Probe, measuring device, and measuring method
The probe with a controlled surface roughness and consistent contact pressure stabilizes the contact state with strain gauges, reducing variations in measured values and ensuring reliable measurements without damaging the gauge.
Patent Information
- Application Number
- JP2020010246
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-01-24
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2040-01-24
AI Technical Summary
Variations in measured values occur when measuring the electrical characteristics of strain gauges and circuit boards due to inconsistent contact between probes and terminals, affecting measurement reliability.
A probe with a contact surface having a maximum height Rz of 3 μm to 8 μm and a measuring device that includes a mechanism to maintain consistent contact pressure and surface roughness, along with a method to periodically dress the contact surface to maintain this range.
The solution stabilizes the contact state between the probe and the terminal, reducing variations in measured values and preventing damage to the strain gauge, thereby enhancing measurement reliability and reducing the need for multiple measurements to achieve reliable results.
Smart Images

Figure 0007586645000001 
Figure 0007586645000002 
Figure 0007586645000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a probe, a measuring device, and a measuring method. [Background technology]
[0002] The manufacturing process of strain gauges includes a measurement process to measure the input resistance, output resistance, and output voltage of the strain gauge. This measurement process is performed to check whether the strain gauge has the designed electrical characteristics. A similar measurement process is also performed when mounting a circuit board to a product.
[0003] In the above measurement step, for example, a probe is brought into contact with a strain gauge or a terminal of a circuit board to pass a test current. Patent Document 1 shows an example of the probe. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2009-210443 A Summary of the Invention [Problem to be solved by the invention]
[0005] When a probe is brought into contact with the terminals of an object to be measured (such as a strain gauge or a circuit board) to measure the electrical characteristics of the object, the measured values may vary. In other words, the results of multiple measurements performed on the same object under the same conditions may not be the same. Such variation in the measured values is undesirable because it affects the reliability of the measurement results.
[0006] An object of the present invention is to provide a probe capable of suppressing variation in measurement values, a measurement device including the probe, and a measurement method using the probe. [Means for solving the problem]
[0007] According to a first aspect of the present invention, A probe for measuring an electrical characteristic of a device under test, comprising: a contact surface to be brought into contact with the object to be measured; The probe has a contact surface having a maximum height Rz of 3 μm or more and 8 μm or less.
[0008] In the probe of the first aspect, an oxide film may be formed on a portion of the object to be measured that comes into contact with the contact surface.
[0009] In the probe of the first aspect, the object to be measured may be a strain gauge.
[0010] According to a second aspect of the present invention, A measuring apparatus for measuring electrical characteristics of a device under test, comprising: A probe according to the first aspect, A jig for holding the probe; There is provided a measuring apparatus including a device for moving the device to hold the device and bring the device into contact with the contact surface of the probe.
[0011] In the measuring device of the second aspect, the object to be measured moving mechanism is configured such that the contact pressure between the contact surface of the probe and the object to be measured is 850 to 1150 gf / mm 2 The object to be measured may be brought into contact with the contact surface of the probe so that the contact surface is in a position such that the object to be measured is in a position such ...
[0012] The measuring device of the second aspect may further comprise a roughening member moving mechanism that holds a roughening member for roughening the contact surface of the probe and brings the roughening member into contact with the contact surface.
[0013] In the measuring apparatus of the second aspect, the jig may be configured to hold a plurality of the probes in a matrix, and the object to be measured moving mechanism may be configured to simultaneously contact the plurality of probes held in the matrix with the object to be measured.
[0014] According to a third aspect of the present invention, A method for measuring an electrical characteristic of a device under test, comprising: bringing the contact surface of the probe of the first aspect into contact with the object to be measured and measuring an electrical characteristic of the object to be measured; A method of measurement is provided that includes roughening the contact surface.
