Holding device
The holding device addresses cooling inefficiencies and temperature non-uniformity in electrostatic chucks by using a low thermal resistance joint with enhanced flexibility and stress relaxation, ensuring efficient and uniform cooling of the wafer surface under high-power plasma exposure.
Patent Information
- Application Number
- JP2022095406
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-06-14
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2042-06-14
AI Technical Summary
Existing electrostatic chucks experience insufficient cooling rates and non-uniform temperature distribution on the wafer mounting surface due to low thermal conductivity and significant thermal resistance in the adhesive layer, especially when exposed to strong plasma energy or high power input, leading to potential damage and reduced processing accuracy.
A holding device with a joint portion having a thermal resistance of 1.1×10^-3 (m^2 K/W) or less, a thermal conductivity ratio of 1.18 or less, and a strain amount of 0.5 mm or more, utilizing materials like aluminum nitride to enhance flexibility and stress relaxation, and incorporating a hole joint portion with lower thermal resistance to improve heat dissipation.
The solution enhances cooling efficiency and uniformity of temperature distribution on the wafer surface, reducing the risk of damage and maintaining processing accuracy even under high-power plasma conditions.
Smart Images

Figure 0007578642000001 
Figure 0007578642000002 
Figure 0007578642000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a retention device. [Background technology]
[0002] Conventionally, as a holding device for holding an object, for example, an electrostatic chuck for holding an object such as a wafer when manufacturing a semiconductor is known. The electrostatic chuck generally includes a plate-shaped portion on which the object is placed, a base portion in which a coolant flow path is formed, and a joint portion for joining the plate-shaped portion and the base portion. For example, Patent Documents 1 and 2 disclose that an adhesive layer (joint portion) is made of a silicone resin or a composite resin in which a thermally conductive filler such as aluminum oxide or aluminum nitride is added to a silicone resin. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 4-287344 [Patent Document 2] JP 2014-207374 A Summary of the Invention [Problem to be solved by the invention]
[0004] When an electrostatic chuck is used in an environment where it is exposed to strong plasma energy or where high power is input to the electrostatic chuck, the wafer mounting surface is likely to become hot. If the electrostatic chucks described in Patent Documents 1 and 2 are used in such an environment, the adhesive layer has a relatively low thermal conductivity, so there is a risk that the wafer mounting surface will not be cooled sufficiently. Therefore, it is desirable to improve the heat dissipation of the bonding portion in order to increase the cooling rate of the wafer mounting surface.
[0005] In addition, when the wafer mounting surface is prone to high temperatures as described above, the base side is used at extremely low temperatures to cool it, so the temperature difference between the top and bottom of the joint as well as within the surface becomes large. The silicone resin described in Patent Documents 1 and 2 above has a temperature range in which the thermal conductivity changes significantly in the low temperature range, so if a temperature distribution occurs in the joint and the thermal conductivity characteristics of the joint change, there is a risk that the in-plane temperature distribution of the wafer mounting surface of the electrostatic chuck will become more non-uniform. Therefore, a joint that has a small degree of change in thermal conductivity depending on temperature is required. Note that these problems are not limited to electrostatic chucks, but are common problems to various holding devices such as semiconductor manufacturing devices such as plasma etching devices.
[0006] The present disclosure has been made to solve at least some of the problems described above, and aims to provide a technology for improving at least one of the cooling rate of the surface on which the object is placed and the uniformity of the in-plane temperature distribution of the surface on which the object is placed in a holding device that holds an object. [Means for solving the problem]
[0007] The present disclosure can be realized in the following forms. (1) According to one aspect of the present disclosure, there is provided a holding device for holding an object. The holding device includes a plate-shaped portion having a first surface on which the object is placed and a second surface that is the reverse side of the first surface, a plate-shaped base portion disposed on the second surface side of the plate-shaped portion, supporting the plate-shaped portion, and having a cooling function, and a joint portion disposed between the plate-shaped portion and the base portion for joining the plate-shaped portion and the base portion, and the thermal resistance of the joint portion is 1.1×10 at −60° C. -3 (m 2 K / W) or less.
[0008] With this type of holding device, the thermal resistance of the junction is 1.1 x 10 at -60°C. -3 (m 2Since the thermal resistance is small, for example, when the plate-shaped part of the holding device becomes hot and the base part is used at an extremely low temperature of about -60°C, the plate-shaped part can be cooled rapidly. Therefore, the cooling speed of the surface on which the object is placed can be improved.
[0009] (2) In the holding device of the above embodiment, the joint may satisfy at least one of the following: λ1 / λ2 is 1.18 or less, where λ1 is the thermal conductivity at -60° C. and λ2 is the thermal conductivity at 25° C.; and θ1 / θ2 is 0.85 or more, where θ1 is the thermal resistance at -60° C. and θ2 is the thermal resistance at 25° C. With this configuration, the change in thermal conductivity of the joint due to a change in temperature is small, and therefore the uniformity of the temperature distribution of the plate-shaped portion can be improved.
[0010] (3) In the holding device of the above embodiment, the joint has a thermal resistance of 1.2×10 at 25° C. -3 (m 2 With this configuration, even when the temperature of the holding device is room temperature (25° C.), the plate-shaped portion can be cooled rapidly because the joint has good thermal conductivity.
[0011] (4) In the holding device of the above embodiment, the joint may have a thermal conductivity of 0.7 (W / mK) or more at 25° C. and −60° C. With this configuration, sufficient thermal conductivity can be obtained both at extremely low temperatures (e.g., −60° C.) and at room temperature.
[0012] (5) In the holding device of the above embodiment, the joint may contain aluminum nitride (AlN), thereby providing a joint having good flexibility, stress relaxation performance, and good thermal conductivity.
[0013] (6) In the above-described holding device, the strain of the joint at maximum shear stress may be 0.5 (mm) or more. With this configuration, it is possible to sufficiently ensure the flexibility and stress relaxation performance of the joint. Therefore, it is possible to suppress damage to the joint when a shear force is applied to the joint.
[0014] (7) In the above-mentioned holding device, the holding device has a hole penetrating the base, an insulating part covering the inner wall of the hole, an end face of the insulating part facing the second surface of the plate-like part, and a hole joint part joining the plate-like part, and the hole joint part may be made of the same material as the material constituting the joint part and may be thinner than the joint part. In this holding device, since the holding device has a hole penetrating the base, the position of the plate-like part corresponding to the hole is difficult to cool. Therefore, with this configuration, the part of the plate-like part corresponding to the hole can be dissipated through the hole joint part having good thermal conductivity, so that the unevenness of the temperature of the plate-like part can be suppressed.
