Silicon carbide semiconductor device and manufacturing method thereof
The silicon carbide semiconductor device addresses the issue of high breakdown voltage by incorporating a gate electrode with an umbrella portion and a tailored gate insulating film to alleviate electric field concentration, thereby improving dielectric breakdown performance.
Patent Information
- Application Number
- JP2021537693
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-08-05
- Filing Date
- 2020-07-22
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-07-22
AI Technical Summary
Conventional silicon carbide semiconductor devices face challenges in achieving high breakdown voltages due to misalignment of the gate electrode, leading to excessive electric field concentration and dielectric breakdown of the gate insulating film.
The silicon carbide semiconductor device incorporates a gate electrode design with an umbrella portion that alleviates electric field concentration by having a maximum width closer to the main surface than the gate trench opening, and a gate insulating film with a specific curvature and composition to enhance dielectric strength.
This design improves the dielectric breakdown voltage by reducing electric field concentration and enhancing the insulation of the gate insulating film, even in the presence of manufacturing misalignments.
Smart Images

Figure 0007593320000001 
Figure 0007593320000002 
Figure 0007593320000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to silicon carbide semiconductor devices and methods for manufacturing the same.
[0002] This application claims priority to Japanese Application No. 2019-143975, filed on August 5, 2019, and incorporates by reference all of the contents of said Japanese application. [Background technology]
[0003] A silicon carbide semiconductor device is known in which a gate trench is formed in one main surface of a silicon carbide substrate, a gate electrode is provided extending from within the gate trench to above the main surface, and a gate insulating film is provided between the silicon carbide substrate and the gate electrode (for example, Patent Document 1). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 2019-96794 Summary of the Invention
[0005] A silicon carbide semiconductor device according to the present disclosure comprises a silicon carbide substrate having a main surface in which a gate trench is provided, a gate insulating film on the silicon carbide substrate, and a gate electrode on the gate insulating film, wherein the gate trench has an inner surface continuous with the main surface, the gate insulating film having a first portion provided on the inner surface and a second portion provided on the main surface and continuous with the first portion, the gate electrode having a base provided in the gate trench via the first portion, and an umbrella portion provided on the base and the second portion and in contact with the second portion, wherein in a cross-sectional view perpendicular to a longitudinal direction of the gate trench, a maximum width of the umbrella portion is greater than a width at an opening end of the gate trench, and a width of the umbrella portion is smaller than the maximum width on the main surface side than a position where the width of the umbrella portion is maximum. [Brief description of the drawings]
[0006] [Figure 1] FIG. 1 is a cross-sectional view showing a configuration of a silicon carbide semiconductor device according to the first embodiment. [Diagram 2] 2A to 2C are cross-sectional views (part 1) illustrating the method for manufacturing the silicon carbide semiconductor device according to the first embodiment. [Diagram 3] FIG. 3 is a cross-sectional view (part 2) illustrating the method for manufacturing the silicon carbide semiconductor device according to the first embodiment. [Figure 4] 4A to 4C are cross-sectional views (part 3) illustrating the method for manufacturing the silicon carbide semiconductor device according to the first embodiment. [Diagram 5] 5A to 5C are cross-sectional views (part 4) illustrating the method for manufacturing the silicon carbide semiconductor device according to the first embodiment. [Figure 6] 6A to 6C are cross-sectional views (part 5) illustrating the method for manufacturing the silicon carbide semiconductor device according to the first embodiment. [Figure 7] FIG. 7 is a cross-sectional view showing a configuration of a silicon carbide semiconductor device according to a modification of the first embodiment. As shown in FIG. [Figure 8] 8A to 8C are cross-sectional views (part 1) illustrating the method for manufacturing the silicon carbide semiconductor device according to the second embodiment. [Figure 9] FIG. 9 is a cross-sectional view (part 2) illustrating the method for manufacturing the silicon carbide semiconductor device according to the second embodiment. [Figure 10] 10A to 10C are cross-sectional views (part 3) illustrating the method for manufacturing the silicon carbide semiconductor device according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] [Problem that this disclosure aims to solve] Conventional silicon carbide semiconductor devices have difficulty in fully meeting the recent demand for higher breakdown voltages.
[0008] In view of the above, an object of the present disclosure is to provide a silicon carbide semiconductor device capable of improving the dielectric strength voltage of a gate insulating film, and a method for manufacturing the same.
[0009] [Effects of this disclosure] According to the present disclosure, the dielectric strength of the gate insulating film can be improved.
[0010] The embodiments for carrying out the invention are described below.
[0011] [Description of the embodiments of the present disclosure] First, the embodiments of the present disclosure are listed and described. In the following description, the same or corresponding elements are given the same symbols, and the same description will not be repeated. In the crystallographic description in this specification, individual faces are indicated with () and collective faces are indicated with {}. In addition, when a crystallographic index is negative, it is usually expressed by placing a "-" (bar) above the number, but in this specification, a negative sign is placed before the number.
[0012] [1] A silicon carbide semiconductor device according to one aspect of the present disclosure comprises a silicon carbide substrate having a main surface provided with a gate trench, a gate insulating film on the silicon carbide substrate, and a gate electrode on the gate insulating film, wherein the gate trench has an inner surface continuous with the main surface, the gate insulating film having a first portion provided on the inner surface and a second portion provided on the main surface and continuous with the first portion, the gate electrode having a base provided in the gate trench via the first portion, and an umbrella portion provided on the base and the second portion and in contact with the second portion, wherein in a cross-sectional view perpendicular to a longitudinal direction of the gate trench, a maximum width of the umbrella portion is greater than a width at an opening end of the gate trench, and a width of the umbrella portion is smaller than the maximum width on the main surface side than a position where the width of the umbrella portion is maximum.
