Method for manufacturing nitride semiconductor device
The method addresses nitrogen loss and void formation in gallium nitride semiconductor layers by forming a rough surface and using an aluminum-containing cap layer to fill voids with aluminum gallium nitride, ensuring effective impurity activation and layer integrity.
Patent Information
- Application Number
- JP2021056017
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-29
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2041-03-29
AI Technical Summary
Existing methods for activating impurities in gallium nitride-based semiconductor layers face issues such as nitrogen loss and pit formation during high-temperature annealing, which can be exacerbated by voids in the cap layer.
A manufacturing method involving ion implantation, rough surface region formation, and cap layer application with aluminum-containing nitride or oxide, followed by annealing in an ammonia atmosphere to fill voids with aluminum gallium nitride, preventing nitrogen escape.
Activates impurities while effectively suppressing nitrogen loss and void formation, maintaining the integrity of the gallium nitride semiconductor layer.
Smart Images

Figure 0007578525000001 
Figure 0007578525000002 
Figure 0007578525000003
Abstract
Description
[Technical field]
[0001] The technology disclosed in this specification relates to a method for manufacturing a nitride semiconductor device including a gallium nitride based semiconductor layer. [Background technology]
[0002] Development of nitride semiconductor devices having gallium nitride semiconductor layers is underway. To manufacture this type of nitride semiconductor device, a technique is required to implant impurity ions into the gallium nitride semiconductor layer and activate the implanted impurity ions to form an n-type or p-type diffusion region.
[0003] In order to activate the impurity ions implanted into the gallium nitride semiconductor layer, a high-temperature annealing process is required. For example, the p-type impurity magnesium requires an annealing process at about 1400° C. or higher. However, it is known that such a high-temperature annealing process decomposes the gallium nitride semiconductor layer, causing nitrogen loss from the surface of the gallium nitride semiconductor layer, and forming pits in the gallium nitride semiconductor layer.
[0004] Patent Document 1 proposes a technique for suppressing the formation of pits by performing a high-temperature annealing process under an atmospheric pressure equal to or higher than the saturated vapor pressure of a gallium nitride-based semiconductor layer.
[0005] Patent Document 2 discloses a technique for forming a cap layer on the surface of a gallium nitride semiconductor layer. The formation of such a cap layer suppresses nitrogen loss from the surface of the gallium nitride semiconductor layer, thereby suppressing the formation of pits. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2020-155469 A [Patent Document 2] JP 2018-010970 A Summary of the Invention [Problem to be solved by the invention]
[0007] When a cap layer is formed, voids may be formed in the cap layer. When such voids are formed, nitrogen escape from the surface of the gallium nitride semiconductor layer is promoted through the voids. The present specification aims to provide a technology capable of activating impurities ion-implanted into a gallium nitride semiconductor layer while suppressing nitrogen escape from the voids in the cap layer. [Means for solving the problem]
[0008] The method for manufacturing a nitride semiconductor device disclosed in this specification can include an ion implantation step (S1) of ion implanting impurities into at least a portion of a region of at least one of the main surfaces (10a) of a gallium nitride semiconductor layer (10), a roughened region formation step (S2) of forming a roughened region (12) by increasing the surface roughness of at least a portion of the surface of the gallium nitride semiconductor layer, a cap layer formation step (S4) of forming a cap layer (30) on at least the one of the main surfaces of the gallium nitride semiconductor layer while exposing the roughened region, and an annealing step (S5) of annealing the gallium nitride semiconductor layer in an ammonia atmosphere. The cap layer is a nitride or oxide containing aluminum.
