Method for drying transport and / or storage containers
A method of continuous evacuation and helium gas supply addresses inefficiencies in drying transport and storage containers for radioactive waste, providing efficient and cost-effective drying for high-heat containers.
Patent Information
- Application Number
- JP2020142682
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-09-16
- Filing Date
- 2020-08-26
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2040-08-26
AI Technical Summary
Existing methods for drying transport and storage containers for radioactive waste, particularly spent fuel elements, are laborious, expensive, and inefficient, especially for containers with high heat output.
A method involving continuous evacuation of the container interior to a negative pressure, followed by continuous helium gas supply, maintaining a specific gas volume percentage, to achieve efficient drying.
The method achieves high drying efficiency with reduced effort and cost, suitable for containers with high heat output, ensuring reliable and precise drying results.
Smart Images

Figure 0007591889000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for drying transport and / or storage containers for radioactive waste, in particular spent fuel elements, which first involves draining or mechanically draining the container, followed by a continuous evacuation or negative pressure within the container's interior, in the following the term transport and / or storage container will also be used for short as container. [Background technology]
[0002] Methods for drying transport and / or storage containers of the aforementioned type are known in principle in various forms in practice. Containers used for spent fuel elements are usually loaded with the spent fuel elements in water, since water constitutes an effective shielding medium for the neutrons that are generated. For further handling, the container is generally first drained or mechanically drained. Following this, the water still remaining in the container is removed from it by drying, in particular vacuum drying.
[0003] It is also already known to remove the moisture still remaining in the container by means of a gas, in particular an inert gas such as nitrogen or helium, which is led through the container interior. For this purpose, reference can be made, for example, to US Pat. No. 10,229,764. In the known procedure, a gas is first led through the container interior for drying, and after the end of this procedure, the container is exposed to a vacuum.
[0004] In this respect, the known drying methods are in part relatively laborious and therefore expensive. Furthermore, many of the known drying methods are notable for their insufficient drying efficiency. This also applies in particular to transport containers and / or storage containers with high heat output. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] U.S. Patent No. 10,229,764 Summary of the Invention [Problem to be solved by the invention]
[0006] In contrast, the technical problem underlying the present invention is to provide a method of the type mentioned at the outset which is easy and can be carried out without much effort, is distinguished by a high drying efficiency and is particularly suitable also for containers with a high heat output. [Means for solving the problem]
[0007] To solve this technical problem, the present invention teaches a method for drying transport and / or storage containers for radioactive waste, in particular spent fuel elements, by first draining or mechanically draining the container, followed by continuously evacuating or maintaining the container interior at a negative pressure, particularly preferably at a constant or approximately constant negative pressure, and simultaneously continuously supplying an inert gas, in particular helium gas, to the container interior, the evacuation and / or inert gas supply or helium gas supply being carried out under conditions that the inert gas or helium gas content in the container interior is 50 vol% to 95 vol%, in particular 55 vol% to 90 vol%, preferably 60 vol% to 85 vol%, advantageously 65 vol% to 85 vol%. According to a preferred variant, the inert gas or helium content in the container interior is 70 vol% to 80 vol%. When referring hereinafter to helium or helium gas, this generally means an inert gas, and advantageously helium or helium gas, within the scope of the present invention.
[0008] The method according to the invention is particularly relevant for drying transport and / or storage containers used for spent fuel elements. Preferably, the method according to the invention is used for containers with a higher or high thermal power, i.e. for a thermal power of 12.5 kW to 42 kW, in particular for a thermal power of 15 kW to 40 kW, in particular for a thermal power of 20 kW to 40 kW, for example for a thermal power of 25 kW to 40 kW. The method can be carried out or is preferably carried out under conditions in which a fuel rod cladding temperature of 320° C. to 400° C., in particular 350° C. to 400° C., is maintained or can be maintained.
