Decomposition of struvite

The method decomposes struvite using mineral acids to separate magnesium and adjust pH, enabling efficient recovery of nitrogen and reuse of magnesium and phosphorus, addressing inefficiencies in existing struvite recovery methods and producing a more soluble fertilizer.

JP7590994B2Active Publication Date: 2024-11-27EASYMINING SWEDEN AB
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021573517
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-06-17
Filing Date
2020-06-11
Publication Date
2024-11-27
Estimated Expiration
2040-06-11

AI Technical Summary

Technical Problem

Current methods for recovering nitrogen, phosphorus, and potassium from wastewater are inefficient, costly, and energy-intensive, with struvite precipitation focused primarily on phosphorus recovery and resulting in low-value fertilizers due to high magnesium content and poor solubility, and existing struvite decomposition methods fail to regenerate calcium or potassium struvite effectively.

Method used

A method and apparatus for decomposing struvite using mineral acids to dissolve and separate magnesium, followed by pH adjustment to precipitate ammonium salts, allowing for the recovery of nitrogen and reuse of magnesium and phosphorus sources, suitable for various struvite compositions, including calcium and potassium forms.

Benefits of technology

The method enables cost-effective recovery of ammonium salts from struvite, recycling magnesium and phosphorus for repeated nitrogen precipitation, and produces a more soluble fertilizer product by separating magnesium, thus improving nutrient recovery efficiency and reducing energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007590994000001
    Figure 0007590994000001
  • Figure 0007590994000002
    Figure 0007590994000002
  • Figure 0007590994000003
    Figure 0007590994000003
Patent Text Reader

Abstract

A method for decomposing struvite includes dissolving a feed material comprising struvite in a mineral acid (S10), thereby producing a solution having an acidic pH. Magnesium is removed from the solution (S30). Magnesium is removed by increasing the pH of the solution to a pH in the range of 4.5 to 6 (S32), precipitating ammonium-free magnesium compounds (S34), and separating the precipitated magnesium compounds from the solution (S36). The resulting solution contains ammonium salts of the mineral acid. Apparatus for carrying out such a method is also disclosed. Additionally, methods and apparatus for recovering at least nitrogen from waste materials based on the decomposition of struvite are disclosed.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present technology relates generally to methods and apparatus for the chemical processing of struvite, and more particularly to methods and apparatus for decomposing struvite to recover at least ammonia from the struvite molecule. [Background technology]

[0002] Nitrogen is a nutrient essential for life and consumed in large quantities by all living organisms. Ammonia is synthesized on a large scale by the fertilizer industry. Approximately 100 Mt of reactive nitrogen are synthesized annually worldwide using the Haber-Bosch process. This anthropogenic ammonia production is on a similar scale to natural nitrogen fixation and is estimated to be approximately 150-200 Mt of nitrogen annually on Earth.

[0003] Humans and animals excrete a significant proportion of the nutrients contained in the food they ingest. Alongside other agricultural sources, these nutrients find their way back into the environment as municipal wastewater effluents, landfill runoff from treated organic matter, agricultural food processing effluents, and more. Anthropogenic loading of nutrients is the main cause of eutrophication of the receiving water bodies. Therefore, wastewater treatment plants are necessary to treat nutrient-rich runoff.

[0004] Both the synthesis and wastewater capture processes of ammonia are energy and resource intensive. In the Haber-Bosch process, ammonia is synthesized by combining hydrogen gas and atmospheric nitrogen at temperatures and pressures of approximately 450 °C and 30 MPa, respectively. The ammonia production industry is heavily dependent on natural gas and energy as a non-renewable precursor for hydrogen. Ammonia synthesis is believed to be responsible for approximately 5% of the world's natural gas consumption. Global ammonia production accounts for 1.3% of the world's fossil fuel-derived energy use and is a significant contributor to greenhouse gas emissions.

[0005] Under typical environmental conditions, most nitrogen in wastewater is present as dissolved ammonium ions. To achieve nitrogen emission targets, wastewater treatment plants use biological nitrogen capture processes such as nitrification, followed usually by denitrification, to ultimately convert ammonia to atmospheric nitrogen.

[0006] Biological processes to extract nitrogen are expensive and complex. The engineered bacteria in such processes are sensitive to a wide range of toxic compounds. High salinity effluents cannot be treated. In addition, biological treatment implementations are very temperature-dependent and less efficient in cold climates. The engineered bacteria require long residence times, which means large bowls. Moreover, the process is also energy intensive, requiring extensive aeration to oxidize all ammonium to nitrate. Expensive sources of carbon, such as methanol, are usually required to obtain an efficient conversion of nitrate to nitrogen gas by the denitrification reaction. The process also produces significant amounts of climatic gases in the form of nitrous oxide. Eventually, the reactive nitrogen needs to be destroyed and converted back to atmospheric nitrogen, which must be recovered again by the resource-intensive Haber-Bosch process.

[0007] Current technologies for removing nitrogen from effluents are expensive and complex. In addition to biological treatment, alternative methods include: a) ammonia stripping - which requires high temperature and / or high pH, ​​high capital and operating costs to treat streams containing relatively low ammonia content, b) ammonia adsorption - for example, on zeolites, which requires chemicals for regeneration, high capital and operating costs, and it is difficult to recover ammonia, and c) breakpoint chlorination - which has high operating costs due to the chemicals required, and loses nitrogen that is not recovered.

[0008] The logical consequence is that nitrogen-containing effluents should be regarded as a nitrogen source rather than a waste product and should be utilised by recovery of the nitrogen in a form that could be used by agriculture or other industries. In Sweden, environmental targets for the recovery of nitrogen from domestic wastewater have been proposed.

[0009] Phosphorus is also an important element essential for life. Its release into surface waters, and its resulting contribution to eutrophication, has led to increasing concerns about water quality. Policies have therefore been implemented worldwide to reduce the levels of phosphorus entering surface waters by implementing technologies to extract phosphorus from domestic and industrial wastewater. In contrast to nitrogen, inorganic phosphorus sources are considered to be limited and finite. In addition, most of the world's phosphorus reserves are controlled in only a few countries. Thus, there is growing interest in the recirculation and beneficial reuse of phosphorus present in domestic wastewater. Several countries have recently introduced mandatory requirements for the recovery of phosphorus from municipal wastewater.

[0010] Potassium is also a nutrient consumed in large quantities by all living organisms. Like phosphorus, potassium is extracted from limited rock deposits in mineral or salt lakes. Potassium reserves worldwide are also controlled only in a few countries. Potassium recovery is still not widely discussed in society, due to the fact that it is not a limiting nutrient in aquatic environments and therefore does not contribute to eutrophication like nitrogen and phosphorus. In addition, there is no feasible technology today to recover potassium from dilute runoff.

[0011] Precipitation of struvite from wastewater has been used to produce struvite as a fertilizer. Struvite is crystalline and occurs in equimolar concentrations of magnesium, ammonium and phosphate combined with six water molecules (MgNH4PO4·6H2O). Its molecular weight is 245.43 g per mole and it is sparingly soluble under neutral and alkaline conditions but readily soluble in acids. The ammonium ions in the struvite crystal lattice can be exchanged for other alkaline ions such as potassium or sodium. Thus, there are two further forms of struvite: a) potassium struvite (MgKPO4·6H2O), which has a molecular weight of 266.46 g per mole, and sodium struvite (MgNaPO4·6H2O), which has a molecular weight of 250.36 g per mole.

[0012] Struvite can be easily precipitated from wastewater if the ratio of magnesium to other nutrients (N+P, or K+P) is sufficient and the pH is adjusted to a neutral or alkaline level. Struvite precipitation from wastewater is easily applied in prior art practice. Applications of struvite precipitation have thus far focused primarily on phosphorus recovery. Most wastewaters contain enough ammonium to extract phosphorus as struvite, and the only addition required for struvite precipitation is usually a magnesium source.

[0013] Ammonium nitrogen is usually present in effluents at much higher concentrations than phosphorus. To extract nitrogen from wastewater in the form of struvite, large amounts of external phosphorus and magnesium are required. However, it is impractical to convert a high-quality source of phosphorus to struvite simply to recover ammonium-nitrogen. Because struvite has low commercial value, such a process would not be economically viable.

[0014] The precipitation of struvite from many different types of wastewater has been reported in the literature. Potential applications include: swine wastewater, calf manure effluent, leather tannery effluent, sewage treatment return effluent, dairy wastewater, sewage sludge digester slurry, digester supernatant, industrial wastewater, landfill leachate, lagoon effluent, poultry manure effluent, agro-industrial waste, slaughterhouse effluent, composting plant effluent, animal manure, goods processing effluent, fractionated urine, and fertilizer plant effluent.

[0015] Modern struvite precipitation has focused on the recovery of phosphorus. This is usually done by adding magnesium in the form of magnesium chloride and sodium hydroxide for pH adjustment, or magnesium hydroxide, which provides both a source of magnesium and hydroxyl ions for pH adjustment. Generally, there are two reasons for recovering struvite from domestic wastewater: the first is to solve the struvite scaling problem in wastewater treatment plants; the second is to allow recovery of phosphorus, which is a limited source.

[0016] The precipitation of struvite is usually carried out in a specific crystallizer that allows to form struvite pellets in a certain size range that can be spread on the arable land using conventional spreading equipment. The precipitated struvite is then usually used as a slow release phosphorus fertilizer. The production of struvite pellets is a complex task. The process requires a long solids residence time of 8 to 50 days, while the typical hydraulic residence time is less than 10 minutes. To keep the pellets fluidized in the reactor, a recirculation flow for the inflow of about 25% or less is necessary. The installation is complex and expensive. It is clear that if pellets are not required, struvite can be precipitated in a simple reactor with a short reaction time, followed by a simple solid-liquid separation, such as by filtration and / or centrifugal sedimentation.

[0017] The main idea behind the latest precipitation of struvite is to use it as a fertilizer. However, struvite is not an optimal fertilizer. Struvite contains too much magnesium relative to nitrogen, phosphorus or potassium. For example, according to the Food and Agriculture Organization of the United Nations, the nutrient requirements for potato crops are 1:78:5:36 in the molar ratio Mg:N:P:K. The nutrient requirements for winter wheat are 1:18:1:7 in the molar ratio Mg:N:P:K. The actual fertilizer requirements depend on the type of crop and the soil's ability to deliver, for example, magnesium or potassium due to release from clay or soil minerals. The main problem with struvite as a fertilizer is that it is not water soluble. This means that the nutrients in struvite are not readily plant available. Therefore, struvite cannot be used as a primary fertilizer, but only as an additional slow-release fertilizer for niche applications. Recently, it has been found that the plant availability of struvite is inhibited by high magnesium content in the soil. This may further limit the large-scale application of struvite as a fertilizer.For the reasons stated above, the fertilizer value, as well as the economic value of struvite in general, is low.