[0015] In the measurement method of the third aspect, The surface roughening treatment may be performed every time a predetermined number of measurements of the object are made, or every time a predetermined time period elapses. Effect of the Invention
[0016] According to the probe of the present invention, a measuring device including the probe, and a measuring method using the probe, it is possible to suppress variation in the measured values. [Brief description of the drawings]
[0017] [Figure 1] FIG. 1(a) is a top view of a strain gauge strip. FIG. 1(b) is a top view of a strain gauge included in the strain gauge strip. FIG. 1(c) is a circuit diagram of a Wheatstone bridge configured within the strain gauge. [Diagram 2] FIG. 2 is a side view of the measurement device according to the embodiment of the present invention. [Diagram 3] FIG. 3 is a perspective view of a table included in the measurement device. [Figure 4] FIG. 4 is a top view, with a portion thereof omitted, of the measurement device according to the embodiment of the present invention. [Diagram 5] FIG. 5 is a side view of a probe according to an embodiment of the present invention. [Figure 6] FIG. 6 is a flowchart of a measurement method according to an embodiment of the present invention. [Figure 7]Figures 7(a) to 7(d) are diagrams for explaining the operation of the measuring device. Figure 7(a) shows the state where the table is in the work exchange position. Figure 7(b) shows the state where the table is in the standby position. Figure 7(c) shows the state where the table is in the work measurement position. Figure 7(d) shows the state where the table is in the marking position. [Figure 8] FIG. 8 is a table showing the evaluation results of maximum height Rz and variation for the probes of Examples 1 to 11 and the probes of Comparative Examples 1 to 3. [Figure 9] 9(a), 9(b), and 9(c) are diagrams for explaining the influence of a change in the contact state between the contact surface of the probe and the terminal on the contact resistance. [Figure 10] 10(a), 10(b), and 10(c) are diagrams for explaining the influence of a change in the contact state between the contact surface of the probe and the terminal on the contact resistance. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] <Embodiment> The probe 50 and measuring device (in-circuit tester) 100 of the embodiment of the present invention will be described using an example in which the electrical characteristics (input resistance, output resistance, output voltage, etc.) of multiple strain gauges included in a strain gauge strip 900 (Figure 1(a)) are measured.
[0019] [Strain Gauge Strip 900] A strain gauge strip 900, which is an object to be measured, includes a gauge base 910 that is substantially rectangular in plan view, and a wiring layer 920 formed on the gauge base 910, as shown in FIG. 1(a).
[0020] The gauge base 910 may be a film-like sheet made of insulating resin, such as PI (polyimide) resin, epoxy resin, PET (polyethylene terephthalate) resin, etc. The thickness of the gauge base 910 may be, for example, about 20 μm to 30 μm. An alignment hole 910h is formed at each of the four corners of the gauge base 910, penetrating the gauge base 910 in the thickness direction.
[0021] The wiring layer 920 is formed of, for example, a copper-nickel alloy. The wiring layer 920 includes a plurality of gauge patterns GP arranged in a matrix of 5 rows and 4 columns. 11 ~GP 54 The thickness of the wiring layer 920 may be, for example, about 3 μm to 5 μm.
[0022] Gauge Pattern GP 11 ~GP 54 As shown in Fig. 1(b) and Fig. 1(c), each of 1 , R 2 , R 3 , R 4 and four terminals T A , T B , T C , T D and wiring W connecting them. Four resistors R 1 ~R 4 , 4 terminals T A ~T D , and wiring W form a Wheatstone bridge circuit.
[0023] A part of the gauge base 910 and a gauge pattern GP formed on the part 11 ~GP 54 This allows the strain gauge SG 11 ~SG 54 Each is composed of the following. 11 ~GP 54 Collectively, these are called Gauge Pattern GP. mn and strain gauge SG 11 ~SG 54 Collectively, these are called strain gauges SG mn It is called.
[0024] [Measuring device 100] 2, the measuring device 100 includes a base 10, a driving mechanism 20 built into the base 10, a table 30 movably supported by the driving mechanism 20, and a probe holding mechanism 40 disposed on the upper surface of the base 10. The probe holding mechanism 40 holds a plurality of probes 50.
[0025] The measuring device 100 further includes a measurement execution unit 60 connected to each of the multiple probes 50 by wiring (not shown), a marking mechanism 70 adjacent to the probe holding mechanism 40, and a control unit CONT that controls the overall operation of the measuring device 100.
[0026] In the following, the left-right direction in Fig. 2 is referred to as the sliding direction of the measuring device 100, and the depth direction in Fig. 2 (the direction perpendicular to the paper surface) is referred to as the width direction of the measuring device 100. The sliding direction is the direction in which the driving mechanism 20 slides the table 30 along the horizontal plane, and the width direction is the direction perpendicular to the sliding direction within the horizontal plane. The up-down direction in Fig. 2, i.e., the direction perpendicular to the sliding direction and the width direction, is referred to as the up-down direction. In the sliding direction, the side where the table 30 is located in Fig. 2 is referred to as the workpiece installation side, and the side where the probe holding mechanism 40 is located is referred to as the workpiece measurement side.
[0027] The base 10 is in the shape of a hollow box and has a top plate 10t extending along a horizontal plane. The top plate 10t has a longitudinal opening 10A (FIGS. 2 and 4) extending in the sliding direction.
