in an integrated process, which improves the productivity of the cell culture device and provides excellent industrial mass production.
[0087] In the method for producing the cell culture component according to the first embodiment, the height difference between the hydrophilic region and the hydrophobic region is preferably 100 nm to 10 μm in the thickness direction of the base material, more preferably 300 nm to 5 μm, and even more preferably 500 nm to 1 μm. When the height difference between the hydrophilic region and the hydrophobic region is equal to or greater than the lower limit of the above-mentioned numerical range, the hydrophilicity imparting liquid is more likely to migrate from the high-position region to the low-position region. This makes it easier to produce the cell culture component, and the industrial mass productivity is more excellent. When the height difference between the hydrophilic region and the hydrophobic region is equal to or less than the upper limit of the above-mentioned numerical range, the migration of cells to the hydrophobic region is less likely to be hindered when the cell culture component (Q1) is used for cell culture.
[0088] In the method for producing a cell culture component according to the first embodiment, the average height of the plurality of convex portions or the plurality of concave portions is preferably 100 nm or more, more preferably 200 nm to 2 μm, and even more preferably 400 nm to 1 μm. When the average height of the plurality of convex portions is equal to or more than the lower limit of the above-mentioned numerical range, the convex portions and the concave portions in the fine concave-convex structure region are easily formed, and industrial mass productivity is further improved. In addition, the hydrophilicity imparting liquid applied during production flows from a high position to a low position in the fine concave-convex structure in the hydrophobic region, so that the thickness of the applied layer of the hydrophilicity imparting liquid becomes thinner at the tops of the plurality of convex portions or the base surfaces of the plurality of concave portions, making it easier for cells to adhere. On the other hand, if the average height of the multiple convex portions is equal to or less than the upper limit of the aforementioned numerical range, the adhesiveness of cells to the microrelief structure region is further improved when the cell culture member (Q1) is used for cell culture.
[0089] There is no particular limitation on the method of forming a hydrophilic region and a hydrophobic region at a position where a height difference is provided in the thickness direction of the substrate from the hydrophilic region on the surface of the substrate. For example, a method is preferred in which an original plate (X1) is produced in which the positional relationship of the fine uneven structure on the surface and the height difference between the hydrophilic region and the hydrophobic region coincides with the cell culture member (Q1), and a mold (Y1) having an inverted surface shape and surface structure of the original plate (X1) is produced from the original plate (X1). This is because the mold (Y1) can be repeatedly used as a stamper to transfer the fine uneven structure and the height difference between the hydrophilic region and the hydrophobic region to the substrate, which makes it more suitable for industrial mass production. In this method, the division of the hydrophilic region and the hydrophobic region and the positional relationship in the thickness direction can be determined when the original plate (X1) is produced.
[0090] The method for producing the master (X1) is not particularly limited. A fine relief structure and height differences between hydrophilic and hydrophobic regions may be formed on the surface of a substrate (e.g., a Si substrate) by a method such as vapor phase etching, colloidal lithography, anodic oxidation, or interference exposure. The master (X1) may be produced using, for example, a monoparticulate film etching mask made of colloidal silica as described in JP 2009-034630 A. A fine relief structure can be formed uniformly and with high precision on the substrate by vapor-phase etching using the monoparticulate film etching mask.
[0091] The method for producing the mold (Y1) is not particularly limited. For example, a metal layer is formed on the surface of the original plate (X1) on which a fine uneven structure or the like is formed, and the fine structure or the like is transferred to the metal layer. The method for forming the metal layer includes, for example, a method in which a metal layer is provided on the surface of the master (X1) by electroless plating or metal vapor deposition, and the thickness of the metal layer is increased by electrolytic plating, but the method for forming the metal layer is not limited to these methods. The material of the metal layer is not particularly limited, and examples thereof include nickel, copper, gold, silver, platinum, titanium, cobalt, tin, zinc, chromium, a gold-cobalt alloy, a gold-nickel alloy, solder, a copper / nickel / chromium alloy, a tin-nickel alloy, a nickel-palladium alloy, and a nickel / cobalt / phosphorus alloy.
