Semiconductor device and its manufacturing method

The semiconductor device addresses the challenge of nitrogen loss and pit formation by using a high-melting-point second layer as a cap layer, ensuring the threshold voltage is maintained without additional processing, thereby reducing costs.

JP7586776B2Active Publication Date: 2024-11-19DENSO CORP +2
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021100862
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-06-17
Publication Date
2024-11-19
Estimated Expiration
2041-06-17

AI Technical Summary

Technical Problem

Forming highly active p-type diffusion regions in compound semiconductors like nitride semiconductors is challenging due to nitrogen loss and pit formation during high-temperature heat treatment, and residual cap layers can lower the threshold voltage.

Method used

A semiconductor device with a compound semiconductor layer comprising a first and second compound semiconductor layer, where the second layer with a higher melting point functions as a cap layer and remains intact, allowing the formation of a body region that spans both layers, thereby preventing a decrease in threshold voltage.

Benefits of technology

The method enables the formation of a semiconductor device with reduced cost by maintaining the second compound semiconductor layer as a channel region, even if it functions as a cap layer, thus preserving the threshold voltage and avoiding additional processing steps.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586776000001
    Figure 0007586776000001
  • Figure 0007586776000002
    Figure 0007586776000002
  • Figure 0007586776000003
    Figure 0007586776000003
Patent Text Reader

Abstract

To solve a problem in which: an n-type or an i-type cap layer remaining on a channel region causes concern about a reduction in threshold voltage.SOLUTION: A method for manufacturing a semiconductor device includes: a first step of preparing a compound semiconductor layer 15 having a first compound semiconductor layer 14 of a first conductivity type and a second compound semiconductor layer 16 of a first conductivity type or an i-type; wherein the second compound semiconductor layer is provided on the first compound semiconductor layer and has a higher melting point than that of the first compound semiconductor layer; a second step of ion-injecting an impurity of a second conductivity type to an upper layer part of the compound semiconductor layer to form a body region 24; a third step of, after the execution of the second step, applying heat treatment on the compound semiconductor layer; and a fourth step of forming an insulating gate 40 on the second compound semiconductor layer of the compound semiconductor layer.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present specification relates to a semiconductor device and a manufacturing method thereof. [Background technology]

[0002] In compound semiconductors such as nitride semiconductors and gallium oxide, it is difficult to form a highly active p-type diffusion region. For example, in the case of nitride semiconductors, heat treatment at 1200° C. or higher is required to activate the p-type dopant. However, when such a high-temperature heat treatment is performed, nitrogen is removed from the surface of the nitride semiconductor layer, and pits are formed on the surface of the nitride semiconductor layer. For this reason, it is not possible to perform a high-temperature heat treatment, and it is considered difficult to form a highly active p-type diffusion region.

[0003] Patent Document 1 proposes a technique for forming a cap layer made of a high melting point material such as aluminum nitride on a nitride semiconductor layer. By using such a cap layer, high temperature heat treatment can be performed while suppressing nitrogen loss, so that a highly active p-type diffusion region can be formed. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2017-108080 A Summary of the Invention [Problem to be solved by the invention]

[0005] In the technology using the cap layer, the cap layer is removed by etching after performing a high-temperature heat treatment. However, the etching may be insufficient and the cap layer may remain. In particular, if the cap layer remains on the channel region, there is a concern that the threshold voltage may be reduced because the cap layer is n-type or i-type. [Means for solving the problem]

[0006] The semiconductor device disclosed in the present specification may include a compound semiconductor layer (15, 115) having a first compound semiconductor layer (14, 114) and a second compound semiconductor layer (16, 116), the second compound semiconductor layer being provided on the first compound semiconductor layer and having a melting point higher than that of the first compound semiconductor layer, and an insulated gate (40, 140) provided on the second compound semiconductor layer of the compound semiconductor layer. The compound semiconductor layer may include a drift region (22, 122) of a first conductivity type, a source region (25, 125) of a first conductivity type, and a body region (24, 124) of a second conductivity type provided between the drift region and the source region and disposed at a position exposed on an upper surface of the compound semiconductor layer. The insulated gate faces the body region located between the drift region and the source region. The body region located between the drift region and the source region is disposed across both the first compound semiconductor layer and the second compound semiconductor layer.

