Powder manufacturing device and powder manufacturing method
The described apparatus and method address the limitations of existing granulators by producing fine powders with arbitrary shapes and precise particle sizes, enhancing yield and versatility through controlled exposure and curing processes.
Patent Information
- Application Number
- JP2020157906
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-18
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2040-09-18
AI Technical Summary
Existing granulators produce powders with large particle sizes and wide distributions, necessitating classification to achieve desired sizes, and can only form simple shapes like spheres or cylinders, leading to reduced yield and limited versatility.
A powder manufacturing apparatus and method utilizing a modeling table, supply means, stretching member, exposure device, and control unit to form and cure composition layers with precise particle sizes and shapes, enabling the production of fine powders with arbitrary shapes and distributions.
Enables the high-precision manufacturing of fine powders with arbitrary shapes and particle size distributions, reducing the need for classification and increasing yield by controlling exposure patterns and using photocurable compositions.
Smart Images

Figure 0007591806000001 
Figure 0007591806000002 
Figure 0007591806000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a powder manufacturing apparatus. and Powder manufacturing method To Regarding. [Background technology]
[0002] Granulators are known as devices for producing powder. For example, in a rolling granulator described in Patent Document 1, raw material consisting of alumina fine powder is placed in a pan-shaped rotating dish. In this state, a liquid agent is sprayed onto the raw material for a predetermined time while the rotating dish is rotated, and then granulated material is produced by firing. In an agitation type granulator described in Patent Document 2, alumina fiber and water are mixed and agitated to produce a granular material. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2015-105223 A [Patent Document 2] JP 2008-138157 A Summary of the Invention [Problem to be solved by the invention]
[0004] It is believed that fine powders can be effectively used as materials for producing various products in the fields of medicine, industry, and the like. However, the average particle size of the powder produced by the granulators of Patent Documents 1 and 2 is relatively large, about 0.1 mm to 5 mm. In addition, since the particle size distribution of the produced powder is large, in order to obtain a powder having a desired average particle size with little variation, it is necessary to classify the produced powder. Therefore, the yield rate decreases. Furthermore, it is preferable that the powder has a shape according to the application, but the granulators of Patent Documents 1 and 2 can only produce powders having simple shapes such as spherical or cylindrical shapes.
[0005] The object of the present invention is to provide a powder manufacturing apparatus capable of manufacturing fine powder particles having any shape with high precision. and Powder manufacturing method of The aim is to provide. [Means for solving the problem]
[0006] (1) A powder manufacturing apparatus according to a first aspect of the present invention includes a modeling table having a modeling surface, a supplying means for supplying a mixture of a ceramic powder or a metal powder and a binder containing a photocurable composition, a spreading member for forming one or more composition layers by spreading the mixture supplied by the supplying means onto the modeling surface of the modeling table, and an exposure device for exposing each composition layer formed by the spreading member to light to form a powder containing a plurality of particles consisting of the one or more hardened composition layers. a control unit for setting a plurality of target particle sizes at particle size intervals equal to or less than a predetermined value so that powder having a predetermined particle size distribution shape is formed; Equipped with.
[0007] In this powder production apparatus, the exposure pattern of the exposure device is controlled so that each composition layer constituting the powder is cured in any shape and size, thereby making it possible to produce fine powder having any shape with high precision. The powder manufacturing apparatus further includes a control unit that sets a plurality of target particle sizes at particle size intervals equal to or smaller than a predetermined value so that powder having a predetermined particle size distribution shape is formed. In this case, powder having an arbitrary particle size distribution shape can be manufactured with high accuracy.
[0008] (2) The exposure by the exposure device may be performed using exposure light having a spot size of 600 μm or less in diameter. In this case, fine powder can be produced more easily.
[0010] ( 3 The powder manufacturing apparatus may further include a mixing means for generating a mixed solution by mixing one or more composition layers containing powder with a solvent, and a filter member for extracting the powder from the mixed solution. In this case, fine powder can be easily extracted.
[0011] ( 4 The average particle size of the powder may be 1000 μm or less. In this case, the powder can be made even finer.
[0012] ( 5) The powder production method according to the second aspect of the present invention comprises: A step of setting a plurality of target particle sizes at particle size intervals equal to or smaller than a predetermined value so that powder having a predetermined particle size distribution shape is formed; The method includes the steps of: supplying a mixture of a ceramic powder or a metal powder and a binder containing a photocurable composition; forming one or more composition layers by spreading the mixture on a modeling surface of a modeling table using a spreading member; exposing each formed composition layer using an exposure device to form a powder containing a plurality of particles consisting of the cured one or more composition layers; and separating the powder from uncured portions of the one or more composition layers by washing.