[0009] Within the scope of the method according to the invention, the vessel is first drained or mechanically drained. Preferably, after such a drainage of the vessel, an initial evacuation of the vessel interior and thus an initial creation of a negative pressure or vacuum in the vessel interior is carried out, without any helium gas supply for the time being. This initial evacuation is expediently carried out until the pressure in the vessel interior is between 8 mbar and 30 mbar, in particular between 8 mbar and 25 mbar, preferably between 8 mbar and 20 mbar, particularly preferably between 10 mbar and 20 mbar. According to a very preferred embodiment of the invention, the pressure or negative pressure created in this case is between 8 mbar and 12 mbar, for example 10 mbar. As has been demonstrated, the initial evacuation is carried out over a period of between 4 hours and 12 hours, in particular between 5 hours and 10 hours.
[0010] Preferably, after the first evacuation of the vessel interior and before the inert gas supply, the evacuation of the vessel interior is interrupted for a period t. Expediently, during this period t, the pressure increase Δp in the vessel interior is equal to or greater than the filling pressure p to be set, in particular for the subsequent helium gas supply. tot is measured to find
[0011] According to a preferred embodiment of the present invention, after the initial evacuation or negative pressure generation, the water vapor partial pressure p H2O is calculated using the measured pressure rise Δp. H2OFrom the above, the filling pressure p required to supply helium to obtain the desired volume percent amount of helium in the vessel (50 vol% to 95 vol%) is tot is calculated, an example of which is disclosed in the following description. The desired volume percent amount of helium is in the vol% range claimed in claim 1.
[0012] Furthermore, it is within the scope of the present invention to carry out a continuous evacuation of the container interior and a simultaneous continuous helium gas supply according to the present invention after the initial evacuation or negative pressure generation and preferably after the pressure rise measurement. The evacuation and the helium gas supply are preferably carried out under conditions in which the pressure in the container interior is 8 mbar to 30 mbar, in particular 8 mbar to 25 mbar, preferably 8 mbar to 20 mbar, advantageously 10 mbar to 20 mbar. According to a preferred embodiment, the pressure in the container interior is 8 mbar to 12 mbar, for example about 10 mbar. Furthermore, it is within the scope of the present invention for this pressure to be kept constant or approximately constant during the continuous evacuation and the simultaneous continuous helium gas supply. According to a particularly preferred embodiment of the present invention, the continuous evacuation and the continuous helium gas supply are carried out for a period of at least 3 hours, preferably at least 4 hours, advantageously at least 4.5 hours, very advantageously at least 5 hours. According to one proven variant of the invention, the continuous evacuation and the simultaneous continuous helium gas supply are carried out over a period of 3 to 35 hours, in particular over a period of 3.5 to 32 hours, preferably over a period of 4 to 31 hours, very preferably over a period of 5 to 30 hours. In this case, the above-mentioned specific pressure in the container interior is expediently maintained, preferably constant or approximately constant, over this period. Preferably, the pressure in the container interior is maintained for at least 95% of this period, preferably constant or approximately constant.
[0013] It is within the scope of the present invention that when the desired degree of dryness is reached in the container interior, the continuous evacuation is terminated and the container interior is continued to be supplied with helium gas for the time being until a predefined pressure is reached in the container interior. The degree of dryness is suitably measured by a pressure rise measurement in relation to the pressure in the container interior. For this purpose, preferably both the continuous evacuation and the supply of helium gas are interrupted and the pressure rise in the container is measured, preferably with the aid of at least one pressure sensor. Thus, when the desired degree of dryness is reached in the container interior, the continuous evacuation is suitably terminated and helium gas is continued to be supplied to the container interior for the time being. In this case, the container interior is preferably filled with helium gas up to an internal pressure of 850 mbar to 1100 mbar, in particular up to an internal pressure of 900 mbar to 1050 mbar, preferably up to an internal pressure of 900 mbar to 1000 mbar. The drying process is then preferably terminated.