[0013] The inventors have made extensive research and have found that one of the causes of dielectric breakdown of the gate insulating film is that the distance between the side of the gate electrode and the upper end of the trench is smaller than the design value due to misalignment of the gate electrode. In the structure of a conventional silicon carbide semiconductor device, the width of the gate electrode is maximum at the portion of the gate electrode that contacts the gate insulating film, so that an electric field is likely to concentrate at the lower end of the side of the gate electrode. Therefore, when the distance between the side of the gate electrode and the upper end of the gate trench is smaller than the design value, an excessive electric field is applied to the gate insulating film between the vicinity of the corner of the opening end of the gate trench, and sufficient dielectric strength may not be obtained. On the other hand, when the gate electrode includes the above-mentioned umbrella portion, the width of the umbrella portion of the gate electrode is smaller than the maximum width on the main surface side than the position where the width of the umbrella portion is maximum, so that the electric field concentration at the lower end of the side of the gate electrode can be alleviated. Therefore, even if the distance between the side of the gate electrode and the opening end of the gate trench becomes smaller than the design value due to misalignment during the manufacturing process, dielectric breakdown is suppressed by alleviating the electric field concentration, and the dielectric strength of the gate insulating film can be improved.
[0014] [2] In [1], a side surface of the umbrella portion may be a convex curved surface toward the main surface between a position where the umbrella portion contacts the gate insulating film and a position where the width of the gate electrode is at its maximum. If the side surface of the second portion is a convex curved surface toward the main surface between a position where the umbrella portion contacts the gate insulating film and a position where the width of the gate electrode is at its maximum, the change in slope from the portion where the width of the gate electrode is at its maximum to a portion above the portion where the width of the gate electrode is at its maximum becomes gentle, and electric field concentration is easily alleviated.
[0015] [3] In [2], the radius of curvature of the curved surface may be 10% to 20% of the thickness of the gate insulating film. When the radius of curvature of the curved surface is 10% to 20%, electric field concentration is moderately alleviated.
[0016] [4] In any one of [1] to [3], the gate insulating film may contain carbon. The gate insulating film containing carbon can be formed by thermal oxidation of a silicon carbide substrate.
[0017] [5] In any of [1] to [4], an insulating film having a different composition from the gate insulating film may be formed by thermal oxidation of the gate electrode, the insulating film being in contact with a side surface and an upper surface of the umbrella portion.
[0018] [6] In any one of [1] to [5], the gate trench may have a trench side surface having a {0-33-8} surface orientation. When the gate trench has a trench side surface having a {0-33-8} surface orientation, good mobility can be obtained on the side surface of the gate trench, and channel resistance can be reduced.
[0019] [7] In any one of [1] to [6], the distance between the main surface and a position on a side surface of the umbrella portion where the width of the gate electrode is maximum may be 5 nm to 15 nm. When this distance is 5 nm to 15 nm, an excellent dielectric strength voltage can be obtained by a simple process.
[0020] [8] A method for manufacturing a silicon carbide semiconductor device according to another aspect of the present disclosure includes the steps of: preparing a silicon carbide substrate having a main surface; forming a gate trench in the main surface, the gate trench having an inner surface continuous with the main surface; forming a gate insulating film on the silicon carbide substrate, the gate insulating film having a first portion provided on the inner surface and a second portion provided on the main surface and continuous with the first portion; and forming a gate insulating film on the gate insulating film, the gate insulating film having a base provided in the gate trench via the first portion, and a pseudo layer provided on the base and the second portion and in contact with the second portion. and forming a gate electrode from the pseudo gate electrode by thermally oxidizing the pseudo umbrella portion, the gate electrode having the base and an umbrella portion provided on the base and the second portion and in contact with the second portion, wherein after the thermal oxidation, in a cross-sectional view perpendicular to the longitudinal direction of the gate trench, a maximum width of the umbrella portion is greater than a width at an opening end of the gate trench, and a width of the umbrella portion is smaller than the maximum width on the main surface side than a position where the width of the umbrella portion is maximum.
[0021] In the thermal oxidation of the pseudo umbrella portion, oxidation proceeds preferentially in the vicinity of the portion where the pseudo umbrella portion contacts the gate insulating film, and the width of the pseudo umbrella portion where the pseudo umbrella portion contacts the gate insulating film becomes smaller than the maximum width. This makes it possible to alleviate the electric field concentration at the bottom end of the side surface of the gate electrode. Therefore, even if the distance between the side surface of the gate electrode and the top end of the trench becomes smaller than the design value due to misalignment during the manufacturing process, the alleviation of the electric field concentration suppresses dielectric breakdown, and the dielectric strength voltage of the gate insulating film can be improved.
[0022] [9] In the method of [8], a step of etching the gate insulating film may be included between the step of forming the pseudo gate electrode and the step of thermally oxidizing the pseudo umbrella portion, and an edge of the gate insulating film may be recessed inward from an edge of the pseudo umbrella portion after the etching. By recessing the edge of the gate insulating film inward from an edge of the pseudo umbrella portion before the thermal oxidation of the pseudo umbrella portion, a wider range of the pseudo gate electrode between the pseudo umbrella portion and the main surface can be oxidized, and a dielectric strength voltage can be further improved.
