Semiconductor device and method for manufacturing the same

By forming a semiconductor device with an uneven surface structure for the barrier metal interface, the adhesion of the gate pad is enhanced, addressing the peeling issue and improving device reliability.

JP7586796B2Active Publication Date: 2024-11-19KK TOSHIBA +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021153436
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-09-21
Publication Date
2024-11-19
Estimated Expiration
2041-09-21

AI Technical Summary

Technical Problem

Existing semiconductor devices, particularly IGBTs, face issues with insufficient adhesion of the gate pad due to peeling from the barrier metal, despite the use of polysilicon and silicide interfaces.

Method used

The semiconductor device incorporates a second layer with uneven portions on its surface, where the barrier metal is formed to match the irregularities, enhancing adhesion through an anchor effect, and optionally using plugs or metal films to further stabilize the interface.

Benefits of technology

The uneven surface structure significantly improves the adhesion of the gate pad, reducing peeling and enhancing the reliability of the semiconductor device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586796000001
    Figure 0007586796000001
  • Figure 0007586796000002
    Figure 0007586796000002
  • Figure 0007586796000003
    Figure 0007586796000003
Patent Text Reader

Abstract

To improve adhesiveness of a gate pad.SOLUTION: A semiconductor device comprises a silicon wafer, a first layer, a second layer, a barrier metal and a gate pad. The first layer is formed from an oxide film provided on the silicon wafer. The second layer is a layer including a rugged part at least selectively on a top face of the first layer, and the rugged part has ruggedness deeper than ruggedness which occurs when forming the layer planar. The barrier metal is formed on a top face of a second layer 2 along a shape of the rugged part. The gate pad is adhered with the silicon wafer via the barrier metal.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD An embodiment of the present invention relates to a semiconductor device and a method for manufacturing a semiconductor device. [Background technology]

[0002] IGBTs (Insulated Gate Bipolar Transistors) are widely used as power devices in vehicles, trains, industrial equipment, and the like, as switching elements, etc. In these IGBTs, oxide films, interlayer films, etc. are formed on a silicon substrate on which drift, collector, etc. are formed, and a gate pad for applying a gate voltage is formed on the upper part via a barrier metal. If a gate pad is simply provided on the barrier metal, the gate pad often peels off from the metal. To address this, there is a technology for improving adhesion by forming polysilicon in the interlayer film and forming silicide at the interface between this polysilicon and the barrier metal, but even in this case, the adhesion may not be sufficient. For this reason, further technological improvements are desired. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 7-263484 Summary of the Invention [Problem to be solved by the invention]

[0004] One embodiment provides a semiconductor device with improved adhesion of a gate pad and a method for manufacturing the semiconductor device. [Means for solving the problem]

[0005] According to one embodiment, the semiconductor device includes a silicon substrate, a first layer, a second layer, a barrier metal, and a gate pad. The first layer is formed of an oxide film provided on the silicon substrate. The second layer has an uneven portion at least selectively on an upper surface of the first layer, the uneven portion having a deeper unevenness than the unevenness that occurs when the layer is formed flat. The barrier metal is formed on the upper surface of the second layer 2 according to the shape of the uneven portion. The gate pad is in close contact with the silicon substrate via the barrier metal. [Brief description of the drawings]

[0006] [Figure 1] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Diagram 2] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Diagram 3] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 4] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Diagram 5] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 6] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 7] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 8] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 9] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 10] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 11] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 12] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 13]1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 14] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 15] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 16] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 17] 1A to 1C are cross-sectional views each showing a schematic process for a semiconductor device according to an embodiment of the present invention. [Figure 18] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 19] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 20] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 21] 1 is a cross-sectional view showing a schematic diagram of a portion of a semiconductor device according to an embodiment; [Figure 22] FIG. 4 is a plan view showing a schematic example of an uneven portion according to an embodiment. [Diagram 23] FIG. 4 is a plan view showing a schematic example of an uneven portion according to an embodiment. [Figure 24] FIG. 4 is a plan view showing a schematic example of an uneven portion according to an embodiment. [Diagram 25] FIG. 4 is a plan view showing a schematic example of an uneven portion according to an embodiment. [Figure 26] FIG. 4 is a plan view showing a schematic example of an uneven portion according to an embodiment. [Figure 27] FIG. 4 is a plan view showing a schematic example of an uneven portion according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, the embodiments will be described with reference to the drawings. Since this disclosure describes the formation of a gate pad, it should be noted that illustrations and descriptions of semiconductors formed in a silicon substrate are omitted. In addition, in the drawings, the ratio of the size of elements to each other, the aspect ratio, or the angle, etc. may be changed to make the structure easier to understand, but the contents of the embodiments are not limited to these ratios and are configured with appropriate sizes. In addition, the parts described as having an angular shape may have a rounded shape at the corner due to process specifications such as etching or design configuration, etc. In addition, the expression "top surface" is used, but this refers to a surface that is vertically upward in a general semiconductor process. In addition, although the uneven portion is described, the number of grooves in this uneven portion in each figure is shown as an example that is not limited, and can be changed arbitrarily.