[0028] The driving mechanism 20 is a mechanism for moving the table 30 in the sliding direction and the up-down direction. The driving mechanism 20 has a main body portion 21 and a support portion 22 that is moved by the main body portion 21.
[0029] The main body 21 is housed inside the base 10 and is located near the top plate 10t. The main body 21 may be any mechanism capable of moving the support part 22 in the sliding direction and the up-down direction. As an example, the main body 21 is composed of a power generation mechanism including a motor and a piezoelectric actuator, and a power transmission mechanism including gears, belts, chains, pulleys, etc.
[0030] The support portion 22 is a columnar structure extending in the vertical direction. The support portion 22 extends from the upper surface of the main body portion 21 through the opening 10A of the top plate 10t to above the top plate 10t.
[0031] As shown in FIG. 3, the table 30 is a flat plate having a substantially square shape in plan view.
[0032] A cylindrical alignment pin 30p standing upright from the top surface 30u is provided at each of the four corners of the top surface 30u of the table 30. A plurality of intake holes 30h are provided along each side at the periphery of the top surface 30u of the table 30. Each of the plurality of intake holes 30h is connected to an intake device (not shown) via an air flow path (not shown) inside the table 30 and a flexible intake hose (not shown) connected to the table 30 and communicating with the air flow path.
[0033] The lower surface of the table 30 is fixed to the upper end of the support portion 22 of the drive mechanism 20. As a result, the table 30 is supported by the drive mechanism 20 in a state in which it can move in the sliding direction and the up-down direction.
[0034] The probe holding mechanism 40 has a rectangular parallelepiped jig 41 that holds the plurality of probes 50 , and four support columns 42 that support the jig 41 .
[0035] 4, the jig 41 has a matrix of holding holes 41h that penetrate the jig 41 in the up-down direction. In this embodiment, 80 holding holes 41h (5 rows in the width direction × 16 columns in the sliding direction) are formed.
[0036] The four support columns 42 extend upward from the upper surface of the top plate 10t and are connected to the four corners of the lower surface of the jig 41. Two support columns 42 aligned in the width direction sandwich the opening 10A in the width direction.
[0037] Each of the multiple probes 50 (FIG. 5) is formed of a metal such as tungsten, copper, platinum, or gold. Each of the multiple probes 50 has a cylindrical shape, for example. One end of the probe 50 is connected to a strain gauge SG mn Terminal T A ~T D The contact surface 50c is in contact with the
[0038] The contact surface 50c is, for example, circular. The diameter of the contact surface 50c may be, for example, about 0.1 mm to 1.2 mm. The surface roughness (maximum height Rz) of the contact surface 50c is preferably 3 μm≦Rz≦8 μm. This reduces the variation in the measured values and prevents damage to the strain gauge during measurement. The reason for this will be described later. In this specification and the present invention, the "maximum height Rz" refers to the maximum height Rz defined and measured in accordance with JIS B 0601-2001.
[0039] The multiple probes 50 are arranged in a matrix by being inserted into multiple holding holes 41h of the jig 41. As shown in Fig. 2, each of the multiple probes 50 is housed inside the holding hole 41h with the contact surface 50c facing downward and penetrating the jig 41 from top to bottom.
[0040] As shown in Fig. 4, the jig 41 holds 80 probes 50 and arranges them in a matrix of 5 rows and 16 columns. If the four probes 50 arranged in the width direction are regarded as a probe set 50S (Fig. 4), the jig 41 holds 20 probe sets 50S and arranges them in a matrix of 5 rows and 4 columns. During measurement, the four probes 50 of each probe set 50S are connected to the respective strain gauges SG mn The four terminals of T A ~T D Contact (details below).
[0041] The measurement execution unit 60 uses the probe 50 to measure the strain gauge SG mnThe measurement execution unit 60 is disposed inside the base 10 and is connected to each of the plurality of probes 50 by wiring (not shown).
[0042] The measurement execution unit 60 includes a power supply 61, a digital multimeter (DMM) 62, and a relay circuit (measurement circuit) 63. The power supply 61 supplies an input voltage for measurement. The DMM 62 is connected to a strain gauge SG mn The input resistance, output resistance, output voltage, etc. of the relay circuit 63 are circuits that connect the power supply 61, the DMM 62, and each of the multiple probes 50. The configuration of the relay circuit 63 is switchable (changeable) depending on the measurement content.