[0023] [Details of the embodiment of the present disclosure] Hereinafter, embodiments of the present disclosure will be described in detail, but the present embodiments are not limited to these.
[0024] [First embodiment] First, a first embodiment of the present disclosure will be described. The first embodiment relates to a so-called vertical silicon carbide semiconductor device. Fig. 1 is a cross-sectional view showing a configuration of the silicon carbide semiconductor device according to the first embodiment.
[0025] As shown in FIG. 1, the silicon carbide semiconductor device 100 according to the first embodiment mainly includes a silicon carbide substrate 1, a source electrode 16, a drain electrode 30, a source wiring 19, a gate insulating film 40, a gate electrode 50, and an interlayer insulating film 45. The silicon carbide substrate 1 includes a silicon carbide single crystal substrate 11 and a silicon carbide epitaxial layer 2. The silicon carbide epitaxial layer 2 is provided on the silicon carbide single crystal substrate 11. The silicon carbide substrate 1 has a first main surface 10 and a second main surface 20. The second main surface 20 is on the opposite side to the first main surface 10. The silicon carbide epitaxial layer 2 constitutes the first main surface 10. The silicon carbide single crystal substrate 11 constitutes the second main surface 20.
[0026] First main surface 10 is, for example, a (000-1) plane or a plane inclined at an off angle of less than 8° with respect to the (000-1) plane. The off angle may be 6° or less, or 4° or less. The off angle may be 2° or more. Silicon carbide single crystal substrate 11 and silicon carbide epitaxial layer 2 are, for example, hexagonal silicon carbide of polytype 4H. Silicon carbide single crystal substrate 11 contains an n-type impurity such as nitrogen (N) and has n-type conductivity.
[0027] Drain electrode 30 is provided on second main surface 20. Drain electrode 30 is made of a material containing, for example, nickel silicide (NiSi) in the case of n-type, or titanium aluminum (TiAl) in the case of p-type, depending on the conductivity type of silicon carbide single crystal substrate 11. Drain electrode 30 may be made of a material containing, for example, titanium aluminum silicon (TiAlSi) regardless of whether it is n-type or p-type.
[0028] Silicon carbide substrate 1 mainly includes drift region 12, body region 13, source region 14, and contact region 18. Drift region 12 includes n-type impurities such as nitrogen and has n-type conductivity (first conductivity type). The concentration of n-type impurities in drift region 12 is, for example, 7×10 15 cm -3 The concentration of n-type impurities in silicon carbide single crystal substrate 11 may be higher than the concentration of n-type impurities in drift region 12.
[0029] The body region 13 is on the drift region 12. The body region 13 is in contact with the drift region 12. The body region 13 contains p-type impurities such as aluminum (Al) and has p-type conductivity (second conductivity type). A channel can be formed in a region of the body region 13 facing the gate insulating film 40.
[0030] The source region 14 is on the body region 13. The source region 14 is in contact with the body region 13. The source region 14 is separated from the drift region 12 by the body region 13. The source region 14 contains n-type impurities such as nitrogen or phosphorus (P) and has n-type conductivity. The source region 14 constitutes a part of the first main surface 10. The concentration of the n-type impurity in the source region 14 may be higher than the concentration of the n-type impurity in the drift region 12.
[0031] The contact region 18 is in contact with, for example, the body region 13 and the source region 14. The contact region 18 contains p-type impurities such as aluminum and has p-type conductivity. The concentration of the p-type impurities contained in the contact region 18 may be higher than the concentration of the p-type impurities contained in the body region 13. The contact region 18 connects the body region 13 and the first main surface 10. The contact region 18 may constitute a part of the first main surface 10. The concentration of the n-type impurities or p-type impurities in each of the impurity regions can be measured by, for example, secondary ion mass spectrometry (SIMS).
[0032] A gate trench 6 is provided on the first main surface 10. For example, the first main surface 10 has a flat portion 5, and the gate trench 6 has an inner surface 6A including a trench side surface 3 and a bottom surface 4. The gate trench 6 is defined by the trench side surface 3 and the bottom surface 4. The trench side surface 3 is continuous with the flat portion 5. In other words, the inner surface 6A is continuous with the first main surface 10. The trench side surface 3 penetrates the body region 13 and the source region 14 to reach the drift region 12. The bottom surface 4 is continuous with the trench side surface 3. The bottom surface 4 is located in the drift region 12.
[0033] In a cross-sectional view from a direction perpendicular to the longitudinal direction of the gate trench 6, the gate trench 6 has, for example, a U-shape. That is, in the cross-sectional view, the trench side surface 3 is approximately perpendicular to the flat portion 5, and the bottom surface 4 is approximately parallel to the flat portion 5. The source region 14, the body region 13, and the drift region 12 form the trench side surface 3 of the gate trench 6. The drift region 12 forms the bottom surface 4 of the gate trench 6.
[0034] The gate insulating film 40 is provided on the inner surface 6A and the first main surface 10. The gate insulating film 40 separates the gate electrode 50 and the silicon carbide substrate 1. The gate insulating film 40 is, for example, a thermally oxidized film of silicon carbide. The gate insulating film 40 is made of, for example, a material containing silicon dioxide (SiO2) and carbon (C). The proportion of carbon in the gate insulating film 40 is, for example, not less than 10 mass % and not more than 90 mass %. The proportion of carbon here can be measured, for example, by a SIMS method.
