Liquid crystal elements, lighting devices, vehicle lights
The triple-seal structure in liquid crystal elements addresses the issue of moisture resistance by using low-permeability and high-adhesion materials, enhancing durability in in-vehicle lighting applications.
Patent Information
- Application Number
- JP2021087213
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-05-24
- Publication Date
- 2024-11-27
- Estimated Expiration
- 2041-05-24
AI Technical Summary
Existing liquid crystal elements lack sufficient moisture resistance for applications requiring higher moisture-proof properties, particularly in in-vehicle lighting devices.
A liquid crystal element configuration with a triple-seal structure comprising first and second substrates, conductive films, inorganic insulating films, alignment films, and a liquid crystal layer, where the seal portions are arranged to cover alignment films and inorganic insulating films, enhancing moisture resistance through materials with low permeability and high adhesion.
The triple-seal structure significantly improves moisture-proofing and vibration resistance of the liquid crystal element, ensuring durability in harsh environments.
Smart Images

Figure 0007590922000001 
Figure 0007590922000002 
Figure 0007590922000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a liquid crystal element, a lighting device, and a vehicle lamp. [Background technology]
[0002] In recent years, in addition to the conventional display applications, liquid crystal elements are being used for a wide range of applications, such as as optical shutters for forming various light distribution patterns in lighting devices such as vehicle lamps. In addition, liquid crystal elements are expected to have higher moisture resistance than ever before in applications such as in-vehicle applications.
[0003] Conventional techniques relating to moisture resistance of liquid crystal elements are described in, for example, JP-A-2003-255357 (Patent Document 1), JP-A-60-26321 (Patent Document 2), JP-A-57-38415 (Patent Document 3), JP-A-57-181527 (Patent Document 4), etc. However, there is room for further improvement in situations where higher moisture resistance is required. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2003-255357 A [Patent Document 2] Japanese Patent Application Publication No. 60-26321 [Patent Document 3] Japanese Patent Application Publication No. 57-38415 [Patent Document 4] Japanese Patent Application Publication No. 57-181527 Summary of the Invention [Problem to be solved by the invention]
[0005] An object of a specific embodiment of the present disclosure is to provide a liquid crystal element having high moisture resistance or a lighting device or the like including the liquid crystal element. [Means for solving the problem]
[0006] [1] A liquid crystal element according to one aspect of the present disclosure includes: (a) a first substrate and a second substrate disposed opposite each other; (b) a first conductive film disposed on one surface of the first substrate; (c) a first inorganic insulating film disposed on one surface of the first substrate farther from the first substrate than the first conductive film; (d) a first alignment film disposed on one surface of the first substrate farther from the first substrate than the first inorganic insulating film; (e) a second conductive film disposed on one surface of the second substrate; (f) a second inorganic insulating film disposed on one surface of the second substrate farther from the second substrate than the second conductive film; and (g) a first alignment film disposed on one surface of the second substrate. (h) a second alignment film disposed farther from the second substrate than the second inorganic insulating film; (h) a liquid crystal layer disposed between the first substrate and the second substrate; and (i) a sealing portion disposed between the first substrate and the second substrate to surround the liquid crystal layer, (j) the sealing portion has at least a first sealing portion and a second sealing portion in the order of proximity to the liquid crystal layer, (k) the first sealing portion is disposed so as to cover an end of the first alignment film and an end of the second alignment film, and (l) the second sealing portion is disposed so as to be in contact with each of the first inorganic insulating film and the second inorganic insulating film. [2] An illumination device according to one aspect of the present disclosure is an illumination device including the liquid crystal element according to [1] above, a pair of polarizing elements arranged opposite each other across the liquid crystal element, and a light source that causes light to enter the liquid crystal element. [3] A vehicle lamp according to one aspect of the present disclosure is a vehicle lamp configured using the lighting device according to [2] above.
[0007] According to the above-mentioned configuration, it is possible to provide a highly moisture-proof liquid crystal element and an illumination device or the like including the same. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a schematic plan view showing the configuration of a liquid crystal element according to the first embodiment. [Diagram 2]2A is a schematic cross-sectional view of the liquid crystal element taken along the line AA' shown in FIG. 1, and FIG. 2B is a schematic cross-sectional view of the liquid crystal element taken along the line BB' shown in FIG. [Diagram 3] FIG. 3 is a plan view for explaining the positional relationship between the inorganic insulating film and the alignment film and the sealing portion. [Figure 4] 4(A) to 4(F) are views for explaining an example of a method for manufacturing the liquid crystal element of the first embodiment. [Diagram 5] FIG. 5 is a schematic plan view showing the configuration of a liquid crystal element according to the second embodiment. [Figure 6] 6(A) to 6(D) are views for explaining an example of a method for manufacturing the liquid crystal element of the second embodiment. [Figure 7] FIG. 7 is a schematic plan view showing the configuration of a liquid crystal element according to the third embodiment. [Figure 8] 8(A) to 8(F) are views for explaining an example of a method for manufacturing the liquid crystal element of the third embodiment. [Figure 9] FIG. 9 is a schematic plan view showing the configuration of a liquid crystal element according to the fourth embodiment. [Figure 10] 10(A) to 10(D) are views for explaining an example of a method for manufacturing the liquid crystal element of the fourth embodiment. [Figure 11] FIG. 11 is a schematic plan view showing the configuration of a liquid crystal element according to the fifth embodiment. [Figure 12] 12(A) to 12(C) are views for explaining an example of a method for manufacturing the liquid crystal element of the fifth embodiment. [Figure 13] FIG. 13 is a diagram showing a configuration of a vehicle lighting system according to the sixth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] (First embodiment) Fig. 1 is a schematic plan view showing the configuration of a liquid crystal element of the first embodiment. Fig. 2(A) is a schematic cross-sectional view of the liquid crystal element in the A-A' direction shown in Fig. 1, and Fig. 2(B) is a schematic cross-sectional view of the liquid crystal element in the B-B' direction shown in Fig. 1. Note that Fig. 1 illustrates the structure of the seal portion 20 in an easy-to-understand manner, but in reality, the seal portion 20 is present between the substrates (inside the substrates) as shown in Figs. 2(A) and 2(B).
