Semiconductor device and its manufacturing method

A semiconductor device with gold-rich bonding layers on chip and lead electrodes, sealed with resin, addresses the issue of lead detachment, enabling miniaturization and thinning without a half-etched region, and enhancing connection strength.

JP7580282B2Active Publication Date: 2024-11-11SEIKO INSTR INC
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021009987
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-26
Publication Date
2024-11-11
Estimated Expiration
2041-01-26

AI Technical Summary

Technical Problem

The half-etched region on the leads of non-lead type semiconductor devices hinders miniaturization and thinning, as it prevents the leads from falling off during resin sealing.

Method used

A semiconductor device with a gold-rich bonding layer on both the semiconductor chip and lead electrodes, connected via a metal joint, is sealed with resin, eliminating the need for a half-etched region, and features external terminals on the lead surfaces.

Benefits of technology

The device achieves miniaturization and thinning by preventing lead detachment from the resin while maintaining strong connections, reducing manufacturing steps and time, and eliminating the need for anchor processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007580282000001
    Figure 0007580282000001
  • Figure 0007580282000002
    Figure 0007580282000002
  • Figure 0007580282000003
    Figure 0007580282000003
Patent Text Reader

Abstract

To provide a compact and thin semiconductor device.SOLUTION: In a semiconductor device with flip chip bonding of a semiconductor chip 1 and a lead 6 via a metal bonding part 5 and encapsulating resin covering these parts, the metal bonding part 5 has a gold-rich bonding layer 5a on a first electrode 3a side of the semiconductor chip 1 and a gold-rich bonding layer 5b on a second electrode 3b side of the lead 6 to make a strong connection between the semiconductor chip 1 and the lead 6, resulting in a compact and thin semiconductor device that does not require an anchor section.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device and a manufacturing method thereof. [Background technology]

[0002] There is a demand for semiconductor devices mounted on portable devices and IC cards to be smaller and thinner. It is well known that the mounting area of ​​semiconductor devices can be reduced by making the lead end surface flush with the package end surface to a non-lead type.

[0003] Patent Document 1 discloses a small and thin non-lead type semiconductor device. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2015-73120 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, in the non-lead type semiconductor device described in Patent Document 1, the peripheral portion on the back side of each lead is cut away by half-etching to form a recessed shape, and the recessed portion is filled with sealing resin, so that the exposed side surface of each lead is surrounded by part of the side surface of the sealing body. The half-etched region of the lead prevents the lead from falling off, but this half-etched region hinders the miniaturization and thinning of the semiconductor device.

[0006] The present invention has been made in view of the above problems, and has an object to provide a smaller and thinner semiconductor device. [Means for solving the problem]

[0007] In order to solve the above problems, the present invention employs the following means. a semiconductor chip having a plurality of first electrodes; a lead having a support surface and a bottom lead surface facing in opposite directions, the lead having a second electrode on the support surface; a metal joint portion connecting the first electrode and the second electrode; a sealing resin that seals the semiconductor chip, the leads, and the metal joints; an external terminal formed on the lead bottom surface and a lead side surface intersecting the lead bottom surface and exposed from the sealing resin, The metal bonding portion is an alloy containing gold, and the semiconductor device is characterized in that it has a first gold-rich bonding layer on the first electrode side having a higher gold content than the alloy, and a second gold-rich bonding layer on the second electrode side having a higher gold content than the alloy. Also,

[0008] A method for manufacturing a semiconductor device in which a semiconductor chip is flip-chip bonded to a lead, comprising the steps of: forming a first bonding underlayer film on a main surface of the semiconductor chip; forming a second bonding underlayer on the support surface of the lead; applying a molten connection material onto the first bonding base film and solidifying the connection material; a step of overlapping the main surface of the semiconductor chip with the main surface facing the support surface of the lead; a step of heating the lead to connect the semiconductor chip and the lead via the metal joint; a step of sealing the semiconductor chip, the leads, and the metal joints with resin; The method for manufacturing a semiconductor device is characterized in that an external terminal is provided on the lead. moreover,