[0035] The gate insulating film 40 has a thickness of, for example, about 20 nm or more and 80 nm or less. The gate insulating film 40 contacts the source region 14, the body region 13, and the drift region 12 at the trench side surface 3. The gate insulating film 40 contacts the drift region 12 at the bottom surface 4. The gate insulating film 40 has a first portion 41 provided on the inner surface 6A, and a second portion (flange portion) 42 provided on the first main surface 10 and continuous with the first portion 41.
[0036] The gate electrode 50 is made of polysilicon containing an impurity such as phosphorus. The impurity such as phosphorus is contained, for example, to adjust the threshold voltage. The gate electrode 50 has a T-shaped cross-sectional shape in a cross-sectional view. That is, the gate electrode 50 has a base 51 in the gate trench 6 and an umbrella portion 52 on the base 51. The umbrella portion 52 protrudes to both sides of the gate trench 6 in the in-plane direction and covers the second portion 42 of the gate insulating film 40. The in-plane direction is an in-plane direction perpendicular to the thickness direction of the silicon carbide substrate 1. The lower end of the side surface 53 of the umbrella portion 52 contacts the second portion 42. The side surface 53 has an upper inclined portion 54 that is spaced apart from the base 51 in the in-plane direction as it moves downward from the upper end of the umbrella portion 52, and a lower inclined portion 55 that is spaced apart from the base 51 in the in-plane direction as it moves upward from a contact portion 57 with the second portion 42 of the gate insulating film 40.
[0037] The width of the gate electrode 50 is maximum at the height of the boundary 56 between the upper inclined portion 54 and the lower inclined portion 55. That is, the gate electrode 50 has a maximum width WG1 of the gate electrode 50 at the height of the boundary 56. Moreover, the width WG1 at the height of the boundary 56 is larger than the opening width WT at the upper end of the gate trench 6. In the lower inclined portion 55, the side surface 53 is farther away from the base portion 51 in the in-plane direction as it moves upward from the contact portion 57 with the second portion 42, so that the width WG2 at the contact portion 57 of the gate electrode 50 is smaller than the width WG1. That is, the width of the umbrella portion 52 is smaller than the maximum width WG1 on the first main surface 10 side than the position where the width of the umbrella portion 52 is maximum. As described later, the upper inclined portion 54 and the lower inclined portion 55 may be formed by thermal oxidation of the gate electrode 50, and the lower inclined portion 55 is, for example, a convex curved surface toward the first main surface 10 between the contact portion 57 and the boundary 56. The radius of curvature of this convex curved surface is preferably 10% or more and 20% or less of the thickness of the gate insulating film 40. If the radius of curvature is less than 10% of the thickness of the gate insulating film 40, the boundary 56 having the maximum width WG1 of the gate electrode 50 is too close to the gate insulating film 40, and it may be difficult to obtain an excellent dielectric strength voltage. If the radius of curvature is more than 20% of the thickness of the gate insulating film 40, when the upper inclined portion 54 and the lower inclined portion 55 are formed by thermal oxidation of the gate electrode 50, the thermal oxidation of the gate electrode 50 may be excessive. For example, during the thermal oxidation of the gate electrode 50, new oxygen atoms may reach the interface between the gate insulating film 40 and the body region 13, further oxidizing the body region 13, and the characteristics of this interface may be deteriorated. More preferably, the radius of curvature of the convex curved surface of the lower inclined portion 55 is 15% or more and 20% or less of the thickness of the gate insulating film 40. Specifically, the radius of curvature of the convex curved surface of the lower inclined portion 55 is, for example, not less than 5 nm and not more than 15 nm, and preferably not less than 10 nm and not more than 15 nm.
[0038] It is preferable that side surface 53 has a gentle convex curve at boundary 56. This is because if the slope of side surface 53 changes abruptly near boundary 56, an electric field is likely to concentrate near boundary 56. Base portion 51 is an example of a first portion, and umbrella portion 52 is an example of a second portion. In the thickness direction of silicon carbide substrate 1, the thickness of a portion of gate electrode 50 located closer to the bottom of gate trench 6 than first main surface 10 is, for example, 60% to 90% of the thickness of gate electrode 50.
[0039] A coated insulating film 60 is formed in contact with the side surface 53 and the top surface 58 of the umbrella portion 52. The coated insulating film 60 is, for example, a thermally oxidized film of polysilicon containing impurities such as phosphorus. The coated insulating film 60 is made of, for example, silicon dioxide and a material containing impurities such as phosphorus. Between the umbrella portion 52 and the flat portion 5, the coated insulating film 60 has a bird's beak shape. Between the boundary 56 and the flat portion 5, the coated insulating film 60 and the gate insulating film 40 are present, and the distance L between the boundary 56 and the flat portion 5 is preferably 5 nm or more and 15 nm or less, more preferably 10 nm or more and 15 nm or less. If the distance L is less than 5 nm, the boundary 56 having the maximum width WG1 of the gate electrode 50 is too close to the gate insulating film 40, and it may be difficult to obtain an excellent dielectric strength voltage. To make the distance L exceed 15 nm, a complicated process may be required.
[0040] The interlayer insulating film 45 is provided in contact with the cover insulating film 60 and the gate insulating film 40. The interlayer insulating film 45 is made of a material containing silicon dioxide, for example. The interlayer insulating film 45 and the cover insulating film 60 electrically insulate the gate electrode 50 and the source electrode 16 from each other.
