Arc welding device and arc welding method

The arc welding device stabilizes the buried arc by controlling welding current fluctuations through gradual voltage transitions, ensuring a stable welding process and reducing noise.

JP7590238B2Active Publication Date: 2024-11-26DAIHEN CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021044959
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-18
Publication Date
2024-11-26
Estimated Expiration
2041-03-18

AI Technical Summary

Technical Problem

Existing arc welding methods using buried arcs experience instability due to rapid fluctuations in welding current when the set voltage is varied in a rectangular waveform, leading to unstable molten and arc states.

Method used

The arc welding device controls the welding current by alternately switching the set voltage between upper and lower limit values over a defined period, ensuring gradual changes in current fluctuations.

Benefits of technology

This approach stabilizes the buried space and arc, minimizing sudden current changes and reducing noise, thereby maintaining a stable welding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007590238000001
    Figure 0007590238000001
  • Figure 0007590238000002
    Figure 0007590238000002
  • Figure 0007590238000003
    Figure 0007590238000003
Patent Text Reader

Abstract

To provide an arc-welding device and an arc-welding method capable of suppressing abrupt variation of welding current at a rise and a fall by properly controlling a set voltage.SOLUTION: An arc-welding device which inserts a tip part of a welding wire to an inside space of a concave melting portion formed in base material and performs arc welding includes a power source part which controls a set voltage in order to change a welding current flowing in the welding wire and controls a change of the welding current when conversion between a rise and a fall in the welding current occurs.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a consumable electrode type arc welding apparatus and an arc welding method. [Background technology]

[0002] Arc welding is performed by bringing the tip of a welding wire held by the tip of a welding torch close to a groove provided in a base metal, applying a voltage between the welding wire and the base metal, and generating an arc.

[0003] There is a technology that realizes one-pass welding of thick plates by feeding the welding wire at a higher speed and supplying a large current of 300A or more compared to general arc welding. When the welding wire is fed at a higher speed and a large current is supplied, a concave molten part is formed in the base metal, and the tip of the welding wire enters the inner space of the molten part surrounded by the molten part. In this way, the tip of the welding wire enters deeper than the surface of the base metal, so that the molten part penetrates to the back side of the base metal in the thickness direction, making one-pass welding possible. Hereinafter, the inner space surrounded by the concave molten part is referred to as the buried space, and the arc generated between the tip of the welding wire that has entered the buried space and the base metal or the molten part is referred to as the buried arc.

[0004] For example, Patent Document 1 discloses that in buried arc welding using a buried arc, in order to stably maintain the buried space, the set voltage is periodically changed, thereby periodically changing the welding current flowing through the welding wire. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2017-144480 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, as in Patent Document 1, when the set voltage is changed to stably maintain the buried space, if the set voltage changes in a rectangular waveform, that is, if the set voltage changes abruptly at the rise and fall, the welding current that changes accordingly also changes abruptly at the rise and fall. In this way, when the welding current rises or falls abruptly, there is a problem that the state of the molten part becomes unstable or the arc becomes unstable.

[0007] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide an arc welding apparatus and an arc welding method that can suppress sudden fluctuations in the welding current at the rise and fall by appropriately controlling the set voltage. [Means for solving the problem]

[0008] The arc welding apparatus according to the present invention is an arc welding apparatus that performs arc welding by inserting the tip of the welding wire into the inner space of a concave molten portion formed in a base material, and is equipped with a power supply unit that controls a set voltage to vary the welding current flowing through the welding wire and controls the variation of the welding current when a transition occurs between increasing and decreasing in the welding current.

[0009] In the present invention, the power supply unit controls a set voltage for varying the welding current flowing through the welding wire, thereby suppressing a sudden change in the welding current when the welding current changes from increasing to decreasing, or from decreasing to increasing.

[0010] In the arc welding device of the present invention, the power supply unit alternately switches the set voltage between an upper limit value and a lower limit value, and switches from the lower limit value to the upper limit value or from the upper limit value to the lower limit value over a first time period.

