Method and apparatus for manufacturing semiconductor components - Patents.com

Targeted electrical preloading adjusts defect distribution in dielectric layers to extend semiconductor component lifespan by manipulating defect migration and reducing dielectric breakdown.

JP7579454B2Active Publication Date: 2024-11-07ROBERT BOSCH GMBH

Patent Information

Application Number
JP2023540713
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-01-04
Filing Date
2021-12-13
Publication Date
2024-11-07
Estimated Expiration
2041-12-13

AI Technical Summary

Technical Problem

Defects in dielectric layers of semiconductor components can migrate during operation, leading to dielectric breakdown near electrodes, which shortens the component's lifespan.

Method used

A method involving targeted electrical preloading is applied to manipulate the initial position and distribution of defects in the dielectric layer by applying specific voltages and temperatures to adjust the defect migration, thereby extending the component's lifetime.

Benefits of technology

The method effectively delays defect accumulation at deteriorating interfaces, optimizing the semiconductor component's lifespan and reducing leakage current levels.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007579454000010
    Figure 0007579454000010
  • Figure 0007579454000011
    Figure 0007579454000011
  • Figure 0007579454000012
    Figure 0007579454000012
Patent Text Reader

Abstract

An apparatus and method for manufacturing a semiconductor component, the method including the steps of: disposing a dielectric layer between a first electrode and a second electrode of a semiconductor component, with defects of a first defect type present in the dielectric layer (302); determining a time period for moving the defects of the first defect type to target locations in the dielectric layer (304); determining a first voltage for moving the defects in the dielectric layer to target locations (306); and applying the first voltage between the first electrode and the second electrode for the time period (308).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method and apparatus for manufacturing semiconductor components. [Background technology]

[0002] Such semiconductor components may contain dielectric layers having defects that may move within the dielectric layer between the electrodes of the semiconductor component during normal operation of the semiconductor component. The defects may accumulate adjacent to one of the electrodes, which may cause a dielectric breakdown adjacent to this electrode that shortens the life of the semiconductor component.

[0003] After dielectric breakdown, the functionality of semiconductor components can be achieved again under certain conditions, as described, for example, in J. Wang, C. Salm, E. Houwman, M. Nguyen, J. Schmitz, "Humidity and polarity influence on MIM PZT capacitor degradation and breakdown," 2016 IEEE International Integrated Reliability Workshop (IIRW), South Lake Tahoe, CA, 2016, pp. 65-68, doi:10.1109 / IIRW.2016.7904903. [Prior art documents] [Non-patent literature]

[0004] [Non-Patent Document 1] J. Wang, C. Salm, E. Houwman, M. Nguyen, J. Schmitz, “Humidity and polarity influence on MIM PZT capacitor degradation and breakdown”, 2016 IEEE International Integrated Reliability Workshop (IIRW), South Lake Tahoe, CA, 2016, pp. 65-68, doi:10.1109 / IIRW.2016.7904903 Summary of the Invention [Means for solving the problem]

[0005] The method and apparatus according to the independent claims allow defect migration in order to produce semiconductor components with extended lifetimes. Electrical pretreatment extends lifetime by targeted influence on the physical degradation mechanism caused by defect migration within the dielectric layer.

[0006] This is made possible by targeted electrical pre-stressing before delivery to the customer, which allows to manipulate the initial defect location and / or defect distribution in the dielectric layer of the semiconductor component, thereby adjusting the lifetime of the semiconductor component.

[0007] In one aspect, the method slows the accumulation of defects at degrading interfaces associated with the proper operation of semiconductor components. The method for manufacturing the semiconductor component includes the steps of disposing a dielectric layer between a first electrode and a second electrode of the semiconductor component, with defects of a first defect type present in the dielectric layer, determining a time period for moving the defects of the first defect type to target locations in the dielectric layer, determining a first voltage for moving the defects in the dielectric layer, determining a temperature for applying a load with the first voltage, and applying the first voltage between the first electrode and the second electrode at the temperature and for the time period.

[0008] It is preferred that the first voltage or duration is determined depending on a property of the dielectric layer characterizing a starting position of the defect of the first defect type and a property characterizing a speed of movement of the defect of the first defect type within the dielectric layer, and that the first voltage or duration is determined depending on the distance between the starting position and the target position.

[0009] It is preferred that a temperature is determined, which together determines a speed of movement of defects of the first defect type within the dielectric layer, and that the first voltage is determined depending on the speed such that when the first voltage is applied for a period of time, the defect of the first defect type will reach the target position within or at the end of the period, and / or that the period is determined depending on the speed such that when the first voltage is applied for a period of time, the defect of the first defect type will reach the target position within or at the end of the period.

[0010] It may be envisaged that defects of a first defect type are movable in a first direction towards a first electrode upon application of a first voltage having a first polarity between the first electrode and the second electrode, and defects of the first defect type are movable in a second direction towards a second electrode upon application of a second voltage having a second polarity opposite to the first polarity between the first electrode and the second electrode, and the method may comprise the following steps: applying a second voltage, detecting a change in the current flowing through the first and second electrodes and / or a change in the surface properties of the first electrode and / or a change in the properties of the boundary layer between the first electrode and the dielectric layer, measuring the duration of application of the first voltage until this detection, and determining a target position or duration depending on this duration.

[0011] In one embodiment, a defect is provided that offsets another defect that would otherwise degrade the interface during normal operation. A property of the dielectric layer characterizing a starting location of the defect of the second defect type is determined, and the first voltage or time period is preferably determined in dependence on the distance between the starting location of the defect of the second defect type and the second electrode, thereby allowing the location of the defect of the second defect type in the dielectric layer to be adjusted.

[0012] It is preferred that a temperature is determined, which together with the temperature determines the rate of migration of defects of the second defect type within the dielectric layer, and the first voltage is determined depending on the rate of migration of the defects of the second defect type, such that when the first voltage is applied at the temperature and for the period of time, defects of the second defect type will reach the second electrode within or at the end of the period, and / or the period is determined depending on the rate of migration of the defects of the second defect type, such that when the first voltage is applied at the temperature and for the period of time, defects of the second defect type will reach the second electrode within or at the end of the period.

[0013] In one embodiment, defects of a second defect type are present in the dielectric layer, and the method additionally includes determining a second voltage with a polarity opposite to that of the first voltage for applying a load to the dielectric layer, determining a time period and a temperature for the load, and applying the second voltage between the first electrode and the second electrode at the temperature and for the time period. If the defects of the first defect type move at a different speed than the defects of the second defect type, the second defects can be displaced relative to the first defects. This allows a desired distribution of defects in the dielectric layer to be tailored. The defects of the second defect type can move in the same direction as the defects of the first defect type under the load of the first voltage. Furthermore, the defects of the second defect type can move in a direction opposite to the direction in which the defects of the first defect type move under the load of the first voltage.

[0014] The method may envisage placing this semiconductor component in an actuator, a MEMS, a micromirror, a print head or a speaker, among others. An apparatus for manufacturing a semiconductor component or an actuator includes regulating and / or control mechanisms configured to carry out the steps in the method.