[0015] The present disclosure may be realized in various forms other than those described above, for example, in the form of a semiconductor manufacturing apparatus including a holding device, a manufacturing method for a holding device, a method for forming a joint, and the like. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is an explanatory diagram illustrating a schematic configuration of an electrostatic chuck according to a first embodiment. [Diagram 2] FIG. 2 is an explanatory diagram illustrating a cross-sectional configuration of the electrostatic chuck. [Diagram 3] FIG. 11 is an explanatory diagram illustrating the evaluation results of each sample. [Figure 4] FIG. 2 is an explanatory diagram showing the composition of each sample. [Diagram 5] FIG. 1 shows the particle size distribution of 10 μm alumina. [Figure 6] FIG. 1 shows an SEM image and particle size distribution of 15 μm aluminum nitride. [Figure 7]FIG. 1 shows an SEM image and particle size distribution of aluminum nitride 5 μm. [Figure 8] FIG. 1 shows an SEM image and particle size distribution of 2 μm aluminum nitride. [Figure 9] FIG. 4 is an explanatory diagram showing the temperature dependence of thermal conductivity of each sample. [Figure 10] FIG. 4 is an explanatory diagram showing the temperature dependence of thermal resistance of each sample. [Figure 11] FIG. 4 is an explanatory diagram showing the temperature dependence of thermal resistance of each sample. [Figure 12] FIG. 2 is an explanatory diagram illustrating a method for calculating a maximum shear stress and an amount of strain. [Figure 13] FIG. 4 is a diagram showing the composition and thermal conductivity of a sample using a first silicone resin. [Figure 14] FIG. 4 is a diagram showing the composition and thermal conductivity of a sample using a first silicone resin. [Figure 15] 1 shows a ternary diagram of the thermal conductivity of a sample using a first silicone resin. [Figure 16] FIG. 13 is a diagram showing the composition and thermal conductivity of a sample using a second silicone resin. [Figure 17] FIG. 13 is a diagram showing the composition and thermal conductivity of a sample using a second silicone resin. [Figure 18] FIG. 13 shows a ternary diagram of the thermal conductivity of a sample using a second silicone resin. [Figure 19] FIG. 11 is a cross-sectional view illustrating a schematic configuration of an electrostatic chuck according to a second embodiment. [Figure 20] FIG. 20 is an enlarged view of a portion X in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] A. First embodiment: (A-1) Overall structure of electrostatic chuck: FIG. 1 is an explanatory diagram that shows a schematic configuration of an electrostatic chuck 10 in the first embodiment. FIG. 2 is an explanatory diagram that shows a schematic cross-sectional configuration of the electrostatic chuck 10. In FIG. 1, a part of the electrostatic chuck 10 is cut away. In addition, in the figure, mutually orthogonal X, Y and Z axes are shown in order to specify the direction. In this specification, for convenience, the positive direction of the Z axis is referred to as the upward direction, and the negative direction of the Z axis is referred to as the downward direction, but the electrostatic chuck 10 may actually be installed in a direction different from such an orientation. The X axis, Y axis and Z axis shown in each figure each represent the same direction. Note that each of the above figures shows the arrangement of each part typically, and does not accurately show the ratio of the dimensions of each part.
[0018] The electrostatic chuck 10 is a device that attracts and holds an object by electrostatic attraction, and is used, for example, to fix a wafer W (FIG. 2) that is an object in a vacuum chamber of a semiconductor manufacturing device. The electrostatic chuck 10 includes a plate-shaped portion 20, a base portion 30, and a joint portion 40. These are stacked in the order of the plate-shaped portion 20, the joint portion 40, and the base portion 30 toward the -Z axis direction (vertically downward). The electrostatic chuck 10 in this embodiment is also referred to as a "holding device."
[0019] The plate-shaped part 20 is a substantially circular plate-shaped member having a first surface 24 on which an object is placed and a second surface 26 that is the reverse side of the first surface 24, and is formed mainly of ceramic (for example, aluminum oxide, aluminum nitride, etc.). In the present specification, when a specific component is "the main component" or "the material that mainly forms" it means that the content of the specific component is 50 volume % or more. The diameter of the plate-shaped part 20 may be, for example, about 50 mm to 500 mm, and is usually about 200 mm to 350 mm. The thickness of the plate-shaped part 20 may be, for example, about 1 mm to 10 mm. In other embodiments, the plate-shaped part 20 may be formed mainly of a material other than ceramic, such as a resin such as polyimide.
[0020] As shown in FIG. 2, an adsorption electrode 22 is disposed inside the plate-shaped portion 20. The adsorption electrode 22 is formed of a conductive material such as tungsten or molybdenum. When a voltage is applied to the adsorption electrode 22 from a power source (not shown), an electrostatic attraction is generated, and the wafer W is adsorbed and fixed to the first surface 24 of the plate-shaped portion 20 by this electrostatic attraction. The adsorption electrode 22 may be of a bipolar type or a unipolar type. In addition, a heater electrode (not shown) may be provided inside the plate-shaped portion 20, which is composed of a resistance heating element formed of a conductive material (such as tungsten or molybdenum) and is used to heat the wafer W adsorbed and fixed to the first surface 24.
[0021] The base portion 30 is a plate-like member that is disposed on the second surface 26 side of the plate-like portion 20, supports the plate-like portion 20, has a cooling function, and is formed in a substantially circular shape. The base portion 30 may contain at least one metal selected from the group consisting of aluminum, magnesium, molybdenum, titanium, tungsten, and nickel. Among the above-mentioned metals, molybdenum, titanium, and tungsten have relatively small coefficients of thermal expansion, and therefore, when the base portion 30 is constructed using at least one of these metals, it is desirable to suppress the difference in coefficient of thermal expansion between the base portion 30 and the plate-like portion 20. In this specification, the term "coefficient of thermal expansion" refers to the "coefficient of linear expansion." Furthermore, since magnesium has a relatively small Young's modulus, when the base portion 30 is constructed using magnesium, it is desirable to reduce the thermal stress generated in the base portion 30. Furthermore, aluminum has a relatively high thermal conductivity, is easy to process, and is low in cost. Therefore, when the base portion 30 is constructed using aluminum, it is desirable to increase the cooling efficiency of the plate-like portion 20 and the wafer W by the base portion 30 and suppress the manufacturing cost of the electrostatic chuck 10. From the viewpoint of suppressing manufacturing costs while increasing the cooling efficiency of the base portion 30, it is desirable that the base portion 30 contains a high metal content, and it is desirable that the base portion 30 contains metal as a main component. For example, it is desirable that the base portion 30 contains 90 mass % or more of aluminum, which is highly versatile (for example, it is made of an aluminum alloy such as A6061 or A5052). However, the base portion 30 may contain components other than metal, such as ceramic. The diameter of the base portion 30 may be, for example, about 220 mm to 550 mm, and is usually 220 mm to 350 mm. The thickness of the base portion 30 may be, for example, about 20 mm to 40 mm.
[0022] A plurality of coolant channels 32 are formed inside the base portion 30 along the XY plane. The base portion 30 is cooled by flowing a coolant such as a fluorine-based inert liquid, water, or liquid nitrogen through the coolant channels 32. The plate portion 20 is cooled by heat transfer between the base portion 30 and the plate portion 20 via the joint portion 40, and the wafer W held on the first surface 24 of the plate portion 20 is cooled. This realizes temperature control of the wafer W. In addition to the form having the coolant channels 32 inside the base portion 30, the base portion 30 may be provided with a cooling function by cooling the base portion 30 from the outside of the base portion 30.
[0023] The joint 40 is disposed between the plate-shaped portion 20 and the base portion 30 to join the plate-shaped portion 20 and the base portion 30. The joint 40 includes an adhesive formed of a resin material. The joint 40 may further include various fillers (inorganic fillers) for adjusting the properties of the joint 40 and the properties of the paste for forming the joint 40. That is, the joint 40 can be formed of a composite containing an adhesive and an inorganic filler. However, as long as the joint 40 satisfies the properties described below, the joint 40 may not include an inorganic filler. From the viewpoint of reducing the thermal resistance of the joint 40, the thickness of the joint 40 may be, for example, 1.00 mm or less, preferably 0.60 mm or less, more preferably 0.50 mm or less, and even more preferably 0.35 mm or less. From the viewpoint of ensuring the flexibility and strength of the joint 40, the thickness of the joint 40 may be, for example, 0.05 mm or more. The joint 40 will be described in detail later.