[0011] In the present invention, the power supply unit switches the set voltage from the lower limit value to the upper limit value, or from the upper limit value to the lower limit value, over a first hour, thereby suppressing a sudden change in the welding current when such switching occurs.

[0012] In the arc welding device according to the present invention, the set voltage changes at a constant rate during the first period of time.

[0013] In the present invention, the power supply unit changes the set voltage at a constant rate during the first period of time, thereby making it possible to suppress abrupt changes in the welding current.

[0014] In the arc welding device according to the present invention, the change in the set voltage in the first half of the first time period is smaller than that in the second half of the first time period.

[0015] In the present invention, the power supply unit changes the set voltage so that the change in the first half of the first time period is smaller than the change in the second half of the first time period, thereby suppressing abrupt changes in the welding current.

[0016] In the arc welding apparatus according to the present invention, the power supply unit maintains the set voltage at the upper and lower limit values ​​for a second time period, and the first time period is 5-15% of the second time period.

[0017] In the present invention, the first time is 5-15% of the second time during which the set voltage is maintained at the upper and lower limit values, so that sudden changes in the welding current can be suppressed while minimizing the impact on the arc welding.

[0018] In the arc welding apparatus according to the present invention, the first time period is 8-12% of the second time period.

[0019] In the present invention, the first time is 8-12% of the second time during which the set voltage is maintained at the upper and lower limit values, so that sudden changes in the welding current can be suppressed while minimizing the impact on the arc welding.

[0020] In the arc welding method according to the present invention, a tip of the welding wire is inserted into an inner space of a concave molten portion formed in a base metal to perform arc welding, and a set voltage is controlled to vary the welding current flowing through the welding wire, and the variation of the welding current is controlled when a transition occurs between increasing and decreasing in the welding current.

[0021] In the present invention, by controlling the set voltage for varying the welding current flowing through the welding wire, a sudden change in the welding current is suppressed when the welding current changes from increasing to decreasing, or from decreasing to increasing. Effect of the Invention

[0022] According to the present invention, by appropriately controlling the set voltage, it is possible to suppress the welding current, which varies with the set voltage, from suddenly varying at the rise and fall. [Brief description of the drawings]

[0023] [Figure 1] 1 is a schematic diagram showing one configuration of an arc welding device according to a first embodiment. [Diagram 2] 3 is a flowchart showing a procedure of arc welding in the arc welding device according to the first embodiment. [Diagram 3] FIG. 2 is a side cross-sectional view showing the base material to be welded. [Figure 4] 4 is a graph showing a set voltage generated by a power supply unit and a fluctuation in welding current according to the set voltage. [Diagram 5] 1 is a schematic diagram showing buried arc welding according to the first embodiment. FIG. [Figure 6] 10 is a graph showing a set voltage generated by a power supply unit in the arc welding device according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] Hereinafter, an arc welding apparatus and an arc welding method according to an embodiment of the present invention will be described in detail with reference to the drawings. Note that the present invention is not limited to these examples, but is defined by the claims, and is intended to include all modifications within the meaning and scope of the claims.

[0025] (Embodiment 1) 1 is a schematic diagram showing one configuration of an arc welding apparatus 100 according to embodiment 1. The arc welding apparatus 100 according to embodiment 1 is a so-called consumable electrode type gas shielded arc welding apparatus, and is used for manual or semi-automatic arc welding. The arc welding apparatus 100 can perform both buried arc welding using a buried arc and open arc welding.