[0009] A method for manufacturing a semiconductor device in which a semiconductor chip is flip-chip bonded to a lead, comprising the steps of: forming a first bonding underlayer film on a main surface of the semiconductor chip; forming thickened and thinned regions in the leads; forming a second bonding underlayer on a support surface of the thinned region of the lead; applying a molten connection material onto the first bonding base film and solidifying the connection material; a step of overlapping the main surface of the semiconductor chip with a second electrode on the support surface of the lead; a step of heating the lead to connect the semiconductor chip and the lead via the metal joint; a step of sealing the semiconductor chip, the leads, and the metal joints with resin; The method for manufacturing a semiconductor device is characterized in that an external terminal is provided on the lead. Effect of the Invention

[0010] By using the above-mentioned means, it is possible to obtain a small and thin semiconductor device while preventing the leads from falling off from the sealing resin. [Brief description of the drawings]

[0011] [Figure 1] 1 is a cross-sectional view of a semiconductor device according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a bottom view of the semiconductor device according to the first embodiment of the present invention. [Diagram 3] 2 is an enlarged cross-sectional view of a bonding portion of the semiconductor device according to the first embodiment of the present invention. FIG. [Figure 4] 1A to 1C are schematic diagrams illustrating a method for manufacturing a semiconductor device according to a first embodiment of the present invention. [Diagram 5] 5 is a schematic diagram illustrating the method for manufacturing the semiconductor device according to the first embodiment of the present invention, continuing from FIG. 4. [Figure 6] 6 is a schematic diagram illustrating the method for manufacturing the semiconductor device according to the first embodiment of the present invention, following FIG. 5. [Figure 7] FIG. 4 is a cross-sectional view of a semiconductor device according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A semiconductor device according to an embodiment of the present invention will now be described with reference to the drawings. (First embodiment)

[0013] FIG. 1 is a cross-sectional view of a semiconductor device according to a first embodiment of the present invention. The semiconductor device 10 is a flip-chip type package with a non-lead structure including a semiconductor chip 1, leads 6, metal joints 5, and sealing resin 7. The flip-chip type package does not require bonding wires or die pads. The leads 6 are made of copper (Cu) or a copper alloy of uniform thickness, and have a support surface 61 on the front surface and a lead bottom surface 62 on the back surface 1b opposite to the front surface. The semiconductor chip 1 is connected to the support surface 61. An electrode (not shown) provided on the main surface 1a of the semiconductor chip 1 and an electrode (not shown) provided on the support surface 61 of the lead 6 are electrically connected via a metal joint 5 containing gold (Au), but the semiconductor chip 1 is inverted and connected so that its main surface 1a faces downward.

[0014] The semiconductor chip 1, the leads 6, and the metal joints 5 are covered with a sealing resin 7, but the lead bottom surface 62 and the lead side surface 63 are exposed from the sealing resin 7. The semiconductor device 10 is rectangular in cross section, the lead bottom surface 62 is flush with the resin bottom surface 72 of the sealing resin 7, and the lead side surface 63 is flush with the resin side surface 73 of the sealing resin 7. The lead bottom surface 62 and the lead side surface 63 are covered with external terminals 11 for mounting on a substrate. The external terminals 11 are laminated films in which a nickel (Ni) film and a gold (Au) film are deposited in this order from the lead bottom surface 62 side and the lead side surface 63 side. Alternatively, they are laminated films in which a nickel (Ni) film, a palladium (Pd) film, and a gold (Au) film are deposited in this order.

[0015] FIG. 2 is a bottom view of the semiconductor device according to the first embodiment of the present invention. In FIG. 2, the sealing resin 7 is shown in perspective for ease of understanding. The semiconductor device 10 is a package with a non-lead structure having four leads 6, one end of each of the leads 6 is arranged apart from each other, and the end face of the other end of the lead 6 is flush with the outer periphery of the sealing resin 7. A semiconductor chip 1 (shown by a broken line) is arranged in the center of the rectangular sealing resin 7, and the four corners of the semiconductor chip 1 overlap with each of the leads 6. Electrodes are arranged at the four corners of the semiconductor chip 1, and metal joints 5 (shown by a broken line) are provided on the electrodes, and the semiconductor chip 1 and the leads 6 are connected via the metal joints 5. The planar areas of the metal joints 5 arranged at the four corners of the semiconductor chip 1 are shaped to be included in the planar areas of the leads 6.

