Semiconductor device and its manufacturing method
A semiconductor device with a thick gate oxide film on the drain side and strategically positioned LDD regions suppresses GIDL, enhancing performance by expanding the potential barrier and reducing electric field strength while maintaining cost-effectiveness.
Patent Information
- Application Number
- JP2023067885
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-04-18
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2043-04-18
AI Technical Summary
Increasing the thickness of the oxide on the source side of a MOSFET leads to increased source resistance and difficulty in securing electric current, while gate-induced drain leakage (GIDL) is exacerbated by the electric field strength between the gate and drain-side LDD, necessitating a solution that suppresses GIDL without increasing manufacturing costs.
A semiconductor device with a gate oxide film having a thick film portion on the drain side and a source-side LDD region spaced apart from the drain side LDD region, along with a shallow drain region, is manufactured using conventional processes to reduce GIDL without additional costs.
The solution effectively suppresses GIDL by expanding the potential barrier and reducing electric field strength, improving semiconductor device performance without increasing manufacturing costs.
Smart Images

Figure 0007593565000001 
Figure 0007593565000002 
Figure 0007593565000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device and a manufacturing method thereof. [Background technology]
[0002] Patent Document 1 describes a technique for improving the on-resistance and breakdown voltage of an LDMOSFET by increasing the thickness of the oxide on the drain side without adversely affecting the field oxide film that separates elements. LDMOSFETs do not have LDD (Lightly Doped Drain) implantation on the source side, and their impurity profiles (source-drain (SD), LDD, channel, etc.) are significantly different from those of general MVMOSFETs. Therefore, if the LDMOSFET structure is adopted as is, the source resistance will be high and I on In addition, in a MOSFET (MVMOSFET) with a gate voltage of 8 V, when the substrate bias voltage is 0 V, the leakage current due to gate-induced drain leakage (GIDL) may be constant at the order of 1+e-11 A / μm, regardless of the amount of overlap between the polysilicon gate electrode and the LDD.
[0003] In addition, in a MOSFET with a thicker oxide on the drain side and a gate voltage of 8 V, I off In order to obtain a current performance of the order of 1e-15 [A / μm], it is necessary to reduce the GIDL. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] U.S. Patent No. 8,119,507 Summary of the Invention [Problem to be solved by the invention]
[0005] In MVMOSFETs, if the thickness of the oxide on the source side is increased, the source resistance becomes too large when the gate voltage is less than 10 V, and the I on In addition, since GIDL is caused by the electric field strength between the gate and the drain-side LDD, it is necessary to reduce the electric field strength between the gate and the LDD in order to suppress GIDL.
[0006] The present invention has been made in consideration of the above circumstances, and has an object to provide a semiconductor device and a manufacturing method thereof that can suppress GIDL of the semiconductor device without increasing manufacturing costs. [Means for solving the problem]
[0007] A semiconductor device according to a first aspect of the present disclosure includes a gate oxide film having a thick film portion formed on the drain side to be thicker than the source side, a drain-side LDD region formed to cover a lower surface of the thick film portion, a source-side LDD region formed on the lower surface of the gate oxide film and spaced apart in the width direction from the drain-side LDD region, and a drain region formed on the drain side of the drain-side end of the thick film portion and with a junction position shallower than the junction position of the drain-side LDD region.