[0009] According to the above manufacturing method, gallium is released from the rough surface region in the annealing step. If voids are formed in the cap layer, the released gallium reacts with the nitrogen contained in ammonia and the aluminum contained in the cap layer, and aluminum gallium nitride (AlGaN) is filled in the voids. In this way, even if voids are formed in the cap layer, gallium is preferentially released from the rough surface region, thereby preventing nitrogen from escaping from the first main surface of the gallium nitride semiconductor layer through the voids. As a result, according to the above manufacturing method, it is possible to activate the impurity ions implanted into the gallium nitride semiconductor layer while preventing nitrogen from escaping from the voids in the cap layer. [Brief description of the drawings]
[0010] [Figure 1] 1 shows a flowchart of a part of a method for manufacturing a nitride semiconductor device. [Diagram 2] 1A and 1B are schematic cross-sectional views of a main portion of a gallium nitride based semiconductor layer in a process of a method for manufacturing a nitride semiconductor device. [Diagram 3] 1A and 1B are schematic cross-sectional views of a main portion of a gallium nitride based semiconductor layer in a process of a method for manufacturing a nitride semiconductor device. [Figure 4] 1A and 1B are schematic cross-sectional views of a main portion of a gallium nitride based semiconductor layer in a process of a method for manufacturing a nitride semiconductor device. [Diagram 5] 1A and 1B are schematic cross-sectional views of a main portion of a gallium nitride based semiconductor layer in a process of a method for manufacturing a nitride semiconductor device. [Figure 6] 1A and 1B are schematic cross-sectional views of a main portion of a gallium nitride based semiconductor layer in a process of a method for manufacturing a nitride semiconductor device. [Figure 7] 1A and 1B are schematic cross-sectional views of a main portion of a gallium nitride based semiconductor layer in a process of a method for manufacturing a nitride semiconductor device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, a method for manufacturing a nitride semiconductor device including a gallium nitride based semiconductor layer will be described with reference to the drawings. Below, the steps from the ion implantation step to the annealing step for diffusing the implanted impurities among the steps for manufacturing a nitride semiconductor device will be described. For the steps other than these among the steps for manufacturing a nitride semiconductor device, known manufacturing methods can be used.
[0012] A flowchart of a portion of a method for manufacturing a nitride semiconductor device is shown in Fig. 1. Figs. 2 to 7 are schematic cross-sectional views of essential parts of a gallium nitride based semiconductor layer in the manufacturing process corresponding to the flowchart in Fig. 1.
[0013] As shown in FIG. 2, the gallium nitride based semiconductor layer 10 is divided into an element region 10A and a non-element region 10B. The element region 10A is a region in which a functional structure for performing an electrical function is formed. In the element region 10A, a functional structure for performing, for example, a switching function is formed. Examples of such a functional structure include a type of functional structure called a MISFET (Metal Insulator Semiconductor Field Effect Transistor) or a MOSFET (Metal Oxide Semiconductor Field Effect Transistor). The non-element region 10B is a region in which a functional structure for performing an electrical function is not formed. The non-element region 10B is not particularly limited, and may be, for example, a region corresponding to a scribe line to be removed by dicing.
[0014] The gallium nitride based semiconductor layer 10 is a semiconductor layer made of a III-V group compound semiconductor containing nitrogen and gallium. The gallium nitride based semiconductor layer 10 is not particularly limited, but may be, for example, gallium nitride (GaN), aluminum gallium nitride (AlGaN), or indium gallium nitride (InGaN).
[0015] The gallium nitride based semiconductor layer 10 has a first main surface 10a and a second main surface 10b. When a functional structure of a MISFET or MOSFET is formed in the element region 10A of the gallium nitride based semiconductor layer 10, an insulated gate structure is formed on the first main surface 10a of the gallium nitride based semiconductor layer 10. In this specification, the surface of the gallium nitride based semiconductor layer 10 is used to include the first main surface 10a and the second main surface 10b, as well as the side surface between the first main surface 10a and the second main surface 10b.
[0016] As shown in Fig. 3, a mask 20 is formed by photolithography to cover a part of the first main surface 10a of the gallium nitride semiconductor layer 10. The mask 20 has an opening through which at least a part of the first main surface 10a of the element region 10A is exposed. Next, an ion implantation step is performed by ion implantation to implant impurities through the opening of the mask 20 toward the first main surface 10a of the gallium nitride semiconductor layer 10 (S1 in Fig. 1). As a result, an ion implantation region 22 is formed in the gallium nitride semiconductor layer 10. The impurities to be ion implanted are not particularly limited, but may be, for example, magnesium. After the ion implantation step is performed, the mask 20 is removed.