[0010] 2(A) and 2(B), the liquid crystal element 100a includes a first substrate 11 and a second substrate 12 arranged opposite each other, a first conductive film 13, a second conductive film 14, a first inorganic insulating film 15, a second inorganic insulating film 16, a first alignment film 17, a second alignment film 18, a liquid crystal layer 19, a first seal portion 21, a second seal portion 22, a third seal portion 23, a conductive material 24, a plurality of protrusions 25, and sealing portions 26, 27, and 28. The first seal portion 21, the second seal portion 22, and the third seal portion 23 form a seal portion 20.
[0011] The first substrate 11 and the second substrate 12 are, for example, rectangular substrates in plan view, and are arranged so that one side of each substrate faces the other. Each substrate may be a transparent substrate such as a glass substrate or a plastic substrate. The thickness of each substrate is, for example, about 0.7 mm. In this specification, "transparent" means that at least visible light can be sufficiently transmitted. Between the first substrate 11 and the second substrate 12, spherical spacers (not shown) made of, for example, resin or the like are dispersed and arranged, and the substrate gap is maintained at a desired size (for example, about several μm) by these spherical spacers. Instead of the spherical spacers, pillars made of, for example, resin or the like may be provided on the first substrate 11 side or the second substrate 12 side, and these may be used as spacers.
[0012] The first conductive film 13 is provided on one surface of the first substrate 11. The second conductive film 14 is provided on one surface of the second substrate 12. The first conductive film 13 and the second conductive film 14 are formed by appropriately patterning a transparent conductive film made of an oxide such as indium tin oxide (ITO). The thickness of each conductive film is, for example, about 280 Å. The alignment state of the liquid crystal layer 19 can be variably set by applying a voltage between the first conductive film 13 and the second conductive film 14. A pixel section (light modulation section) is formed in the portion where the first conductive film 13 and the second conductive film 14 face each other.
[0013] The first inorganic insulating film 15 is provided on one surface of the first substrate 11 above the first conductive film 13, i.e., on the side farther from the first substrate 11 than the first conductive film 13. The second inorganic insulating film 16 is provided on one surface of the second substrate 12 above the second conductive film 14, i.e., on the side farther from the second substrate 12 than the second conductive film 14. In this embodiment, the first inorganic insulating film 15 and the second inorganic insulating film 16 are each formed using an inorganic material. Specifically, the first inorganic insulating film 15 and the second inorganic insulating film 16 can be composed of a siloxane-based inorganic insulating film, a titanosiloxane-based inorganic insulating film, or the like. The siloxane-based inorganic insulating film and the titanosiloxane-based inorganic insulating film can be formed by firing a polysiloxane-based material and a polytitanosiloxane-based material, respectively. In particular, the first inorganic insulating film 15 and the second inorganic insulating film 16 are preferably made of a siloxane-based inorganic insulating film and a titanosiloxane-based inorganic insulating film, and are made of a material containing a hydroxyl group (OH group) as a functional group. The first inorganic insulating film 15 and the second inorganic insulating film 16 are more dense than the first conductive film 13 and the second conductive film 14 made of ITO. The thickness of each inorganic insulating film is, for example, about 800 Å.
[0014] The first alignment film 17 is provided on one surface of the first substrate, above the first inorganic insulating film 15, i.e., on the side farther from the first substrate 11 than the first inorganic insulating film 15. The second alignment film 18 is provided on one surface of the second substrate, above the second inorganic insulating film 16, i.e., on the side farther from the second substrate 12 than the second inorganic insulating film 16. These first alignment film 17 and second alignment film 18 are for setting the initial alignment state of the liquid crystal layer 19. The first alignment film 17 and second alignment film 18 are subjected to a uniaxial alignment treatment, such as a rubbing treatment, and have a uniaxial alignment regulating force that regulates the alignment of the liquid crystal molecules of the liquid crystal layer 19 along that direction. The thickness of each alignment film is, for example, about 500 Å. The first alignment film 17 and second alignment film 18 can be made of an organic material such as polyimide, or an inorganic material such as a silicon oxide film that can be formed by oblique deposition or printing. The first alignment film 17 and the second alignment film 18 can be made of a siloxane-based alignment film having a basic skeleton similar to that of the material of the first inorganic insulating film 15 and the second inorganic insulating film 16 and an appropriate functional group. The first alignment film 17 and the second alignment film 18 can be made of a material having a side chain for alignment control and containing fewer hydroxyl groups than the material of the first inorganic insulating film 15 and the second inorganic insulating film 16.
[0015] The liquid crystal layer 19 is provided between the first substrate 11 and the second substrate 12 in contact with the first alignment film 17 and the second alignment film 18. The liquid crystal layer 19 is made of, for example, a nematic liquid crystal material having fluidity. There are no particular limitations on the alignment mode (operation mode) of the liquid crystal layer 19, and various alignment modes such as a vertical alignment mode and a twisted nematic mode can be adopted. The layer thickness of the liquid crystal layer 19 is, for example, about 4 μm.
[0016] The seal portion 20 is disposed between the first substrate 11 and the second substrate 12, surrounding the liquid crystal layer 19. As shown in FIG. 1, the seal portion 20 defines a space between the first substrate 11 and the second substrate 12 for accommodating the liquid crystal layer 19. The seal portion 20 has a first seal portion 21, a second seal portion 22, and a third seal portion 23, in the order of proximity to the liquid crystal layer 19. As shown in FIG. 1, the seal portion 20 is configured to have a substantially rectangular shape in a plan view, and is disposed along the outer edges of each of the first substrate 11 and the second substrate 12. A spacer such as glass fiber having a diameter slightly larger than the thickness of the liquid crystal layer 19 may be added to each of the seal portions 21, 22, and 23.
[0017] The first seal portion 21 is provided in contact with the liquid crystal layer 19 so as to surround the liquid crystal layer 19. The first seal portion 21 is disposed so as to cover the end of the first alignment film 17 and to cover the end of the second alignment film 18. In detail, the first seal portion 21 is disposed so as to cover the stepped portion of the end of the first alignment film 17 and to be in contact with the first inorganic insulating film 15 below it, and is disposed so as to cover the stepped portion of the end of the second alignment film 18 and to be in contact with the second inorganic insulating film 16 below it. The first seal portion 21 is preferably made of a material that is insoluble in the liquid crystal layer 19 and has a high adhesiveness, for example, a moisture permeability of 50 to 70 g / m 2 Materials such as thermosetting epoxy resin with a hardness of about 24h (JISK7126-1) can be used.
