Canister

The canister design addresses warpage issues by using angled, shorter rod-shaped units and recesses to enhance cooling and moldability, enabling efficient production and cost reduction.

JP7586804B2Active Publication Date: 2024-11-19FUTABA IND CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2021185793
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-11-15
Publication Date
2024-11-19
Estimated Expiration
2041-11-15

AI Technical Summary

Technical Problem

The manufacturing of canisters with rod-shaped parts is hindered by warpage due to temperature deviations caused by uneven cooling during injection molding, particularly at the thicker roots of elongated rods, making it difficult to produce the adjustment member.

Method used

The canister design incorporates a resin member with rod-shaped units arranged in directions intersecting the gas flow at angles of 45° to 90°, featuring shorter rod-like portions and recesses to form gaps with granular adsorbents, allowing for separate mold formation and improved cooling, thereby preventing warpage.

Benefits of technology

This design facilitates easy manufacturing by reducing warpage, improving dimensional accuracy, reducing resin usage, and lowering costs while maintaining low ventilation resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586804000001
    Figure 0007586804000001
  • Figure 0007586804000002
    Figure 0007586804000002
  • Figure 0007586804000003
    Figure 0007586804000003
Patent Text Reader

Abstract

To makes it easy to manufacture a canister.SOLUTION: Provided is a canister including at least one chamber and a resin member. The resin member is arranged in an object chamber, which is any of the at least one chamber. An adsorbent arranged in the object chamber is formed as a plurality of granular bodies. The resin member is an integrally formed member of resin, and includes a coupling member and at least one rod-shaped unit. The at least one rod-shaped unit includes a plurality of rod-shaped portions extending from the coupling member in a direction substantially parallel to an extension direction intersecting a gas flow direction in the object chamber at an angle of 45° or more and 90° or less.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a canister for adsorbing fuel vapors generated from a fuel tank. [Background technology]

[0002] The canister of Patent Document 1 is provided with a target chamber in which an adjustment member having a plurality of rod-shaped parts and a connecting part that connects the bases of the plurality of rod-shaped parts is disposed. The rod-shaped parts extend approximately parallel to the gas flow direction and are disposed at intervals throughout the target chamber. Gaps are generated between each rod-shaped part and activated carbon pellets, which are granular adsorbents, disposed in the target chamber, and as a result, the airflow resistance of the target chamber is suppressed.

[0003] Here, it is considered that the adjustment member is manufactured from resin by injection molding. In order to perform the injection molding, it is necessary to form a draft taper on the outer peripheral surface of each rod-shaped portion by inclining the outer peripheral surface of each rod-shaped portion so that it becomes thinner as it moves away from the joint, so that the adjustment member can be removed from the mold. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2018-96254 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, when the multiple rod-shaped portions are long, the base of each rod-shaped portion needs to be made thicker when forming the draft taper, which makes it easier for heat to accumulate around the base of the multiple rod-shaped portions during injection molding.

[0006] That is, generally, a cooling pipe for flowing a refrigerant for cooling the molded member is provided inside the injection molding die, but since the intervals between the rod-shaped parts of the adjustment member are narrow, it is difficult to arrange the cooling pipe so that it passes between the rod-shaped parts, although it is possible to provide the cooling pipe around the adjustment member in the die for the adjustment member.

[0007] For this reason, the periphery of the base of each rod-shaped portion, which has become thicker due to the draft taper, is more difficult to cool than other portions. As a result, temperature deviation occurs around the base of the rod-shaped portions, which causes the rod-shaped portions to tilt (hereinafter, also referred to as warping). For this reason, when the rod-shaped portions are long, it becomes difficult to manufacture the adjustment member.

[0008] One aspect of the present disclosure aims to facilitate the manufacture of the canister. [Means for solving the problem]

[0009] One aspect of the present disclosure is a canister configured to be mounted on a vehicle having an engine, the canister comprising at least one chamber, an inflow port, an atmospheric port, an outflow port, and a resin member. An adsorbent for adsorbing fuel vapor is disposed in the at least one chamber. The inflow port is configured to allow fuel vapor to flow from a fuel tank of the vehicle into the at least one chamber. The atmospheric port is configured to allow atmospheric air to flow into the at least one chamber from the outside of the vehicle. The outflow port is configured to allow fuel vapor adsorbed in the adsorbent to flow out toward the engine by atmospheric air flowing in from the atmospheric port. The resin member is disposed in a target chamber which is one of the at least one chamber. The adsorbent disposed in the target chamber is configured as a plurality of granular members. The resin member is an integrally formed member made of resin, and has a connecting portion and at least one rod-shaped unit. The rod-shaped unit has a plurality of rod-shaped portions extending from the connecting portion in a direction substantially parallel to an extension direction intersecting with a gas flow direction in the target chamber at an angle of 45° to 90°.