[0016] FIG. 3 is an enlarged cross-sectional view of the joint between the semiconductor chip and the lead. The metal joint 5 is an alloy containing gold (Au), for example, made of a gold-tin (AuSn) alloy, and is connected to the electrode 3a on the semiconductor chip 1 side through the gold-rich joint layer 5a on the semiconductor chip 1 side. Also, on the lead 6 side, it is connected to the electrode 3b on the lead 6 side through the gold-rich joint layer 5b. The electrodes 3a and 3b are made of nickel (Ni) films 4a and 4b, which are barrier films. The Au / Sn component ratio of the gold-rich joint layers 5a and 5b is higher than the Au / Sn component ratio of the metal joint 5, that is, the gold (Au) content is high. Also, the components in the gold-rich joint layers 5a and 5b are not uniform, and the ratio is higher the closer to the nickel film 4a in distance. Compared to the plane area of ​​the metal joint 5 and the gold-rich joint layer 5a on the semiconductor chip 1 side, the plane area of ​​the metal joint 5 and the gold-rich joint layer 5b on the lead 6 side is larger. In this figure, the nickel film 4b is provided on a limited part of the support surface 61 of the lead 6, but the nickel film 4b as a barrier film may be applied to the entire support surface. The gold-rich bonding layers 5a, 5b located between the metal bonding portion 5 and the nickel film 4a are formed by diffusing the components of the metal bonding portion 5, and the bonding region formed is strong. In addition, the distance between the semiconductor chip 1 and the leads 6 in the thickness direction is extremely small, 3 to 5 μm. As described above, the semiconductor chip 1 and the leads 6 are firmly connected, so they do not easily peel off. Therefore, although the periphery of the semiconductor chip 1 is completely covered with the sealing resin 7, there is no concern that the pull-out strength of the leads 6 is reduced and the leads 6 fall off from the sealing resin 7, and anchor processing such as forming a thin-walled portion to prevent the leads from falling off from the sealing resin 7 is not required. Therefore, the leads 6 do not need to have the thickness or width required for anchor processing, and the plate thickness of the leads 6 can be made thin and the area can be made small. This makes it possible to realize a thin (low-profile) and small-sized semiconductor device. In addition, an additional process of anchor processing is not required, and the number of steps in manufacturing can be reduced.

[0017] A method for manufacturing a semiconductor device according to a first embodiment of the present invention will be described with reference to FIGS. First, the semiconductor chip 1 shown in FIG. 4 is prepared. The figure shows a top view of the semiconductor chip 1 before being connected to the leads 6 and an enlarged cross-sectional view of the pad portion. As shown in FIG. 4(a), in this example, four bonding underlayer films 4 are provided so as to cover the pads 2 at each of the four corners of the main surface 1a of the rectangular semiconductor chip 1. FIG. 4(b) shows the cross-sectional structure of the pad portion, in which an aluminum (Al) film is formed as the pad 2 on the main surface 1a of the semiconductor chip 1. The aluminum film as the pad 2 is the same layer as the top wiring of the semiconductor chip 1. A nickel (Ni) film 4a and a gold (Au) film 44a are laminated in this order on the pad 2 as the bonding underlayer film 4. The nickel film 4a serves as a barrier film, and the gold film 44a serves to improve wettability. The aluminum film is prone to oxidation and corrosion in air, but the nickel film 4a and the gold film 44a are formed on the surface to make it less susceptible to oxidation and corrosion. The nickel film 4a and the gold film 44a are preferably formed by a wet plating method (nickel plating, gold flash plating). In the case of a three-layer laminated film including a palladium (Pd) film, the formation of the bonding undercoat film 4 on the pad 2 is completed by carrying out nickel plating, palladium plating, and gold flash plating in this order.