[0018] The second seal portion 22 is provided so as to contact the first seal portion 21 and surround the outside of the first seal portion 21. The second seal portion 22 is disposed so as to contact each of the first inorganic insulating film 15 and the second inorganic insulating film 16. As shown in FIG. 2(A), the second seal portion 22 is provided so as to contact and adhere only to the first inorganic insulating film 15 and the second inorganic insulating film 16 in a large part thereof. As shown in FIG. 2(B), the second seal portion 22 is provided so as to contact the first inorganic insulating film 15 and the first conductive film 13 on the first substrate 11 side in another part thereof, and to contact the second inorganic insulating film 16 and the second conductive film 14 on the second substrate 12 side in another part thereof. The part here refers to a part close to a part where the first conductive film 13 and the second conductive film 14 are physically and electrically connected to each other by the conductive material 24 partially contained in the third seal portion 23. The second seal portion 22 is preferably made of a material with low moisture permeability, and in particular, is preferably made of a material with lower moisture permeability than the first seal portion 21. For example, the moisture permeability is 2 to 4 g / m 2 It is preferable to use a material having a hardness of 24h (JISK7126-1), for example, a material such as ultraviolet-curing epoxy or modified acrylate can be used.
[0019] The third seal portion 23 is provided so as to contact the second seal portion 22 and surround the outside of the second seal portion 22. As shown in FIG. 2(B), the third seal portion 23 has a conductive material 24 in a part thereof, and the conductive material 24 is arranged so as to contact each of the first conductive film 13 and the second conductive film 14, and as shown in FIG. 2(A), the third seal portion 23 is arranged so as to contact each of the first inorganic insulating film 13 and the second inorganic insulating film 14 in the other most part. The conductive material 24 is, for example, a gold-plated sphere. As shown in FIG. 2(A), the third seal portion 23 is arranged so as to cover the end of the first conductive film 13, the end of the first inorganic insulating film 15, the end of the second conductive film 14, and the end of the second inorganic insulating film 16 in the most part. That is, in the most part of the annular seal portion 20 shown in FIG. 1, the third seal portion 23 is formed so as to fill the gap between the first inorganic insulating film 15 and the second inorganic insulating film 16 up to the end, as shown in FIG. 2(A). The third seal portion 23 is preferably made of a material with high adhesiveness, for example, a material such as a thermosetting epoxy resin, and may be made of the same material as the first seal portion 21.
[0020] As shown in each figure, the first seal portion 21, the second seal portion 22, and the third seal portion 23 are arranged in contact with one another in a direction substantially perpendicular to the thickness direction of the liquid crystal layer 19. In detail, the second seal portion 22 is arranged in contact with the first seal portion 21 on the side closer to the liquid crystal layer 19, and in contact with the third seal portion 23 on the side farther from the liquid crystal layer 19. The first seal portion 21 and the third seal portion 23 are made of the same material. The second seal portion 22 has relatively lower moisture permeability than the first seal portion 21 and the third seal portion 23.
[0021] 1, the multiple protrusions 25 are provided dispersedly along the outer periphery of the third seal portion 23. In the illustrated example, two protrusions 25 are provided on the left and right sides near the sealants 26 and 27, and two protrusions 25 are provided near the sealant 28. The function of these protrusions 25 will be described later.
[0022] The first sealing material 26 and the second sealing material 27 are end seal parts for sealing an injection port 51 (see FIG. 4(D) described later) of the liquid crystal layer 19 during manufacturing (see FIG. 1). A material having incompatibility with the liquid crystal material of the liquid crystal layer 19 is used as the first sealing material 26. A material having high gas barrier properties is used as the second sealing material 27. When a material having both functions is used, only the first sealing material 26 is sufficient.
[0023] The third sealing material 28 is an end seal portion for sealing the injection port 52 (see FIG. 4(C) described later) of the second seal portion 22 during manufacturing (see FIG. 1). A material having high gas barrier properties is used as the third sealing material 28. The third sealing material 28 can be provided as desired, and may be unnecessary if the second seal portion 22 has high gas barrier properties.
[0024] Fig. 3 is a plan view for explaining the positional relationship between the inorganic insulating film and the alignment film and the sealing portion. Note that the scale of the sealing portion and the like is changed from that of Fig. 1 in order to show the positional relationship. Hereinafter, with reference to Fig. 3 and Fig. 2(A) or Fig. 2(B) described above, the formation ranges of the first inorganic insulating film 15 and the first alignment film 17 on one surface side of the first substrate 11 will be explained, and the formation ranges of the second inorganic insulating film 16 and the second alignment film 18 on one surface side of the second substrate 12 will be explained.
[0025] As shown in FIG. 2(A) or FIG. 2(B), on one surface side of the first substrate 11, the first conductive film 13 may have a portion whose end is provided to the outermost side, that is, the side close to the end of the first substrate 11. Also, as shown in FIG. 2(A) or FIG. 2(B), on one surface side of the second substrate 12, the second conductive film 14 may have a portion whose end is provided to approximately the same position as the end of the second alignment film 18. In some cases, the ends of both the first conductive film 13 and the second conductive film 14 overlap with the third seal portion 23. The first conductive film 13 and the second conductive film 14 are each appropriately patterned. For example, the first conductive film 13 may include a plurality of pixel electrodes and a plurality of wirings connected thereto.
[0026] The first inorganic insulating film 15 is provided so that its end is located inside (closer to the liquid crystal layer 19) than the end of the third seal portion 23 (shown by a dotted line in FIG. 3). The first inorganic insulating film 15 also has a notch 15a as shown in FIG. 3. This notch 15a is provided at a position corresponding to the portion where the conductive material 24 shown in FIG. 2(B) is provided, and is for allowing the first conductive film 13 to contact the conductive material 24 without being covered by the first inorganic insulating film 15. A similar notch is also provided in the second inorganic insulating film 16. The second inorganic insulating film 16 is provided so that its end is located inside (closer to the liquid crystal layer 19) than the end of the second conductive film 14 in the notch portion corresponding to the notch 15a. The ends of both the first inorganic insulating film 15 and the second inorganic insulating film 16 overlap with the third seal portion 23 in most parts except for the parts corresponding to the notch and the like, and are arranged inside the outer end of the third seal portion 23.
[0027] The first alignment film 17 is provided so that its end is on the innermost side (the side closest to the liquid crystal layer 19). Similarly, the second alignment film 18 is provided so that its end is on the innermost side (the side closest to the liquid crystal layer 19). Most of the ends of both the first alignment film 17 and the second alignment film 18 overlap with the first seal portion 21, and are disposed inside the outer end of the first seal portion 21.