[0008] (First embodiment) FIG. 1 is a cross-sectional view showing a schematic view of a part of a semiconductor device according to a first embodiment.

[0009] The semiconductor device 1 is, for example, an IGBT (Insulated Gate Bipolar Transistor). The semiconductor device 1 includes a silicon substrate 10, an oxide film 12, an interlayer film 14, polysilicon 16, a barrier metal 18, and a gate pad 20. The semiconductor device 1 operates as a power device by applying a voltage to a semiconductor layer formed on the silicon substrate 10 via the gate pad 20.

[0010] The silicon substrate 10 is a substrate on which various semiconductor layers are formed, for example, a drift layer and a collector layer. As a non-limiting example, when the semiconductor device 1 is an n-channel IGBT, a channel is formed in a p-type semiconductor layer formed on the upper part of an n-type drift layer by applying a voltage from the gate pad 20 through the oxide film 12. A collector current flows from the collector to an emitter electrode formed on the silicon substrate 10 through the p-type semiconductor layer, the n-type drift layer, and the channel. Of course, even in the case of a p-channel IGBT, a collector current is appropriately output based on the voltage applied to the gate pad 20.

[0011] The oxide film 12 is a gate insulating film formed as a first layer on the silicon substrate 10, and is formed, for example, of a thermal oxide film (SiO2) obtained by thermally oxidizing Si. As another example, it may be replaced by a thermal nitride film (SiON) obtained by thermally nitriding Si.

[0012] The interlayer film 14 is an interlayer insulating film formed on the oxide film 12, and separates the wiring arranged on the silicon substrate 10. The interlayer film 14 is, for example, an insulating film formed by doping fluorine or the like into a SiO2 film.

[0013] The polysilicon 16 is formed on the oxide film 12 of the silicon substrate 10, selectively in the interlayer film 14 so as to be in contact with the barrier metal 18. In the process of manufacturing the semiconductor device 1, a silicide is formed between this polysilicon 16 and the material of the barrier metal 18. The formation of the silicide improves the adhesion between the silicon substrate 10 and the barrier metal 18 (and the gate pad 20). In this embodiment, the second layer 2 is formed by this interlayer film 14 and the polysilicon 16.

[0014] The barrier metal 18 is a metal film formed between the polysilicon 16 (a predetermined region of the second layer 2) and the gate pad 20. The barrier metal 18 is a metal film formed to prevent diffusion or mutual reaction of the metal material used in the gate pad 20. For example, the barrier metal 18 is made of a material that forms a silicide with the polysilicon 16 and has good adhesion to the gate pad 20.

[0015] The gate pad 20 functions as a gate electrode and controls the current flowing through the semiconductor device 1 by a voltage input to the gate pad 20. The gate pad 20 may be made of, for example, Al, AlSi, AlCu, AlSiCu, Cu, Au, W, WSi, Ti, TiSi, or the like.

[0016] The material of the barrier metal 18 is appropriately selected depending on the material of the gate pad 20. For example, if the gate pad 20 is Al or AlSi, the barrier metal 18 may be made of Ti or TiN, and if the gate pad 20 is Cu, the barrier metal 18 may be made of Ta or TaN. The material is not limited to these, and the barrier metal 18 may be made of a material having the appropriate properties described below. In the following, as an example, the gate pad 20 is described as AlSi, and the barrier metal 18 is described as Ti or TiN.

