Glass Composite
The glass composite addresses communication and lighting issues by employing a structured light reflecting layer with specific metal thickness and area ratios, enhancing electromagnetic wave transmission and lighting control.
Patent Information
- Application Number
- JP2024048430
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-03-25
- Publication Date
- 2024-11-11
- Estimated Expiration
- 2044-03-25
AI Technical Summary
Existing glass composites with metal shielding layers for electromagnetic interference and reflection issues hinder communication and lighting performance, particularly at night.
A glass composite structure with a light reflecting layer having thick and thin metal portions, allowing for electromagnetic wave transmission and controlled lighting, achieved by using a metal vapor-deposited layer with specific thickness and area ratios, and bonded with intermediate resins.
Improves electromagnetic wave permeability and lighting performance while reducing night reflections, ensuring effective communication and adequate lighting through controlled light transmission.
Smart Images

Figure 0007580646000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a glass composite having at least a pair of glass layers as a laminated glass and exhibiting a radiative cooling function. [Background technology]
[0002] Radiative cooling is known as a function for cooling objects. Radiative cooling is a phenomenon in which a substance's temperature drops when it radiates electromagnetic waves such as infrared rays to its surroundings. By utilizing this phenomenon, for example, it is possible to realize a composite cooling device that cools objects without consuming energy such as electricity.
[0003] Patent Document 1 discloses a glass composite in which a high-emissivity coating layer that emits infrared light from its radiation surface and a low-emissivity coating layer that reflects light are laminated on a glass substrate. Here, it is disclosed that the low-emissivity coating layer includes a shielding layer that blocks infrared and ultraviolet rays, and that the shielding layer is made of a metal material such as silver. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Special Publication No. 2022-543529 Summary of the Invention [Problem to be solved by the invention]
[0005] When the glass composite shown in Patent Document 1 has a shielding layer made of a metal material such as silver, for example in a structure such as a vehicle having a window that separates an external area from an internal area with the glass composite, there are problems such as the blocking of electromagnetic waves used for communication between the external area and the internal area, poor lighting from the external area to the internal area, and increased reflections when viewing the external area from the internal area through the glass composite at night. However, the technology disclosed in Patent Document 1 does not recognize such a problem, and there is room for improvement.
[0006] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to provide a glass composite that can improve electromagnetic wave transmittance and daylighting properties and can reduce glare at night, etc. [Means for solving the problem]
[0007] The characteristic configuration of the glass composite for achieving the above object is as follows: an infrared radiation glass layer that emits infrared light from a first radiation surface that is a radiation surface, and a back surface glass layer that is provided opposite to a surface of the infrared radiation glass layer opposite to a side on which the first radiation surface is present, a light reflecting layer that reflects light is provided between the infrared radiation glass layer and the back surface glass layer; the light reflecting layer has a thick portion in a stacking direction and a thin portion whose thickness in the stacking direction is 2 / 3 or less of the thickness of the thick portion, The thin portion is provided continuously and integrally in a plan view perpendicular to the first radiation surface, and has an area of 5 cm 2 a first metal thin portion having an area equal to or greater than the area of the first metal thin portion, and a second metal thin portion provided integrally and continuously in the plan view and having an area in the plan view less than the area of the first metal thin portion, The second thin metal portion is provided in a plurality of portions in a dispersed manner in the plan view, The overall surface average solar reflectance is 40% or more, and the surface average emissivity, which is the wavelength average of the emissivity of infrared light of 8 μm or more and 13 μm or less, is 80% or more.
[0008] According to the above characteristic configuration, the light reflecting layer has a thick portion in the stacking direction and a thin portion whose thickness in the stacking direction is 2 / 3 or less of the thickness of the thick portion, and the thin portion is provided continuously and integrally in a plan view perpendicular to the first radiation surface and has an area of 5 cm in plan view. 2Since the glass composite has a first thin metal portion having an area of the above size, by setting the thickness of the first thin metal portion to an appropriate thickness that allows electromagnetic waves for communication to pass through, for example, it becomes possible to communicate by electromagnetic waves through the glass composite. Furthermore, as the thin portions of the light-reflecting layer, a plurality of second thin metal portions which are provided as a continuous, integral part in a planar view and whose area in a planar view is less than the area of the first thin metal portion are provided in a dispersed and distributed form in a planar view, so that a predetermined amount of light can be obtained through the glass composite in a dispersed manner in the planar direction along the radiating surface. Furthermore, the second thin metal portions, which are provided in a dispersed manner in a plan view, have a smaller area in a plan view than the first thin metal portions, so that a certain degree of reflectance can be ensured as a light reflective layer. With the above-described configuration, a glass composite having laminated glass that has an overall surface average solar reflectance of 40% or more and a surface average average emissivity, which is the wavelength average of the emissivity of infrared light of 8 μm or more and 13 μm or less, of 80% or more can be realized, thereby improving electromagnetic wave transmittance and daylighting properties and reducing reflections at night, etc.