[0092] After the metal layer is formed, the metal layer is separated from the original plate (X1) to obtain a mold (Y1) having an inverted surface shape and surface structure of the original plate (X1). This mold (Y1) may be used for nanoimprinting, injection molding, or the like to form a hydrophilic region and a hydrophobic region located at a height difference in the thickness direction of the substrate from the hydrophilic region on the surface of the substrate, and a fine relief structure region including multiple convex portions or multiple concave portions in the hydrophobic region. Thereafter, a hydrophilicity imparting liquid is applied to the entire surface of the substrate, and the applied layer is dried and solidified to produce a cell culture member (Q1).
[0093] (Method for manufacturing a cell culture component according to the second embodiment) In the manufacturing method of the cell culture component according to the second embodiment, the surface of the substrate is divided into a hydrophilic region and a hydrophobic region, and a fine concave-convex structure region including a plurality of convex portions having an average height of 100 nm or more or a plurality of concave portions having an average depth of 100 nm or more is formed in the hydrophobic region.
[0094] The microrelief structure region includes a plurality of convex portions having an average height of 100 nm or more or a plurality of concave portions having an average depth of 100 nm or more. Therefore, the hydrophilicity imparting liquid in the coating layer flows from the higher positions to the lower positions of the microrelief structure in the hydrophobic region, and the thickness of the coating layer of the hydrophilicity imparting liquid becomes thinner at the tops of the plurality of convex portions or the base surfaces of the plurality of concave portions, facilitating cell adhesion. Therefore, when forming the hydrophilic region and the hydrophobic region, a hydrophilicity imparting liquid can be applied to the entire surface of the base material in an integrated process, which improves the productivity of the cell culture device and provides excellent industrial mass production. In the method for producing a cell culture component according to the second embodiment, the average height of the plurality of protrusions or the average depth of the plurality of recesses is preferably 100 nm or more, more preferably 200 nm to 2 μm, and even more preferably 400 nm to 1 μm.
[0095] There is no particular limitation on the method of dividing the surface of the substrate into a hydrophilic region and a hydrophobic region, and forming a microrelief structure region including a plurality of convex portions with an average height of 100 nm or more in the hydrophobic region. For example, a method is preferred in which a master (X2) whose surface microrelief structure matches that of the cell culture member (Q2) is produced, and a mold (Y2) having an inverted surface shape and surface structure of the master (X2) is produced from the master (X2). The details of the method for producing the master (X2) are the same as those described for the master (X1), except that the average height of the plurality of convex portions or the average depth of the plurality of concave portions is set to 100 nm or more.
[0096] In the second embodiment, a height difference may or may not be provided between the hydrophilic region and the hydrophobic region. If further improvement in industrial mass productivity is required, it is preferable to form the hydrophobic region at a position where there is a height difference relative to the hydrophilic region in the thickness direction of the substrate. In the second embodiment, the division of the hydrophilic region and the hydrophobic region and their positional relationship in the thickness direction can also be determined when the master (X2) is produced.
[0097] In the manufacturing method of the cell culture component according to the second embodiment, the absolute value of the height difference between the hydrophilic region and the hydrophobic region is preferably 0 to 10 μm in the thickness direction of the base material, more preferably 300 nm to 5 μm, and even more preferably 500 nm to 1 μm. When the height difference between the hydrophilic region and the hydrophobic region is equal to or greater than the lower limit of the above-mentioned numerical range, the hydrophilicity imparting liquid is likely to migrate from the higher position region to the lower position region. When the height difference between the hydrophilic region and the hydrophobic region is equal to or less than the upper limit of the above-mentioned numerical range, the migration of cells to the hydrophobic region is less likely to be hindered when the cell culture component (Q2) is used for cell culture.
[0098] When the difference in height between the hydrophilic and hydrophobic regions is set to zero in the thickness direction of the substrate, the thickness of the hydrophilic coating layer is adjusted to be smaller than the average height of the multiple convex portions when the hydrophilicity imparting liquid is applied to the entire surface of the substrate.