[0010] According to the above-mentioned configuration, it is possible to arrange the rod-shaped parts throughout the entire area of ​​the target chamber while encouraging the rod-shaped parts to be short, thereby preventing the base of the rod-shaped parts from becoming thicker due to the formation of a draft taper. This makes it possible to prevent the rod-shaped parts from warping during injection molding of the resin member, and as a result, makes it easier to manufacture the canister.

[0011] In one aspect of the present disclosure, the target chamber may have an elongated shape extending in the direction of gas flow in the target chamber. According to the above-mentioned configuration, the rod-shaped portions can be further shortened, and thus the base of the rod-shaped portions can be prevented from becoming thicker due to the formation of the draft taper, and thus the occurrence of warping in the rod-shaped portions during injection molding of the resin member can be further prevented.

[0012] In one embodiment of the present disclosure, at least some of the plurality of rod-shaped portions may have at least one recess formed in the outer circumferential surface thereof. According to the above-mentioned configuration, a gap is formed between the recess formed in the rod-shaped portion and the adsorbent which is a plurality of granular members, so that the airflow resistance of the canister can be reduced.

[0013] In one embodiment of the present disclosure, the resin member may have a first and a second rod-shaped unit as at least one rod-shaped unit. The connecting portion may have a first portion and a second portion. The second portion is located on the opposite side of the first portion. The rod portions of the first rod-shaped unit may extend from the first portion substantially parallel to an extension direction determined corresponding to the first rod-shaped unit. The rod portions of the second rod-shaped unit may extend from the second portion substantially parallel to an extension direction determined corresponding to the second rod-shaped unit.

[0014] According to the above configuration, during injection molding, the first and second rod-shaped units can be formed by separate dies located on both sides of the connecting portion. Also, the rod-shaped portions in each of the first and second rod-shaped units extend in different directions from the connecting portion located between these rod-shaped units. Therefore, while arranging the rod-shaped portions throughout the entire target chamber, the rod-shaped portions of each rod-shaped unit can be further shortened. This further suppresses the occurrence of warping in the rod-shaped portions during injection molding of the resin member.

[0015] In one embodiment of the present disclosure, the extension direction of the multiple rod-shaped portions may be a direction intersecting the flow direction of gas in the target chamber at an angle of approximately 90°. According to the above-mentioned configuration, the rod-shaped portions can be further shortened, and thus the base of the rod-shaped portions can be prevented from becoming thicker due to the formation of the draft taper, and thus the occurrence of warping in the rod-shaped portions during injection molding of the resin member can be further prevented. [Brief description of the drawings]

[0016] [Figure 1] 3 is a cross-sectional view of the canister as viewed from the side. FIG. [Diagram 2] FIG. [Diagram 3] FIG. [Figure 4] FIG. 4 is a bottom view of the resin member as viewed from the first end side. [Diagram 5] 4 is a cross-sectional view of a first rod-shaped portion 51 in which a recess is formed. FIG. [Figure 6] 4 is a cross-sectional view of a first rod-shaped portion 51 in which a recess is formed. FIG. [Figure 7] FIG. 2 is an explanatory diagram of injection molding of a resin member. [Figure 8] FIG. 13 is a front view of a resin member according to a modified example. [Figure 9] FIG. 13 is a front view of a resin member according to a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. Note that the embodiments of the present disclosure are not limited to the following embodiments, and various forms may be adopted as long as they fall within the technical scope of the present disclosure.

[0018] [1. Canister configuration] The canister 1 of the first embodiment is mounted on a vehicle (see FIG. 1). Hereinafter, the vehicle on which the canister 1 is mounted will be referred to as the host vehicle. The canister 1 has a synthetic resin container 10 provided with first to third chambers 20 to 40, in which adsorbents 60 to 62 for adsorbing fuel vapor are disposed, respectively. The number of chambers in the canister 1 may be, for example, two or less, or four or more.