[0009] Further characteristic features of the glass composite include: the light reflecting layer is a metal deposition layer formed by depositing a metal on a resin material, The metal is at least one of silver, a silver alloy, aluminum, an aluminum alloy, and a copper alloy; The intermediate resin that bonds the infrared radiation glass layer and the metal vapor deposition layer, and the back glass layer and the metal vapor deposition layer, is made of one or more of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane.
[0010] As in the above characteristic configuration, a metal vapor deposition layer formed by vapor-depositing a metal onto a resin material is used as the light-reflecting layer, and the metal is at least one of silver, a silver alloy, aluminum, an aluminum alloy, and a copper alloy. The infrared-emitting glass layer and the metal vapor deposition layer, and the rear glass layer and the metal vapor deposition layer are bonded together with an intermediate resin made of any one of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane, so that the infrared-emitting glass layer and the rear glass layer can be bonded well with the light-reflecting layer interposed therebetween. Incidentally, in this configuration, by using a resin consisting of any one of polyvinyl butyral, polyethylene vinyl acetate, polyurethane, and polyethylene terephthalate as the resin material onto which metal is vapor-deposited as the light-reflecting layer, adhesion by the above-mentioned intermediate resin can be achieved satisfactorily.
[0011] Further characteristic features of the glass composite include: the light reflecting layer is a ceramic layer formed on a surface of the infrared radiation glass layer, The intermediate resin that bonds the light reflecting layer and the rear glass layer is made of any one of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane.
[0012] As described above, the light-reflecting layer is a ceramic layer formed on the surface of the infrared-emitting glass layer, and the light-reflecting layer and the rear glass layer are bonded together with an intermediate resin made of any one of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane. This makes it possible to achieve good adhesion between the infrared-emitting glass layer and the rear glass layer with the light-reflecting layer made of ceramics interposed between them.
[0013] Further characteristic features of the glass composite include: In the stacking direction, the thickness of each of the first thin metal portion and the second thin metal portion is not less than 0 nm and not more than 50 nm. Furthermore, it is preferable that the thickness of each of the first thin metal portion and the second thin metal portion in the stacking direction is not less than 0 nm and not more than 10 nm.
[0014] As in the above characteristic configuration, the thickness of each of the first thin metal portion and the second thin metal portion in the stacking direction is preferably 0 nm or more and 50 nm or less, and more preferably 0 nm or more and 10 nm or less. The inventors set the thickness of the first metal thin portion in the product direction to 50 nm or less, and, as described above, set the area in plan view to 5 cm 2 It has been confirmed that by doing the above, electromagnetic waves for communication can be transmitted satisfactorily for communication. In addition, it has been confirmed that by having a certain area ratio of thick portions while keeping the thickness in the product direction of the second metal thin portion to 50 nm or less, it is possible to obtain appropriate light transmission while ensuring an average surface solar reflectance of 40% or more for the entire glass laminate.
[0015] Further characteristic features of the glass composite include: In the plan view, the area of the second metal thin portion is 0.03 cm 2 That is all there is to it.
[0016] The inventors determined that the area of the second metal thin section was 0.03 cm 2 It has been confirmed that if the thickness is less than this, it is difficult to obtain sufficient lighting for the entire glass laminate, even if the number of second thin metal portions is increased to the extent that the light reflective layer can be maintained as a thin metal film.
[0017] Furthermore, the infrared radiation glass layer and the rear surface glass layer are It is preferable that the glass is made of at least one of alkali-free glass, soda lime glass, alkali borosilicate glass, and acrylic resin glass.
[0018] By selecting the material in this way, the infrared radiation glass layer or the rear surface glass layer can function well as an infrared radiation layer that radiates infrared rays. In addition, when connecting with the above-mentioned intermediate resin, the hydroxyl groups of the infrared radiation glass layer or the rear surface glass layer and the hydroxyl groups of the intermediate resin can be bonded to each other to provide good adhesion.
