CMP polishing pad with lobed protruding structure

The CMP pad with lobed protruding structures addresses the inefficiencies of traditional CMP pads by optimizing contact and structural support, enhancing polishing rates and reducing wear through a parametric design that balances fluid management and mechanical strength.

JP7593747B2Active Publication Date: 2024-12-03DUPONT ELECTRONIC MATERIALS HLDG INC
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020098287
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-06-07
Filing Date
2020-06-05
Publication Date
2024-12-03
Estimated Expiration
2040-06-05

AI Technical Summary

Technical Problem

Existing chemical mechanical polishing (CMP) pads with protruding structures face challenges in achieving effective polishing rates due to increased fluid pressure on the top surface of the structures, reducing pad-wafer contact area and contact stress, leading to slower removal rates and structural integrity issues such as bending or tearing.

Method used

The CMP pad features protruding structures with a cross-section defined by a parametric equation, comprising three or more lobes and a delta parameter between 0.3 to 0.65, which reduces fluid travel distance and enhances mechanical integrity, ensuring sufficient contact and structural support.

Benefits of technology

The design improves polishing efficiency by maintaining contact stress and structural integrity, thereby increasing removal rates while minimizing wear and tear on the protruding structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007593747000003
    Figure 0007593747000003
  • Figure 0007593747000004
    Figure 0007593747000004
  • Figure 0007593747000005
    Figure 0007593747000005
Patent Text Reader

Abstract

To provide an improved pad structure having protruding structures which realizes good contact with the surface being polished with reasonable force and effective polishing in a reasonable time without undue wear on the pad or other negative consequences.SOLUTION: A polishing pad useful in chemical mechanical polishing comprises a base, and a plurality of structures protruding from the base, where a portion of the plurality of structures is defined by a cross section having a perimeter which defines an area. The perimeter can be defined by parametric equations and can have six or more inflection points or the cross-section can comprise three or more lobes. The cross-section has a Delta parameter in the range of 0.2 to 0.75.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THEINVENTION The present invention relates generally to the field of polishing pads for chemical mechanical polishing. In particular, the present invention is directed to a chemical mechanical polishing pad having an abrasive structure useful for chemical mechanical polishing of magnetic, optical and semiconductor substrates, including front-end-of-line (FEOL) or back-end-of-line (BEOL) processing of memory and logic integrated circuits. [Background technology]

[0002] background In the manufacture of integrated circuits and other electronic devices, multiple layers of conductive, semiconductive and insulating materials are deposited on and partially or selectively removed from the surface of a semiconductor wafer. Thin layers of conductive, semiconductive and insulating materials can be deposited using a number of deposition techniques. Common deposition techniques in modern wafer processing include physical vapor deposition (PVD), also known as sputtering, chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD) and electrochemical deposition (ECD), among others. Common removal techniques include wet and dry isotropic and anisotropic etching, among others.

[0003] As layers of material are successively deposited and removed, the top surface of the wafer becomes non-planar. Subsequent semiconductor processing (e.g., photolithography, metallization, etc.) requires the wafer to have a flat surface, so the wafer must be planarized. Planarization is useful for removing undesirable surface topography and surface defects, such as rough surfaces, agglomerated material, crystal lattice damage, scratches, and contaminated layers or materials. Furthermore, in damascene processes, material is deposited to fill recesses created by patterned etching, but the filling step can be imprecise, and overfilling rather than underfilling the recesses is desirable. Therefore, the material outside the recesses must be removed.

[0004] Chemical mechanical planarization, or chemical mechanical polishing (CMP), is a common technique used to planarize or polish workpieces such as semiconductor wafers and remove excess material in damascene processes. In conventional CMP, a wafer carrier or polishing head is mounted on a carrier assembly. The polishing head holds the wafer and positions it in contact with the polishing surface of a polishing pad mounted on a table or platen in the CMP apparatus. The carrier assembly provides a controllable pressure between the wafer and the polishing pad. Simultaneously, a slurry or other polishing medium is dispensed onto the polishing pad and drawn into the gap between the wafer and the polishing layer. To perform the polishing, the polishing pad and wafer usually rotate relative to one another. As the polishing pad rotates under the wafer, the wafer traverses a generally annular polishing track, i.e., a polishing region, in which the surface of the wafer directly faces the polishing layer. The wafer surface is polished and planarized by the chemical and mechanical action of a polishing surface and a polishing medium (eg, a slurry) on the surface.