[0028] 4(A) to 4(F) are diagrams for explaining an example of a method for manufacturing the liquid crystal element of the first embodiment. Note that, although steps related to one liquid crystal element 100a are illustrated here, in practice, a plurality of liquid crystal elements 100a can be manufactured simultaneously (the same applies to other embodiments).
[0029] First, a first conductive film 13 and a second conductive film 14 (not shown) are formed on a pair of substrates that are the base materials of the first substrate 11 and the second substrate 12, respectively. The first conductive film 13 and the second conductive film 14 may be appropriately patterned. Next, as shown in FIG. 4(A), a first inorganic insulating film 15 (not shown) and a first alignment film 17 are formed on one surface side of the base material 50 of the first substrate 11. Similarly, a second inorganic insulating film 16 (not shown) and a second alignment film 18 (not shown) are formed on one surface side of the base material of the second substrate 12. As the first alignment film 17 and the second alignment film 18, a horizontal alignment film or a vertical alignment film is appropriately selected and formed depending on the operation mode of the liquid crystal layer 19, etc.
[0030] There is no particular limitation on the method of forming the inorganic insulating film and the alignment film, and for example, they are applied by flexographic printing and then baked. There is no particular limitation on the alignment treatment of the alignment film, and for example, a rubbing treatment can be used, but other methods (such as photoalignment treatment) may also be used. Also, obliquely evaporated films may be used as each alignment film. In addition, in the case of an operation mode in which openings or protrusions are provided in each conductive film (electrode) to generate an oblique electric field to control the alignment of the liquid crystal layer 19, alignment treatments such as rubbing treatment may be omitted. Note that the same applies to other embodiments.
[0031] As shown in FIG. 4(A), the first seal portion 21 and the third seal portion 23 are formed on one surface of the base material 50 of the first substrate 11 in a position corresponding to the position where the first alignment film 17 is formed. As shown in the figure, the first seal portion 21 and the third seal portion 23 are provided with a gap between them. This gap is for providing the second seal portion 22 in a later process. There is no particular limitation on the method of forming the first seal portion 21 and the third seal portion 23, and for example, a method of applying the material using a dispenser or a method of applying the material by screen printing can be used. At this time, openings as injection ports 51 and 52 are respectively provided. At the same time, each protrusion portion 25 is formed from the same material as the first seal portion 21 and the third seal portion 23.
[0032] Next, the base material 50 of the first substrate 11 and the base material (not shown) of the second substrate 12 are aligned and overlapped. At this time, a gap control material is sprayed on the base material of the second substrate 12 in advance. Depending on the properties of the first seal portion 21 and the third seal portion 23, if they are thermosetting, a heat treatment is performed, and if they are photosetting, a light irradiation treatment is performed, so that the base materials are bonded together. Thereafter, a cutting line (crack) is made in the bonded base materials, and then the bonded base materials are cut along the cutting line, so that a cell is obtained in which the first substrate 11 and the second substrate 12 are bonded to the first seal portion 21 and the third seal portion 23, as shown in FIG. 4(B).
[0033] Next, the second seal portion 22 is formed as shown in FIG. 4(C). Here, the material for the second seal portion 22 is dropped near the injection port 52, and is injected by utilizing the capillary phenomenon. In this sense, the gap between the first seal portion 21 and the third seal portion 23 needs to be wide enough to cause the capillary phenomenon. The material for the second seal portion 22 is one with low moisture permeability (one with high gas barrier properties). For example, a material with a moisture permeability of 2 to 4 g / m 2 24h (JISK7126-1) can be used. From the viewpoint of shortening the injection time, it is preferable that the viscosity of the material is low, for example, it is preferable to use a material with a viscosity of approximately 10 Pa·s or less. If a highly viscous material is used, the injection may be performed while the cell is heated. After injection, depending on the characteristics of the second seal portion 22, if it is thermosetting, a heat treatment is performed, if it is photosetting, a light irradiation treatment is performed, and if both heat treatment and light irradiation treatment are necessary, each treatment is performed to complete the second seal portion 22. As an example, ultraviolet light containing a wavelength of 365 nm is applied at 6 J / cm 2 Then, heat treatment is performed at 150° C. for 1 hour.
[0034] Here, even if the material of the second seal portion 22 overflows from the injection port 52, the flow of the material is blocked by the protrusions 25 provided on the left and right of the injection port 52 and the protrusions 25 provided on the left and right of the injection port 51 on the opposite side. If these protrusions 25 were not present, capillary action would occur in the gap at the outer edges of the first substrate 11 and the second substrate 12, and the material would flow ahead to the outlet on the opposite side, which could result in the second seal portion 22 not being completely filled. By providing the protrusions 25, such a problem can be avoided. For this reason, it is preferable to provide a large number of protrusions 25 along the outer periphery of the third seal portion 23.
[0035] Next, as shown in FIG. 4(D), liquid crystal material is injected from the injection port 51. Here, a vacuum injection method is used. Specifically, the cell is placed in a vacuum chamber, and the vacuum chamber is brought to a low pressure, and then the injection port 51 is placed so as to contact the liquid crystal material in the injection tank 53. The vacuum chamber is then returned to atmospheric pressure, and the liquid crystal material is injected from the injection port 51, and the liquid crystal layer 19 is formed as shown in FIG. 4(E). The liquid crystal material of the liquid crystal layer 19 has a dielectric anisotropy of positive / negative appropriately selected according to the operation mode. In addition, an ultraviolet-curable monomer may be added to the liquid crystal material. In this case, a polymer-stabilized liquid crystal layer 19 is obtained by later irradiating the liquid crystal with ultraviolet light.
[0036] Next, as shown in FIG. 4(E), a sealant 26 is formed to seal the injection port 51. After the liquid crystal material is injected, the cell may be thicker near the center and bulge. In this case, the material of the sealant 26 is applied near the injection port 51 while the cell is pressed, and then the press is released. Alternatively, the cell is cooled. This reduces the cell thickness near the center of the cell, and some of the material of the sealant 26 is absorbed. The material is then hardened by light irradiation or the like, forming the sealant 26 at a position slightly inward from the injection port 51.