[0019] Further characteristic features of the glass composite include: In the plan view, the ratio of the area of the thin portion to the entire area of the light reflecting layer is 1% or more and 50% or less.
[0020] According to the above-mentioned characteristic configuration, a glass composite having an overall surface average solar reflectance of 40% or more can be successfully realized.
[0021] Further characteristic features of the glass composite include: The infrared radiation glass layer has a light control layer having a light control function on the side opposite to the side where the first radiation surface is present.
[0022] As explained above, the glass composite of the present invention has an overall surface average solar reflectance of 40% or more by providing thin sections in the light-reflecting layer, so it is anticipated that in some cases, too much light may pass through the gas composite. As described above, by providing a light control layer having a light control function on the side of the infrared radiation glass layer opposite to the side on which the light reflecting layer is present, it is possible to adjust the light transmission by increasing the amount of light attenuation by the light control layer, for example, when the amount of light passing through the glass composite is too large. [Brief description of the drawings]
[0023] [Figure 1] FIG. 1 is a schematic cross-sectional view of a glass composite, and a vehicle as a structure including the glass composite. [Diagram 2] FIG. 13 is a diagram for explaining the sequential sputtering of materials for a light reflecting layer onto an infrared radiation glass. [Diagram 3] FIG. 2 is a plan view of an example of a glass composite (or a light reflecting layer). [Figure 4] FIG. 13 is a schematic cross-sectional view of another embodiment of a glass composite. [Diagram 5] FIG. 2 is a schematic cross-sectional view of a glass composite according to a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] The glass composite W according to the embodiment of the present invention can improve electromagnetic wave transparency and daylighting properties, and can also reduce glare at night or other times. Hereinafter, an embodiment of the glass composite W will be described with reference to the drawings.
[0025] As shown in Fig. 1, the glass composite W is preferably provided, for example, as window glass to be fitted into a frame C1 of a vehicle C as a structure that divides an internal area IS from an external environment OS. The window is a front window, rear window, side window, sunroof, etc. of the vehicle C. Other examples of the structure include commercial buildings and residential buildings, and the glass composite W can be suitably used as window glass for these. In this embodiment, the side of the atmosphere from which infrared rays are radiated is the side indicated by the arrow in the stacking direction Z.
[0026] The glass composite W has an infrared emitting glass layer G1 that emits infrared light from a first emitting surface H1 that is an emitting surface H, and a back surface glass layer G2 that is provided facing the surface of the infrared emitting glass layer G1 opposite to the side where the first emitting surface H1 exists, and has a light reflecting layer B that reflects light between the infrared emitting glass layer G1 and the back surface glass layer G2. Here, the back surface glass layer G2 can be an infrared emitting back surface glass layer that emits infrared light from a second emitting surface H2 that is the emitting surface H on the side opposite to the side where the light reflecting layer B exists. 1, the light reflecting layer B has a thick portion B3 in the stacking direction Z and a thin portion B2 whose thickness in the stacking direction Z is ⅔ or less of the thickness of the thick portion B3. In the thin portion B2, the proportion of transmitted light Lt in the incident light L from the first radiation surface H1 side is relatively high and the proportion of reflected light Lr is relatively low, compared to the thick portion B3.
[0027] Regarding the thin portion of the light reflecting layer B, as shown in the plan view of the light reflecting layer B (or the glass composite W) in FIG. 3, the thin portion is provided continuously and integrally in a plan view perpendicular to the first radiation surface H1 and has an area of 5 cm2 in plan view. 2 and a second thin metal portion B2 which is provided integrally and continuously in a plan view and has an area in a plan view less than the area of the first thin metal portion B1. Here, the second thin metal portion B2 is provided in a plurality of locations so as to be dispersed in a plan view, and the area of one second thin metal portion B2 is 0.03 cm 2 That's all.
[0028] The light-reflecting layer B is preferably a metal-vapor-deposited layer deposited on the side of the infrared-emitting glass layer G1 opposite to the side on which the first emitting surface H1 is present. The deposited metal is preferably at least one of silver, a silver alloy, aluminum, an aluminum alloy, and a copper alloy.
[0029] Furthermore, in the light reflecting layer B, the thickness of each of the first thin metal portion B1 and the second thin metal portion B2 in the stacking direction Z is preferably 0 nm or more and 50 nm or less, more preferably 0 nm or more and 10 nm or less. Incidentally, the thickness of the thick portion B3 is preferably 50 nm or more and 500 nm or less, more preferably 70 nm or more and 200 nm or less. With the above configuration, the first thin metal portion B1 can transmit electromagnetic waves for communication (for example, electromagnetic waves with frequencies of about 300 MHz or more and 300 GHz or less) well, and the second thin metal portion B2 can transmit visible light for daylighting well. In addition, it is possible to reduce glare at night, etc.
