Tagged container, tag fixing method and tag fixing structure

The use of condensation reaction type silicone rubber with specific surface features on containers ensures precise RFID tag positioning, addressing positioning challenges and enhancing reading accuracy in RFID-tagged containers.

JP7580240B2Active Publication Date: 2024-11-11SHIN ETSU POLYMER CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020180462
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-28
Publication Date
2024-11-11
Estimated Expiration
2040-10-28

AI Technical Summary

Technical Problem

Conventional RFID-tagged containers face challenges in accurately positioning the RFID tags, leading to interference and unclear correspondence when multiple containers are lined up for reading.

Method used

The use of condensation reaction type silicone rubber with a concave mounting portion and convex or recessed features on the container surface to securely embed the RFID tag, ensuring precise positioning and orientation.

Benefits of technology

This method allows for accurate and stable fixation of RFID tags, preventing wave interference and ensuring clear identification of tagged containers during reading, even when stacked.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007580240000002
    Figure 0007580240000002
  • Figure 0007580240000003
    Figure 0007580240000003
  • Figure 0007580240000004
    Figure 0007580240000004
Patent Text Reader

Abstract

To provide a container with a tag allowing accurate positioning of an RFID tag fixed to the container, a fixing method of a tag, a fixing structure of a tag, and a package used therefor.SOLUTION: In a container 1 with a tag having a container 10, an RFID tag 20 and a fixing material 30 formed of condensation reaction type silicone rubber, a recessed fitting part 12 is formed on the outer surface 11a of a bottom part 11 of the container 10, multiple protrusions 16 are formed on an inner face 14 of the fitting part 12, and the RFID tag 20 is buried in the fitting part 12 by the fixing material 30, in a state of in contact with the protrusions 16.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a tagged container and a method for fixing the tag. and Fixed tag structure To make Regarding. [Background technology]

[0002] For example, when collecting reproductive cells or tissues from a patient before anti-cancer treatment and storing them frozen, it is necessary to carefully manage which patient each sample in a container such as a centrifuge tube or sampling tube belongs to. In this type of management, identification using RFID tags (electronic tags) is used to avoid human error.

[0003] Patent Document 1 discloses attaching an electronic tag to a cap attached to a container. Patent Document 2 discloses providing a cover part at the bottom of the container and disposing an electronic tag between the bottom of the container and the cover part. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2001-356688 A [Patent Document 2] JP 2006-168757 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, with conventional tagged containers such as those described in Patent Documents 1 and 2, it is difficult to accurately position the RFID tag when fixing it to the container. In particular, when multiple tagged containers are lined up, if the position of each RFID tag is not accurate, radio waves will cross when reading information from each RFID tag, and the correspondence between the read information and the container may become unclear.

[0006] An object of the present invention is to provide a tagged container that facilitates accurate positioning of an RFID tag fixed to a container, a tag fixing method, a tag fixing structure, and a package used therewith. [Means for solving the problem]

[0007] The present invention has the following aspects. [1] A method for manufacturing a container, an RFID tag, and a fixing material, The fixing material is made of a condensation reaction type silicone rubber, A recessed mounting portion is formed on an outer surface of the container, A plurality of protrusions are formed on the inner surface of the mounting portion, The RFID tag is embedded in the mounting portion with the fixing material while being in contact with the protrusion. [2] A method for manufacturing a device comprising: a container; an RFID tag; and a fixing material; The fixing material is made of a condensation reaction type silicone rubber, A recessed mounting portion is formed on an outer surface of the container, The mounting portion has an inner surface formed with one or more recesses, The RFID tag is embedded in the mounting portion with the fixing material while being in contact with the portion of the inner surface surrounding the recess. [3] A tagged container according to [1] or [2], wherein the condensation reaction type silicone rubber has self-adhesive properties. [4] The tagged container according to any one of [1] to [3], wherein the condensation reaction type silicone rubber has a Williams plasticity at 25° C. in an uncrosslinked state in the range of 100 to 600. [5] A method for fixing an RFID tag to a container, comprising: A recessed mounting portion is formed on the outer surface of the container, A plurality of protrusions are formed on the inner surface of the mounting portion, A method for fixing a tag, comprising the steps of: bringing the RFID tag into contact with the protruding portion, and embedding the RFID tag in the mounting portion using a fixing material made of uncrosslinked condensation reaction type silicone rubber. [6] A method for fixing an RFID tag to a container, comprising: A recessed mounting portion is formed on the outer surface of the container, The mounting portion has an inner surface formed with one or more recesses, A method for fixing a tag, comprising the steps of: bringing the RFID tag into contact with the area surrounding the recess on the inner surface; and embedding the RFID tag in the mounting portion using a fixing material made of uncrosslinked condensation reaction type silicone rubber. [7] The method for fixing a tag described in [5] or [6], wherein the condensation reaction type silicone rubber has self-adhesive properties. [8] The method for fixing a tag according to any one of [5] to [7], wherein the condensation reaction type silicone rubber has a Williams plasticity at 25° C. in an uncrosslinked state in the range of 100 to 600. [9] A tag fixing structure in which an RFID tag is fixed to a container, A recessed mounting portion is formed on the outer surface of the container, A plurality of protrusions are formed on the inner surface of the mounting portion, A tag fixing structure, in which the RFID tag is embedded in the mounting portion with a fixing material made of condensation reaction type silicone rubber while in contact with the protrusion.

[10] A structure in which an RFID tag is fixed to a container, A recessed mounting portion is formed on the outer surface of the container, The mounting portion has an inner surface formed with one or more recesses, A tag fixing structure, in which the RFID tag is embedded in the mounting portion with a fixing material made of condensation reaction type silicone rubber, with the RFID tag in contact with the portion surrounding the recess on the inner surface.

[11] A tag fixing structure according to [9] or

[10] , wherein the condensation reaction type silicone rubber has self-adhesive properties.

[12] The tag fixing structure according to any one of [9] to

[11] , wherein the condensation reaction type silicone rubber has a Williams plasticity at 25°C in an uncrosslinked state in the range of 100 to 600.