[0037] 4(F), a sealant 27 is formed on the outside of the sealant 26 at the injection port 51, and a sealant 28 is formed at the injection port 52. Specifically, the materials of the sealants 27 and 28 are applied to the vicinity of the injection ports 51 and 52, and then the materials are hardened by a light irradiation process or the like, thereby forming the sealants 27 and 28. Thereafter, the entire cell is appropriately cleaned, and the liquid crystal element 100a is completed.
[0038] According to the first embodiment described above, at least the first seal portion 21 and the second seal portion 22 are provided so as to contact the first inorganic insulating film 15 and the second inorganic insulating film 16, so that it is possible to improve moisture resistance. The reason for this is presumed to be as follows. In general, it is considered that the siloxane-based material and the titanosiloxane-based material constituting the first inorganic insulating film 15 and the second inorganic insulating film 16 have more OH groups on the film surface than the conductive film such as an alignment film or ITO. And, since there are more OH groups, the adhesion with each seal portion is higher, so that the function of the second seal portion 22 with low moisture permeability can be maintained, and it is considered that a seal structure with low moisture permeability can be formed. Specifically, the bonding strength is improved by the formation of covalent bonds between the organic functional groups of the material of each seal portion and the OH groups of the material constituting the first inorganic insulating film 15 and the second inorganic insulating film 16. In addition, the third sealing portion 23 is also provided so as to fill the space between the ends of the first inorganic insulating film 15 and the second inorganic insulating film 16, and similarly forms a covalent bond between the organic functional group of the sealing material and the OH group of the material constituting the first inorganic insulating film 15 and the second inorganic insulating film 16, thereby increasing the bonding strength.
[0039] Furthermore, according to the first embodiment, since the sealing portion 20 has a triple structure, its width in a planar view becomes larger (wider), so that the first substrate 11 and the second substrate 12 can be fixed more firmly, which has the secondary effect of improving vibration resistance.
[0040] Second embodiment 5 is a schematic plan view showing the configuration of a liquid crystal element of the second embodiment. The liquid crystal element 100b of the second embodiment basically has the same configuration as the liquid crystal element 100a of the first embodiment, and differs mainly in that the injection port 51 is omitted, and therefore the sealing material 26 is also omitted. In this case, the liquid crystal layer 19 is formed by, for example, an ODF (One Drop Fill) method. In the following, a description of the configuration common to the liquid crystal element 100a of the first embodiment will be omitted, and differences in the configuration will be mainly described.
[0041] The first seal portion 21b does not have an opening such as an injection port, and is provided to form a closed space surrounding the liquid crystal layer 19. Accordingly, the second seal portion 22b is provided such that two ends sealed by the sealing material 27 are adjacent to each other with a partition wall 29 interposed therebetween. The cross-sectional structure of the seal portion 20b including these is the same as that of the first embodiment (see Figs. 2(A) and 2(B)). The protrusions 25 and the partition wall 29 are formed, for example, from the same material as the first seal portion 21b.
[0042] 6(A) to 6(D) are diagrams for explaining an example of a method for manufacturing a liquid crystal element according to the second embodiment. As in the first embodiment, a first conductive film 13 and a second conductive film 14 (not shown) are formed in advance on a pair of substrates that serve as base materials for the first substrate 11 and the second substrate 12, respectively.
[0043] 6(A), a first inorganic insulating film 15 (not shown) and a first alignment film 17 are formed on one surface of the base material 50 of the first substrate 11. Similarly, a second inorganic insulating film 16 (not shown) and a second alignment film 18 (not shown) are formed on one surface of the base material of the second substrate 12.
[0044] 6(A), the first seal portion 21b and the third seal portion 23 are formed on one surface side of the base material 50 of the first substrate 11. At this time, an opening is provided as an injection port 52. Furthermore, the protrusions 25 and the partition walls 29 are formed of the same material as the first seal portion 21b.
[0045] Next, as shown in FIG. 6B, liquid crystal material is dropped into the space surrounded by the first seal portion 21b by the ODF method or the like. The liquid crystal material used is sufficiently degassed, and the volume of the dropped liquid crystal material is precisely controlled. Next, the base material 50 of the first substrate 11 and the base material of the second substrate 12 (not shown) are aligned, overlapped, and bonded together. After that, a cutting line (crack) is made in the bonded base materials, and then the bonded materials are cut along the cutting line to obtain a cell formed by bonding the first substrate 11 and the second substrate 12 together.
[0046] Next, the second seal portion 22b is formed as shown in FIG. 6(C). Here, too, the material for the second seal portion 22b is dropped near the injection port 52, and is injected by utilizing the capillary phenomenon. After injection, the second seal portion 22b is completed by performing heat treatment or light irradiation treatment as appropriate. At this time, when the material injected counterclockwise and the material injected clockwise in the figure join at the outlet side, the partition wall 29 ensures an escape route for air even if an imbalance occurs due to a difference in injection speed, etc., so that the formation of the second seal portion 22b can be prevented. Note that the partition wall 29 may be omitted when the injection speeds are almost the same.
[0047] 6(D), the material of each of the sealants 27 and 28 is applied to a predetermined position, and then the material is cured by light irradiation or the like to form each of the sealants 27 and 28. Thereafter, the entire cell is appropriately cleaned, and the liquid crystal element 100b is completed.
[0048] According to the second embodiment described above, the same moisture resistance as in the first embodiment can be obtained. In addition, a secondary effect of improving vibration resistance can be obtained. Furthermore, according to the second embodiment, a method other than the vacuum injection method, such as the ODF method, can be applied to form the liquid crystal layer 19.
[0049] Third embodiment 7 is a schematic plan view showing the configuration of a liquid crystal element of the third embodiment. The liquid crystal element 100c of the third embodiment basically has the same configuration as the liquid crystal element 100a of the first embodiment, and differs mainly in that the first seal portion 21c and the third seal portion 23c are connected to each other on the side of the sealing materials 26 and 27. In this case, the second seal portion 22 is formed by using a vacuum injection method. In the following, a description of the points in common with the liquid crystal element 100a of the first embodiment will be omitted, and the points of difference in the configuration will be mainly described.
[0050] The first seal portion 21c has injection ports 51 and 52 (see FIG. 8A), and is provided to define a substantially closed space surrounding the liquid crystal layer 19. The third seal portion 23c is provided along the outer periphery of the second seal portion 22, and is connected to the first seal portion 21c on the side where the injection port 51 is provided. The cross-sectional structure of the seal portion 20c including these is the same as in the first embodiment (see FIGS. 2A and 2B).