[0099] In the cell culture member (Q2), the hydrophilic region and the hydrophobic region may be positioned in any positional relationship in the thickness direction of the base material, and the hydrophobic region may be positioned lower than the hydrophilic region. Therefore, in manufacturing the cell culture member (Q2), the cell culture member (Q1) may be used as a mold (excluding the use of a cell culture member (Q1) in which the average height of a plurality of convex portions or the average depth of a plurality of concave portions is less than 100 nm). By using the cell culture member (Q1) as a mold, the surface shape and surface structure of the cell culture member (Q1) can be inverted and transferred to a substrate, and the surface of the substrate can be divided into hydrophilic and hydrophobic regions. In this case, the preparation of the master plate (X2) and mold (Y2) can be omitted, which is advantageous for industrial mass production. Other than that, the method of producing and using the mold (Y2) is the same as that explained for the mold (Y1).
[0100] The cell culture members (Q1) and (Q2) obtained by the manufacturing methods of the first and second embodiments described above, respectively, are different from each other and are also different from the cell culture members (P1) and cell culture members (P2) described above. However, the cell culture member (P1) can be suitably manufactured by the manufacturing method for a cell culture member according to the first embodiment. The cell culture member (P2) can be suitably manufactured by the manufacturing method for a cell culture member according to the second embodiment. When manufacturing the cell culture member (P1) and the cell culture member (P2), the area ratio (S2 / (S1+S2)) may be set within the range of 0.02 to 0.95 when preparing the master plate. In the following description of this specification, the term "a cell culture member according to an embodiment" includes at least the cell culture member (P1), the cell culture member (P2), the cell culture member (Q1), and the cell culture member (Q2).
[0101] In one embodiment of the cell culture component, a stimuli-responsive material may be applied to the surface of the cell culture component to facilitate detachment and recovery of cultured cells. As the stimuli-responsive material, a temperature-responsive polymer whose water affinity changes with temperature change is preferable, and poly-N-isopropylacrylamide (PIPAAm) is preferable.
[0102] In the cell culture component according to one embodiment, a stimuli-responsive material may be further applied to the substrate. In this case, the microrelief region may be formed after the stimuli-responsive material is applied to the substrate, or the stimuli-responsive material may be applied to the substrate after the microrelief region is formed. However, when the stimuli-responsive material is applied to the substrate after the microrelief region is formed, it is preferable to apply the stimuli-responsive material to the substrate before the hydrophilization treatment.
[0103] <Culture container> Since the culture vessel according to an embodiment includes the cell culture component according to an embodiment, the orientation of the cultured cells can be controlled and the culture vessel is also suitable for industrial mass production. An example of a culture vessel is one in which a cell culture member is provided on the inner wall surface of a vessel body that contains a culture solution containing cells. The inner wall surface of the vessel body is not particularly limited as long as it is a surface that can come into contact with the culture solution, and may be the bottom surface of the vessel body or the inner side surface of the vessel body. The cell culture member may be provided on the inner wall surface of the vessel body via an adhesive.
[0104] The shape and size of the culture vessel are not particularly limited. Examples of the culture vessel include a culture plate having one or more wells (holes), a dish (petri dish), a culture flask, a culture plate in the shape of a slide glass, and the like. The number of wells in the culture plate is not particularly limited, and is set according to the purpose of the cultured cells, the analytical device to be used, etc. The shape of the well in a plan view is not particularly limited. Examples include a perfect circle, an ellipse, a triangle, a square, a rectangle, and a pentagon. The shape of the bottom of the well is also not particularly limited. Examples include a flat bottom, a round bottom, and an uneven bottom.
[0105] The material of the culture vessel is not particularly limited. Examples of the material include polymeric materials, metal materials, and inorganic materials. Examples of polymeric resins include polystyrene, polyethylene, polypropylene, polycarbonate, polyester, polyisoprene, cycloolefin polymers, polyimide, polyamide, polyamideimide, (meth)acrylic resins, epoxy resins, and silicones. Examples of metal materials include stainless steel, copper, iron, nickel, aluminum, titanium, gold, silver, and platinum. Examples of inorganic materials include glass made of various inorganic mixtures, silicon oxide (quartz glass), aluminum oxide, titanium oxide, zirconium oxide, iron oxide, silicon nitride, and the like.