[0008] A manufacturing method of a semiconductor device according to a second aspect of the present disclosure is a manufacturing method of a semiconductor device including a FET, and includes a gate oxide film formation step of forming a gate oxide film having a thick film portion on the drain side that is formed to be thicker than the source side, an LDD region formation step of forming a drain-side LDD region so as to cover a lower surface of the thick film portion and a source-side LDD region on the lower surface of the gate oxide film and spaced apart in the width direction from the drain-side LDD region, and a drain region formation step of forming a drain region by injecting impurities into the drain-side LDD region on the drain side of the drain-side end of the thick film portion with an injection energy lower than the injection energy of impurities used to form the drain-side LDD region. Effect of the Invention
[0009] According to the present invention, it is possible to suppress GIDL in a semiconductor device without increasing the manufacturing cost. [Brief description of the drawings]
[0010] [Figure 1] 1 is a cross-sectional view showing the structure of an MVMOSFET according to one embodiment of the present invention. [Diagram 2] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Diagram 3] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 4] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Diagram 5] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 6] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 7] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 8] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 9] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 10] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 11] 1A to 1C are diagrams illustrating a manufacturing process of an MVMOSFET according to an embodiment of the present invention. [Figure 12] FIG. 2 is a comparison diagram of potential barriers of an MVMOSFET in accordance with an embodiment of the present invention. [Figure 13] 4 is a graph illustrating a comparison of output characteristics of an MVMOSFET in accordance with an embodiment of the present invention. [Figure 14] FIG. 2 is a comparison diagram of potential barriers of an MVMOSFET in accordance with an embodiment of the present invention. [Figure 15] FIG. 11 is a cross-sectional view of an example of the structure of an MVMOSFET according to another embodiment of the present invention. [Figure 16] FIG. 11 is a cross-sectional view of an example of the structure of an MVMOSFET according to another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of a semiconductor device and a manufacturing method thereof according to the present invention will be described with reference to the drawings.
[0012] (MVMOSFET embodiment 1) Fig. 1 is a cross-sectional view showing the structure of an MVMOSFET according to this embodiment. In this embodiment, as shown in Fig. 1, a direction perpendicular to a thickness (depth) direction X of a semiconductor substrate 2 is called a width direction Y. In addition, with respect to the depth direction perpendicular to each of the thickness direction X and the width direction Y, a cross section as shown in Fig. 1 is formed continuously over a predetermined range, and a description thereof will be omitted. In addition, in the following description, an example of thickness and width is given, but this is not limited to this example, and for example, errors in the injection amount during the manufacturing process, and a range of errors in the thickness, width, etc. of the finished product are allowed.
[0013] In this embodiment, the semiconductor device has an MVMOSFET 1. The MVMOSFET 1 includes a semiconductor substrate 2 in which a P-well region is formed by implanting P-type impurities, a shallow trench isolation (STI) (not shown), a source-side LDD region 3, a drain-side LDD region 4, a source-side SD region 5, a drain-side SD region (drain region) 6, a gate oxide film 7, and a gate (gate electrode) G. The gate oxide film 7 includes a thin film portion 8 having a small thickness and a thick film portion 9 having a thickness thicker than the thin film portion 8.
[0014] In this embodiment, the MVMOSFET 1 is described as an MVNMOS (medium voltage NMOS) by way of example, but may be a MOS of another structure. An MVNMOS is a MOSFET whose operating voltage is generally classified as being between 2.5V and 8V.
[0015] In this embodiment, the semiconductor substrate 2 is a silicon substrate. The semiconductor substrate 2 includes a P-well region and an STI (not shown). The P-well region is a region having a P-type polarity formed by implanting a P-type impurity such as boron (B) into the semiconductor substrate 2. The STI is a structure for isolating each region formed in the semiconductor substrate 2, and is formed by digging a groove (trenches) at a predetermined position and filling the groove with a silicon oxide film. The STI is made of an insulator, and therefore electrically isolates each region formed on the silicon substrate surface.
[0016] The source-side LDD region 3 is a low-concentration region formed in the semiconductor layer by implanting N-type impurities such as arsenic (As) or phosphorus (P) into the semiconductor substrate 2. By forming the low-concentration region in the semiconductor layer, the depletion layer expands and the electric field strength is reduced. The source-side LDD region 3 is located below the source-side thin-film portion 8 in the thickness direction X of the MVMOSFET 1, and is formed so as to cover a part of the lower surface of the source-side thin-film portion 8.