[0017] Next, as shown in Fig. 4, a rough surface region forming step is carried out to form a rough surface region 12 by increasing the surface roughness of at least a part of the first main surface 10a of the non-element region 10B (S2 in Fig. 1). The rough surface region 12 is not particularly limited, but may be formed by using a dry etching technique, for example. Even if such a rough surface region 12 is formed, since the rough surface region 12 is located in the non-element region 10B, it is possible to prevent adverse effects on the electrical characteristics of the functional structure formed in the element region 10A.
[0018] Next, as shown in Fig. 5, a cap layer deposition step is performed in which a cap layer 30 is deposited so as to cover the surface of the gallium nitride semiconductor layer 10 while exposing the rough surface region 12 (S3 in Fig. 1). In this example, the cap layer 30 is deposited on the first main surface 10a and the second main surface 10b, and further on the side surface between the first main surface 10a and the second main surface 10b, and only the rough surface region 12 is exposed from the opening of the cap layer 30. Alternatively, the cap layer 30 may be deposited only on the first main surface 10a on the side where the ion implantation region 22 is formed. As shown in Fig. 5, unintended voids 30a are formed in the cap layer 30.
[0019] The cap layer 30 is an aluminum-containing nitride or oxide. The cap layer 30 is a material having a higher melting point than the gallium nitride semiconductor layer 10, and is used to suppress nitrogen loss from the gallium nitride semiconductor layer 10 in the annealing step described below. The cap layer 30 is not particularly limited, and may be, for example, aluminum nitride (AlN) or aluminum oxide (Al2O3). The cap layer 30 is formed on the surface of the gallium nitride semiconductor layer 10 by using a deposition technique. The deposition technique is not particularly limited, and may be, for example, atomic layer deposition.
[0020] 4 and the cap layer deposition step shown in Fig. 5 may be performed in the reverse order from the example described above. For example, the cap layer 30 may be deposited in a state where at least a portion of the first main surface 10a of the non-element region 10B is exposed, and then the surface roughness of the exposed region may be increased to form the rough surface region 12.
[0021] 6, an annealing step is performed in which the gallium nitride based semiconductor layer 10 is annealed in an ammonia atmosphere (S4 in FIG. 1). This makes it possible to form a diffusion region 14 in the gallium nitride based semiconductor layer 10.
[0022] This annealing step is performed in an ammonia atmosphere. Therefore, the annealing step is performed under a high nitrogen partial pressure, so that nitrogen escape from the surface of the gallium nitride semiconductor layer 10 is suppressed. Furthermore, in the manufacturing method disclosed in this specification, a rough surface region 12 is formed on a part of the surface of the gallium nitride semiconductor layer 10, and the rough surface region 12 is exposed without being covered by the cap layer 30. Therefore, in the annealing step, gallium is released from the rough surface region 12. The released gallium reacts with the nitrogen contained in the ammonia and the aluminum contained in the cap layer 30, and aluminum gallium nitride (AlGaN) is filled in the voids 30a of the cap layer 30. Thus, in the manufacturing method disclosed in this specification, even if the voids 30a are formed in the cap layer 30, gallium is preferentially released from the rough surface region 12, so that the voids 30a are filled with aluminum gallium nitride (AlGaN), so that nitrogen is suppressed from escaping from the surface of the gallium nitride semiconductor layer 10 through the voids 30a. As a result, according to the manufacturing method disclosed in this specification, it is possible to activate the impurities ion-implanted into the gallium nitride based semiconductor layer 10 while suppressing loss of nitrogen from the voids 30a of the cap layer 30.
[0023] In the manufacturing method described above, the rough surface region 12 is formed in a portion of the first main surface 10a of the non-element region 10a. As shown in Fig. 7, the rough surface region 12 may be formed in a portion of the second main surface 10a of the non-element region 10a. Alternatively, the rough surface region 12 may be formed on a side surface of the gallium nitride based semiconductor layer 10.