[0007] In the above semiconductor device, the second compound semiconductor layer remains functioning as a cap layer. However, in the above semiconductor device, the body region located between the drift region and the source region, i.e., the channel region, is formed across both the first compound semiconductor layer and the second compound semiconductor layer. Therefore, even if the second compound semiconductor layer remains functioning as a cap layer, the second compound semiconductor layer is configured as the channel region, so that a decrease in the threshold voltage of the above semiconductor device is suppressed.

[0008] The present specification discloses a method for manufacturing a semiconductor device, comprising the steps of: a first step of preparing a compound semiconductor layer (15, 115) having a first conductive type first compound semiconductor layer (14, 114) and a first conductive type or i-type second compound semiconductor layer (16, 116), the second compound semiconductor layer being provided on the first compound semiconductor layer and having a melting point higher than that of the first compound semiconductor layer; and a second step of ion-implanting a second conductive type impurity into an upper layer portion of the compound semiconductor layer to form a body region (24, 124), the body region being a first conductive type. The method can include a second step of providing an insulating gate (40, 140) on the second compound semiconductor layer, the insulating gate being disposed between a drift region (22, 122) of a first conductivity type and a source region (25, 125) of a first conductivity type and arranged across both the first compound semiconductor layer and the second compound semiconductor layer, a third step of heat treating the compound semiconductor layer after performing the second step, and a fourth step of forming an insulating gate (40, 140) on the second compound semiconductor layer, the insulating gate facing the body region located between the drift region and the source region.

[0009] In the above manufacturing method, the body region, i.e., the channel region, located between the drift region and the source region is formed in the second compound semiconductor layer functioning as a cap layer, and the insulated gate is formed on the second compound semiconductor layer without removing the second compound semiconductor layer. Therefore, the above manufacturing method can configure the second nitride semiconductor layer as the channel region, and therefore it is possible to manufacture a semiconductor device in which a decrease in threshold voltage is suppressed even if the second compound semiconductor layer functioning as a cap layer remains. [Brief description of the drawings]

[0010] [Figure 1] 1 is a schematic cross-sectional view of a main portion of an embodiment of a semiconductor device; [Diagram 2] 2 shows a manufacturing flow of a part of the semiconductor device of FIG. [Diagram 3] 2 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. [Figure 4]2 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. [Diagram 5] 2 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. [Figure 6] 1 is a schematic cross-sectional view of a main portion of another embodiment of a semiconductor device; [Figure 7] 7 shows a manufacturing flow of a part of the semiconductor device of FIG. [Figure 8] 7 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. 6. [Figure 9] 7 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. 6. [Figure 10] 7 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. 6. [Figure 11] 7 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. 6. [Figure 12] 7 is a schematic cross-sectional view of a main part in one manufacturing process of the manufacturing method of the semiconductor device of FIG. 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, a semiconductor device and a manufacturing method thereof disclosed in this specification will be described with reference to the drawings. In each drawing, for the purpose of clarity, common components may be marked with a reference symbol only for one of the components.

[0012] (First embodiment) As shown in FIG. 1, the semiconductor device 1 includes a compound semiconductor substrate 12, a compound semiconductor layer 15, a drain electrode 32 provided so as to cover the lower surface of the compound semiconductor substrate 12, a source electrode 34 provided so as to cover part of the upper surface of the compound semiconductor layer 15, and a planar-type insulated gate 40 provided so as to cover part of the upper surface of the compound semiconductor layer 15.

[0013] The compound semiconductor substrate 12 is not particularly limited, and may be, for example, a gallium nitride substrate (GaN substrate). The compound semiconductor substrate 12 is a base substrate for epitaxially growing the compound semiconductor layer 15, as described later. The compound semiconductor substrate 12 also contains a high concentration of n-type dopant, and functions as the drain region 21. The n-type dopant is not particularly limited, and may be, for example, silicon. The drain region 21 is in ohmic contact with the drain electrode 32.

[0014] The compound semiconductor layer 15 is provided so as to be in contact with the upper surface of the compound semiconductor substrate 12, and is configured by laminating a first compound semiconductor layer 14 and a second compound semiconductor layer 16. The broken line shown in the figure indicates the interface between the first compound semiconductor layer 14 and the second compound semiconductor layer 16. The compound semiconductor layer 15 is not particularly limited, and may be configured, for example, of a nitride semiconductor. As an example, the first compound semiconductor layer 14 may be a gallium nitride layer (GaN layer), and the second compound semiconductor layer 16 may be an aluminum nitride layer (AlN layer). The first compound semiconductor layer 14 is provided so as to be in contact with the upper surface of the compound semiconductor substrate 12, and is disposed between the compound semiconductor substrate 12 and the second compound semiconductor layer 16. The second compound semiconductor layer 16 is provided so as to be in contact with the upper surface of the first compound semiconductor layer 14, and is disposed at a position exposed to the upper surface of the compound semiconductor layer 15.