[0017] Similarly, the drain-side LDD region 4 is a low-concentration region formed in the semiconductor layer by implanting N-type impurities such as arsenic (As) or phosphorus (P) into the semiconductor substrate 2. By forming the low-concentration region in the semiconductor layer, a depletion layer expands in the P-well region under the gate G, reducing the electric field strength. In addition, the drain-side LDD region 4 is located below the thick film portion 9 in the thickness direction X of the MVMOSFET 1, and is formed to cover the lower surface of the thick film portion 9.
[0018] The source-side SD region 5 is formed by implanting impurities into a region where a transistor source is to be provided. In other words, the source-side SD region 5 is a region where a source electrode made of a material such as polysilicon is to be formed. The source-side SD region 5 is formed so that the junction position is shallower than the junction position of the source-side LDD region 3.
[0019] The drain-side SD region (drain region) 6 is formed by implanting impurities into a region where a transistor drain is to be provided. In other words, the drain-side SD region 6 is a region where a drain electrode made of a material such as polysilicon is to be formed. The drain-side SD region 6 is formed so that the junction position is shallower than the junction position of the drain-side LDD region 4. For example, the source-side SD region 5 and the drain-side SD region 6 are formed by implanting N-type impurities such as arsenic (As) or phosphorus (P) into the semiconductor substrate 2.
[0020] The gate oxide film 7 is an oxide film formed on the surface of the semiconductor substrate 2. The source-side thin film portion 8 is located in the source-side region of the gate oxide film 7, and has a film thickness of, for example, 14 nm.
[0021] The thick film portion 9 is located in the drain side region of the gate oxide film 7, and has a thickness of, for example, 120 [nm]. The width of the thick film portion 9 is, for example, 200 to 300 [nm]. By thickening the gate oxide film on the drain side in this manner, the breakdown voltage of the MVMOSFET 1 can be increased, and the GIDL can be reduced.
[0022] The source-side LDD region 3 and the drain-side LDD region 4 are preferably formed by implanting N-type impurities of the same dose type and amount. By satisfying these conditions, the breakdown voltage of the MVMOSFET1 can be increased more effectively, and the GIDL can be reduced.
[0023] The gate electrode G is made of polysilicon. The gate electrode G is formed on the gate oxide film 7, and the thickness of the gate electrode G is, for example, 200 [nm]. Note that the gate electrode G may be made of a high dielectric constant insulating film / metal gate (MGHK: metal gate / high-k) in addition to polysilicon. It is preferable that the overlap amount between the source side LDD region 3 and the gate electrode G in the width direction Y is equal to the overlap amount between the drain side LDD region 4 and the gate electrode G in the width direction Y. Note that the overlap amount is preferably 200 [nm].
[0024] (MVMOSFET manufacturing method) Next, an example of a manufacturing process (process flow) for the MVMOSFET 1 in this embodiment will be described with reference to FIGS.
[0025] 2, an STI is formed in the semiconductor substrate 2. The STI is a structure for isolating each region, and is formed by digging a groove (trenches) at a predetermined position and filling the groove with a silicon oxide film. Since the STI is made of an insulator, it electrically isolates each region formed in the semiconductor substrate 2. Next, a P-type impurity such as boron (B) is implanted into the semiconductor substrate 2 to form a P-well region in the semiconductor substrate 2.
[0026] Next, in step S12 shown in FIG. 3, N-type impurities are implanted into the P-well region to form the source-side LDD region 3 and the drain-side LDD region 4. First, on the surface of the semiconductor substrate 2 on which the MOSFET is to be formed, the regions other than the regions on which the source-side LDD region 3 and the drain-side LDD region 4 are to be formed are masked with photoresist. Here, the position of the mask is designed taking into consideration the SD regions on which the source and drain are to be formed, which will be described later.
[0027] Next, impurities are implanted with the surface of the semiconductor substrate 2 masked to form the source-side LDD region 3 and the drain-side LDD region 4. For example, the source-side LDD region 3 and the drain-side LDD region 4 are formed by implanting an N-type impurity such as phosphorus (P) into a P-well region at a dose of the order of 1e+13 [atoms / cm 2 ] and form it.