[0015] The apparatus preferably includes a contact mechanism for the wafer, the wafer including a first electrode, a second electrode, and a dielectric layer disposed between the first and second electrodes, the contact mechanism configured to apply a voltage between the first and second electrodes of the wafer based on settings of the adjustment and / or control mechanism.

[0016] Further advantageous embodiments are evident from the following description and drawings. [Brief description of the drawings]

[0017] [Figure 1] 1 is a schematic diagram of a first embodiment of a semiconductor component; [Diagram 2] 1 is a schematic diagram of an apparatus for manufacturing semiconductor components; [Figure 3a] FIG. 3a illustrates steps in a method for manufacturing the first embodiment. [Figure 3b] FIG. 3b illustrates steps in a method for manufacturing the first embodiment. [Figure 3c] FIG. 3c illustrates a step in a method for manufacturing the first embodiment. [Figure 3d] FIG. 3d illustrates a step in a method for manufacturing the first embodiment. [Figure 4] 1 is a graph showing the density of the distribution of defects at the starting position. [Diagram 5] 13 is a graph showing the density of the distribution of defects at the final position. [Figure 6] 1 is a graph showing the density of the distribution during regular operation. [Figure 7] 1 is a graph showing a current transition. [Figure 8] FIG. 2 is a schematic diagram of a second embodiment of a semiconductor component. [Figure 9] 5A-5D show steps in a method for manufacturing the second embodiment. [Figure 10] 1 is a graph showing the distribution of defects. [Figure 11] 1 is a graph showing a shift in distribution. [Figure 12] 1 is a graph showing the distribution of defects at the end of a move. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] 1 shows a schematic diagram of a semiconductor component 100 according to a first embodiment. The semiconductor component 100 includes a first electrode 102, a second electrode 104, and a dielectric layer 106. The dielectric layer 106 is disposed between the first electrode 102 and the second electrode 104. In this example, the first electrode 102 and the second electrode 104 are disposed on opposite sides of the dielectric layer 106.

[0019] Defects D1 of a first defect type are present in the dielectric layer. These defects D1 are located in a starting position in this example, which is defined in this example by the manufacturing process of the dielectric layer. In particular, the defects D1 are located closer to the second electrode 104 than to the first electrode 102.

[0020] The first defect type, defects D1, are charged defects that, depending on their charge, move to the boundary layer between the dielectric layer 106 and the first electrode 102 or the second electrode 104, respectively, when a potential is applied between them. This boundary layer is hereinafter referred to as the "interface". This transport of the charged defects is determined by the defect properties and the "hopping mechanism".

[0021] The hopping mechanism in this context means that the defects move, i.e. hop, in the electric field E acting in the dielectric layer 106 of thickness d due to the respective applied voltage U. The defects of defect type i are spaced apart by an average effective spacing a i This means that the defect of defect type i moves along the localized defect state at a velocity v i Velocity v i is explained via the known approach of variable region hopping.

[0022]

number

[0023] In the formula, C 0,i (a i ) is the distribution of defects with respect to location, expressed as a characteristic velocity v of defect i in the dielectric layer 106. i The defect distribution represents the properties of the dielectric layer 106, which together determine the migration of defects of defect type i within the dielectric layer 106. The defect parameters of defect type i, the decay length α, the average effective spacing a i , activation energy E A,0,i , charge N q,i is a physical property. k B Let T denote the temperature around the considered defect, specifically the temperature within the dielectric layer 106.

[0024] Leakage current density J until dielectric breakdown TED The time course of can be determined by the equations of the thermionic emission diffusion theory by Crowell and Sze.

[0025]

number

[0026] where q is the unit charge, N C is the effective density of states in the conduction band, v R is the effective recombination velocity, v D is the effective diffusion rate,

[0027]

number

[0028] represents the effective Schottky barrier, kB is the Boltzmann constant, T is the ambient temperature, and U is the voltage across the dielectric layer 106. Positively charged defects i move to the negative electrode and accumulate at the interface. Negatively charged defects i move to the positive electrode and accumulate at the interface. This results in an effective Schottky barrier

[0029]

number

[0030] changes. Barrier height change ΔΦ produced by defect i i is its maximum height δΦ i and the characteristic time constant τ i The characteristic time constant τ i is the change in barrier height ΔΦ i defines the duration over which changes most strongly along time t.

[0031]

number

[0032] Maximum height δΦ i is the number of defects i, Z i It is a function of and depends on the type of interface.

[0033]

number

[0034] describes the time-dependent accumulation of the statistical distribution of defects i in the material, and in particular the time of accumulation of the respective starting positions. The starting positions are in this example the centroids of the distribution. In case there are several peaks of defects of defect type i, one of these peaks can be selected instead of the centroids to define the starting position. Preferably, the peak with the greatest impact on the lifetime extension is selected.

[0035] Various defect types may exist in the dielectric layer 106. Depending on their charge, the effective Schottky barrier

[0036]

number

[0037] The barrier height change ΔΦ that increases i This reduces the leakage current level. In this context, the defects are exemplarily referred to as "healing" defects. Based on their charge, the effective Schottky barrier

[0038]

number

[0039] The barrier height change ΔΦ that reduces i , which causes the leakage current level to increase. In this context, the defects are illustratively referred to as "degrading" defects. Detailed below are techniques for manipulating the defect centroid location of "healing" and "degrading" defects through targeted electrical loading, possibly under varying temperatures and voltages.

[0040] Activation Energy E A,0,i and charge N q,i Due to the difference in temperature and / or voltage, the transport velocities of the defects involved can be very significantly altered relative to one another, and thus the relative positions of the defect distributions can be altered. The starting position of the defect distribution in the dielectric layer 106 of thickness D can be manipulated in a targeted manner.

[0041] Applying a voltage causes the defects to move. Depending on the activation energy and charge, certain defects can be dominated faster. By shifting the defects this way and that way by changing the voltage, voltage polarity, and temperature, the distribution of defects can be manipulated in a targeted way.

[0042] The starting location of defect i is, in this example, the distance d between the center of gravity of the distribution of defect i and the interface to which defect i is aimed during normal operation of semiconductor component 100. i is defined by therefore, a) The defect configuration, i.e. the time sequence or the arrangement of starting positions of the accumulation of defects i, may be varied. b) In order to optimize lifetime or leakage current levels, the defect center of the defect i associated with degradation may be moved away from the interface that is intended for it during normal operation of the semiconductor component 100 . c) In order to optimize the leakage current level or to achieve a stabilization of the interface, the defect centers of the defect i associated with the repair may already be accumulated at the interface.

[0043] The choice of voltage, field strength and / or temperature at which the targeted loading is performed can be optimized for the respective defect configuration. Under elevated field strength and at elevated temperature the process can be accelerated decisively. However, generally more defects can be accumulated at lower voltages, since the voltage-dependent threshold of the defect density at the interface for dielectric breakdown is higher than at higher voltages. Different kinetics / populations of the existing defect species under temperature and voltage can also be taken into account in order to obtain the optimum conditions of time and action.