[0015] The compound semiconductor layer 15 includes an n-type drift region 22 and a p - a body region 24 of the type; + A source region 25 of p + and a body contact region 26 of the same type.

[0016] The drift region 22 is provided so as to be in contact with the upper surface of the drain region 21, and is disposed between the drain region 21 and the body region 24. The drift region 22 also has a JFET region 23 provided so as to be sandwiched between the body region 24 in the surface direction of the compound semiconductor layer 15. In other words, the JFET region 23 is a part of the drift region 22 provided so as to penetrate the body region 24 from the upper surface of the compound semiconductor layer 15. The JFET region 23 is provided at a position exposed on the upper surface of the compound semiconductor layer 15, and is in contact with the insulating gate 40. The JFET region 23 is disposed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. The drift region 22 contains an n-type dopant at a lower concentration than the drain region 21. The n-type dopant is not particularly limited, and may be, for example, silicon.

[0017] The body region 24 is provided in contact with the upper surface of the drift region 22, and is disposed adjacent to the side surface of the JFET region 23. A part of the body region 24 is provided at a position exposed on the upper surface of the compound semiconductor layer 15, and is in contact with the insulated gate 40. A part of the body region 24 is disposed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. The body region 24 contains a p-type dopant. The p-type dopant is not particularly limited, and may be, for example, magnesium.

[0018] The source region 25 is provided so as to be in contact with the upper surface of the body region 24, and is separated from the drift region 22 by the body region 24. The source region 25 is provided at a position exposed on the upper surface of the compound semiconductor layer 15, and is in contact with the insulating gate 40. The source region 25 is disposed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. The source region 25 contains an n-type dopant at a higher concentration than the drift region 22. The n-type dopant is not particularly limited, and may be, for example, silicon. The source region 25 is in ohmic contact with the source electrode 34.

[0019] The body contact region 26 is provided so as to be in contact with the upper surface of the body region 24. The body contact region 26 is provided at a position exposed on the upper surface of the compound semiconductor layer 15, and is arranged across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. The body contact region 26 contains a p-type dopant at a higher concentration than the body region 24. The p-type dopant is not particularly limited, and may be, for example, magnesium. The body contact region 26 is in ohmic contact with the source electrode 34.

[0020] The insulated gate 40 is provided so as to contact a part of the upper surface of the second compound semiconductor layer 16 of the compound semiconductor layer 15, and has a gate insulating film 42 made of silicon oxide and a gate electrode 44 made of polysilicon. The gate electrode 44 faces the body region 24 at a position separating the JFET region 23, which is a part of the drift region 22, from the source region 25, and the JFET region 23 via the gate insulating film 42.

[0021] Next, the operation of the semiconductor device 1 will be described. During use, a positive voltage is applied to the drain electrode 32, and the source electrode 34 is grounded. When a positive voltage higher than the gate threshold voltage is applied to the gate electrode 44, an inversion layer is formed in the body region 24, i.e., the channel region, at a portion separating the JFET region 23 and the source region 25. Electrons flow from the source region 25 to the JFET region 23 through the inversion layer formed in the channel region. The electrons that flow into the JFET region 23 flow vertically through the JFET region 23 and the drift region 22 toward the drain electrode 32. This brings the drain electrode 32 and the source electrode 34 into conduction, and the semiconductor device 1 is turned on. When the gate electrode 44 is grounded, the inversion layer disappears, and the semiconductor device 1 is turned off. In this way, the semiconductor device 1 can perform a switching operation that switches between on and off between the drain electrode 32 and the source electrode 34 based on the voltage applied to the gate electrode 44.

[0022] (Method of Manufacturing Semiconductor Device 1) 2 is a manufacturing flow showing a flow of some steps among those for manufacturing the semiconductor device 1. FIGS. 3 to 5 are cross-sectional views of the main part in the manufacturing process corresponding to the manufacturing flow of FIG.