[0018] There is a need for methods and devices that can enable the simultaneous recovery of all the major plant nutrients: phosphorus, nitrogen and possibly potassium from wastewater. Summary of the Invention [Problem to be solved by the invention]

[0019] The general object is to provide a method and apparatus that allows for the recovery of key plant nutrients from wastewater.

[0020] The above object is achieved by methods and devices according to the independent claims. Preferred embodiments are defined in the dependent claims. [Means for solving the problem]

[0021] Generally speaking, in a first aspect, a method for decomposing struvite includes dissolving a feed material comprising struvite in a mineral acid, thereby producing a solution having an acidic pH; removing magnesium from the solution; removing magnesium by increasing the pH of the solution to a pH in the range of 4.5 to 6, precipitating ammonium-free magnesium compounds, and separating the precipitated magnesium compounds from the solution, such that the post-magnesium removal solution comprises an ammonium salt of the mineral acid.

[0022] In a second embodiment, a method for recovering at least nitrogen from a waste material comprises precipitating struvite from a first waste material solution by adding an ammonium-free magnesium compound to the first waste material solution and adjusting the pH of the first waste material solution to an alkaline pH. The precipitated struvite is separated from the first waste material solution. The separated struvite is decomposed by the method according to the first embodiment.

[0023] In a third embodiment, the apparatus for decomposing struvite comprises a dissolver arranged to dissolve a feed material comprising struvite in a mineral acid, thereby producing a solution having an acidic pH. The dissolver comprises an input for the feed material, an input for said mineral acid and an output for a solution having an acidic pH. The apparatus further comprises a magnesium removal section arranged to remove magnesium from the solution, thereby obtaining a solution comprising an ammonium salt of the mineral acid. The magnesium removal section comprises an input connected to the output for the solution having an acidic pH of the dissolver, an output for precipitated magnesium compounds, and an output for a solution comprising an ammonium salt of the mineral acid. The magnesium removal section is arranged to increase the pH of the solution from the dissolver to a pH in the range of 4.5 to 6, precipitate the ammonium-free magnesium compounds, and separate the precipitated magnesium compounds from the solution.

[0024] In a fourth aspect, the apparatus for recovering at least nitrogen from a waste material comprises a struvite precipitation device. The struvite precipitation device comprises an input for a waste priming solution and an input for an ammonium-free magnesium compound. The struvite precipitation device is arranged for mixing the waste priming solution and the magnesium compound and for adjusting the pH of the waste priming solution to an alkaline pH. This results in the struvite being precipitated. The struvite precipitation device comprises a separation device arranged for separating precipitated struvite from the waste priming solution, and an output for precipitated struvite. The apparatus further comprises a device for decomposing struvite according to the third aspect. The feed input of the dissolution reactor is connected to the output for precipitated struvite of the struvite precipitation device.

[0025] One advantage of using the proposed technology is that it provides a cost-effective method for decomposing struvite, which in turn allows for the production of useful ammonium salts using the nitrogen content in the struvite itself, while allowing for the reuse of the magnesium source for repeated nitrogen precipitation. Other advantages will be appreciated upon reading the detailed description. [Brief description of the drawings]

[0026] The invention, together with further objects and advantages thereof, will best be understood by reference to the following description taken together with the accompanying drawings, in which: [Figure 1] 1 shows a flow diagram illustrating the steps of an embodiment of a method for decomposing struvite. [Diagram 2] 1 illustrates a schematic representation of an embodiment of an apparatus for decomposing struvite. [Diagram 3] 1 shows a flow diagram of steps of an embodiment of a method for recovering at least nitrogen from a waste product. [Figure 4] 1 illustrates an embodiment of an apparatus for recovering at least nitrogen from waste. [Diagram 5] 1 shows a process flow diagram of another embodiment of a method for decomposing struvite. [Figure 6] 1 shows a process flow diagram of another embodiment of a method for decomposing struvite. [Figure 7] 1 shows a process flow diagram of another embodiment of a method for decomposing struvite. [Figure 8] 1 shows a portion of an embodiment of an apparatus for struvite decomposition. [Figure 9] 1 shows a portion of another embodiment of an apparatus for struvite decomposition. [Figure 10] 1 shows a portion of yet another embodiment of an apparatus for struvite decomposition. [Figure 11] 1 shows a flow diagram of a portion of an embodiment of a process for removing magnesium from a solution. [Figure 12]1 shows a flow diagram of part steps of another embodiment of a process for removing magnesium from a solution. [Figure 13] 13A and 13B are schematic diagrams illustrating an embodiment of a magnesium removal portion; [Figure 14] 1 shows a flow diagram of part steps of yet another embodiment of a process for removing magnesium from a solution. [Figure 15] 1 shows a flow diagram of part steps of yet another embodiment of a process for removing magnesium from a solution. [Figure 16] 13A and 13B are schematic diagrams illustrating another embodiment of the magnesium removal portion; [Figure 17] 1 shows a flow diagram of yet another embodiment of a process for removing magnesium from a solution. [Figure 18] 13A and 13B are schematic diagrams illustrating another embodiment of the magnesium removal portion; [Figure 19] 1 shows a flow diagram of a portion of another embodiment of a method for decomposing struvite. [Figure 20] 13A-13C are schematic diagrams illustrating a portion of another embodiment of an apparatus for decomposing struvite; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0027] The same reference numbers are used throughout the drawings for like or corresponding elements.

[0028] Where inexpensive sources of magnesium and phosphorus are available, there is potential for the use of struvite precipitation to recover ammonia from nutrient-rich wastewater, rather than biologically converting it back to atmospheric nitrogen.

[0029] What all prior art related to struvite decomposition has in common is that they focus exclusively on the recovery or extraction of ammonium nitrogen. There are no prior art methods that could allow the reuse of magnesium and phosphorus sources for repeated nitrogen precipitation in the form of struvite.

[0030] Therefore, there is a need for a robust process that can enable nitrogen recovery as well as decomposition of struvite to allow reuse of magnesium and phosphorus sources for subsequent ammonium nitrogen extraction where the regeneration efficiency is not affected by, for example, calcium phosphate, calcium carbonate, magnesium carbonate or potassium struvite.

[0031] There is a need for a method that can enable the recycling of magnesium and phosphorus from reactive forms of struvite, such as dimagnesium phosphate or high quality newberryite. A constant quality of the recovered magnesium and phosphorus source should be guaranteed, independent of the struvite composition and the number of repeated cycles.

[0032] There is a need for a robust method for the decomposition of struvite that is not energy intensive.

[0033] There is a need for a method of treating struvite that can obviate the need to precipitate struvite in the form of pellets in dedicated fluidized bed reactors, which require high capital and operating costs during wastewater treatment.

[0034] What is needed is a method for the decomposition of struvite that has a favorable mass balance in which input chemicals are converted to end products.

[0035] There is a need for a process that allows for the recovery of ammonia in different ammonium salt forms.

[0036] What is needed is a cost-effective method for the decomposition of struvite that allows for the production of useful ammonium salts using the nitrogen content in the struvite itself, while at the same time allowing for the reuse of magnesium and phosphorus sources for repeated nitrogen precipitation.

[0037] According to this technology, an inexpensive source of magnesium and phosphorus can be derived from the struvite molecule itself, which can then be used to precipitate struvite from the water eluate, allowing the recovery of ammonium bound within the struvite but derived from the water eluate.

[0038] There have been several attempts in the literature to provide a method for the decomposition of struvite that allows the recovery or extraction of ammonia.

[0039] Extensive research has been devoted to the pyrolysis of struvite, which allows the liberation of ammonia from struvite by heating, for example by Stefanowicz et al. 1992. The main drawback of this approach is that after pyrolysis of struvite, magnesium pyrophosphate residues are produced that are not effective for the precipitation of ammonium nitrogen from wastewater.

[0040] The thermal decomposition of struvite occurs in several stages. In the first stage, ammonium struvite (MgNH4PO4·6H2O) is converted to zidmarite (MgNH4PO4·H2O) by removal of water. Zidmarite is more thermally stable than struvite. Further heating of the resulting zidmarite results in the liberation of additional water and ammonia, ultimately forming magnesium pyrophosphate (Mg2P2O7).

[0041] Farhana, 2015 proposed pyrolysis of ammonium struvite in a fluidized bed reactor, maintaining fluidization of the struvite pellets in the reactor for 2-4 hours at a temperature of 85 °C and 95% relative humidity. The aim was to decompose the struvite to dimagnesium phosphate instead of magnesium pyrophosphate by having a relatively low temperature and high humidity. The drawbacks of this method include high complexity due to the need for struvite pellets of a certain size and hardness to maintain fluidization. The conversion of struvite to dimagnesium phosphate was found to be incomplete in some of the struvite pellets tested. The hardness and size of the pellets are the main factors regarding the conversion efficiency and process operation. Soft pellets would not be treatable as they would generate dust. In addition, the process is energy intensive, requiring large amounts of hot air and steam.

[0042] Common to all thermal struvite conversion processes is that the process is not suitable for decomposition of potassium struvite or calcium phosphate. Many wastewaters contain significant amounts of dissolved potassium and calcium. This means that when struvite precipitates from such wastewaters at high pH, ​​a mixture of several forms of struvite is usually present, such as ammonium struvite (MgNH4PO4·6H2O) along with potassium struvite (MgKPO4·6H2O). The presence of dissolved calcium leads to the co-precipitation of calcium phosphate with struvite. Since thermal struvite regeneration is based on the thermal extraction of gaseous ammonia, it is not possible to regenerate calcium phosphate or potassium struvite. This means that if the struvite decomposition products from the thermal process are reused in wastewater treatment, the efficiency will decrease rapidly over time due to the accumulation of calcium and potassium in the residue, which cannot be regenerated.

[0043] Zhang, S. et al. 2004 proposed a method to decompose ammonium struvite in hot hydrochloric acid solution at a pH of 4-5.5. The principle was to convert struvite to dimagnesium phosphate based on the fact that dimagnesium phosphate has low solubility compared to struvite at slightly acidic pH and temperatures above 25°C. The drawbacks of this method include the low efficiency of recrystallization of struvite to dimagnesium phosphate. In addition, the method cannot regenerate phosphorus from co-precipitated calcium phosphate because the solubility of calcium phosphate is much lower than dimagnesium phosphate at acidic pH. Furthermore, high phosphorus solubility at low pH results in significant phosphorus loss in each regeneration cycle. In addition, the recrystallization conditions by Zhang et al. result in a very dilute ammonium chloride solution with a nitrogen concentration of only about 7 grams per liter, which is expensive to transport.

