Weed control materials and weed control application methods
A combination of bark and alkaline soil, processed to maintain high C/N ratio and water permeability, addresses the limitations of existing weed control methods by ensuring long-term effectiveness, safety, and ecological sustainability.
Patent Information
- Application Number
- JP2021047738
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-22
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2041-03-22
AI Technical Summary
Existing weed control methods, such as manual weeding and herbicide spraying, are labor-intensive, pose safety risks, and have environmental concerns, while alternative methods like alkaline soil and wood chips face issues with sustainability, stability, and fire hazards.
A weed control material composed of bark and alkaline soil, where the bark is peeled from coniferous logs using a hydraulic barker to maintain a high C/N ratio and water permeability, and the alkaline soil is lime residue with a pH of 9.6 or higher, combined with a specific construction method that includes leveling, spreading, and inclining to ensure long-term effectiveness and safety.
The solution provides effective, long-lasting weed control with minimal environmental impact, maintains aesthetic appeal, and enhances fire safety by using materials that are inherently non-flammable and visually integrated with the landscape.
Smart Images

Figure 0007578282000001 
Figure 0007578282000002 
Figure 0007578282000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a weed-control material and a weed-control method using the same. [Background technology]
[0002] The proliferation of weeds and shrubs is unavoidable on the slopes and median strips of expressways, as well as in parks, vacant lots, embankments, riverbanks, etc., and this causes many problems, such as a deterioration in public safety due to poor visibility, the occurrence of pests, and the outbreak of wildfires. In addition, with the increase in power generation facilities using solar panels in recent years, suppressing the proliferation of weeds on such premises has also become an issue. To solve such problems, regular weeding work is required.
[0003] Traditionally, such weeding work has involved manual weeding and spraying herbicides. However, manual work requires a lot of labor and labor costs, and depending on the work location, it can be dangerous, among other drawbacks. In addition, spraying herbicides has been restricted in residential areas and around rivers due to concerns about the adverse effects on the human body caused by the herbicides flying or running off after spraying.
[0004] In recent years, in order to solve these shortcomings, various weed control and weed prevention measures have been proposed that are "nature-friendly" and aim to reduce the environmental burden. For example, the technology disclosed in Patent Document 1 is a method of adding alkaline soil to the area where weed prevention measures are to be implemented. In general, it is said that the hydrogen ion exponent (pH) suitable for plant growth is near neutral pH 6 to 7. Since alkaline soil mainly composed of limestone has a high pH value of pH 9 or higher, it is possible to sufficiently inhibit the growth of weeds in the implementation area where such soil has been added.
[0005] The technology disclosed in Patent Document 2 involves covering the weed control area with bags or mats filled with wood chips of cedar, cypress, etc. In general, the bark and leaves of coniferous trees such as cedar and cypress contain components that inhibit plant growth, so by carrying out such treatment, it is possible to prevent the growth of weeds in the weed control area. Furthermore, thinned wood and bark that would normally be considered industrial waste can be reused in this way, which is ecological and further reduces the environmental burden.
[0006] [Patent Document 1] JP 2014-201528 A [Patent Document 2] JP 2006-320244 A DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]
[0007] However, the technology shown in Patent Document 1 had a problem in that the alkaline soil added to the weed control area was likely to be scattered or washed away by strong winds or rain after construction, and there was a problem with the stable long-term sustainability of the weed control effect. Also, because the layer of added soil was exposed to the ground surface in the weed control area, the visually noticeable white alkaline soil was directly visible to the naked eye, and there was a problem with the landscape after construction.
[0008] On the other hand, the technology disclosed in Patent Document 2 uses wood chips as weed control material, which are themselves flammable, so there is a risk that a discarded cigarette or careless disposal while cooking at a campsite could spread to the weed control construction area and cause a large-scale wildfire or forest fire.