[0014] It is within the scope of the method according to the invention that the container is closed during the continuous evacuation of the container interior and the simultaneous continuous supply of helium gas, in particular by at least one or one primary lid. It is further within the scope of the invention that the container is closed or by at least one primary lid, in particular by one primary lid, during the first evacuation of the container interior and / or during the pressure rise measurement after the first evacuation and / or during the pressure rise measurement for determining the dryness and / or during the final filling of the container interior with helium gas. Preferably, the evacuation of the container and the helium supply to the container are carried out via the primary lid of the container. According to a preferred embodiment of the invention, the suction or evacuation of the container interior is carried out by means of at least one evacuation lance, which expediently penetrates the primary lid of the container.
[0015] It has been demonstrated that helium gas is supplied in the upper region of the vessel. Preferably, the evacuation or evacuation of the vessel interior takes place in the lower region of the vessel or of the vessel interior. According to a particularly preferred embodiment of the invention, the evacuation or the evacuation and the helium gas supply takes place by means of at least one double tube, which consists of an outer tube and an inner tube surrounded by the outer tube. Expediently, this double tube passes through the primary lid of the vessel. Preferably, the inner tube extends to the lower region of the vessel and the outer tube ends in the upper region of the vessel. Expediently, the vessel interior is evacuated via the inner tube, and preferably, the vessel interior is supplied with helium via the outer tube. If the free volume of the vessel interior is less than 2 m 3 ~8m 3 , preferably 3m 3 ~6m 3 In this case, free volume means the internal volume of the vessel not including the fuel basket and fuel elements.
[0016] As mentioned above, according to an advantageous embodiment of the invention, after the first evacuation of the container interior and before the helium gas supply, the evacuation is interrupted for a period t, during which the filling pressure p of the helium supply to be set is set to 0.5. tot The pressure rise Δp in the container interior is measured to determine the pressure rise Δp in the container interior. This determination will be explained in detail based on the following examples or calculation examples.
[0017] Within the scope of the embodiment, the filling pressure P for the helium gas supply to obtain a helium proportion of 75 vol.% in the container atmosphere is tot The water vapor partial pressure p H2O Helium partial pressure p He For the required voltage division ratio of p He / p H2O =75 / 25=3 is established, As a result, for helium partial pressure, P He =3×p H2O The required filling pressure p for helium supply is obtained. totIn contrast, p tot =p He +p H2O =4×p H2O is obtained.
[0018] 200m 3 / h (effective pumping speed S eff ≧200×0.573≧114.6m 3 The maximum water vapor partial pressure p during vacuum drying at H2O is determined by a preceding pressure rise measurement, which in this case is taken over a period t of 15 minutes. The evaporation rate q PV For (hPa×l / s), q PV =p×V q PV =Δp×V / t holds true.
[0019] Here, Δp represents the pressure rise (hPa), V represents the free volume inside the container (l), and t represents the measurement time (seconds). In this case, the water vapor partial pressure p H2O In contrast, p H2O =q PV / S eff = Δp × V / (t × S eff ) p H2O =Δp*5220 / (900×31.8) holds true.
[0020] Therefore, the filling pressure P should be set to ensure a helium fraction of 75 vol% by the helium supply. tot =4×p H2O From the 15-minute pressure rise, p tot =0.73×Δp It is calculated with respect to
[0021] The invention is based on the realization that the drying method according to the invention allows an extremely easy, low-effort and at the same time extremely accurate and reliable functioning drying of the container interior of a transport container and / or storage container. In this case, the method is distinguished by an unexpectedly high drying efficiency. In this respect, the method according to the invention has a significant advantage over drying methods known hitherto in practice or in the prior art. The equipment effort required for carrying out the drying method is relatively low in view of the results obtained. The method according to the invention is distinguished by a high functioning reliability and a low frequency of failures. The drying method is particularly suitable for containers with higher or higher heat output, but not exclusively. The parameters according to the invention can be easily and reproducibly maintained when carrying out the method. The costs for carrying out the method according to the invention are relatively low.