[13] A package in which a fixing material made of condensation reaction type silicone rubber and an RFID tag are vacuum-packed as a single unit.

[14] The package described in

[13] , wherein the condensation reaction type silicone rubber has self-adhesive properties.

[15] The package according to

[13] or

[14] , wherein the condensation reaction type silicone rubber has a Williams plasticity at 25°C in an uncrosslinked state in the range of 100 to 600. Effect of the Invention

[0008] According to the present invention, it is possible to provide a tagged container that facilitates accurate positioning of an RFID tag fixed to a container, a tag fixing method, a tag fixing structure, and a package used therefor. [Brief description of the drawings]

[0009] [Figure 1] 2 is a cross-sectional view of a tagged container according to an embodiment, cut in the height direction. FIG. [Diagram 2] 2 is an enlarged cross-sectional view showing the bottom of the tagged container of FIG. 1. [Diagram 3] 2 is a bottom view of the mounting portion of the tagged container of FIG. 1. [Figure 4] 13 is a cross-sectional view of the attachment portion of a tagged container according to another embodiment. [Diagram 5] 5 is a bottom view of the mounting portion of the tagged container of FIG. 4. [Figure 6] 13 is a cross-sectional view of the attachment portion of a tagged container according to another embodiment. [Figure 7] 13 is a bottom view of the mounting portion of a tagged container according to another embodiment. FIG. [Figure 8] 13 is a bottom view of the mounting portion of a tagged container according to another embodiment. FIG. [Figure 9] 13 is an enlarged cross-sectional view showing the bottom of a tagged container according to another embodiment. FIG. [Figure 10] 13 is an enlarged cross-sectional view showing an upper portion of a tagged container according to another embodiment. FIG. [Figure 11] 13 is an enlarged cross-sectional view showing the bottom of a tagged container according to another embodiment. FIG. [Figure 12] 12 is a bottom view of the mounting portion of the tagged container of FIG. 11. [Figure 13] 13 is an enlarged cross-sectional view showing the bottom of a tagged container according to another embodiment. FIG. [Figure 14]13 is a bottom view of the mounting portion of a tagged container according to another embodiment. FIG. [Figure 15] 15 is a cross-sectional view of the attachment portion of the tagged container shown in FIG. 14 . [Figure 16] 16 is a cross-sectional view showing a state in which an RFID tag is embedded in the attachment part of FIG. 15 using a fixing material. [Figure 17] 13 is a cross-sectional view of a tagged container according to another embodiment, cut in the height direction. FIG. [Figure 18] FIG. 11 is a cross-sectional view showing a tagged container according to another embodiment. [Figure 19] FIG. 2 is a cross-sectional view showing the packaging body of the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. Note that the dimensions of the drawings shown in the following description are merely examples, and the present invention is not necessarily limited thereto, and can be appropriately modified and implemented without departing from the spirit and scope of the present invention.

[0011] [First embodiment] As shown in FIGS. 1 and 2, a tagged container 1 of this embodiment includes a container 10, an RFID (Radio Frequency Identification) tag 20, and a fixing material 30. The tagged container 1 includes a container 10, an RFID (Radio Frequency Identification) tag 20, and a fixing material 30.

[0012] The container 10 is cylindrical with a bottom, with an opening 10a formed at the top. The bottom 11 of the container 10 is semispherical, and a concave mounting portion 12 is formed on its outer surface (bottom surface) 11a. When the container 10 is cut in the height direction along the central axis, the cross-sectional shape of the mounting portion 12 is approximately rectangular. The inner surface 14 of the bottom of the mounting portion 12 is perpendicular to the central axis of the container 10.

[0013] The shape of the container 10 is not limited to that of this example. The tagged container 1 may be provided with a lid member that closes the opening 10a at the top of the container 10 in an openable and closable manner. The vessel 10 is not particularly limited, and examples thereof include culture vessels such as centrifuge tubes and sampling tubes.

[0014] FIG. 3 is a bottom view of the mounting portion 12 provided on the bottom portion 11 of the container 10 as viewed from the bottom side, with the fixing material 30 omitted. 2 and 3, a plurality of hemispherical protrusions 16 are provided on the inner surface 14 of the bottom of the mounting part 12, which is rectangular when viewed from the bottom side. The RFID tag 20 is embedded in the mounting part 12 with the fixing material 30 in a state where the RFID tag 20 is in contact with the tip of each of the protrusions 16 in the height direction. By providing a plurality of protrusions 16, the RFID tag 20 can be stably contacted with each of the protrusions 16 while allowing the excess fixing material 30 present on the protrusion 16 side of the RFID tag 20 to escape between the protrusions 16 when embedding. This prevents the excess fixing material 30 from remaining on the inner surface 14 side of the RFID tag 20 in the mounting part 12 and causing the RFID tag 20 to tilt, thereby improving the accuracy of the mounting position and mounting direction of the RFID tag 20.

[0015] The height of the multiple protrusions 16 may be set so that the RFID tag 20 fixed in the mounting part 12 while in contact with the protrusions 16 can be controlled to a desired position and orientation. The multiple protrusions 16 in this example have the same height. Therefore, the RFID tag 20 embedded in the mounting part 12 while in contact with each protrusion 16 is parallel to the inner surface 14 of the bottom of the mounting part 12.

[0016] The height of the multiple protrusions 16, i.e., the distance from the inner bottom surface 14 of the mounting portion 12 to the tip of the protrusion 16, can be appropriately set depending on the size of the RFID tag 20 within a range in which the RFID tag 20 can be fixed by embedding it in uncrosslinked condensation reaction type self-adhesive silicone rubber, and can be, for example, 0.1 to 3.0 mm.

[0017] The shape of the protrusion 16 is not limited to a hemisphere, and may be, for example, a cylinder, a square prism, a cone, or a truncated cone. The maximum diameter of the protrusion 16 as viewed from the tip side may be appropriately set according to the dimensions of the RFID tag 20. In this example, the number of protrusions 16 is 16. The number of protrusions 16 is not limited to 16 and may be appropriately set according to the dimensions of the RFID tag 20, and may be, for example, 3 or more. In this example, the arrangement pattern of the multiple protrusions 16 on the inner surface 14 of the mounting portion 12 is a lattice arrangement aligned vertically and horizontally in a 4 x 4 pattern. Note that the arrangement pattern of the multiple protrusions 16 is not limited to a lattice arrangement, and may be, for example, a staggered arrangement.