[0017] In this embodiment, the polysilicon 16 and the barrier metal 18 are not in contact with each other at a plane interface, but have a selectively formed uneven portion 100 in their cross section. The height h of this uneven portion 100 is sufficiently larger than the unevenness (up to about 150 nm) that occurs when polysilicon is formed on a plane. For example, h may be about 300 to 600 nm, and is formed to be sufficiently larger than the unevenness that occurs when polysilicon 16 is formed. In other words, the uneven portion 100 formed in polysilicon 16 has a depth sufficiently deeper than the depth of the unevenness that may occur when polysilicon 16 is formed flat.

[0018] In addition, in the barrier metal 18, a metal film such as W may be formed at least on the sidewall region of the unevenness formed in the barrier metal 18 so as not to fill the unevenness.

[0019] According to this shape, the gate pad 20 is also formed with projections and recesses. By forming the gate pad 20 in this manner, it is possible to suppress bond peeling between the silicon substrate 10 and the gate pad 20 due to the anchor effect. Furthermore, by forming a silicide at the interface, it is possible to further suppress bond peeling. Furthermore, when a metal film such as W is formed at the contact surface between the gate pad 20 and the barrier metal 18, this metal film can further improve adhesion. These features are the same in the following embodiments.

[0020] A manufacturing process for the semiconductor device 1 according to this embodiment will be described with reference to FIGS.

[0021] 2, a semiconductor layer is formed in a silicon substrate 10 by various processes so as to operate appropriately, and an oxide film 12 is formed on the upper surface of the silicon substrate 10. Then, polysilicon 16 is formed on the upper surface of the oxide film 12. This process is performed by a general process.

[0022] 3, a mask 30 is selectively formed on the upper surface of the polysilicon 16. The mask 30 is formed according to the region where the gate electrode is to be disposed on the silicon substrate 10, so that the polysilicon 16 is formed on this region. In the case of photolithography, the mask 30 is a photoresist.

[0023] Next, the polysilicon 16 is etched as shown in Fig. 4. This etching may be performed by RIE (Reactive Ion Etching) or CDE (Chemical Dry Etching).

[0024] 5, the mask 30 formed in the process of FIG. 3 is removed, and a new mask 32 is formed. This mask 32 is selectively formed so that unevenness is appropriately generated on the polysilicon 16.

[0025] Next, as shown in Fig. 6, a second etching (e.g., CDE) of the polysilicon 16 is performed. This etching process is performed so as to form a concave recess of an appropriate depth, rather than etching away the polysilicon 16 down to the interface with the oxide film 12. That is, unlike a typical CDE process, the material to be etched in the opening of the mask is not completely removed, but the process ends when the material is partially removed. Through this process, the uneven portion 100 shown in Fig. 1 is formed.

[0026] Next, as shown in FIG. 7, after removing the mask 32, the interlayer film 14 is formed on the upper surfaces of the oxide film 12 and the polysilicon 16.

[0027] 8, a mask 34 is formed based on the region where the gate pad is to be formed. This mask 34 is formed to secure a contact region in the interlayer film 14 that electrically connects the polysilicon 16 and the gate pad.

[0028] Next, as shown in FIG. 9, the interlayer film 14 is selectively removed by RIE processing to form a contact region.

[0029] Next, as shown in FIG. 10, after removing the mask 34, a barrier metal 18 is formed on the upper surfaces of the interlayer film 14 and the polysilicon 16.

[0030] 11, a conductor that forms the gate pad 20 is deposited on the upper surface of the barrier metal 18. Then, excess portions of the conductor and barrier metal are removed so that they remain in appropriate regions, thereby manufacturing the semiconductor device 1 shown in FIG.

[0031] As an example, the process may be performed so that polysilicon 16 is 1000 nm in FIG. 2, the opening of mask 32 is 450 nm wide in FIG. 5, and the recess of polysilicon 16 is 300 nm deep and 500 nm wide in FIG. 6, but is not limited to these dimensions.

[0032] Second embodiment FIG. 12 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the second embodiment.

[0033] The semiconductor device 1 includes a plug 22 in the uneven portion 100. Furthermore, a metal film 24 may be provided between the barrier metal 18 and the gate pad 20 on the side wall of the contact region of the gate pad 20.

[0034] The plug 22 is, for example, a plug made of W, and is formed so as to fill the uneven portion 100. That is, W is formed so as to flatten the uneven region caused by the uneven portion 100 formed in the barrier metal 18.

[0035] The gate pad 20 is formed on the upper surface planarized by the plug 22. Since the lower surface is flat, after the gate pad 20 is formed, the upper surface of the contact region of the gate pad 20 is also formed flat.