[0022] The invention will now be explained in more detail with reference to the drawings, which show only one embodiment. [Brief description of the drawings]
[0023] [Figure 1] FIG. 1 is a schematic diagram for carrying out the drying method according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] FIG. 1 clearly illustrates the drying method according to the invention in a simplified manner. A transport and / or storage vessel 1 is shown in which a fuel basket (not shown) containing spent fuel elements is accommodated. The accommodation takes place underwater, firstly after the vessel 1 has been drained or mechanically drained. Advantageously, in the embodiment, the vessel 1 is fitted with a primary lid 2 which closes the vessel 1. Expediently, in the embodiment, a double tube 3 passes through the primary lid 2 of the vessel 1 and leads into the vessel interior 4. Preferably, in the embodiment, the double tube 3 has an inner tube 5 which is configured as a vacuum exhaust lance and which extends to the lower region of the vessel interior 4. As shown, in the embodiment, the inner tube 5 is surrounded by an outer tube 6 which in this case terminates in the upper region of the vessel 1 or, advantageously, in the embodiment, below the primary cover 2.
[0025] According to an advantageous embodiment, a helium gas source 7 is connected to the outer tube 6 via a valve V1. A vacuum pump 8 is preferably connected to the outer tube 6 via a valve V2. Furthermore, a pressure sensor 9 is preferably provided in the embodiment, which is connected to the outer tube 6 and thus to the vessel interior 4 via a valve V3. The pressure sensor 9 is used in particular to measure the pressure rise Δp.
[0026] Preferably, first, an initial evacuation of the vessel interior 4 is carried out by means of the vacuum pump 8 with the valve V2 open and the valves V1 and V3 closed. Expediently, this initial evacuation is carried out until a pressure of 10 mbar is reached in the vessel interior 4. As has been demonstrated, in the exemplary embodiment, this evacuation is carried out for a period of 3 to 12 hours, in particular 4 to 11 hours, preferably 5 to 10 hours. Expediently, after the initial evacuation of the vessel interior 4, the evacuation is interrupted for a period t before the helium gas supply. The period t can be, for example, 15 minutes. During this period t, the to-be-set filling pressure p of the helium gas supply is preferably maintained at 10 mbar. tot In order to determine the pressure rise Δp in the container inner space 4, the pressure rise Δp is measured. The pressure rise Δp is measured by means of a pressure sensor 9. For this purpose, the valve V2 leading to the vacuum pump 8 is closed and the valve V3 leading to the pressure sensor 9 is opened, with the valve 1 still closed. From the measured pressure rise Δp, the water vapor partial pressure p in the container inner space 4 can advantageously be determined. H2O is calculated, and the water vapor partial pressure p H2O , the fill pressure p required for the helium supply to obtain the desired volume percent amount of helium in the vessel 1. tot is calculated, as has already been described in detail above.
[0027] It is within the scope of the present invention to carry out a continuous evacuation of the container interior 4 according to the invention and a simultaneous continuous supply of helium gas to the container interior 4 after the initial evacuation and after the pressure rise measurement. For this purpose, the valves V1 and V2 are open. This continuous evacuation and simultaneous continuous supply of helium gas is preferably carried out under the condition that the pressure in the container interior 4 is between 8 mbar and 30 mbar, in particular between 10 mbar and 20 mbar, particularly preferably not below 10 mbar. Expediently, the continuous evacuation and simultaneous continuous supply of helium gas is carried out over a period of at least 4 hours, for example between 5 hours and 30 hours.
[0028] According to a preferred embodiment of the invention, when the desired degree of dryness is reached in the container inner space 4, the continuous evacuation is terminated by closing the valve V2 and helium gas is continued to be fed into the container inner space 4 with the valve V1 open until a predetermined pressure is reached. The desired degree of dryness can preferably be determined again via a pressure rise measurement with the pressure sensor 9. Expediently, the container inner space 4 is then filled with helium gas up to an internal pressure of 850 mbar to 1100 mbar, preferably up to an internal pressure of 900 mbar to 1000 mbar. This concludes the drying method.