[0018] The pitch P (FIG. 3) between the multiple protrusions 16 is preferably set appropriately according to the length and width of the RFID tag 20. For example, when the length and width of the RFID tag 20 are 3.2 mm and 3.2 mm, the pitch P is preferably 3.2 mm or less, and when it is 1.6 mm or less, the RFID tag 20 can be fixed by four protrusions 16. When the length and width of the RFID tag 20 are 1.2 mm and 1.2 mm, the pitch P is preferably 1.2 mm or less, and preferably 0.6 mm or less, for the same reason. The lower limit of the pitch P is limited by the size of the protrusions 16. The larger the pitch P, the more easily the excess fixing material 30 present on the protrusion 16 side of the RFID tag 20 is pushed out between the protrusions 16 and pushed out around the RFID tag 20 when embedding, and the positioning of the RFID tag 20 in the mounting part 12 becomes easier. The pitch P between the protrusions 16 is the distance between the centers of the protrusions 16 when the protrusions 16 are viewed from the tip side. If the shape of the protrusions 16 when viewed from the tip side is not a perfect circle, the center of the circumscribing circle of that shape is taken as the center of the protrusions 16. Even if the protrusions 16 are arranged in a staggered pattern, the pitch P may be set as described above.

[0019] In this embodiment, all of the 16 protrusions 16 provided on the inner surface 14 of the mounting portion 12 are in contact with the RFID tag 20 to fix the RFID tag 20, but the present invention may be such that some of the multiple protrusions are in contact with the RFID tag. For example, as shown in Figures 4 and 5, the RFID tag 20 may be fixed in a state where only the four protrusions 16 located in the center out of the 16 protrusions 16 are in contact with the RFID tag 20. Note that Figure 5 is a bottom view of the mounting portion 12 with the fixing material 30 omitted. In the case of protruding convex portions 16 having a hemispherical or other shape, it is preferable that the RFID tag 20 contacts three or more convex portions 16, since this increases the accuracy of the attachment position and attachment direction of the RFID tag 20.

[0020] In this way, when only some of the multiple protrusions 16 are in contact with the RFID tag 20, the pitch P between the protrusions 16A in contact with the RFID tag 20 is A and the pitch P between the convex portions 16B that are not in contact with the RFID tag 20. B The pitch P between the protrusions 16A in contact with the RFID tag 20 may be the same or different. A The preferred range of the pitch P is the same as the preferred range of the pitch P between the protrusions 16B that are not in contact with the RFID tag 20. B may be larger than the preferable upper limit of the pitch P described above, in that the condensation reaction type self-adhesive silicone rubber can easily get in between and escape.

[0021] The protrusions 16 are not limited to the hemispherical protrusions in this example, and may be ridges. In the case of the ridge-shaped protrusions 16, the cross-sectional shape perpendicular to the length direction of the protrusions 16 is not particularly limited, and examples thereof include a semicircular shape, a triangular shape, a rectangular shape, and a grid shape. The width and length of the protrusions 16 formed on the ridges may be appropriately set according to the dimensions of the RFID tag 20. In the case of the protruding protrusions 16, it is preferable that the RFID tag 20 contacts two or more protrusions 16, since this increases the accuracy of the attachment position and attachment direction of the RFID tag 20.

[0022] The material constituting the container 10 is not particularly limited, and examples thereof include resins such as polypropylene, polyethylene, polycarbonate, polyamide, and polyethylene terephthalate, and glass. Among these, polypropylene is preferable because of its excellent transparency, moldability, and light weight. The material constituting the container 10 may be one type or two or more types. The method for manufacturing the container 10 is not particularly limited, and in the case of a resin container 10, for example, injection molding can be mentioned.

[0023] The RFID tag 20 is capable of transmitting and receiving data to and from a corresponding reader in a non-contact manner. There are no particular limitations on the RFID tag 20, and any known RFID tag can be used. The RFID tag 20 may or may not have a built-in battery. The RFID tag 20 may be of an electromagnetic induction type or a radio wave type. The shape of the RFID tag 20 is not particularly limited, and examples include a rectangular parallelepiped, a sphere, an egg, a card, a coin, a stick, and a label.

[0024] The fixing material 30 is made of condensation reaction type silicone rubber. The fixing material 30 is a non-liquid condensation reaction type silicone rubber having a Williams plasticity of 100 to 600, preferably 150 to 450, at 25°C in an uncrosslinked state. The uncrosslinked condensation reaction type silicone rubber has the Williams plasticity and can maintain a self-supporting shape and can be deformed according to a pressing force. The uncrosslinked condensation reaction type silicone rubber can be deformed according to the shapes of the mounting part 12 and the RFID tag 20 to embed the RFID tag 20. The amount of condensation reaction type silicone rubber to be embedded in the mounting part 12 needs to be set to an amount that sufficiently embeds the RFID tag 20, and is appropriately set by adjusting the width, length, and thickness of the condensation reaction type silicone rubber to be used according to the structure of the mounting part 12 and the dimensions of the RFID tag 20. The shape of the condensation reaction type silicone rubber is not particularly limited, and examples thereof include a sheet shape, a dumpling shape, and a hemispherical shape. From the viewpoints of facilitating accurate fixing of the RFID tag 20 and providing excellent workability, it is preferable that the condensation reaction type silicone rubber is formed in advance into a sheet shape with a thickness, width, and length corresponding to the embedding amount. The above-mentioned Williams plasticity is measured using a parallel plate plasticity meter (Williams Plastometer) in accordance with the measurement method specified in JIS K 6249 "Test methods for uncured and cured silicone rubber".

[0025] The condensation reaction type silicone rubber may include, for example, one containing an organopolysiloxane and a crosslinking agent. The condensation reaction type silicone rubber may also contain additives such as a curing catalyst and a filler.