[0018] Next, the connecting material 9, which is an alloy of two or more metals including gold (Au), is dispensed (drop-applied) in a molten state onto the pad 2 of the semiconductor chip 1. FIG. 5 is a diagram showing the state before and after the connecting material 9 is dispensed onto the pad 2. FIG. 5(a) shows the semiconductor chip 1 and the heating pod 12. The heating pod 12 has a heating means, a degassing means, and a dispensing means, and the connecting material 9 in a molten state is stored in the heating pod 12. The connecting material 9 is a gold-tin alloy, and has a component ratio of, for example, Au / Sn=80 / 20 or Au / Sn=78 / 22. The heating pod 12 is controlled to 300 to 320° C. by the heating means, and minute bubbles in the connecting material 9 in a molten state are removed by the degassing means. In addition, organic matter and the like are sufficiently desolvated. A dispensing means is provided at the lower end of the heating pod 12, and the surroundings are purged with nitrogen, and the surrounding temperature is room temperature. The semiconductor chip 1 is also not heated and is kept at room temperature.

[0019] 5(b), when the molten connecting material 9 is dispensed onto the bonding underlayer 4 on the pad 2 of the semiconductor chip 1, the molten connecting material 9 has a certain surface tension, and therefore assumes a shape with a certain curvature on the bonding underlayer 4. In addition, the size of the connecting material 9 dispensed at this time is smaller than the size of the pad 2 of the semiconductor chip 1.

[0020] When dispensing the connection material 9 on the semiconductor chip 1, it is preferable that the semiconductor chip 1 is an individual chip that has been diced from a semiconductor wafer. It is more efficient to dispense the connection material 9 on the semiconductor chip 1 before dicing, but if the semiconductor chip 1 is diced after dispensing, it will be exposed to cutting waste and moisture generated at that time. In order to avoid this, it is preferable to dispense the connection material 9 after dicing.

[0021] FIG. 5(c) shows a state where the connecting material 9 is dispensed on the bonding underlayer 4 on the pad 2 of the semiconductor chip 1 and then solidified on the pad 2. The molten connecting material 9 dispensed at 310-320°C melts with the bonding underlayer 4 on the pad 2, and is cooled to room temperature to form the following structure. That is, a nickel film 4a is laminated on the pad 2, and a gold-rich bonding layer 5a is formed on the nickel film 4a. The gold-rich bonding layer 5a is formed by diffusing the metal bonding portion 5 into the gold film 44a, and the Au / Sn component ratio of the gold-rich bonding layer 5a is higher than the Au / Sn component ratio of the metal bonding portion 5, that is, the gold (Au) content is high. Also, the components in the gold-rich bonding layer 5a are not uniform, and the closer to the nickel film 4a, the higher the ratio.

[0022] By dispensing the molten gold and tin as the connection material 9 on the bonding underlayer 4 on each pad 2 for all pads 2 on the semiconductor chip 1 as described above, the connection between the metal bonding portion 5 and the semiconductor chip 1 is completed. The connection between the semiconductor chip 1 and the metal bonding portion 5 obtained by this method can be performed with fewer steps than the conventional connection method. For example, in the conventional method of forming bumps, many steps such as a pattern formation step using a resist for bump formation, a plating step, a resist removal step, and a reflow step are required, but in this manufacturing method, the connection is completed with an extremely small number of steps, such as only dispensing the previously melted connection material 9 on the bonding underlayer 4 on the pad 2. In addition, since the connection temperature is higher than that in the conventional semiconductor device shown in Patent Document 1, the connection between the semiconductor chip 1 and the metal bonding portion 5 obtained by this manufacturing method is a strong connection with few voids.

[0023] Next, as shown in FIG. 6, the semiconductor chip 1 provided with the metal bonding portion 5 is connected to the lead 6. FIG. 6(a) illustrates the state before connection, in which the semiconductor chip 1 is waiting above the lead 6. The back surface 1b side of the semiconductor chip 1 is picked up using a collet 13, and the main surface 1a of the semiconductor chip 1 on which the metal bonding portion 5 is formed is inverted downward and faces the support surface 61 of the lead 6. At a predetermined location of the support surface 61 of the opposing lead 6, a nickel (Ni) film 4b and a gold (Au) film 44b are laminated in order as the bonding base film 4. Alternatively, a nickel (Ni) film, a palladium (Pd) film, and a gold (Au) film are laminated in order. The bonding base film 4 is formed by a wet plating method. The bonding base film 4 on the lead 6 side is formed to have a larger planar area than the bonding base film 4 formed on the semiconductor chip 1 side.