[0036] The width of the uneven portion 100 may be, for example, 500 nm and the depth may be 300 nm, as in the first embodiment, or the depth may be changed within a range of 300 to 600 nm, for example.

[0037] To form the plug 22, the uneven portion 100 of the polysilicon 16 may be formed such that its width does not change compared to the first embodiment.

[0038] In order to form the plug 22 in this embodiment, the process of FIG. 6 is performed by RIE, for example. After this RIE process, a barrier metal 18 is formed, and then, for example, W is used to form the plug 22 and the metal film 24. After this, patterning is performed so that the plug 22 and the metal film 24 are appropriately formed, and the entire surface is etched back again by RIE. After forming a film of a metal such as W, the entire surface in the contact region is etched back to form the plug 22, and the etchback process similarly forms a metal film 24 on the side wall of the contact region. If necessary, the metal film 24 may be removed, but there is no particular problem even if it exists.

[0039] According to this embodiment, like the first embodiment, it is possible to suppress peeling of the bond by the anchor effect. Furthermore, by filling the recess of the polysilicon with a plug, the upper surface of the gate pad 20 formed on the upper surface is flattened. By flattening the upper surface of the gate pad 20, it is possible to improve the adhesion of the wire during bonding.

[0040] Although the width of the plug 22 is set to 500 nm as an example, the width is not limited to this and may be any width that allows the plug to be appropriately formed.

[0041] Third embodiment FIG. 13 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the third embodiment.

[0042] The uneven portion 100 may be configured to include a plug 22 along its sidewall. That is, unlike the second embodiment, the recess of the barrier metal 18 along the uneven portion 100 is not filled, but the plug 22 may be provided along the sidewall of the recess. Therefore, compared to the second embodiment, the width of the uneven portion 100 may be made larger. The width of the uneven portion 100 may be, for example, 5 μm, but is not limited to this, and may be a width such that the recess in the barrier metal 18 is not filled with metal (for example, W).

[0043] The process of this semiconductor device 1 is substantially the same as that of the second embodiment, except for widening the width of the uneven portion 100. However, in the process of forming the plug 22, the metal is formed so as not to fill the recesses of the barrier metal 18.

[0044] In this way, by forming projections and recesses on the surface of the polysilicon in contact with the barrier metal, it is possible to suppress peeling of the bonding due to the anchor effect.

[0045] (Fourth embodiment) FIG. 14 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the fourth embodiment.

[0046] The uneven portion 100 formed in the polysilicon 16 may be in a form in which at least its bottom surface is in contact with the oxide film 12. In the semiconductor device 1 of this embodiment, the metal film 24 may also be formed on the sidewall of the recess of the barrier metal 18 and on the sidewall region of the contact region of the gate pad 20 in the barrier metal 18. The width of the uneven portion 100 may be, for example, 5 μm, but is not limited to this.

[0047] The process of this semiconductor device 1 is implemented by appropriately widening the mask pattern width in the process of Fig. 5, and etching the polysilicon 16 by the height thereof by CDE in the process of Fig. 6. The subsequent process is the same as that of the first embodiment.

[0048] In this manner, by forming projections and recesses on the surface of the polysilicon 16 in contact with the barrier metal 18, peeling of the bonding can be suppressed by the anchor effect.

[0049] Fifth embodiment FIG. 15 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the fifth embodiment.

[0050] In this semiconductor device 1, in the second layer 2, an uneven portion 100 is formed by the interlayer film 14 on the upper surface of the polysilicon 16. The uneven portion 100 formed by the interlayer film 14 is formed so that the polysilicon 16 and the barrier metal 18 are in contact with each other on the lower surface. For example, the width of this recess is 500 nm.

[0051] In the barrier metal 18, a plug 22 is formed in a recess caused by the uneven portion 100 so as to fill the recess.

[0052] The process of this semiconductor device 1 will be described. The processes in Figs. 2 to 4 are the same as those in the first embodiment. After that, the process of forming the interlayer film 14 in Fig. 7 is carried out without carrying out the processes in Figs. 5 and 6. As an example, the interlayer film 14 may be formed to a height of 1000 nm.

[0053] 16 and 17 are cross-sectional views which diagrammatically show the subsequent process.

[0054] After the interlayer film 14 is formed, a mask 34 is formed based on a pattern for forming projections and recesses using the interlayer film 14 as shown in FIG.