[0051] 8(A) to 8(F) are diagrams for explaining an example of a method for manufacturing a liquid crystal element according to the third embodiment. As in the first embodiment, a first conductive film 13 and a second conductive film 14 (not shown) are formed in advance on a pair of substrates that serve as base materials for the first substrate 11 and the second substrate 12, respectively.
[0052] 8(A), a first inorganic insulating film 15 (not shown) and a first alignment film 17 are formed on one surface of the base material 50 of the first substrate 11. Similarly, a second inorganic insulating film 16 (not shown) and a second alignment film 18 (not shown) are formed on one surface of the base material of the second substrate 12.
[0053] 8(A), the first seal portion 21c and the third seal portion 23c are formed on one surface of the base material 50 of the first substrate 11. At this time, openings are provided as injection ports 51 and 52. Furthermore, each protrusion portion 25 is formed of the same material as the third seal portion 23c.
[0054] Next, the base material 50 of the first substrate 11 and the base material (not shown) of the second substrate 12 are aligned, overlapped, and bonded together. After that, a cutting line (crack) is made in the bonded base materials, and then the bonded base materials are cut along the cutting line to obtain a cell formed by bonding the first substrate 11 and the second substrate 12 together (see FIG. 8(B)).
[0055] Next, the second seal portion 22 is formed as shown in FIG. 8(C). Here, a vacuum injection method is used. Specifically, the cell is placed in a vacuum chamber, and the vacuum chamber is made low pressure, after which the injection port 52 is placed so as to contact the sealing material in the injection tank 54. The vacuum chamber is then returned to atmospheric pressure, and the sealing material is injected from the injection port 52. After the injection, the second seal portion 22 is completed by appropriately performing a heat treatment or a light irradiation treatment.
[0056] Next, as shown in FIG. 8(D), the injection port 51 of the cell is placed in contact with the liquid crystal material in an injection tank 53 by vacuum injection, and the liquid crystal material is injected from the injection port 51 to form the liquid crystal layer 19.
[0057] 8(E) and 8(F), the material of each of the sealants 26, 27, and 28 is applied to a predetermined position, and then the material is cured by light irradiation or the like to form each of the sealants 26, 27, and 28. Thereafter, the entire cell is appropriately cleaned, and the liquid crystal element 100c is completed.
[0058] According to the third embodiment as described above, moisture resistance similar to that of the above-mentioned embodiments can be obtained. In addition, a secondary effect of improving vibration resistance can be obtained. Furthermore, according to the third embodiment, the portion of the second seal portion 22 exposed to the outside can be reduced, so that moisture resistance can be improved.
[0059] (Fourth embodiment) 9 is a schematic plan view showing the configuration of a liquid crystal element of the fourth embodiment. The liquid crystal element 100d of the fourth embodiment basically has the same configuration as the liquid crystal element 100a of the first embodiment, and mainly differs in that the injection port 51 is omitted, and therefore the sealants 26, 27 are also omitted, and the part of the third seal portion 23d opposite to the injection port 52 is closed. In this case, the second seal portion 22 is formed by a vacuum injection method, and the liquid crystal layer 19 is formed by an ODF (One Drop Fill) method. In the following, the description of the common points of the configuration with the liquid crystal element 100a of the first embodiment will be omitted, and the different points of the configuration will be mainly described.
[0060] The first seal portion 21d does not have an opening such as an injection port, and is provided to form a closed space surrounding the liquid crystal layer 19. The third seal portion 23d has an opening 52 (see FIG. 10(A)), and is provided with a gap between it and the first seal portion 21d. The cross-sectional structure of the seal portion 20d including these is similar to that of the first embodiment (see FIGS. 2(A) and 2(B)).
[0061] 10(A) to 10(D) are diagrams for explaining an example of a method for manufacturing a liquid crystal element of the fourth embodiment. As in the first embodiment, a first conductive film 13 and a second conductive film 14 (not shown) are formed in advance on a pair of substrates that serve as the base materials of the first substrate 11 and the second substrate 12, respectively. In addition, a first inorganic insulating film 15 (not shown) and a first alignment film 17 are formed on one surface side of the base material 50 of the first substrate 11, and a second inorganic insulating film 16 (not shown) and a second alignment film 18 (not shown) are formed on one surface side of the base material of the second substrate 12.
[0062] 10(A), the first seal portion 21d and the third seal portion 23d are formed on one surface side of the base material 50 of the first substrate 11. At this time, an opening is provided as the injection port 52. In addition, each protrusion portion 25 is formed from the same material as the third seal portion 23d.
[0063] 10(B), a liquid crystal material is dropped into the space surrounded by the first seal portion 21d by the ODF method or the like to form a liquid crystal layer 19. Next, the base material 50 of the first substrate 11 and the base material (not shown) of the second substrate 12 are aligned, overlapped, and bonded together. After that, a cutting line (crack) is made in the bonded base materials, and then the bonded materials are cut along the cutting line to obtain a cell formed by bonding the first substrate 11 and the second substrate 12 together.
[0064] Next, the second seal portion 22 is formed as shown in Fig. 10(C). Here, similar to the third embodiment described above, a seal material is injected by vacuum injection using an injection tank 54. Thereby, the second seal portion 22 is completed.
[0065] 10(D), a material for the sealant 28 is applied to a predetermined position, and then the material is cured by light irradiation or the like to form the sealant 28. Thereafter, the entire cell is appropriately cleaned, and the liquid crystal element 100d is completed.
[0066] According to the fourth embodiment as described above, moisture resistance similar to that of the above-mentioned embodiments can be obtained. In addition, a secondary effect of improving vibration resistance can be obtained. Furthermore, according to the fourth embodiment, the portion of the second seal portion 22 exposed to the outside can be reduced, so that moisture resistance can be improved.
[0067] Fifth embodiment 11 is a schematic plan view showing the configuration of a liquid crystal element of the fifth embodiment. The liquid crystal element 100e of the fifth embodiment basically has the same configuration as the liquid crystal element 100a of the first embodiment, and is mainly different in that the injection ports 51 and 52 are omitted, and the first seal portion 21e and the third seal portion 23e together form a closed space, and the sealants 26, 27, and 28 are also omitted accordingly. In this case, both the second seal portion 22 and the liquid crystal layer 19 are formed by the ODF (One Drop Fill) method. In the following, the description of the common points of the configuration with the liquid crystal element 100a of the first embodiment will be omitted, and the different points of the configuration will be mainly described.