[0044] An effective way to realize the manufacturing process is to perform the loading at wafer level, i.e. a full-surface deposited stack, for example including at least two electrodes and a dielectric layer therebetween, can be preloaded over the entire wafer instead of loading the layer elements of each manufactured component individually.

[0045] The time constant τ for the movement under the influence of the first voltage U1 i is the time constant τ for the movement under the influence of the second voltage U2 i The time constant τ ican be defined by the mobility of defect i under the influence of an electric field E in the dielectric layer 106 and the path it follows in the dielectric layer 106 to reach the respective interface. As it moves within the dielectric layer 106, the distance d between the center of gravity of its distribution and the interface i The speed v i together with the characteristic time constant τ for the accumulation process of defect i i but,

[0046]

number

[0047] And so it is brought about. From the measurement of the leakage current over time, the evaluation of the time-dependent transition using the equation of thermionic emission diffusion theory by Crowell and Sze, and the time-dependent behavior of the change in the barrier height, the time constant τ i can be determined. τ under various temperatures T and voltages U i By multiple measurements of A,0,i and charge N q,i can be determined.

[0048] Application of a first voltage U1 having a first polarity causes a charged defect D1 of a first defect type to move in a first direction towards the first electrode 102. Application of a second voltage U2 having an opposite polarity to the first voltage U1 causes the charged defect D1 of the first defect type to move in a second direction towards the second electrode 102.

[0049] Charged defects D1 of a first defect type that reach the interface at the first electrode 102 or the second electrode 104 accumulate at the interface. The semiconductor component 100 according to the first embodiment may have more than two electrodes, and more than one dielectric layer between each of the two electrodes.

[0050] In such semiconductor components, dielectric breakdown may occur when voltage is applied to the components for operation. Dielectric breakdown may result in partial or total destruction of the interface. Dielectric breakdown may result in a shortened life span of the semiconductor component 100. Dielectric breakdown may occur, for example, when the number of charged defects accumulated at the interface exceeds a voltage-dependent threshold.

[0051] Optimizing the process conditions and / or process controls during the manufacture of the dielectric layer 106 can affect the physical properties and the manufacturing effects on the physical properties, thereby improving lifetime.

[0052] The process conditions and / or process controls may, for example, affect the growth, growth conditions, material composition, etc. The process conditions and / or process controls may, for example, result in intentional or unintentional doping and / or contamination during the growth process or in subsequent processes.

[0053] The lifetime of the semiconductor component 100 is increased by targeted alteration of the starting location of the defects D1 of the first defect type after fabrication of the dielectric layer 106 having the above physical properties, as described below.

[0054] In FIG. 2, an apparatus 200 for manufacturing a semiconductor component 100 according to a first embodiment is shown diagrammatically. The apparatus 200 includes a regulation and / or control mechanism 202 configured to perform steps in the below-described method for manufacturing the semiconductor component 100 according to the first embodiment. The apparatus 200 is at least temporarily connectable to a first electrode 102 of the semiconductor component 100 via a first conductor 204. The apparatus 200 is at least temporarily connectable to a second electrode 104 of the semiconductor component 100 via a second conductor 206.

[0055] The regulating and / or control mechanism 202 is configured to output a first voltage U1, in this example, having a first polarity, such that the first voltage U1 is applied between the first electrode 102 and the second electrode 104 when the first electrode 102 and the second electrode 104 are connected to the device 200 by respective conductors and the regulating and / or control mechanism 202 outputs the first voltage U1.

[0056] The regulating and / or control mechanism 202 is configured to output a second voltage U2, in this example having a polarity opposite to the first polarity, in which case the second voltage U2 is applied between the first electrode 102 and the second electrode 104 when the first electrode 102 and the second electrode 104 are connected to the device 200 by respective conductors and the regulating and / or control mechanism 202 outputs the second voltage U2.

[0057] The control mechanism may be configured to output a substantially constant value of the first voltage U1 and / or the second voltage U2, for example in the range 1 volt to 80 volts, preferably 1 volt, 2 volts or 5 volts or 10 volts or 20 volts or 40 or 80 volts.

[0058] Dielectric layer 106 is preferably formed as a polycrystalline oxide high-κ insulator. The dielectric layer 106 is formed, inter alia, as a PZT layer. PZT is in this case Pb(Zr x Ti 1-x )O3.

[0059] The dielectric layer 106 is formed in particular as a KNN layer. KNN in this case is x Na 1-x )NbO3. The dielectric layer 106 may be, among others, a HfO2 layer, a HfZrO2 layer, a ZrO2 layer, a BaTiO3 layer, a SrTiO3 layer, or a (Ba x Sr 1-x ) TiO3 layer.

[0060] The dielectric layer 106 is preferably doped, for example a PZT layer doped with nickel. Pb(Zr x Ti 1-x )O3Ni y Both the PZT and KNN layers can have dopings other than nickel, such as Nb, La, Mn, Mg.

[0061] The dielectric layer is preferably formed as a sputtered PZT layer. In this case, a so-called target material is deposited on the substrate in a plasma. PZT is used as the target material, for example. The sputtered PZT layer preferably has a deposition temperature of less than 500° C. in this connection.

[0062] The thickness of the dielectric layer is preferably in the range of 500 nm to 4 μm. This is a range that is meaningful for actuator devices. The layer thickness is preferably 1 μm or 4 μm. Larger layer thicknesses are also possible. The procedure described above is feasible for all layer thicknesses.

[0063] Smaller layer thicknesses are also possible. For applications, e.g. away from actuator devices, it is preferred that the thickness of the dielectric layer is in the range of less than 500 nm. An example in this respect is the application of high-κ insulators, e.g. as memory. The memory can be a resistive memory ReRAM or a ferroelectric memory FeRAM. For these other applications, thicknesses between 15 nm and 200 nm make sense, depending on the application.

[0064] In addition to this, very thin high-κ insulators, for example with layers as gate oxides, can be used in many applications. For the dielectric layer 106, for example HfO2 or SiO2 with a layer thickness of 50 nm or less can be envisaged.

[0065] The regulating mechanism can be formed to regulate the first voltage U1 to a setpoint value, which is for example in the range 1 volt to 80 volts, preferably 1 volt, 2 volts or 5 volts or 10 volts or 20 volts or 40 volts or 80 volts.

[0066] The regulating mechanism can be formed to regulate the second voltage U2 to a setpoint value, which is for example in the range of 1 volt to 80 volts, preferably 1 volt, 2 volts or 5 volts or 10 volts or 20 volts or 40 volts or 80 volts.

[0067] In this case, provision may be made for a voltage measurement mechanism to be configured to capture the voltage between the first electrode 102 and the second electrode 104. The adjustment mechanism is then configured to reduce a control deviation that is determined depending on the difference between this captured voltage and a setpoint value.

[0068] For example, a wafer is fabricated having a dielectric layer 106 disposed between a first electrode 102 and a second electrode 104 . The apparatus 200, in this example, optionally includes a heating mechanism 208. The heating mechanism 208 is configured to heat the dielectric layer 106, in this example.