[0024] The electrostatic chuck 10 further includes a plurality of gas supply paths 50. The gas supply paths 50 are provided penetrating the plate-shaped portion 20, the joint portion 40, and the base portion 30 in the Z direction, and open at gas discharge ports 52 formed on the first surface 24 (see FIG. 1). The gas supply paths 50 receive an inert gas, such as helium gas, from a gas supply device (not shown), and supply the inert gas from the gas discharge ports 52 to the space between the first surface 24 and the wafer W. This improves the heat transfer between the plate-shaped portion 20 and the wafer W, and further improves the controllability of the temperature distribution of the wafer W. The gas supply paths 50 are not essential, and the electrostatic chuck 10 may not be provided with the gas supply paths 50.
[0025] (A-2) Joint configuration: The thermal resistance of the joint 40 of the electrostatic chuck 10 of this embodiment is 1.1×10 -3 (m 2 The thermal resistance of the junction 40 is R(m 2 The thermal resistance R of the joint 40 is calculated by the following formula (1), where the thermal conductivity of the joint 40 is λ (W / mK), the thickness of the joint 40 is t (m), and the thermal conductivity of the joint 40 is λ (W / mK).
[0026] R(m 2 K / W) = t(m) ÷ λ(W / mK) … (1)
[0027] When the electrostatic chuck 10 is used in an environment where it is exposed to strong plasma energy or where high power is input to the electrostatic chuck 10, the first surface 24 of the plate-shaped portion 20 is likely to become hot. In the case of a use condition where the first surface 24 of the plate-shaped portion 20 becomes, for example, 120°C, the temperature of the coolant supplied to the base portion 30 may be set to, for example, about -60°C in order to cool the plate-shaped portion 20. When the base portion 30 becomes cold, the joint portion 40 also becomes cold. Therefore, by setting the thermal resistance of the joint portion 40 at -60°C to the above value, when the temperature of the base portion 30 is set to an extremely low temperature (for example, -60°C), heat transfer between the base portion 30 and the plate-shaped portion 20 via the joint portion 40, i.e., heat dissipation from the plate-shaped portion 20 to the base portion 30, is facilitated, and the cooling efficiency of the electrostatic chuck 10 can be improved. As described above, the joint portion 40 includes an adhesive made of resin, and the thermal conductivity of the adhesive generally decreases as the temperature increases. That is, when the thickness of the joint 40 is constant, the thermal resistance tends to increase as the temperature rises. If the thermal resistance of the joint 40 at -60°C is set to the above value, sufficient cooling performance can be obtained even if the temperature of the joint 40 becomes higher than -60°C. Therefore, the cooling speed of the surface (first surface 24) on which the object is placed can be improved.
[0028] The thermal conductivity of the bonding portion 40 is not particularly limited, but when the thermal conductivity at -60°C is λ1 and the thermal conductivity at 25°C is λ2, it is preferable that λ1 / λ2 is 1.18 or less. Here, 25°C is the room temperature (normal temperature) when the electrostatic chuck 10 is used. As described above, the thermal conductivity of an adhesive generally decreases as the temperature increases. When the thermal conductivity of the bonding portion 40 is set as described above, the change in thermal conductivity associated with the temperature change of the bonding portion 40 is small. When the change in thermal conductivity associated with the temperature change of the bonding portion 40 is large, the low-temperature portion is cooled more and the high-temperature portion is cooled slower, so that there is a risk that the temperature difference between the top, bottom, and in-plane of the bonding portion 40 will be large. In contrast, when the thermal conductivity of the bonding portion 40 is set as described above, the change in thermal conductivity associated with the temperature change of the bonding portion 40 is small, so that the temperature difference between the top, bottom, and in-plane of the bonding portion 40 can be suppressed. In other words, the uniformity of the temperature distribution of the plate-shaped portion 20 can be improved. Incidentally, λ1 / λ2 is usually 1.00 or more.
[0029] Regarding the thermal resistance of the joint 40, when the thermal resistance at -60°C is θ1 and the thermal resistance at 25°C is θ2, it is preferable that θ1 / θ2 is 0.85 or more. In this way, the change in thermal resistance due to the temperature change of the joint 40 is small, so that the temperature difference above and below and within the plane of the joint 40 can be suppressed. In other words, the uniformity of the temperature distribution of the plate-shaped part 20 can be improved. Note that θ1 / θ2 is usually 1.00 or less.
[0030] The thermal resistance of the joint 40 at 25° C. is not particularly limited, but is preferably 1.2×10 -3 (m 2 In this way, even when the electrostatic chuck 10 is used at room temperature (25° C.), the plate-shaped portion 20 can be cooled rapidly because the bonding portion 40 has good thermal conductivity.
[0031] The strain amount at maximum shear stress of the joint 40 is not particularly limited, but is preferably 0.5 mm or more, more preferably 1.0 mm or more, and even more preferably 1.1 mm or more. The strain amount at maximum shear stress of the joint 40 is usually 5.0 mm or less. The strain amount at maximum shear stress is a value that serves as an index of the flexibility and stress relaxation performance of the joint 40, and refers to the magnitude of the strain (displacement in the shear force direction) generated at the joint 40 when the shear stress generated at the joint 40 becomes maximum when a shear force is applied to the joint 40, that is, when the maximum shear stress occurs at the joint 40. The larger the strain amount at maximum shear stress, the higher the flexibility of the joint 40. A specific measurement method using a tensile tester for measuring the strain amount at maximum shear stress will be described in detail later. If the strain amount at maximum shear stress of the joint 40 is set to the above value, it is possible to sufficiently ensure the flexibility and stress relaxation performance of the joint 40. Therefore, damage to the joint 40 when a shear force is applied to the joint 40 can be suppressed.
[0032] The lower limit of the thermal resistance of the joint 40 is, for example, 0.6×10 -4 (m 2 K / W). In order to suppress the thermal resistance of the joint 40, as described above, a method of appropriately selecting the material constituting the inorganic filler and increasing the content ratio of the inorganic filler is considered. However, if the content ratio of the inorganic filler is excessively increased, the flexibility of the joint 40 is impaired, and it may be difficult to sufficiently ensure the magnitude of the strain amount at maximum shear stress of the joint 40 described later. In addition, in order to suppress the thermal resistance of the joint 40, a method of thinning the joint 40 is considered. However, if the joint 40 is excessively thinned, the strength of the joint 40 is reduced and it is difficult to ensure the flexibility of the joint 40, and it may be difficult to set the strain amount at maximum shear stress in a desired numerical range. Therefore, the thermal resistance of the joint 40 is set to the above-mentioned 0.6×10 -4 (m 2 It is desirable to set the temperature at or above 100 K / W.
[0033] The strain amount at maximum shear stress of the joint 40 can be changed by the adhesive (resin) contained in the joint 40. For example, the strain amount at maximum shear stress can be changed by the type of resin constituting the joint 40. In addition, even when the same type of resin is used, the strain amount at maximum shear stress of the joint 40 can be changed by controlling the distance between crosslinking points in the resin, which is a polymer material. Specifically, when the content (functional group equivalent) of the functional group that becomes the crosslinking point in the resin is reduced, the distance between the crosslinking points is increased and the flexibility of the resin is improved, so that the strain amount at maximum shear stress can be increased. In addition, even when the content of the reactive functional group in the resin is the same, the distance between the crosslinking points can be controlled by the curing conditions such as the curing temperature and curing time of the resin. That is, when the curing temperature is increased or the curing time is increased, the curing of the resin proceeds further, the crosslinking density increases, and the distance between the crosslinking points is shortened.