[0005] The interactions between the polishing layer, the polishing media and the wafer surface during CMP have been the subject of increasing research, analysis and advanced mathematical modeling over the last few years to optimize polishing pad design. Since the inception of CMP as a semiconductor manufacturing process, most of the polishing pad development has been experimental in nature, including testing many different porous and non-porous polymeric materials and the mechanical properties of such materials. Much of the design of the polishing surface, or layer, has focused on providing these layers with various microstructures, patterns of void and solid areas, and macrostructures, or arrangements of surface perforations or grooves, that are required to increase the polishing rate, improve polishing uniformity, or reduce polishing defects (scratches, holes, delamination areas, and other surface or subsurface damage). Over the years, a great number of different microstructures and macrostructures have been proposed to enhance CMP performance. See, for example, U.S. Patents 6,817,926; 7,226,345; 7,517,277; or 9,649,742.

[0006] Among the various structures that have been proposed are protruding structures, e.g., in the shape of prisms, pyramids, truncated pyramids, cylinders, truncated cones, crosses, hexagons (see U.S. Patent 6,817,926), or structures having reservoirs defined by raised "c" or "v" shapes and / or "jagged edges" or hexagonal boundaries (see U.S. Patent 7,226,345) or quadrangles (including those with arcuate sides or notched vertices) (see U.S. Patent 9,649,742).

[0007] There remains a need for an improved pad structure having protruding structures that provide good contact with the surface being polished with a reasonable force and effective polishing in a reasonable amount of time without excessive wear or other negative consequences on the pad.

[0008] Summary of the Invention According to one aspect, a polishing pad useful in chemical mechanical polishing includes a base and a plurality of structures protruding from the base, a portion of the plurality of structures being defined by a cross section having a perimeter that defines an area, wherein the perimeter comprises: x:=(a1*sin(2*f1*π*t)+a3*sin(2*f3*π*t)+a5*sin(2*f5*π*t)) / G1 y:=(a2*cos(2*f2*π*t)+a4*cos(2*f4*π*t)+a6*cos(2*f6*π*t)) / G2 [In the formula, a1, a2, a3, a4, a5, and a6 each independently represent −10 12 ~10 12 and f1, f2, f3, f4, f5, and f6 are numbers from 0 to 10. 12 where t is a parametric independent variable that defines the perimeter and increases from 0 to 1 by delta t, and delta t is preferably 0.05 or less, and G1 and G2 are greater than 0 to 10. 12 Disclosed herein is a polishing pad whose cross section is further characterized by a delta parameter in the range of 0.20 to 0.75; the "delta parameter" is defined as the distance from the furthest point inside and from the periphery to the closest point on the periphery divided by the equivalent radius of a circle having an area equal to the area of ​​the cross section. The equivalent radius is the square root of the area of ​​the cross section / π.

[0009] According to another aspect, disclosed herein is a polishing pad comprising a base and a plurality of structures protruding from the base, a portion of the plurality of structures defined by a cross-section having three or more lobes and having a perimeter defining an area, the cross-section characterized by a delta parameter in the range of 0.3 to 0.65. [Brief description of the drawings]

[0010] [Figure 1] 1 is a representative embodiment of a cross-section of a protruding structure such as may be used on the pad of the present invention. [Diagram 2] 1 is a representative embodiment of a cross-section of a protruding structure such as may be used on the pad of the present invention. [Diagram 3] 1 is a representative embodiment of a cross-section of a protruding structure such as may be used on the pad of the present invention. [Figure 4] 1 is an embodiment of a cross-section of a protruding structure having a delta circularity parameter of 0.15. [Diagram 5] 1 shows a portion of a pad having a three lobed protruding structure thereon. [Figure 6] 1 illustrates the orientation of the protruding structures relative to the surface of the base of the pad.