[0009] The present invention aims to dispel such concerns by providing a weed-control material that has a high weed-control effect that lasts for a long period of time, has an excellent appearance after application, and is also highly safe in terms of fire prevention, etc., and a weed-control application method using the same. [Means for solving the problem]
[0010] The weed-controlling material according to the first aspect of the present invention comprises: A weed-control material made of bark material and alkaline soil material, The bark material is mainly composed of bark that has been peeled off from a coniferous log by a hydraulic barker-type bark peeling device or by manual peeling, and does not contain any woody part of the log that would cause the material to rot or induce the germination of seeds that have flown in, has a carbon rate (C / N ratio) of 90% or more, a hydraulic conductivity of 0.1 or more, and fiber components with fiber lengths of 10 mm to 85 mm account for at least 50% of the entire material, and is dried in an environment of temperature of 10 degrees Celsius or more for five full days (40 hours of actual sunshine) or more for bark peeled off by manual peeling, and the moisture content of the material is reduced to 9.5% or less. The alkaline soil material is a lime residue material discharged when various lime products are produced from limestone, and is mainly composed of dolomite (CaMg(CO3)2), calcium carbonate (CaCO3), and silicon dioxide (SiO2), and is characterized by having a pH value of 9.6 or higher.
[0011] In addition, the weed control construction method according to the second aspect of the present invention comprises the steps of: The first work process is to level the construction area; A second work step of spreading the alkaline soil material according to claim 1 evenly in the work area where the first step has been completed; A third work step of applying a predetermined pressure to the entire area of the construction area where the second step is completed, to adjust the thickness of the alkaline soil material to 10 to 20 cm; A fourth work process of providing a slope of at least 5% in any short direction of the implementation area after the third process is completed; After the fourth step, the bark material according to claim 1 is applied to the upper layer of the applied area at a rate of 30 to 50 liters / m 2 a fifth work step of laying the wire in a ratio of After the fifth step, the alkaline soil material is applied to the construction area to a thickness of 1 to 3 mm / m. 2 A sixth work step of low density spraying at a rate of The present invention is characterized by comprising:
[0012] Further, a weed control method according to a third aspect of the present invention comprises: A first work step of digging down the existing soil in the construction area to a predetermined depth; A second work process in which unevenness is corrected for the construction area after the first process, and then a slope of at least 5% is provided in any short direction of the construction area; A third work process is to lay a drainage pipe with a permeable cylindrical side along the longitudinal direction of the roadbed surface at the lower part of the short-side slope of the construction area after the second process is completed; A fourth work step of spreading the alkaline soil material according to claim 1 evenly in the area where the third step has been completed; A fifth work step of applying a predetermined pressure to the entire area where the fourth work step is completed, to adjust the thickness of the alkaline soil material to 10 to 20 cm; After the fifth step, the bark material according to claim 1 is applied to the upper part of the application area at 30 to 50 liters / m 2 a sixth work step of laying the wire in a ratio of The alkaline soil is applied to the area where the sixth step has been completed to a thickness of 1 to 3 mm / m. 2 A seventh work step of low density spraying at a rate of The present invention is characterized by comprising: Effect of the Invention
[0013] By using the present invention, it is possible to realize an ecological weed-control material and weed-control application method that has a high weed-control effect that lasts for a long period of time, has a small environmental impact, does not harm the scenery of the application area, and is highly safe. BEST MODE FOR CARRYING OUT THEINVENTION
[0014] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Preferred embodiments of the present invention will now be described with reference to the accompanying drawings.
[0015] [1] Weed-control material based on the present invention The weed-control material of the present invention is mainly composed of two main materials: a bark material and an alkaline soil material. Each of these two materials will be described in detail below. [1-1] Bark material The bark material referred to in the present invention is the bark of coniferous trees such as cedar and cypress, and is mainly made from surplus wood discarded from sawmills and the like during sawing.
[0016] These bark materials are peeled off from the surface of logs when the logs are processed into products such as pillars and boards, and generally have little value as useful wood resources, so are usually discarded or incinerated as industrial waste. In light of the fact that such industrial waste can be effectively reused, the present invention can be said to be extremely ecological and contribute to reducing the environmental burden.
[0017] Incidentally, it is known that the bark of coniferous trees such as cedar and cypress contains a large amount of plant germination inhibitors such as ferruginol and tannin. Therefore, as shown in the above-mentioned Patent Document 2, these bark materials have been widely used as weed control materials. In addition, the bark of coniferous trees such as cedar and cypress contains a large amount of a component called lignin that inhibits the decay and decomposition of plant materials. However, if the woody part of the log (heartwood of wood) is mixed in a large amount with such bark material, it may start to decay and turn into compost due to the influence of decay fungi on the ground after it is spread as a weed control material, and may actually promote the growth and development of plants (weeds).