[0013] According to this powder production method, the exposure pattern by the exposure device is controlled, so that each composition layer constituting the powder is cured in any shape and size, thereby making it possible to produce fine powder having any shape with high precision. In addition, a plurality of target particle sizes are set at particle size intervals equal to or smaller than a predetermined value so that powder having a desired particle size distribution shape is formed. In this case, powder having a desired particle size distribution shape can be produced with high accuracy. Effect of the Invention
[0015] According to the present invention, fine powder having any desired shape can be produced with high precision. [Brief description of the drawings]
[0016] [Figure 1] 1 is a schematic side view of a powder manufacturing apparatus according to an embodiment of the present invention. [Diagram 2] FIG. [Diagram 3] FIG. [Figure 4] FIG. 2 is a diagram showing the particle size range of single particles contained in a powder. [Diagram 5] FIG. 13 is a diagram showing an example of a pseudo particle size distribution shape. [Figure 6] FIG. 13 is a diagram showing recipes for a plurality of target particle sizes set by a control device. [Figure 7] FIG. 11 is a diagram showing another example of a pseudo particle size distribution shape. [Figure 8] 1 is a micrograph showing the powder in the first example. [Figure 9]1 is a micrograph showing the powder in the second example. [Figure 10] 11 is a micrograph showing the powder in the third example. [Figure 11] 11 is a micrograph showing the powder in the fourth example. [Figure 12] 2 is a flowchart showing a powder production process executed by the control device of FIG. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] (1) Configuration of powder manufacturing equipment Hereinafter, a powder manufacturing apparatus, a powder manufacturing method, and powder according to an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a schematic side view of a powder manufacturing apparatus according to an embodiment of the present invention. In FIG. 1, as indicated by the arrows, directions perpendicular to each other in a horizontal plane are called the X direction and the Y direction, and the vertical direction is called the Z direction. As shown in FIG. 1, the powder manufacturing apparatus 100 includes a modeling table 10, a supply unit 20, a stretching member 30, an exposure device 40, a storage device 50, a control device 60, and a cleaning device 70.
[0018] The modeling table 10 is, for example, a flat plate having a rectangular shape. The modeling table 10 is disposed substantially horizontally such that one pair of sides are parallel to the X direction and the other pair of sides are parallel to the Y direction. As a result, one surface (top surface) of the modeling table 10 faces upward. The top surface of the modeling table 10 becomes a modeling surface 11 on which the powder 3 is produced.
[0019] The supply unit 20 is, for example, a dispenser, and includes, for example, a cylindrical syringe extending in the Z direction, and a nozzle disposed at the bottom end of the syringe. The supply unit 20 stores therein a mixture 1 in which a ceramic powder or a metal powder is mixed with a binder containing a resin-made photocurable composition. A discharge hole 21 is formed at the tip of the supply unit 20 (for example, at the bottom end of the nozzle). The supply unit 20 discharges the stored mixture from the discharge hole 21 onto the modeling surface 11 of the modeling table 10.
[0020] The stretching member 30 is, for example, a recoater, which extends in the X direction and is provided above the modeling table 10 so as to be movable in the Y direction. In this example, the stretching member 30 is a blade member, but may be a roller member. With the mixture 1 supplied by the supply unit 20, the stretching member 30 moves in the Y direction, whereby the mixture 1 is stretched in the Y direction on the modeling surface 11 as a composition layer 2. As a result, one or more composition layers 2 are formed.
[0021] The exposure device 40 is disposed above the modeling table 10 and is configured to be capable of emitting exposure light having a wavelength in the photosensitive wavelength region. In this example, the exposure device 40 includes a laser light source and emits laser light having a wavelength in the ultraviolet region (e.g., 315 nm to 400 nm) as the exposure light. The spot size of the exposure light may be 10 μm or more. The spot size of the exposure light may be 600 μm or less. The spot size is the size of the range in which the photocurable composition undergoes a curing reaction. The exposure light emitted by the exposure device 40 is scanned so as to be partially irradiated onto each composition layer 2 formed by the stretching member 30.