[0069] The heating mechanism 208 can be a furnace, in which case the wafer is temperature regulated within the furnace. The heating mechanism 208 may be implemented as a heating coil. The heating mechanism 208 is disposed on the dielectric layer 106 in this example. The heating mechanism 208 is disposed electrically and / or electromagnetically insulated from the dielectric layer 106 in this example. It may be disposed on a side of one of the electrodes not facing the dielectric layer 106 accordingly. The heating mechanism 208 may be removably disposed on the first electrode 102. The heating mechanism 208 may be removably disposed on the second electrode 104. The heating mechanism 208 may be removably disposed on the dielectric layer 106.

[0070] The heating mechanism 208 may be disposed externally in a housing around the semiconductor component 100. Within this housing, the dielectric layer 106 and the first and second electrodes 102, 104 may be disposed. The heating mechanism 208 may be removably disposed in the housing.

[0071] In this example, the heating mechanism 208 is electrically heatable via a first contact 210 and a second contact 212 . The regulating and / or control mechanism 202, in this example, is at least temporarily connectable to the first contact 210 via a third conductor 214 and to the second contact 212 via a fourth conductor 216. The regulating and / or control mechanism 202, in this example, is configured to output a current I1 to cause a current I1 through the heating mechanism 208.

[0072] The apparatus 200, in this example, optionally includes a voltage and / or current source 218. The apparatus 200, in this example, includes a computing mechanism 220, in particular a microprocessor, configured to carry out the methods described below.

[0073] The control mechanism may be configured to output a substantially constant value of the current I1, for example within a range that causes the heating mechanism 208 to heat the dielectric layer to a temperature between 100°C and 200°C. The regulating mechanism may be formed to regulate the current I1 to a setpoint value, which is for example in a range in which the heating mechanism 208 heats the dielectric layer to a temperature between 100° C. and 200° C. In this case, a temperature measuring mechanism may be provided, which is formed to capture the temperature of the dielectric layer 106. The regulating mechanism is then formed to reduce a control deviation, which is determined depending on the difference between this captured temperature and the setpoint value. The temperature may also be captured elsewhere, for example at the housing, at the heating mechanism 208 or at a point around the dielectric layer 106.

[0074] A method for manufacturing a semiconductor component 100 according to the first embodiment is explained below on the basis of FIG. 3a. The method adjusts the location of the defect centroids by targeted electrical loading as a step in the manufacturing process. Defects associated with interface degradation can be moved further away from the target interface under operating conditions, i.e., from the interface where these defects accumulate due to their charge depending on the polarity used during the specified operation of the semiconductor component 100. This extends the life. In this regard, the maximum distance to the target interface during operation is the complete accumulation of substantially all defects at the opposite interface.

[0075] The method defines in this example the following steps: Step 302 A dielectric layer 106 is disposed between the first electrode 102 and the second electrode 104 .

[0076] Within the dielectric layer 106 are defects of a first defect type D1. 4 shows a schematic representation of the density ρ of the distribution 400 of defects of a first defect type D1 along the extension x of the dielectric layer 106 at a starting position 402, i.e., the center of gravity, of the distribution 400 at the beginning of the application of the first voltage U1. The density ρ of the defects of the first defect type D1 is greatest at the starting position 402 and drops off sharply with increasing distance from the starting position 402. In this example, the density ρ tends to zero at the location 408 of the first electrode 102 and at the location 406 of the second electrode 104. The defects of the first defect type D1 move in a direction 404 away from the location 406 of the second electrode 104 towards the location 408 of the first electrode 102 during the application of the first voltage U1.

[0077] Step 304: Determine a time period for moving the defects D1 of the first defect type to the target location in the dielectric layer. The period can be selected shorter as the first voltage U1 increases in the case of a constant or increasing temperature. The period can be selected shorter as the temperature increases in the case of a constant or increasing first voltage U1. The period can be defined in the range of 1 minute to 60 minutes, in the range of 1 hour to 24 hours or more than one day. The period can be, for example, 3 hours, 1 day, 2 days or 3 days long.

[0078] The time period may be determined for the maximum possible lifetime based on the starting location 402 of the first defect type defect D1. The time period may be selected shorter than the time period for achieving the maximum lifetime based on time constraints in the manufacturing process in which the method is used, or based on lower requirements for the lifetime of the semiconductor component 100, or based on considerations regarding the stability of the interface at the first electrode 102 after the first defect type defect D1 is displaced thereto.

[0079] It may be contemplated that the temperature may be set based on the conditions of normal operation, and it may be contemplated to set the temperature for operation at a higher or lower temperature.

[0080] The test may be intended to determine the starting position of the defect, its velocity under the conditions, and its activation energy and charge. For example, tests are performed varying the first voltage U1 and temperature used until suitable conditions are found.

[0081] For example, a first time to first dielectric breakdown is determined in the normal operation of the semiconductor component 100 without the prior application of the first voltage U1. The first time represents the time it takes for the defects D1 of the first defect type to move from the starting position until they accumulate at the deteriorating interface enough to cause dielectric breakdown. In the test, for example, different first voltages U1 are applied to different semiconductor components 100 at different temperatures for different durations. For example, a second time to first dielectric breakdown during normal operation is determined for each of these processed semiconductor components 100. For example, a first voltage U1, temperature, and duration are determined from the test for the manufacturing process, where the second time is three times the first time.

[0082] If the duration thus found is too long to be economically realizable, it may be attempted to find conditions under which the duration is shorter, in particular without the second time being shorter, for example by increasing the temperature, for example by increasing the first voltage U1.

[0083] It may be contemplated to look for a first voltage U1 having a particularly large ratio of duration to the second time. The test preferably starts with a first voltage U1 of, for example, 1 V and a temperature of, for example, 200° C., and in subsequent tests increases the first voltage U1 and / or the temperature.

[0084] It may be provided that a goal defect structure is selected, which has a maximum distance between the starting positions of all defects D1 of the first defect type or a selected starting point for the defects D1 of the first defect type and the interface deteriorating during the specified operation. This may be done under the basic condition that the proportion of defects D1 of the first defect type that accumulate at the opposite interface is smaller than a critical threshold. It may be provided that a duration of application of the first voltage U1 is determined, among other things, an economically feasible load time. It may be provided that the test searches for a combination of temperature and first voltage U1, at which temperature and for which duration the number of defects D1 of the first defect type that accumulate at the opposite interface when the voltage U1 is applied is smaller than a critical threshold.

[0085] A weighted sum can be determined that defines, among other things, the number of different degrading defect types. For example, in addition to the defect D1 of the first defect type, further defects are contained in the semiconductor component 100 that move in the same direction as the defect D1 of the first defect type under the first voltage U1. By taking into account, among other things, the number of these effects in the weighted sum, it is avoided that too many of these defects accumulate at the interface during the duration of the first voltage U1.

[0086] The period of time may be determined by testing a portion of a wafer from which semiconductor component 100 is fabricated, as described below. Step 306 determines the first voltage U1 and the temperature for loading with the first voltage U1 to move these defects in the dielectric layer 106.