[0018] Incidentally, the rate at which composting progresses, that is, the ease with which the material decays and decomposes, can be objectively evaluated by the carbon ratio (C / N ratio) of the material. Here, the C / N ratio refers to the ratio of the amount of carbon [C] to the amount of nitrogen [N] in the material, and the higher this value, the more difficult it is to compost and the more stable the material can be maintained. Incidentally, the C / N ratio of compost made from ordinary chicken manure is about 6-10%, while that of bark from cedars and cypresses is said to be over 90%. However, as mentioned above, if the woody parts of the logs are mixed into the bark material, the C / N ratio may drop significantly.
[0019] In the present invention, in order to prevent the mixing of woody parts into the bark material as much as possible, a hydraulic barker is used as a bark peeling device (generally called a "barker") used when peeling bark from logs. Incidentally, barkers used when peeling bark from logs are broadly divided into, for example, ring barkers and cut barkers that peel bark from logs with mechanical blades, and hydraulic barkers that peel bark by water pressure.
[0020] Ring barkers and cut barkers use mechanical blades to scrape the surface of logs, so their structure is relatively simple and they are easy to maintain and use. However, the peeled layer becomes thick and the bark material peeled from the log contains a lot of woody parts of the log, which reduces the C / N ratio of the bark material after peeling from the log, making the bark material more susceptible to rot after peeling.
[0021] On the other hand, hydraulic barkers are specialized barkers that spray water at logs at high pressure in the form of a tornado-like jet to peel the bark as thinly as possible, and can quickly peel only the bark without damaging the logs. Hydraulic barkers are also called jet barkers due to the way they work.
[0022] Also, in order to prevent wood from being mixed into the bark material, the bark may be removed from the logs by hand rather than using mechanical power such as a barker. By performing such manual work, it is possible to reliably select and remove only the bark material without causing unnecessary damage to the logs.
[0023] In the present invention, in order to increase the C / N ratio of bark material used as a weed control material, only bark material peeled from logs such as cedar and cypress using a hydraulic barker or manual peeling is used. As a result, it is possible to maintain the C / N ratio of the bark material according to the present invention at 90% or more.
[0024] In addition, in the present invention, a predetermined standard is set for the length of the plant fibers contained in the bark material used, so as to maintain uniformity in the properties of the bark material. That is, in such bark materials, the fiber length has traditionally been controlled to approximately 30 mm or less throughout. However, such conventional fiber lengths cause the material to maintain a high moisture content, and when the bark material is laid on the ground, there is a risk that seeds that fly into the material will germinate faster. Therefore, in the present invention, the fiber length of at least 50% of the fibers in the bark material is limited to 10 mm to 85 mm.
[0025] Furthermore, when using bark material as a weed control material, it is necessary to process the material so that moisture does not accumulate within it, so that weed seeds that may fly in after installation in the weed control area do not take root on the surface of the bark material. In other words, the bark material needs to be kept well drained. The drainage of a material can generally be objectively evaluated based on the material's hydraulic conductivity. Here, hydraulic conductivity is defined as the speed at which water penetrates the material in one second (cm / sec), and the higher (faster) this value is, the better the material's hydraulic conductivity.
[0026] The permeability coefficient of normal black soil is about 7.0×10 -5 (cm / sec), which indicates that water permeates black soil at a speed of about 0.007 mm per second. Incidentally, the bark material used in the present invention has a hydraulic conductivity set to about 0.1 (cm / sec) or more. In other words, this indicates that water permeates the bark material used in the present invention at a speed of about 1 mm or more per second.
[0027] This is an extremely high value compared to the permeability coefficient of 0.016 (cm / sec) of fine sand (grain size 0.125 to 0.25 mm), which is generally considered to have high permeability (good drainage), and can be said to demonstrate the good drainage of the bark material used in the present invention.
[0028] In the present invention, in order to further increase the high hydraulic conductivity, the harvested bark material is subjected to the following drying and water-repellent treatment. (a) Bark material collected using a hydraulic barker-type bark peeling device After the bark material is harvested, the bark material is dried in the sun for at least five days (approximately 40 hours of actual sunlight) in an environment with a temperature of 10 degrees Celsius or higher. (b) Bark material collected by hand peeling After the bark material is harvested, the bark material is dried in the sun for at least three days (approximately 24 hours of actual sunlight) in an environment with a temperature of 10 degrees Celsius or higher.