[0023] First, as shown in FIG. 3, the first compound semiconductor layer 14 is crystal-grown from the upper surface of the compound semiconductor substrate 12 using an epitaxial growth technique, and the second compound semiconductor layer 16 is crystal-grown from the upper surface of the first compound semiconductor layer 14 to form the compound semiconductor layer 15 (step S1 in FIG. 2). The first compound semiconductor layer 14 is formed by crystal growth so as to include an n-type dopant. The second compound semiconductor layer 16 may be formed by crystal growth so as to include an n-type dopant, or may be formed by crystal growth without doping. The thickness of the second compound semiconductor layer 16 is 15 nm or less. When the thickness of the second compound semiconductor layer 16 is 15 nm or less, cracks are prevented from occurring in the second compound semiconductor layer 16 due to the influence of the lattice constant difference between the first compound semiconductor layer 14 (GaN layer in this example) and the second compound semiconductor layer 16 (AlN layer in this example), and the second compound semiconductor layer 16 can be formed with good quality.

[0024] Next, as shown in Fig. 4, a p-type dopant or an n-type dopant is implanted into a predetermined region in the upper layer of the compound semiconductor layer 15 using an ion implantation technique to form a body region 24, a source region 25, and a body contact region 26 (step S2 in Fig. 2). The order in which these semiconductor regions 24, 25, and 26 are formed is not particularly limited. The dopants for forming these semiconductor regions 24, 25, and 26 are implanted so as to straddle both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. When the second compound semiconductor layer 16 is an i-type, an n-type dopant may be implanted into a portion of the second compound semiconductor layer 16 corresponding to the JFET region 23.

[0025] Next, a heat treatment is performed to activate these semiconductor regions 24, 25, and 26 (step S3 in FIG. 2). The temperature of the heat treatment is not particularly limited, but may be, for example, 1200° C. or higher. Such a high-temperature heat treatment can satisfactorily activate the implanted dopants, particularly magnesium, which is a p-type dopant. In addition, the second compound semiconductor layer 16 (in this example, the AlN layer) is made of a material having a higher melting point than the first compound semiconductor layer 14 (in this example, the GaN layer). Therefore, the second compound semiconductor layer 16 can function as a cap layer, and can suppress nitrogen loss from the upper surface of the compound semiconductor layer 15 and suppress the formation of pits on the upper surface of the compound semiconductor layer 15.

[0026] Next, as shown in FIG. 5, an insulated gate 40 is formed on the compound semiconductor layer 15 (step S4 in FIG. 2). Specifically, a gate insulating film 42 is formed by using a deposition technique so as to cover the upper surface of the second compound semiconductor layer 16 of the compound semiconductor layer 15. The deposition technique is not particularly limited, but may be an atomic layer deposition method or a plasma CVD method. Next, a heat treatment technique is performed to improve the film quality of the gate insulating film 42. The heat treatment temperature may be 800° C. or higher. Next, a gate electrode 44 is formed on the upper surface of the gate insulating film 42 by using a deposition technique. Furthermore, the gate insulating film 42 and the gate electrode 44 are processed by using an etching technique to form the insulated gate 40. Thereafter, a drain electrode 32 and a source electrode 34 are formed by using a known manufacturing technique, thereby manufacturing the semiconductor device 1 shown in FIG. 1.

[0027] In a conventional manufacturing method using a cap layer, an n-type or i-type cap layer is formed after ion implantation into a compound semiconductor layer. Then, a heat treatment is performed for activation. After the heat treatment, the cap layer is removed, and an insulating gate is formed on the compound semiconductor layer from which the cap layer has been removed. In such a conventional manufacturing method, there is a concern that the threshold voltage will be lowered if the n-type or i-type cap layer remains on the channel region. In addition, if a CMP technique, for example, is used to prevent the cap layer from remaining, there is a concern that the cost will increase and the channel region will be damaged.

[0028] In the manufacturing method disclosed in this specification, a diffusion region is also formed in the second compound semiconductor layer 16 functioning as a cap layer, and an insulated gate 40 is formed on the second compound semiconductor layer 16 without removing the second compound semiconductor layer 16. In particular, in this manufacturing method, a body region at a position separating the drift region 22 and the source region 25, i.e., a channel region, is formed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. Therefore, in this manufacturing method, a part of the second compound semiconductor layer 16 can be configured as the channel region, so that a semiconductor device 1 can be manufactured in which a decrease in threshold voltage is suppressed even if the second compound semiconductor layer 16 functioning as a cap layer remains.