[0034] Moreover, the strain amount at maximum shear stress of the joint 40 can be increased by increasing the thickness of the joint 40 .
[0035] Furthermore, the greater the content of inorganic filler in joint 40, the smaller the strain amount at maximum shear stress of joint 40. This is believed to be because, as the content of inorganic filler increases, the inorganic filler restrains the surrounding resin (resin composition) to a greater extent, reducing the flexibility of joint 40 and making joint 40 less susceptible to strain.
[0036] The adhesive constituting the joint 40 may be, for example, a silicone resin, an acrylic resin, or an epoxy resin. Silicone resin is particularly preferable because it has relatively excellent heat resistance and flexibility. Among these resins, silicone resin is preferable because it has a relatively low elastic modulus, so it has a high function of alleviating thermal stress generated at the joint 40, and also has a relatively high heat resistance temperature.
[0037] As the inorganic filler, granular or powdery substances made of various inorganic materials including ceramics, metal oxides, metals, or other inorganic compounds can be used. Specifically, as the inorganic filler, for example, aluminum nitride (AlN), aluminum oxide (alumina: Al2O3), zirconium oxide (zirconia: ZrO2), yttrium oxide (yttria: Y2O3), yttrium fluoride (YF3), silicon carbide (SiC), silicon nitride (Si3N4), silicon dioxide (silica: SiO2), iron oxide, barium sulfate, calcium carbonate, etc. can be used. Since the above-mentioned inorganic materials constituting the inorganic filler generally have a higher thermal conductivity than the resin that is the adhesive, the thermal conductivity of the joint 40 can be increased by adding the inorganic filler to the joint 40. In particular, from the viewpoint of relatively high thermal conductivity and easy suppression of the thermal resistance of the joint 40, aluminum nitride, aluminum oxide, and silicon carbide are preferable as materials constituting the inorganic filler, and aluminum nitride and aluminum oxide are particularly preferable.
[0038] The joint 40 may further include a catalyst for promoting a curing reaction, a silane coupling agent for promoting curing and adhesion to provide adhesiveness, a crosslinking agent, a reaction inhibitor for adjusting the curing speed of the adhesive, or a viscosity adjuster. As the catalyst contained in the joint 40, various conventionally known catalysts can be used, such as a platinum catalyst, a rhodium catalyst, a titanium catalyst, a bismuth catalyst, etc. Among them, it is preferable to use a platinum catalyst, which has high reactivity. There is no particular restriction on the silane coupling agent contained in the joint 40, and it can be appropriately selected from conventionally known silane coupling agents, such as those having any of a vinyl group, an epoxy group, a methacryl group, an amino group, a mercapto group, and an isocyanate group as an organic reactive group. In addition, a titanate-based coupling agent or an aluminate-based coupling agent may be used instead of the above silane coupling agent. As the crosslinking agent contained in the joint 40, an organohydrogenpolysiloxane having at least three hydrosilyl groups in one molecule can be used. More specifically, for example, at least one of polymethylhydrogensiloxane and poly(dimethylsiloxane-methylhydrogensiloxane) can be used.
[0039] As the reaction inhibitor contained in the joint 40, various conventionally known reaction inhibitors can be used, for example, 1,3,5,7-tetramethyl-1,3,5,7-tetravinylcyclotetrasiloxane, 1,1,3,3-tetramethyl-1,3-divinyldisiloxane, triallyl isocyanurate, etc. can be used. As the viscosity adjuster contained in the joint 40, various conventionally known viscosity adjusters can be used, for example, fumed silica, fumed silica, colloidal silica, fumed alumina, fumed alumina, colloidal alumina, etc. can be used. The types and amounts of the above-mentioned catalysts, silane coupling agents, crosslinking agents, reaction inhibitors, viscosity adjusters, etc. may be appropriately selected depending on, for example, the type of resin constituting the joint 40, etc.
[0040] According to formula (1), the thermal resistance of the joint 40 can be reduced by reducing the thickness of the joint 40. For example, by making the thickness of the joint 40 0.5 mm or less, the thermal resistance of the joint 40 at −60° C. can be reduced to 1.1×10 -3 (m 2 In addition, by increasing the thermal conductivity of the joint 40 to, for example, 0.7 W / mK or more, the thermal resistance of the joint 40 at −60° C. can be reduced to 1.1×10 -3 (m 2 In order to increase the thermal conductivity of the joint 40, for example, as described below, an inorganic filler made of a material with a higher thermal conductivity may be used or the content ratio of the inorganic filler may be increased.
[0041] The thermal resistance of the joint 40 can be changed by, for example, the material of the inorganic filler contained in the joint 40, the content of the inorganic filler in the joint 40, or the type of resin contained in the joint 40. By using an inorganic filler made of a material with higher thermal conductivity, by increasing the content of the inorganic filler, or by using a resin with higher thermal conductivity, the thermal conductivity of the joint 40 can be increased and the thermal resistance of the joint 40 can be reduced.
[0042] Furthermore, the thermal resistance of the joint 40 can be changed by the shape of the particles of the inorganic filler contained in the joint 40 .
[0043] The inorganic filler may be formed from a homogeneous material, or may have a coating layer on the surface made of a material different from the material constituting the inorganic filler particle body. By appropriately selecting the material constituting the coating layer, it is possible to increase the water resistance of the inorganic filler, improve the compatibility between the inorganic filler and the resin, and increase the flexibility of the joint 40. For example, when aluminum nitride powder is used as the inorganic filler, a coating layer containing silicon dioxide (SiO2), aluminum oxide (Al2O3), or aluminum phosphate (AlPO4) may be provided on the surface of the aluminum nitride particles constituting the inorganic filler.
[0044] In the electrostatic chuck 10, the base portion 30 generally has a higher thermal expansion coefficient than the plate-shaped portion 20, and expands and contracts significantly due to temperature changes. Therefore, depending on the temperature conditions, the degree of thermal expansion of the base portion 30 may be greater than the degree of thermal expansion of the plate-shaped portion 20. In this way, since the degree of expansion and contraction differs between the plate-shaped portion 20 and the base portion 30, a shear force in the X-axis direction is applied to the joint portion 40, and a shear stress is generated. Therefore, by increasing the magnitude of the strain amount at the maximum shear stress of the joint portion 40 as described above, even when a large shear force is applied to the joint portion 40, the shear stress generated in the joint portion 40 can be reduced and damage to the joint portion 40 can be suppressed.
[0045] As described above, according to the electrostatic chuck 10 of the present embodiment, the thermal resistance of the joint 40 of the electrostatic chuck 10 is 1.1×10 -3 (m 2 K / W) or less. Therefore, even when the heat input to the plate-shaped portion 20 is greater and the base portion 30 is kept at a very low temperature (for example, −60° C.), the cooling performance of the electrostatic chuck 10 can be improved. As a result, an excessive temperature rise in the plate-shaped portion 20 is suppressed, and a decrease in the processing accuracy of the wafer caused by the temperature rise is suppressed, and the shear stress generated in the bonding portion 40 due to the temperature difference between the plate-shaped portion 20 and the base portion 30 can be suppressed.
[0046] Furthermore, for joint 40, if the thermal conductivity at -60°C is λ1 and the thermal conductivity at 25°C is λ2, and λ1 / λ2 is 1.18 or less, or if the thermal resistance at -60°C is θ1 and the thermal resistance at 25°C is θ2, and θ1 / θ2 is 0.85 or more, the change in thermal conductivity due to temperature change at joint 40 can be reduced, and the temperature difference above, below, and within the plane of joint 40 can be suppressed.