[0029] In the present invention, the moisture content of the bark material is suppressed to 9.5% or less of the material mass by carrying out the drying and water-repellent treatment. When carrying out the drying and water-repellent treatment indoors, ultraviolet rays, infrared rays, or far-infrared rays may be irradiated onto the bark material from the respective heat ray irradiation devices for a period of time equivalent to the above-mentioned actual sunlight hours.
[0030] [1-2] Alkaline soil material Next, we will explain the alkaline soil material, which is another main ingredient of the weed-control material of the present invention. The alkaline soil material used in the present invention is a residual material discharged after producing various lime-applied products from limestone, and is usually discarded as industrial waste from manufacturing plants of various lime products.
[0031] Conventionally, these waste materials were treated in the same way as other industrial waste such as construction waste soil and demolition materials, and were only used for filling rivers and coasts, and for land development in industrial areas. The present invention is extremely ecological, as it opens the way to regenerating resources from such industrial waste.
[0032] These residue materials are mainly composed of dolomite (CaMg(CO3)2), calcium carbonate (CaCO3), and silicon dioxide (SiO2). The ratio of these components is not particularly limited, but in view of practical implementation, it is preferable that the ratio is about 70% dolomite, about 20% calcium carbonate, and about 10% silicon dioxide (all by mass).
[0033] In this embodiment, the alkaline soil material is as follows: Dolomite = 70% Calcium carbonate = 17% Silicon dioxide = 7% Other moisture etc.) = 6% (Both are based on calculations using X-ray diffraction (XRD) and X-ray fluorescence analysis (XRF).) In addition, it is preferable that the alkaline soil material has a pH value of 9.6 or higher.
[0034] [2] Weed control method according to the present invention Next, we will explain the weed control application method using the weed-control material of the present invention. There are two weed control application methods based on the present invention, and each will be explained below.
[0035] [2-1] First construction method The first application method is a method in which the weed-control material of the present invention is directly laid in the weed-control application area. A schematic cross-sectional view of a weed-control application area applied based on this application method is shown in the attached Figure 1, and an outline of the work process is shown in the flowchart of Figure 2.
[0036] As is clear from the flowchart, the construction method includes a first work step of leveling the construction area, a second work step of spreading the alkaline soil material according to the present invention evenly over the construction area after the first work step, a third work step of applying a predetermined pressure over the entire construction area after the second work step to adjust the thickness of the alkaline soil material to 10 to 20 cm, a fourth work step of providing a slope of at least 5% in any short direction of the construction area after the third work step, and a fourth work step of applying the bark material at a rate of 30 to 50 liters / m to the upper layer of the construction area after the fourth work step. 2 The fifth work step is to lay the above-mentioned alkaline soil material in the construction area after the fifth work step is completed at a thickness of 1 to 3 mm / m. 2 and a sixth work step of low-density spraying at a rate of 100%.
[0037] The contents of each work step of the construction method will be described in detail below. [2-1-1] 1st work process The first work process is to correct unevenness in the construction area, that is, to level the ground by filling in depressions in the ground and removing protrusions, etc. Specifically, this work is carried out using civil engineering machines such as bulldozers.
[0038] There are no particular limitations on the specifications and performance of the civil engineering machinery used in this process, but for example, a bulldozer with an operating weight of about 3.0 tons can be used. It goes without saying that the specifications and performance can be selected as desired depending on the actual construction conditions, such as the size of the construction area and the soil quality.
[0039] [2-1-2]Second work process The second work process involves distributing a predetermined amount of the alkaline soil material, which is one of the main components of the weed-control material of the present invention, in bags in the area where the first work process has been completed, and spreading it evenly in the area by using a backhoe (hydraulic excavator) or by hand. 3However, the performance of the civil engineering machine is not limited to this and can be selected arbitrarily depending on the construction conditions, etc.
[0040] In this work process, the alkaline soil material is evenly spread in the work area, and then the surface of the alkaline soil material in the work area is leveled. This leveling work is preferably carried out using a 0.1 ton roller (ground leveling machine) or a rake (a large rake for ground leveling work) in combination with human power.