[0022] The composition layer 2 is exposed to light in a given pattern, whereby the exposed portions of the composition layer 2 are cured. In FIG. 1, the cured portions of the composition layer 2 are shown by a hatched pattern. A plurality of cured composition layers 2 are stacked to form a powder 3 containing a plurality of particles. The powder 3 may be formed from a single cured composition layer 2. Note that in the powder 3 formed from a plurality of composition layers 2, the boundary lines between the stacked composition layers 2 appear on the outer surface of the powder 3.
[0023] The storage device 50 includes, for example, a volatile memory or a hard disk, and stores drawing data in which multiple shape data showing the three-dimensional shapes of multiple particles contained in the powder 3 to be manufactured are described. The control device 60 is configured, for example, with a CPU (Central Processing Unit). The control device 60 controls the operations of the supply unit 20, the stretching member 30, and the exposure device 40 so that the powder 3 is manufactured based on the drawing data stored in the storage device 50. The cleaning device 70 separates the manufactured powder 3 from one or more uncured portions of the composition layer 2 by performing a cleaning process. The cleaning process will be described in detail later.
[0024] (2) Cleaning process 2 and 3 are diagrams showing the cleaning process. As shown in FIG. 2, a cleaning device 70 is provided with a storage container 71. In the storage container 71, a composition layer 2 containing a powder 3 is stored together with a solvent 4. Here, the uncured portion of the composition layer 2 has a slurry state. The solvent 4 may be an organic solvent such as alcohol, or may be an aqueous solvent.
[0025] Next, the composition layer 2 and the solvent 4 are mixed. In this case, the composition layer 2 is diluted with the solvent 4 to generate a mixed solution 5 having high fluidity. The composition layer 2 and the solvent 4 may be mixed, for example, by ultrasonic vibration or by stirring with a stirring rod. Next, as shown in FIG. 3, the mixed solution 5 is passed through a filter member 72 having a predetermined mesh size. The filter member 72 includes a mesh, a porous membrane, or a sieve. This separates the uncured composition layer 2 and the powder 3, and the powder 3 is extracted from the mixed solution 5 onto the filter member 72.
[0026] Thereafter, the separated powder 3 is dried to remove the remaining components of the solvent 4. The drying may be natural drying or vacuum drying. Alternatively, the drying may be thermal drying at, for example, about 100° C. In this state, the binder components including the photocurable composition remain in the powder 3.
[0027] Therefore, the powder 3 may be degreased by heating to, for example, about 500° C. This removes the components of the photocurable composition from the powder 3. The powder 3 may also be subjected to a further heat treatment (firing), which sinters the powder 3. On the other hand, in the case where the components of the photocurable composition may remain in the powder 3, the powder 3 may not be degreased or sintered.
[0028] The produced powder 3 may have porosity. For example, when the photocurable composition contains a porous resin, the powder 3 having porosity can be produced by omitting degreasing and sintering the powder 3. Alternatively, even when the photocurable composition does not contain a porous resin, the portions of the powder 3 from which the components of the photocurable composition have been removed can be left as pores by performing baking at a relatively low temperature. In this case as well, the powder 3 having porosity can be produced.
[0029] (3) Examples of powders In the powder manufacturing apparatus 100, the average particle size, particle size distribution, and shape of the powder 3 to be formed can be adjusted arbitrarily by using any drawing data. The average particle size of the powder 3 may be 10 μm or more. The average particle size of the powder 3 may be 1000 μm or less. Depending on the application of the powder 3, the powder 3 having an average particle size of less than 100 μm or less than 50 μm is formed. In this example, the average particle size of the powder 3 is a circle equivalent diameter measured by a microscopic method. For example, the average particle size can be obtained by measuring the circle equivalent diameters of at least 300 particle images included in a micrograph and calculating the average of these.
[0030] FIG. 4 is a diagram showing the particle size range of a single particle contained in the powder 3. In the example of FIG. 4, the particle size distribution shape has a Gaussian distribution. In this example, it is possible to reduce the width of the particle size distribution of the powder 3. The width of the particle size distribution means the difference (D90-D10) between D90 and D10 of the particle set corresponding to the peak. For example, when the particle size is 100 μm or less, the width of the particle size distribution is the median particle size ±5 μm, and when the particle size is 100 μm or more, D90 / D10 is 1.1 or less. Therefore, the powder 3 having a desired average particle size can be efficiently obtained without performing a classification operation. This prevents a decrease in yield.