[0041] The source electrode 16 is in contact with the first main surface 10. Specifically, the source electrode 16 is in contact with the source region 14 on the first main surface 10. The source electrode 16 may be in contact with the contact region 18. The source electrode 16 is made of a material including, for example, titanium (Ti), aluminum, and silicon (Si). The source electrode 16 is in ohmic contact with, for example, the source region 14. The source wiring 19 is in contact with the source electrode 16. The source wiring 19 is made of a material including, for example, aluminum.
[0042] Next, a method for manufacturing the silicon carbide semiconductor device 100 according to the first embodiment will be described. Figures 2 to 6 are cross-sectional views showing the method for manufacturing the silicon carbide semiconductor device 100 according to the first embodiment.
[0043] First, as shown in FIG. 2, a silicon carbide substrate 1 is prepared. For example, a sublimation method is used to prepare a silicon carbide single crystal substrate 11. The maximum diameter of the silicon carbide single crystal substrate 11 is, for example, 100 mm or more, and preferably 150 mm or more. Next, an epitaxial layer is formed on the silicon carbide single crystal substrate 11. For example, a drift region is formed by epitaxial growth on the silicon carbide single crystal substrate 11 by a chemical vapor deposition (CVD) method using a mixed gas of silane (SiH4) and propane (C3H8) as a source gas, hydrogen gas (H2) as a carrier gas, and ammonia (NH3) as a dopant gas.
[0044] Next, ion implantation is performed. A p-type impurity such as aluminum is ion-implanted into the surface of the drift region 12. This forms a body region 13 in contact with the drift region 12. Next, an n-type impurity such as phosphorus is ion-implanted into the body region 13. This forms a source region 14 having an n-type conductivity. The source region 14 constitutes the first main surface 10. The concentration of the n-type impurity contained in the source region 14 is higher than the concentration of the p-type impurity contained in the body region 13. Next, a p-type impurity such as aluminum is ion-implanted into the source region 14 to form a contact region 18.
[0045] Next, activation annealing is performed to activate the impurity ions implanted into silicon carbide substrate 1. The temperature of the activation annealing is preferably 1500° C. or higher and 1900° C. or lower. The time of the activation annealing is, for example, about 30 minutes. The atmosphere of the activation annealing is preferably an inert gas atmosphere, for example an argon (Ar) atmosphere.
[0046] Next, as shown in FIG. 3, a gate trench 6 is formed. For example, a mask having an opening at a position where the gate trench 6 is to be formed is formed on the first main surface 10 including the source region 14 and the contact region 18. Then, a part of the source region 14, a part of the body region 13, and a part of the drift region are removed by etching using the mask. As an etching method, for example, reactive ion etching (RIE), particularly inductively coupled plasma reactive ion etching (ICP-RIE), can be used. Specifically, for example, inductively coupled plasma reactive ion etching using sulfur hexafluoride (SF6) or a mixed gas of SF6 and oxygen (O2) as a reactive gas can be used. After the gate trench 6 is formed, the mask is removed.
[0047] Next, the gate insulating film 40 is formed. For example, the silicon carbide substrate 1 is heated in an atmosphere containing oxygen at a temperature of, for example, 1300° C. or more and 1400° C. or less. As a result, the gate insulating film 40 including the first portion 41 and the second portion 42 is formed. The first portion 41 contacts the drift region 12 at the bottom surface 4, and contacts the drift region 12, the body region 13, and the source region 14 at the trench side surface 3. The gate insulating film 40 formed by thermal oxidation of the silicon carbide substrate 1 contains, for example, silicon dioxide and carbon. The gate insulating film 40 may be formed by other methods such as a CVD method. When the gate insulating film 40 is formed by thermal oxidation, a part of the silicon carbide substrate 1 is taken into the gate insulating film 40. For this reason, in the subsequent processing, it is assumed that the first main surface 10 and the inner surface 6A have moved slightly to the interface between the gate insulating film 40 and the silicon carbide substrate 1 after thermal oxidation. On the other hand, when the gate insulating film 40 is formed by a deposition method such as a CVD method, the silicon carbide substrate 1 is not incorporated into the gate insulating film 40, so that the positions of the first main surface 10 and the inner surface 6A do not move.
[0048] After the gate insulating film 40 is formed, the silicon carbide substrate 1 may be subjected to a heat treatment (NO annealing) in a nitric oxide (NO) gas atmosphere. In the NO annealing, the silicon carbide substrate 1 is held, for example, for about one hour under conditions of 1100° C. or more and 1300° C. or less. This introduces nitrogen atoms into the interface region between the gate insulating film 40 and the body region 13. As a result, the formation of interface states in the interface region is suppressed, and the channel mobility can be improved. Note that, if nitrogen atoms can be introduced, a gas other than NO gas (for example, N2O) may be used as the atmosphere gas. After the NO annealing, Ar annealing using argon (Ar) as the atmosphere gas may be further performed. The heating temperature of the Ar annealing is, for example, equal to or higher than the heating temperature of the NO annealing. The time of the Ar annealing is, for example, about one hour. This further suppresses the formation of interface states in the interface region between the gate insulating film 40 and the body region 13.
[0049] Next, the pseudo gate electrode 50X is formed. For example, a polysilicon film is deposited by a low pressure chemical vapor deposition (LPCVD) method, and then the polysilicon film is dry etched. At this point, the pseudo gate electrode 50X has a base 51 and a pseudo umbrella portion 52X, and a side surface 53X of the pseudo umbrella portion 52X is an inclined surface that is spaced apart from the base 51 in the in-plane direction as it goes downward from the upper end of the pseudo umbrella portion 52X.