[0106] <Production method of cultured cells> In the method for producing cultured cells according to one embodiment, cells are cultured using the cell culture component according to one embodiment, and then the cultured cells are detached from the cell culture component. In the method for producing cultured cells, since the cells are cultured using the cell culture component according to the above-described one embodiment, the cells tend to gather in the hydrophobic region, and the orientation of the cultured cells can be controlled.
[0107] In the method for producing cultured cells, it is preferable to seed cells on the surface of the cell culture component on which hydrophobic and hydrophilic regions are formed, and allow the cells to adhere to the surface of the cell culture component. The cells are not particularly limited. Cells that can express functions based on orientation and morphology in vivo can be suitably selected. Examples include myoblasts, fibroblasts, cardiomyocytes, nerve cells, vascular endothelial cells, hepatocytes, osteoblasts, and chondrocytes. The cells used may be stem cells such as iPS cells, differentiated cells differentiated from stem cells, or tumor cells. The animal species of the cells, stem cells, differentiated cells, and tumor cells are not particularly limited, and examples thereof include mammals such as humans, pigs, mice, rats, rabbits, guinea pigs, hamsters, cows, horses, cats, dogs, sheep, and goats.
[0108] The culture conditions are not particularly limited and can be changed depending on the cell type, the purpose of the cultured cells, and the like. When the cultured cells become confluent, a cell detachment agent may be used for detaching the cells. The cell detachment agent is not particularly limited as long as it is a detachment agent that is generally used for cell culture.
[0109] <Cultured cells with cell culture components> A cultured cell with a cell culture component according to one embodiment includes: a cell culture component according to one embodiment; and cultured cells attached to a hydrophobic region of the cell culture component. The cultured cells attached to the cell culture member according to one embodiment are produced by culturing the cells in a state in which the cells are attached to the surface of the cell culture member using the above-mentioned cell culture member. Therefore, the cultured cells with controlled cell adhesion regions and orientation can be attached to the surface of the cell culture member. The type of cells is not particularly limited, and may be the same as those exemplified in the section on the method for producing cultured cells.
[0110] Although one embodiment has been described above, the present invention is not limited to the embodiment disclosed in this specification, and can be appropriately modified and implemented without departing from the gist of the present invention. The embodiment disclosed in this specification can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the gist of the invention. EXAMPLES
[0111] Hereinafter, one embodiment will be described in more detail using examples, but the present invention is not limited to these examples.
[0112] <Example 1> A monoparticle film etching mask made of colloidal silica was prepared on a Si wafer with a stripe pattern (width 10 μm, height 1 μm, photoresist layer arranged at 10 μm intervals) using a general photolithography method, by the method described in JP 2009-034630 A. A fine uneven structure was formed on a Si substrate by a gas-phase etching method using this monoparticle film etching mask, and the remaining photoresist was removed to prepare a convex Si surface microstructure original plate (1) in which multiple flat parts (which become hydrophilic regions) and multiple convex aggregate parts (which become hydrophobic regions) were alternately arranged in stripes. In the convex Si surface microstructure original plate (1), the distance of the stripe arrangement was 10 μm in the short axis direction of the flat parts and 10 μm in the short axis direction of the convex aggregate parts. In addition, the area ratio (S2 / (S1+S2)) of the convex aggregate parts which become hydrophobic regions was 0.5. The microrelief structure contained a plurality of convex portions each having an approximately conical shape, the average pitch of the plurality of convex portions was 600 nm, the average height of the plurality of convex portions was 500 nm, and the hydrophobic region was located lower than the hydrophilic region, with a height difference of 550 nm. Next, a concave Ni electroformed stamper (1) was produced from a convex Si surface microstructure original plate (1). Then, using the concave Ni electroformed stamper (1), a convex structure to be placed on the surface of a 150 μm thick polystyrene sheet was transferred by thermal nanoimprinting to produce a convex resin transfer member (1). Specifically, the structure surface of the concave Ni electroformed stamper (1) was placed opposite the surface of a 150 μm thick polystyrene sheet and set in the pressure unit of the nanoimprinting device. In this state, the temperature was increased, and pressure of 4 MPa was applied at 130° C. for 5 minutes. After 5 minutes, the pressure unit was cooled to room temperature, and the concave Ni electroformed stamper (1) was released from the surface of the polystyrene sheet. The obtained convex resin transfer member (1) was subjected to a hydrophilic treatment by a UV ozone method, and then coated with PREVELEX AP1 (registered trademark, manufactured by Nissan Chemical Industries, Ltd.) to obtain a convex cell culture member of Example 1 having a hydrophilic coating layer with an average thickness of 5 nm in the hydrophilic areas.