[0024] The features of the technology disclosed in this specification are summarized below. Note that the technical elements described below are independent technical elements that exhibit technical usefulness alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing.
[0025] The method for manufacturing a nitride semiconductor device disclosed in this specification may include an ion implantation step of ion-implanting impurities toward at least a part of a region of at least one of the main surfaces of a gallium nitride semiconductor layer, a rough surface region forming step of forming a rough surface region by increasing the surface roughness of at least a part of the surface of the gallium nitride semiconductor layer, a cap layer forming step of forming a cap layer on at least the one of the main surfaces of the gallium nitride semiconductor layer while exposing the rough surface region, and an annealing step of annealing the gallium nitride semiconductor layer in an ammonia atmosphere. The cap layer is a nitride or oxide containing aluminum. Either the rough surface region forming step or the cap layer forming step may be performed first. The cap layer may be aluminum nitride (AlN) or aluminum oxide (Al2O3).
[0026] The gallium nitride based semiconductor layer may be partitioned into an element region and a non-element region. In this case, the region into which the impurities are ion-implanted in the ion implantation step may be located in the element region. Furthermore, the rough surface region formed in the rough surface region formation step may be located in the non-element region. Since the rough surface region is formed in the non-element region, it is possible to prevent adverse effects on electrical characteristics of a functional structure formed in the element region.
[0027] The non-element region may be a region corresponding to a scribe line of the gallium nitride based semiconductor layer.
[0028] In the rough surface region forming step, the rough surface region may be formed by utilizing a dry etching technique.
[0029] Although specific examples of the present invention have been described above in detail, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and variations of the specific examples exemplified above. Furthermore, the technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. Furthermore, the technology exemplified in this specification or drawings can achieve multiple objectives simultaneously, and achieving one of these objectives is itself technically useful. [Explanation of symbols]
[0030] 10: gallium nitride semiconductor layer, 10A: element region, 10B: non-element region, 12: rough surface region, 14: diffusion region, 20: mask, 22: ion implantation region, 30: cap layer, 30a: gap
Claims
1. A method for manufacturing a nitride semiconductor device, comprising the steps of: An ion implantation step (S1) of ion-implanting impurities into at least a partial region of at least one of the main surfaces (10a) of the gallium nitride based semiconductor layer (10); a roughened region forming step (S2) of forming a roughened region (12) by increasing the surface roughness of at least a part of the surface of the gallium nitride based semiconductor layer; a cap layer deposition step (S4) of depositing a cap layer (30) on at least the one main surface of the gallium nitride based semiconductor layer while exposing the rough surface region; and an annealing step (S5) of annealing the gallium nitride based semiconductor layer in an ammonia atmosphere, The method of manufacturing wherein the cap layer is an aluminum-containing nitride or oxide.
2. The cap layer may be aluminum nitride (AlN) or aluminum oxide (Al 2 O 3 2. The method according to claim 1 , wherein
3. The gallium nitride based semiconductor layer is partitioned into an element region (10A) and a non-element region (10B), a region into which the impurity is ion-implanted in the ion implantation step is located in the element region; The manufacturing method according to claim 1 , wherein the rough surface region formed in the rough surface region forming step is located in the non-element region.
4. The method according to claim 3 , wherein the non-element region is a region corresponding to a scribe line of the gallium nitride based semiconductor layer.
5. The manufacturing method according to any one of claims 1 to 4, wherein in the rough surface region forming step, the rough surface region is formed by utilizing a dry etching technique.
Citation Information
Patent Citations
Semiconductor device chip for image sensor and manufacture thereof
JP1992212457A
Manufacturing method of semiconductor device, and semiconductor device
JP2009290160A
Manufacturing method for semiconductor device
JP2012190864A
Semiconductor device manufacturing method
JP2017228703A
Method of manufacturing semiconductor device
JP2018010970A