[0041] [2-1-3] Third work process The third work step is a work step of applying pressure to the alkaline soil material that has been spread evenly in the work area and has had its surface leveled. That is, after the second step is completed, a predetermined pressure is applied to the alkaline soil material in the work area to compact it, and the thickness of the alkaline soil material in the work area is adjusted to be approximately uniform.
[0042] This step is preferably carried out repeatedly in the lengthwise and widthwise directions over the entire area of the construction area using a civil engineering machine such as a 2.5-ton to 4.0-ton roller (land leveling machine). By carrying out such a rolling operation, it is preferable to compress the alkaline soil material laid in the construction area to a thickness of about 10 to 20 cm.
[0043] [2-1-4] 4th work process The fourth work process is a process of providing a predetermined inclination in one of the short sides of the construction area after the completion of the third process. Usually, the shape of the weed control construction area provided on the roadside or riverbed is generally rectangular with the long side along the road or river and the short side perpendicular to the long side.
[0044] In this process, a predetermined inclination is provided in either one of the short sides. In this case, the inclination angle is preferably about 5%. Incidentally, this inclination angle is said to be the inclination value customarily used for the purpose of drainage of the construction area when leveling or constructing schoolyards such as ordinary elementary and junior high schools.
[0045] In addition, since this step uses the same civil engineering equipment as the rollers used in the previous step, this step may be carried out in conjunction with step 3. Also, when the construction area itself is a slope from the beginning, such as a road slope or a river dam, it is possible to omit this step by utilizing the natural slope of the land.
[0046] [2-1-5] 5th work process The fifth work step is a step of laying the aforementioned bark material, which is another main component of the weed-control material of the present invention, in the application area where the fourth step has been completed. That is, the aforementioned bark material is laid evenly on top of an alkaline soil material that has been almost uniformly leveled in the application area to a thickness of about 10 to 20 cm.
[0047] The aforementioned alkaline soil material, like various lime products, has a very noticeable white color. Therefore, by carrying out this process, the surface of the construction area will be completely covered with bark material with a calm brown color. This means that the color of the surface of the area where weed control work was carried out will not be too noticeable, and the scenery of the weed control work area after construction can be maintained in a good condition.
[0048] In addition, as mentioned above, the bark material based on the present invention has extremely good water permeability and water repellency, so rainwater that falls on the surface quickly penetrates and is absorbed by the lower layer of the bark material. Therefore, by carrying out this process, it is possible to prevent puddles of rainwater from forming on the surface of the construction area.
[0049] The amount of bark material to be put into the work area in this step is approximately 30 to 50 liters per square meter. The thickness of the bark material layer formed on the alkaline soil material is preferably about 1 / 4 of the thickness of the alkaline soil material layer. Incidentally, in an experimental work example of this work method, the thickness of the alkaline soil material layer in the third step was about 12 cm. And, in this step, the bark material was put into the work area at a rate of about 30 liters / m. 2The bark material was poured into the construction area at a ratio of 1:1 and spread evenly over the entire construction area. As a result, the thickness of the bark material layer in the construction area was approximately 3 cm.
[0050] [2-1-6] 6th work process The sixth work step is to spread the alkaline soil material described above at a low density on the construction area where the fifth work step has been completed. The purpose of this work step is to roughly and thinly cover the surface of the bark material layer laid in the previous work step with the alkaline soil material described above.
[0051] This allows the surface of the bark material to be roughly coated with particles of the non-flammable alkaline soil material, which can prevent, for example, floating sparks from discarded cigarette butts or bonfires from falling onto the surface of the bark material and spreading the fire. The amount of alkaline soil material to be spread in this process is preferably enough to roughly cover the surface of the work area to a thickness of just under 3 mm.
[0052] With this level of low-density spraying, the surface of the bark material is not completely covered by the sprayed alkaline soil material, and the brown color of the bark material remains strong on the surface of the weed control construction area, so there is no risk of the surface appearance of the construction area being marred by the conspicuous white color of the alkaline soil material.
[0053] [2-2] Second construction method The second construction method according to the present invention is a method in which the weed-control construction area is dug down to a predetermined depth and the weed-control material according to the present invention is laid therein. A schematic cross-sectional view of a weed-control construction area constructed based on this construction method is shown in the attached Figure 3, and an outline of the work process is shown in the flowchart of Figure 4.