[0047] In addition, the thermal resistance of the junction 40 at 25°C is 1.2×10 -3 (m 2When the heat transfer coefficient is set to 1.0 K / W or less, even when the electrostatic chuck 10 is used at room temperature (25° C.), the joining portion 40 has good thermal conductivity, so that the plate-shaped portion 20 can be cooled rapidly.
[0048] Furthermore, the larger the strain amount at maximum shear stress of joint 40, the higher the stress relaxation performance of joint 40. Therefore, by setting the strain amount at maximum shear stress of joint 40 to 0.5 mm or more, even if shear stress occurs at joint 40, damage to joint 40 caused by shear stress can be suppressed.
[0049] Such an effect is particularly noticeable when the heat input to the plate-shaped portion is large, such as when the electrostatic chuck 10 is exposed to a higher-power plasma. For example, even if a heater electrode for heating the plate-shaped portion 20 is not provided, when the electrostatic chuck 10 is used with high plasma power, the temperature difference between the mounting surface of the plate-shaped portion 20 and the base portion 30 is likely to become large, and therefore the effect of this embodiment is significantly achieved. EXAMPLES
[0050] The holding device of the present disclosure will be described below based on examples. Here, sheet-like samples 1 to 11 were prepared as samples corresponding to various joints having at least one of different thermal conductivity, thermal resistance, and strain amount at maximum shear stress. In addition, samples in the form of electrostatic chucks having joints with the same composition as each of the sheet-like samples 1 to 11 were prepared. In the following, the samples in the form of electrostatic chucks will be referred to by the same sample numbers as the sheet-like samples having the same composition as the joints.
[0051] FIG. 3 is an explanatory diagram showing the evaluation results of the temperature distribution of the plate-shaped part in the electrostatic chuck and the temperature drop rate together with the thickness of the joint of each sample, the thermal conductivity (-60°C, 25°C), the ratio of thermal conductivity (-60°C / 25°C), the thermal resistance, the ratio of thermal resistance (-60°C / 25°C), and the strain amount at maximum shear stress. FIG. 4 is an explanatory diagram showing the composition of each sample. FIG. 5 is a diagram showing the particle size distribution of alumina 10 μm used in the sample. FIG. 6 is a diagram showing the SEM image and particle size distribution of aluminum nitride 15 μm used in the sample. FIG. 7 is a diagram showing the SEM image and particle size distribution of aluminum nitride 5 μm used in the sample. FIG. 8 is a diagram showing the SEM image and particle size distribution of aluminum nitride 2 μm used in the sample. FIG. 9 is an explanatory diagram showing the temperature dependence of the thermal conductivity of each sample. FIG. 10 and FIG. 11 are explanatory diagrams showing the temperature dependence of the thermal resistance of each sample. 10 and 11 show samples with a thickness of 0.5 mm (samples 1, 3, 4, 6, 8, and 10). Fig. 11 shows samples 1, 3, 4, and 6 in an enlarged scale (the maximum value of the vertical axis is smaller than that in Fig. 10).
[0052] <Preparation of each sample> [Preparation of sheet-like samples] In each sample, silicone resin was used as an adhesive. Specifically, either polydimethylsiloxane or polydimethylsiloxane containing 5 mol % of phenyl groups was used as an adhesive material (resin material) before curing. Specifically, samples 1 to 3 used polydimethylsiloxane containing 5 mol % of phenyl groups, and samples 4 to 11 used polydimethylsiloxane. As shown in FIG. 4, samples 1 and 2, samples 4 and 5, samples 6 and 7, samples 8 and 9, and samples 10 and 11 each have the same composition, and as shown in FIG. 3, one has a thickness of 0.5 mm, and the other has a thickness of 1 mm. The composition of each sample is as shown in FIG. 4.
[0053] Among the fillers shown in FIG. 4, “alumina 10 μm” refers to alumina particles with an average particle size of 10 μm and a BET specific surface area of 1.3 m 2 / g. The particle size distribution is as shown in Figure 5. The average particle diameter was determined using the particle size distribution by the following method. The shape of 10 μm alumina is almost a perfect sphere (Figure 4). Here, when the radius of the inscribed circle when the filler is viewed in cross section is R1 and the radius of the circumscribed circle is R2, a filler is defined as a "true sphere" when the average value of "R2 / R1" is close to 1.0 (for example, less than 1.05). The average particle size can be measured using a known particle size distribution measuring device. After dispersing the filler in water, the particle size distribution is measured using, for example, a Microtrac MT3000II, and the diameter at which the cumulative frequency is 50% is taken as the average particle size. The method of determining the average particle size is the same for aluminum nitride.
[0054] "Aluminum nitride 15μm" is aluminum nitride particles with an average particle diameter of 15μm and a BET specific surface area of 0.9m 2 / g. The particle size distribution is as shown in Figure 6. "Aluminum nitride 5 μm" is aluminum nitride particles with an average particle size of 5 μm and a BET specific surface area of 1.3 m 2 / g. The particle size distribution is as shown in Figure 7. "Aluminum nitride 2 μm" is aluminum nitride particles with an average particle diameter of 2 μm and a BET specific surface area of 2.8 m 2 / g. The particle size distribution is as shown in FIG. 8. The shape of the aluminum nitride is angular granular. Here, "angular granular" refers to particles that are angular and irregular, and are not cuboid, spherical, rod-like, or plate-like, as shown in the SEM (scanning electron microscope) images of FIG. 6 to FIG. 8. When the particle shape of the filler is angular rather than spherical, the number of contact points between the particles increases, making it easier to form a heat conduction path within the joint 40, and reducing the thermal resistance of the joint 40.
[0055] The sheet-like sample was prepared as follows. The filler and silicone resin were mixed to prepare a paste-like adhesive. There is no particular restriction on the mixing method, and mixing with a known stirring blade, a three-roll, a kneader, a rotation / revolution mixer, a planetary mixer, etc. can be used. The prepared paste-like adhesive can be spread on a film with releasability using a known coating device and cured to obtain a sheet-like sample. For example, a roll coater, a bar coater, a die coater, a knife coater, etc. can be used as the coating device. For example, a polyethylene terephthalate (PET) film can be used as the film with releasability, and a PET film coated with a release agent may be used to improve releasability. In order to obtain a thick cured product or a block-like cured product that is difficult to mold using the various coating devices described above, the adhesive may be placed in a container of a specified size and then cured. A container made of polytetrafluoroethylene (PTFE) is preferable because it is easy to remove. Heating may be used for curing as necessary.
[0056] [Preparation of electrostatic chuck-type sample] The electrostatic chucks of Samples 1 to 12 all have the same configuration as the electrostatic chuck 10 of the first embodiment shown in Fig. 2. The samples in the form of the electrostatic chuck 10 were produced by disposing the above-mentioned semi-cured adhesive paste between the plate-shaped portion 20 and the base portion 30, and then curing the adhesive paste. The plate-shaped portion 20 was made of aluminum oxide (thermal expansion coefficient 7 ppm / K), and the base portion 30 was made of aluminum (thermal expansion coefficient 23 ppm / K). The diameters of the plate-shaped portion 20 and the joint portion were 350 mm.
[0057] <Evaluation method> Thermal conductivity The thermal conductivity of a block-shaped sample was measured by a hot wire method (probe method) using a known thermal conductivity meter (Agne thermal conductivity measuring device ARC-TC-1000). When measuring the thermal conductivity of a joint built into an electrostatic chuck instead of a block-shaped sample, the plate-shaped part of the electrostatic chuck can be scraped off with a surface grinder or the like to expose the joint, and then the joint can be peeled off with a knife or the like to measure the thermal conductivity.