[0030] In plan view, the ratio of the area of the thin portion to the entire area of the light reflecting layer B is preferably 1% or more and 50% or less. From the viewpoint of light collection, the ratio of the area of the second metal thin portion B2 to the entire area of the light reflecting layer B is preferably 1% or more. In the plan view of FIG. 3, the first thin metal portion B1 is rectangular and the second thin metal portion B2 is circular, but they are not limited to this and may be various shapes such as elliptical or polygonal.
[0031] As shown in FIG. 2, the light reflecting layer B is formed by sputtering (deposition by physical vapor deposition (PVD)) a metal material as the light reflecting layer B onto a predetermined resin film Bj (an example of a resin material) via a punching metal PM.
[0032] The method for forming the light reflecting layer B is not particularly limited, and may be a chemical vapor deposition (CVD) method, a plasma enhanced chemical vapor deposition (PECVD) method, magnetron sputtering, an ion beam assisted deposition method, or the like. The deposition method of the infrared emitting layer J may be the same as or different from that of the light reflecting layer B, and may be spray coating, dip coating, or a plasma enhanced chemical vapor deposition (PECVD) method.
[0033] As the punched metal PM, as shown in Fig. 2, a first flat plate portion PM1 shaped to overlap the first metal thin portion B1 (shown in Fig. 3) in a plan view and a second flat plate portion PM2 shaped to overlap the second metal thin portion B2 (shown in Fig. 3) are preferably connected integrally to a metal frame body PM4. Note that, although a plurality of second flat plate portions PM2 are present dispersedly in a plan view, the plurality of second flat plate portions PM2 are connected to the metal frame body PM4 by, for example, connection lines PM3 that are sufficiently thin in a plan view.
[0034] Although details will be described later, the glass composite W shown in Fig. 1 is manufactured by applying a predetermined pressure bonding technique to melt the intermediate resin Tu and the resin film Bj, with the intermediate resin Tu being interposed between the resin film Bj on which the above-mentioned metal material is sputtered and the infrared radiation glass layer G1, and between the resin film Bj on which the above-mentioned metal material is sputtered and the back glass layer G2. Note that the resin film Bj is not shown in Fig. 1.
[0035] Here, the intermediate resin Tu can be preferably made of any one of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane. The resin film Bj can be made of the same resin as the intermediate resin Tu, and can also be made of polyethylene terephthalate. With this configuration, the infrared radiation glass layer G1 and the rear surface glass layer G2 (infrared radiation rear surface glass layer) can maintain the glass fragments when they are broken due to an impact.
[0036] The infrared radiation glass layer G1 and the back surface glass layer G2 (infrared radiation back surface glass layer) are preferably glass for vehicles, and more preferably made of at least one of alkali-free glass, soda-lime glass, alkali borosilicate glass, and acrylic resin glass. The infrared radiation glass layer G1 and the back surface glass layer G2 (infrared radiation back surface glass layer) may be made of the same material or different materials. The infrared radiation glass layer G1 and the back surface glass layer G2 (infrared radiation back surface glass layer) may be configured as tempered glass, and a single layer glass treated by heat treatment or chemical treatment can be suitably used, and the strength can be increased compared to that of ordinary glass (i.e., untempered glass such as soda-lime silica glass or annealed glass). Furthermore, the infrared-emitting glass layer G1 and the back glass layer G2 (infrared-emitting back glass layer) may be reinforced with fillers and / or fibers. The infrared radiation glass layer G1 and the rear surface glass layer G2 (infrared radiation rear surface glass layer), and the intermediate resin Tu are preferably transparent to visible light.