[0055] 17, the interlayer film 14 is etched by RIE. In the above example, by etching the interlayer film 14 by 1000 nm, it becomes possible to form an uneven portion using the interlayer film 14 so that the barrier metal 18 can contact the polysilicon 16 on the lower surface of the recess.

[0056] The subsequent process is the same as in the second embodiment.

[0057] In this way, by forming irregularities on the surface of the second layer 2 in contact with the barrier metal 18, it is possible to suppress bonding peeling by the anchor effect. Furthermore, in this embodiment, by filling the recesses in the interlayer film 14 with the plugs 22, the upper surface of the gate pad 20 formed thereon is flattened. By flattening the upper surface of the gate pad 20, it is possible to improve the adhesion of the wire during bonding. The recess width of the interlayer film is, for example, 500 nm, but is not limited to this and can be any value as long as it forms the plugs 22.

[0058] Sixth embodiment FIG. 18 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the sixth embodiment.

[0059] In the semiconductor device 1, the uneven portion 100 is formed in the second layer 2 by using the interlayer film 14 as in the fifth embodiment. Then, on the upper surface of the barrier metal 18, a metal film 24 is formed on the side wall of the recess formed by the uneven portion 100.

[0060] The process of the semiconductor device 1 is a combination of the fifth embodiment and the third embodiment. That is, in the etching of the interlayer film 14 in the fifth embodiment, the pattern of the mask 34 is changed, and the mask 34 is arranged so that the width of the recess in the second layer 2 is 5 μm, for example. Thereafter, the interlayer film 14 is etched in the same manner as in the fifth embodiment. Following this etching, a process is performed in which a metal film 24 is formed on the side wall of the recess in the barrier metal 18, in the same manner as in the third embodiment.

[0061] In this way, by forming projections and recesses on the surface of the second layer 2 in contact with the barrier metal 18, it is possible to suppress peeling of the bonding due to the anchor effect.

[0062] Seventh embodiment FIG. 19 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the seventh embodiment.

[0063] In this semiconductor device 1, in the second layer 2, an uneven portion 100 is formed by using an interlayer film 14 as in the fifth embodiment. In the uneven portion 100 between at least one interlayer film 14, a plug 22 is formed on the upper surface of the barrier metal 18, and in the uneven portion 100 where the plug 22 is not formed, a metal film 24 is formed on the side wall of the barrier metal 18. The lower surface of the recess of the barrier metal 18 contacts the polysilicon 16.

[0064] In the uneven portion 100 of the interlayer film 14, the recess widths are, by way of example only, 500 nm and 5 μm, but are not limited thereto. In the recess with a width of 500 nm, the recess formed in the barrier metal 18 has a plug 22. In the recess with a width of 5 μm, a metal film 24 is formed on the sidewall of the barrier metal 18.

[0065] The process of this semiconductor device 1 can be realized by the same process as that of the fifth embodiment by changing the pattern of the mask for forming the concave-convex portion 100.

[0066] In this way, by forming unevenness on the surface of the interlayer film 14 in contact with the barrier metal 18, it is possible to suppress peeling of the bonding by the anchor effect. In this embodiment, the widths of the recesses in the interlayer film are 500 nm and 5 μm, but any value can be used as long as the widths allow the plugs 22 to be formed and the metal film 24 is formed without forming the plugs 22.

[0067] Eighth embodiment FIG. 20 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the eighth embodiment.

[0068] In this semiconductor device 1, the second layer 2 is configured to include an interlayer film 14 and polysilicon 16. The uneven portion 100 is formed in two stages. More specifically, the uneven portion 100 is formed by a concave portion formed in the polysilicon 16 and a convex portion formed on the upper surface of the polysilicon 16 by using the interlayer film 14.

[0069] A plug 22 is formed in the uneven portion 100 via a barrier metal 18. A gate pad 20 is formed in contact with the upper surface of the plug 22 and the barrier metal 18.

[0070] The process of this semiconductor device 1 can be implemented by performing isotropic etching such as RIE in FIGS. 5 and 6, and by patterning a mask so as to form projections and recesses due to the interlayer film 14 in FIGS.

[0071] As an example, the numerical values ​​are not limited, and the recess width of the interlayer film 14 is 500 nm or less, and the height is about 1400 nm. The lower surface of the uneven portion 100 may be formed so as to be in contact with the oxide film 12.