[0028] Next, in step S14 shown in FIG. 4, after removing the mask for forming the source-side LDD region and the drain-side LDD region, a silicon nitride (SiN) film of about 70 to 200 [nm] is formed by the CVD method.
[0029] Furthermore, photoresist is applied onto the silicon nitride film, and the areas on the surface of the semiconductor substrate 2 other than the areas where the thick film portions 9 are to be formed are masked with a resist layer PR. Then, with the mask formed on the surface of the semiconductor substrate 2, dry etching is performed using radio frequency (RF) discharge or the like. By performing dry etching, grooves into which oxide to form the thick film portions 9 are to be filled are formed.
[0030] 5, after the dry etching is completed, the resist layer is removed and chemical cleaning is performed. Then, for example, a thick film portion 9 having a thickness of about 120 [nm] is formed by a thermal oxidation method. The thermal oxidation method may be any of dry oxidation, wet oxidation, and steam oxidation.
[0031] 6, wet etching is performed using a chemical such as a phosphoric acid (H3PO4) based solution to remove the silicon nitride (SiN) film formed on the semiconductor substrate 2. Thereafter, similar to the process of forming the thick film portion 9, a thin film portion 8 with a thickness of 14 nm is formed at a position closer to the source side than the thick film portion 9 by thermal oxidation. In this way, the gate oxide film 7 under the gate G has a structure in which the thickness is thick in the region on the drain side and thin in the region on the source side.
[0032] Next, in step S20 shown in FIG. 7, after forming a thin film portion 8 on the source side, a gate electrode G made of polysilicon and having a thickness of 200 [nm] is patterned by lithography.
[0033] Next, in step S22 shown in FIG. 8, after removing the photoresist, polysilicon is deposited in a predetermined region on the surface of the semiconductor substrate 2 by a film formation method using a CVD method, and a polysilicon gate electrode G having a thickness of 200 nm is formed so that the drain side of the deposited polysilicon overlaps with the channel side of the thick film portion 9.
[0034] 9, after a dielectric film is formed by a CVD method, sidewalls SW are formed on both side surfaces of the gate electrode G by reactive ion etching (RIE). The sidewall SW on the source side is formed on the thin film portion 8 on the source side. The sidewall SW on the drain side is formed on the thick film portion 9.
[0035] 10, N-type impurities such as phosphorus (P) are implanted into the source-side LDD region 3 and the drain-side LDD region 4 to form N-type source-side SD region 5 and drain-side SD region 6. In FIG. 10, the drain-side end of the gate electrode G is provided so as to be located on the thick film portion 9 of the gate oxide film 7. Furthermore, the drain-side SD region 6 is formed so as to be spaced a predetermined distance from the drain-side end of the gate electrode G. The junction positions of the source side SD region 5 and the drain side SD region 6 are shallower than the junction position of the drain side LDD region 4 by making the impurity injection energy when forming the source side SD region 5 and the drain side SD region 6 lower than the injection energy when forming the source side LDD region 3 and the drain side LDD region 4. Furthermore, since the thick film portion 9 is formed thick, the N-type impurity implanted when the drain-side SD region 6 is formed does not penetrate into the drain-side LDD region 4 below the thick film portion 9 .
[0036] Next, a nickel (Ni) film is formed on the surface of the semiconductor substrate 2 by a PVD method such as sputtering. By performing an annealing process after the nickel film is formed, the junction between silicon (Si) and nickel is changed to nickel silicide (NiSi). After that, only the nickel on the oxide film is removed by a chemical process. Incidentally, silicide such as nickel silicide is formed by a general silicide process flow as described above.