[0037] As an example of a method for manufacturing the glass composite W shown in FIG. 1, first, a laminate is formed by interposing an intermediate resin Tu between the resin film Bj on which the above-mentioned metal material is sputtered and the infrared radiation glass layer G1, and between the resin film Bj on which the above-mentioned metal material is sputtered and the back surface glass layer G2. Next, the glass composite W is temporarily bonded by a method such as a nipper roll method in which the laminated glass composite W is heated to about 70 to 100°C, then sandwiched between rollers and temporarily bonded while removing the air, a rubber channel method in which the ends (four sides) of the glass composite W in a planar view are tied with rubber tubes, the air is removed, and temporarily bonded, or a rubber bag method in which the glass composite W is placed in a rubber bag and the inside of the rubber bag is vacuumed to temporarily bond the glass composite W. Finally, the components are permanently bonded by autoclaving at about 100 to 130° C. for about 1 to 2 hours under pressure to remove all air and bond the components together. Furthermore, when the intermediate resin Tu is heated during the bonding process, it flows into the portion of the light-reflecting layer B where the thin portion B2 exists, and when the thickness of the thin portion B2 is 0 μm, it directly connects the infrared radiation glass layer G1 and the back surface glass layer G2.
[0038] As another configuration of the glass composite W, as shown in FIG. 4, a structure in which an infrared emitting glass layer G1, a light reflecting layer B, an intermediate resin Tu, and a back surface glass layer G2 are laminated from the side of a first emitting surface H1 as the emitting surface H may be used. The light reflecting layer B is formed, for example, by spraying ceramics having a predetermined color (e.g., white) onto the surface of the infrared radiation glass layer G1 opposite to the side where the first radiation surface H1 exists, by screen printing or the like, and then baking and hardening the ceramics to adhere to the surface. That is, the light reflecting layer B is a ceramic layer formed on the surface of the ceramics of the infrared radiation glass layer G1. Titanium oxide, magnesium oxide, etc. can be suitably used as the ceramics. The light-reflecting layer B has a thick portion B3 and thin portions B1 and B2, similar to the glass composite W shown in FIG. The glass composite W is manufactured by carrying out the above-mentioned temporary pressure bonding and main pressure bonding with an intermediate resin Tu interposed between the infrared radiation glass layer G1 to which the light reflecting layer B is fixed and the back surface glass layer G2. Incidentally, in both the glass composite W shown in FIG. 1 and the glass composite W shown in FIG. 4, the back glass layer G2 can be used as the air side (the side indicated by the arrow Z).
[0039] From the viewpoint of exerting the above-mentioned infrared radiation performance, in the glass composite W shown in Fig. 1, the thickness of the infrared radiation glass layer G1 is preferably 200 µm or more and 10,000 µm or less, and in the glass composite W shown in Fig. 4, the thickness of the infrared radiation glass layer G1 is preferably 200 µm or more and 10,000 µm or less. In addition, in the glass composite W in which the back surface glass layer G2 is on the air side (the side indicated by the arrow Z), the thickness of the back surface glass layer G2 is preferably 200 µm or more and 10,000 µm or less, and in the glass composite W shown in Fig. 4, the thickness of the back surface glass layer G2 is preferably 200 µm or more and 10,000 µm or less.
[0040] The glass composite W described thus far has an overall surface average solar reflectance of 40% or more, and a surface average average emissivity, which is the wavelength average of the emissivity of infrared light of 8 μm or more and 13 μm or less, of 80% or more. It is more preferable that the overall surface average solar reflectance is 60% or more, and the surface average average emissivity, which is the wavelength average of the emissivity of infrared light of 8 μm or more and 13 μm or less, is 85% or more.
[0041] [Test Results] Regarding the glass composite W described above, those having the structure shown in Fig. 1 were designated as Examples 1, 2, and 4, and those having the structure shown in Fig. 4 were designated as Examples 3 and 5. In addition, as shown in Fig. 5, a structure in which an infrared emitting glass layer G, a light reflective layer B, and an infrared emitting layer J were laminated in the listed order from the air side was designated as Comparative Example 1, and an infrared emitting glass layer alone was designated as Comparative Example 2.
[0042] The conditions for the glass composite W tested in the examples and comparative examples are as shown in the following Table 2. The test results are shown in Table 1.
[0043] [Table 1]
[0044] [Table 2]
[0045] The above test results show that the glass composites W according to Examples 1 to 5 provide good results in terms of emissivity, visible light reflectance, radio wave transmittance, daylighting properties, and glare resistance. On the other hand, in the glass composite W of Comparative Example 1, since the light-reflecting layer B does not have a thin portion, it is presumed that the test conditions for radio wave transmittance, lighting, and anti-reflection properties are not satisfied. Moreover, in the glass composite W according to Comparative Example 2, the light reflecting layer B is not provided, and therefore it is presumed that the test conditions for visible light reflectance are not satisfied.
[0046] [Another embodiment] (1) The glass composite W described above may have a configuration in which a light control layer (not shown) having a light control function is provided on the side of the infrared emitting glass layer G1 opposite to the side on which the first emitting surface H1 is present.