[0050] Next, as shown in FIG. 4, the coated insulating film 60 is formed. For example, the pseudo gate electrode 50X is heated in an atmosphere containing oxygen at a temperature of, for example, 850° C. to 950° C. The ratio of oxygen in the atmosphere is, for example, 10% by volume to 100% by volume, and preferably 80% by volume to 90% by volume. As a result, the gate electrode 50 having the base 51 and the umbrella portion 52 is formed from the pseudo gate electrode 50X, and the coated insulating film 60 contacting the side surface 53 and the upper surface 58 of the umbrella portion 52 is formed. The oxidation of the side surface 53X does not progress uniformly, and oxidation progresses preferentially in the vicinity of the contact portion 57 with the second portion 42. As a result, a lower inclined portion 55 is formed on the side surface 53, which is spaced apart from the base 51 in the in-plane direction as it moves upward from the contact portion 57. In the portion not affected by the preferential oxidation, the oxidation progresses almost uniformly, forming an upper inclined portion 54 that is spaced apart from the base portion 51 in the in-plane direction from the upper end of the umbrella portion 52 downward. The coated insulating film 60 formed by thermal oxidation of the pseudo gate electrode 50X contains impurities such as silicon dioxide and phosphorus.
[0051] As a result, the width of the gate electrode 50 is maximum at the height of the boundary 56 between the upper inclined portion 54 and the lower inclined portion 55. That is, the umbrella portion 52 has the maximum width WG1 of the gate electrode 50 at the height of the boundary 56. Moreover, the width WG1 at the height of the boundary 56 is larger than the opening width WT at the upper end of the gate trench 6. In the lower inclined portion 55, the side surface 53 is farther away from the base portion 51 in the in-plane direction as it goes upward from the contact portion 57, so that the width WG2 of the gate electrode 50 at the contact portion 57 is smaller than the width WG1. That is, the width of the umbrella portion 52 is smaller than the maximum width WG1 on the first main surface 10 side than the position where the width of the umbrella portion 52 is maximum.
[0052] Moreover, the degree of oxidation of side surface 53X changes continuously, and lower inclined portion 55 of side surface 53 becomes a convex curved surface toward first main surface 10, for example, between contact portion 57 and boundary 56. As a result, coated insulating film 60 has a bird's beak shape between umbrella portion 52 and flat portion 5. Moreover, side surface 53 becomes a convex curved surface at boundary 56 as well.
[0053] Next, as shown in FIG. 5, an interlayer insulating film 45 is formed. For example, the interlayer insulating film 45 is formed so as to cover the gate electrode 50 and the cover insulating film 60 and to be in contact with the gate insulating film 40. The interlayer insulating film 45 is formed, for example, by a CVD method. The interlayer insulating film 45 is made of a material containing silicon dioxide, for example. Next, a part of the interlayer insulating film 45 and the gate insulating film 40 is etched so as to form openings on the source region 14 and the contact region 18. As a result, the contact region 18 and the source region 14 are exposed from the gate insulating film 40.
[0054] Next, as shown in FIG. 6, the source electrode 16 and the source wiring 19 are formed. Specifically, the source electrode 16 is formed in contact with the source region 14 and the contact region 18 on the first main surface 10. The source electrode 16 is formed by, for example, a sputtering method. The source electrode 16 is made of, for example, a material including Ti, Al, and Si. Next, alloying annealing is performed. Specifically, the source electrode 16 in contact with the source region 14 and the contact region 18 is held at a temperature of, for example, 900° C. or more and 1100° C. or less for about 5 minutes. As a result, at least a part of the source electrode 16 reacts with the silicon contained in the silicon carbide substrate 1 and is silicided. As a result, the source electrode 16 that is in ohmic contact with the source region 14 is formed. Next, the source wiring 19 that is electrically connected to the source electrode 16 is formed. The source wiring 19 is formed on the source electrode 16 and the interlayer insulating film 45.
[0055] Next, the drain electrode 30 is formed on the second main surface 20. The drain electrode 30 is made of a material containing, for example, NiSi. The material constituting the drain electrode 30 is formed by, for example, sputtering. Next, the material formed by sputtering is subjected to laser annealing. As a result, the material constituting the drain electrode 30 is alloyed. Note that, instead of alloying by laser annealing, alloying by heat treatment, for example, rapid thermal annealing (RTA) treatment, may be performed. The rear surface of the silicon carbide substrate 1 may be polished before the formation of the drain electrode 30.
[0056] In this manner, silicon carbide semiconductor device 100 according to the first embodiment can be manufactured.
[0057] In the silicon carbide semiconductor device 100 according to the first embodiment, the width WG2 at the contact portion 57 of the gate electrode 50 is smaller than the width WG1 at the height of the boundary 56 between the upper inclined portion 54 and the lower inclined portion 55. This makes it possible to alleviate electric field concentration at the lower end of the side surface 53 of the umbrella portion 52. Therefore, even if the distance between the side surface 53 of the gate electrode 50 and the upper end of the gate trench 6 becomes smaller than the design value due to misalignment of the gate electrode 50 during the manufacturing process, an excellent dielectric strength voltage can be obtained.
[0058] Moreover, the lower inclined portion 55 can be easily formed into a convex curved surface by thermal oxidation of the gate electrode 50. When the lower inclined portion 55 is formed into a convex curved surface, the change in the inclination of the side surface 53 is gentle, and the electric field concentration can be further alleviated.
[0059] Furthermore, since the insulating cover film 60 formed by, for example, thermal oxidation of the gate electrode 50 is present between the gate insulating film 40 and the umbrella portion 52, the electric field applied to the gate insulating film 40 can be further alleviated.