[0044] Zhang, T. et al. 2009 tested the thermal decomposition of ammonium struvite in hot alkaline aqueous solution. The idea was to first liberate ammonia into the aqueous solution which produces trimagnesium phosphate. The ammonia in hot alkaline solution can be converted to gas and separated. The method has some drawbacks. The conversion of struvite to trimagnesium phosphate was found to be incomplete. The method cannot regenerate phosphorus from the co-precipitated calcium phosphate because calcium phosphate is not soluble in alkaline solution, which means that the decomposition products are gradually blocked with calcium, reducing its efficiency.

[0045] Huang et al. 2015 proposed a method to decompose struvite to produce dimagnesium phosphate by adding sodium hypochlorite. The main drawback of the method is that nitrogen cannot be recovered and is lost in the form of nitrogen gas. In addition, the method has high operating costs, and like others, the struvite decomposition method cannot regenerate either potassium struvite or calcium phosphate, which reduces the efficiency of the decomposition products when used repeatedly in real wastewater.

[0046] Huang et al. 2015 further proposed a method for decomposing struvite by using microwave irradiation. Struvite is mixed with sodium hydroxide and treated with microwave irradiation to liberate ammonia and convert struvite into sodium magnesium phosphate compounds, which are claimed to be reactive for aqueous ammonia removal by struvite precipitation. The disadvantages of this method include high operating costs and high capital requirements, complex equipment requirements, and large amounts of sodium hydroxide requirements. In addition, the method is not suitable for regenerating potassium struvite or calcium phosphate, resulting in poor ammonia removal capacity over time.

[0047] Hao et al., 2011 proposed an electrochemical decomposition method for struvite. The main drawback is that nitrogen cannot be recovered and is lost in the form of nitrogen gas, and it requires high capital and operating costs.

[0048] However, according to the technology provided herein, a mineral acid is used to dissolve the struvite. The acidic solution is preferably free of calcium in the first place. The magnesium and preferably also at least a major portion of the phosphate components are then separated from the ammonium. The extracted ammonium is provided in a commercially attractive form. The separated phosphorus and magnesium can be reused, for example, in wastewater applications. There are many attractive solutions with different fractionation methods.

[0049] FIG. 1 shows a flow diagram illustrating the steps of an embodiment of a method for decomposing struvite. In step S10, a feed material comprising struvite is dissolved in a mineral acid. This dissolution results in the production of a solution having an acidic pH. The solution so produced is usually a clear solution, but may show some precipitated compounds as described herein below. This acidic solution comprises phosphate ions, magnesium ions and ammonium ions. All common mineral acids can be used in this regard.

[0050] The dissolution of struvite in sulfuric acid occurs according to the following chemical reaction: 2NH4MgPO4·6H2O+3H2SO4 → 2H3PO4+(NH4)2SO4+2MgSO4+12H2O Sulfuric acid is produced as a by-product from several industrial processes, such as the smelting of copper sulfide ores, the smelting of iron sulfide ores, and others.

[0051] Since sulfuric acid is an unavoidable by-product of the manufacture of several useful products, the manufacture of such products is often limited by finding an outlet for the by-product sulfuric acid. Usually, this is solved by industrial symbiosis, i.e., the by-product sulfuric acid is used as a raw material in the manufacture of another product.

[0052] The dissolution of struvite in hydrochloric acid occurs according to the following chemical reaction:

[0053] NH4MgPO4·6H2O+3HCl → H3PO4+NH4Cl+MgCl2+6H2O

[0054] Hydrochloric acid is produced as a by-product from several industrial processes such as the chlor-alkali industry, vinyl chloride production, polytetrafluoroethylene production, PVC incineration, sodium sulfate production, potassium sulfate production, chlorine combustion, perchloroethylene production, dichloromethane production, trichloroethylene production, and as a by-product of the phosgene-polyurethane chain.

[0055] Since hydrochloric acid is an unavoidable by-product of the manufacture of several useful products, the manufacture of such products is often limited by finding an outlet for the by-product hydrochloric acid. Usually, this is solved by industrial symbiosis, i.e., the by-product hydrochloric acid is used as a raw material for the manufacture of other products such as calcium chloride, magnesium chloride, etc.

[0056] The dissolution of struvite in nitric acid occurs according to the following chemical reaction: NH4MgPO4·6H2O+3HNO3→ H3PO4+NH4NO3+Mg(NO3)2+6H2O

[0057] Nitric acid is a desired component in fertilizers. The dissolution of struvite in phosphoric acid occurs according to the following chemical reaction: NH4MgPO4·6H2O+3H3PO4→ NH4H2PO4+H3PO4+Mg(H2PO4)2+6H2O As mentioned in the introduction, struvite rarely precipitates in the pure form of ammonium struvite: wastewaters usually contain significant amounts of calcium, potassium and carbonates, which lead to significant co-precipitation of calcium phosphate, calcium carbonate, potassium struvite, and magnesium carbonate.

[0058] According to the present technique, said co-precipitation can be easily removed or does not interfere with the struvite processing process, which makes the method according to the present invention a robust technique capable of processing a mixture of different struvite precipitates originating from different applications and therefore having different chemical compositions in a single central plant, which is illustrated by the different preferred embodiments.

[0059] In one embodiment, such as the embodiment shown in Figure 1, the method may include an optional step S20 in which Ca is removed from the acidic solution. This optional embodiment is shown in dotted lines. This embodiment is preferred when the feed material further comprises a calcium compound. In such a case, the feed material dissolving step S10 further comprises at least temporarily dissolving the calcium compound in solution. This removal of calcium from the acidic solution S20 is performed prior to removing magnesium and phosphorus from solution, as further described below.

[0060] In sub-step S22, the calcium compounds are precipitated from the solution. In sub-step S24, the precipitated calcium compounds are filtered from the solution. The details of these steps may vary somewhat depending on the actual mineral acid used, which is described further below.

[0061] The precipitated struvite may contain some acid insoluble components, such as sand, etc. Therefore, the non-insoluble residue is separated using any suitable solid-liquid separation technique, such as filtration, centrifugation, centrifugal sedimentation, etc. This can be done prior to or in combination with step S20, if any.

[0062] Some organic material can also co-precipitate with struvite, so some dissolved organic matter can enter the struvite leachate. Therefore, it is preferable to separate the dissolved organic matter from the struvite leachate. There are several options for separation of the dissolved organic matter, such as adsorption onto activated carbon, chemical oxidation, coagulation, and others.

[0063] According to the techniques presented herein, the dissolution of struvite is preferably carried out in a manner that allows the production of a leachate having the highest possible concentration. The production of a concentrated solution during the dissolution of struvite allows the efficient recovery of salts from the mineral acid in the form of a fertilizer.

[0064] To this end, in a preferred embodiment, a portion of the leachate after the dissolution treatment is back-bled, as indicated by arrow S29 in Figure 1, i.e., a portion of the leachate is recycled and utilized as additional solvent in the subsequent dissolution step. Experiments have shown that a bleed back of 20% of the leachate can lead to a doubling of the phosphate concentration in the leachate when using sulfuric acid, compared to the no-bleed-back approach. A bleed back of 30% results in almost 2.5 times the final phosphate concentration.

[0065] That is, in a preferred embodiment, a part of the solution after the calcium removal step is fed back to S29 and added in the subsequent feed material dissolution step.

[0066] In a preferred embodiment, the amount of bleed back in step S29 is controlled to obtain a final phosphate concentration after calcium removal step S20 of at least 1 molar.

[0067] After pretreatment, the struvite leachate is ready for chemical treatment.

[0068] Thus, depending on the composition of the co-precipitate, the struvite leachate will contain at least the following elements in soluble form: ammonium and magnesium, as well as the anions corresponding to the mineral acids used.

[0069] The main advantage of this technology is that the struvite entering the treatment plant does not need to be in the form of pellets as in, for example, state-of-the-art struvite precipitation technology. The main reason for this is that the idea is not to spread struvite on agricultural land, but instead to dissolve it in mineral acid. Since no pellets are required, the struvite precipitation process can be carried out in a simple and low-cost manner. The struvite can be precipitated in a simple reactor with a short reaction time, followed by a simple solid-liquid separation, such as by filtration and / or centrifugal sedimentation.

[0070] Returning now to FIG. 1, in step S30, magnesium is removed from the acidic solution. In the embodiment of FIG. 1, the removal comprises several sub-steps. In step S32, the pH of the solution is increased to a pH in the range of 4.5 to 6. The ammonium-free magnesium compounds are precipitated in step S34. In step S36, the precipitated magnesium compounds are separated from the solution. This means that after the magnesium removal step S30, the solution comprises ammonium salts of mineral acids.

[0071] In one embodiment, the dissolution of struvite may not be completely complete. It has been found that the recrystallization of struvite to newberryite may occur even before complete dissolution of the solid portion occurs. This can be explained as if the dissolution step S10 of the feed material and the precipitation step S34 of the ammonium-free magnesium compounds occur at least partially simultaneously. The struvite dissolves and the phosphate and magnesium ions instantly precipitate with hydrogen instead of the ammonium ions.

[0072] The overall reaction can be roughly written as follows: NH4MgPO4·6H2O(s)+Hac(aq) → MgHPO4·3H2O(s)·+3H2O+NH4Ac(aq), In the formula, Ac is a mineral acid anion.

[0073] This example is further described below.

[0074] If calcium is present in the solution and sulfuric acid is used or otherwise added for dissolution, gypsum will precipitate along with the newberyite. As described elsewhere, if this newberyite is reused to generate new struvite, for example by exposure to wastewater, the gypsum will gradually concentrate. In such cases, it may therefore be necessary to completely dissolve the struvite from time to time in order to be able to remove the gypsum. An alternative method may be to use a leach stream to keep the gypsum content limited.

[0075] The solutions of ammonium salts of mineral acids may be used as end products or as feed chemicals to other processes, however, in order to take advantage of the fertilizing properties of these salts, it is preferred to convert the salt solutions into solid end products.

[0076] That is, as indicated by optional step S50, the ammonium salt of the mineral acid is solidified from solution.

[0077] Fig. 2 shows a schematic diagram of an embodiment of an apparatus 1 for decomposing struvite. In this embodiment, the apparatus 1 for decomposing struvite comprises a dissolver 10 and a magnesium removal section 30. The dissolver 10 is arranged for dissolving a feed material 13 comprising struvite in a mineral acid 15, thereby generating a solution having an acidic pH 17. The dissolver 10 comprises an input 11 for receiving the feed material 13 comprising struvite. The dissolver 10 also comprises an input 14 for receiving the mineral acid 15. The dissolver 10 further comprises an output 18 for an acidic solution comprising dissolved struvite 19. The dissolver 10 is thereby configured to mix the struvite of the feed material 13 and the mineral acid 15 for causing said dissolution of the struvite.