[0026] Examples of the organopolysiloxane include a diorganopolysiloxane represented by the following formula (1) and a diorganopolysiloxane represented by the following formula (2). The organopolysiloxane may be one type or two or more types.

[0027] [ka]

[0028] In the formulas (1) and (2), R is a monovalent hydrocarbon group. A is an oxygen atom or -(CH2) m - (wherein m is 1 to 8). n is an arbitrary number. B is a hydrolyzable group. x is 2 or 3.

[0029] The hydrocarbon group for R preferably has 1 to 12 carbon atoms, and more preferably has 1 to 10 carbon atoms. Examples of R include alkyl groups (methyl, ethyl, propyl, butyl, 2-ethylbutyl, octyl, etc.), cycloalkyl groups (cyclohexyl, cyclopentyl, etc.), alkenyl groups (vinyl, propenyl, butenyl, heptenyl, hexenyl, allyl, etc.), aryl groups (phenyl, tolyl, xylyl, naphthyl, diphenyl, etc.), and aralkyl groups (benzyl, phenylethyl, etc.). R may be a hydrocarbon group in which at least a part of the hydrogen atoms bonded to the carbon atoms is replaced with a halogen or a cyano group (chloromethyl, trifluoropropyl, 2-cyanoethyl, 3-cyanopropyl, etc.). R may be one type or two or more types.

[0030] A is preferably an oxygen atom or an ethylene group. n is the kinematic viscosity of the polyorganosiloxane at 25°C of 100 to 1,000,000 cm 2 / s, and the kinematic viscosity is preferably in the range of 500 to 500,000 cm 2 / s is more preferable.

[0031] Examples of B include alkoxy groups (such as a methoxy group, an ethoxy group, a propoxy group, and a butoxy group), ketoxime groups (such as a dimethylketoxime group and a methylethylketoxime group), acyloxy groups (such as an acetoxy group), and alkenyloxy groups (such as an isopropenyloxy group and an isobutenyloxy group).

[0032] The diorganopolysiloxane may have a branched structure. The organopolysiloxane can be produced by a known method.

[0033] Examples of the crosslinking agent include silanes having two or more, preferably three or more, hydrolyzable groups in one molecule, or partial hydrolysis condensates of the silanes. Examples of the hydrolyzable groups include alkoxy groups (methoxy groups, ethoxy groups, butoxy groups, etc.), ketoxime groups (dimethylketoxime groups, methylethylketoxime groups, etc.), acyloxy groups (acetoxy groups, etc.), alkenyloxy groups (isopropenyloxy groups, isobutenyloxy groups, etc.), amino groups (N-butylamino groups, N,N-diethylamino groups, etc.), and amide groups (N-methylacetamide groups, etc.). Among these, alkoxy groups, ketoxime groups, acyloxy groups, and alkenyloxy groups are preferred. The crosslinking agent may be one type or two or more types.

[0034] The amount of the crosslinking agent in the condensation reaction type silicone rubber is preferably 1 to 50 parts by mass, more preferably 2 to 30 parts by mass, and even more preferably 5 to 20 parts by mass, per 100 parts by mass of the organopolysiloxane.

[0035] The curing catalyst is not particularly limited, and examples thereof include alkyl tin ester compounds (dibutyltin diacetate, etc.), titanate esters or titanium chelate compounds (tetraisopropoxytitanium, etc.), other organometallic compounds (zinc naphthenate, etc.), aminoalkyl group-substituted alkoxysilanes (3-aminopropyltriethoxysilane, etc.), amine compounds or their salts (hexylamine, etc.), quaternary ammonium salts (benzyltriethylammonium acetate, etc.), lower fatty acid salts of alkali metals (potassium acetate, etc.), dialkylhydroxylamine (dimethylhydroxylamine, etc.), and silanes or siloxanes having a guanidyl group (tetramethylguanidylpropyltrimethoxysilane, etc.). The crosslinking agent may be one type or two or more types.

[0036] The amount of the curing catalyst in the condensation reaction type silicone rubber is preferably 0 to 20 parts by mass, more preferably 0.001 to 10 parts by mass, and even more preferably 0.01 to 5 parts by mass, per 100 parts by mass of the organopolysiloxane.

[0037] The filler is not particularly limited, and examples thereof include reinforcing agents (silica such as fumed silica, zeolite, etc.), fibrous fillers (glass fiber, carbon fiber, cellulose nanofiber, etc.), and basic fillers (calcium carbonate, etc.). Among these, silica, calcium carbonate, and zeolite are preferred, and fumed silica and calcium carbonate whose surfaces have been hydrophobized are more preferred.

[0038] The amount of the filler blended in the condensation reaction type silicone rubber is preferably 1 to 90% by volume, and more preferably 5 to 60% by volume, based on the total volume of the organopolysiloxane. This condensation reaction type silicone rubber may have self-adhesive properties. Condensation reaction type silicone rubber with self-adhesive properties adheres to materials that come into contact with it during the crosslinking process even without applying a primer or other treatment to the surface of the adherend, and will adhere to general RFID tags and, depending on the material of the container, will also adhere to these.

[0039] In the tag fixing structure of the present embodiment as described above, an RFID tag 20 is fixed to a container 10, in which a concave mounting portion 12 is formed on an outer surface 11a of a bottom 11 of the container 10, and a plurality of protrusions 16 are formed on an inner surface 14 of the mounting portion 12. The RFID tag 20 is embedded in the mounting portion 12 by a fixing material 30 in a state in which the RFID tag 20 is in contact with the protrusions 16.

[0040] A method for fixing the RFID tag 20 to the container 10 will now be described. In this embodiment, a fixing material 30 made of uncrosslinked condensation reaction type silicone rubber is used, and the RFID tag 20 is pushed into the mounting portion 12 of the container 10 together with the fixing material 30, and the RFID tag 20 is embedded in the mounting portion 12 by the fixing material 30 with the RFID tag 20 in contact with the protrusion 16.