[0024] Organic solvent 14 is applied in dots to the surface of bonding base film 4 of opposing lead 6. The area where organic solvent 14 is applied corresponds to the position where semiconductor chip 1 is to be connected, and serves the purpose of self-alignment and temporary fixation when semiconductor chip 1 is connected to lead 6. At this time, both semiconductor chip 1 and lead 6 are placed in a room temperature atmosphere.

[0025] Next, the collet 13 is lowered together with the semiconductor chip 1, and the metal joints 5 of the semiconductor chip 1 are placed on the areas where the organic solvent 14 has been applied in dots. Even if the semiconductor chip 1 and the leads 6 are slightly misaligned, the self-aligning effect of the organic solvent 14 is utilized to move the semiconductor chip 1 slightly and correct the position to the correct position. The organic solvent 14 for temporary fixing is preferably one that is liquid at room temperature and evaporates when heated, and is preferably an alcohol such as isopropyl alcohol (IPA) or a ketone such as methyl ethyl ketone (MEK). The above description is given using an example in which the organic solvent 14 is used, but the step of temporary fixing with the organic solvent 14 is not necessarily required. However, by using this step, it is possible to achieve highly accurate overlapping and to obtain a smaller semiconductor device 10.

[0026] Thereafter, the lead 6 carrying the semiconductor chip 1 is moved to a heating stage in a nitrogen atmosphere and heated from the back side of the lead 6. The heating temperature in this step is preferably lower than the temperature at which the semiconductor chip 1 is connected to the metal bonding portion 5, and is preferably 295 to 305°C.

[0027] As shown in Fig. 6(b), the organic solvent 14 evaporates upon heating, and the metal bonding portion 5 melts and connects to the bonding base film 4. The metal bonding portion 5 melts into the gold film 44b constituting the bonding base film 4 to form a gold-rich bonding layer 5b, which firmly connects the semiconductor chip 1 and the lead 6 (see Fig. 3). Note that, although the surface of the metal bonding portion 5 before connection is covered with an extremely thin oxide film, according to this method, since connection is made at a higher temperature than in the conventional bump method, very good wetting and spreading can be obtained without the need for flux or the like for the purpose of removing the oxide film and activating it.

[0028] Next, the semiconductor chip 1, the leads 6, and the metal joints 5 are covered with a sealing resin 7, and then the leads 6 are formed as necessary. External terminals 11 are formed on the surfaces of the lead bottom surface 62 and the lead side surface 63. If the external terminals 11 are a laminated film of a nickel (Ni) film and a gold (Au) film, the external terminals 11 can be formed by sequentially carrying out nickel plating and gold flash plating. If the external terminals 11 are a three-layer laminated film including a palladium (Pd) film, the external terminals 11 can be formed by sequentially carrying out nickel plating, palladium plating, and gold flash plating. Through the above steps, a semiconductor device 10 as shown in FIG. 1 is completed.

[0029] In the conventional semiconductor device shown in Patent Document 1, the temperature when the gold bumps are bonded to the leads is about 250°C, and the bonding layer formed between the gold bumps and the leads is thin and island-shaped. When mounting such a conventional semiconductor device on a printed circuit board, reflow is performed, and the heat treatment temperature at that time is 255 to 265°C, which is higher than the connection temperature between the gold bumps and the leads. Therefore, there is a possibility that the leads may fall off from the gold bumps due to the mounting on the printed circuit board, and to prevent this, a half-etched region (anchor portion) is provided on the periphery of the back side of the leads. In contrast, the heat treatment temperature (295°C or higher) of the metal bonding portion 5 of the semiconductor device 10 obtained through the above steps is higher than the printed circuit board mounting temperature of 255 to 265°C, and there is no concern that the metal bonding portion 5 melts due to the mounting on the printed circuit board, weakening the connection between the semiconductor chip 1 and the leads 6, and the leads 6 fall off from the sealing resin 7. In other words, it is possible to prevent the leads from falling off without providing a half-etched region that was required in the conventional semiconductor device. By eliminating the need for a half-etched region on the periphery of the leads, the leads become smaller, which contributes to the miniaturization of the semiconductor device. Furthermore, the half-etched region needs to have a certain thickness to ensure strength, but since this is not necessary, it is possible to reduce the thickness of the lead. Reducing the thickness of the lead contributes to making the semiconductor device thinner. As described above, the semiconductor device of the present invention, which does not require a half-etched region, can be made even smaller and thinner.