[0113] <Example 2> A convex structure serving as a mounting portion was transferred from the convex Si surface microstructure original plate (1) produced in Example 1 to a cycloolefin polymer film surface having a thickness of 188 μm by thermal nanoimprinting to produce a concave resin original plate (1). A convex Ni electroformed stamper (1R) was produced from the concave resin original plate (1). Thereafter, a concave cell culture component of Example 2 was produced by the same production method as in Example 1, except that the convex Ni electroformed stamper (1R) was used.
[0114] <Example 3> A monoparticle film etching mask made of colloidal silica was prepared on a Si wafer with a stripe pattern (width 10 μm, height 1 μm, photoresist layer arranged at 5 μm intervals) using a general photolithography method, by the method described in JP 2009-034630 A. A fine uneven structure was formed on a Si substrate by a gas phase etching method using this monoparticle film etching mask, and the remaining photoresist was removed to prepare a convex Si surface microstructure original plate (2) in which multiple flat parts (which become hydrophilic regions) and multiple convex aggregate parts (which become hydrophobic regions) were alternately arranged in stripes. In the convex Si surface microstructure original plate (2), the distance of the stripe arrangement was 10 μm in the short axis direction of the flat parts and 5 μm in the short axis direction of the convex aggregate parts. In addition, the area ratio (S2 / (S1+S2)) of the convex aggregate parts which become hydrophobic regions was 0.33. The microrelief structure contained a plurality of convex portions each having an approximately conical shape, with an average pitch of 600 nm and an average height of 500 nm. The hydrophobic region was located lower than the hydrophilic region, with a height difference of 550 nm. Next, a concave Ni electroformed stamper (2) was produced from the convex Si surface microstructure master plate (2). Thereafter, the convex cell culture component of Example 3 was produced by the same production method as in Example 1 using the concave Ni electroformed stamper (2).
[0115] <Example 4> A concave resin master plate (2) made of a cycloolefin polymer film having a thickness of 188 μm was produced from the convex Si surface microstructure master plate (2) produced in Example 3 in the same manner as in Example 2. A convex Ni electroformed stamper (2R) was produced from the concave resin master plate (2). Thereafter, a concave cell culture component of Example 4 was produced by the same production method as in Example 1, except that the convex Ni electroformed stamper (2R) was used.
[0116] <Example 5> A monoparticulate film etching mask made of colloidal silica was prepared on a Si wafer with a stripe pattern (a photoresist layer with a width of 10 μm and a height of 1 μm arranged at 10 μm intervals) using a general photolithography method, by the method described in JP 2009-034630 A. A fine uneven structure was formed on a Si substrate by a gas-phase etching method using this monoparticulate film etching mask, and unlike Example 1, the photoresist on which the fine uneven structure was formed was used as it was without being removed. A convex Si surface microstructure original plate (3) was prepared in which two types of convex aggregate parts with different shapes were alternately arranged in a stripe pattern. In the convex Si surface microstructure original plate (3), the distance of the stripe pattern arrangement was 10 μm in the minor axis direction of the flat part and 10 μm in the minor axis direction of the convex aggregate part. The fine uneven structure made of photoresist included a plurality of convex portions having a substantially conical shape, the average pitch of the plurality of convex portions was 600 nm, and the average height of the plurality of convex portions was 300 nm, while the fine uneven structure made of Si included a plurality of convex portions having a substantially conical shape, the average pitch of the plurality of convex portions was 600 nm, and the average height of the plurality of convex portions was 500 nm. The height difference between the two types of convex portion aggregates was 800 nm. Next, a concave Ni electroformed stamper (3) was produced from the convex Si surface microstructure master plate (3). Thereafter, the convex Ni electroformed stamper (3) was used to produce a convex cell culture component of Example 5 by the same production method as in Example 1, except that a hydrophilic coating layer having an average thickness of 300 nm was provided. In addition, the area ratio (S2 / (S1+S2)) of the convex aggregate portion that becomes the hydrophobic region was 0.5.