[0037] 11, an interlayer insulating film is formed on the conductive layer, electrodes, and wiring of the MVMOSFET 1 by CVD and CMP (Chemical Mechanical Polishing). Then, contact holes for connecting the source S, drain D, and gate G electrodes are formed by dry etching. Then, tungsten (W) is embedded in the contact holes to form contacts, and metal wiring or the like is laid on the surface of the formed contacts to form the source S, drain D, and gate G electrodes. The MVMOSFET 1 according to this embodiment is manufactured through the above process flow.
[0038] (MVMOSFET performance evaluation) Fig. 12 is a comparison diagram of the potential barriers of MVMOSFETs, and Fig. 13 is a graph showing a comparison of the GIDL of MVMOSFETs with different structures.
[0039] In FIG. 12, the horizontal axis (thickness direction X) indicates the electric field strength between the gate G and the drain D. The vertical axis (width direction Y) indicates the electric field strength between the source S and the drain D. The solid lines in the figure indicate the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band of a MOSFET with a shallow LDD region. The dashed lines indicate the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band of a MOSFET with a deep LDD region. The dashed lines indicate the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band of a MOSFET with a deep LDD region and a thick gate oxide film. The solid line, dashed line, and dashed line located on the negative side of the Y axis in the figure indicate the electric field strength Ev of the valence band, and the solid line, dashed line, and dashed line located on the positive side of the Y axis in the figure indicate the electric field strength Ec of the conduction band.
[0040] In FIG. 12, the region between the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band represents a potential barrier. The potential barriers in each structure of the MVMOSFET are compared using the lines in the figure. Comparing the solid line and the dashed line, the potential barrier of the dashed line is larger. That is, by forming each LDD region of the MVMOSFET deep with respect to the gate oxide film, the electric field strengths of the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band in the X-axis direction are reduced near the gate oxide film, and the potential barrier is expanded. In addition, by forming each LDD region of the MVMOSFET deep with respect to the gate oxide film, an electric field is generated even at a position deep with respect to the gate oxide film (the right side of the X-axis direction in FIG. 12), and a potential barrier is formed. In this way, the expansion of the potential barrier reduces the number of electrons passing through the potential barrier, and GIDL can be further suppressed.
[0041] Moreover, comparing the dashed and dotted lines, the potential barrier of the dashed line is wider. By forming each LDD region of the MVMOSFET deeper than the gate oxide film and by having the gate oxide film have a thick portion, the electric field strengths of the conduction band Ec and the valence band Ev in the X-axis direction are further reduced near the gate oxide film, and the potential barrier is wider. In this way, the wider potential barrier reduces the number of electrons passing through the potential barrier, further suppressing GIDL.
[0042] Figure 13 is a graph comparing the output characteristics of MVMOSFETs. The horizontal axis of Figure 13 represents gate voltage Vg, and the vertical axis represents drain current Id. In Figure 13, the dashed-dotted line represents the GIDL of a MOSFET in which each LDD region is formed deep relative to the gate oxide film. The solid line represents the GIDL of a MOSFET in which each LDD region is formed deep relative to the gate oxide film and in which the gate oxide film has a thick portion. The minimum value of drain current Id represented by the dashed-dotted line and solid line is the evaluation value of the GIDL of the MOSFET.
[0043] 13, the GIDL of a MOSFET in which each LDD region is formed deep relative to the gate oxide and has a thick portion in the gate oxide is approximately 2.5 orders of magnitude lower than the GIDL of a MOSFET in which each LDD region is formed deep relative to the gate oxide. In other words, the GIDL of a MOSFET is improved by forming a thick portion in the gate oxide. From the above, it is possible to suppress GIDL by modifying the MOSFET structure and expanding the potential barrier.
[0044] Fig. 14 is a comparison diagram of potential barriers of MVMOSFETs. In Fig. 14, the horizontal axis (thickness direction X) indicates the electric field strength between the gate G and the drain D, and the vertical axis (width direction Y) indicates the electric field strength between the source S and the drain D. In Fig. 14, the solid lines indicate the electric field strengths of the conduction band Ec and the valence band Ev of an MVMOSFET in which each LDD region is formed deep relative to the gate oxide film and the gate oxide film has a thick film portion. The dashed lines indicate the electric field strengths of the conduction band Ec and the valence band Ev of an MVMOSFET (embodiment 1) in which each LDD region is formed deep relative to the gate oxide film and the gate oxide film has a thick film portion, and further in which a predetermined distance is provided between the end of the drain side SD region and the drain side end of the gate electrode G.