[0030] Although the above description has been given of an example in which a gold-tin alloy is used for the metal joint 5 and the connection material 9, the same effect can be obtained when a gold-germanium alloy is used instead of the gold-tin alloy.

[0031] Second embodiment FIG. 7 is a cross-sectional view of a semiconductor device according to a second embodiment of the present invention. In the semiconductor device according to the first embodiment shown in FIG. 1, the thickness of the lead 6 is uniform. However, in the semiconductor device 20 according to this embodiment, the lead thickness t1 on the lead side surface 63 and the lead thickness t2 on the support surface 61 where the semiconductor chip is bonded to the lead 6 are different, and the lead thickness t2 on the support surface 61 is thinner than the lead thickness t1 on the lead side surface 63. That is, the lead 6 has a structure in which the lead side surface 63 side, that is, the peripheral side of the lead 6, is a thick region 66, and the part bonded to the semiconductor chip 1 is a thin region 67. The back surfaces of the thick region 66 and the thin region 67 form the same plane together with the resin bottom surface 72, and a step portion 65 is arranged between the thick region 66 and the upper surface of the thin region 67, and the step portion 65 is a forward tapered inclined surface. The semiconductor chip 1 is arranged inside the step portion 65, that is, on the thin region 67 of the lead 6. Moreover, the value of the height h1 of the main surface 1a of the semiconductor chip 1 from the resin bottom surface 72 at this time is smaller than the value of the lead thickness t1 and larger than the value of the lead thickness t2. Note that the thin region 67 in this example can be formed as the support surface 61 by partially pressing or half-etching the lead, which has a uniform thickness like the semiconductor device of the first embodiment, from above. Here, the part where the lead is relatively thick, such as the part not subjected to pressing or the like, corresponds to the thick region 66.

[0032] As described above, by forming the lead 6 into a shape having the thick region 66 and the thin region 67, and mounting the semiconductor chip 1 on the thin region 67 via the metal joint 5, the semiconductor device 10 can be made thinner (lower in height) without impairing the mountability of the semiconductor device 10 on the printed circuit board. Usually, the connection region when mounting on the printed circuit board corresponds to the external terminal 11 of the semiconductor device 10, but when the semiconductor device 10 is made thinner, the thickness of the lead becomes thinner accordingly, and the area of ​​the external terminal 11 attached to the lead side surface 63 becomes smaller. Correspondingly, the connection strength of the semiconductor device 10 to the printed circuit board becomes smaller. In contrast, in the semiconductor device 20 of this embodiment, the thick region 66 is provided on the lead 6, and the lead side surface 63 is formed there, so that the area of ​​the external terminal 11 attached to the lead side surface 63 does not become smaller, and the connection strength to the printed circuit board does not become smaller. Furthermore, since the semiconductor chip 1 is mounted on the thin region 67 of the lead 6, the semiconductor device 10 can be made thinner. Furthermore, since the semiconductor chip 1 and the leads 6 are firmly connected, the leads 6 can be prevented from falling off the sealing resin 7.

[0033] 6 is used for temporary fixing when bonding the semiconductor chip 1 to the lead 6, but even if the metal bonding portion 5 of the semiconductor chip 1 is placed outside the application range of the organic solvent 14, the semiconductor chip 1 is guided by the step portion 65 provided on the lead 6 and the position is corrected to the thin region 67, and further the position is finely adjusted by self-alignment by the organic solvent 14. In this way, the effect of guiding the semiconductor chip 1 to the appropriate position on the lead 6 also contributes to further miniaturization of the semiconductor device.