[0043] The marking mechanism 70 marks a predetermined strain gauge SG based on the result of the measurement performed by the measurement execution unit 60. mn The marking mechanism 70 is disposed on the workpiece installation side of the jig 41 in the sliding direction.
[0044] The marking mechanism 70 has a pen 71 having a pen tip 71t, and a pen holding mechanism 72 that holds the pen 71 so as to be movable in the width direction and the up-down direction. Note that the marking mechanism 70 is not limited to one that uses a pen, and may be one that performs marking with a needle or a cutter.
[0045] The pen 71 is held by a pen holding mechanism 72 with the pen tip 71t facing downward. The pen holding mechanism 72 may be any mechanism capable of moving the pen 71 in the width direction and the up-down direction. One example of the pen holding mechanism 72 is an air slider.
[0046] The control unit CONT is housed inside the base 10. The control unit CONT is connected to the drive mechanism 20, the measurement execution unit 60, and the marking mechanism 70 and is capable of communicating with them.
[0047] [Measurement method] Strain gauge SG using probe 50 and measuring device 100 mnMeasurement of electrical characteristics (input resistance, output resistance, output voltage, etc.) includes a work setting step S1, a measurement step S2, and a marking step S3, as shown in the flowchart of FIG.
[0048] In the workpiece setting step S1, the strain gauge strip 900, which is the object to be measured, is set on the table 30 of the measuring device 100. Specifically, the workpiece setting step S1 is performed, for example, as follows.
[0049] First, the table 30 is moved to the position farthest from the jig 41 (FIG. 7(a); hereinafter, referred to as the "workpiece installation position"), and the strain gauge strip 900 is installed on the table 30. At this time, by arranging the alignment pins 41p at the four corners of the table 30 respectively inside the alignment holes 910h at the four corners of the gauge base 910, the strain gauge strip 900 can be easily aligned with the table 30.
[0050] Next, air is sucked in through the air intake holes 30h of the table 30 to suck the strain gauge strip 900, and the strain gauge strip 900 is fixed to the table 30. In addition to or instead of the suction through the air intake holes 30h, a weight can be used. Specifically, for example, a weight having a resin attached to the bottom surface of a picture frame-like metal frame can be placed on the peripheral portion of the strain gauge strip 900 to press down on the peripheral portion of the strain gauge strip 900 from above.
[0051] By bringing the strain gauge strip 900 into close contact with the upper surface 30u of the table 30, in other words by holding the strain gauge strip 900 flat, the multiple probes 50 are attached to the multiple strain gauges SG mn Terminal T A ~T D This allows the contact with the sample in a uniform state, thereby improving the accuracy of the measurement in the measurement step S2.
[0052] In the measurement step S2, the strain gauge SG included in the strain gauge strip 900 mnThe electrical characteristics of each of the above are measured mainly using the multiple probes 50 and the measurement execution unit 60. Specifically, the measurement step S2 is performed as follows, for example.
[0053] First, the table 30 is slid to a position directly below the jig 41 (FIG. 7(b) hereinafter referred to as the "standby position"). After that, the table 30 is raised to a position where the contact surfaces 50c of the multiple probes 50 contact the strain gauge strip 900 (FIG. 7(c) hereinafter referred to as the "measurement position"), and then stopped.
[0054] When the table 30 is stopped at the measurement position, each of the multiple probes 50 is in contact with the multiple strain gauges SG of the strain gauge strip 900. mn Specifically, the four probes 50 included in each probe set 50S contact each of the strain gauges SG mn Each terminal T A ~T D The contact pressure (probe pressing pressure) is, for example, about 60 to about 80 gf (about 850 to about 1150 gf / mm) per probe 50. 2 ) degree.
[0055] Next, the measurement execution unit 60 measures the strain gauge SG mn The input resistance, output resistance, and output voltage are measured for each of the following. A specific measurement method is as follows, for example.
[0056] The measurement execution unit 60 first performs the following steps to measure the strain gauge SG 11 Measurements are taken.
[0057] (1) Using the relay circuit 63, the power supply 61, terminal T A Probe 50 contacting terminal T A , terminal T C , terminal T C A closed circuit is formed connecting the probe 50 that contacts the strain gauge SG 11 Measure the input resistance. (2) Using the relay circuit 63, the power supply 61, terminal T BProbe 50 contacting terminal T B , terminal T D , terminal T D A closed circuit is formed connecting the probe 50 that contacts the DMM 62 and the strain gauge SG 11 Measure the output resistance. (3) Using the relay circuit 63 and the probe 50, connect the power supply unit 61 to the terminal T A , T C and connect the DMM62 to terminal T B , T D The power supply unit 61 connects to the strain gauge SG 11 to the input voltage V in With the strain gauge SG applied, 11 Output voltage V out (zero balance measurement).