[0026] The arc welding device 100 includes a welding power source 1 , a torch 2 , and a wire feeder 3 . Torch 2 has a contact tip and a nozzle (not shown). The contact tip is in the shape of a round bar having a small diameter hole penetrating the axis, and is made of a conductive material such as a copper alloy. It guides welding wire 5 to the part to be welded of base material 4 and supplies welding current I required to generate arc 7 (see FIG. 5). The contact tip comes into contact with welding wire 5 passing through its interior and supplies welding current I to welding wire 5. Torch 2 also has a cylindrical nozzle surrounding the contact tip, which sprays shielding gas to the part to be welded. The shielding gas is for preventing oxidation of base material 4 and welding wire 5 melted by arc 7. The shielding gas is, for example, carbon dioxide gas, a mixture of carbon dioxide gas and argon gas, an inert gas such as argon, or the like.

[0027] The welding wire 5 is, for example, a solid wire having a diameter of 0.9 mm to 1.6 mm, and functions as a consumable electrode. The welding wire 5 is, for example, a packed wire wound in a spiral shape and stored in a pail pack, or a reel wire wound around a wire reel.

[0028] Wire feeder 3 has a feed roller that feeds welding wire 5 to torch 2, and a motor that rotates the feed roller. Wire feeder 3 pulls out welding wire 5 from a pail pack or a wire reel by rotating the feed roller, and supplies the pulled-out welding wire 5 at a predetermined speed to torch 2. In the case of buried arc welding, the feed speed of welding wire 5 is, for example, about 5 to 100 m / min.

[0029] The welding power source 1 is connected to the contact tip of the torch 2 and the base material 4 via a power supply cable, and includes a power source unit 11 that supplies a welding current I, and a feed speed control circuit 12 that controls the feed speed of the welding wire 5.

[0030] The power supply unit 11 is a power supply with constant voltage characteristics, and controls the welding current I to be periodically increased or decreased by controlling the voltage output to the contact tip of the torch 2 and the base material 4. The power supply unit 11 includes a power supply circuit 11a that outputs a PWM-controlled direct current, a voltage control circuit 11b, a current setting circuit 11d, a voltage detection unit 11e, and a current detection unit 11f.

[0031] The current etc. setting circuit 11d outputs a current setting signal Ir indicating a set current value of the welding current I to the voltage control circuit 11b and the feed speed control circuit 12. The feed speed control circuit 12 controls the feed speed of the welding wire 5 based on the current setting signal Ir. During buried arc welding, the current etc. setting circuit 11d outputs a current setting signal Ir indicating a set current value of 300 A or more, preferably a set current value of 300 A or more and 1000 A or less, and more preferably a set current value of 500 A or more and 800 A or less, to the voltage control circuit 11b and the feed speed control circuit 12.

[0032] Moreover, the current etc. setting circuit 11d determines the frequency at which the welding voltage V and welding current I between the base material 4 and the welding wire 5 are periodically varied, the amplitude of the periodically varying welding current I, the average current of the periodically varying welding current I, etc., and generates a set voltage that is set so that the welding current I has a target frequency, current amplitude and average current. The current etc. setting circuit 11d is a circuit that outputs an output voltage setting signal Er indicating the set set voltage to the voltage control circuit 11b.

[0033] The voltage detection unit 11e detects the welding voltage V, and outputs a voltage value signal Vd indicating the detected voltage value to the voltage control circuit 11b.

[0034] The current detection unit 11f detects, for example, the welding current I that is supplied from the welding power source 1 via the torch 2 to the welding wire 5 and flows through the arc 7, and outputs a current value signal Id indicating the detected current value to the current setting circuit 11d.

[0035] The voltage control circuit 11b is a circuit that operates with constant voltage characteristics and controls the operation of the power supply circuit 11a so that a voltage corresponding to the output voltage setting signal Er is output from the power supply circuit 11a. The voltage control circuit 11b electronically controls the electric resistance R and the reactor L present in the current path of the welding power supply 1 to realize the constant voltage characteristics.

[0036] The voltage control circuit 11b calculates a difference signal Ei based on the voltage value signal Vd output from the voltage detection unit 11e and the current setting signal Ir and output voltage setting signal Er output from the current setting circuit 11d, and outputs the calculated difference signal Ei to the power supply circuit 11a. The difference signal Ei is a signal indicating the difference between the detected current value and the current value to be output from the power supply circuit 11a.