[0060] Furthermore, according to the above manufacturing method, even if the gate electrode 50 is misaligned, the gate electrode 50 and the insulating cover film 60 can be easily formed to have an appropriate width and to suppress electric field concentration.
[0061] [Modification of the first embodiment] Next, a modification of the first embodiment will be described. The modification differs from the first embodiment in the cross-sectional shape of the gate trench. Fig. 7 is a cross-sectional view showing a configuration of a silicon carbide semiconductor device according to the modification of the first embodiment.
[0062] In the silicon carbide semiconductor device 100 according to the first embodiment, the gate trench 6 has a U-shape in cross section, whereas in the silicon carbide semiconductor device 101 according to the modification, the gate trench 6 has a V-shape in cross section. That is, in the silicon carbide semiconductor device 101, the trench side surface 3 is inclined such that the width of the gate trench 6 tapers toward the bottom surface 4 in cross section. The trench side surface 3 is inclined at an angle of 52° or more and 72° or less with respect to the (000-1) plane, for example. The trench side surface 3 includes, for example, a {0-33-8} plane. The bottom surface 4 is approximately parallel to the flat portion 5.
[0063] The other configuration is similar to that of the first embodiment.
[0064] The silicon carbide semiconductor device 101 according to the modified example also provides the same effects as those of the silicon carbide semiconductor device 100. Furthermore, since the trench side surface 3 is inclined within an appropriate range with respect to the (000-1) plane, good mobility can be obtained on the trench side surface 3, and the channel resistance can be reduced.
[0065] Second Embodiment Next, a second embodiment will be described. The second embodiment differs from the first embodiment in terms of the manufacturing method. Based on the difference in the manufacturing method, the second embodiment also differs from the first embodiment in terms of the configurations of the gate electrode 50 and the coated insulating film 60. Below, the manufacturing method of the silicon carbide semiconductor device according to the second embodiment will be described, while the configuration of the silicon carbide semiconductor device according to the second embodiment will also be described. FIGS. 8 to 10 are cross-sectional views showing the manufacturing method of the silicon carbide semiconductor device according to the second embodiment.
[0066] First, similarly to the first embodiment, the process up to the formation of the pseudo gate electrode 50X is performed (see FIG. 3). Next, as shown in FIG. 8, a part of the gate insulating film 40 on the flat portion 5 is removed. Specifically, of the gate insulating film 40 on the flat portion 5, a part exposed from the pseudo gate electrode 50X and a part near both sides of the pseudo umbrella portion 52X between the pseudo umbrella portion 52X of the pseudo gate electrode 50X and the flat portion 5 are removed, and a part of the gate insulating film 40 is left between the pseudo umbrella portion 52X and the flat portion 5. That is, the edge of the gate insulating film 40 is recessed inward from the edge of the pseudo umbrella portion 52X. As a result, a part of the lower surface 59 of the pseudo umbrella portion 52X is exposed. The ratio of the part of the gate insulating film 40 removed between the pseudo umbrella portion 52X and the flat portion 5 is, for example, about 1% to 5%. The part of the gate insulating film 40 is removed by, for example, wet etching. For example, hydrofluoric acid (HF) is used as an etching solution for the wet etching.
[0067] Next, as shown in FIG. 9, the coated insulating film 60 is formed. For example, the pseudo gate electrode 50X is heated in an atmosphere containing oxygen at a temperature of, for example, 850° C. to 950° C. The ratio of oxygen in the atmosphere is, for example, 10% by volume to 100% by volume, and preferably 80% by volume to 90% by volume. As a result, the gate electrode 50 having the base 51 and the umbrella portion 52 is formed from the pseudo gate electrode 50X, and the coated insulating film 60 in contact with the side surface 53 and the upper surface 58 of the umbrella portion 52 is formed. The oxidation of the side surface 53X does not progress uniformly, and oxidation progresses preferentially in the vicinity of the contact portion 57 with the second portion 42. As a result, a lower inclined portion 55 is formed on the side surface 53, which is spaced apart from the base 51 in the in-plane direction as it moves upward from the contact portion 57. In the portion not affected by preferential oxidation, the oxidation progresses almost uniformly, forming an upper inclined portion 54 that is spaced further away from the base portion 51 in the in-plane direction as it moves downward from the upper end of the umbrella portion 52. As a result, an upper inclined portion 54 and a lower inclined portion 55 are formed on the side surface 53. In addition, since the flat portion 5 is also oxidized, the gate insulating film 40 again comes to include portions in contact with the source region 14 and the contact region 18.
[0068] In the second embodiment, before the formation of the insulating cover 60, a part of the gate insulating film 40 is removed between the pseudo umbrella portion 52X and the flat portion 5. Therefore, the insulating cover 60 penetrates closer to the base 51 compared to the first embodiment. In other words, the insulating cover 60 has a bird's beak shape with a deeper tip compared to the first embodiment.
[0069] Next, as shown in FIG. 10, the processes after the formation of the interlayer insulating film 45 are carried out in the same manner as in the first embodiment.
[0070] In this manner, silicon carbide semiconductor device 200 according to the second embodiment can be manufactured.
[0071] In the silicon carbide semiconductor device 200 according to the second embodiment, the coated insulating film 60 can be formed over a wider range in the thickness direction of the silicon carbide substrate 1 between the umbrella portion 52 and the flat portion 5, thereby enabling a further improvement in the dielectric strength voltage.