[0078] In a preferred embodiment, a pretreatment of the dissolution solution is performed to prepare the solution for the next operational step. Particularly in applications where the feed material further comprises calcium compounds, separation of undesired substances may be important. In such cases, the dissolver 10 further dissolves, at least temporarily, the calcium compounds in the solution. The dissolver 10 preferably further comprises a calcium removal section 20 arranged to remove calcium from the acidic solution. The calcium removal section 20 comprises a means for causing precipitation of calcium compounds 22 from the solution, and a filter 24 for filtering the precipitated calcium compounds from the solution. The filter 24 can also be used to filter out other insoluble substances, such as sand, which may have contained struvite.

[0079] In a further preferred embodiment, the dissolver 10 may include an organic compound removal device. Organic compounds may be removed, for example, by the use of activated carbon, chemical oxidation, or other methods as are known in the art. This allows additional materials to be added to the dissolver 10 or impurities to be removed.

[0080] As further noted above, a backbleed of the solution is usually advantageous, although not necessarily required. Thus, in a preferred embodiment, a backbleed connection 60 is provided as part of the dissolver features. The backbleed connection 60 is arranged to recycle a portion 61 of the solution exiting the calcium removal section 20 for use in subsequent struvite dissolution. Typically, the backbleed portion 61 re-enters the dissolver 10 along with the mineral acid 15 through the input 14. Alternatively, the backbleed may comprise a separate input into the dissolver 10.

[0081] That is, a feedback connection is provided between the output for the filtered solution of the calcium removal section and the input to the dissolver for adding a portion of the filtered solution to be added for subsequent dissolution of the feed material.

[0082] The precipitation tank 40 is configured to precipitate magnesium compounds 43 from the incoming solution by increasing the pH of the solution. The precipitation tank 40 comprises a separation device 48 for separating the precipitated magnesium compounds 43 from the remaining solution. The precipitation tank 40 comprises an input 41 for a solution connected directly or indirectly to the output 24 for the solution after phosphate ion extraction 25 of the phosphate ion removal section 20. The precipitation tank 40 also comprises an input 44 for a pH adjusting substance 45. The precipitation tank 40 further comprises an output 42 for the precipitated magnesium compounds 43 and an output 46 for a solution comprising ammonium sulfate 47.

[0083] The device 1 for decomposing struvite further comprises a magnesium removal section 30 arranged to remove magnesium from the solution, thereby producing a solution 39 comprising an ammonium salt of a mineral acid. The magnesium removal section 30 comprises an input 31 connected to the output 18 for a solution having an acidic pH of 17 from the dissolver 10. The magnesium removal section 30 further comprises an output 32 for precipitated magnesium compounds 41 and an output 38 for a solution 39 comprising an ammonium salt of a mineral acid. The magnesium removal section 30 is arranged to increase the pH of the solution from the dissolver 10 to a pH in the range of 4.5 to 6, precipitating the ammonium-free magnesium compounds. The magnesium removal section 30 is further arranged to separate the precipitated magnesium compounds from the solution, for example by means of a filter 42. Different embodiments of such devices will be further described below.

[0084] In a preferred embodiment, the device 1 for decomposing struvite is also arranged for processing a salt solution. In such an embodiment, the device 1 for decomposing struvite comprises a terminal solidification device 50 connected to an output 38 for a solution 39 comprising an ammonium salt of a mineral acid of the magnesium removal section 30. The terminal solidification device 50 is arranged to crystallize the ammonium salt of a mineral acid from the solution. The terminal solidification device 50 comprises an output 52 for a solid product 51 of the ammonium salt of a mineral acid.

[0085] The method and apparatus of Figure 1 can be operated as such for the general decomposition of struvite to decompose it into useful materials comprising the components phosphorus, typically in the form of a magnesium or ammonium compound, nitrogen, typically in the form of an ammonium salt, and magnesium, typically in the form of a phosphate compound.

[0086] As further described below, a preferred method of separating at least a portion of the magnesium and phosphorus from the struvite leach solution is by precipitation of magnesium compounds.

[0087] The magnesium content is thus made available and is preferably reused as a source of magnesium for wastewater treatment or reintroduced into the process at some other point, as described below, but may also be converted into other products of commercial interest.

[0088] However, struvite decomposition can also be carried out as part of other industrial processes. As mentioned in the background, some wastewater treatment approaches extract nitrogen and phosphorus by struvite precipitation. By utilizing the struvite decomposition presented above, such wastewater treatment can be further developed to be more economical and efficient, especially if the separated magnesium product can be reused for struvite precipitation.

[0089] Figure 3 shows a flow diagram of the steps of an embodiment of a method for recovering at least nitrogen from a waste product. In step S1, struvite is precipitated from the waste product liquor. This is done by adding a magnesium source to the waste product liquor and adjusting the pH of the waste product liquor to an alkaline pH. In step S2, the precipitated struvite is separated from the waste product liquor. In step S3, the separated struvite is decomposed. This is preferably done by a method according to that described herein above.

[0090] That is, an embodiment of a method for recovering at least nitrogen from a waste material includes precipitating struvite from the waste material priming solution by adding an ammonium-free magnesium compound to the waste material priming solution and adjusting the pH of the waste material priming solution to an alkaline pH, separating the precipitated struvite from the waste material priming solution, and decomposing the separated struvite by methods following procedures disclosed elsewhere in this disclosure.

[0091] Preferably, at least a portion of the precipitated ammonium-free magnesium compound in the decomposition step of the separated struvite is used as at least a portion of the added ammonium-free magnesium compound in the subsequent step of precipitating struvite from the initial waste liquid, so that magnesium can be recycled in the system without being consumed, and thus magnesium contributes to the extraction of nitrogen in the form of ammonium, but can later be recovered from the produced struvite and used for the next nitrogen extraction operation.

[0092] In one embodiment, the ammonium-free precipitated magnesium compound comprises newberryite.

[0093] It has further been found that when struvite crystals are added to the waste along with other magnesium compounds, the use of magnesium compounds can significantly improve the kinetics of struvite precipitation from the waste, and these struvite provided to the waste priming solution therefore act as seeds.

[0094] As considered above, the calcium provided with the struvite may be removed, for example precipitated, as gypsum and will not interfere with the rest of the process. Lime is a relatively inexpensive base and is therefore a suitable choice for adjusting the pH of the waste initial liquor. That is, the adjustment of the waste initial liquor to an alkaline pH is preferably performed by adding lime, thereby separating precipitated calcium compounds together with the precipitated struvite.

[0095] 4 likewise shows an embodiment of an apparatus 9 for recovering at least nitrogen from waste. In this embodiment, the apparatus 9 for recovering at least nitrogen from waste comprises a struvite precipitation apparatus 2, herein in the form of a waste treatment tank, and an apparatus 1 for decomposing struvite. Preferably, the apparatus 1 for decomposing struvite is arranged according to any of the embodiments of the apparatus for decomposing struvite presented in the present disclosure.

[0096] The struvite precipitator 2 comprises an inlet 3 for the waste initial solution 135. The struvite precipitator 2 also comprises an inlet 5 for a magnesium source 136. Depending on the type of magnesium source 136, it may also be necessary to provide an inlet 4 for a base 137, if necessary. Of course, the inlets 4 and 5 may be arranged as one common inlet. The struvite precipitator 2 is configured to precipitate struvite 100 from the waste initial solution 135. This is done by adding a magnesium source 136 and adjusting the pH of the waste initial solution 135 to an alkaline pH. For example, when magnesium hydroxide is used, this pH adjustment may be performed by the magnesium source. For other magnesium sources, such as newberryite, for example, an additional base 137 may be added to adjust the pH. As mentioned above, lime is a cheap base and calcium is easily separated as gypsum in a continuous process.

[0097] In one embodiment, the struvite precipitator 2 is equipped with an input for lime to make it possible to adjust the pH of the waste initial solution 135 to an alkaline pH.

[0098] The struvite precipitator 2 comprises a separation device 7 configured to separate precipitated struvite 100 from a waste priming solution 135. The struvite precipitator 2 comprises an outlet 8 for a waste priming solution 138 separated from the precipitated struvite 100, and an outlet 6 for the precipitated struvite 100.

[0099] That is, an embodiment of the apparatus for recovering at least nitrogen from a waste product comprises a struvite precipitator and an apparatus for decomposing struvite. The struvite precipitator comprises an input for a waste priming solution and an input for an ammonium-free magnesium compound. The struvite precipitator is arranged for mixing the waste priming solution and the magnesium compound and for adjusting the pH of the waste priming solution to an alkaline pH, whereby struvite precipitates. The struvite precipitator comprises a separation device arranged for separating precipitated struvite from the waste priming solution, and an output for precipitated struvite.

[0100] The apparatus for decomposing struvite is arranged according to the principles presented elsewhere in this disclosure: the feed input of the dissolution reactor is connected to the output for precipitated struvite of the struvite precipitation apparatus.

[0101] Preferably, the output for precipitated magnesium compounds of the magnesium removal section is connected to the input for ammonium-free magnesium compounds of the struvite precipitation unit in order to use at least a portion of the precipitated ammonium-free magnesium compounds produced in the unit for decomposing struvite in the subsequent struvite precipitation. In one embodiment, such magnesium compounds comprise newberryite.

[0102] Additionally, similar to that described herein above, the struvite precipitator 2 preferably includes an input for adding struvite to the waste priming stream for use as a seed.

[0103] Preferably, the struvite precipitator includes an input for adding a calcium compound to effect pH adjustment, thereby separating any precipitated calcium compounds along with the precipitated struvite.

[0104] As described in more detail below, at least a portion of the magnesium compounds 41 removed during decomposition of struvite in the apparatus for decomposing struvite 1 may be reused as at least a portion of the magnesium source 136 entering the struvite precipitation apparatus 2, thereby providing a magnesium recycle connection 99 from the apparatus for decomposing struvite into the waste treatment tank 2.

[0105] Step S20 of the preferred embodiment of Figure 1, in which Ca is removed from the acidic solution, can be carried out in different ways depending on the actual mineral acid used in the struvite dissolution. When sulfuric acid is used, sulfate ions are provided to the solution and, as a result, calcium phosphate that is co-precipitated with struvite recrystallizes in sulfuric acid in combination with calcium as gypsum according to the following formula:

[0106] Ca3(PO4)2(s)+3H2SO4→ 2H3PO4+3CaSO4(s)

[0107] The coprecipitated calcium carbonate is similarly dissolved in sulfuric acid under evolution of carbon dioxide, and the calcium precipitates as gypsum according to the following equation: CaCO3(s)+H2SO4→ CaSO4(s)+CO2↑+H2O

[0108] In such applications, step S22 can be considered a substep of the actual dissolution step S10, as shown in Figure 5. In step S10A, struvite is dissolved in sulfuric acid, thereby producing an acidic solution. In step S22A, gypsum is precipitated, and in step S24A, the precipitated gypsum is filtered.