[0117] <Example 6> A concave resin master plate (2) made of a cycloolefin polymer film having a thickness of 188 μm was produced from the convex Si surface microstructure master plate (3) produced in Example 5 in the same manner as in Example 2. A convex Ni electroformed stamper (3R) was produced from the concave resin master plate (3). Thereafter, a concave cell culture component of Example 6 was produced by the same production method as in Example 5, except that the convex Ni electroformed stamper (3R) was used.
[0118] <Culture of mouse myoblast cells> Using the cell culture substrates of Examples 1 to 6, mouse-derived myoblasts (C2C12 cells) were cultured. 2 ) and C2C12 cells were cultured at 37°C in a 5% CO2 atmosphere using DMEM (Dulbecco's modified Eagle's medium) supplemented with 10% FBS (fetal bovine serum). Trypsin was used to collect the cells. After counting the number of cells using a hemocytometer, 7.6 × 10 4 A cell suspension was prepared at a concentration of cells / ml. The substrates of Examples 1 to 6 cut into 10 mm squares were placed on the bottom of a multi-well plate (24 holes) for cell culture. After washing the cell culture member with phosphate buffered saline, 0.5 ml of the prepared cell suspension was dispensed and cells were seeded. The multi-well plate seeded with the cells was cultured at 37°C in a 5% CO2 atmosphere for 48 hours. Furthermore, the cell culture members to which the cells had attached were fixed with paraformaldehyde, actin was stained with phalloidin, and cell nuclei were stained with DAPI, and two-dimensional images were obtained using an all-in-one fluorescence microscope (BZ-X800, Keyence Corporation). In both cell culture members, the cultured cells attached to the fine concave-convex structure regions, and the cultured cells extended in stripes along each of the fine concave-convex structures. On the other hand, almost no cultured cells attached to the surface of the flat hydrophilic region. Figure 15 shows the two-dimensional images of Example 1. It was confirmed that, according to the cell culture substrates of Examples 1 to 6, C2C12 cells adhere specifically to the microrelief structure region, making it possible to control the orientation of the cultured cells.
[0119] <Culture of human umbilical vein endothelial cells> Human umbilical vein endothelial cells (HUVEC) were cultured using the cell culture devices of Examples 1 to 6. The cells and dedicated medium were purchased from ScienCell Research Laboratories. Human umbilical vein endothelial cells were cultured in fibronectin-coated cell culture flasks (25 cm 2 ) were used and cultured in a dedicated medium at 37°C in a 5% CO2 atmosphere. The medium was changed every two days until the cells became confluent. Trypsin was used to recover the cells. After counting the number of cells using a hemocytometer, 2.8 × 10 4 A cell suspension was prepared at a concentration of cells / ml. The substrates of Examples 1 to 6 cut into 10 mm squares were placed on the bottom surface of a multi-well plate (24 holes) for cell culture, and fibronectin coating was performed for 1 hour. After removing the fibronectin and washing the substrate sheet with sterile water, 0.5 ml of the prepared cell suspension was dispensed and cells were seeded. The multi-well plate seeded with cells was cultured for 4 days at 37°C in a 5% CO2 atmosphere. In all cell culture components, the cultured cells adhered to the fine concave-convex structure region, and the cultured cells extended in a striped pattern along each of the fine concave-convex structures. On the other hand, almost no cultured cells adhered to the surface of the flat hydrophilic region. It was confirmed that, according to the cell culture substrates of Examples 1 to 6, human umbilical vein endothelial cells adhere specifically to the microrelief structure region, making it possible to control the orientation of the cultured cells. [Industrial Applicability]
[0120] According to one embodiment, there are provided a cell culture component that can control the orientation and adhesive area of cultured cells and has excellent industrial mass productivity; and a method for producing the same; a culture vessel equipped with the cell culture component; a method for producing cultured cells using the cell culture component; and cultured cells with the cell culture component equipped with the cell culture component. [Explanation of symbols]
[0121] Reference Signs List 1...cell culture member, 2...substrate, 3...hydrophilic region, 4...hydrophobic region, 5...hydrophilic coating layer, 6...fine uneven structure region, 7...convex portion, 8...hydrophilic layer, 9...concave portion.