[0019] The adsorbent 61 in the second chamber 30 is composed of pellets, which are granular activated carbon. The adsorbent 61 in the second chamber 30 may be composed of a granular adsorbent other than pellets. The adsorbents 60 and 62 in the first and third chambers 20 and 40 may be composed of, for example, powdered activated carbon or pellets. The adsorbent 62 in the third chamber 40 may be composed of honeycomb carbon, for example. The honeycomb carbon has a cylindrical side wall and is arranged in the third chamber 40 in a state of stretching in the gas flow direction. A plurality of flow paths are provided inside the side wall, penetrating the honeycomb carbon in the stretching direction. The adsorbents 60 to 62 in the first to third chambers 20 to 40 may be composed of a material other than activated carbon.

[0020] An inlet port 11, an outlet port 12, and an atmospheric port 13 are provided at the ends of the container 10. The inlet port 11 and the outlet port 12 connect the inside of the first chamber 20 to the outside of the container 10, and the atmospheric port 13 connects the inside of the third chamber 40 to the outside of the container 10.

[0021] Hereinafter, the side of the container 10 of the canister 1 on which the inlet port 11, the outlet port 12, and the atmospheric port 13 are provided will be referred to as the port side. The container 10 also has an opening on the opposite side to the port side. The opening is closed by a lid member 14. Hereinafter, the side opposite to the port side (in other words, the side on which the lid member 14 is provided) will be referred to as the lid side.

[0022] The inflow port 11 is connected to a fuel tank of the engine of the vehicle. Fuel vapor generated in the fuel tank flows into the inside of the canister 1 through the inflow port 11 and is adsorbed by the adsorbents 60 to 62 in each chamber. As a result, fuel is accumulated inside the canister 1.

[0023] The outlet port 12 is connected to an intake pipe of the engine of the vehicle, and the atmospheric port 13 is connected to the outside of the vehicle. The negative intake pressure of the engine causes atmospheric air (in other words, purge air) to flow into the canister 1 via the atmospheric port 13. The inflow of purge air causes the fuel adsorbed in the adsorbents 60-62 to be desorbed, and the desorbed fuel flows out from the outlet port 12 toward the intake pipe together with the purge air. This causes a purge to remove the fuel adsorbed in the adsorbents 60-62, and the adsorbents 60-62 are regenerated.

[0024] In other words, the fuel vapor flowing in from the inlet port 11, the fuel vapor flowing out from the outlet port 12 during purging, and the purge air flowing in from the atmospheric port 13 during purging flow through each of the chambers 20 to 40 in the direction in which the port side end and the lid side end face each other.

[0025] The first chamber 20 has, as an example, a substantially rectangular parallelepiped shape, and has an elongated shape extending from the lid side to the port side, and the port side end is connected to the inlet port 11 and the outlet port 12. Filters 21 and 22 are disposed at the port side end and the lid side end of the first chamber 20, respectively, and an adsorbent 60 is disposed between the filters 21 and 22.

[0026] The first chamber 20 has an end on the lid side connected to a communication passage 15. The communication passage 15 is provided along the lid member 14 and connects the first chamber 20 and the second chamber 30. A permeable porous plate 23 is disposed between the filter 22 on the lid side of the first chamber 20 and the communication passage 15, and a coil spring 16 is disposed between the porous plate 23 and the lid member 14. The coil spring 16 presses the porous plate 23 toward the port side. Therefore, inside the canister 1, the fluid can travel between the first chamber 20 and the second chamber 30 via the communication passage 15.

[0027] The second chamber 30 and the third chamber 40 are adjacent to the first chamber 20 and have an elongated shape extending from the lid side to the port side. As an example, the L / D of the second chamber 30 and / or the third chamber 40 may be greater than 1. L means the length in the gas flow direction in the chamber, and D means the equivalent diameter of the cross section perpendicular to the gas flow direction in the chamber. The second and third chambers 30, 40 are arranged from the lid side to the port side with their ends adjacent to each other, and the second chamber 30 and the third chamber 40 are separated by a plate-shaped partition member 18 having permeability. Therefore, the fluid can pass through the partition member 18 and travel between the internal space of the second chamber 30 and the internal space of the third chamber 40.