[0058] The measurement execution unit 60 measures the strain gauge SG 11 The input resistance, output resistance, and output voltage of are sent to the control unit CONT.
[0059] The measurement execution unit 60 is a strain gauge SG 11 After the measurement is completed, switch relay circuit 63 to connect strain gauge SG 12 The measurement execution unit 60 performs similar measurements on 20 strain gauges SG mn The same measurement is carried out for all of the strain gauges SG in order. mn The input resistance, output resistance, and output voltage of each of these are sent to a control unit CONT.
[0060] In the marking step S3, the marking mechanism 70 marks the strain gauge SG mn Marking is performed on a predetermined one of the strain gauges. Specifically, the marking step is performed, for example, as follows.
[0061] First, the table 30 is lowered from the measurement position to the standby position, and then slid to a position directly below the marking mechanism 70 (FIG. 7(d) (hereinafter referred to as the "marking position").
[0062] On the other hand, the control unit CONT receives the strain gauge SG mn Each measured value (input resistance, output resistance, output voltage) is compared with a predetermined reference value to determine whether each measured value is within an allowable tolerance.
[0063] The control unit CONT is a multi-strain gauge SG mn If the measured value is outside the allowable tolerance in any of the above, the strain gauge is placed directly under the pen 71. The alignment in the sliding direction is performed by moving the table 30, and the alignment in the width direction is performed by moving the pen holding mechanism 72.
[0064] Next, the control unit CONT uses the pen holding mechanism 72 to lower the pen 71 and mark the strain gauges whose measured values are determined not to be within the allowable tolerance.
[0065] The control unit CONT performs marking on all the strain gauges whose measured values are determined to be outside the allowable tolerance, and then returns the table 30 to the workpiece installation position.
[0066] Thereafter, the strain gauge strip 900 that has been measured is removed from the table 30, and the workpiece setting step S1, the measurement step S2, and the marking step S3 are repeated.
[0067] [Dressing method] Here, a dressing method (surface roughening method) for dressing (roughening) the contact surface 50c of the probe 50 to give the contact surface 50c a desired surface roughness will be described.
[0068] It has been observed that when measurements of the strain gauge strip 900 using the measuring device 100 are continuously performed, the surface roughness of the contact surface 50c of the probe 50 of the measuring device 100 decreases (the maximum height Rz becomes smaller). This is because the contact surface 50c of the terminal T A ~T D This is because the contact surface 50c is pressed by the contact hole 50b and becomes smooth.
[0069] Therefore, it is preferable to dress the contact surface 50c after every predetermined number of measurements of the strain gauge strip 900 or after every predetermined time (periodically) to return the maximum height Rz of the contact surface 50c to the range of 3 μm≦Rz≦8 μm.
[0070] Specifically, the dressing is carried out, for example, as follows.
[0071] First, the table 30 is moved to a work placement position, and a sandpaper (roughened member) having a rectangular shape in plan view is placed on the table 30. Alignment holes may be provided at the four corners of the sandpaper so that alignment can be performed using the alignment pins 30p. The sandpaper may have the same dimensions and thickness as the strain gauge strip 900.
[0072] Next, the table 30 on which the sandpaper is placed is moved to a standby position and raised. As a result, the sandpaper is pressed against the contact surface 50c with a predetermined pressure (for example, about 60 gf to about 80 gf per probe), the roughness of the sandpaper is transferred to the contact surface 50c, and the contact surface 50c is dressed. The table 30 may be raised and lowered multiple times to press the sandpaper against the contact surface 50c multiple times.
[0073] Thereafter, the table 30 is returned to the workpiece placement position, and the sandpaper is replaced with a cleaning cloth (wiping cloth), which is pressed against the contact surface 50c once or multiple times in the same manner as the sandpaper. The cleaning cloth may be soaked in ethanol or the like.
[0074] After wiping is completed, return the table 30 to the work installation position, replace the cleaning cloth with the next object to be measured (strain gauge strip 900), and then mn Resume measurement of the electrical characteristics.
[0075] [Significance of keeping surface roughness (maximum height Rz) at 3μm≦Rz≦8μm] Next, the reason why it is preferable to set the maximum height Rz of the contact surface 50c in the probe 50 of this embodiment to 3 μm or more and 8 μm or less will be explained.
[0076] First, the reason why it is preferable to set the maximum height Rz of the contact surface 50c to 3 μm or more is as follows.