[0031] On the other hand, it is also possible to increase the width of the particle size distribution of the powder 3. Specifically, the control device 60 can set a plurality of target particle sizes at particle size intervals of a predetermined value or less so that the powder 3 is formed with a predetermined particle size distribution shape. In this case, the powder 3 having a pseudo arbitrary particle size distribution shape can be manufactured with high accuracy. The predetermined interval may be, for example, 10 μm or less, 5 μm or less, or 1 μm or less. In addition, the particle size distribution shape may be set to a Gaussian distribution or may be set to a distribution other than a Gaussian distribution.
[0032] FIG. 5 is a diagram showing an example of a pseudo particle size distribution shape. FIG. 6 is a diagram showing a plurality of recipes for target particle sizes set by the control device 60. In the example of FIG. 6, a target particle size and the number of particles are set in each of "Recipe Number 1" to "Recipe Number 9". The target particle sizes of "Recipe Number 2", "Recipe Number 5" and "Recipe Number 8" correspond to D10, D50 and D90, respectively. Nine particle size distribution shapes corresponding to "Recipe Number 1" to "Recipe Number 9" are shown by solid lines in FIG. 6. In this case, the pseudo particle size distribution shape becomes large, as shown by the dashed line in FIG. 6. As a result, a powder 3 having an arbitrary particle size distribution width (D90-D10) can be obtained.
[0033] FIG. 7 is a diagram showing another example of a pseudo particle size distribution shape. In the example of FIG. 7, a plurality of particle size distribution shapes corresponding to a plurality of recipes are shown by solid lines. This realizes a pseudo particle size distribution shape including a plurality of peaks (three in this example) having various widths, as shown by the dashed dotted line. In this way, it is possible to make the particle size distribution have a plurality of peaks, and to arbitrarily adjust the width of each peak of the particle size distribution. In these cases, powders 3 having various average particle sizes can be efficiently obtained.
[0034] Furthermore, not only powders having simple shapes such as spheres or cylinders, but also powders 3 having more complicated shapes can be produced. Figures 8 to 11 are micrographs showing powders 3 in the first to fourth examples, respectively. In each of Figures 8 to 11, the upper part shows particles of powder 3 before debinding, and the lower part shows particles of powder 3 after debinding and sintering.
[0035] As shown in Fig. 8, the powder 3 in the first example has an annular shape, and the particle size of the powder 3 is about 200 µm. Specifically, the powder 3 has a circular annular shape, but may have other annular shapes such as a rectangular frame shape. As shown in Fig. 9, the powder 3 in the second example has a polygonal shape, and the particle size of the powder 3 is about 200 µm. Specifically, the powder 3 has a hexagonal shape, but may have other polygonal shapes such as a pentagonal shape or a star shape.
[0036] As shown in FIG. 10, the powder 3 in the third example has a cross shape, and the particle size of the powder 3 is about 200 μm. As shown in FIG. 11, the powder 3 in the fourth example has a C-shape, and the particle size of the powder 3 is about 200 μm. In the first to fourth examples, the upper and lower surfaces of the powder 3 may be parallel flat surfaces or curved surfaces. The powder 3 may have a shape having at least one or a plurality of openings, or may be disk-shaped. Furthermore, the boundary line between the plurality of laminated composition layers may be visible on the outer surface of the powder 3.
[0037] As another example of the powder 3, powder 3 having a fibrous (thread-like) or wave-dissipating block shape (Tetrapod (registered trademark) shape) can be manufactured according to the application. For example, when the powder 3 is formed of thermally conductive particles, a thermally conductive sheet having high thermal conductivity in one direction can be manufactured by using the fibrous powder 3. Alternatively, an artificial bone having high bone density can be manufactured by using minute powder 3 having a wave-dissipating block shape. In addition, the powder 3 can be used, for example, as a component of an electric device such as a secondary battery (for example, a material for a separator of a secondary battery).
[0038] Powder 3 having the above-mentioned various shapes is manufactured by scanning the exposure light so that a predetermined drawing is performed by the exposure light on the composition layer 2 corresponding to the surface or each cross section of powder 3. Here, in this example, since the powder 3 is minute, when the powder 3 has corners as in the above-mentioned second example, even if the exposure light is scanned so that the shape of the target corners is drawn on the composition layer 2, the corners of the powder 3 may not be formed appropriately.
[0039] Therefore, when the powder 3 has a corner, the exposure light is scanned so as to draw a corner having an angle sharper (smaller) than the angle of the target corner in an area inside the target corner in the composition layer 2. This makes it possible to appropriately form the corner of the powder 3 even when the powder 3 is very small.