[0028] A filter 31 is disposed at the end of the second chamber 30 on the lid side, and an adsorbent 61 is disposed between the filter 31 and the partition member 18. A filter 41 is disposed at the end of the third chamber 40 on the port side, and an adsorbent 62 is disposed between the filter 41 and the partition member 18.

[0029] A permeable porous plate 32 is disposed between the filter 31 on the lid side of the second chamber 30 and the communication passage 15, and a coil spring 17 is disposed between the porous plate 32 and the lid member 14. The coil spring 17 presses the porous plate 32 toward the port side. The third chamber 40 has an end on the port side connected to the atmospheric port 13.

[0030] [2. Plastic parts] In this embodiment, as an example, the second chamber 30 is configured as the target chamber, and the resin member 5 is disposed in the second chamber 30 (see FIG. 1). The first or third chamber 20, 40 may be configured as the target chamber in which the resin member 5 is disposed, or two or more of the first to third chambers 20 to 40 may be configured as the target chamber. Granular adsorbent, for example, pellets, is disposed in the target chamber.

[0031] The resin member 5 is disposed in the second chamber 30 such that the first end 5A is located on the port side and the second end 5B is located on the lid side (see FIGS. 2 to 4). However, conversely, the resin member 5 may be disposed in the second chamber 30 such that the second end 5B is located on the port side and the first end 5A is located on the lid side.

[0032] The resin member 5 is integrally formed from resin, and includes first and second rod-shaped units 50, 52 and a connecting portion . [3. First and second rod-shaped units] The first rod-shaped unit 50 has a plurality of first rod-shaped portions 51 (see Figs. 2 to 4). The plurality of first rod-shaped portions 51 are elongated portions having substantially the same length and extending generally parallel to each other with a high gap therebetween, and extend from a first portion 54A of the connecting portion 54 in a first extension direction 51A. A draft taper is formed in each of the first rod-shaped portions 51, and the first rod-shaped portions 51 become thinner toward the tip. As an example, each of the first rod-shaped portions 51 has a cross section perpendicular to the extension direction (hereinafter simply referred to as a cross section) that is substantially circular. However, the shape of the cross section can be determined as appropriate.

[0033] The second rod-shaped unit 52 also has a plurality of second rod-shaped portions 53 configured similarly to the plurality of first rod-shaped portions 51. The plurality of second rod-shaped portions 53 have approximately the same length as the plurality of first rod-shaped portions 51, and extend in a second extension direction 53A from a second portion 54B on the opposite side of the first portion 54A in the connecting portion 54.

[0034] As an example, the first and second extension directions 51A, 53A intersect with the gas flow direction 5C in the second chamber 30 at approximately 90°, and the first extension direction 51A is opposite to the second extension direction 53A. Also, the base of each first rod-shaped portion 51 is adjacent to the base of any one of the second rod-shaped portions 53, and each first rod-shaped portion 51 and the second rod-shaped portion 53 whose base is adjacent to that of the first rod-shaped portion 51 extend in a substantially straight line with the connecting portion 54 therebetween.

[0035] In other words, the first and second rod-shaped units 50, 52 have approximately the same shape, and the resin member 5 has a shape that is approximately symmetrical with respect to a plane that passes through the connecting portion 54 as the center. Moreover, the multiple first and second rod-shaped portions 51, 53 are, for example, arranged so as to form first to third rows 5D to 5F and are disposed throughout the second chamber 30. Note that the number of rows of the multiple first and second rod-shaped portions 51, 53 and the number of first and second rod-shaped portions 51, 53 arranged in each row can be determined appropriately depending on the size of the chamber in which the resin member 5 is disposed.

[0036] The adsorbent 60 disposed in the second chamber 30 is configured as granular pellets. Therefore, by disposing a plurality of first and second rod-shaped portions 51, 53 (hereinafter also simply referred to as rod-shaped portions) in the second chamber 30, a gap is formed between each rod-shaped portion and the adsorbent 60. This reduces the airflow resistance of the second chamber 30.

[0037] [4.Connection part] The connecting portion 54 is provided from the first end 5A to the second end 5B of the resin member 5, and extends in the gas flow direction 5C in the second chamber 30 (see FIGS. 2 to 4). The connecting portion 54 is located approximately in the center of the resin member 5 in the first and second extension directions 51A, 53A, and connects the bases of the first and second rod-shaped portions 51, 53. It should be noted that in the resin member 5 of this embodiment, the rod-shaped portions 51, 53 are connected by the connecting portion 54, as an example, and are not connected by other components. The connecting portion 54 has a main body portion 55, first and second branch portions 56, 57, and two flat portions 58 (see FIGS. 3 and 4).