[0077] The inventors of the present invention have studied methods for suppressing the variation in measured values that occurs when measuring the electrical characteristics of a strain gauge using a probe, and have focused on the surface roughness (maximum height Rz) of the contact surface of the probe. According to the findings of the inventors of the present invention, the variation in measured values is caused by the contact state between the contact surface of the probe and the terminal of the strain gauge being slightly different each time a measurement is performed, which changes the contact resistance that occurs between the contact surface and the terminal. Furthermore, the inventors of the present invention have found that by making the maximum height Rz of the contact surface of the probe 3 μm or more, the contact state between the contact surface of the probe and the terminal of the strain gauge can be stabilized, and the change in contact resistance can be sufficiently suppressed.
[0078] Based on the above findings, the inventors of the present invention conducted the following tests.
[0079] First, the contact surfaces of the same type of probes were treated with files of different grits to prepare four probes each of Examples 1 to 11 having a maximum contact surface height Rz of about 3 μm or more and Comparative Examples 1 to 3 having a maximum contact surface height Rz of less than about 3 μm. In addition, one sample strain gauge was prepared.
[0080] The probes of Examples 1 to 11 and Comparative Examples 1 to 3 were all made of tungsten, and the contact surface was circular with a diameter of 0.3 mm.
[0081] The maximum heights Rz of the contact surfaces of the probes of Examples 1 to 11 and the probes of Comparative Examples 1 to 3 are as shown in FIG.
[0082] The maximum heights Rz of the probes of Examples 1 to 11 and the probes of Comparative Examples 1 to 3 were measured in accordance with JIS B 0601-2001.
[0083] The sample strain gauge had the structure shown in Figure 1(b). The wiring layer of the sample strain gauge was made of copper-nickel alloy and had a thickness of about 5 μm. The gauge base of the sample strain gauge was made of PI (polyimide) and had a thickness of about 25 μm.
[0084] Next, the probes of Example 1 were held by the jig 41 of the measuring device 100 so as to form one probe set 50S, and the input resistance and output resistance of the sample strain gauge were measured three times each using the measuring device 100. In the three measurements, the probe pressing pressure was constant (70 gf per probe). After that, the variation (difference between the maximum and minimum values) of the three measured values obtained by the three measurements of the input resistance and the output resistance was calculated.
[0085] Also, for each of the probes in Examples 2 to 11 and Comparative Examples 1 to 3, the input resistance and output resistance of the sample strain gauge were each measured three times in the same manner as in Example 1, and the variation of the three measured values for each of the input resistance and output resistance was determined. The same sample strain gauge was used in the measurements of each of the Examples and Comparative Examples.
[0086] The results of the measurement are shown in Fig. 8. In Fig. 8, the input resistance and output resistance for which the variation among the three measured values is less than ±1Ω are indicated with a circle. On the other hand, the input resistance and output resistance for which the variation among the three measured values is ±1Ω or more are indicated with a cross. As shown in Fig. 8, in Examples 1 to 11 in which the maximum height Rz is 3 µm or more, the variation in the measured values is less than ±1Ω, and in Comparative Examples 1 to 3 in which the maximum height Rz is less than 3 µm, the variation in the measured values is ±1Ω or more.
[0087] According to the knowledge of the inventors of the present invention, one of the reasons why the variation in the measurement values becomes large when the maximum height Rz of the contact surface of the probe is small is as follows.
[0088] FIG. 9(a) shows a simplified cross-sectional view of the contact surface CS1 of the probe, and FIG. 10(a) shows a simplified cross-sectional view of the contact surface CS2 of the probe. The maximum height Rz of the contact surface CS1 is smaller than the maximum height Rz of the contact surface CS2. In FIG. 9(a) and FIG. 10(a), the dotted line L 11 , L 21 indicates the surface position of the terminal of the strain gauge. The contact surfaces CS1 and CS2 are indicated by the dotted line L 11 , L 21 In the portion located below, the contact surfaces CS1 and CS2 press down on the surface of the terminal and are embedded inside the terminal. In other words, the contact surfaces CS1 and CS2 are biting into the surface of the terminal.
[0089] As shown in Fig. 9(b) and Fig. 10(b), the probe is at a small angle θ 0 The surface of the terminal is inclined by the dotted line L 12 , L 22 When the probe is moved to the position indicated by , the area of contact between the contact surfaces CS1, CS2 and the terminal surface changes roughly by an amount corresponding to the length of the bold line shown in Figures 9(b) and 10(b). As can be seen from Figures 9(b) and 10(b), when the angle of the probe relative to the terminal changes, there tends to be a large change in the contact area and therefore a large change in contact resistance at contact surface CS1, which has a small maximum height Rz.