[0011] Detailed Description of the Invention In pads having protruding structures in the form of cylinders, polygons (e.g., rectangles, pyramids, hexagons), etc., applicants have found that certain problems occur when the protruding structures approach the surface to be polished. One problem is that the fluid (e.g., polishing slurry) traverses a very long distance over the top of the protruding structure(s). This increases the pressure of the fluid on top of the feature, reducing the pad-wafer contact area and contact stress. This reduces the removal rate.

[0012] In other words, a force is required to press the protruding structures against the surface. However, the distance between the surface and the top of the protruding structures for a given force increases with the top surface area of ​​the protruding structures and the viscosity of the fluid. For example, for a cylindrical protruding structure, the force F on an individual protruding structure is given by:

number

number

[0013] Therefore, it may be difficult to achieve a sufficient degree of closeness of the protruding structures to the surface being polished to have effective polishing in a reasonable time. However, the longer it takes to achieve contact, the slower the relative movement speed of the polishing pad and the surface with respect to each other. This results in a slower removal rate, since the protruding structures will not be able to impart sufficient energy to the surface being polished. To improve contact, one may attempt to reduce the area of ​​the protruding structures by reducing the number of protruding structures on the pad (or increase the spacing, i.e., pitch, of the protruding structures), but this may result in less work (less polishing) being done overall by the pad, and may also result in increased wear and more buckling, bending or bending, since each protruding structure has a greater force for a given force applied to the pad as a whole. Also, reducing the size of the protruding structures (particularly the size of the surface of the protruding structures facing the surface being polished - e.g., the diameter of a cylinder or the length of the side of a square) may also result in buckling, bending or bending of the protruding structures and / or undesirable wear (e.g., breaking of the protruding structures). Increasing the height of the protruding structures can facilitate fluid management, but this can also result in the protruding structures buckling, bending or kinking and potentially fracturing.

[0014] The pad disclosed herein has a protruding structure that reduces the distance that the fluid (slurry) must travel on the top surface of the protruding structure, allowing for better contact with the surface being polished while maintaining sufficient structural or mechanical strength to avoid bending or fracturing. Specifically, the pad disclosed herein provides a protruding structure with a cross section with three or more lobes. Thus, the distance that the fluid must travel on the continuous top surface of the protruding structure can be reduced, while at the same time the lobes can reinforce each other for mechanical integrity, thereby reducing the bending of the structure.

[0015] The protruding structure is as follows: x:=(a1*sin(2*f1*π*t)+a3*sin(2*f3*π*t)+a5*sin(2*f5*π*t)) / G1 y:=(a2*cos(2*f2*π*t)+a4*cos(2*f4*π*t)+a6*cos(2*f6*π*t)) / G2 [In the formula, a1, a2, a3, a4, a5, and a6 each independently represent −10 12 ~10 12 and f1, f2, f3, f4, f5, and f6 are each independently a number from 0 to 10. 12 where t is a parametric independent variable that defines the perimeter and increases from 0 to 1 by delta t, and delta t is preferably 0.05 or less, and G1 and G2 are greater than 0 to 10. 12 a1, a2, a3, a4, a5, a6 are each independently a number from at least -100 or -10 to a maximum of 100 or 10. In certain embodiments, f1, f2, f3, f4, f5, f6 are each independently a number from 0 to 100 or 10. In certain embodiments, G1 and G2 are independently in the range of more than 0 to 100 or 10. For example, in FIG. 1, a1=3, a2=3, a3=-1.3, a4=1.3, a5=.5, a6=.5, f1=1, f2=1, f3=2, f4=2, f5=4, f6=4. The delta t used was 0.002. G1 and G2 were 3.

[0016] According to certain aspects, delta t is equal to or less than 0.01, or 0.005, or 0.002, or 0.001. The smaller the delta t, the more points are made to define the shape.

[0017] According to one aspect, the equation defines a perimeter of the protruding structure having at least six inflection points where the perimeter changes from a concave curve to a convex curve, and the perimeter does not cross itself except at the points where it starts and ends. For example, the perimeter can have 6, 8, 10, 12, 14, 16, or 18 inflection points. According to one aspect, the perimeter has six inflection points. The variables a1, a2, a3, a4, a5, a6; f1, f2, f3, f4, f5, f6 are selected to form a shape with a desired number of inflection points.