[0041] The fixing material 30 made of condensation reaction type silicone rubber is not liquid in an uncrosslinked state but can maintain a self-supporting form, and is a plastic solid that can be deformed by a pressing force, so it deforms according to the force with which it is pressed into the mounting part 12, and excess fixing material 30 present on the convex parts 16 side of the RFID tag 20 is released between the convex parts 16 and is further pushed out around the RFID tag 20 in the mounting part 12 as necessary. The RFID tag 20 is then pressed into the mounting part 12 until it comes into contact with the tips of the convex parts 16. This allows the RFID tag 20 to be embedded and fixed in the mounting part 12 with the mounting position and mounting direction of the RFID tag 20 being controlled with high precision.

[0042] The method for pushing the RFID tag 20 is not particularly limited, and for example, the RFID tag 20 may be pushed in with a fingertip, tweezers, or the like. In that the force pressing the RFID tag 20 against the convex portion 16 is uniform and the RFID tag 20 is easily pushed in, and the attachment position of the RFID tag 20 is easily stabilized, it is preferable to push the RFID tag 20 in with a dedicated pushing tool that matches the dimensions of the attachment portion 12. For example, a tool having a head portion at the tip of a rod-shaped gripping portion, which has a shape complementary to the concave shape of the attachment portion 12 and can be pushed into the attachment portion 12, can be exemplified.

[0043] After the RFID tag 20 is embedded in the attachment portion 12, the uncrosslinked condensation reaction type silicone rubber of the fixing material 30 is left at room temperature, for example, whereby a hardening reaction proceeds due to moisture in the air. When the tagged container 1 is frozen and stored, it may be frozen after the condensation reaction type silicone rubber has hardened, or before crosslinking. The linear expansion coefficient of the condensation reaction type silicone rubber is not significantly different between the uncrosslinked state and the crosslinked state, and there is almost no adverse effect from freezing and storing it before hardening. Therefore, freezing and storing it in an uncrosslinked state has the advantage that it can be frozen and stored quickly without waiting for hardening. In addition, the linear expansion coefficient of the condensation reaction type silicone rubber is larger than that of polypropylene, and it shrinks more than polypropylene during the cooling process, so the fixing force of the RFID tag 20 is large.

[0044] Generally, the glass transition temperature (Tg) of condensation reaction type silicone rubber is about -70°C, which is lower than the Tg of polypropylene (about 0°C to -20°C), and condensation reaction type silicone rubber solidifies below the Tg and is maintained in an extremely low temperature state. If the temperature exceeds the Tg during the thawing process after frozen storage, the condensation reaction type silicone rubber returns to a solid state with plasticity, expands, and recovers the initial filling state, after which crosslinking proceeds.

[0045] For example, when the material of the container 10 is polypropylene, the fixing material 30 made of condensation reaction type silicone rubber does not adhere to the container 10, so that after storage, the RFID tag 20 can be removed from the container 10 together with the fixing material 30, and the RFID tag 20 can be peeled off from the fixing material 30, recovered, and reused. On the other hand, when the material of the container is polycarbonate, polyamide, or polyester, the fixing material 30 made of condensation reaction type silicone rubber having self-adhesiveness adheres and fixes to the container 10 by its self-adhesiveness during the crosslinking process. The adhesion of the RFID tag 20 to the covering material is also performed in the same manner. Examples of materials that seal and cover the RFID tag include epoxy resin, glass epoxy resin, ceramic, silicone resin, etc., and the condensation reaction type silicone rubber has self-adhesiveness with these resins. Therefore, it is easy to prevent the position shift or movement of the RFID tag at the contact surface between the RFID tag and the condensation reaction type silicone rubber.

[0046] As described above, in the tagged container 1 of the first embodiment, the RFID tag 20 is embedded in the attachment portion 12 of the container 10 by the fixing material 30 while in contact with the multiple protrusions 16, so that the positioning of the RFID tag 20 is highly accurate. As a result, even if multiple tagged containers 1 are lined up, for example, radio waves are less likely to cross when information is read from each RFID tag 20 by a reader from below each tagged container 1. Therefore, the correspondence between the read information and the tagged container 1 becomes clear, making it easy to identify them.

[0047] It should be noted that the first embodiment is not limited to the tagged container 1, the tag fixing structure in the tagged container 1, and the method of fixing the tag in the tagged container 1. 6, a through hole 17 extending in a direction intersecting the height direction may be formed in the middle of the height direction of the columnar protrusion 16. When such a through hole 17 is formed in the protrusion 16, the fixing material 30 also enters into the through hole 17 when the RFID tag 20 is embedded. The portion of the fixing material 30 that enters into the through hole 17 serves as a catch to prevent the fixing material 30 and the RFID tag 20 from falling off the attachment portion 12, making it easier to prevent the RFID tag 20 from falling off.

[0048] The shape of the mounting part 12, which is rectangular when viewed from the bottom side, is not limited to a rectangle and can be set appropriately, and may be, for example, a circular shape as shown in Fig. 7. Even in this embodiment, the RFID tag 20 may be in contact with only a portion of the multiple protrusions 16. Moreover, as shown in Fig. 8, the RFID tag 20 only needs to be in contact with the protrusions 16, and the dimensions and arrangement of the RFID tag 20 may be set so that the protrusions 16 in contact with the RFID tag 20 partially protrude from the RFID tag 20 when viewed from the tip side of the protrusions 16.

[0049] The tagged container may be the tagged container 2 illustrated in Fig. 9. The same parts in Fig. 9 as those in Fig. 2 are denoted by the same reference numerals and will not be described. The tagged container 2 has the same configuration as the tagged container 1 except that it has a convex portion 16C instead of the convex portion 16.

[0050] The protrusion 16C is a ridge-like protrusion having a trunk 16a rising from the inner bottom surface 14 of the mounting part 12 and a head 16b protruding on both sides in the width direction from the tip of the trunk 16a. In the tagged container 2, the head 16b of the protrusion 16C gets caught in the fixing material 30, which is advantageous in that the RFID tag 20 and the fixing material 30 are less likely to fall off the mounting part 12 unexpectedly.