[0058] ·Thermal resistance The thermal resistance R was calculated from the thermal conductivity of each sample measured as described above according to the following formula (1): In formula (1), t is the thickness of the joint and λ is the thermal conductivity of the joint, i.e., the thermal conductivity of each sample measured as described above.
[0059] R(m 2 K / W) = t(m) ÷ λ(W / mK) … (1)
[0060] -Strain at maximum shear stress The strain amount at maximum shear stress was measured by a tensile test using a known tensile tester (Shimadzu Corporation Autograph AGS-5kNX).
[0061] FIG. 12 is an explanatory diagram showing a method of calculating the maximum shear stress and the amount of strain. FIG. 12(A) shows the state of the tensile test as seen from the front, and FIG. 12(B) and FIG. 12(C) show the state as seen from the side. Also, FIG. 12(A) and FIG. 12(B) show the state at the start of the test, and FIG. 12(C) shows the state after the start of the test. The test pieces 70 of Samples 1 to 12 were prepared by attaching the semi-cured adhesive sheet of each sample to a 25 mm×12.5 mm portion of two aluminum plates 80, each having a width of 25 mm×length of 100 mm×thickness of 1 mm, from the end to a position of 12.5 mm, and bonding the two aluminum plates 80 in a direction that allows them to be pulled in opposite directions, and then curing the semi-cured adhesive sheet. The thickness t of the test piece 70 at the start of the test was the thickness of the joint shown in FIG. 8 to FIG. 11. Next, the two aluminum plates 80 were held by a tensile test tool and moved relative to each other so that a shear force was applied to the test piece. Here, a tensile tester was used to move one of the aluminum plates in one direction parallel to the adhesive surface at a tensile speed of 2 mm / min, while measuring the load and the amount of strain δ as the distance of movement (see FIG. 12(C)). A tensile tester and a tool having a sufficiently high rigidity were used, and the distance of movement of the tool of the tensile tester was taken as the amount of strain δ. In FIG. 12(B), the direction of the relative movement of the two aluminum plates is shown by a hollow arrow. The shear stress was calculated by dividing the load by the adhesive area (25 mm×12.5 mm) of the test piece before the movement. Such relative movement of the two aluminum plates was continued until the test piece 70 broke, and the shear stress at which the shear stress became maximum was taken as the maximum shear stress (unit: MPa). The strain amount at maximum shear stress (unit: mm) was the strain amount δ when the shear stress reached its maximum in the tensile test shown in Fig. 12. When measuring the strain amount at maximum shear stress of a joint that has already been incorporated into an electrostatic chuck, the measurement is carried out, for example, as follows. First, the joint is cut out together with the adherends (plate-shaped portion and base portion) by a processing method such as laser cutting. The shape of the cut test piece may be such that it can be held by the jig of a tensile tester and that the two joined adherends can be pulled in opposite directions to each other as shown in Fig. 12.Before the tensile test, the area of the bonded portion and the thickness of the bonded portion of the cut-out test piece are measured. Then, the tensile test is performed in the same manner as described above to measure the strain at the maximum shear stress.
[0062] Temperature distribution in plate-shaped part The temperature distribution of the plate-shaped part was evaluated for each of the electrostatic chuck samples 1 to 11. Specifically, the plate-shaped part was heated so that the average value of the surface temperature of the plate-shaped part of each sample was constant over time at about 100°C, and at the same time, a coolant at -60°C was supplied to the coolant flow path of the base part to cool it. At that time, the temperature difference between the maximum and minimum values of the surface temperature of the plate-shaped part was evaluated as "◎" if it was less than 2°C, "〇" if it was 2°C or more and less than 5°C, and "×" if it was 5°C or more. The surface temperature of the plate-shaped part and its change over time were measured using an infrared radiation thermometer. The plate-shaped part can be heated by irradiating the plate-shaped part with plasma. In addition, if a heater electrode is provided on the plate-shaped part, it can also be heated by passing electricity through the heater electrode, which may be used in combination with heating by plasma irradiation.
[0063] -Temperature drop rate of plate part For each of the electrostatic chuck samples 1 to 11, the plate-shaped portion was heated so that the average value of the surface temperature of the plate-shaped portion was constant over time at about 100°C, in the same manner as in the evaluation method for the temperature distribution of the plate-shaped portion described above. At the same time, a coolant at -60°C was supplied to the coolant flow path of the base portion to cool it, after which the heating of the plate-shaped portion was stopped and the cooling of the base portion was continued. Starting from the time when the heating of the plate-shaped portion was stopped, the change over time in the average value of the surface temperature of the plate-shaped portion was measured. The time required for the average temperature of the plate-shaped portion to cool to 0°C or less was measured, and a time of 15 seconds or less was evaluated as "good", and a time of more than 15 seconds was evaluated as "bad".
[0064] Samples 1 to 7 meet the following requirement [1]. [1] The thermal resistance of the junction is 1.1 x 10 at -60°C. -3 (m 2 K / W) or less.
[0065] In addition to the above requirement [1], samples 1 to 3 further satisfy the following requirements [2] and [3]. [2] When the thermal conductivity of the joint is λ1 at -60°C and λ2 at 25°C, the ratio λ1 / λ2 is 1.18 or less. [3] When the thermal resistance of the joint is θ1 at -60°C and θ2 at 25°C, the ratio θ1 / θ2 is 0.85 or greater.
[0066] Samples 1 to 6 satisfy the above requirement [1] as well as the following requirement [4]. [4] The thermal resistance of the junction at 25°C is 1.2×10 -3 (m 2 K / W) or less.
[0067] Samples 1 to 7 further satisfy the following requirement [5]. [5] The joint has a thermal conductivity of 0.7 (W / mK) or more at 25°C and -60°C.
[0068] Samples 1, 2, 4, and 5 further meet the requirement of [6] below. [6] The joint contains aluminum nitride (AlN).
[0069] Samples 1 to 7 further satisfy the following requirement [7]. [7] The strain at maximum shear stress of the joint is 0.5 mm or more.
[0070] Thus, Samples 8 to 11 do not satisfy at least any of the requirements in (1) above, and the temperature distribution and temperature drop rate of the plate-shaped portion are evaluated as "x" (FIG. 3).
[0071] As shown in Figure 3, Sample 1 7 In the test, the temperature distribution and the temperature drop rate were evaluated as "good" or "good". In other words, by satisfying the above requirement [1], it can be said that the transfer of heat from the plate-shaped part to the base part was improved.
[0072] Furthermore, Samples 1 to 3 satisfy the above requirements [2] and [3], and there is no temperature range in which the thermal conductivity and thermal resistance change abruptly, as shown in Figures 9 and 11. Samples 4 to 7 have a smaller thermal resistance than Samples 8 to 11, and can rapidly cool the plate-shaped portion, but the thermal conductivity and thermal resistance change abruptly in the range of -20°C to -40°C (Figures 9 and 11). This may result in a decrease in temperature uniformity, as the lower temperature portion of the plate-shaped portion is cooled more. In contrast, Samples 1 to 3 have no temperature range in which the thermal conductivity and thermal resistance change abruptly, as described above, and therefore the temperature uniformity of the plate-shaped portion is better than that of Samples 4 to 7.
[0073] Samples 1 to 7 satisfy the above requirement [5], and are evaluated as having good temperature distribution and temperature drop rate. If the thermal conductivity of the joint is 0.7 (W / mK) or more at 25°C and -60°C, sufficient thermal conductivity can be obtained over a range from extremely low temperatures to room temperature.