[0018] The variables a1, a2, a3, a4, a5, a6; f1, f2, f3, f4, f5, f6 are selected such that the equations define a perimeter that starts and ends at the same point to form a continuous perimeter that does not intersect itself.

[0019] 1 shows a symmetrical structure, the protruding structures need not have a symmetrical structure: for example, the lobes need not be the same size as measured as the length from the center of the feature to its furthest point, need not have the same radius of curvature, and / or need not have the same width.

[0020] According to certain aspects, the protruding structure can have three or more lobes. For example, the protruding structure can have 3, 4, 5, 6, 7 or 8 lobes. According to one aspect, the protruding structure has three lobes.

[0021] According to one aspect, the cross section of the protruding structure is defined by a delta parameter. The delta parameter is defined as the distance d from the point P inside and farthest from the periphery to the closest point on the periphery. Ptp ) divided by (the equivalent radius of a circle having an area equal to the area of ​​the cross section). Equivalent radius = square root(A / π). Therefore, referring to Figures 2, 3 and 4, the delta parameter = distance d Ptp / equivalent radius. For FIG. 2, the delta parameter is 0.34, and for FIG. 3, the delta parameter is 0.65, and for FIG. 4, the delta parameter is 0.15. According to a particular aspect, the delta parameter is at least 0.2. The delta parameter is not greater than 0.75. According to a particular aspect, the delta parameter is at least 0.25, or 0.3, or 0.35, or 0.4. According to a particular aspect, the delta parameter is not greater than 0.7, or 0.65, or 0.6. FIG. 1 has a delta parameter of 0.46. If the delta parameter is too low, the protruding structure may have thin arms or lobes that do not provide the desired mechanical strength or integrity. If the delta parameter is too high, the polishing slurry traverses the top of the protruding structure for a long distance. This increases the pressure of the fluid on top of the feature, reducing the pad-wafer contact area and contact stress. This reduces the removal rate.

[0022] According to one aspect, the protruding structures can have a constant cross section throughout the height of the structure. According to another aspect, the cross section can vary over the height of the protruding structures. For example, protruding structures for stability can have a slightly wider or larger cross section closer to the base. According to another aspect, the sum of the cross sections of multiple protruding structures is constant, such as to provide a consistent contact area when the structure wears down during use. Thus, if one or more of the protruding structures are thinner at the top, the other structures can be wider at the top, resulting in a constant total cross-sectional area.

[0023] According to certain aspects, the height of the protruding structure can be in the range of at least 0.05 or 0.1 mm to a maximum of 3 or 2.5 or 2 or 1.5 mm from the upper surface of the base. According to certain aspects, the cross-sectional area of ​​the protruding structure can be in the range of at least 0.05 or 0.1 or 0.2 mm. 2 ~30 or 25 or 20 or 15 or 10 or 5mm 2According to certain aspects, the longest dimension of the cross section of the protruding structure (e.g., the longest distance that a fluid will traverse across the top surface of the protruding structure) is at least 0.1 or 0.5 mm or 1 mm. According to certain aspects, the longest dimension of the cross section of the protruding structure (e.g., the longest distance that a fluid will traverse across the top surface of the protruding structure) is no more than 100 or 50 or 20 or 10 or 5 or 3 or 2 mm. According to certain aspects, the shortest dimension of the cross section of the structure (e.g., the shortest distance that a fluid will traverse across the top surface of the protruding structure, e.g., the distance across one lobe) is at least 0.01 or 0.05 or 0.1 or 0.5 mm. According to certain aspects, the shortest dimension of the cross section of the structure (e.g., the shortest distance that a fluid will traverse across the top surface of the protruding structure, e.g., the distance across one lobe) is no more than 5 or 3 or 2 or 1 mm.

[0024] The structures protrude from the top surface of the base of the pad. The base of the pad can be a layer including any material suitable for supporting the protruding structures. For example, the base layer can include or consist of a polymeric material. Examples of such polymeric materials include polycarbonate, polysulfone, nylon, epoxy resin, polyether, polyester, polystyrene, acrylic polymer, polymethylmethacrylate, polyvinyl chloride, polyvinyl fluoride, polyethylene, polypropylene, polybutadiene, polyethyleneimine, polyurethane, polyethersulfone, polyamide, polyetherimide, polyketone, epoxy, silicone, copolymers thereof (e.g., polyether-polyester copolymers), and combinations or blends thereof.