[0054] As is clear from the flowchart, the construction method includes a first work step of digging down the existing soil in the construction area to a predetermined depth, a second work step of leveling the construction area after the first work step and then providing a slope of at least 5% in any short direction of the construction area, a third work step of laying a drainage pipe with a permeable cylindrical side along the long direction of the construction area at the bottom of the short direction slope of the construction area after the second work step is completed, a fourth work step of spreading the alkaline soil material evenly in the construction area after the third work step is completed, a fifth work step of applying a predetermined pressure over the entire construction area after the fourth work step is completed to adjust the thickness of the alkaline soil material to 10 to 20 cm, and a fifth work step of applying 30 to 50 liters / m of the bark material to the upper layer of the construction area after the fifth work step is completed. 2 and a sixth work step of laying the alkaline soil material in a thickness of 1 to 3 mm / m in the construction area where the sixth work step has been completed. 2 and a seventh work step of low-density spraying at a rate of 100%.
[0055] The contents of each work step of the construction method will be described in detail below. [2-2-1] 1st work process First, the first work step of this construction method is a work step of digging up the existing soil in the construction area to a specified depth. In this excavation work, the existing soil in the construction area is excavated to a depth of 20 to 40 cm using, for example, a 2.0 ton tractor. In general, the excavation depth is preferably 30 cm or less.
[0056] [2-2-2]Second work process The second work process involves leveling the bottom of the excavated existing soil (leveling the unevenness of the floor of the construction area) and creating a slope of at least 5% on either side of the construction area. This is to prevent rainwater from accumulating over the entire bottom of the excavated existing soil.
[0057] Weed control construction areas are generally rectangular in shape, with a long side and a short side perpendicular to the long side. For example, when carrying out weed control construction work in an area along a road, the long side of the weed control construction area will be an extremely long strip. Therefore, it is extremely reasonable to provide a slope toward one of the short sides of the bottom of the excavated construction area in terms of drainage at the bottom of the construction area.
[0058] In other words, rainwater, etc. that has permeated the alkaline soil material that will be laid in the construction area in the work process described below will be collected at the bottom of the slope on one of the short sides of the construction area due to the slope on the bottom surface, and rainwater, etc. will not accumulate on the entire bottom surface of the construction area. Incidentally, a slope angle of about 5% is a slope that is commonly used for the purpose of drainage of the construction area when leveling and constructing schoolyards for general elementary and junior high schools, etc.
[0059] [2-2-3] Third work process The third work step is a work step of laying a drainage pipe along the longitudinal direction of the construction area at the lower inclination of the short side of the construction area created in the second work step. In other words, it can be said to be a work of installing equipment to drain rainwater, etc., collected at the lower inclination of the short side of the construction area to the outside of the construction area. The shape and size of the drainage pipe used in this step are not particularly limited, but it is required that the cylindrical side surface has water permeability, and for example, a pipe with many water permeation holes on the cylindrical side surface is suitable.
[0060] [2-2-4] 4th work process The fourth work step is to distribute a predetermined amount of alkaline soil material, which is one of the main components of the weed-control material of the present invention, in a bag on the bottom of the application area and spread it evenly within the application area using a backhoe (hydraulic excavator) or by hand. 3 However, it goes without saying that the performance of the civil engineering machine is not limited to this and can be changed as appropriate according to the actual situation, such as the size of the construction area.
[0061] In this process, the alkaline soil material is evenly spread in the work area, and then the surface of the alkaline soil material in the work area is leveled. This leveling work is preferably carried out using a 0.1 ton roller (leveling machine) and manual labor using a rake, for example.
[0062] [2-2-5] 5th work process The fifth work step is a work step of applying pressure to the alkaline soil material that has been spread evenly in the work area and has completed the surface leveling work. That is, after the fourth work step is completed, a predetermined pressure is applied to the alkaline soil material in the work area to compact it and keep the thickness of the alkaline soil material at a uniform value.
[0063] This step is preferably carried out repeatedly in the vertical and horizontal directions over the entire area of the pavement using a civil engineering machine such as a 2.5 to 4.0 ton roller (land leveling machine). By carrying out such compaction work, it is preferable to compress the alkaline soil material laid in the construction area to a thickness of about 10 to 20 cm.
[0064] [2-2-6] 6th work process In the sixth work step, the bark material, which is another main component of the weed-control material of the present invention, is laid in the application area after the fifth work step has been completed. That is, the bark material is laid evenly on top of the alkaline soil material that has been leveled almost uniformly to a thickness of about 10 to 20 cm in the application area.