[0072] In this way, by forming unevenness on the surface of the polysilicon and interlayer film in contact with the barrier metal, it is possible to suppress bonding peeling due to the anchor effect. Also, by embedding the plug 22 in the recess of the polysilicon 16 and the interlayer film 14, the surface of the gate pad 20 formed thereon is flattened. By flattening the surface of the gate pad 20, it is possible to improve the adhesion of the wire during bonding. Although the case where the recess width of the polysilicon 16 and the interlayer film 14 is 500 nm has been shown, any value can be used as long as it is a value that forms the plug 22.

[0073] Ninth embodiment FIG. 21 is a cross-sectional view illustrating a schematic view of a portion of the semiconductor device according to the ninth embodiment.

[0074] In the semiconductor device 1, the second layer 2 is configured to include an interlayer film 14 and polysilicon 16, as in the eighth embodiment. The uneven portion 100 is formed in two stages. More specifically, the uneven portion 100 is formed by a concave portion formed in the polysilicon 16 and a convex portion formed on the upper surface of the polysilicon 16 by using the interlayer film 14.

[0075] As an example, the numerical values ​​are not limited, and the recessed portion of polysilicon 16 has a width of 500 nm or less, and this recessed portion of polysilicon 16 is filled with plug 22. The height of the recessed portion of polysilicon 16 is about 300 to 600 nm, and has a shape deeper than the unevenness (about 150 nm) of the surface after polysilicon 16 is formed.

[0076] The recess in the interlayer film 14 has a width of 5 μm, and a metal film 24 is formed on the side wall of the recess in the interlayer film 14 .

[0077] The process of the semiconductor device 1 is the same as that of the eighth embodiment. In the process described in the eighth embodiment, the semiconductor device 1 according to this embodiment can be manufactured by appropriately controlling the patterning width of the mask in FIG.

[0078] As an example, the numerical values ​​of which are not limited, polysilicon 16 is deposited to a thickness of 1000 nm on the upper surface of oxide film 12. Then, by using an appropriate etching process, a cutout pattern having a width of 500 nm is formed in polysilicon 16, and the polysilicon is etched to have a width of 500 nm. As a result, a recess having a height of 300 nm and a width of 500 nm is formed on the surface of polysilicon 16.

[0079] Next, after depositing the interlayer film 14 to a thickness of 1000 nm, a 5 μm-wide hole pattern is formed on the recess of the polysilicon 16, and the interlayer film 14 is etched. As a result, a 5 μm-wide recess is formed on the surface of the interlayer film 14.

[0080] Thereafter, the semiconductor device 1 according to this embodiment can be manufactured by forming the barrier metal 18, the plug 22, the metal film 24, and the gate pad 20. Note that, similarly to the eighth embodiment, the lower surface of the uneven portion 100 may be formed so as to be in contact with the oxide film 12.

[0081] In this way, by forming irregularities on the surfaces of polysilicon 16 and interlayer film 14 in contact with barrier metal 18, it is possible to suppress bonding peeling by the anchor effect. Although the case where the width of the recess in polysilicon is 500 nm has been shown, any value can be used as long as plug 22 is formed. Also, although the case where the width of the recess in interlayer film 14 is 5 μm has been shown, any value can be used as long as plug 22 is not formed.

[0082] Tenth embodiment In the above-described embodiments, the cross section of the uneven portion 100 has been described, but in this embodiment, various forms in plan view will be described. In each figure, the shape of the uneven portion 100 formed in the second layer 2 is shown in plan view. Fig. 22 to Fig. 27 are diagrams showing some non-limiting examples of the shape of the uneven portion 100 formed in the second layer 2 in plan view.

[0083] As shown in FIG. 22, the concave-convex portion 100 may be formed in a stripe pattern on the second layer 2.

[0084] As shown in FIG. 23, the projections and recesses 100 may be formed in the second layer 2 in the shape of a rectangle, each of which has a width.

[0085] 24, the concave-convex portion 100 may be formed in a spiral shape having width in the second layer 2. Although this spiral shape is configured as a rectangle, it may be another polygonal shape, or may be a circular spiral shape without corners (for example, a helical shape having width).

[0086] As shown in FIG. 25, the uneven portion 100 may be formed in the second layer 2 in a checkered pattern.

[0087] As shown in FIG. 26, the uneven portion 100 may be formed in a honeycomb shape in the second layer 2.