[0038] The main body portion 55 is a rod-shaped portion extending substantially linearly along the gas flow direction 5C. The main body portion 55 connects the bases of the first and second rod-shaped portions 51, 53 in the second row 5E. The first branches 56 are provided so as to protrude from the base of each rod-shaped portion in the second row 5E toward the first row 5D. Each of the first branches 56 is located closer to the second end 5B than the rod-shaped portion in the second row 5E and connects the base of the rod-shaped portion in the first row 5D to the nearest base of the rod-shaped portion.

[0039] The second branches 57 are provided so as to protrude from the base of each rod-shaped portion in the second row 5E toward the third row 5F. Each second branch 57 is located closer to the second end 5B than the rod-shaped portion in the second row 5E and connects the base of the rod-shaped portion in the third row 5F to the base of the rod-shaped portion closest to the second branch 57.

[0040] The flat portions 58 are provided in the first row 5D and the third row 5F. The flat portions 58 in the first row 5D connect the bases of the three rod-shaped portions aligned from the first end 5A in the first row 5D to each other. The flat portions 58 in the third row 5F connect the bases of the three rod-shaped portions aligned from the first end 5A in the third row 5F to each other.

[0041] Each flat portion 58 has a flat shape that is approximately parallel to the gas flow direction 5C and extends approximately perpendicular to the first and second extension directions 51A, 53A, and protrudes toward and contacts the inner wall of the second chamber 30. As a result, a gap is formed between the multiple rod-shaped portions in the first row 5D and the third row 5F and the inner wall of the second chamber 30.

[0042] [5. Concave section] At least some of the rod-shaped parts in the first and / or second rod-shaped units 50, 52 may have recesses 59 formed on the outer circumferential surface (see Figs. 5 and 6). Specifically, for example, the recesses 59 may be formed as groove-like parts extending from the base or vicinity of the rod-shaped part to the tip or vicinity of the tip in a direction substantially parallel to the extension direction of the rod-shaped part. As an example, four recesses 59 may be provided at substantially equal intervals, and the cross section of the rod-shaped part may be formed in an X shape (see Fig. 5). Also, for example, five recesses 59 may be provided at substantially equal intervals, and the cross section of the rod-shaped part may be formed in a star shape (see Fig. 6).

[0043] Of course, the recess 59 is not limited to this, and may be formed as a groove-like portion extending in a direction different from the elongation direction. Also, the recess 59 is not limited to a groove shape, and may be formed as, for example, a plurality of dot-like regions on the outer circumferential surface of the rod-shaped portion.

[0044] The rod-shaped portions in the first and / or rod-shaped second units 50, 52 may include a plurality of types of rod-shaped portions having different cross-sectional shapes, or may include at least one specific rod-shaped portion. The specific rod-shaped portion is aligned in the extension direction of the specific rod-shaped portion and has a plurality of sections having different cross-sectional shapes.

[0045] [6. Manufacturing method of resin parts] The resin member 5 is manufactured by injection molding using first and second molds 7A and 7B (see FIG. 7). The first mold 7A is configured to form the first rod-shaped unit 50 (in other words, the multiple first rod-shaped portions 51) and the first portion 54A of the connecting portion 54. The second mold 7B is configured to form the second rod-shaped unit 52 (in other words, the multiple second rod-shaped portions 53) and the second portion 54B of the connecting portion 54.

[0046] The first mold 7A includes a recess 70, a plurality of holes 71, a contact surface 72, and a cooling pipe 73. The recess 70 is a portion for forming the first portion 54A of the connecting portion 54, and is provided on the contact surface 72.

[0047] The multiple holes 71 are cylindrical portions for forming the multiple first rod-shaped portions 51, and are provided at the bottom of the recess 70. In order to form a draft taper in each of the first rod-shaped portions 51, the diameter of each hole 71 narrows toward the bottom side of the hole 71.

[0048] The cooling pipes 73 are portions through which a coolant flows to cool the resin filled in the recess 70 and the holes 71 during injection molding. The cooling pipes 73 are disposed so as to pass around the first rod-shaped portions 51. However, the cooling pipes 73 do not pass between the first rod-shaped portions 51.