[0065] The amount of bark material to be put into the construction area is approximately 30 to 50 liters per square meter. The thickness of the bark material layer formed on the alkaline soil material put into the construction area is preferably approximately 1 / 4 the thickness of the alkaline soil material layer. For example, if the excavation depth of the existing soil in the first step is approximately 15 cm, and the thickness of the layer of alkaline soil material laid in the fifth step is approximately 12 cm, it is preferable to spread the bark material evenly over the entire construction area in that step, and make the thickness of the bark material layer approximately 3 cm.
[0066] [2-2-7] 7th work process The seventh work step is to spread the alkaline soil material mentioned above at a low density on the construction area where the sixth work step has been completed. The purpose of this work step is to cover the surface of the bark material layer laid in the previous work step with the alkaline soil material in a rough and thin layer.
[0067] This allows the surface of the bark material to be coarsely coated with particles of the non-flammable alkaline soil material, which can prevent, for example, floating sparks from discarded cigarette butts or bonfires from falling onto the surface of the bark material and spreading the fire. The amount of alkaline soil material to be spread in this process is preferably enough to roughly cover the treatment area to a depth of just under 3 mm.
[0068] With this level of low-density spraying, the surface of the bark material is not completely covered by the alkaline soil material, and the brown color of the bark material remains strong on the surface of the weed control construction area, so there is no risk of the appearance of the surface of the construction area being harmed by the conspicuous white-colored alkaline soil material.
[0069] [3] Test construction example according to the present invention [3-1] Overview of test construction Next, the results of the test construction according to the present invention will be explained based on the test photographs in Figures 5 to 7. The test construction area was a rectangular area measuring 1m x 1m, surrounded by a wooden frame, and the first construction method according to the present invention was carried out.
[0070] In both Figures 5 to 7, the right side of the photographs is the test construction area, where the alkaline soil material of the present invention was applied on top of the existing soil at a depth of about 12 cm, and bark material was applied on top of that at a rate of 30 liters / m 2The bark material layer was laid at a ratio of 1:1. The thickness of the bark material layer was about 3cm on average. In addition, the above-mentioned alkaline soil material was spread at a low density on the surface of the construction area to a thickness of just under 3mm. Also, in order to compare the weed control effect, normal red-black soil was added to the left side of the photo to a height of about 15cm, and the area was 1m2, the same as the test construction area on the right. 2 It is.
[0071] At the start of the test, several kinds of weed seeds (total 20g) were evenly scattered in both the test area on the right and the effect comparison area on the left in order to accelerate the verification of the results of the weed control effect. The details of the weed seeds scattered are as follows. Shiba Insect Grass: 2.5g Bidens : 1.5g Marubarukou: 3.5g Italian line glass: 12.5g These weeds are commonly found in vacant lots and riverbeds in the Kanto Plain.
[0072] [3-2] Follow-up observation after the start of the study [3-2-1] Five days after the start of the test (see the photo in Figure 5) Weed seeds have already germinated in the comparison area on the left, whereas no germinant growth was observed in the test area.
[0073] [3-2-2] 21 days after test construction (see photo in Figure 6) In the comparison area on the left, weeds proliferated, with some individual plants reaching a height of 20 cm. Meanwhile, in the test area on the right, some weed seeds were observed to germinate, but they all died within a few days.
[0074] [3-2-3] 53 days after test construction (see photo in Figure 7) In the comparison area on the left, weeds proliferated significantly, with some individual plants exceeding 30cm in height. On the other hand, in the test area on the right, no weeds were found to be growing normally after germination.
[0075] As explained above, the weed-control material and weed-control application method of the present invention can be expected to have an extremely effective weed-control effect by utilizing alkaline soil material and bark material that would otherwise be disposed of. In addition, the alkaline soil material and bark material laid in the application area have a high antibacterial effect, and the heat of vaporization from the bark material can also suppress the so-called heat island effect in urban areas.
[0076] In addition, because the bark material appears on the surface of the construction area, the natural landscape of the weed control construction area can be maintained compared to when weed control work was previously carried out using only alkaline soil material; furthermore, by scattering (dusting) the alkaline soil material at a low density on the surface of the bark material, its fire safety can be improved.