[0109] That is, when the mineral acid is sulfuric acid, the step S10A of dissolving the feed material and the step S22A of precipitating calcium compounds occur simultaneously. The precipitated calcium compounds comprise gypsum.

[0110] The use of sulfuric acid to dissolve struvite generally leads to the solution comprising ammonium sulfate after the magnesium removal step S30.

[0111] Alternatively, other mineral acids can be used to dissolve the struvite, as described above. In embodiments where the mineral acid is at least one of hydrochloric acid, phosphoric acid, and nitric acid, any co-dissolved calcium compounds can be further removed as gypsum. Figure 6 illustrates such an embodiment. In step S10B, struvite is dissolved in at least one of hydrochloric acid, phosphoric acid, and nitric acid. In step S22B, sulfate ions are introduced by adding sulfuric acid to the already acidic solution. These sulfate ions precipitate as gypsum along with any calcium ions in solution. This selective precipitation has been tested to be operable with hydrochloric acid, phosphoric acid, and nitric acid all as the primary dissolving acids.

[0112] Preferably, the amount of sulfuric acid is adapted to the amount of calcium in the struvite feedstock, whereby the amount of sulfuric acid should be sufficient to cause precipitation of all calcium ions from the acidic solution, while at the same time keeping the excess amount of sulfuric acid low if the final product specifications are known.

[0113] That is, in embodiments where the mineral acid is at least one of hydrochloric acid, phosphoric acid, and nitric acid, the step of precipitating calcium compounds includes adding sulfuric acid, thereby precipitating said calcium compounds as gypsum.

[0114] Alternatively, in embodiments where the mineral acid comprises nitric acid, other possibilities exist for extracting Ca. Figure 7 illustrates such an embodiment. In step S10C, struvite is dissolved in nitric acid. Nitric acid solutions comprising Ca ions have a relatively high solubility for calcium nitrate at room temperature or above. However, cooling of the acidic solution reduces the solubility immediately, eventually resulting in the precipitation of calcium nitrate, which can be easily filtered out. Thus, in step S22C, the acidic solution is cooled, causing the precipitation of calcium nitrate. In step S24C, the calcium nitrate is filtered out.

[0115] That is, in the embodiment where the mineral acid is nitric acid, the step of precipitating the calcium compounds includes, after the step of dissolving the feed material S10, cooling the solution S22C, thereby causing precipitation of calcium nitrate.

[0116] The use of nitric acid to dissolve struvite generally leads to the solution comprising ammonium nitrate after the magnesium removal step S30.

[0117] The use of hydrochloric acid to dissolve struvite generally leads to the solution comprising ammonium chloride after the magnesium removal step S30.

[0118] The use of phosphoric acid to dissolve struvite generally leads to the solution comprising ammonium phosphate after the magnesium removal step S30.

[0119] The use of a different mineral acid has no influence on the detailed configuration of the apparatus. In FIG. 8, a part of an embodiment of the apparatus is shown, in which sulfuric acid is used for dissolving struvite. An input 14 provides sulfuric acid 15A to the dissolver 10. At the same time, however, any Ca is precipitated as gypsum by the sulfate ions. That is, it can be understood that dissolution of the feed material 13 takes place in the calcium removal section 20A. The means for causing the precipitation of calcium compounds 22A in this respect comprises an input 14 for sulfuric acid 15A. The precipitated calcium compounds comprise gypsum.

[0120] 9 shows a portion of another embodiment of an apparatus for struvite decomposition, where the mineral acid is at least one of hydrochloric acid, phosphoric acid, and nitric acid. An input 14 provides hydrochloric, phosphoric, or nitric acid 15B to the dissolver 10. In this embodiment, the means for causing precipitation of calcium compounds 22 includes an input 23 for adding sulfuric acid 27, thereby causing precipitation of calcium compounds as gypsum.

[0121] In Figure 10, a portion of yet another embodiment of an apparatus for struvite decomposition is shown, where the mineral acid comprises nitric acid. An input 14 provides nitric acid 15C to the dissolver 10. The means for causing precipitation of calcium compounds 22 comprises a cooling device 21 arranged to cool the solution after dissolution of the feed material 13, thereby causing precipitation of calcium nitrate.

[0122] The magnesium ions can be removed in different ways. If the magnesium ions are to be used in any particular way, the form of magnesium ion removal can be adapted to the end use of the ions. As suggested herein above, magnesium ions together with phosphate ions are necessary to cause struvite precipitation from the waste. If the available amount of phosphorus in the waste is too low, for example, compared to the nitrogen content, it may be interesting to add both magnesium ions and phosphate ions in connection with the struvite precipitation. The magnesium ions separated from the dissolved struvite can then be reused, and the form in which the magnesium ions are removed may be suitable for such recycling. In a preferred embodiment, the magnesium ions are removed by precipitation of a material comprising both magnesium and phosphate.

[0123] When the pH level of a solution containing dissolved struvite is increased by the addition of ammonia, solid material begins to precipitate when the pH exceeds a level of about 4.5. Ammonia is a natural choice since ammonium ions are already present in the solution, therefore no additional ions are introduced.

[0124] According to the literature (Abbona et al, 1982) for dilute dissolved struvite solutions having a concentration of 0.5 moles / liter or less, an increase in pH above 4.5 would result in the precipitation of newberryite. However, after Applicant's extensive experimentation, which included the addition of ammonia having a concentration of about 1 molar to dissolved struvite solutions at pH levels of 4.5 to 6, analysis of the resulting solid material indicates that it constitutes struvite, i.e., the dissolution of struvite is only reversed.

[0125] The conclusion was that it was not possible to obtain the precipitation of newberryite by adding ammonia to dissolved struvite having a concentration of 1 molar or more.

[0126] The supersaturation (β) of struvite (S) and newberyite (N) can be defined according to the following equation: β S = a(Mg 2+ )a(NH3)a(HPO4 2- ) / K SP (S) β N = a(Mg 2+ )a(HPO4 2- ) / K SP (N) where a(X) is the activity of X, and K SP is the solubility product of the species in the reaction.

[0127] From the above equation, high concentrations of ammonia favor the precipitation of struvite, in contrast to newberyite.

[0128] The disappointing experimental results obtained when increasing the pH with ammonia are most likely due to the high activity of ammonium ions in solution.

[0129] According to the literature, the supersaturation of newberyite can be increased by increasing the temperature of the solution, however, there is no information on the behavior of systems in which ammonia is added to a dissolved struvite solution at concentrations greater than 1 molar.

[0130] Therefore, applicants have experimentally tested an approach in which ammonia at high concentrations, greater than 1 molar, is added to a dissolved struvite solution accompanied by heating.

[0131] In one embodiment, the addition of ammonia is performed simultaneously with heating of the solution to a temperature of 50° C. or higher. This can be done separately or at least partially simultaneously. Surprisingly, it has been found that heating of a solution having a pH in the range of 4.5-6, which occurs with the addition of ammonia, causes precipitation of newberryite, leaving ammonia in the solution despite its high concentration. Preliminary testing has shown that the co-precipitation of any small amount of struvite is reduced even at high temperatures. At temperatures above 65° C., only trace amounts of struvite can be found, and above 80° C., the total precipitated material is essentially free of struvite, below the detection limit of the assay used.

[0132] In experiments with struvite solutions heated to 80°C, ammonia was used to increase the pH to about 5. The resulting precipitated material had an atomic ratio of P(PO4) / Mg of about 0.96, while the atomic ratio of N(NH4) / Mg was 0.01.

[0133] A minor drawback of this approach is the need for heating. However, as described further below, there are embodiments that can be combined with post-treatment of the ammonium salt solution to reduce overall energy needs. Other alternatives are also described further below.

[0134] Figure 11 shows a flow diagram of the sub-steps of an embodiment of step S30 of removing magnesium from the solution, where step S32 of increasing the pH is performed by step S33 of adding ammonia, and step S34 of precipitating the Mg compounds is performed by increasing the temperature of the solution to 50°C or higher, preferably 65°C or higher, and most preferably 80°C or higher. Steps S32 and S34 are shown to be performed separately. However, steps S32 to S35 can also be performed with at least partial overlap.

[0135] The tendency of newberyite and struvite to co-precipitate increases as the pH of the solution increases. However, this experiment shows that complete removal of magnesium from the solution could be achieved at a pH of 6. Therefore, according to the invention, the precipitation of magnesium can be preferably carried out in two stages. In the first stage, ammonia is added to a pH of 4.5 or higher, but below 6 during heating of the solution, precipitating newberyite. In the second stage, the remaining magnesium in the solution is precipitated in the form of struvite by increasing the pH to 6, and the precipitated struvite is recycled to the dissolution reactor.

[0136] In one embodiment, according to these ideas, two additional steps are provided: step S41, which occurs after separation of precipitated magnesium compounds in step S36, adds additional ammonia to further increase the pH to cause precipitation of any remaining magnesium as struvite, and step S42, which separates any precipitated struvite and preferably re-enters the subsequent struvite decomposition process as part of the starting material.

[0137] In certain embodiments, step S33 may occur after step S35, as shown in Figure 12. Step S33 then becomes a substep of step S32, which in turn becomes a substep of step S34, reducing the risk of the first formation of struvite, which must then undergo a possibly time-consuming recrystallization as newberryite.

[0138] Figure 13 shows an embodiment of magnesium removal section 30. In this embodiment, magnesium removal section 30 comprises an inlet 35 for ammonia 31 to mix with the solution to increase its pH. Magnesium removal section 30 further comprises a heating device 33 for heating said mixture of solution and ammonia, thereby causing precipitation of magnesium compounds 41. Heating device 33 is arranged such that it can heat the mixture of solution and ammonia to a temperature of 50°C or more, preferably 65°C or more, most preferably 80°C or more. A filter 42 is used to separate the precipitated magnesium compounds 41 from the remaining solution. Further preferred embodiments of heating device 33 are further described below.

[0139] If the above two-step separation approach is to be operated, inlet 35 and filter 42 can be reused to filter out remaining struvite, or a separate means for carrying out these additional steps can be provided as well.