[0088] As shown in FIG. 27, the concave-convex portion 100 may be formed in the second layer 2 in an octagonal shape having a width.

[0089] In either example, the concave and convex patterns of the polysilicon 16 and the interlayer film 14 can be arranged in a manner that takes into consideration the bonding direction and efficiently utilizes the anchor effect.

[0090] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims.

[0091] For example, although the above-mentioned embodiments have all been described as IGBTs, they may be MOSFETs. Also, the present disclosure is not limited to this. As some non-limiting examples, the embodiments of the present disclosure can be applied to the formation of the electrodes in semiconductor devices having an insulating film and an electrode to which a voltage is applied via the insulating film, and also to both planar and trench types. [Explanation of symbols]

[0092] 1: Semiconductor device, 2: 2nd layer, 10: Silicon substrate, 12: oxide film, 14: Interlayer film, 100: uneven part, 16: Polysilicon, 18: Barrier metal, 20: Gate pad, 22: Plug, 24: Metal film, 30, 32, 34: Mask

Claims

1. A silicon substrate; A first layer formed of an oxide film provided on an upper surface of the silicon substrate; A second layer provided on an upper surface of the first layer, a polysilicon layer selectively formed on the upper surface of the first layer and having a recess on the upper surface; a second layer including: a layer having at least selectively uneven portions on an upper surface of the polysilicon, the uneven portions including at least unevenness caused by the recesses on the upper surface of the polysilicon, and having unevenness deeper than unevenness that would occur if the layer were formed to have a flat surface; a barrier metal formed on an upper surface of the second layer in accordance with the shape of the projections and recesses; a gate pad facing the second layer via the barrier metal; Equipped with the polysilicon is in close contact with the barrier metal at the recess and at a planar upper surface around the recess; Semiconductor device.

2. IGBT (Insulated Gate Bipolar Transistor) or MOSFET (Metal-Oxide-Semiconductor Field-Effect Transistor), The semiconductor device according to claim 1.

3. The second layer is an interlayer film formed at least in a region of the top surface of the first layer where the polysilicon is not formed; 3. The semiconductor device according to claim 1, further comprising:

4. The second layer is an interlayer film formed at least in a region of the top surface of the first layer where the polysilicon is not formed; Equipped with the interlayer film is selectively formed on the upper surface of the polysilicon in a region other than the recess such that a planar upper surface of the polysilicon remains around the recess; the uneven portion includes unevenness formed by the interlayer film selectively disposed on the upper surface of the polysilicon; 3. The semiconductor device according to claim 1 or 2.

5. a metal plug formed on at least a side wall of the concave-convex portion of the barrier metal on the upper surface of the barrier metal; Further equipped with the gate pad is formed on an upper surface of the barrier metal via the plug in at least a portion of the gate pad; The semiconductor device according to any one of claims 1 to 4.

6. the plug is formed flat by filling the unevenness of the barrier metal formed according to the uneven portion, the gate pad is formed on an upper surface of the barrier metal via the plug; The semiconductor device according to claim 5.

7. The uneven portion is formed in a stripe shape, a square shape, a spiral shape, a checkered shape, a honeycomb shape, or an octagonal shape in a plan view. The semiconductor device according to any one of claims 1 to 6.

8. A first layer, which is an oxide film, is formed on the top surface of a silicon substrate. forming polysilicon on an upper surface of the first layer; forming a mask based on a pattern of projections and recesses on an upper surface of the polysilicon; forming the uneven portion in the polysilicon by etching based on the mask; removing the mask; forming a barrier metal film on an upper surface of the polysilicon; forming a metal film for forming a gate pad on an upper surface of the barrier metal formed on at least an upper surface of the polysilicon forming the uneven portion and the planar polysilicon around the uneven portion; A method for manufacturing a semiconductor device.

9. between the deposition of the barrier metal and the deposition of the metal forming the gate pad, a metal different from the metal forming the barrier metal and the metal forming the gate pad is deposited on at least a side wall of a region in which the barrier metal is formed along the uneven portion; The method of claim 8.

Citation Information

Patent Citations

  • Semiconductor device

    JP1995263484A

  • Semiconductor device

    JP1996203952A

  • Semiconductor device with improved contact pads and method of making same

    JP2009510758A

  • Semiconductor device and method of manufacturing the same

    JP2016111084A

  • JPP7435804B