[0045] 14, the end of the drain-side SD region is offset by the drain-side LDD region, thereby reducing the amount of impurities diffusing from the drain-side SD region to the drain-side LDD region below the gate electrode. This further reduces the electric field strengths of the conduction band Ec and the valence band Ev in the X-axis direction near the gate oxide film, expanding the potential barrier. As described above, by offsetting the edge of the drain-side SD region from the edge of the gate electrode on the drain side, GIDL of the MOSFET can be suppressed.
[0046] (MVMOSFET embodiment 2) 15 is a cross-sectional view of a structural example of an MVMOSFET according to another embodiment. The MVMOSFET 11 of this embodiment differs from the MVMOSFET 1 in that the end of the drain-side SD region 6 is not offset by the drain-side LDD region 4, and the end of the gate (gate electrode) G is located on the bird's beak of the thick film portion 9 (the part indicated by the two-dot chain line in the figure). The manufacturing process of the MVMOSFET 11 in this embodiment is the same as that of embodiment 1, except that the positions at which the resist layer and the thick film portion are formed in the above-mentioned steps S14 and S16 are different.
[0047] According to the MVMOSFET 11 of this embodiment, since there is no specified distance between the end of the drain side SD region 6 and the drain side end of the gate electrode G, the MVMOSFET 11 can be shortened in the width direction Y, and the size can be reduced. The manufacturing process of the MVMOSFET 11 in this embodiment is similar to that in the first embodiment, except that the position where polysilicon is deposited in step S20 described above is different.
[0048] (MVMOSFET embodiment 3) 16 is a cross-sectional view of an example of the structure of an MVMOSFET 21 according to another embodiment. In the MVMOSFET 21 of this embodiment, the thick film portion 9 is formed by a CVD method instead of a thermal oxidation method. Also, the MVMOSFET 21 differs from the MVMOSFET 1 in that the drain side end of the gate electrode G is located on the drain side end of the thick film portion 9.
[0049] The manufacturing process of MVMOSFET 21 in this embodiment is the same as that of embodiment 1, except that in step S16 described above, thick film portion 9 is formed by CVD. In thermal oxidation, a gate oxide film is formed by applying heat treatment to a semiconductor substrate using a high-temperature process, resulting in the formation of a bird's beak. In contrast, unlike thermal oxidation, CVD does not form a bird's beak, and can more accurately form the thick film portion and thin film portion regions during the gate oxide film formation.
[0050] In addition, since there is no need to add a new mask, it is possible to manufacture a MOSFET with improved GIDL without increasing manufacturing costs. Furthermore, by performing sacrificial oxidation before forming the gate oxide film by CVD, it is possible to form a gate oxide film with higher uniformity by removing the damaged layer and contamination on the semiconductor substrate surface.
[0051] As described above, the semiconductor device and the manufacturing method thereof according to each embodiment include a gate oxide film (7) having a thick film portion (9) formed on the drain side to be thicker than the source side, a drain-side LDD region (4) formed to cover the lower surface of the thick film portion, a source-side LDD region (3) on the lower surface of the gate oxide film and spaced apart from the drain-side LDD region in the width direction, and a drain region (6) formed on the drain side of the drain-side end of the thick film portion and with a junction position shallower than the junction position of the drain-side LDD region. As a result, the potential barrier is expanded near the gate oxide film, and the electric field strengths in the respective directions of the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band are reduced, so that the MVMOSFET can suppress GIDL. In addition, since the conventional MOSFET manufacturing process can be used, there is no need to add new manufacturing processes or masks. Therefore, the performance of the semiconductor device can be improved without increasing the manufacturing cost.