[0051] The present invention is not limited to an embodiment in which an attachment portion for embedding an RFID tag is provided at the bottom of a container. For example, a tagged container 3 as illustrated in Fig. 10 may be used. The same parts in Fig. 10 as those in Figs. 1 and 2 are given the same reference numerals and will not be described. The tagged container 3 includes a container 10A, an RFID tag 20, and a fixing material 30. The container 10A includes a cylindrical container body 40 with a bottom having an opening 40a at the top, and a lid member 41 that can freely open and close the opening 40a of the container body 40.

[0052] The form of the lid member 41 is not particularly limited, and for example, it can be attached to the upper part of the container body 40 by screwing. In the tagged container 3, a concave mounting portion 42 is formed on the upper outer surface 41a of the lid member 41. A plurality of ridge-like protrusions 46 are provided in parallel on the inner surface 44 of the bottom of the mounting portion 42, similar to the mounting portion 12 of the tagged container 1. In this manner, the tagged container 3 is equipped with the lid member 41, and is similar to the tagged container 1 except that, instead of the tagged container 1 having the mounting portion 12 on the bottom 11 of the container 10, the tagged container 3 has the mounting portion 42 on the lid member 41.

[0053] The cross-sectional shape perpendicular to the length direction, height, width, length, number and pitch of the multiple protrusions 46 are similar to those of the protrusions 16 of the tagged container 1, and the preferred embodiments are also similar. The material constituting the container body 40 and the lid member 41 is not particularly limited, and may be the same as that exemplified for the container 10. The material constituting the container body 40 and the lid member 41 may be one type or two or more types.

[0054] In the tagged container 3 as well, the RFID tag 20 is embedded in the mounting portion 42 by the fixing material 30 with the RFID tag 20 in contact with the tip of each of the protrusions 46. This allows excess fixing material 30 present on the protrusion 46 side of the RFID tag 20 when embedding to escape between the protrusions 46, and furthermore, makes it easier to be pushed out around the RFID tag 20 in the mounting portion 42 as necessary. This makes it difficult for unexpected lumps of fixing material 30 to remain between the inner surface 44 of the mounting portion 42 and the RFID tag 20, and prevents the RFID tag 20 from tilting in the mounting portion 42 and becoming inaccurately positioned.

[0055] Furthermore, the convex portions 16 (16A, 16B), 16C, and 46 of the tagged containers 1 to 3 were projection-shaped, but the convex portions formed on the mounting portion of the tagged container of this embodiment are not limited to projection-shaped and may be ridges.

[0056] [Second embodiment] An example of the second embodiment of the present invention will be described below. As shown in Fig. 11 and Fig. 12, a tagged container 4 of this embodiment includes a container 10B, an RFID (Radio Frequency Identification) tag 20, and a fixing material 30. The container 10B has a similar configuration to the container 10, except that a groove-like recess 18 is formed on the inner surface 14 of the bottom of the attachment portion 12 instead of the protrusion 16.

[0057] In the container 10B, a plurality of recesses 18 are formed in parallel on the inner surface 14 of the bottom of the mounting part 12. The RFID tag 20 is embedded in the mounting part 12 by the fixing material 30 in a state of contacting the surrounding portion of each recess 18 on the inner surface 14 of the bottom of the mounting part 12. As a result, the excess fixing material 30 present on the recess 18 side of the RFID tag 20 when embedding is allowed to escape into the recess 18, and is easily pushed out around the RFID tag 20 in the mounting part 12 as necessary. Therefore, it is difficult for an unexpected lump of the fixing material 30 to remain between the inner surface 14 of the mounting part 12 and the RFID tag 20, and it is possible to prevent the RFID tag 20 from tilting in the mounting part 12 and becoming inaccurate in its position.

[0058] The depth, width, and length of the groove-like recess 18 may be appropriately set according to the dimensions of the RFID tag 20. The longer, deeper, and wider the recess 18, the easier it is for the excess fixing material 30 present on the recess 18 side of the RFID tag 20 to escape to the surroundings through the recess 18 when embedding, making it easier to position the RFID tag 20. As shown in FIG. 13, in this example, the groove-like recess 18 is formed so as to extend to the outside of the RFID tag 20 when viewed from the opening side of the mounting part 12 with the RFID tag 20 fixed. Note that the groove-like recess 18 may be formed so as to remain within the area where the RFID tag 20 is located when viewed from the opening side of the mounting part 12 with the RFID tag 20 fixed.

[0059] The depth of the groove-like recess 18, that is, the distance between the deepest part of the recess 18 and the inner surface 14 at the bottom of the attachment portion 12, can be, for example, 0.1 to 10 mm. The width of the groove-like recess 18 may be, for example, 0.3 to 10 mm.

[0060] In this example, the cross-sectional shape perpendicular to the length direction of the groove-shaped recess 18 is semicircular. Note that the cross-sectional shape of the recess 18 is not limited to a semicircular shape, and may be a triangular shape, a rectangular shape, or the like. The number of groove-like recesses 18 is one or more and may be appropriately set according to the dimensions of the RFID tag 20, and may be, for example, 1 to 30. When a plurality of groove-like recesses 18 are formed, the interval between adjacent recesses 18 can be, for example, 0.5 to 30 mm.

[0061] The tag fixing structure of this embodiment is a structure in which an RFID tag 20 is fixed to a container 10B, in which a concave mounting portion 12 is formed on the outer surface 11a of the bottom 11 of the container 10, and one or more recesses 18 are formed on the inner surface 14 of the mounting portion 12. The RFID tag 20 is embedded in the mounting portion 12 by a fixing material 30 in a state in which the RFID tag 20 is in contact with a portion surrounding the recess 18 on the inner surface 14 of the bottom of the mounting portion 12.

[0062] A method for fixing the RFID tag 20 to the container 10B will be described below. In this embodiment, a fixing material 30 made of uncrosslinked condensation reaction type self-adhesive silicone rubber is used, and the RFID tag 20 is pushed into the mounting portion 12 of the container 10B together with the fixing material 30, and the RFID tag 20 is embedded in the mounting portion 12 by the fixing material 30 while being in contact with the area surrounding the recess 18 on the inner surface 14 of the bottom of the mounting portion 12.