[0049] The second mold 7B has the same configuration as the first mold 7A, and includes a recess 70, a plurality of holes 71, a contact surface 72, and a cooling pipe 73. When manufacturing the resin member 5, the first and second molds 7A and 7B are arranged so that the abutment surfaces 72 abut against each other. At this time, the recess 70 and the multiple holes 71 of the first mold 7A and the recess 70 and the multiple holes 71 of the second mold 7B are approximately symmetrical with respect to the abutment surfaces 72.

[0050] Next, high-temperature resin is filled into the spaces formed by the recesses 70 and the holes 71 of the first and second molds 7A and 7B. Then, a cooling liquid is caused to flow through the cooling pipes 73 to cool the filled resin and harden the resin.

[0051] When the resin has completely hardened, the first and second molds 7A, 7B are separated, and the resin member 5 is taken out from inside the first and second molds 7A, 7B. The first mold 7A may be formed of a plurality of molds, and the first rod-shaped unit 50 and the first portion 54A of the connecting part 54 may be formed by these molds during injection molding. Similarly, the second mold 7B may also be formed of a plurality of molds.

[0052] [7. Modifications] In this embodiment, the angle at which the first extension direction 51A of the first rod-shaped portion 51 intersects with the gas flow direction 5C (hereinafter, the first intersecting angle) is approximately 90°. Also, the angle at which the second extension direction 53A of the second rod-shaped portion 53 intersects with the gas flow direction 5C (hereinafter, the second intersecting angle) is also approximately 90° (see FIG. 2).

[0053] However, the first and second intersection angles are not limited to approximately 90°, and can be set in the range of 45° or more and 90° or less. The tips of the first and second rod-shaped parts 51, 53 may be located closer to the second end 5B than the base as shown in FIG. 8, or may be located closer to the first end 5A as shown in FIG. 9. In either case, the first and second intersection angles are not limited to approximately 90°, and can be set in the range of 45° or more and 90° or less. The first and second intersection angles may be approximately the same value or different values.

[0054] Even if the first and second intersection angles are values ​​other than approximately 90°, or if the first and second intersection angles are different, the resin member 5 is manufactured by injection molding in the same manner as in this embodiment.

[0055] [8. Effects] (1) According to the above embodiment, the rod-shaped parts can be arranged over the entire area of ​​the second chamber 30 while being encouraged to be short. This prevents the base of the rod-shaped parts from becoming thicker due to the formation of a draft taper, and prevents heat from accumulating around the base of the rod-shaped parts during injection molding. This prevents the rod-shaped parts from warping, making it easier to manufacture the canister 1.

[0056] Furthermore, by suppressing warping of the rod-shaped portions, the dimensional accuracy of the resin member 5 is improved. Even if warping occurs in the rod-shaped portions, the rod-shaped portions can be shortened to suppress dimensional deviations due to warping. Furthermore, by shortening the rod-shaped portions, the injection stroke when manufacturing the resin member 5 by injection molding can be reduced, and injection molding can be performed in a shorter cycle. Furthermore, by suppressing the base of the rod-shaped portions from becoming thicker, the amount of resin required to manufacture the resin member 5 can be reduced, making the canister 1 lighter and reducing costs.

[0057] (2) Furthermore, because the resin member 5 is disposed in the second chamber 30 having an elongated shape, the rod-shaped portions can be further shortened. This can prevent the bases of the rod-shaped portions from becoming thicker due to the formation of a draft taper, and as a result, it can be further prevented that the rod-shaped portions will warp during injection molding of the resin member 5.

[0058] (3) Furthermore, by forming recesses 59 in the rod-shaped portions, gaps are formed between the recesses 59 and the pellets serving as the adsorbent. This makes it possible to reduce the airflow resistance of the canister 1. (4) Furthermore, during injection molding, the first and second rod-shaped units 50, 52 can be formed by the first and second molds 7A, 7B located on both sides of the connecting portion 54, respectively. Furthermore, the first rod-shaped portions 51 in the first rod-shaped unit 50 and the second rod-shaped portions 53 in the second rod-shaped unit 52 extend in opposite directions. This makes it possible to arrange the rod-shaped portions throughout the entire area of ​​the second chamber 30 while encouraging each rod-shaped portion to become even shorter. This further prevents the rod-shaped portions from warping during injection molding of the resin member 5.