[0037] The power supply circuit 11a includes an AC-DC converter that converts commercial AC to DC, an inverter circuit that converts the converted DC to a required AC by switching, a rectifier circuit that rectifies the converted AC, etc. The power supply circuit 11a performs PWM control of the inverter in accordance with a difference signal Ei output from the voltage control circuit 11b so as to reduce the difference signal Ei, and outputs a voltage to the welding wire 5. As a result, a welding voltage V that periodically rises and falls is applied between the base material 4 and the welding wire 5, and a welding current I that periodically rises and falls flows.

[0038] The welding power source 1 is configured to receive an output instruction signal from the outside via a control communication line (not shown), and the power source unit 11 starts supplying voltage to the power source circuit 11a using the output instruction signal as a trigger. The output instruction signal is a signal output from the torch 2 to the welding power source 1 when, for example, a hand-operated switch provided on the torch 2 is operated.

[0039] FIG. 2 is a flow chart showing the procedure of arc welding in the arc welding device 100 according to this embodiment, and FIG. 3 is a side cross-sectional view showing the base material 4 to be welded. In the following, an example will be described in which buried arc welding is performed using a solid wire with a diameter of 1.4 mm as the welding wire 5, carbon dioxide gas as the shielding gas, a welding current of 500 A, and a welding voltage of 42 V. The set voltage is fluctuated within ±10 V with a period of 11 ms.

[0040] First, a pair of base materials 4 to be joined are prepared, and welding conditions including voltage and current, welding mode, etc. are set (step S11). For example, as shown in Fig. 3, plate-shaped first base material 41 and second base material 42 are prepared, and end faces 41a, 42a, which are the parts to be welded, are butted together and arranged at a predetermined welding position. If necessary, grooves of any shape, such as Y-shaped or L-shaped, may be provided in the first base material 41 and the second base material 42. The first and second base materials 41, 42 are, for example, steel plates such as mild steel, carbon steel for mechanical construction, and alloy steel for mechanical construction.

[0041] After various settings are made, the welding power source 1 determines whether the output instruction signal is input, thereby determining whether the voltage output start condition is satisfied (step S12). If the output instruction signal is not input and it is determined that the voltage output start condition is not satisfied (step S12: NO), the welding power source 1 repeats this determination until the output instruction signal is input.

[0042] If it is determined that the voltage output start condition is met (step S12: YES), the feed speed control circuit 12 of the welding power source 1 outputs a feed instruction signal to the wire feeder 3 to instruct the wire feeder 3 to feed the welding wire 5, and causes the welding wire 5 to be fed at a speed according to the current setting signal Ir (step S13).

[0043] Next, power supply unit 11 of welding power source 1 detects welding voltage V and welding current I using voltage detection unit 11e and current detection unit 11f (step S14), and PWM controls the output of power supply unit 11 so that the detected welding voltage V and welding current I and the external characteristics of welding power source 1 match the set welding conditions (step S15). For example, power supply unit 11 has external characteristics such that the drop in welding voltage V in response to an increase in welding current I of 100 A is 2 V or more and 20 V or less.

[0044] That is, the power supply unit 11 performs PWM control by generating and outputting a set voltage so that the frequency, current amplitude, and average current of the detected welding current I match the set welding conditions and the welding current I periodically rises and falls in a constant voltage characteristic.

[0045] Furthermore, in the arc welding apparatus 100 according to the present embodiment, the set voltage is appropriately controlled to prevent the welding current I from suddenly changing at an extreme value portion where the welding current I periodically fluctuates up and down and transitions between rising and falling. This will be described in detail below.

[0046] Fig. 4 is a graph showing a set voltage generated by power supply unit 11 and a change in welding current I according to the set voltage. The horizontal axis of each graph shown in Fig. 4 represents time, and the vertical axis of each graph shown in Fig. 4A-Fig. 4B represents the set voltage and the welding current I, respectively.