[0063] Since the fixing material 30 is in an uncrosslinked state, it deforms in response to the force with which it is pressed into the mounting part 12, and excess fixing material 30 present on the recess 18 side of the RFID tag 20 escapes into the recess 18 and, as necessary, is pushed out around the RFID tag 20 inside the mounting part 12. Then, by pressing the RFID tag 20 into the mounting part 12 until it comes into contact with the portion surrounding the recess 18 on the inner surface 14 of the bottom of the mounting part 12, the RFID tag 20 can be embedded in the mounting part 12 with the RFID tag 20 accurately positioned.

[0064] After embedding the RFID tag 20 in the attachment portion 12, the uncrosslinked condensation reaction type self-adhesive silicone rubber of the fixing material 30 is left at room temperature, for example, whereby a crosslinking reaction proceeds due to moisture in the air. When the tagged container 4 is frozen and stored, it may be frozen and stored after the condensation reaction type self-adhesive silicone rubber is crosslinked, or it may be frozen and stored without crosslinking, while maintaining the uncrosslinked state.

[0065] As described above, in the tagged container 4 of the second embodiment, the RFID tag 20 is embedded in the mounting part 12 of the container 10B by the fixing material 30 while being in contact with the portion surrounding the recess 18 on the inner surface 14 of the bottom of the mounting part 12, so that the positioning of the RFID tag 20 is highly accurate. Therefore, even when multiple tagged containers 4 are lined up, radio waves are unlikely to cross when information is read from the RFID tag 20 by a reader from below each tagged container 4, and the correspondence between the read information and the tagged container 4 becomes clear, making it easy to identify them.

[0066] The second embodiment is not limited to the tagged container 4, the structure for fixing the tag in the tagged container 4, and the method for fixing the tag in the tagged container 4. For example, the tagged container 5 shown in Fig. 13 may be used. The same parts in Fig. 13 as those in Fig. 12 are denoted by the same reference numerals and will not be described. The tagged container 5 has the same configuration as the tagged container 4, except that it has a recess 18A instead of the recess 18.

[0067] The recess 18A is a groove having a first groove portion 18a extending upward from the inner surface 14 of the bottom of the mounting portion 12, and a second groove portion 18b expanding to both sides in the width direction from an upper portion of the first groove portion 18a. In the tagged container 5, the fixing material 30 that enters the recess 18A is caught in the second groove portion 18b, which is advantageous in that the RFID tag 20 and the fixing material 30 are unlikely to fall off the mounting portion 12 unexpectedly.

[0068] The recesses formed on the inner surface of the mounting part are not limited to groove-shaped recesses. For example, as shown in Fig. 14 and Fig. 15, instead of groove-shaped recesses, a plurality of columnar recesses 18B may be formed on the inner surface 14 of the mounting part 12. Fig. 14 and Fig. 15 are a cross-sectional view and a bottom view showing the state before the RFID tag 20 is fixed to the mounting part 12 with a fixing material 30.

[0069] In this example, the cross-sectional shape of recess 18B cut perpendicularly to the depth direction is rectangular. The cross-sectional shape of recess 18B is not limited to a rectangle, and may be, for example, a circle or a triangle. The diameter of the opening of recess 18B may be appropriately set according to the dimensions of RFID tag 20. In this example, the number of recesses 18B is 52. Note that the number of recesses 18B is not limited to 52 and may be set appropriately depending on the size of the attachment portion 12, and may be, for example, 10 or more.

[0070] In this example, the arrangement pattern of the multiple recesses 18B on the inner surface 14 of the mounting portion 12 is a lattice arrangement. Note that the arrangement pattern of the multiple recesses 18B is not limited to the lattice arrangement, and may be, for example, a staggered arrangement. The preferred range of the pitch between the multiple recesses 18B is the same as the preferred range of the pitch P between the protrusions 16. The pitch between the recesses 18B is the distance between the centers of the openings of the recesses 18B. If the opening shape of the recess 18B is not a perfect circle, the center of the circumscribing circle of the opening shape is set as the center of the recess 18B.

[0071] In this embodiment, the RFID tag 20 may be fixed so that all of the recesses 18B provided on the inner surface 14 of the attachment portion 12 are covered with the RFID tag 20, or the RFID tag 20 may be fixed so that only some of the multiple recesses 18B are covered with the RFID tag 20. As shown in Fig. 16, in this example, the RFID tag 20 is fixed so that only some of the recesses 18B are covered with the RFID tag 20. When only some of the multiple recesses 18B are covered with the RFID tag 20, the pitch between the recesses 18B covered with the RFID tag 20 and the pitch between the recesses 18B not covered with the RFID tag 20 may be the same or different.

[0072] The present invention may be a tagged container in which a recess is formed instead of the protrusion 46 on the inner surface 44 of the bottom of the mounting portion 42 of the lid member 41 in the tagged container 3 .

[0073] In the tagged container 1, the attachment portion 12 is provided on the outer surface (bottom surface) of the bottom 11 of the container 10, but as shown in Fig. 17, a tagged container 6 may be provided with a container 10C instead of the container 10. The container 10C is provided with a cylindrical container body 50 with a bottom and an opening 50a at the top, and a rectangular parallelepiped fixing structure portion 52 provided on the bottom side of the container body 50 and having a concave attachment portion 12 on its underside.

[0074] Examples of materials constituting the fixing structure 52 include the same materials as those exemplified as materials constituting the container 10 . The tagged container 6 has excellent self-supporting ability because the bottom surface of the fixing structure 52 is flattened. The tagged container 6 can adopt the same configuration as the tagged container 1, etc., except that the RFID tag 20 is embedded and fixed to the attachment portion 12 of the fixing structure 52 by the fixing material 30.

[0075] Also, as shown in FIG. 18, instead of the fixing structure 52 having the mounting portion 12, a fixing structure 52A having an insertion recess 54 may be provided on the bottom side of the container body 50, and an insertion member 60 having an RFID tag 20 embedded with a fixing material 30 may be inserted into the insertion recess 54 in the mounting portion 12 of a box-shaped frame 62.