[0140] As further mentioned above, the produced newberryite may be utilized, for example, to precipitate struvite from a waste liquor. For such applications, as well as other applications, the newberryite is preferably washed to remove impurities. However, washing with, for example, deionized water has been found to result in the re-formation of struvite. Presumably, this is due to an increase in pH resulting from the water and some residual ammonium. To avoid such struvite formation, it is preferred to wash the precipitated newberryite with an acidic wash water with a pH<5. In such cases, no conversion to struvite has been observed.

[0141] However, as briefly mentioned above, if newberryite is used, for example, to precipitate struvite from a waste liquor, some struvite acting as a seed may be effective.

[0142] In another embodiment, the step S32 of increasing the pH and the step S34 of precipitating the magnesium compound are carried out at least partially as a single process. This single process is the step S32A of adding a base other than ammonia to the solution after the filtration step. In this way, no additional ammonium ions are added to the solution and at least a portion of the magnesium and phosphorus content may be precipitated, for example, as newberryite. Even though this embodiment can essentially work in most cases, however, this embodiment has a few drawbacks that are specific to many applications. The added base may introduce additional types of ions into the solution. For example, when sodium hydroxide is added, sodium ions will remain in the solution and will be present in the final product mixed with the ammonium salt. Also, the precipitated material tends to comprise a mixture between newberryite and other compounds, for example, struvite.

[0143] In experiments with struvite solutions, the pH was increased to about 5 with NaOH at room temperature and at high concentrations of dissolved struvite, about 1 molar. The resulting precipitated material had an atomic ratio of P(PO4) / Mg of about 0.86, while the atomic ratio of N(NH4) / Mg was less than 0.01.

[0144] Thus, this type of embodiment comprises the use of hydromagnesite as an ammonia-free base. This ensures that no additional ion species are introduced into the system. The addition of hydromagnesite is believed to follow the following reaction: 10MgNH4PO4(aq)+15H2SO4(aq)+2Mg5(CO3)4(OH)2→ 10MgHPO4·3H2O(s)+8H2CO3(aq)+5(NH4)2SO4(aq)+10MgSO4(aq)

[0145] The second reaction can also produce gaseous carbon dioxide which can be released from solution, the handling of which is described later in this document.

[0146] Since magnesium is added to the system, this means that phosphorus is taken out with the newberyite along with 1 / 2 the magnesium. This therefore means that magnesium will still be present in the solution even after the removal of the newberyite. This can be additionally treated in a subsequent step using ammonia to further increase the pH. In the absence of phosphate ions, this again results in the precipitation of hydromagnesite according to: 8H2CO3(g)+5(NH4)2SO4(aq)+10MgSO4(aq)+20NH3(g)+4H2O → 2Mg5(CO3)4(OH)2(s)+15(NH4)2SO4(aq)

[0147] The precipitated hydromagnesite can then be reused in the next batch for the ammonia-free base addition step.

[0148] When carbon dioxide gas is allowed to escape from the reactor, it can be scrubbed with added ammonia, and a composted scrubbed solution of ammonium carbonate is added in parallel with the addition of ammonia to produce precipitated hydromagnesite.

[0149] 14 shows a flow diagram of the substeps of an embodiment of step S30 of removing magnesium from solution, where step S34 is performed by increasing the pH without the use of ammonia, where the Mg compounds are precipitated. The precipitated Mg compounds are separated in step S36.

[0150] Figure 15 shows a flow diagram of the partial steps of one preferred embodiment of step S30 for removing magnesium from the solution, where step S32A is performed where the pH is increased without the use of ammonia, where step S34 is performed where the Mg compounds are precipitated, and then by the addition of hydromagnesite, which precipitates newberyite which is separated in step S36.

[0151] The remaining solution still contains magnesium, and preferably step S30 also includes step S38, where ammonia is added, which results in the hydromagnesite being re-precipitated. In step S39, the hydromagnesite is removed from the solution.

[0152] In an embodiment, the recovered hydromagnesite is used in the subsequent step S37 to increase the pH of the subsequent solution as indicated by arrow S40, i.e. at least a portion of the recovered precipitated hydromagnesite is recycled in S40 for use in the subsequent step of adding ammonia-free base, i.e. step S32A.

[0153] Figure 16 shows a schematic diagram of an embodiment of magnesium removal section 30. Magnesium removal section 30 comprises an inlet 35 for an ammonia-free base to the solution. The addition of this base causes the precipitation of magnesium compounds. In a particular embodiment, inlet 35 is provided for hydromagnesite inlet 31A. Magnesium compounds 33 are precipitated and separated by filter 42 and removed through outlet 32.

[0154] In one embodiment, the magnesium removal section 30 further comprises a mixing volume 44 with an inlet 46 for the solution after separation of the precipitated magnesium compounds 32 and an inlet 48 for the ammonia 31. The mixing of the ammonia and the solution further increases the pH, thereby causing the precipitation of hydromagnesite 31A. A hydromagnesite removal device 49, e.g., a filter, is provided for removing the precipitated hydromagnesite 31A from the solution.

[0155] In one embodiment, the magnesium removal section 30 further comprises a recycle apparatus 43 arranged to recycle at least a portion of the precipitated hydromagnesite 31A removed from the hydromagnesite removal apparatus 49 to the ammonia-free base inlet 35 for use in subsequent addition of ammonia-free base.

[0156] In another embodiment, the removal of magnesium from the solution can be assisted by the addition of struvite. Figure 17 shows a flow diagram of the partial steps of one preferred embodiment of step S30 of removing magnesium from the solution. Here, step S32A is performed by increasing the pH without the use of ammonia, whereby step S34 of precipitating the Mg compounds is performed. In this embodiment, this pH increase is due to the addition of struvite S37A, which is a base. This pH increase precipitates newberryite, despite the fact that additional ammonium ions are added. The effect of the pH increase in favor of newberryite precipitation is stronger than the effect of the increased ammonium concentration. Newberryite is separated in step S36.

[0157] The remaining solution still contains magnesium, and preferably step S30 also includes step S38A, in which additional base, e.g., ammonia, is added, which results in struvite re-precipitating, removing at least a portion of the remaining phosphate and magnesium ions. In step S39A, the struvite is removed from the solution.

[0158] In an embodiment, the removed struvite is used in a subsequent step S37A to increase the pH of the subsequent solution as indicated by arrow S40, i.e., at least a portion of the removed struvite is recycled in S40 for use in a subsequent step of adding ammonia-free base, i.e., step S32A.

[0159] In the test, three different struvites were prepared; one in water, one in 0.35M (NH4)2SO4 solution and one in 2.75M (NH4)2SO4 solution. Sulfuric acid was added to reduce the pH to within the range of 3-6. It can be noticed that the ammonium nitrogen concentration in the solution is high compared to the concentration of magnesium ions or phosphate ions in the higher pH range. When lower pH values ​​are reached, the concentration of magnesium ions or phosphate ions also increases. This is interpreted as newberryite precipitates at higher pH but dissolves at lower pH.

[0160] Starting at a pH value of 3, struvite was added to the three sample slurries. The concentration of ammonium nitrogen increased, which may be considered evident as more ammonium was added. However, at the same time, both magnesium and phosphate ions decreased in solution despite the addition of these ions to the slurry. From a pH of about 4.5 to a pH of about 6, this effect intensified. This is interpreted as if the added struvite dissolved and instead reprecipitated as newberryite. This effect was also found to be present at relatively high concentrations of sulfate ions.

[0161] Thus, most of the magnesium and phosphate ions can be removed by such a procedure. However, the last small remnants of magnesium and phosphate ions may be removed by further increasing the pH, where struvite precipitation becomes prominent. At such a stage, even ammonia can be used to increase the pH. The struvite so produced can then be reused as a pH-increasing addition in an earlier step of the process.

[0162] The above experiments were carried out with sulfate ions present in solution, i.e. under conditions similar to dissolution with sulfuric acid, however similar behavior is achieved by using other mineral acids which, for example, result in relatively high concentrations of chloride, nitrate or phosphate ions.

[0163] Figure 18 shows a schematic diagram of an embodiment of magnesium removal section 30. Magnesium removal section 30 includes an inlet 35A for struvite to the solution. The addition of this base causes the precipitation of magnesium compounds, usually newberryite. The magnesium compounds 33 are precipitated and separated by filter 42 and removed through outlet 32.

[0164] In one embodiment, the magnesium removal section 30 further comprises a mixing volume 44 with an inlet 46 for the solution after separation of the precipitated magnesium compounds 32 and an inlet 48 for a base, e.g., ammonia 31. Mixing the ammonia and the solution further increases the pH, thereby causing precipitation of struvite 31B. A struvite removal device 49A, e.g., a filter, is provided to remove the precipitated struvite 31B from the solution.

[0165] In one embodiment, the magnesium removal section 30 further comprises a recirculation device 43 arranged to recirculate at least a portion of the precipitated struvite 31B removed from the struvite removal device 49A to the inlet 35A for struvite to be used in the subsequent addition of base.

[0166] As further described above, in certain embodiments, the produced newberryite may be washed according to the principles further described above.

[0167] As mentioned before, the solution of ammonium salt of mineral acid may be converted to a solid end product as described in step S50. Such crystallization can be performed in different ways, but the most straightforward approach is to evaporate the solvent, i.e., water. In Figure 19, steps of some embodiments of the method for decomposing struvite are shown. Here, the step S50 of solidifying the ammonium salt of mineral acid includes a step S52 of heating the solution after the step S30 of removing magnesium. This forms a solid product of ammonium salt of mineral acid together with the hot condensate.

[0168] In one embodiment as further described above, the temperature of the solution is increased. Since hot condensate was generated in heating step S52, this thermal energy can also be utilized for further steps. To this end, in a particular embodiment, step S35 of heating the solution, as indicated by arrow S54, includes step S37 of exchanging heat between the hot condensate generated by step S52 prior to heating the solution after step S30 of removing magnesium, and the solution.

[0169] Figure 20 shows parts of an embodiment of an apparatus for decomposing struvite; the magnesium removal section 30 and the terminal solidification device 50. The terminal solidification device 50 comprises a heating device 54 arranged to heat a solution 39 comprising an ammonium salt of a mineral acid. This produces a solid product 51 of the ammonium salt of a mineral acid, which is outputted via outlet 52. As a result of this heating, a hot condensate 55 is also produced, usually water vapor. The terminal solidification device 50 therefore also comprises an output 53 for the hot condensate 55. This embodiment works with all previously described alternatives of the magnesium removal section.