[0047] In the arc welding apparatus 100 according to this embodiment, the power supply unit 11 having constant voltage characteristics periodically increases and decreases the set voltage as shown in Fig. 4A. For example, the set voltage may be periodically increased and decreased at a frequency of 10 Hz or more and 1000 Hz or less, preferably 50 Hz or more and 300 Hz or less, and more preferably 80 Hz or more and 200 Hz or less.

[0048] As shown in FIG. 4A, the set voltage is alternately switched between an upper limit value (+10V) and a lower limit value (-10V). That is, the set voltage is switched from the lower limit value to the upper limit value, or from the upper limit value to the lower limit value, every half cycle. The upward switching from the lower limit value to the upper limit value and the downward switching from the upper limit value to the lower limit value are performed over a first time period. That is, in the case of the upward switching, the set voltage gradually increases at a constant rate from the lower limit value to the upper limit value in a straight line during the first time period. Also, in the case of the downward switching, the set voltage gradually decreases at a constant rate from the upper limit value to the lower limit value in a straight line during the first time period. In other words, the rising edge and the falling edge of the set voltage are oblique to the horizontal axis.

[0049] After the upward transition, the setpoint voltage is maintained at the upper limit value for a second time period before being switched to the lower limit value. After the downward transition, the setpoint voltage is maintained at the lower limit value for a second time period before being switched to the upper limit value.

[0050] As described above, the fluctuation period of the set voltage is 11 ms, the first time is 0.5 ms, and the second time is 5 ms, i.e., the upward switching and downward switching are performed for 10% of the second time during which the upper or lower limit value is maintained.

[0051] When the set voltage is periodically increased and decreased in this manner, the welding current I also periodically increases and decreases accordingly, as shown in Fig. 4B. As described above, in the arc welding apparatus 100 of this embodiment, the set voltage is controlled so that the upward and downward switching of the set voltage is performed over a predetermined time. That is, the upward and downward switching of the set voltage is controlled not to occur suddenly, that is, the rising edge and falling edge of the set voltage are not vertical.

[0052] This suppresses sudden changes at the extremes of the welding current I, which fluctuates up and down, and controls it gently. That is, the welding current I changes gently, tracing a curve, at the minimum part where the welding current I stops flowing downward and turns upward (see P1 in Fig. 4), and at the maximum part where the welding current I stops flowing upward and turns downward (see P2 in Fig. 4).

[0053] 5 is a schematic diagram showing buried arc welding according to the first embodiment. For example, a welding current I of 300A or more is supplied to the welding wire 5, and the welding wire 5 is fed at about 5 to 100m / min. At this time, a concave molten portion 6 consisting of the base material 4 and the molten metal of the welding wire 5, which are melted by the heat of the arc 7 generated between the tip 5a of the welding wire 5 and the welded part, is formed in the base material 4, and the tip 5a of the welding wire 5 enters the buried space 6a surrounded by the molten portion 6. When the power supply unit 11 periodically increases and decreases the welding current I (set voltage), a first state (see FIG. 5A) in which the welding wire 5 deeply enters the buried space 6a and an arc 7 is generated between the tip 5a of the welding wire 5 and the bottom 61 of the molten portion 6 and a second state (see FIG. 5B) in which the welding wire 5 shallowly enters the buried space 6a and an arc 7 is generated between the tip 5a and the side 62 of the molten portion 6 are periodically generated.

[0054] In the first state, the tip 5a of the welding wire 5 penetrates deeply into the buried space 6a, and deep penetration is achieved by the arc 7 irradiated to the bottom 61 of the molten portion 6. In the second state, the tip 5a of the welding wire 5 penetrates shallowly into the buried space 6a, and the molten portion 6 is supported by the force of the arc 7 irradiated to the side portion 62 of the molten portion 6. As described above, by periodically increasing and decreasing the welding current I, the first state and the second state are periodically repeated, so that the buried space 6a can be stably maintained.