[0040] (4) Powder manufacturing and processing Fig. 12 is a flowchart showing the powder production process executed by the control device 60 of Fig. 1. As shown in Fig. 12, first, n pieces of cross-sectional data (n is an integer equal to or greater than 1) are acquired based on the graphic data stored in the storage device 50 (step S1). Each piece of cross-sectional data represents the planar shape of each composition layer 2 of the powder 3. The acquired n pieces of cross-sectional data are each assigned a unique number from 1 to n, starting from the bottom. The first row of cross-sectional data corresponds to the bottommost composition layer 2, and the nth row of cross-sectional data corresponds to the topmost composition layer 2.
[0041] Next, the value of the variable i, which indicates the number of layers, is set to 1 (step S2). Then, the supply unit 20 discharges the mixture 1 (step S3). As a result, when the value of the variable i is 1, the mixture 1 is supplied onto the modeling surface 11 of the modeling table 10. On the other hand, when the value of the variable i is 2 or more, the mixture 1 is supplied onto the composition layer 2. After that, the supplied mixture 1 is stretched by the stretching member 30 to form the composition layer 2 (step S4).
[0042] Next, the formed composition layer 2 is exposed by the exposure device 40 based on the i-th cross-sectional data (step S5). This causes the exposed portion of the composition layer 2 to harden. Then, it is determined whether the value of the variable i is n (step S6). If the value of the variable i is not n, the value of the variable i is incremented by 1 (step S7), and the process returns to step S3. Steps S3 to S7 are repeated until the value of the variable i becomes n.
[0043] When the value of the variable i is n, the powder 3 is completed. In this case, the formed powder 3 is washed by the washing device 70 to extract the powder 3 (step S8). Then, the powder 3 is degreased (step S9). Finally, the powder 3 is sintered (step S10). This completes the powder manufacturing process. Step S10 may be omitted. Alternatively, step S9 may also be omitted.
[0044] (5) Effects In the powder manufacturing apparatus 100 according to the present embodiment, a mixture 1 obtained by mixing a ceramic powder or a metal powder with a binder containing a photocurable composition is supplied by a supply unit 20. The mixture 1 is spread by a spreading member 30 onto a modeling surface 11 of a modeling table 10, thereby forming one or more composition layers 2. Each formed composition layer 2 is exposed by an exposure device 40, thereby forming a powder 3 consisting of one or more cured composition layers 2. The powder 3 is separated from uncured portions of the one or more composition layers 2 by cleaning by a cleaning device 70.
[0045] According to this configuration, the exposure pattern by the exposure device 40 is controlled, so that each composition layer 2 constituting the powder 3 is cured in any shape and size. This makes it possible to manufacture fine powder 3 having any shape with high precision.
[0046] In the cleaning device 70, a composition layer 2 containing powder 3 and a solvent 4 are mixed in a storage container 71 to generate a mixed solution 5. Furthermore, the powder 3 is extracted from the mixed solution 5 by a filter member 72. In this case, fine powder 3 can be easily extracted.
[0047] Moreover, exposure by the exposure device 40 is performed using exposure light having a spot size of 10 μm or more and 600 μm or less in diameter. This makes it possible to easily manufacture powder 3 having an average particle size of 10 μm or more and 1000 μm or less. The spot size may be 200 μm or less, or 50 μm or less. Moreover, the average particle size of the powder 3 may be 300 μm or less, or 100 μm or less.
[0048] (6) Correspondence between each component of the claims and each component of the embodiment Below, examples of the correspondence between each component of the claims and each element of the embodiment will be described, but the present invention is not limited to the following examples. Various other elements having the configuration or function described in the claims can also be used as each component of the claims.