[0029] As can be seen from the drawing, the helium supply takes place at the upper end of the vessel inner chamber 4 via the outer tube 6 of the double tube 3, whereas the suction or evacuation takes place in the lower region of the vessel inner chamber 4 via the inner tube 5 configured as an evacuation lance. This advantageous embodiment is demonstrated as special within the scope of the present invention. This application relates to the invention described in the claims, but also includes the following as other aspects. 1. A method for drying transport and / or storage containers (1) for radioactive waste, in particular spent fuel elements, comprising the steps of: First, the vessel (1) is drained or mechanically drained, Subsequently, the container interior (4) is continuously evacuated or maintained at a negative pressure, and at the same time, an inert gas, preferably helium gas, is continuously supplied to the container interior (4); The vacuum evacuation and / or the supply of inert gas or helium gas is carried out under the condition that the content of inert gas or helium gas in the inside of the container is 50 vol% to 95 vol%, particularly 55 vol% to 90 vol%, preferably 60 vol% to 85 vol%, and advantageously 65 vol% to 85 vol%. A method for drying a transport and / or storage container (1). 2. 2. The process according to claim 1, wherein after draining of the vessel (1), a first evacuation of the vessel interior (4) is carried out, for the time being without an inert gas feed or helium feed, until the pressure in the vessel interior (4) is preferably between 8 mbar and 30 mbar, in particular between 10 mbar and 30 mbar, advantageously between 10 mbar and 20 mbar. 3. After the initial evacuation of the vessel interior (4) and before the inert gas supply or the helium gas supply, the evacuation is interrupted for a period t, during which the filling pressure p of the inert gas supply or the helium gas supply to be set is increased by 1000 MPa. tot The method according to claim 2, wherein the pressure rise Δp in the container inner chamber (4) is measured to obtain 4. After the first evacuation, the partial pressure of water vapor in the vessel interior (4) p H2O is calculated using the measured pressure rise Δp, and the filling pressure p required for the inert gas supply or helium supply to obtain the desired volume percentage amount (50 vol% to 95 vol%) of inert gas or helium in the container (1) is calculated. tot The water vapor partial pressure p H2O The method 3 above is used to calculate from the above. 5. 5. The method according to claim 3 or 4, wherein after the initial evacuation or after the pressure rise measurement, the vessel interior (4) is continuously evacuated and simultaneously continuously supplied with inert gas or with helium gas, preferably under conditions in which the pressure in the vessel interior (4) is between 8 mbar and 30 mbar, in particular between 10 mbar and 30 mbar, and advantageously between 10 mbar and 20 mbar. 6. 6. Any one of the methods of 1 to 5 above, wherein the continuous evacuation and the continuous inert gas supply or helium gas supply are carried out for a period of at least 3 hours, preferably at least 4 hours, and advantageously at least 4.5 hours. 7. 7. Any one of the methods 1 to 6 above, wherein when a desired degree of dryness is reached in the container inner chamber (4), the continuous evacuation is terminated and an inert gas or helium gas is continuously supplied to the container inner chamber (4) for the time being until a predetermined pressure is obtained in the container inner chamber (4). 8. 8. The method according to claim 7, wherein the container inner chamber (4) is filled with an inert gas or helium gas until the inner chamber pressure reaches 850 mbar to 1100 mbar, in particular until the inner chamber pressure reaches 900 mbar to 1050 mbar, and advantageously until the inner chamber pressure reaches 900 mbar to 1000 mbar. 9. 9. The method of any one of 1 to 8 above, wherein the inert gas or helium gas is supplied at an upper region of the vessel (1). 10. 10. The method according to any one of claims 1 to 9, wherein the evacuation or evacuation of the vessel interior (4) is carried out in the area below the vessel (1) using at least one evacuation lance. 11. 11. The method according to any one of 1 to 10 above, wherein the evacuation and the inert gas supply or the helium gas supply are carried out using at least one double tube (3) consisting of an outer tube (6) and an inner tube (5) surrounded by the outer tube (6), and preferably the inner tube (5) extends to a lower region of the container (1) and the outer tube (6) terminates in an upper region of the container (1). [Explanation of symbols]