Claims
1. A cell culture device having a substrate, A hydrophilic region and a hydrophobic region are formed on the surface of the substrate, the hydrophobic region is located at a position having a height difference relative to the hydrophilic region in the thickness direction of the base material, the hydrophilic region is a region whose entire surface is covered with a hydrophilic coating layer, the hydrophobic region is a region having a fine uneven structure including a plurality of convex portions or a plurality of concave portions, and at least the tops of the plurality of convex portions or the tops of convex portions between the plurality of concave portions are not covered with a hydrophilic coating layer; A cell culture component for forming a cell sheet, wherein a ratio of an area of the hydrophobic region to a sum of an area of the hydrophilic region and an area of the hydrophobic region when the cell culture component is viewed in a plane is 0.02 to 0.
95.
2. A cell culture component for forming a cell sheet as described in claim 1, wherein in addition to the hydrophilic region, all parts of the hydrophobic region other than the tops of the convex portions or the tops of the convex portions between the multiple concave portions are covered with a hydrophilic coating layer.
3. The cell culture component for forming a cell sheet according to claim 1 or 2, wherein an average height of the plurality of convex portions or an average depth of the plurality of concave portions is greater than a thickness of the hydrophilic coating layer.
4. A cell culture component for forming a cell sheet described in any one of claims 1 to 3, wherein the hydrophobic region is located at a relatively higher position than the hydrophilic region in the thickness direction of the substrate.
5. The cell culture member for forming a cell sheet according to any one of claims 1 to 4, wherein the base material comprises at least one resin selected from the group consisting of polyethylene terephthalate, triacetyl cellulose, polycarbonate, cycloolefin polymer, cycloolefin copolymer, acrylic resin, polystyrene, and dimethylpolysiloxane.
6. A method for producing a cell culture component having a substrate, comprising the steps of: A hydrophilic region and a hydrophobic region are formed on a surface of the substrate, the hydrophilic region being located at a position with a relative difference in height from the hydrophilic region in the thickness direction of the substrate, and a fine relief structure region including a plurality of convex portions or a plurality of concave portions is formed in the hydrophobic region; A method for producing a cell culture member for forming a cell sheet, characterized in that a hydrophilic coating layer is then formed on the entire surface except for the tops of the plurality of convex portions or the tops of the convex portions between the plurality of concave portions by applying a hydrophilic imparting liquid to the entire surface.
7. A method for manufacturing a cell culture component for forming a cell sheet as described in claim 6, wherein the hydrophilic liquid is applied to the entire surface at a thickness smaller than the average height of the multiple convex portions formed in the hydrophobic region or the average depth of the multiple concave portions.
8. A method for manufacturing a cell culture component for forming a cell sheet as described in claim 6 or 7, wherein the hydrophobic region is formed at a relatively higher position than the hydrophilic region in the thickness direction of the substrate.
9. A culture vessel comprising the cell culture component for forming a cell sheet according to any one of claims 1 to 5.
10. A method for producing cultured cells, comprising culturing cells using the cell culture component for forming a cell sheet according to any one of claims 1 to 5, and then detaching the cultured cells from the cell culture component.
11. A cell culture component for forming a cell sheet according to any one of claims 1 to 5, Cells attached to the cell culture member; A cultured cell with a cell culture member.
Citation Information
Patent Citations
Cell culture vessel, method for producing the same and cultured cell
JP2006325532A
Tool for recovering cell pattern controlled in orientation
JP2010119304A
Method for producing cell culture substrate, cell culture substrate, and method for producing cell sheet therewith
JP2013099272A
Method for producing substrate for cell culture
JP2016067314A
Cell sheet forming member, manufacturing method of cell sheet forming member, and manufacturing method of cell sheet
JP2019037220A