[0074] Samples 1, 2, 4, and 5 contain aluminum nitride (AlN) as a filler, and samples 3, 6, and 7 contain alumina as a filler (Figure 4). Therefore, Samples 1, 2, 4, and 5 have higher thermal conductivity and lower thermal resistance than Samples 3, 6, and 7 (Figures 3, 9 to 11), and the temperature drop rate of the plate-shaped part is faster than Samples 3, 6, and 7.
[0075] The strain amount at maximum shear stress is 0.5 mm or more for Samples 1, 3, 4, and 6. The strain amount at maximum shear stress is a value that serves as an index of flexibility and stress relaxation performance, and if it is 0.5 mm or more, it is possible to sufficiently ensure the flexibility and stress relaxation performance of the joint of the electrostatic chuck.
[0076] <Consideration of methods for adjusting thermal conductivity> In order to create a material capable of forming the joint 40 of the above embodiment, a method for adjusting the thermal conductivity of the forming material was examined. Specifically, a plurality of samples were created with different types of silicone resin (silicone adhesive) and different types and ratios of filler, and the thermal conductivity was measured. In detail, a silicone resin mainly composed of polydimethylsiloxane containing 5 mol% of phenyl groups was used as the first silicone resin, and a silicone resin mainly composed of polydimethylsiloxane was used as the second silicone resin. As the filler, three types of aluminum nitride with different particle sizes (15 μm, 5 μm, and 2 μm) were used. Both the first silicone resin and the second silicone resin are silicone resins (silicone adhesives) that can be cured and bonded by heating, and contain a known silane coupling agent, a crosslinking agent having a polydimethylsiloxane structure and a functional group required for curing, a silicone curing catalyst, etc. in addition to the main component.
[0077] 13 and 14 are diagrams showing the composition and thermal conductivity of a sample using the first silicone resin. FIG. 15 shows a ternary diagram of the thermal conductivity of a sample using the first silicone resin. FIG. 16 and 17 are diagrams showing the composition and thermal conductivity of a sample using the second silicone resin. FIG. 18 shows a ternary diagram of the thermal conductivity of a sample using the second silicone resin. In FIG. 15 and FIG. 18, the axis is the weight percentage, and the conductivity is shown next to the point. The thermal conductivity in FIG. 13, FIG. 14, FIG. 16, and FIG. 17 was measured using a thermal conductivity measuring device TCi manufactured by C-THERM. The thermal conductivity shown in FIG. 3 was measured by the hot wire method (probe method) using a thermal conductivity measuring device ARC-TC-1000 manufactured by Agne, and the relationship of the magnitude of the measurement results does not change because the measurement mechanisms are different, but the values themselves do not necessarily match.
[0078] The composition of sample S1 shown in FIG. 13 is consistent with the compositions of samples 1 and 2 shown in FIG. 4. In FIGS. 13 and 14, the thermal conductivity of sample S1 is taken as the reference ("1"), and the thermal conductivity of the remaining samples is shown as the "thermal conductivity ratio." Moreover, the composition of sample S18 shown in FIG. 16 is consistent with the composition of samples 4 and 5 shown in FIG. 4. In FIGS. 16 and 17, the thermal conductivity of sample S18 is taken as the reference ("1"), and the thermal conductivity of the remaining samples is shown as the "thermal conductivity ratio."
[0079] In Fig. 15, thermal conductivity of 1.35 W / mK or more is circled. In Fig. 18, thermal conductivity of 1.30 W / mK or more is circled. As shown in Figs. 15 and 18, when using the first silicone resin and when using the second silicone resin, the thermal conductivity was higher when the ratio of 15 um particles was high. However, a higher thermal conductivity was obtained when 5 um and 2 um particles were added than when only 15 um particles were used. This is thought to be because the smaller particles entered between the larger particles, bringing the particles closer to each other.
[0080] Adhesives whose thermal conductivity does not change significantly are those whose phase transition temperatures, such as glass transition temperature and crystallization temperature, do not exist within the operating temperature range. Among silicone-based adhesives, such adhesives are silicone adhesives that contain 5 mol% phenyl groups. It is presumed that because phenyl groups have large steric hindrance, they do not crystallize even at low temperatures, are flexible, and show little change in thermal conductivity.
[0081] Silicone adhesives can be made more thermally conductive by blending them with inorganic fillers. To achieve high thermal conductivity, it is necessary to blend in a large amount of filler, but the shapes of fillers that can be blended in large amounts are spherical or granular. Rod-, plate-, or needle-shaped fillers reduce fluidity, making it difficult to blend in large amounts, and even a small amount increases the hardness of the adhesive, making it unusable for applications such as electrostatic chucks, which require bonding materials with different thermal expansion coefficients.
[0082] In order to increase the thermal conductivity of an adhesive containing a filler, it is preferable for the filler to be granular rather than spherical. It is preferable for the filler particles to be in contact with each other or as close as possible to each other in many places. This is thought to be because granular particles have some protrusions or depressions, which increases the number of contact points with neighboring particles.
[0083] From the viewpoint of increasing the thermal conductivity of the adhesive, it is preferable to have an aromatic functional group. The aromatic functional group has a higher density, and when mixed at the same weight ratio, the volumetric content of the aromatic functional group is thought to be reduced by the resin and increased by the filler. Another reason is that pi bonds such as aromatic groups have higher thermal conductivity than sigma bonds such as polydimethylsiloxane. In addition, aromatic groups can be coordinated to metal atoms such as aluminum in alumina and aluminum nitride, and phosphorus atoms contained in surface treatment agents, and therefore can contribute to lowering the thermal resistance at the interface between the filler and the adhesive and increasing the overall thermal conductivity.
[0084] B. Second embodiment: Fig. 19 is a cross-sectional view showing a schematic configuration of an electrostatic chuck 10A of a second embodiment. Fig. 20 is an enlarged view of a portion X in Fig. 19. The electrostatic chuck 10A of the second embodiment includes a terminal through hole 60 (Fig. 19) in addition to the electrostatic chuck 10 of the first embodiment. In the electrostatic chuck 10A of the second embodiment, parts common to the electrostatic chuck 10 of the first embodiment are denoted by the same reference numerals. The terminal through hole 60 is also simply referred to as a "hole portion."
[0085] 19, the terminal through-hole 60 penetrates the base portion 30A and the joint portion 40A, and reaches below the chucking electrode 22 in the plate-shaped portion 20A. An electrode terminal 62 is disposed in the terminal through-hole 60 and is electrically connected to the chucking electrode 22 through a via 72.
[0086] 20, an electrode pad 74 is disposed on the plate-shaped portion 20A, which is electrically connected to the chucking electrode 22 through a via 72. In this embodiment, the shape of the electrode pad 74 is substantially circular when viewed in the Z-axis direction. The electrode pad 74 and the via 72 are made of a conductive material (for example, tungsten, molybdenum, etc.).
[0087] A columnar electrode terminal 62 extending in the Z-axis direction is disposed in the terminal through-hole 60 formed in the base portion 30A. In this embodiment, the cross section (cross section parallel to the surface direction) of the electrode terminal 62 is circular. The upper end of the electrode terminal 62 reaches the electrode pad 74, and the electrode terminal 62 is joined to the electrode pad 74 by a joint made of, for example, a metallic brazing material.