[0072] Although the embodiments have been described in detail above, the present invention is not limited to the specific embodiments, and various modifications and changes are possible within the scope of the claims. [Explanation of symbols]
[0073] 1: Silicon carbide substrate 2: Silicon carbide epitaxial layer 3: Trench side 4: Bottom 5: Flat part 6: Gate trench 6A: Inner surface 10: First main surface 11: Silicon carbide single crystal substrate 12: Drift region 13: Body area 14: Source area 16: Source electrode 18: Contact area 19: Source wiring 20: Second main surface 30: Drain electrode 40: Gate insulating film 41: Part 1 42:Second part 45: Interlayer insulating film 50: Gate electrode 50X: Pseudo gate electrode 51: Base 52: Umbrella part 52X: Pseudo umbrella part 53, 53X: Side 54: Upper slope 55: Lower slope part 56: Boundary 57: Contact part 58:Top surface 59: Bottom surface 60: Covered insulation film 100, 101, 200: Silicon carbide semiconductor device
Claims
1. a silicon carbide substrate having a main surface provided with a gate trench; a gate insulating film on the silicon carbide substrate; a gate electrode on the gate insulating film; having the gate trench has an inner surface continuous with the main surface, The gate insulating film is A first portion disposed on the inner surface; A second portion provided on the main surface and connected to the first portion; having The gate electrode is a base provided in the gate trench via the first portion; a cap portion provided on the base and the second portion and in contact with the second portion; having A cross-sectional view taken along a direction perpendicular to a longitudinal direction of the gate trench, the maximum width of the umbrella portion is greater than the width of the gate trench at an opening end thereof; a side surface of the umbrella portion is a convex curved surface toward the main surface between a position where the umbrella portion contacts the gate insulating film and a position where the width of the gate electrode is maximum, a width of the umbrella portion on the main surface side relative to a position where the width of the umbrella portion is maximum, the width being smaller than the maximum width;
2. The silicon carbide semiconductor device according to claim 1 , wherein a radius of curvature of said curved surface is equal to or greater than 10% and equal to or less than 20% of a thickness of said gate insulating film.
3. The silicon carbide semiconductor device according to claim 1 , wherein the gate insulating film contains carbon.
4. The silicon carbide semiconductor device according to claim 1 , further comprising an insulating film in contact with a side surface and an upper surface of the umbrella portion, the insulating film having a composition different from that of the gate insulating film.
5. 5. The silicon carbide semiconductor device according to claim 1, wherein the gate trench includes a trench side surface having a plane orientation of {0-33-8}.
6. 6 . The silicon carbide semiconductor device according to claim 1 , wherein a distance between a position on a side surface of the umbrella portion where the width of the gate electrode is maximum and the main surface is not less than 5 nm and not more than 15 nm.
7. A silicon carbide substrate having a main surface provided with a gate trench; a gate insulating film on the silicon carbide substrate; a gate electrode on the gate insulating film; having the gate trench has an inner surface continuous with the main surface, The gate insulating film is A first portion disposed on the inner surface; A second portion provided on the main surface and connected to the first portion; having The gate electrode is a base provided in the gate trench via the first portion; a cap portion provided on the base and the second portion and in contact with the second portion; having A cross-sectional view taken along a direction perpendicular to a longitudinal direction of the gate trench, the maximum width of the umbrella portion is greater than the width of the gate trench at an opening end thereof; The width of the umbrella portion is smaller than the maximum width on the main surface side than the position where the width of the umbrella portion is maximum, a distance between the main surface and a position on a side surface of the umbrella portion where the width of the gate electrode is maximum is equal to or greater than 5 nm and equal to or less than 15 nm;
8. providing a silicon carbide substrate having a main surface; forming a gate trench in the main surface, the gate trench having an inner surface continuous with the main surface; forming a gate insulating film on the silicon carbide substrate, the gate insulating film having a first portion provided on the inner surface and a second portion provided on the main surface and continuous with the first portion; forming a pseudo gate electrode on the gate insulating film, the pseudo gate electrode having a base portion provided in the gate trench via the first portion, and a pseudo umbrella portion provided on the base portion and the second portion and in contact with the second portion; forming a gate electrode from the pseudo gate electrode by thermally oxidizing the pseudo umbrella portion, the gate electrode having the base portion and an umbrella portion provided on the base portion and the second portion and in contact with the second portion; having After the thermal oxidation, in a cross-sectional view taken in a direction perpendicular to the longitudinal direction of the gate trench, the maximum width of the umbrella portion is greater than the width of the gate trench at an opening end thereof; A method for manufacturing a silicon carbide semiconductor device, wherein a width of the umbrella portion is smaller on the main surface side than a position where the width of the umbrella portion is maximum, than the maximum width.
9. Between the step of forming the pseudo gate electrode and the step of thermally oxidizing the pseudo umbrella portion, Etching the gate insulating film, The method for manufacturing a silicon carbide semiconductor device according to claim 8 , wherein after said etching, an edge of said gate insulating film is recessed inward from an edge of said pseudo umbrella portion.
Citation Information
Patent Citations
Semiconductor device and manufacturing method thereof
JP2014222734A
Silicon carbide semiconductor device and manufacturing method of the same
JP2015156429A
Silicon carbide semiconductor device manufacturing method and silicon carbide semiconductor device
JP2016012677A
Semiconductor device and method for manufacturing the same
JP2016018860A
Silicon carbide semiconductor device and silicon carbide semiconductor device manufacturing method