[0090] In addition, in the contact surface CS1 with a small maximum height Rz, the probe is at a small angle θ 13 If the contact surface CS1 is tilted beyond the dotted line L 13 The probe is separated from the surface of the terminal at the position indicated by and the contact area becomes small. 23 If the contact surface CS2 is tilted beyond the dotted line L 23 The terminal at the position indicated by is completely separated from the surface, but the angle θ 23 is the angle θ13 Greater than.
[0091] In this way, when the angle of the probe relative to the terminal changes, the contact area and contact resistance tend to change more significantly on contact surface CS1, which has a relatively small maximum height Rz, than on contact surface CS2, which has a relatively large maximum height Rz.
[0092] In addition, as shown in Fig. 9(c) and Fig. 10(c), the probe is located at a small distance d 0 The surface of the terminal is moved away by the dotted line L 14 , L 24 When the probe is moved to the position indicated by , the contact area between the contact surfaces CS1, CS2 and the terminal surface changes roughly by an amount corresponding to the length of the bold line shown in Figures 9(c) and 10(c). As can be seen from Figures 9(c) and 10(c), even when the distance between the probe and the terminal changes, there tends to be a large change in the contact area and a large change in contact resistance at contact surface CS1, which has a small maximum height Rz.
[0093] In this way, when the maximum height Rz of the contact surface of the probe is small, the contact area and therefore the contact resistance change in response to changes in the contact state with the terminal, and the measurement values tend to vary more.
[0094] In addition, the terminals of the strain gauge made of copper-nickel alloy usually have an oxide film of about 3 μm or thinner. According to the findings of the inventors of the present invention, when the maximum height of the contact surface is greater than 3 μm, the convex parts of the contact surface (parts forming micro-mountains in the cross-sectional view of the contact surface) break through the oxide film, and a larger area of the contact surface directly contacts the terminals of the strain gauge. In this way, by bringing a larger area of the contact surface into direct contact with the terminals without an oxide film, the contact state is stabilized, and the amount of change in contact resistance according to changes in the contact state is suppressed.
[0095] For these reasons, it is preferable that the maximum height Rz of the contact surface 50c is set to 3 μm or more, which can effectively suppress the variation in the measurement values.
[0096] Next, the reason why it is preferable to set the maximum height Rz of the contact surface 50c to 8 μm or less is as follows.
[0097] A strain gauge generally has a structure in which a conductive wiring layer including a resistor is formed on a gauge base made of a flexible dielectric material, and when in use, the gauge base is attached to a strain element which is a conductor such as metal. In other words, the gauge base serves to insulate the wiring from the strain element.
[0098] In order to measure strain using a strain gauge, the resistor in the wiring layer needs to expand and contract appropriately in response to the expansion and contraction of the strain body, so it is not realistic to make the gauge base thicker just to consider insulation.
[0099] Taking the above into consideration, a strain gauge generally has a wiring layer with a thickness of about 3 to 5 μm and a gauge base with a thickness of about 25 μm.
[0100] According to the findings of the inventors of the present invention, when the maximum height of the contact surface of the probe is 8 μm or less, the convex portion of the contact surface of the probe does not excessively damage the gauge base when the contact surface of the probe is brought into contact with the terminal of the strain gauge. Therefore, it is possible to prevent the insulation performance of the gauge base from being deteriorated due to damage to the gauge base, which may cause the performance degradation of the strain gauge.
[0101] In view of the above, it is preferable that the maximum height Rz of the contact surface 50c is 8 μm or less.
[0102] The advantages of the probe 50, the measuring device 100, and the measuring method of this embodiment are summarized below.
[0103] The probe 50 of this embodiment is a strain gauge SG mn Terminal T A ~T D The surface roughness (maximum height Rz) of the contact surface that comes into contact with the terminal T is 3 μm or more. A ~TD The change in contact resistance in response to a change in the contact state with respect to the contact area is small, and the variation in the measured values can be suppressed when measurements are performed multiple times.
[0104] In addition, strain gauge SG mn Terminal T A ~T D Generally, an oxide film of about 3 μm or thinner is formed on the terminal T. Therefore, by making the maximum height of the contact surface 3 μm or more, the oxide film can be broken through and the contact surface 50 c and the terminal T A ~T D This makes it possible to suppress the amount of change in contact resistance in response to changes in the contact state, thereby suppressing the variation in the measured values.