[0055] Returning to the explanation of Fig. 2, power supply unit 11 of welding power supply 1 then determines whether or not to stop outputting welding current I (step S16). Such a determination is made based on whether or not the input of the output instruction signal is continuing. If the input of the output instruction signal is continuing, power supply unit 11 determines not to stop outputting voltage (step S16: NO), and processing returns to step S13. If the input of the output instruction signal is not continuing, power supply unit 11 determines to stop outputting voltage (step S16: YES), and processing returns to step S12.

[0056] As described above, in buried arc welding, in order to stably maintain the buried space 6a, the welding current I is periodically increased and decreased by periodically increasing and decreasing the set voltage. However, if the fluctuation of the set voltage has a rectangular wave shape and the fluctuation of the set voltage at the rising and falling edges is rapid, the welding current I, which fluctuates up and down accordingly, also fluctuates rapidly at the rising and falling edges. When the welding current I rises (rises) abruptly, the force received from the arc 7 in the region where the arc 7 is formed in the molten portion 6 changes abruptly, so that the state of the molten portion 6 becomes unstable. On the other hand, when the welding current I falls (drops) abruptly, the rigidity of the arc 7 is instantly lost and the arc 7 becomes unstable because it fluctuates.

[0057] In contrast, in the arc welding apparatus 100 of the present embodiment, as described above, when the set voltage is periodically increased and decreased, the set voltage is switched upward and downward over a predetermined time period so that the switching upward and downward does not occur suddenly. This suppresses abrupt changes at the extreme values ​​of the welding current I, which fluctuates up and down, and obtains a gentle fluctuation. This prevents the above-mentioned problems of the state of the molten portion 6 becoming unstable when the welding current I rises suddenly, and the problem of the arc 7 becoming unstable when the welding current I falls suddenly. Furthermore, since the sudden change in the welding current I is suppressed, it is possible to reduce the noise generated when the welding current I changes suddenly.

[0058] In the above, an example has been described in which the first time required for upward switching and downward switching is 10% of the second time during which the upper or lower limit value of the set voltage is maintained, but this is not limited to this.

[0059] If the first time is less than 5% of the second time, the current change at the rise / fall of the welding current I is not sufficiently suppressed, the above-mentioned problem cannot be solved, and the buried arc cannot be stabilized. If the first time is more than 15% of the second time, the buried arc becomes more unstable than when the set voltage is changed in a rectangular shape. Therefore, the first time should be 5%-15% of the second time, and within this range, the effect on the stability of the buried arc is negligible.

[0060] Furthermore, as the first time becomes 5% or more of the second time, a stabilizing effect on the buried arc is obtained, and when it becomes 8% or more, the above-mentioned noise is alleviated. On the other hand, when the first time exceeds 12% of the second time, the amount of current change becomes smaller overall compared to when the control of the upward and downward switching of the set voltage of this embodiment is not performed, and the originally intended buried arc stabilizing effect begins to decrease. Therefore, it is more preferable that the first time is 8%-12% of the second time.

[0061] (Embodiment 2) Fig. 6 is a graph showing a set voltage generated by the power supply unit 11 in the arc welding apparatus 100 according to embodiment 2. The horizontal axis of the graph shown in Fig. 6 indicates time, and the vertical axis indicates the set voltage. In the arc welding apparatus 100 according to embodiment 2, too, in buried arc welding, in order to stably maintain the buried space 6a, control is performed to periodically increase and decrease the set voltage, thereby periodically increasing and decreasing the welding current I.

[0062] The set voltage is alternately switched between an upper limit (+10V) and a lower limit (-10V). That is, it is switched from the lower limit to the upper limit, or from the upper limit to the lower limit, every half cycle. The upward switching from the lower limit to the upper limit, and the downward switching from the upper limit to the lower limit, are performed over a first time period. That is, in the case of the upward switching, the set voltage continues to gradually increase from the lower limit to the upper limit in a downwardly convex curve during the first time period. Also, in the case of the downward switching, the set voltage continues to gradually decrease from the upper limit to the lower limit in an upwardly convex curve during the first time period. In both the case of the upward switching and the downward switching, the change in the set voltage in the first half of the first time period is smaller than that in the second half of the first time period.