[0077] It goes without saying that the embodiments of the present invention are not limited to the examples described above. For example, the shape and arrangement of each part constituting each example, or the material, elapsed time, set temperature, etc., can be appropriately changed in accordance with the actual implementation without departing from the spirit of the present invention. [Industrial Applicability]
[0078] The configuration and method of the present invention described above can be used in the field of weed control treatment in areas such as vacant lots and roadsides. [Explanation of symbols]
[0079] 1. Alkaline soil material 2. Bark material 3. Water drainage pipe [Brief description of the drawings]
[0080] [Figure 1] FIG. 2 is a schematic cross-sectional view of a treatment area according to a first weed control treatment method according to the present invention. [Diagram 2]1 is a flowchart showing a first weed control method according to the present invention. [Diagram 3] FIG. 11 is a schematic cross-sectional view of a treatment area according to a second weed control method according to the present invention. [Figure 4] 4 is a flowchart showing a second weed control method according to the present invention. [Diagram 5] 1 is a test photograph showing a demonstration test of a weed control method based on the present invention (1). [Figure 6] 1 is a test photograph showing a demonstration test of a weed control method based on the present invention (2). [Figure 7] 1 is a test photograph showing a demonstration test of a weed control method based on the present invention (3).
Claims
1. A weed-control material comprising a bark material and an alkaline soil material, The bark material is mainly composed of bark that has been peeled off from a coniferous log by a hydraulic barker-type bark peeling device or by manual peeling, and does not contain any log wood that would induce decay of the material or germination of airborne seeds, has a carbon rate (C / N ratio) of 90% or more, a hydraulic conductivity of 0.1 or more, and fiber components with fiber lengths of 10 mm to 85 mm account for at least 50% of the entire material, and is dried in an environment of temperature of 10 degrees Celsius or higher for five full days (40 hours of actual sunshine) or more for bark peeled off by manual peeling, to reduce the moisture content in the material to 9.5% or less. The alkaline soil material is a lime residue material discharged when various lime products are produced from limestone, and is mainly dolomite (CaMg(CO 3 ) 2 ), calcium carbonate (CaCO 3 ), and silicon dioxide (SiO 2 ) and characterized in that it has a pH value of 9.6 or more.
2. A first work process for leveling the construction area; A second work step of spreading the alkaline soil material according to claim 1 evenly in the work area where the first work step has been completed; A third work step of applying a predetermined pressure to the entire area of the work area where the second work step is completed, to adjust the thickness of the alkaline soil material to 10 to 20 cm; A fourth work step of providing a slope of at least 5% in any short direction of the application area after the third step is completed; After the fourth step, the bark material according to claim 1 is applied to the upper layer of the applied area at a rate of 30 to 50 liters / m 2 A fifth work step of laying the wire in a ratio of After the fifth step, the alkaline soil material is applied to the work area to a thickness of 1 to 3 mm / m. 2 A sixth work step of low density spraying at a rate of A weed control method comprising the steps of:
3. A first work step of digging down existing soil in a construction area to a predetermined depth; A second work process in which unevenness is corrected for the construction area after the first process, and then a slope of at least 5% is provided in any short direction of the construction area; A third work step of laying a water drainage pipe having a permeable cylindrical side surface along the longitudinal direction of the construction area in the lower part of the inclined short side of the construction area after the second step is completed; A fourth work step of spreading the alkaline soil material according to claim 1 evenly on the area where the third step has been completed; A fifth work step of applying a predetermined pressure to the entire area where the fourth work step is completed, to adjust the thickness of the alkaline soil material to 10 to 20 cm; After the fifth step, the bark material according to claim 1 is applied to the upper layer of the applied area at a rate of 30 to 50 liters / m 2 A sixth work step of laying the wire in a ratio of The alkaline soil material is applied to the area where the sixth step has been completed to a thickness of 1 to 3 mm / m. 2 A seventh work step of low density spraying at a rate of A weed control method comprising the steps of:
Citation Information
Patent Citations
Mulch composition
EP3682729A1
Weed-preventing structure
JP1997074905A
Weed-preventing material subjected to flame retardant treatment, and method for installing fire- / weed-preventing construction
JP2004261149A
Mulching construction method
JP2012034613A
Flame retardant organic porous composite and production method thereof
JP2012080801A