[0068] The first seal portion 21e does not have an opening such as an injection port, and is provided to form a closed space surrounding the liquid crystal layer 19. The third seal portion 23e does not have an opening such as an injection port, and is provided with a gap from the first seal portion 21e to form a closed space. The cross-sectional structure of the seal portion 20e including these is the same as in the first embodiment (see FIGS. 2(A) and 2(B)).
[0069] 12(A) to 12(C) are diagrams for explaining an example of a method for manufacturing a liquid crystal element of the fifth embodiment. As in the first embodiment, a first conductive film 13 and a second conductive film 14 (not shown) are formed in advance on a pair of substrates that serve as the base materials of the first substrate 11 and the second substrate 12, respectively. In addition, a first inorganic insulating film 15 (not shown) and a first alignment film 17 are formed on one surface side of the base material 50 of the first substrate 11, and a second inorganic insulating film 16 (not shown) and a second alignment film 18 (not shown) are formed on one surface side of the base material of the second substrate 12.
[0070] 12(A), a first seal portion 21e and a third seal portion 23e are formed on one surface of the base material 50 of the first substrate 11. Then, a liquid crystal material is dropped into the space surrounded by the first seal portion 21e by an ODF method or the like to form a liquid crystal layer 19.
[0071] Next, as shown in FIG. 12(B), a sealing material is dropped into the gap between the first seal portion 21a and the third seal portion 23e by an ODF method or the like, thereby forming the second seal portion 22.
[0072] Next, the base material 50 of the first substrate 11 and the base material (not shown) of the second substrate 12 are aligned, overlapped, and bonded together. After that, a cutting line (crack) is made in the bonded base materials, and then the bonded materials are cut along the cutting line to obtain a cell formed by bonding the first substrate 11 and the second substrate 12 together. Thereafter, the entire cell is appropriately cleaned, and the liquid crystal element 100e is completed.
[0073] According to the fifth embodiment as described above, moisture resistance similar to that of each of the above-mentioned embodiments can be obtained. In addition, a secondary effect of improving vibration resistance can be obtained. Furthermore, according to the fifth embodiment, the second seal portion 22 is not exposed to the outside, and the entire outer periphery can be surrounded by the third seal portion 23e, so that moisture resistance can be further improved.
[0074] Sixth embodiment Fig. 13 is a diagram showing the configuration of a vehicle lamp system according to a sixth embodiment. The vehicle lamp system shown in Fig. 13 is configured using liquid crystal elements 100a to 100e according to any one of the above embodiments, and includes a lamp unit (vehicle lamp) 101, a controller 102, and a camera 103. This vehicle headlamp system detects the positions of a vehicle ahead, a face of a pedestrian, etc. existing around the vehicle based on an image captured by the camera 103, sets a certain range including the position of the vehicle ahead, etc. as a non-illumination range (light reduction region), sets the other range as a light illumination range, and selectively irradiates light and irradiates light of various shapes onto the road surface.
[0075] The lamp unit 101 is disposed at a predetermined position in the front of the vehicle, and produces light for illuminating the area ahead of the vehicle. Note that, although one lamp unit 101 is provided on each of the left and right sides of the vehicle, only one is shown here.
[0076] The controller 102 controls the operation of the light source 110 and the liquid crystal element 115 of the vehicle lamp 101. The controller 102 is realized by using a computer system having, for example, a CPU (Central Processing Unit), a ROM (Read Only Memory), a RAM (Random Access Memory), etc., and executing a predetermined operation program in the computer system. The controller 102 of this embodiment turns on the light source 110 according to the operation state of a light switch (not shown) installed in the driver's seat, sets a light distribution pattern according to an object detected by the camera 103, such as a forward vehicle (oncoming vehicle, preceding vehicle), a pedestrian, a road sign, a white line on the road, etc., and supplies a control signal to the liquid crystal element 115 to form an image corresponding to the light distribution pattern.
[0077] The camera 103 captures an image of the space ahead of the vehicle and generates an image, and performs a predetermined image recognition process on this image to detect the position, range, size, type, etc. of an object such as the vehicle ahead. The detection result by the image recognition process is supplied to the controller 102 connected to the camera 103. The camera 103 is installed at a predetermined position inside the vehicle cabin (e.g., above the windshield) or at a predetermined position outside the vehicle cabin (e.g., inside the front bumper). If the vehicle is equipped with a camera for another purpose (e.g., an automatic braking system, etc.), that camera may be used in common.
[0078] The image recognition function of camera 103 may be substituted by controller 102. In that case, camera 103 outputs the generated image to controller 102, and image recognition processing is performed on the controller 102 side based on this image. Alternatively, both the image and the result of the image recognition processing based on the image may be supplied from camera 103 to controller 102. In that case, controller 102 may further perform its own image recognition processing using the image obtained from camera 103.
[0079] The lamp unit 101 shown in Fig. 13 includes a light source 110, reflectors 111 and 113, a polarizing beam splitter 112, a quarter-wave plate 114, a liquid crystal element 115, an optical compensation plate 116, a polarizing plate 117, and a projection lens 118. These elements are integrated, for example, in a single housing. The light source 110 and the liquid crystal element 115 are each connected to the controller 102. In this embodiment, the polarizing beam splitter 112 and the polarizing plate 117 correspond to the "polarizing element."
[0080] The light source 110 emits light under the control of the controller 102. The light source 110 includes a light emitting element such as a number of white LEDs (Light Emitting Diodes) and a drive circuit. The configuration of the light source 110 is not limited to this. For example, the light source 110 may be a laser element, or a light source generally used in vehicle lamp units such as a light bulb or a discharge lamp.
[0081] The reflector 111 is disposed in correspondence with the light source 110, and reflects and collects the light emitted from the light source 110, directing it toward the polarizing beam splitter 112 and causing it to enter the liquid crystal element 115. The reflector 111 is, for example, a reflecting mirror having an ellipsoidal reflecting surface. In this case, the light source 110 can be disposed near the focal point of the reflecting surface of the reflector 111. Note that a collecting lens may be used as a light collecting unit instead of the reflector 111.
[0082] The polarizing beam splitter 112 is a reflective polarizing element that transmits a polarized component of the incident light in a specific direction and reflects a polarized component in a direction perpendicular to the specific direction. For example, a wire grid polarizing element or a multilayer film polarizing element can be used as the polarizing beam splitter 112.