[0105] In the probe 50 of this embodiment, the surface roughness (maximum height Rz) of the contact surface 50c is 8 μm or less. A ~T D The gauge base 910 is prevented from being damaged by contact with the terminal T. A ~T D This also prevents contact marks from remaining on the surface.
[0106] That is, in the probe 50 of this embodiment, the surface roughness (maximum height Rz) of the contact surface 50c is set to 3 μm or more, so that the terminal T A ~T D By stabilizing the contact state with the SG, the variation in the measured value can be suppressed, and by making the surface roughness (maximum height Rz) of the contact surface 50c 8 μm or less, the strain gauge SG that may occur during measurement can be suppressed. mn This can prevent damage to the
[0107] The measuring device 100 of this embodiment includes a probe 50 with reduced variation in measured values (i.e., highly reliable measured values), and therefore uses only one strain gauge SG mnA highly reliable measurement value can be obtained by performing only one measurement per strain gauge. Therefore, the measurement time can be significantly reduced compared to conventional measuring devices that require multiple measurements for one strain gauge to be performed and then averaged to increase the reliability of the measurement value.
[0108] The measurement method of this embodiment uses the measurement apparatus 100, and therefore produces the same effects as the measurement apparatus 100. In addition, the contact surface 50c of the probe 50 is dressed (roughened) at a predetermined timing to maintain the maximum height Rz of the contact surface 50c at 3 μm or more and 8 μm or less, so that highly reliable measurements can be continuously performed for a long period of time.
[0109] <Modification> In the probe 50, the measuring device 100, and the measuring method of the above embodiment, the following modifications may also be used.
[0110] The probe 50 of the above embodiment may be used independently of the measuring device 100. Specifically, for example, an operator operates the probe 50 to measure the strain gauge SG mn Terminal T A ~T D By contacting the probe with the strain gauge SG mn The electrical properties of the device may be measured.
[0111] In the above embodiment, the probe 50 has a cylindrical shape and the contact surface 50c is circular, but this is not limited to the above. The probe 50 and the contact surface 50c may have any shape. For example, the contact surface 50c may have a square or polygonal shape.
[0112] The object to be measured is a strain gauge SG mn Specifically, for example, the probe 50 can be used in measuring electrical characteristics (such as circuit resistance) of a PCBA (printed circuit board assembly). The terminals of the PCBA are also generally made of a copper-nickel alloy, and an oxide film of about 3 μm or thinner is formed thereon.
[0113] The object to be measured may be any other electric or electronic component whose electrical characteristics need to be measured.
[0114] In the measuring device 100 of the above embodiment, 80 holding holes 41h (5 rows in the width direction × 16 columns in the sliding direction) are formed in the jig 41, but this is not limited to this. The number and arrangement of the holding holes 41h in the jig 41, i.e., the number and arrangement of the probes 50 held by the jig 41, can be set arbitrarily depending on the design of the measuring device 100.
[0115] The measuring apparatus 100 of the above embodiment can be modified as needed to become a measuring apparatus for measuring any electric or electronic component whose electrical characteristics need to be measured. Specifically, for example, the configuration of the table 30 or the configuration of the jig 41 can be modified.
[0116] As long as the characteristics of the present invention are maintained, the present invention is not limited to the above-described embodiments, and other forms conceivable within the scope of the technical idea of the present invention are also included within the scope of the present invention. [Explanation of symbols]
[0117] 10 base, 20 drive mechanism, 30 table, 40 probe holding mechanism, 50 probe, 60 measurement execution unit, 70 marking mechanism, 100 measurement device, 900 strain gauge strip, SG mn Strain gauges
Claims
1. A method for measuring electrical characteristics of a strain gauge, comprising the steps of: a probe having a contact surface, the maximum height Rz of which is 3 μm or more and 8 μm or less, is brought into contact with a surface of a terminal of the strain gauge, the terminal having an oxide film formed on its surface, to measure electrical characteristics of the strain gauge; A measuring method comprising subjecting the contact surface to a roughening treatment.
2. The measurement method according to claim 1 , wherein the surface roughening treatment is performed every time a predetermined number of measurements are made with the strain gauge, or every time a predetermined time has elapsed.
Citation Information
Patent Citations
Wafer prober
JP1988170933A
Probe structure
JP2000002746A
Contact terminal and connector for semiconductor device inspection using the same
JP2007024613A
Mutilayer-type probe pin and probe card
JP2007256078A
Contact probe and method for manufacturing the same
JP2009210443A