[0052] Moreover, the semiconductor device and the manufacturing method thereof according to this embodiment include a gate electrode (G) provided on a gate oxide film, and the drain side end of the gate electrode is located on the thick film portion. That is, the structure may be such that the gate electrode is formed on the thick film portion of the gate oxide film. That is, the MOSFET has a structure in which a predetermined distance is provided between the drain side end of the gate electrode and the end of the drain region. This makes it possible to prevent impurities diffusing from the drain region to the drain side LDD region from diffusing into the region below the gate electrode in the drain side LDD region, causing the impurity concentration to become excessively high, and thus makes it possible to suppress GIDL.
[0053] Furthermore, the semiconductor device and the manufacturing method thereof according to this embodiment include a gate electrode provided on a gate oxide film, and the drain side end of the gate electrode is located on the bird's beak of the thick film portion. In other words, this structure does not provide an offset between the drain side end of the MOSFET gate electrode and the drain region. This makes it possible to suppress an increase in size of the semiconductor device and to suppress GIDL.
[0054] In addition, according to the semiconductor device and the manufacturing method thereof of this embodiment, the same type and amount of ions are implanted into the drain side LDD region and the source side LDD region. This reduces the source side resistance and reduces the I on The decrease in current can be suppressed.
[0055] According to the semiconductor device and the manufacturing method thereof of each embodiment, a manufacturing method of a semiconductor device including a MOSFET includes a gate oxide film forming step of forming a gate oxide film having a thick film portion formed on the drain side to be thicker than the thickness on the source side, an LDD region forming step of forming a drain-side LDD region so as to cover the lower surface of the thick film portion and forming a source-side LDD region on the lower surface of the gate oxide film and spaced apart from the drain-side LDD region in the width direction, and a drain region forming step of forming a drain region by injecting impurities into the drain-side LDD region on the drain side of the drain-side end of the thick film portion with an injection energy lower than the injection energy of the impurities used in forming the drain-side LDD region. This makes it possible to manufacture a semiconductor device including a gate oxide film having a thick film portion formed on the drain side to be thicker than the thickness on the source side, a drain-side LDD region formed to cover the lower surface of the thick film portion, a source-side LDD region on the lower surface of the gate oxide film and spaced apart from the drain-side LDD region in the width direction, and a drain region formed on the drain side of the drain-side end of the thick film portion and whose junction position is shallower than the junction position of the drain-side LDD region. In addition, since the drain region is formed by injecting impurities with lower injection energy than the injection energy of impurities when forming the drain-side LDD region, the junction position is formed shallower than the junction position of the drain-side LDD portion. In addition, in the manufactured semiconductor device, the potential barrier is expanded near the gate oxide film, and the electric field strength in each direction of the electric field strength Ec of the conduction band and the electric field strength Ev of the valence band is small, so that GIDL can be suppressed. In addition, since the conventional MOSFET manufacturing process can be used, there is no need to add new manufacturing processes or masks. Therefore, the performance of the semiconductor device can be improved without increasing the manufacturing cost.
[0056] Moreover, according to the semiconductor device and the manufacturing method thereof according to the present embodiment, the LDD region has a deeper junction than the SD region, and the ion dose is on the order of 1e+13 [atoms / cm 2Here, the junction depths of the LDD and SD regions are different, for example, in the case of PMOS, boron (B) is implanted with an implantation energy of 20 keV to form the LDD region, and boron (B) is implanted with an implantation energy of 6 keV to form the SD region. In addition, in the case of NMOS, phosphorus (P) is implanted with an implantation energy of 70 keV to form the LDD region, and phosphorus (P) is implanted with an implantation energy of 30 keV to form the SD region. This makes it possible to more effectively suppress GIDL.
[0057] Furthermore, in the semiconductor device and the manufacturing method thereof according to the present embodiment, the LDD region formation process is a process prior to the gate oxide film formation process. This makes it possible to form an LDD region having a deep junction without having to consider punch-through caused by ion implantation of polysilicon when forming the gate electrode. In other words, a semiconductor device in which GIDL is suppressed can be manufactured using conventional manufacturing processes.