[0059] 9. Other Embodiments (1) The resin member 5 in the above embodiment includes the first and second rod-shaped units 50, 52, but may include only the first rod-shaped unit 50. That is, a plurality of first rod-shaped portions 51 may be provided only in the first portion 54A of the connecting portion 54. The length of the plurality of first rod-shaped portions 51 may be adjusted, and the resin member 5 may be disposed in the chamber such that the connecting portion 54 and the tip of each of the first rod-shaped portions 51 are located on the inner wall of the second chamber 30 or in the vicinity thereof. Moreover, three or more rod-shaped units may be provided in the resin member 5 by providing a plurality of rod-shaped units in the first and / or second portions 54A, 54B of the resin member 5 in the above embodiment.

[0060] (2) Multiple functions possessed by one component in the above embodiments may be realized by multiple components, or one function possessed by one component may be realized by multiple components. Also, multiple functions possessed by multiple components may be realized by one component, or one function realized by multiple components may be realized by one component. Also, part of the configuration of the above embodiments may be omitted. Also, at least part of the configuration of the above embodiments may be added to or substituted for the configuration of another of the above embodiments. [Explanation of symbols]

[0061] 1...canister, 20-40...first to third chambers, 5...resin member, 5A...first end, 5B...second end, 5C...gas flow direction, 50...first rod-shaped unit, 51...first rod-shaped portion, 51A...first extension direction, 52...second rod-shaped unit, 53...second rod-shaped portion, 53A...second extension direction, 54...connecting portion, 54A...first portion, 54B...second portion, 59...recess, 60-62...adsorbent, 7A...first mold, 7B...second mold.

Claims

1. A canister configured to be mounted on a vehicle having an engine, at least one chamber having an adsorbent disposed therein for adsorbing fuel vapor; an inlet port configured to admit fuel vapor from a fuel tank of the vehicle into the at least one chamber; an atmospheric port configured to allow atmospheric air to enter the at least one chamber from outside the vehicle; an outlet port configured to allow the fuel vapor adsorbed in the adsorbent to flow out toward the engine by the atmospheric air flowing in from the atmospheric air port; A resin member disposed in a target chamber which is any one of the at least one chambers; The adsorbent disposed in the target chamber is configured as a plurality of granular members, the resin member is an integrally formed member made of resin and has a connecting portion and at least one rod-shaped unit; The rod-shaped unit has a plurality of rod-shaped portions extending from the connecting portion in an extension direction intersecting with a gas flow direction in the target chamber at an angle of 45° to 90°, The rod-shaped portions are tapered toward their tips, extend substantially in parallel, and are arranged to form a plurality of rows aligned in the gas flow direction. Canister.

2. 2. The canister of claim 1, The target chamber has an elongated shape extending in the direction of gas flow in the target chamber. Canister.

3. 3. The canister according to claim 1 or 2, At least one recess is formed on the outer circumferential surface of at least a portion of the plurality of rod-shaped portions. Canister.

4. A canister according to any one of claims 1 to 3, the resin member has a first and a second rod-shaped unit as the at least one rod-shaped unit, The coupling portion has a first portion and a second portion located on an opposite side of the first portion, the plurality of rod-shaped portions of the first rod-shaped unit extend from the first portion in a direction substantially parallel to an extension direction determined corresponding to the first rod-shaped unit, The plurality of rod-shaped portions of the second rod-shaped unit extend from the second portion in a direction substantially parallel to an extension direction determined corresponding to the second rod-shaped unit. Canister.

5. A canister according to any one of claims 1 to 4, The extension direction of the plurality of rod-shaped portions is a direction intersecting the flow direction of the gas in the target chamber at an angle of approximately 90°. Canister.

6. A canister according to any one of claims 1 to 5, The connecting portion extends in the gas flow direction and has a rod-shaped portion connected to a base of the rod-shaped portion. Canister.

Citation Information

Patent Citations

  • Canister for preventing discharge of vaporizing fuel

    JP1988246462A

  • Evaporate fuel disposal device

    JP1993202818A

  • Canister

    JP2008240683A

  • Evaporated fuel treatment device

    JP2009156030A

  • Canister

    JP2018096254A