[0034] Figure 7 illustrates a case in which the height h2 of the back surface 1b, which is the opposite side to the main surface 1a of the semiconductor chip 1, from the resin bottom surface 72 is greater than the value of the lead thickness t1, i.e., greater than the height of the upper surface of the thick region 66 of the lead 6 from the resin bottom surface 72. However, it is clear that the semiconductor device 10 can be made even thinner by further reducing the thickness of the semiconductor chip 1, for example by making the height h2 of the back surface 1b of the semiconductor chip 1 from the resin bottom surface 72 smaller than the height of the upper surface of the thick region 66 of the lead 6 from the resin bottom surface 72. [Industrial Applicability]

[0035] The semiconductor device according to the present invention can be used in a wide range of applications, from portable toys, health care products, wearable terminals, mobile terminals, card terminals, and home appliances to in-vehicle and outdoor applications in harsh operating environments. [Explanation of symbols]

[0036] 1. Semiconductor chip 1a Main surface 1b back side 2 Pad 3a, 3b electrode 4 Bonding base film 4a, 4b Nickel film (barrier film) 44a, 44b gold film 5 Metal joints 5a, 5b Gold-rich bonding layer 6 Lead 61 Support surface 62 Lead bottom 63 Lead Side 65 Step 66 Thick wall area 67 Thin area 7 Sealing resin 72 Resin bottom 73 Resin side 9 Connectors 10, 20 Semiconductor device 11 External terminal 12 Heating Pods 13 Colette 14 Organic Solvents t1, t2 lead thickness h1, h2 Height from the bottom of the resin

Claims

1. a semiconductor chip having a plurality of first electrodes; a lead having a support surface, a lead bottom surface, and a lead side surface, the lead having a second electrode on the support surface; a metal joint portion connecting the first electrode and the second electrode; a sealing resin that seals the semiconductor chip, the leads, and the metal joints; external terminals formed on the bottom surface and the side surface of the lead and exposed from the sealing resin; A semiconductor device comprising: The metal bonding portion is an alloy containing gold, and has a first gold-rich bonding layer on the first electrode side having a higher gold content than the alloy, and a second gold-rich bonding layer on the second electrode side having a higher gold content than the alloy, The semiconductor device is characterized in that the lead comprises a thick region provided on the lead side on which the external terminal is formed, and a thin region extending inward from the thick region, and the semiconductor chip is mounted on the thin region.

2. 2. The semiconductor device according to claim 1, wherein a bonding area of ​​the metal bonding portion on the second electrode side is larger than a bonding area of ​​the metal bonding portion on the first electrode side.

3. A method for manufacturing a semiconductor device in which a semiconductor chip is flip-chip bonded to a lead, comprising the steps of: forming a first bonding underlayer film on a main surface of the semiconductor chip; forming thickened and thinned regions in the leads; forming a second bonding undercoat on a support surface of the thinned region of the lead; applying a molten connection material onto the first bonding base film and solidifying the connection material to form a metal bond; a step of overlapping the main surface of the semiconductor chip with the second electrode of the support surface of the lead; a step of heating the lead to connect the semiconductor chip and the lead via the metal joint; a step of sealing the semiconductor chip, the leads, and the metal joints with resin; A method of manufacturing a semiconductor device, comprising the steps of: providing an external terminal on said lead;

4. Before the step of overlapping the main surface of the semiconductor chip with the supporting surface of the lead facing each other, 4. The method for manufacturing a semiconductor device according to claim 3, further comprising the step of applying an organic solvent onto the second bonding underlayer film on the supporting surface.

Citation Information

Patent Citations

  • Method of packaging electronic parts and its packaging equipment

    JP2004319993A

  • Resin-sealed semiconductor device, etching member used for the same, method for manufacturing resin-sealed semiconductor device, and stacked type resin-sealed semiconductor device

    JP2009135406A

  • Forming method of solder bump and paste for forming base

    JP2013004929A

  • Semiconductor device manufacturing method

    JP2015073120A

  • Thermoelectric conversion module, and method for manufacturing the same

    JP2016174117A