[0088] In order to insulate between the electrode terminal 62 arranged in the terminal through hole 60 of the base portion 30A and the base portion 30A, an insulating portion 64 is arranged in the terminal through hole 60 of the base portion 30A. The insulating portion 64 continuously surrounds the electrode terminal 62 so as to be interposed between the electrode terminal 62 and the surface of the terminal through hole 60. The insulating portion 64 is made of an insulating material such as resin or ceramics. In this embodiment, the thermal conductivity of the insulating portion 64 is lower than that of the plate-shaped portion 20A (i.e., the thermal conductivity of the plate-shaped portion 20A is higher than that of the insulating portion 64). Note that hole joints 66 are arranged around the insulating portion 64, specifically between the insulating portion 64 and the electrode terminal 62, between the insulating portion 64 and the plate-shaped portion 20A, and between the insulating portion 64 and the base portion 30A. The hole joint 66 is made of the same material as the material constituting the joint 40A, and joins the insulating part 64 to the electrode terminal 62, the plate-shaped part 20A, and the base part 30A. In detail, the hole joint 66 joins the end face 64S of the insulating part 64 facing the second surface 26 of the plate-shaped part 20A to the plate-shaped part 20A. The hole joint 66 is thinner than the joint 40A. The terminal through hole 60 has low thermal conductivity in the base part 30A, and is likely to cause a temperature difference in the temperature distribution of the plate-shaped part 20A. The material constituting the joint 40A has a lower thermal conductivity than the material constituting the base part 30A, so by making the hole joint 66 thinner than the joint 40A, the decrease in thermal conductivity is suppressed and the possibility of a temperature difference is reduced.
[0089] The configuration for supplying power to the adsorption electrode 22 is as described above. When the electrostatic chuck 10 is used, a voltage is applied to the adsorption electrode 22 through a conductive path extending from a power source (not shown) to the adsorption electrode 22 via the electrode terminal 62, the electrode pad 74, and the via 72. This generates an electrostatic attractive force for adsorbing and fixing the wafer W to the adsorption surface S1.
[0090] If the insulating portion 64 and the electrostatic chuck 10A are bonded to each other at the terminal through hole 60 using a resin adhesive such as a general silicone adhesive, the adhesive has poor thermal conductivity, and therefore the heat dissipation of the portion of the plate-shaped portion 20A corresponding to the terminal through hole 60 may decrease, and the temperature non-uniformity of the first surface 24 of the plate-shaped portion 20A may become large. In contrast, the electrostatic chuck 10A of the present embodiment can dissipate heat from the portion of the plate-shaped portion 20A corresponding to the terminal through hole 60 via the hole bonding portion 66, which is made of the same material as the bonding portion 40A and has good thermal conductivity. As a result, the temperature non-uniformity of the plate-shaped portion 20A can be further suppressed.
[0091] The present disclosure is not limited to the above-mentioned embodiments, etc., and can be realized in various configurations without departing from the spirit of the present disclosure. For example, the technical features in the embodiments corresponding to the technical features in each form described in the Summary of the Invention column can be appropriately replaced or combined in order to solve some or all of the above-mentioned problems or to achieve some or all of the above-mentioned effects. Furthermore, if a technical feature is not described as essential in this specification, it can be appropriately deleted.
[0092] The present disclosure can also be realized in the following application examples. [Application example 1] A holding device for holding an object, A plate-shaped portion having a first surface on which the object is placed and a second surface that is the reverse side of the first surface; a base portion formed in a plate shape, the base portion being disposed on the second surface side of the plate portion, supporting the plate portion, and having a cooling function; a joint portion disposed between the plate-shaped portion and the base portion and joining the plate-shaped portion and the base portion; Equipped with The thermal resistance of the junction is 1.1 x 10 at -60°C. -3 (m 2 K / W) or less. holding device. [Application example 2] The holding device according to Application Example 1, The joint is When the thermal conductivity at -60°C is λ1 and the thermal conductivity at 25°C is λ2, λ1 / λ2 is 1.18 or less; and When the thermal resistance at -60°C is θ1 and the thermal resistance at 25°C is θ2, θ1 / θ2 is 0.85 or more. The present invention is characterized in that at least one of the following is satisfied: holding device. [Application example 3] The holding device according to Application Example 1 or Application Example 2, The thermal resistance of the junction at 25°C is 1.2×10 -3 (m 2 K / W) or less. holding device. [Application example 4] The holding device according to any one of Application Examples 1 to 3, The joint has a thermal conductivity of 0.7 (W / mK) or more at 25°C and -60°C. holding device. [Application example 5] The holding device according to any one of Application Examples 1 to 4, The bonding portion contains aluminum nitride (AlN). holding device. [Application Example 6] The holding device according to any one of Application Examples 1 to 5, The strain amount at maximum shear stress of the joint is 0.5 (mm) or more. holding device. [Application Example 7] The holding device according to any one of Application Examples 1 to 6, a hole penetrating the base portion; an insulating portion covering an inner wall of the hole; a hole joint portion that joins an end surface of the insulating portion facing the second surface of the plate-shaped portion and the plate-shaped portion; having The hole joint is formed of the same material as the material constituting the joint, and is thinner than the joint. holding device. [Explanation of symbols]
[0093] 10, 10A...Electrostatic chuck 20, 20A…Plate-shaped part 22...Adsorption electrode 24...Side 1 26…Second side 30, 30A...Base section 32... Coolant flow path 40, 40A...joint 50…Gas supply line 52…Gas outlet 60...Through hole for terminal 62...Electrode terminal 64…Insulation section 64S…end face 66…hole joint 70...Test piece 72…Beer 74...Electrode pad 80…Aluminum plate W…wafer
Claims
1. A holding device for holding an object, A plate-shaped portion having a first surface on which the object is placed and a second surface that is the reverse side of the first surface; a base portion formed in a plate shape, the base portion being disposed on the second surface side of the plate portion, supporting the plate portion, and having a cooling function; a joint portion disposed between the plate-shaped portion and the base portion and joining the plate-shaped portion and the base portion; Equipped with The thermal resistance of the junction is 1.1×10 at −60° C. -3 (m 2 K / W) or less, The holding device comprises: a hole penetrating the base portion; an insulating portion covering an inner wall of the hole; a hole joint portion that joins an end surface of the insulating portion facing the second surface of the plate-shaped portion and the plate-shaped portion; and The hole joint is formed of the same material as the material constituting the joint, and is thinner than the joint. holding device.
2. A holding device as described in claim 1, The joint is When the thermal conductivity at -60°C is λ1 and the thermal conductivity at 25°C is λ2, λ1 / λ2 is 1.18 or less; and When the thermal resistance at -60°C is θ1 and the thermal resistance at 25°C is θ2, θ1 / θ2 is 0.85 or more. The present invention is characterized in that at least one of the following is satisfied: holding device.
3. A holding device as described in claim 1, The joint has a thermal resistance of 1.2×10 −3 (m 2 K / W) or less at 25° C. holding device.
4. A holding device according to any one of claims 1 to 3, The joint has a thermal conductivity of 0.7 (W / mK) or more at 25°C and -60°C. holding device.
5. A holding device according to any one of claims 1 to 3, The bonding portion contains aluminum nitride (AlN). holding device.
6. A holding device according to any one of claims 1 to 3, The strain amount at maximum shear stress of the joint is 0.5 (mm) or more. holding device.
Citation Information
Patent Citations
Bonding structure of electrostatic chuck
JP1992287344A
Electrostatic chuck device
JP2007194320A
Placement table and plasma processing apparatus
JP2013131541A
Part for semiconductor manufacturing device, and method for manufacturing the same
JP2014207374A
Composite member and adhesive composition
JP2020023088A