[0087] Steps 302, 304, and 306 may be performed in this order or one of the other orders. Step 308 applies a first voltage between the first electrode 102 and the second electrode 104 for a period of time.

[0088] This causes the defect D 1 of the first defect type to move in the direction 404 . 5 shows a schematic representation of the density ρ of the distribution 400 of defects D1 of a first defect type along the extension x of the dielectric layer 106 at a final position, i.e., at the end of the time period. The density ρ of the defects D1 of the first defect type is greatest at position 502, i.e., the centroid of the distribution 400, and drops off sharply with increasing distance from position 502. In this example, the density ρ tends to zero at location 406 of the first electrode 102 and location 406 of the second electrode 104.

[0089] A defect D1 of the first defect type may move in a direction 504 away from the location 408 of the first electrode 102 toward the location 406 of the second electrode 104 while the second voltage U2 is applied during normal operation. Most defects D1 of the first defect type must travel a distance 506 between the position 502 and the location 406 of the second electrode 104 before reaching the location 406 of the second electrode 104.

[0090] The first voltage U1 or duration may be determined depending on the properties of the dielectric layer 106 characterizing the starting position of the first defect type defect D1 and the properties characterizing the speed of movement of the first defect type defect within the dielectric layer.

[0091] The first voltage U1 or the period may be determined depending on the distance between the starting position and the target position. In this example, the period for defects D1 of the first defect type is selected such that the period is smaller than the time constant t1 determined for these defects with respect to movement in a first direction toward the first electrode 102.

[0092] To determine this time constant t1, the method may for example envisage the following steps illustrated in FIG. 3002 A first voltage U1 is applied to another semiconductor component, in particular manufactured in the same manufacturing process as the semiconductor component 100 or with the same charge as the semiconductor component 100. The first voltage U1 is preferably applied at a set temperature.

[0093] 3004 detects a change in the current flowing through the first and second electrodes of the other semiconductor component. 6 shows a schematic representation of the density ρ of the distribution 400 of defects D1 of the first defect type along the extension x of the dielectric layer 106. The density ρ of the defects D1 of the first defect type is highest at the location 602 and drops off sharply with increasing distance from the location 602. In this example, the density ρ increases at the location 406 of the second electrode 104, where the defects D1 of the first defect type that have accumulated during operation of the semiconductor component 100 at the second voltage U2 have accumulated. The defects D1 of the first defect type that have accumulated at the interface cause leakage current. In this example, the density ρ tends to zero at the location 408 of the first electrode 102.

[0094] 3006 Measure the duration of application of the first voltage U1 until dielectric breakdown is detected. This duration defines the time constant t1. 3008 Determine the target position or period depending on the duration.

[0095] Steps 3002, 3004, 3006, and 3008 are optional. It may be contemplated that these steps are performed before step 302. Instead of determining the time constant t1 in this way, it may be envisaged to determine the starting position of the defect D1 of the first defect type, as shown in FIG. 3c, in the following steps:

[0096] 3102 A first voltage U1 is applied to another semiconductor component, in particular manufactured in the same manufacturing process as the semiconductor component 100 or with the same charge as the semiconductor component 100. From the current progression over time, a first duration is determined during which a characteristic time τ1 for the accumulation of defects of defect type 1 at the interface (102) can be derived.

[0097] The first voltage U1 is preferably applied at a set temperature. 3104 A second voltage U2 is applied to another semiconductor component, notably manufactured in the same manufacturing process as the semiconductor component 100 or with the same charge as the semiconductor component 100. From the current progression over time a second duration is determined, during which a characteristic time τ2 for the accumulation of defects of defect type 1 at the interface (104) can be derived. The second voltage U2 is applied in this example with the same voltage magnitude as the first voltage U1 and with opposite polarity to the first voltage U1. Thus the expected rate of defects D1 of the first defect type in the dielectric layer 106 is the same.

[0098] 3106. Determine a starting position of the defect D1 of the first defect type from the ratio of the first duration to the second duration, the ratio being proportional to the ratio of both partial distances from the starting position to the first electrode 102 and from the starting position to the second electrode 104. In this example, based on the known layer thickness of the dielectric layer, the starting position of the defect D1 of the first defect type is determined from this ratio.

[0099] 3108 Determine the length of at least one of the partial distances. Depending on the length and duration of these partial distances, determine the velocity of the defect D1 of the first defect type. Depending on the layer thickness and the velocity, determine the time constant t1.

[0100] As a further alternative, the following procedure illustrated in FIG. 3d may be contemplated. 3202 A second voltage U2 is applied to another semiconductor component, particularly one manufactured in the same manufacturing process as the semiconductor component 100 or with the same charge as the semiconductor component 100.

[0101] The first voltage U2 is preferably applied at a set temperature. 3204 detects a change in the current flowing through the first and second electrodes of this other semiconductor component.

[0102] 6 shows a schematic representation of the density ρ of the distribution 400 of defects D1 of the first defect type along the extension x of the dielectric layer 106. The density ρ of the defects D1 of the first defect type is highest at the location 602 and drops off sharply with increasing distance from the location 602. In this example, the density ρ increases at the location 406 of the second electrode 104, where the defects D1 of the first defect type that have accumulated during operation of the semiconductor component 100 at the second voltage U2 have accumulated. The defects D1 of the first defect type that have accumulated at the interface cause leakage current. In this example, the density ρ tends to zero at the location 408 of the first electrode 102.

[0103] 3206 Measure the duration of application of the second voltage U2 until dielectric breakdown is detected. This duration defines the time constant t2. 3208 Determine the target position or period depending on the duration.

[0104] 7 shows a first current profile 702 over time t for this case. The portion of the wafer on which the first current profile 702 is measured was operated for one day at a first voltage U1=+5. The first current profile 702 is for a temperature of 150° C. and a second voltage U2, which produces an electric field strength E=50 kV / cm at the negative pole of the first electrode 102. In this example, the electric field strength is 2.2×10 5 In this example, dielectric breakdown occurs in 1×10 -6 Dielectric breakdown occurs when a current surge into amperes occurs.

[0105] 7 shows a second current profile 704 for operation of another portion of the wafer operated at the same second voltage U2 and the same temperature. The second current profile 704 occurs when this portion of the wafer is operated at the first voltage U1=+5 for two days with otherwise unchanged parameters. In this example, the current profile is 2.9×10 5 In this example, dielectric breakdown occurs in 1×10 -6 Dielectric breakdown occurs when a current surge into amperes occurs.

[0106] 7 shows a third current profile 706 for operation of another portion of the wafer operated at the same second voltage U2 and the same temperature. The third current profile 706 occurs when this portion of the wafer is operated at the first voltage U1=+5 for three days with otherwise unchanged parameters. In this example, the current profile is 3.5×10 5 In this example, dielectric breakdown occurs in 1×10 -6 Dielectric breakdown occurs when a current surge into amperes occurs.