[0029] Second embodiment Fig. 6 shows a semiconductor device 2 which is a modified example of the semiconductor device 1 shown in Fig. 1. Components common to the semiconductor device 1 shown in Fig. 1 are indicated by adding "1" to the hundreds digit, and descriptions of those components may be omitted to avoid repetition.

[0030] 6, the semiconductor device 2 is characterized by including a trench-type insulating gate 140 provided in a trench TR formed in the upper surface of the compound semiconductor layer 115. As with the semiconductor device 1 shown in Fig. 1, the compound semiconductor substrate 112 is a gallium nitride substrate (GaN substrate), the first compound semiconductor layer 114 is a gallium nitride layer (GaN layer), and the second compound semiconductor layer 116 is an aluminum nitride layer (AlN layer).

[0031] The compound semiconductor layer 115 is configured by laminating a first compound semiconductor layer 114 and a second compound semiconductor layer 116. The dashed line shown in the figure indicates the interface between the first compound semiconductor layer 114 and the second compound semiconductor layer 116. The first compound semiconductor layer 114 is provided so as to be in contact with the upper surface of the compound semiconductor substrate 112, and is disposed between the compound semiconductor substrate 112 and the second compound semiconductor layer 116. The second compound semiconductor layer 116 is provided so as to be in contact with the upper surface of the first compound semiconductor layer 114, and is disposed at a position exposed at the upper surface of the compound semiconductor layer 115. In this specification, the side surface and bottom surface of the trench TR are also included in the upper surface of the compound semiconductor layer 115.

[0032] The compound semiconductor layer 115 includes an n-type drift region 122 and a p - A body region 124 of the type, + A source region 125 of type p + A body contact region 126 of the p - and an electric field relaxation region 127 of the type.

[0033] The drift region 122 is provided so as to be in contact with an upper surface of the drain region 121, and is disposed between the drain region 121 and the body region 124. A part of the drift region 122 is provided at a position exposed at a corner between the side surface and the bottom surface of the trench TR, and is in contact with the side surface and the bottom surface of the insulating gate 140. The drift region 122 at a position exposed at the corner between the side surface and the bottom surface of the trench TR is disposed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16.

[0034] The body region 124 is provided so as to be in contact with an upper surface of the drift region 122. A part of the body region 124 is provided at a position exposed to the side surface of the trench TR and is in contact with a side surface of the insulating gate 140. The body region 124 at a position exposed to the side surface of the trench TR is disposed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16.

[0035] The source region 125 is provided in contact with an upper surface of the body region 124 and is separated from the drift region 122 by the body region 124. The source region 125 is provided at a position exposed to the side surface of the trench TR and in contact with a side surface of the insulating gate 140. The source region 125 is disposed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16.

[0036] The body contact region 126 is provided so as to be in contact with the upper surface of the body region 124. The body contact region 126 is provided at a position exposed on the upper surface of the compound semiconductor layer 115, and is disposed across both the first compound semiconductor layer 114 and the second compound semiconductor layer 116.

[0037] The electric field relaxation region 127 is provided at a position exposed at the bottom surface of the trench TR, and is in contact with the bottom surface of the insulated gate 140. The electric field relaxation region 127 is disposed between the insulated gate 140 and the drift region 122, and is provided to relax the electric field at the bottom surface of the insulated gate 140. The electric field relaxation region 127 is disposed across both the first compound semiconductor layer 114 and the second compound semiconductor layer 116. The electric field relaxation region 127 contains a p-type dopant to the same extent as the body region 124. The p-type dopant is not particularly limited, and may be, for example, magnesium.

[0038] The insulating gate 140 is provided in the trench TR, and has a gate insulating film 142 made of silicon oxide and a gate electrode 144 made of polysilicon. The gate insulating film 142 is provided so as to cover the side and bottom surfaces of the trench TR. The gate electrode 144 is separated from the compound semiconductor layer 115 by the gate insulating film 142, and faces, via the gate insulating film 142, the body region 124 at a position separating the drift region 122 and the source region 125.

[0039] Next, the operation of the semiconductor device 2 will be described. During use, a positive voltage is applied to the drain electrode 132, and the source electrode 134 is grounded. When a positive voltage higher than the gate threshold voltage is applied to the gate electrode 144, an inversion layer is formed in the body region 124 at a position separating the drift region 122 and the source region 125, i.e., in the channel region. Electrons flow from the source region 125 to the drift region 122 through the inversion layer formed in the channel region. The electrons that flow into the drift region 122 flow vertically through the drift region 122 toward the drain electrode 132. This brings the drain electrode 132 and the source electrode 134 into conduction, and the semiconductor device 2 is turned on. When the gate electrode 144 is grounded, the inversion layer disappears, and the semiconductor device 2 is turned off. In this way, the semiconductor device 2 can perform a switching operation that switches between on and off between the drain electrode 132 and the source electrode 134 based on the voltage applied to the gate electrode 144.