[0170] In a further embodiment, further advantages can be obtained if the magnesium removal section 30 is arranged with a heating device 33 for heating the mixture of solution and ammonia. In such an embodiment, the output 53 for the hot condensate 55 of the terminal solidification device 50 is connected to the heating device 33 for heating the mixture of solution and ammonia of the magnesium removal section 30. The heating device 33 for heating the mixture of solution and ammonia is then preferably arranged for heat exchange between the hot condensate 55 produced by previous heating of the solution in the terminal solidification device 50 and the mixture of solution and ammonia of the magnesium removal section 30. In such a method, the heat energy required in the terminal solidification device 50 can be at least partially reused in the magnesium removal section 30, thereby improving the energy efficiency. Furthermore, since the solution of the magnesium removal section 30 is heated to a temperature of at least 50° C., preferably at least 80° C., the solution 39 comprising the ammonium salt of a mineral acid is already at a high temperature and the further heating required to complete the solidification is much smaller than when operating on a cold solution.

[0171] A major advantage of the present invention is that it allows for the handling of all the co-precipitating impurities with ammonium struvite, such as calcium phosphate, calcium carbonate, magnesium carbonate and potassium struvite, as previously described.

[0172] Large amounts of co-precipitated calcium phosphate can result in a dissolved struvite solution with a phosphorus to magnesium ratio greater than 1. After removal of calcium and magnesium, the excess phosphorus ends up in the fertilizer product in the form of ammonium phosphate. Phosphorus is a desired element in fertilizers. If phosphorus is undesirable in the final product, it can be separated by known methods such as precipitation with lime, solvent extraction, etc.

[0173] Co-precipitating potassium struvite will result in potassium ions in the final fertilizer product. Potassium is a desired element in fertilizers.

[0174] In the above description, external ammonia is used to precipitate magnesium compounds, both directly and indirectly. However, according to the present idea, the ammonia used can also be recycled from a partial stream of the produced ammonium salt solution itself. In this embodiment, there is no need to add any external ammonia to the process.

[0175] In a first alternative, a partial stream of the ammonium salt solution is treated by bipolar membrane electrodialysis to recover ammonia and acid, both of which are recycled into the process. This method uses electricity instead of input chemicals.

[0176] Another alternative is to use a base to increase the pH of a partial stream of the ammonium salt solution and strip the gaseous ammonia for recycle into the process. Any type of base can be used for this purpose, such as lime, potassium hydroxide, etc. The cations of the base can be incorporated into the fertilizer product or removed from the ammonium salt solution, for example, by precipitation.

[0177] When lime is used as an ammonia stripper, it can be removed from the ammonium salt solution by precipitation as calcium sulfate or calcium phosphate after addition of appropriate reactants such as sulfuric acid or a phosphoric acid source. Addition of lime to an ammonium sulfate solution will precipitate calcium sulfate.

[0178] When nitric acid is used for struvite dissolution, lime is added to the ammonium nitrate partial stream to increase the pH and allow ammonia stripping at elevated temperatures. After ammonia stripping, the solution will consist of a mixture of ammonium nitrate and calcium nitrate, the desired fertilizer. Calcium nitrate can also be precipitated from this solution by cooling to produce a more specific ammonium nitrate fertilizer.

[0179] In the above description, the struvite is described as ammonium struvite. This is perhaps the most interesting feature of this technical discovery. However, as pointed out in the background section, other materials in the waste may also be of interest.

[0180] Similar tests were also carried out with potassium struvite, as presented above. A slurry of struvite with 0.33M K2SO4 solution was brought to a pH of 6-3 by the addition of sulfuric acid. The potassium ion concentration in the solution is already high at pH 6, while the magnesium ion and phosphate ion concentrations only increase at low pH. This indicates the precipitation of newberryite at the high pH end and its complete dissolution at lower pH values.

[0181] When potassium struvite was added to such a solution, the potassium ion concentration increased, but the magnesium ion and phosphate ion concentrations decreased with increasing pH, at least from pH 4.5 to pH 6. This indicates that the same procedure as described for ammonium struvite is also feasible for potassium struvite.

[0182] The above embodiments should be understood as a few illustrative examples of the present invention. Those skilled in the art will understand that various modifications, combinations and changes may be made to the embodiments without departing from the scope of the present invention. In particular, different part solutions in different embodiments may be combined in other configurations, where technically possible. However, the scope of the present invention is defined by the appended claims. References

[0183] Abbona F., Lundager Madsen HE, Boistelle R., 1982. Crystallization of two magnesium phosphates, struvite and newberyite: Effect of pH and concentration. J. Crystal Growth 57, 6-14. Haiming Huang, Lingyun Huang, Qingrui Zhang, Yang Jiang, Li Ding, 2015. Chlorination decomposition of struvite and recycling of its product for the removal of ammonium-nitrogen from landfill leachate. Chemosphere 136, 289-296. Haiming Huang, Jiahui Liu, Jing Xiao, Peng Zhang, and Faming Gao, 2016. Highly Efficient Recovery of Ammonium Nitrogen from Coking Wastewater by Coupling Struvite Precipitation and Microwave Radiation Technology ACS Sustainable Chem. Eng., 4 (7), pp 3688-3696. Li X.Z., Zhao Q.L., Hao X.D., Ammonium removal from landfill leachate by chemical precipitation, Waste Management, Volume 19, Issue 6, 1999, Pages 409-415. Moerman W., Carballa M., Vandekerckhove A., Derycke D., Verstraete W. 2009. Phosphate removal in agro-industry: Pilot- and full-scale operational considerations of struvite crystallization. Water Research, Vol 43, 7, 1887-1892. Siles J.A., Brekelmans J., Martin M.A., Chica A.F., Martin A., 2010. Impact of ammonia and sulphate concentration on thermophilic anaerobic digestion. Bioresource Technology, Vol 101, 23, 9040-9048. Stefanowicz, T., Napieralska-Zagozda, S., Osinska, M., Samsonowska, K., 1992. Ammonium removal from waste solutions by precipitation of MgNH4PO4II. Ammonium removal and recovery with recycling of regenerate. Resour. Conserv. Recycl. 6, 339-345. Sugiyama, S., Yokoyama, M., Ishizuka, H., Sotowa, K.I., Tomida, T., Shigemoto, N., 2005. Removal of aqueous ammonium with magnesium phosphates obtained from the ammonium-elimination of magnesium ammonium phosphate. Wilson, C.W., 2013. Ammonia recovery from municipal wastewater through a struvite formation-thermal decomposition cycle. M.A.Sc. Thesis, Department of Civil Engineering, The University of British Columbia, Vancouver, BC. Ying Hao, Sanjay Kumar, Jung Hoon Kwag, Jae Hwan Kim, Jeong Dae Kim, and Chang Six Ra, 2011. Recycle of electrolytically dissolved struvite as an alternative to enhance phosphate and nitrogen recovery from swine wastewater. Journal of Hazardous Materials 195, 175-181 Zhang, S., Yao, C., Feng, X., Yang, M., 2004. Repeated use of MgNH4PO4·6H2O residues for ammonium removal by acid dipping. Desalination 170, 27-32. Zhang, T., Ding, L., Ren, H., Xiong, X., 2009. Ammonium nitrogen removal from coking wastewater by chemical precipitation recycle technology. Water Res. 43, 5209-5215.

Claims

1. 1. A method for decomposing struvite, the method comprising: - dissolving (S10) a feed material comprising struvite (13) in a mineral acid (15), thereby producing a solution having an acidic pH; - a step (S30) of removing magnesium from the solution, said magnesium removing step (S30) comprising: - a substep (S32) of increasing the pH of said solution to a pH in the range from 4.5 to 6; - a partial step (S34) of precipitating ammonium-free magnesium compounds; - a partial step (S36) of separating the precipitated magnesium compounds from the solution, A process including Including; As a result, the solution after the magnesium removal step (S30) contains an ammonium salt of the mineral acid. method.

2. the feed material further comprises a calcium compound, whereby said dissolving (S10) of said feed material dissolves said calcium compound in said solution; A step of extracting calcium from the acidic solution (S20) prior to the magnesium removal step (S30), the calcium extraction step (S20) includes the steps of: - a partial step (S22) of precipitating calcium compounds from said solution; - a substep (S24) of filtering said precipitated calcium compounds from said solution; and further steps of the process including: The method according to claim 1 , characterized in that

3. a further step of feeding back (S29) a portion of the solution to be added to the subsequent step of dissolving the feed material (S10) after the calcium removal step (S20), The method according to claim 2 , characterized in that

4. 4. The method according to claim 3, characterized in that the feedback amount in the feedback step (S29) is controlled so as to obtain a final phosphate ion concentration after the calcium removal step (S20) exceeds 1 molar concentration.

5. the mineral acid being at least one of hydrochloric acid, phosphoric acid, and nitric acid; whereby, the step of precipitating the calcium compounds includes adding sulfuric acid (S22B) to cause precipitation of the calcium compounds as gypsum; The method according to any one of claims 2 to 4, characterized in that

6. said mineral acid being nitric acid; Thus, the calcium compound precipitation step includes, after the supply material dissolving step (S10), cooling the solution (22C) to cause precipitation of calcium nitrate; The method according to any one of claims 2 to 4, characterized in that

7. The method according to any one of claims 1 to 6, characterized in that the mineral acid is nitric acid, whereby the solution after the magnesium removal step (S30) comprises ammonium nitrate.

8. The method according to any one of claims 1 to 5, characterized in that the mineral acid is hydrochloric acid, whereby the solution after the magnesium removal step (S30) comprises ammonium chloride.

9. 6. The method according to claim 1, wherein the mineral acid is phosphoric acid, whereby the solution after the magnesium removal step (S30) comprises ammonium phosphate.

10. said mineral acid being sulfuric acid; This allows the dissolution step (S10) of the feed material and the precipitation step (S22) of the calcium compounds to occur simultaneously; whereby the precipitated calcium compound comprises gypsum; The method according to any one of claims 2 to 4, characterized in that

11. 11. The method according to any one of claims 1, 2, 3, 4 or 10, characterized in that the mineral acid is sulfuric acid, whereby the solution after the magnesium removal step (S30) comprises ammonium sulfate.

12. 12. The method according to any one of claims 1 to 11, characterized in that the step (S10) of dissolving the feed material (13) and the step (S34) of precipitating the ammonium-free magnesium compounds occur at least partially simultaneously, whereby struvite in the feed material recrystallizes into newberyite.

13. The step of increasing the pH (S32) includes adding ammonia to the solution (S31); the magnesium compound precipitation step (S34) comprises heating the solution (S33) to a temperature of 50° C. or higher, preferably 65° C. or higher, and most preferably 80° C. or higher; The method according to any one of claims 1 to 12, characterized in that

14. 14. The method of claim 13, wherein the precipitated magnesium compound comprises newberryite.

15. 15. The method of claim 14, characterized by the further step of washing the precipitated newberryite with an acidic wash water having a pH<5.