[0107] 7 shows the current profile 708 for the operation of a wafer that has not been processed after preparation and is operated at the same second voltage U2 and at the same temperature. Unprocessed in this context means that the wafer has not been operated at the first voltage U1. In this example, the current profile 708 is 1.5×10 5 In this example, dielectric breakdown occurs in 1×10 -6Dielectric breakdown has occurred when a current jump to amperes occurs. The time that has passed from the application of the second voltage U2 to the dielectric breakdown is a measure for the starting position of the defect D1 of the first defect type. The starting position can be determined depending on the speed of the defect D1 of the first defect type in the dielectric layer 106, if the time, temperature, and second voltage U2 are known. For maximum life of the semiconductor component 100, it may be contemplated to select the interface at the first electrode 102 as the target position. The duration during which the displacement of the defect D1 of the first defect type from this starting position to there occurs is readily known for this temperature and second voltage U2. For a different second voltage U2 or a different temperature, the duration can be determined using the speed depending on the distance between the starting position and the interface at the first electrode 102. For the same voltage and the same temperature, any desired target position can be selected. If the starting position is known, the velocity can be used to determine the duration from the distance between the starting position and the target position, i.e. the distance the first defect type defect D1 must travel to reach the target position.

[0108] It can then be checked whether the duration until the current change is ascertained, is it one day? The period can be selected shorter as the second voltage U2 increases in the case of a constant or an increasing temperature. The period can be selected shorter as the temperature increases in the case of a constant or an increasing second voltage U2. The period can be defined in the range of 1 minute to 60 minutes, in the range of 1 hour to 24 hours or more than one day. This process can be carried out for various durations, for example 3 hours or 2 or 3 days.

[0109] Instead of detecting a change in current, a change in the surface properties of the first electrode 102 and / or a change in the properties of the boundary layer between the first electrode 102 and the dielectric layer 106 may be detected. It may be contemplated that a temperature T characterizing a speed v1 of migration of defects D1 of the first defect type in the dielectric layer 106 is determined.

[0110] In this case, it may be intended that the first voltage is determined depending on the speed v1 so that when the first voltage is applied during that period, the defect D1 of the first defect type reaches the target position within that period or at the end of that period.

[0111] In this case, it may be intended that the period is determined depending on the speed v1 such that when a first voltage is applied during that period, the defect D1 of the first defect type reaches the target position within that period or at the end of that period.

[0112] The defect D1 of the first defect type moves in a first direction to a target position in a time period determined for it upon application of a first voltage U1. Then, in the normal operation of the semiconductor component 100, the defect D1 of the first defect type moves in a second direction from the target position towards the second electrode upon application of a second voltage U2. The target position is defined by a goal set to be achieved, for example that the semiconductor component has a lifetime of more than 2 days, which is longer than its lifetime without pre-treatment.

[0113] 8 is a schematic diagram of a semiconductor component 100 according to a second embodiment. The semiconductor component 100 according to the second embodiment is implemented like the semiconductor component 100 according to the first embodiment with respect to a defect D1 of a first defect type. In contrast to the first embodiment, in the second embodiment a defect D2 of a second defect type is additionally present in the dielectric layer. The defect D2 is in this example located at a different starting position than the defect D1 due to the manufacturing process of the dielectric layer 106. The defect D2 is located, in particular, closer to the second electrode 104 than to the first electrode 104.

[0114] The semiconductor component 100 according to the second embodiment is formed like the semiconductor component 100 according to the first embodiment with respect to the application of the first voltage U1 and the second voltage U2, and with respect to the movement of the defects D1 of the first defect type within the dielectric layer 106. In addition, charged defects D2 of the second defect type may be movable by the first voltage U1 in the same direction as the defects D1 of the first defect type or in the opposite direction.

[0115] The semiconductor component 100 according to the second embodiment may have more than two electrodes, and more than one dielectric layer between each of the two electrodes. The process conditions and / or process controls may, for example, affect the growth, growth conditions, material composition of the first defect type defects D1 and / or the second defect type defects D2, and may, for example, result in intentional or unintended doping and / or contamination during the growth process or in a subsequent process.

[0116] The lifetime of the semiconductor component 100 is increased by targeted alteration of the starting location of defects D1 of a first defect type and / or targeted alteration of the starting location of defects D2 of a second defect type after fabrication of the dielectric layer 106 having the above physical properties, as described below.

[0117] A method for manufacturing the semiconductor component 100 according to the second embodiment will now be described with reference to FIG. By this method, by targeted electrical loading as a step in the manufacturing process, the defect centroid locations of the defects D2 of the "to be repaired" second defect type may be accumulated generally at the "deteriorating" interface during the normal operation of the semiconductor component 100. By this method, the defect centroid locations of the defects D2 of the "to be repaired" second defect type may be maintained at this interface during the normal operation of the semiconductor component 100 by measures described below. In addition, leakage current levels may be reduced, which is advantageous for many applications as it may improve the signal-to-noise ratio and / or reduce energy losses due to leakage currents.

[0118] The method in this example includes the following steps: 902 A dielectric layer 106 is disposed between the first electrode 102 and the second electrode 104 . Within the dielectric layer 106 are defects of a first defect type D1 and defects of a second defect type D2.

[0119] 904 Determine a time period for moving the defects D1 of the first defect type to a target location in the dielectric layer 106. The period may be determined for the maximum possible lifetime. The period may be selected to be shorter than the period for achieving the maximum lifetime based on time constraints in the manufacturing process in which the method is used, or based on lower requirements for the lifetime of the semiconductor component 100, or based on considerations regarding the stability of the interface at the first electrode 102 after a defect D1 of the first defect type is displaced thereto.

[0120] 906 Determine a first voltage U1 and a temperature for loading with the first voltage U1 to move these defects in the dielectric layer 106. The first voltage U1 and the temperature may be set based on the conditions of operation as specified. It may be set to operate at a higher temperature or a higher voltage or at a lower temperature or a lower voltage.

[0121] The first voltage U1 or the duration may be determined depending on the distance between the starting position of the defect D2 of the second defect type and the second electrode 102. In particular, it may be intended that the temperature T around the defect D2 of the second defect type is determined, and this temperature T together determines the velocity v2 of the movement of the defect D2 of the second defect type within the dielectric layer 106.

[0122] The first voltage U1 can be determined depending on the speed v2 of movement of the defect D2 of the second defect type such that when the first voltage U1 is applied during that period, the defect D2 of the second defect type reaches the second electrode 104 within that period or at the end of that period 104.

[0123] The period can be determined depending on the speed v2 of movement of the second defect type defect D2 such that when the first voltage U1 is applied during that period, the second defect type defect D2 reaches the second electrode 104 within or at the end of that period.

[0124] If the period thus found is too long to be economically feasible, it may be attempted to find a condition with a shorter period, for example by increasing the temperature, for example by increasing the first voltage U1.