[0040] (Method of Manufacturing Semiconductor Device 2) 7 is a manufacturing flow showing a flow of some steps among those for manufacturing the semiconductor device 2. FIGS. 8 to 12 are cross-sectional views of the main part in the manufacturing process corresponding to the manufacturing flow of FIG.

[0041] 8, a first compound semiconductor layer 114 is crystal-grown from the upper surface of a compound semiconductor substrate 112 by using an epitaxial growth technique (Step S11 in FIG. 7). The first compound semiconductor layer 14 is formed by crystal growth so as to contain an n-type dopant.

[0042] Next, as shown in FIG. 9, a trench TR extending from the upper surface of the first compound semiconductor layer 114 toward the depth thereof is formed using photolithography and etching techniques (Step S12 in FIG. 7).

[0043] Next, as shown in FIG. 10, the second compound semiconductor layer 116 is crystal-grown from the upper surface of the first compound semiconductor layer 114 using an epitaxial growth technique to form the compound semiconductor layer 115 (step S13 in FIG. 7). The second compound semiconductor layer 116 is also formed in the trench TR. The second compound semiconductor layer 116 may be formed by crystal growth so as to include an n-type dopant, or may be formed by crystal growth without doping. The thickness of the second compound semiconductor layer 116 is 15 nm or less. When the thickness of the second compound semiconductor layer 116 is 15 nm or less, cracks are prevented from occurring in the second compound semiconductor layer 116 due to the influence of the lattice constant difference between the first compound semiconductor layer 114 (in this example, a GaN layer) and the second compound semiconductor layer 116 (in this example, an AlN layer), and a good quality second compound semiconductor layer 116 can be formed.

[0044] 11, a p-type dopant or an n-type dopant is implanted into a predetermined region in the upper part of the compound semiconductor layer 115 using an ion implantation technique to form a body region 124, a source region 125, a body contact region 126, and an electric field relaxation region 127 (step S14 in FIG. 7). The order in which these semiconductor regions 124, 125, 126, and 127 are formed is not particularly limited. The dopants for forming these semiconductor regions 124, 125, 126, and 127 are implanted so as to straddle both the first compound semiconductor layer 114 and the second compound semiconductor layer 116.

[0045] Next, a heat treatment is performed to activate these semiconductor regions 124, 125, 126, and 127 (step S15 in FIG. 7). The temperature of the heat treatment is not particularly limited, but may be, for example, 1200° C. or higher. Such a high-temperature heat treatment can satisfactorily activate the implanted dopant, particularly magnesium, which is a p-type dopant. In addition, the second compound semiconductor layer 116 (in this example, the AlN layer) is made of a material having a higher melting point than the first compound semiconductor layer 114 (in this example, the GaN layer). Therefore, the second compound semiconductor layer 116 can function as a cap layer, and can suppress nitrogen loss from the upper surface of the compound semiconductor layer 115 and suppress the formation of pits on the upper surface of the compound semiconductor layer 115.

[0046] Next, as shown in FIG. 12, an insulated gate 140 is formed on the compound semiconductor layer 115, and the insulated gate 140 is disposed in the trench TR (step S16 in FIG. 7). Specifically, a gate insulating film 142 is formed by using a deposition technique so as to cover the upper surface of the second compound semiconductor layer 116 including the inside of the trench TR. Next, a gate electrode 144 is formed on the upper surface of the gate insulating film 142 by using a deposition technique. Furthermore, the gate insulating film 142 and the gate electrode 144 are processed by using an etching technique to form the insulated gate 140 in the trench TR. Thereafter, a drain electrode 132 and a source electrode 134 are formed by using a known manufacturing technique, whereby the semiconductor device 2 shown in FIG. 7 can be manufactured.

[0047] Even in this manufacturing method, a part of the channel region of the body region 124 is formed across both the first compound semiconductor layer 14 and the second compound semiconductor layer 16. Therefore, even in this manufacturing method, a part of the second compound semiconductor layer 116 can be configured as the channel region, so that a semiconductor device 2 in which a decrease in the threshold voltage is suppressed can be manufactured even if the second compound semiconductor layer 116 functioning as a cap layer remains.