[0083] Reflector 113 is provided at a position where the light reflected by polarizing beam splitter 112 can be incident, and reflects the incident light in the direction of polarizing beam splitter 112 .
[0084] The quarter-wave plate 114 is disposed on the optical path between the polarizing beam splitter 112 and the reflector 113, and imparts a phase difference to the incident light. In this embodiment, the light reflected by the polarizing beam splitter 112 passes through the quarter-wave plate 114, is reflected by the reflector 113, and passes through the quarter-wave plate 114 again, causing the polarization direction to rotate by 90° and to re-enter the polarizing beam splitter 112. This allows the re-entering light to pass through the polarizing beam splitter 112, improving the light utilization efficiency.
[0085] The liquid crystal element 115 is disposed at a position where light reflected and collected by each of the reflectors 111 and 113 can be incident. The liquid crystal element 115 includes a plurality of pixel units (light modulation units) that can be controlled independently of each other. In this embodiment, the liquid crystal element 115 has a driver (not shown) for applying a drive voltage to each pixel unit. The driver applies a drive voltage to the liquid crystal element 115 for individually driving each pixel unit based on a control signal supplied from the controller 102. Any of the liquid crystal elements 100a to 100e according to the above embodiments is used as this liquid crystal element 115.
[0086] The optical compensation plate 116 is for compensating for the phase difference of the light transmitted through the liquid crystal element 115 and for increasing the degree of polarization. Note that the optical compensation plate 116 may be omitted.
[0087] The polarizing plate 117 is disposed on the light output side of the liquid crystal element 115. An image corresponding to the light distribution pattern of the light irradiated ahead of the vehicle is formed by the polarizing beam splitter 112, the polarizing plate 117, and the liquid crystal element 115 disposed therebetween.
[0088] The projection lens 118 is disposed at a position where the light reflected and collected by the reflectors 111 and 113 and transmitted through the liquid crystal element 115 can enter the projection lens 118, and projects the incident light forward of the vehicle. The projection lens 118 is disposed so that its focal point corresponds to the position of the liquid crystal layer of the liquid crystal element 115.
[0089] According to the sixth embodiment as described above, a vehicle lamp and a vehicle lamp system including a liquid crystal element having excellent moisture resistance can be obtained.
[0090] (Modification) The present disclosure is not limited to the contents of the above-mentioned embodiments, and can be modified in various ways within the scope of the gist of the present disclosure. For example, the configuration of the vehicle lighting system is not limited to the configuration of the sixth embodiment, and the liquid crystal element according to the present disclosure can be applied to any device that forms a light distribution pattern using a liquid crystal element. The liquid crystal element of each embodiment can be applied to various lighting devices (e.g., liquid crystal projectors, etc.) other than vehicle applications, and can also be applied to liquid crystal elements for general display applications. [Explanation of symbols]
[0091] 11: first substrate, 12: second substrate, 13: first conductive film, 14: second conductive film, 15: first inorganic insulating film, 16: second inorganic insulating film, 17: first alignment film, 18: second alignment film, 19: liquid crystal layer, 20: sealing portion, 21: first sealing portion, 22: second sealing portion, 23: third sealing portion, 24: conductive material, 25: protrusion portion, 26, 27, 28: sealing portion, 100a: liquid crystal element
Claims
1. A first substrate and a second substrate disposed opposite each other; A first conductive film disposed on one surface side of the first substrate; a first inorganic insulating film disposed on one surface side of the first substrate farther from the first substrate than the first conductive film; a first alignment film disposed on one surface side of the first substrate, the first alignment film being farther from the first substrate than the first inorganic insulating film; A second conductive film disposed on one surface side of the second substrate; a second inorganic insulating film disposed on one surface side of the second substrate farther from the second substrate than the second conductive film; a second alignment film disposed on one surface side of the second substrate farther from the second substrate than the second inorganic insulating film; a liquid crystal layer disposed between the first substrate and the second substrate; a seal portion disposed between the first substrate and the second substrate to surround the liquid crystal layer; Including, the sealing portion includes at least a first sealing portion and a second sealing portion in the order of proximity to the liquid crystal layer, the first sealing portion is disposed so as to cover an end portion of the first alignment film and an end portion of the second alignment film; the second sealing portion is disposed so as to be in contact with each of the first inorganic insulating film and the second inorganic insulating film; Liquid crystal element.
2. the first sealing portion is disposed so as to cover a stepped portion of an end portion of the first alignment film and to be in contact with the first inorganic insulating film, and is disposed so as to cover a stepped portion of an end portion of the second alignment film and to be in contact with the second inorganic insulating film; The liquid crystal device according to claim 1 .
3. Each of the first inorganic insulating film and the second inorganic insulating film is made of a siloxane-based material or a titanosiloxane-based material.
3. A liquid crystal device according to claim 1 or 2.
4. The material constituting the second seal portion has a relatively lower moisture permeability than the material constituting the first seal portion.
4. A liquid crystal device according to claim 1.
5. the sealing portion further includes a third sealing portion disposed at a position farther from the liquid crystal layer than the second sealing portion, the third seal portion has a conductive material in a part thereof and is arranged so that the conductive material is in contact with each of the first conductive film and the second conductive film, and is arranged so that the third seal portion is in contact with each of the first inorganic insulating film and the second inorganic insulating film in another part thereof; 5. A liquid crystal device according to claim 1.
6. the third sealing portion is disposed so as to cover an end portion of the first conductive film, an end portion of the first inorganic insulating film, an end portion of the second conductive film, and an end portion of the second inorganic insulating film in the other part. The liquid crystal device according to claim 5 .
7. The first seal portion and the third seal portion are made of the same material.
7. A liquid crystal device according to claim 5.
8. the first seal portion and the third seal portion are in close contact with the second seal portion in a direction substantially perpendicular to a thickness direction of the liquid crystal layer; The liquid crystal device according to any one of claims 5 to 7.
9. A liquid crystal element according to any one of claims 1 to 8, a pair of polarizing elements disposed opposite to each other with the liquid crystal element therebetween; a light source that causes light to be incident on the liquid crystal element; 13. A lighting device comprising:
10. A vehicle lamp comprising the lighting device according to claim 9.
Citation Information
Patent Citations
Packaging structure and method of display panel
CN105549272A
JP1978108945U
Formation of moistureproof film for substrate
JP1982038415A
Liquid crystal display device
JP1982181527A
Manufacture of liquid crystal display device
JP1985026321A