[0125] It may be provided to select a goal defect structure, which has a maximum distance between the starting positions of all defects D1 of the first defect type or a selected starting point for the defects D1 of the first defect type and the interface deteriorating during the specified operation. This may be done under the basic condition that the proportion of defects D1 of the first defect type that accumulate at the opposite interface is smaller than a critical threshold. As the duration of the application of the first voltage U1, a load time that is inter alia economically feasible may be defined. It may be provided to search for a combination of temperature and first voltage U1, at which temperature and for which duration the number of defects D1 of the first defect type that accumulate at the opposite interface when the voltage U1 is applied is smaller than a critical threshold.

[0126] 908 A first voltage U1 is applied between the first electrode 102 and the second electrode 104 for that period of time. In addition, the method may contemplate the following steps before step 902 or before step 904.

[0127] 900-A A first voltage U1 is applied to the semiconductor component 100. 900-B detects changes in the current flowing through the first and second electrodes. 900-C Measure the duration of application of the first voltage U1 until detection.

[0128] 900-D Determine target position or period depending on duration. In step 900-D, it may be contemplated that a characteristic of the dielectric layer 106 is determined that represents a starting position for the defects D2 of the second defect type. In this case, a target position or time period is determined such that most of the defects D2 of the second defect type are at a desired position in the dielectric layer 106 when the defects D1 of the first defect type reach their target position.

[0129] If the desired positions of the defects D1 of the first defect type and / or the defects D2 of the second defect type cannot be adjusted by one application of the first voltage U1, the method may contemplate applying the first voltage U1 at a first temperature for a first duration, applying the second voltage U2 at a second temperature for a second duration, and then applying the first voltage U1 again at the first temperature. The implementation of these steps may be iterative. The voltage and / or temperature may be changed for each iteration. For example, the first voltage U1 may be applied at a temperature T=200° C., and then the second voltage U2 may be applied at a temperature T=100° C. This may be repeated multiple times. This exploits the different voltage and temperature accelerations that occur for different defects.

[0130] It may be envisaged to consider several load iterations. Load iterations with varying temperatures and voltages may be considered. These voltages and temperatures may be envisaged to be determined such that the basic condition is always met that under these conditions accumulation at the deteriorating interface does not lead to a first dielectric breakdown. It is preferable to start with one load step and one iteration at a high temperature, for example 175° C., and a low voltage, for example 5 V. If the duration required to reach the target position is longer than the load time, it is preferable to increase the temperature. If a dielectric breakdown is reached, it is preferable to decrease the first voltage U1.

[0131] Instead of detecting a change in current, a change in the surface properties of the first electrode 102 and / or a change in the properties of the boundary layer between the first electrode 102 and the dielectric layer 106 may be detected. Instead of applying the first voltage U1 to the semiconductor component 100, steps 900-A to 900-D may be performed on another semiconductor component 100 having the same characteristics as this semiconductor component 100.

[0132] The change in the distribution of defects will now be described with reference to FIGS. 10 shows a distribution 1002 of defects D1 of a first defect type with its centroid near location 406 of second electrode 104 and a distribution 1004 of defects D2 of a second defect type with its centroid near location 408 of first electrode 102. The defects D2 of the second defect type provide a defect buffer for the interface at the first electrode 102.

[0133] FIG. 11 shows that the distribution 1002 of defects D1 of the first defect type moves away from the location 406 of the second electrode 104 towards the location 408 of the first electrode 102. FIG. 11 shows that the distribution 1004 of defects D2 of the second defect type moves away from the location 408 of the first electrode 102 towards the location 406 of the second electrode 104.

[0134] When applying a second voltage U2 at temperature T, the velocity v1 of movement of the defect D1 of the first defect type is greater than the velocity v2 of movement of the defect D2 of the second defect type. In this example, the velocity v1 of the defect D1 of the first defect type and the defect D2 of the second defect type are selected such that the velocity v1 is sufficient for the defect D1 of the first defect type to overcome the distance between the first electrode 102 and the second electrode before the defect D2 of the second defect type can move away from the interface at velocity v2.

[0135] 12 shows a distribution 1002 of defects D1 of a first defect type with its center of gravity near the location 408 of the first electrode 102 and a distribution 1004 of defects D2 of a second defect type with its center of gravity near the location 408 of the first electrode 102. The defects D2 of the second defect type offset the defects D1 of the first defect type at the interface, thereby avoiding or delaying dielectric breakdown and / or causing less leakage current than would be possible without this location of the defects D2 of the second defect type, thereby increasing lifetime.

[0136] The above method is to determine the occurrence and location of the "desired" defect, i.e., its starting location, e.g., the distance d between the defect and the desired interface. i can be replenished by influencing

[0137] This can be done, for example, by adding an additional layer of the material used for dielectric layer 106 that is highly defective near the electrodes at the desired interface. The insertion of displaceable defects is also possible by doping, for example by diffusion or ion implantation.

[0138] Adjustment of process conditions that favor the generation of defects may also be contemplated. For example, from a layer with a minimal oxygen vacancy density, a layer with many oxygen vacancies may be generated near the electrodes at the desired interface, for example by reducing the oxygen partial pressure during sputtering deposition or by changing the sol composition during chemical solution deposition (CSD) and / or by changing the temperature and / or additional annealing at the end of the deposition during CSD. The defects of this layer can then be used as a buffer in a targeted manner.

[0139] The defects D2 of the second defect type are in this example selected to counteract the effect of the defects D1 of the first defect type in lowering the effective Schottky barrier. The defects D2 of the second defect type are moved by the method to a specific location in the dielectric layer 106 where they become a defect buffer. The defect buffer in the dielectric layer 106 or in the additional layer thus produced has a defect density of, for example, 10^16 / cm2 ~10^18 / cm 2 density of defect buffers. Defect buffers with lower or higher densities of repairing defects are feasible.

[0140] In the case of the semiconductor component 100 according to the second embodiment, defects D2 of a second defect type that can offset the defects D1 of the first defect type are taken into account. It may also be intended to take into account defects D3 of a third defect type that can cause a dielectric breakdown like the defects D1 of the first defect type. Dielectric breakdown occurs, for example, when the number of charged defects D3 of the third defect type that accumulate at the interface exceeds a threshold value. If this exceeds and a dielectric breakdown occurs, the interface is also partially or completely destroyed. This may result in a shortened lifetime of the semiconductor component 100, especially if the defects D3 of the third defect type reach the interface before the defects D1 of the first defect type.

[0141] The determination of the starting position of the defect D3 of the third defect type and the displacement of the starting position are performed as described for the defect D1 of the first defect type. The period during which the first voltage U1 is applied is determined in this example depending on the defect that first arrives at the interface to be protected during normal operation. Optionally, this period is the maximum period during which the first voltage U1 allows the defect D3 of the third defect type and the defect D1 of the first defect type to move, but the defect D1 of the first defect type and the defect D3 of the third defect type cannot accumulate at the interface.

[0142] The method described above may contemplate that the semiconductor component 100 is arranged in an actuator, a MEMS, a micromirror, a print head, or a speaker, among others.