[0048] The features of the technology disclosed in this specification are summarized below. Note that the technical elements described below are independent technical elements that exhibit technical usefulness alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing.

[0049] The semiconductor device disclosed in this specification may include a compound semiconductor layer having a first compound semiconductor layer and a second compound semiconductor layer, the second compound semiconductor layer being provided on the first compound semiconductor layer and having a melting point higher than that of the first compound semiconductor layer, and an insulated gate provided on the second compound semiconductor layer. The material of the compound semiconductor layer is not particularly limited, and may be, for example, a nitride semiconductor or gallium oxide. When the material of the compound semiconductor layer is a nitride semiconductor, the material of the first compound semiconductor layer may be gallium nitride, and the material of the second compound semiconductor layer may be aluminum nitride. The compound semiconductor layer may have a drift region of a first conductivity type, a source region of a first conductivity type, and a body region of a second conductivity type provided between the drift region and the source region and disposed at a position exposed on the upper surface of the compound semiconductor layer. The insulated gate faces the body region located between the drift region and the source region. The body region located between the drift region and the source region is disposed across both the first compound semiconductor layer and the second compound semiconductor layer.

[0050] In the above semiconductor device, when the material of the first compound semiconductor layer is gallium nitride and the material of the second compound semiconductor layer is aluminum nitride, the second compound semiconductor layer may have a thickness of 15 nm or less.

[0051] The insulated gate of the semiconductor device may be of a planar type or a trench type. When the insulated gate is of a planar type, the drift region may be disposed at a position exposed on the upper surface of the compound semiconductor layer, and may have a JFET region of a first conductivity type adjacent to the body region. In this case, the insulated gate may face the body region located between the JFET region and the source region. When the insulated gate is of a trench type, a trench (TR) may be formed on the upper surface of the compound semiconductor layer. The body region located between the drift region and the source region may be disposed at a position exposed to a side surface of the trench. In this case, the insulated gate may be provided in the trench.

[0052] The method for manufacturing a semiconductor device disclosed in the present specification may include a first step of preparing a compound semiconductor layer having a first conductive type first compound semiconductor layer and a second conductive type or i-type compound semiconductor layer, the second compound semiconductor layer being provided on the first compound semiconductor layer and having a higher melting point than the first compound semiconductor layer, a second step of ion-implanting a second conductive type impurity into an upper layer portion of the compound semiconductor layer to form a body region, the body region being provided between a first conductive type drift region and a first conductive type source region and being disposed across both the first compound semiconductor layer and the second compound semiconductor layer, a third step of heat-treating the compound semiconductor layer after the second step is performed, and a fourth step of forming an insulated gate on the second compound semiconductor layer, the insulated gate facing the body region located between the drift region and the source region. The material of the compound semiconductor layer is not particularly limited, and may be, for example, a nitride semiconductor or gallium oxide. When the material of the compound semiconductor layers is a nitride semiconductor, the material of the first compound semiconductor layer may be gallium nitride, and the material of the second compound semiconductor layer may be aluminum nitride.

[0053] In the above-mentioned method for manufacturing a semiconductor device, when the material of the first compound semiconductor layer is gallium nitride and the material of the second compound semiconductor layer is aluminum nitride, the thickness of the second compound semiconductor layer may be 15 nm or less. When the thickness of the second compound semiconductor layer is 15 nm or less, cracks are prevented from occurring in the second compound semiconductor layer due to the influence of the lattice constant difference between the first compound semiconductor layer and the second compound semiconductor layer, and a high-quality second compound semiconductor layer can be formed.

[0054] In the method for manufacturing a semiconductor device described above, when the material of the compound semiconductor layer is a nitride semiconductor, the heat treatment temperature in the third step may be 1200° C. or higher, thereby making it possible to effectively activate the dopant.

[0055] In the above manufacturing method, the first step may include a step of growing the first compound semiconductor layer from a surface of a compound semiconductor substrate, and a step of growing the second compound semiconductor layer from a surface of the first compound semiconductor layer. The second compound semiconductor layer functioning as a cap layer can be formed prior to ion implantation.