[0058] Although the present invention has been described above using each embodiment, the technical scope of the present invention is not limited to the scope described in the above embodiment. Various modifications or improvements can be made to the above embodiment without departing from the gist of the invention, and the forms in which such modifications or improvements are made are also included in the technical scope of the present invention. In addition, the above embodiments may be combined as appropriate. In addition, the flow of the manufacturing process described in each of the above embodiments is also an example, and unnecessary steps may be deleted, new steps may be added, or the order of steps may be changed without departing from the spirit of the present invention. In addition, various design values such as specific doses and thicknesses described in each of the embodiments are also an example, and may be changed without departing from the spirit of the present invention. [Explanation of symbols]
[0059] 1 MVMOSFET 2. Semiconductor Substrate 3 Source side LDD region 4 Drain side LDD region 5 Source side SD area 6 Drain side SD region 7 Gate oxide 8 Thin Film Section 9 Thick Film Section 11 MVMOSFET 21 MVMOSFET D Drain Ec Electric field strength in the conduction band Ev Electric field strength in the valence band G Gate (gate electrode) Id Drain current PR resist layer S Source SW Sidewall Vg Gate voltage X thickness direction Y Width direction
Claims
1. a gate oxide film having a thick portion formed on the drain side to be thicker than the source side; a drain-side LDD region formed to cover a lower surface of the thick film portion; a source-side LDD region provided at a widthwise interval from the drain-side LDD region so as to be in contact with a lower surface of the gate oxide film; a drain region formed closer to the drain side than the drain side end of the thick film portion and having a junction position shallower than the junction position of the drain side LDD region; Equipped with The semiconductor device has an overlap amount between the source side LDD region and the gate electrode equal to an overlap amount between the drain side LDD region and the gate electrode.
2. a gate electrode provided on the gate oxide film; 2. The semiconductor device according to claim 1, wherein an end portion of the gate electrode on the drain side is located on the thick film portion.
3. a gate electrode provided on the gate oxide film; 2. The semiconductor device according to claim 1, wherein an end portion of said gate electrode on a drain side is located on a bird's beak of said thick film portion.
4. 2. The semiconductor device according to claim 1, wherein the drain side LDD region and the source side LDD region are implanted with the same type and amount of ions.
5. A method for manufacturing a semiconductor device including a MOSFET, comprising the steps of: a gate oxide film forming step of forming a gate oxide film having a thick film portion on a drain side that is formed to be thicker than a source side; an LDD region forming step of forming a drain-side LDD region so as to cover a lower surface of the thick film portion, and forming a source-side LDD region spaced apart from the drain-side LDD region in a width direction so as to contact a lower surface of the gate oxide film; a drain region forming step of forming a drain region by injecting impurities into the drain-side LDD region on the drain side of the drain-side end portion of the thick film portion with an injection energy lower than an injection energy of the impurities used to form the drain-side LDD region; having A method for manufacturing a semiconductor device in which an overlap amount between the source side LDD region and the gate electrode is equal to an overlap amount between the drain side LDD region and the gate electrode.
6. The dose of ions implanted in the LDD region formation step is on the order of 1e+13 [atoms / cm 2 6. The method for manufacturing a semiconductor device according to claim 5,
7. 6. The method for manufacturing a semiconductor device according to claim 5, wherein the step of forming the LDD region is a step prior to the step of forming the gate oxide film.
Citation Information
Patent Citations
Locos MOS device for ESD protection and its formation method
JP1999168146A
Semiconductor device and its manufacture
JP2000174271A
Semiconductor device and its manufacturing method
JP2002124670A
Semiconductor device and fabrication process therefor
JP2010021221A
Semiconductor Device and Method Comprising a High Voltage Reset Driver and an Isolated Memory Array
US20080304314A1