[0049] In the above embodiment, the modeling surface 11 is an example of a modeling surface, the modeling table 10 is an example of a modeling table, the mixture 1 is an example of a mixture, and the supply unit 20 is an example of a supply means. The composition layer 2 is an example of a composition layer, the stretching member 30 is an example of a stretching member, the powder 3 is an example of a powder, the exposure device 40 is an example of an exposure device, and the control device 60 is an example of a control unit. The powder manufacturing device 100 is an example of a powder manufacturing device, the solvent 4 is an example of a solvent, the mixed solution 5 is an example of a mixed solution, the storage container 71 is an example of a mixing means, and the filter member 72 is an example of a filter member. (7) Reference form (7-1) A powder manufacturing apparatus according to a first reference embodiment includes a modeling table having a modeling surface, a supplying means for supplying a mixture of a ceramic powder or a metal powder and a binder containing a photocurable composition, a stretching member for forming one or more composition layers by stretching the mixture supplied by the supplying means onto the modeling surface of the modeling table, and an exposure device for exposing each composition layer formed by the stretching member to light to form a powder containing a plurality of particles consisting of one or more hardened composition layers. In this powder production apparatus, the exposure pattern of the exposure device is controlled so that each composition layer constituting the powder is cured in any shape and size, thereby making it possible to produce fine powder having any shape with high precision. (7-2) The exposure by the exposure device may be performed using exposure light having a spot size of 600 μm or less in diameter. In this case, fine powder can be produced more easily. (7-3) The powder manufacturing apparatus may further include a control unit that sets a plurality of target particle sizes at particle size intervals equal to or smaller than a predetermined value so that powder having a predetermined particle size distribution shape is formed. In this case, powder having an arbitrary particle size distribution shape can be manufactured with high accuracy. (7-4) The powder manufacturing apparatus may further include a mixing means for mixing one or more composition layers containing powder with a solvent to generate a mixed solution, and a filter member for extracting the powder from the mixed solution. In this case, fine powder can be easily extracted. (7-5) The powder may have an average particle size of 1000 μm or less. In this case, the powder can be made finer. (7-6) A powder manufacturing method according to a second reference embodiment includes the steps of: supplying a mixture of a ceramic powder or a metal powder and a binder containing a photocurable composition; forming one or more composition layers by spreading the mixture on a modeling surface of a modeling table using a spreading member; exposing each of the formed composition layers using an exposure device to form a powder containing a plurality of particles consisting of the one or more hardened composition layers; and separating the powder from unhardened portions of the one or more composition layers by washing. According to this powder production method, the exposure pattern by the exposure device is controlled, so that each composition layer constituting the powder is cured in any shape and size, thereby making it possible to produce fine powder having any shape with high precision. (7-7) The powder according to the third embodiment has an average particle size of 1000 μm or less, and is in the form of a ring, a polygon, a cross, a C-shape, a shape having at least one or a plurality of openings, a disk, or a fiber. In this case, the powder can be used to manufacture various products. [Explanation of symbols]
[0050] 1... mixture, 2... composition layer, 3... powder, 4... solvent, 5... mixed solution, 10... modeling table, 11... modeling surface, 20... supply section, 21... discharge hole, 30... stretching member, 40... exposure device, 50... storage device, 60... control device, 70... cleaning device, 100... powder manufacturing device
Claims
1. a modeling table having a modeling surface; A supplying means for supplying a mixture of a ceramic powder or a metal powder and a binder containing a photocurable composition; a spreading member for spreading the mixture supplied by the supplying means onto the modeling surface of the modeling table to form one or more composition layers; an exposure device that exposes each composition layer formed by the spreading member to light to form a powder containing a plurality of particles composed of the one or more hardened composition layers; and a control unit that sets a plurality of target particle sizes at particle size intervals equal to or smaller than a predetermined value so that the powder is formed in a predetermined particle size distribution shape.
2. 2. The powder manufacturing apparatus according to claim 1, wherein the exposure by the exposure device is performed using exposure light having a spot size of 600 [mu]m or less in diameter.
3. a mixing means for mixing the one or more composition layers containing the powder with a solvent to generate a mixed solution; The powder manufacturing apparatus according to claim 1 , further comprising a filter member for extracting the powder from the mixed solution.
4. 4. The powder manufacturing apparatus according to claim 1, wherein the powder has an average particle size of 1000 μm or less.
5. A step of setting a plurality of target particle sizes at particle size intervals equal to or less than a predetermined value so that a powder having a predetermined particle size distribution shape is formed; Providing a mixture of a ceramic or metal powder and a binder including a photocurable composition; spreading the mixture onto a build surface of a build table with a spreading member to form one or more composition layers; forming the powder containing a plurality of particles consisting of one or a plurality of hardened composition layers by exposing each of the formed composition layers with an exposure device; and separating the powder from uncured portions of the one or more composition layers by washing.
Citation Information
Patent Citations
Lightweight unburned tile
JP2001247355A
Micromachine part, its manufacturing method and manufacturing method of mold for micromachine part
JP2007021993A
Granules and heat-conductive resin composition using the same
JP2008138157A
Photo-curable composition for micro-optical shape-forming, metal shaped article, and manufacturing method therefor
JP2009084619A
Porous granulated calcination product and production method thereof
JP2015105223A