16. The magnesium removal step (S30) comprises: - adding more ammonia (S41) to the solution after the separation step (S36) of the precipitated magnesium compounds, thereby causing the precipitation of struvite; - Removing the precipitated struvite from the solution (S42); The method according to any one of claims 13 to 15, characterized in that it comprises the further step of:

17. 13. The method according to any one of claims 1 to 12, characterized in that the step of increasing the pH (S32) and the step of precipitating the magnesium compound (S34) are carried out at least partly as a one-step process, the one-step process being the addition of a base to the solution after the filtering step (S32A).

18. 18. The method of claim 17, wherein the base is struvite.

19. 20. The method of claim 18, wherein the precipitated magnesium compound comprises newberryite.

20. 20. The method of claim 19, characterized by the further step of washing the precipitated newberryite with an acidic wash water having a pH<5.

21. The magnesium removal step (S30) comprises: - adding (S38) further base to the solution after the separation step (S36) of the precipitated magnesium compounds, thereby causing precipitation of at least a portion of the remaining magnesium and phosphorus as struvite; - Removing the precipitated struvite from the solution (S39); and The method according to any one of claims 18 to 20, characterized in that it comprises the further step of:

22. 22. The method according to claim 21, characterized by the further step of recycling (S40) at least a portion of the removed precipitated struvite to be used in a subsequent step of adding (S32A) the base.

23. The method according to any one of the preceding claims, characterized by the further step of solidifying (S50) the ammonium salt of the mineral acid from the solution.

24. 24. The method of claim 23, wherein the step of solidifying (S50) the ammonium salt of the mineral acid comprises heating (S52) the solution after the magnesium removal step (S30), thereby producing a solid product of the ammonium salt of the mineral acid and a hot condensate.

25. The method of claim 25, wherein the step of increasing the pH (S32) includes adding ammonia to the solution (S31); the magnesium compound precipitation step (S34) comprises heating the solution (S33) to a temperature of 50° C. or higher, preferably 65° C. or higher, and most preferably 80° C. or higher; 25. The method according to claim 24, characterized in that heating the solution (S33) includes a step (S37) of exchanging heat between the hot condensate produced by the previous heating step (S52) of the solution after the magnesium removal step (S30) and the solution.

26. The method according to any one of claims 1 to 25, characterized in that the struvite is at least one of ammonium struvite and potassium struvite.

27. 1. A method for recovering at least nitrogen from a waste product, the method comprising: - precipitating struvite from the waste liquor (S1) by adding an ammonium-free magnesium compound to the waste liquor (S4) and adjusting the pH of the waste liquor to an alkaline pH (S5); - separating the precipitated struvite from the initial solution of the waste (S2); - a step (S3) of decomposing the separated struvite by a method according to any one of claims 1 to 26, A method comprising:

28. 28. The method according to claim 27, characterized in that at least a part of the precipitated magnesium compounds not containing ammonium in the step (S3) of decomposing the separated struvite is used as at least a part of the added magnesium compounds not containing ammonium in the subsequent step (S1) of precipitating the struvite from the initial solution of the waste (13).

29. 29. The method according to claim 27 or 28, characterized in that the struvite precipitation step (S1) further comprises adding struvite to the initial waste solution as seed crystals.

30. 30. The method according to any one of claims 27 to 29, characterized in that the adjustment (S5) of the pH of the initial solution is carried out at least in part by adding (S6) a calcium compound, thereby separating any precipitated calcium compounds together with the precipitated struvite.

31. 1. An apparatus for decomposing struvite, the apparatus comprising: - a dissolver (10) arranged to dissolve a feed material (13) comprising struvite in a mineral acid (15) to thereby produce a solution (17) having an acidic pH, said dissolver comprising an input (11) for said feed material (13), an input (14) for said mineral acid (15) and an output (18) for said solution (17) having an acidic pH; a magnesium removal section (30) arranged to remove magnesium (S30) from said solution, thereby obtaining a solution (39) comprising the ammonium salt of said mineral acid, the magnesium removal section (30) comprises an input (34) connected to the output (18) of the dissolver (10) for the solution (17) having an acidic pH, an output (32) for precipitated magnesium compounds, and an output (38) for the solution (39) comprising the ammonium salt of the mineral acid, the magnesium removal section (30) being arranged to increase the pH of the solution from the dissolver (10) to a pH in the range of 4.5 to 6, precipitate ammonium-free magnesium compounds, and separate the precipitated magnesium compounds from the solution; An apparatus comprising:

32. the feed material further comprises a calcium compound, whereby the dissolver (10) further dissolves the calcium compound in the solution, and the dissolver (10) further comprises a calcium removal section (20) arranged to remove calcium from the acidic solution; The calcium removal section (20) comprises a means for causing precipitation of calcium compounds (22) from the solution, and a filter (24) for filtering the precipitated calcium compounds from the solution.

32. The apparatus of claim 31.

33. a feedback connection (60) between the output for the filtered solution of the calcium removal section (20) and an input to the dissolver (10) for adding a portion of the filtered solution to be added for subsequent dissolution of the feed material; 33. The device according to claim 32, characterized in that

34. the mineral acid being at least one of hydrochloric acid, phosphoric acid, and nitric acid; Thus, the means for causing precipitation of the calcium compounds (22) comprises an input (23) for adding sulfuric acid (27) and thereby causing precipitation of the calcium compounds as gypsum; 34. Apparatus according to claim 32 or 33, characterized in that

35. said mineral acid being nitric acid; whereby said means for causing precipitation of said calcium compound (22) comprises a cooling device (21) arranged to cool said solution after said dissolution of said feed material, thereby causing precipitation of calcium nitrate; 34. Apparatus according to claim 32 or 33, characterized in that

36. said mineral acid being sulfuric acid; whereby the dissolution of the feed material occurs in the calcium removal section (20); Thereby, the means for causing precipitation of said calcium compound (22) comprises said input for said mineral acid (15); whereby the precipitated calcium compound comprises gypsum; 34. Apparatus according to claim 32 or 33, characterized in that

37. The magnesium removal section (30) comprises: - an inlet (35) for ammonia (31) to mix with said solution and increase its pH; a heating device (33) for heating the mixture of said solution and ammonia, thereby causing the precipitation of the magnesium compound (41), a heating device (33) arranged to heat the mixture of solution and ammonia to a temperature of 50° C. or more, preferably 65° C. or more, and most preferably 80° C. or more; Device according to any one of claims 31 to 36, characterized in that it comprises:

38. 37. Apparatus according to any one of claims 31 to 36, characterized in that the magnesium removal section (30) comprises an inlet (35) for a base into the solution, thereby causing precipitation of the magnesium compounds, the inlet (35) for the base being arranged for the inlet of struvite.

39. The magnesium removal section (30) comprises: a mixing volume (44) provided with an inlet (46) for said solution after said separation step of the precipitated magnesium compounds and an inlet (48) for ammonia (31), thereby causing the precipitation of struvite (31B); - a struvite removal device (49A) for removing the precipitated struvite (31B) from the solution; 40. The apparatus of claim 38, further comprising:

40. 40. Apparatus according to claim 39, further comprising a recirculation device (43) arranged for recirculating at least a portion of the removed precipitated struvite (31B) from the struvite removal device (49A) to the inlet (35) for base to be used in a subsequent base addition.

41. a terminal solidification device (50) connected to the output for the solution (39) comprising the ammonium salt of the mineral acid of the magnesium removal section (30) and arranged for crystallizing the ammonium salt of the mineral acid from said solution, the terminal solidification device (50) having an output (52) for the solidified product (51) of the ammonium salt of the mineral acid; The device according to any one of claims 31 to 40, further comprising:

42. the terminal solidification device (50) comprising a heating device (54) arranged to heat the solution (39) comprising the ammonium salt of the mineral acid, thereby producing the solid product of the ammonium salt of the mineral acid and a hot condensate; Thereby, the terminal solidification device (50) is provided with an output (53) for the hot condensate; 42. The apparatus of claim 41 .

43. The magnesium removal portion (30): - an inlet (35) for ammonia (31) to mix with said solution and increase its pH; a heating device (33) for heating the mixture of said solution and ammonia, thereby causing the precipitation of the magnesium compound (41), a heating device (33) arranged to heat the mixture of solution and ammonia to a temperature of 50° C. or more, preferably 65° C. or more, and most preferably 80° C. or more; The present invention provides 43. Apparatus according to claim 42, characterized in that the output (53) for the hot condensate of the terminal solidification device (50) is connected to the heating device (33) for heating the mixture of the solution and ammonia of the magnesium removal section (30), whereby the heating device (33) for heating the mixture of the solution and ammonia is arranged for heat exchange between the hot condensate produced by previous heating of the solution in the terminal solidification device (50) and the mixture of the solution and ammonia of the magnesium removal section (30).

44. 1. An apparatus for recovering at least nitrogen from a waste product, comprising: - a struvite precipitation device (2), said struvite precipitation device (2) comprising an input (3) for a waste priming solution (135) and an input (5) for an ammonium-free magnesium compound (136); said struvite precipitator (2) being arranged for mixing said waste priming solution (135) and said magnesium compound (136) and for adjusting the pH of said waste priming solution to an alkaline pH, thereby precipitating struvite (100); said struvite precipitation device (2) comprising a separation device (7) arranged for separating said precipitated struvite from said waste initial solution (135), and an output (6) for said precipitated struvite (100); - a device (1) for decomposing struvite (100) according to any one of claims 31 to 43, Equipped with the feed input (11) of the dissolution reaction vessel (10) is connected to the output (6) of the struvite precipitation device (2) for the precipitated struvite (100); Device.

45. 45. Apparatus according to claim 44, characterized in that the output for precipitated magnesium compounds of the magnesium removal section (30) is connected to the input (5) for ammonium-free magnesium compounds (136) of the struvite precipitation unit (2) in order to use at least a part of the ammonium-free precipitated magnesium compounds produced in the unit (1) for decomposing struvite (100) in a subsequent struvite precipitation.

46. 46. ​​Apparatus according to claim 44 or 45, characterized in that the struvite precipitation device (2) comprises an input for adding a calcium compound for effecting the pH adjustment and thereby separating any precipitated calcium compounds together with the precipitated struvite.

47. 47. Apparatus according to any one of claims 44 to 46, characterized in that the struvite precipitator (2) comprises an input for adding struvite as seeds into the initial waste stream.

Citation Information

Patent Citations

  • Method for removing and recovering phosphorus, aluminum and heavy metals from various carbonized materials

    JP2002001259A

  • Phosphorus and magnesium stripping process from excess activated sludge and struvite generation system

    JP2011510809A

  • Treatment of phosphate-containing wastewater

    US20130062289A1

  • Ammoniacal nitrogen and phosphorus recovery agent and method for producing same

    WO2013136677A1