[0063] After the upward switch, the set voltage is maintained at the upper limit for a second time and then switched to the lower limit. After the downward switch, the set voltage is maintained at the lower limit for a second time and then switched to the upper limit. As in embodiment 1, the first time for the upward switch and downward switch is 10% of the second time for which the upper or lower limit is maintained.

[0064] When the set voltage is periodically increased and decreased in this manner, the welding current I also periodically increases and decreases accordingly. As described above, in the arc welding apparatus 100 of this embodiment, the set voltage is switched upward and downward over a predetermined period of time so that the set voltage is not switched upward or downward suddenly. This suppresses abrupt changes at the extreme values ​​of the welding current I that fluctuates up and down, and the welding current I fluctuates gently (see FIG. 4).

[0065] In the above, a case has been described in which both the switching of the set voltage from the lower limit value to the upper limit value and the switching of the set voltage from the upper limit value to the lower limit value are performed over the first hour, but this is not limited to this. It is also possible to configure the setting so that only one of the switching of the set voltage from the lower limit value to the upper limit value and the switching of the set voltage from the upper limit value to the lower limit value is performed over the first hour.

[0066] In the above, the control of the set voltage has been described to suppress abrupt changes at the extreme values ​​of the welding current I, which fluctuates up and down, but the present invention is not limited to this. For example, when the welding current I rises or falls, a limit may be placed on the rate of change of the welding current I to suppress abrupt changes at the extreme values ​​of the welding current I.

[0067] The disclosed embodiments 1 and 2 are illustrative in all respects and should not be considered as limiting. The scope of the present invention is indicated by the claims, not by the above meaning, and is intended to include all modifications within the meaning and scope of the claims. At least some of the above-mentioned embodiments may be arbitrarily combined. [Explanation of symbols]

[0068] 4 Base material 5 Welding Wire 5a Tip 6 Melted part 11 Power supply section 100 Arc welding equipment

Claims

1. In an arc welding apparatus for performing arc welding by inserting a tip of a welding wire into an inner space of a concave molten portion formed in a base material, An arc welding device comprising a power supply unit that controls a set voltage to vary the welding current flowing through the welding wire, and controls the variation of the welding current when a transition occurs between an increase and a decrease in the welding current.

2. The power supply unit includes: The set voltage is alternately switched between an upper limit value and a lower limit value, Switching from the lower limit value to the upper limit value or from the upper limit value to the lower limit value is performed over a first time period.

2. The arc welding apparatus of claim 1.

3. The set voltage varies at a constant rate during the first period of time.

3. The arc welding apparatus of claim 2.

4. The change in the set voltage during the first half of the first period is smaller than the change in the set voltage during the second half of the first period.

3. The arc welding apparatus of claim 2.

5. the power supply unit maintains the set voltage at the upper limit and the lower limit for a second time; The first time period is 5-15% of the second time period.

5. An arc welding apparatus according to claim 2 .

6. The first time period is 8-12% of the second time period.

6. The arc welding apparatus according to claim 5.

7. In an arc welding method, a tip end of a welding wire is inserted into an inner space of a concave molten portion formed in a base metal to perform arc welding, An arc welding method comprising controlling a set voltage to vary a welding current flowing through the welding wire, and controlling the variation of the welding current when a transition between an increase and a decrease in the welding current occurs.

Citation Information

Patent Citations

  • Method and device for detecting run-out in one line submerged arc welding

    JP1996294791A

  • Pulse arc welding output control method

    JP2016132003A

  • Arc-welding method and arc-welding device

    JP2017144480A

  • Arc-welding method and arc-welding device

    JP2018069253A