[0030] 1 container 2 Primary lid 3 double tube 4 Inner chamber of container 5 Inner tube 6 outer tube 7. Helium gas source 8. Vacuum Pump 9. Pressure Sensor
Claims
1. A method for drying a transport and / or storage container (1) for radioactive waste or spent fuel elements, comprising the steps of: First, the vessel (1) is drained or mechanically drained, After draining the vessel (1), a first evacuation of the vessel interior (4) is carried out, for the time being without an inert gas supply or a helium gas supply, Subsequently, the container interior (4) is continuously evacuated or maintained at a negative pressure, and at the same time, an inert gas or helium gas is continuously supplied to the container interior (4); After the initial evacuation of the container interior (4) and before the inert gas supply or the helium gas supply, the evacuation is interrupted for a period of time t, during which time t the pressure rise Δp in the container interior (4) is measured in order to determine the filling pressure p tot to be set for the inert gas supply or the helium gas supply, The evacuation and / or the supply of the inert gas or the helium gas is carried out under the condition that the content of the inert gas or the helium gas in the inside of the container is 50 vol % to 95 vol %. A method for drying a transport and / or storage container (1).
2. The method according to claim 1, wherein the initial evacuation of the vessel interior (4) is carried out until the pressure in the vessel interior (4) is between 8 mbar and 30 mbar.
3. After the initial evacuation, the water vapor partial pressure p H2O is calculated using the measured pressure rise Δp, and the filling pressure p required for the inert gas supply or helium gas supply to obtain the desired volume percent amount (50 vol% to 95 vol%) of inert gas or helium in the container (1) is calculated. tot The water vapor partial pressure p H2O The method according to claim 1 or 2, wherein the calculation is carried out from
4. 4. The method according to claim 1, further comprising the steps of: after the initial evacuation or after the pressure rise measurement, a continuous evacuation of the vessel interior (4) and a simultaneous continuous supply of inert gas or helium gas.
5. 5. The method according to any one of claims 1 to 4, wherein the continuous evacuation and the continuous inert gas supply or helium gas supply are performed for a period of at least 3 hours.
6. 6. The method according to claim 1, further comprising the steps of: terminating the continuous evacuation when the desired degree of dryness is reached in the container interior (4); and temporarily continuing to supply the container interior (4) with inert gas or helium gas until a predetermined pressure is reached in the container interior (4).
7. 7. The method according to claim 6, wherein the vessel interior (4) is filled with inert gas or helium gas to an interior pressure of 850 mbar to 1100 mbar.
8. 8. The method according to claim 1, wherein the inert gas or helium gas is supplied in the upper region of the vessel (1).
9. 9. The method according to claim 1, wherein the evacuation or evacuation of the vessel interior (4) is carried out in the lower region of the vessel (1) by means of at least one evacuation lance.
10. 10. The method according to claim 1, wherein the evacuation and the inert gas supply or the helium gas supply are carried out using at least one double tube (3) consisting of an outer tube (6) and an inner tube (5) surrounded by the outer tube (6).
Citation Information
Patent Citations
Spent fuel storage tank for vertical type and horizontal type storage
CN109545410A
Irradiated fuel assembly stores bucket vacuum drying helium charging unit
CN206697239U
Method and container for housing spent fuel
JP1997080196A
Method and device for replacing fluid in used-fuel transporting container
JP1999142583A
Method and device for storing spent fuel
JP2001242294A