[0076] This embodiment is easy to manufacture because the container body 50 and the fixing structure 52A are molded as a single unit, the frame body 62 is molded separately, the RFID tag 20 is embedded in the mounting portion 12 with the fixing material 30 to form the fitting member 60, and these can be combined. Similarly, in the tagged container 1, a fitting recess may be provided in the bottom 11 of the container 10 instead of the attachment portion 12, and the fitting member 60 may be fitted into the fitting recess.

[0077] In addition, within the scope of the invention, the components in the above-described embodiments may be replaced with well-known components, and the above-described modified examples may be combined as appropriate.

[0078] [Packaging] An example of the packaging body of the present invention will now be described. 19, the package 100 is formed by vacuum-packaging the RFID tag 20 and the fixing material 30 made of uncrosslinked condensation reaction type self-adhesive silicone rubber as a single unit in a packaging material 110. In this example, a plurality of sets of the fixing material 30 and the RFID tag 20 integrated together are vacuum-packaged at intervals along the length of the tape-shaped packaging material 110.

[0079] For example, the fixing material 30 and the RFID tag 20, which are vacuum-packaged, can be removed from the packaging body 100, and pushed into an attachment portion provided on the bottom or lid member of the container, and the RFID tag 20 can be embedded to fix the RFID tag 20 to the container.

[0080] The material constituting the packaging material 110 is not particularly limited, and any material having moisture-proof properties can be used, such as biaxially oriented polypropylene film (OPP), biaxially oriented nylon film (ONY), PVDC-coated film in which polyvinylidene fluoride is coated on a base film (polyethylene terephthalate (PET) film, etc.), deposition film in which aluminum or silica is deposited on a base film (PET film, polypropylene (PP) film, etc.), ONY-based co-extruded film, and ethylene-vinyl alcohol copolymer (EVOH) co-extruded OPP film can be exemplified. These films preferably have a sealant layer because they can be sealed by heat. The material constituting the packaging material 110 may be one type or two or more types.

[0081] The package of the present invention is not limited to package 100, but may be one in which a set of a fixing material and an RFID tag are individually vacuum-packed. Also, it is not limited to a tape shape, but may be, for example, one wound in a reel shape. [Explanation of symbols]

[0082] 1 to 6...containers with tags, 10, 10A to 10C...containers, 12, 42...mounting portion, 14, 44...inner surface, 16, 16A to 16C, 46...protruding portion, 17...through hole, 18, 18A, 18B...recess, 20...RFID tag, 30...fixing material, 52, 52A...fixing structure portion, 54...fitting recess, 60...fitting member, 100...packaging body.

Claims

1. The device includes a container, an RFID tag, and a fixing material, The fixing material is made of a condensation reaction type silicone rubber, A recessed mounting portion is formed on an outer surface of the container, A plurality of protrusions are formed on the inner surface of the mounting portion, The RFID tag is embedded in the mounting portion with the fixing material so as to be located on the tip side of the height direction of the multiple protrusions, in contact with the height direction tips of the multiple protrusions.

2. The tagged container according to claim 1 , wherein the plurality of protrusions are formed spaced apart from the side wall of the mounting portion.

3. 3. The tagged container according to claim 1, wherein the condensation reaction type silicone rubber has self-adhesive properties.

4. A tagged container described in any one of claims 1 to 3, wherein the Williams plasticity of the condensation reaction type silicone rubber in an uncrosslinked state at 25°C, measured using a parallel plate plasticity meter in accordance with the measurement method specified in JIS K 6249 "Test methods for uncured and cured silicone rubber", is in the range of 100 to 600.

5. A method for fixing an RFID tag to a container, comprising: A recessed mounting portion is formed on the outer surface of the container, A plurality of protrusions are formed on the inner surface of the mounting portion, The plurality of protrusions are formed at a distance from a side wall of the mounting portion, The RFID tag is pressed into the mounting portion together with a fixing material made of uncrosslinked condensation reaction type silicone rubber, and while allowing excess fixing material present on the convex portion side of the RFID tag to escape between the convex portions, the RFID tag is further pressed into the mounting portion until it comes into contact with the tips of the convex portions in the height direction, A method for fixing a tag, comprising embedding the RFID tag in the mounting portion using the fixing material so that the RFID tag is positioned on the tip side of the heightwise tips of the multiple convex portions while being in contact with the heightwise tips of the multiple convex portions.

6. 6. The tag fixing method according to claim 5, wherein the condensation reaction type silicone rubber has self-adhesive properties.

7. A method for fixing a tag as described in claim 5 or 6, wherein the Williams plasticity of the condensation reaction type silicone rubber in an uncrosslinked state at 25°C, measured using a parallel plate plasticity meter in accordance with the measurement method specified in JIS K 6249 "Test methods for uncured and cured silicone rubber", is in the range of 100 to 600.

8. A tag fixing structure in which an RFID tag is fixed to a container, comprising: A recessed mounting portion is formed on the outer surface of the container, A plurality of protrusions are formed on the inner surface of the mounting portion, The RFID tag is embedded in the mounting portion with a fixing material made of condensation reaction type silicone rubber so as to be in contact with the height-wise tips of the plurality of protrusions and positioned on the tip side of the height-wise tips of the plurality of protrusions.

9. The tag fixing structure according to claim 8 , wherein the plurality of protrusions are formed spaced apart from the side wall of the attachment portion.

10. 10. The tag fixing structure according to claim 8, wherein the condensation reaction type silicone rubber has self-adhesive properties.

11. A fixing structure for a tag described in any one of claims 8 to 10, wherein the Williams plasticity of the condensation reaction type silicone rubber in an uncrosslinked state at 25°C, measured using a parallel plate plasticity meter in accordance with the measurement method specified in JIS K 6249 "Test methods for uncured and cured silicone rubber", is in the range of 100 to 600.

Citation Information

Patent Citations

  • Vessel with RFID tag

    EP2383682A1

  • Adhesive sealing member and double glazing glass formed by using the same

    JP1999100239A

  • Information management method for container, mounting method and mounting device for radio information memory medium

    JP2001356688A

  • Tableware

    JP2003102610A

  • Container with electronic tag

    JP2006168757A