[0056] Although specific examples of the present invention have been described above in detail, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and variations of the specific examples exemplified above. Furthermore, the technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. Furthermore, the technology exemplified in this specification or drawings can achieve multiple objectives simultaneously, and achieving one of these objectives is itself technically useful. [Explanation of symbols]

[0057] 12,112: compound semiconductor substrate, 14,114: first compound semiconductor layer, 15,115: compound semiconductor layer, 16,116: second compound semiconductor layer, 21,121: drain region, 22,122: drift region, 23,123: JFET region, 24,124: body region, 25,125: source region, 26,126: body contact region, 32,132: drain electrode, 34,134: source electrode, 40,140: insulated gate

Claims

1. A semiconductor device (1, 2), a compound semiconductor layer (15, 115) having a first compound semiconductor layer (14, 114) and a second compound semiconductor layer (16, 116), the second compound semiconductor layer being provided on the first compound semiconductor layer and having a melting point higher than that of the first compound semiconductor layer; an insulated gate (40, 140) provided on the second compound semiconductor layer, The compound semiconductor layer is A drift region (22, 122) of a first conductivity type; A source region (25, 125) of a first conductivity type; a body region (24, 124) of a second conductivity type provided between the drift region and the source region and disposed at a position exposed on an upper surface of the compound semiconductor layer, the insulated gate faces the body region at a position between the drift region and the source region; the body region located between the drift region and the source region is disposed across both the first compound semiconductor layer and the second compound semiconductor layer.

2. 2. The semiconductor device according to claim 1, wherein the material of said compound semiconductor layer is a nitride semiconductor.

3. the material of the first compound semiconductor layer is gallium nitride; The semiconductor device according to claim 2 , wherein the material of the second compound semiconductor layer is aluminum nitride.

4. The semiconductor device according to claim 3 , wherein the second compound semiconductor layer has a thickness of 15 nm or less.

5. the drift region is disposed at a position exposed on the upper surface of the compound semiconductor layer and has a first conductivity type JFET region (23) adjacent to the body region, 5. The semiconductor device according to claim 1, wherein the insulated gate is a planar type and faces the body region located between the JFET region and the source region.

6. a trench (TR) is formed on the top surface of the compound semiconductor layer; the body region located between the drift region and the source region is disposed at a position exposed to a side surface of the trench; 5. The semiconductor device according to claim 1, wherein the insulated gate is of a trench type and is provided within the trench.

7. A method for manufacturing a semiconductor device, comprising: a first step of preparing a compound semiconductor layer (15, 115) having a first compound semiconductor layer (14, 114) of a first conductivity type and a second compound semiconductor layer (16, 116) of a first conductivity type or an i-type, the second compound semiconductor layer being provided on the first compound semiconductor layer and having a melting point higher than that of the first compound semiconductor layer; a second step of ion-implanting a second conductivity type impurity into an upper layer portion of the compound semiconductor layer to form a body region (24, 124), the body region being provided between a first conductivity type drift region (22, 122) and a first conductivity type source region (24, 124) and being disposed across both the first compound semiconductor layer and the second compound semiconductor layer; a third step of heat-treating the compound semiconductor layer after the second step is performed; a fourth step of forming an insulated gate (40, 140) on the second compound semiconductor layer, the insulated gate facing the body region located between the drift region and the source region.

8. The method for manufacturing a semiconductor device according to claim 7 , wherein the material of the compound semiconductor layer is a nitride semiconductor.

9. the material of the first compound semiconductor layer is gallium nitride (GaN); 9. The method for manufacturing a semiconductor device according to claim 8, wherein a material of the second compound semiconductor layer is aluminum nitride (AlN).

10. 10. The method for manufacturing a semiconductor device according to claim 9, wherein the second compound semiconductor layer has a thickness of 15 nm or less.

11. 11. The method for manufacturing a semiconductor device according to claim 8, wherein the heat treatment temperature in the third step is 1200° C. or higher.

12. The first step comprises: growing the first compound semiconductor layer from a surface of a compound semiconductor substrate (12, 112); 12. The method for manufacturing a semiconductor device according to claim 7, further comprising: growing the second compound semiconductor layer from a surface of the first compound semiconductor layer.

Citation Information

Patent Citations

  • Manufacture of p-type gallium nitride based compound semiconductor

    JP1993183189A

  • Method of manufacturing nitride semiconductor device

    JP2017108080A

  • Semiconductor device manufacturing method

    JP2018056257A

  • Semiconductor device and manufacturing method of the same

    JP2018056297A

  • Nitride semiconductor device

    JP2021009989A