[0047] (2) The glass composite W described above may have a configuration in which an ultraviolet reflective layer that reflects ultraviolet rays is provided along the emitting surface H. In the case of the glass composite W, the ultraviolet reflective layer can be suitably made of a material such as an aluminum alloy.
[0048] Furthermore, the configurations disclosed in the above embodiments (including other embodiments, the same applies below) can be applied in combination with configurations disclosed in other embodiments, provided that no contradiction arises. Furthermore, the embodiments disclosed in this specification are merely examples, and the embodiments of the present invention are not limited thereto, and can be appropriately modified within the scope that does not deviate from the purpose of the present invention. [Industrial Applicability]
[0049] INDUSTRIAL APPLICABILITY The glass composite of the present invention can be effectively used as a glass composite that can improve electromagnetic wave transmittance and daylighting properties and can reduce glare at night, etc. [Explanation of symbols]
[0050] 2: Thin wall part B:Light reflective layer B1: 1st metal thin section B2: 2nd metal thin section B3:Thick part G1: Infrared radiation glass layer G2: Rear glass layer H: Radiation surface H1: 1st radiation surface H2: Second radiation surface J: Infrared radiation layer Tu: Intermediate resin W: Glass composite Z:Lamination direction
Claims
1. an infrared radiation glass layer that emits infrared light from a first radiation surface that is a radiation surface, and a back surface glass layer that is provided opposite to a surface of the infrared radiation glass layer opposite to a side on which the first radiation surface is present, a light reflecting layer that reflects light is provided between the infrared radiation glass layer and the back surface glass layer; the light reflecting layer has a thick portion in a stacking direction and a thin portion whose thickness in the stacking direction is 2 / 3 or less of the thickness of the thick portion, The thin portion is provided continuously and integrally in a plan view perpendicular to the first radiation surface and has an area of 5 cm 2 a first metal thin portion having an area equal to or greater than the area of the first metal thin portion, and a second metal thin portion provided integrally and continuously in the plan view and having an area in the plan view less than the area of the first metal thin portion, The second thin metal portion is provided in a plurality of portions in a dispersed manner in the plan view, A glass composite having an overall surface average solar reflectance of 40% or more and a surface average average emissivity, which is the wavelength average of the emissivity of infrared light of 8 μm or more and 13 μm or less, of 80% or more.
2. the light reflecting layer is a metal deposition layer formed by depositing a metal on a resin material, The metal is at least one of silver, a silver alloy, aluminum, an aluminum alloy, and a copper alloy; 2. The glass composite according to claim 1, wherein the intermediate resin bonding between the infrared radiation glass layer and the metal vapor deposition layer and between the rear glass layer and the metal vapor deposition layer is made of any one of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane.
3. the light reflecting layer is a ceramic layer formed on a surface of the infrared radiation glass layer, 2. The glass composite according to claim 1, wherein an intermediate resin that bonds the light-reflecting layer and the rear glass layer is made of any one of polyvinyl butyral, polyethylene vinyl acetate, and polyurethane.
4. 3 . The glass composite according to claim 1 , wherein the first thin metal portion and the second thin metal portion each have a thickness in the stacking direction of 0 nm or more and 50 nm or less.
5. 3 . The glass composite according to claim 1 , wherein the first thin metal portion and the second thin metal portion each have a thickness in the stacking direction of 0 nm or more and 10 nm or less.
6. In the plan view, the area of the second metal thin portion is 0.03 cm 2 The glass composite according to claim 1 or 2.
7. The infrared radiation glass layer and the rear surface glass layer are 3. The glass composite according to claim 1, which is made of at least one of alkali-free glass, soda-lime glass, alkali borosilicate glass, and acrylic resin glass.
8. 3 . The glass composite according to claim 1 , wherein a ratio of an area of the thin portion to an entire area of the light reflective layer in the plan view is 1% or more and 50% or less.
9. The glass composite according to claim 1 or 2, further comprising a light control layer having a light control function, on a side of the infrared radiation glass layer opposite to a side on which the first radiation surface is present.
Citation Information
Patent Citations
Windshield for vehicle and method for manufacturing the same
JP2002020142A
Highly heat insulating dimming glass and method of manufacturing the same
JP2006206398A
Laminate and vehicle roof window
JP2014034486A
Substantially transparent substrate with high-emissivity and low-emissivity coating layers - Patent Application 20070122997
JP2022543529A