Claims

1. A method for manufacturing a semiconductor component (100), comprising the steps of: disposing (302, 902) a dielectric layer (106) between a first electrode (102) and a second electrode (104) of the semiconductor component (100), wherein defects (D1) of a first defect type are present in the dielectric layer (106); determining (304, 904) a time period for moving the defects (D1) of the first defect type to a target location in the dielectric layer (106); determining (306, 906) a first voltage for moving the defect (D1) in the dielectric layer (106); determining a temperature for loading at the first voltage (306, 906); applying (308, 908) the first voltage between the first electrode (102) and the second electrode (104) at the temperature and for the period of time. the first voltage or the period is determined depending on a property of the dielectric layer (106) characterizing a starting position of a defect (D1) of the first defect type and a property characterizing a speed of movement of the defect (D1) of the first defect type within the dielectric layer (106), the first voltage or the period being determined depending on a distance between the starting position and the target position.

2. A method for manufacturing a semiconductor component (100), comprising: disposing (302, 902) a dielectric layer (106) between a first electrode (102) and a second electrode (104) of the semiconductor component (100), wherein defects (D1) of a first defect type are present in the dielectric layer (106); determining (304, 904) a time period for moving the defects (D1) of the first defect type to a target location in the dielectric layer (106); determining (306, 906) a first voltage for moving the defect (D1) in the dielectric layer (106); determining a temperature for loading at the first voltage (306, 906); applying (308, 908) the first voltage between the first electrode (102) and the second electrode (104) at the temperature and for the period of time; The method according to claim 1, characterized in that the temperature is determined, the temperature together determining a speed of movement of defects of the first defect type in the dielectric layer, the first voltage is determined depending on the speed such that when applying the first voltage for the period of time, a defect of the first defect type (D1) reaches the target position within or at the end of the period, and / or the period is determined depending on the speed such that when applying the first voltage for the period of time, a defect of the first defect type reaches the target position within or at the end of the period.

3. A method for manufacturing a semiconductor component (100), comprising: disposing (302, 902) a dielectric layer (106) between a first electrode (102) and a second electrode (104) of the semiconductor component (100), wherein defects (D1) of a first defect type are present in the dielectric layer (106); determining (304, 904) a time period for moving the defects (D1) of the first defect type to a target location in the dielectric layer (106); determining (306, 906) a first voltage for moving the defect (D1) in the dielectric layer (106); determining a temperature for loading at the first voltage (306, 906); applying (308, 908) the first voltage between the first electrode (102) and the second electrode (104) at the temperature and for the period of time. a defect (D1) of the first defect type is movable in a first direction toward the first electrode (102) when a first voltage having a first polarity is applied between the first electrode (102) and the second electrode (104), and the defect (D1) of the first defect type is movable in a second direction toward the second electrode (104) when a second voltage having a second polarity opposite to the first polarity is applied between the first electrode (102) and the second electrode (104); The method comprises: applying the second voltage; detecting a change in the current flowing through the first and second electrodes and / or a change in a surface property of the first electrode (102) and / or a change in a property of the boundary layer between the first electrode (102) and the dielectric layer (106); measuring the duration of application of the second voltage until said detection; determining the target position or the duration in dependence on the duration; The method further comprising:

4. A method for manufacturing a semiconductor component (100), comprising: disposing (302, 902) a dielectric layer (106) between a first electrode (102) and a second electrode (104) of the semiconductor component (100), wherein defects (D1) of a first defect type are present in the dielectric layer (106); determining (304, 904) a time period for moving the defects (D1) of the first defect type to a target location in the dielectric layer (106); determining (306, 906) a first voltage for moving the defect (D1) in the dielectric layer (106); determining a temperature for loading at the first voltage (306, 906); applying (308, 908) the first voltage between the first electrode (102) and the second electrode (104) at the temperature and for the period of time. the dielectric layer (106) includes defects (D2) of a second defect type movable in a direction toward the second electrode (104) upon application of the first voltage; The method comprises: detecting (900-B) a change in the current flowing through the first or second electrode when applying the first voltage and / or a change in the surface properties of the second electrode and / or a change in the properties of the boundary layer between the second electrode and the dielectric layer that occurs when applying the first voltage; measuring the duration of application of the first voltage until said detection (900-C); determining (900-D) the target position or the period depending on the duration; The method further comprising:

5. A method for manufacturing a semiconductor component (100), comprising: disposing (302, 902) a dielectric layer (106) between a first electrode (102) and a second electrode (104) of the semiconductor component (100), wherein defects (D1) of a first defect type are present in the dielectric layer (106); determining (304, 904) a time period for moving the defects (D1) of the first defect type to a target location in the dielectric layer (106); determining (306, 906) a first voltage for moving the defect (D1) in the dielectric layer (106); determining a temperature for loading at the first voltage (306, 906); applying (308, 908) the first voltage between the first electrode (102) and the second electrode (104) at the temperature and for the period of time. A further defect type (D2) is present in the dielectric layer (106); The method comprises: determining a further voltage having an opposite polarity to the first voltage for stressing the dielectric layer (106); determining a duration and a temperature for said loading; applying said further voltage between said first electrode (102) and said second electrode (104) at said temperature for said period of time; The method further comprising:

6. 5. The method of claim 4, wherein a characteristic of the dielectric layer (106) characterizing a starting position of a defect (D2) of the second defect type is determined, and the first voltage or the period is determined depending on the distance between the starting position of the defect (D2) of the second defect type and the second electrode.

7. 7. The method according to claim 4 or 6, characterized in that a temperature is determined, said temperature together determining a speed of migration of the defects (D2) of the second defect type in the dielectric layer, and said first voltage is determined depending on the speed of migration of the defects (D2) of the second defect type at said temperature and for said period of time such that when applying said first voltage at said temperature and for said period of time the defects (D2) of the second defect type reach said second electrode (104) within said period or at the end of said period and / or said period is determined depending on the speed of migration of the defects (D2) of the second defect type at said temperature and for said period of time such that when applying said first voltage at said temperature and for said period of time the defects (D2) of the second defect type reach said second electrode (104) within said period or at the end of said period.

8. A method according to any one of claims 1 to 7, characterized by a step of arranging the semiconductor component in a memory or actuator, in particular a MEMS, a micromirror, a print head or a speaker.

9. An apparatus (200) for manufacturing a semiconductor component or an actuator or a memory, characterized in that the apparatus (200) includes an adjustment and / or control mechanism (202) configured to perform the steps of the method according to any one of claims 1 to 8.

10. The apparatus (200), comprising: a contact mechanism (204, 206) for a wafer; the wafer includes a first electrode (102), a second electrode (104), and a dielectric layer (106) disposed between the first electrode (102) and the second electrode (104); the contact mechanism (204, 206) is configured to apply a voltage between the first electrode (102) and the second electrode (104) of the wafer based on settings of the adjustment and / or control mechanism (202); 10. The apparatus (200) of claim 9.

Citation Information

Patent Citations

  • Regenerating method for piezoelectric element

    JP1994342946A

  • Vibration measuring apparatus

    JP2007227854A

  • Driving method of piezo electric element, piezo electric element, and piezo electric element applied device

    JP2016144289A

Cited By

  • Semiconductor element monitoring device and semiconductor element monitoring method

    JP2024502092A