[0025] Preferably, the matrix is ​​polyurethane. For the purposes of this specification, "polyurethane" refers to products derived from difunctional or polyfunctional isocyanates, such as polyetherureas, polyisocyanurates, polyurethanes, polyureas, polyurethaneureas, copolymers thereof, and mixtures thereof. Thus, the CMP polishing pad can be produced by a method including providing an isocyanate-terminated urethane prepolymer; separately providing a curable component; and combining the isocyanate-terminated urethane prepolymer and the curable component to form a combination, and then reacting the combination to form a product. The polishing layer can be formed by skiving the cast polyurethane cake to a desired thickness and grooving or drilling the polishing layer. Optionally, the cake mold can be preheated with IR irradiation, induction, or direct current to reduce product variability when casting the porous polyurethane matrix. Optionally, either a thermoplastic polymer or a thermosetting polymer can be used. Most preferably, the polymer is a crosslinked thermosetting polymer.

[0026] Preferably, the polyfunctional isocyanate used in forming the polishing layer of the chemical mechanical polishing pad of the present invention is selected from the group consisting of aliphatic polyfunctional isocyanates, aromatic polyfunctional isocyanates, and mixtures thereof. More preferably, the polyfunctional isocyanate used in forming the polishing layer of the chemical mechanical polishing pad of the present invention is a diisocyanate selected from the group consisting of 2,4-toluene diisocyanate, 2,6-toluene diisocyanate, 4,4'-diphenylmethane diisocyanate, naphthalene-1,5-diisocyanate, tolidine diisocyanate, para-phenylene diisocyanate, xylylene diisocyanate, isophorone diisocyanate, hexamethylene diisocyanate, 4,4'-dicyclohexylmethane diisocyanate, cyclohexane diisocyanate, and mixtures thereof. Even more preferably, the polyfunctional isocyanate used in forming the polishing layer of the chemical mechanical polishing pad of the present invention is an isocyanate-terminated urethane prepolymer formed by the reaction of a diisocyanate with a prepolymer polyol.

[0027] Preferably, the isocyanate-terminated urethane prepolymer used in forming the polishing layer of the chemical mechanical polishing pad of the present invention has 2-12 wt% unreacted isocyanate (NCO) groups. More preferably, the isocyanate-terminated urethane prepolymer used in forming the polishing layer of the chemical mechanical polishing pad of the present invention has 2-10 wt% unreacted isocyanate (NCO) groups (even more preferably, 4-8 wt%; most preferably, 5-7 wt%).

[0028] Preferably, the prepolymer polyol used to form the multifunctional isocyanate-terminated urethane prepolymer is selected from the group consisting of diols, polyols, polyol diols, copolymers thereof and mixtures thereof.More preferably, the prepolymer polyol is selected from the group consisting of polyether polyols (e.g., poly(oxytetramethylene) glycol, poly(oxypropylene) glycol and mixtures thereof); polycarbonate polyols; polyester polyols; polycaprolactone polyols; mixtures thereof; and mixtures thereof with one or more low molecular weight polyols selected from the group consisting of ethylene glycol; 1,2-propylene glycol; 1,3-propylene glycol; 1,2-butanediol; 1,3-butanediol; 2-methyl-1,3-propanediol; 1,4-butanediol; neopentyl glycol; 1,5-pentanediol; 3-methyl-1,5-pentanediol; 1,6-hexanediol; diethylene glycol; dipropylene glycol; and tripropylene glycol. Even more preferably, the prepolymer polyol is selected from the group consisting of polytetramethylene ether glycol (PTMEG); ester-based polyols (such as ethylene adipate, butylene adipate); polypropylene ether glycol (PPG); polycaprolactone polyols; copolymers thereof; and mixtures thereof. Most preferably, the prepolymer polyol is selected from the group consisting of PTMEG and PPG.

[0029] Preferably, when the prepolymer polyol is PTMEG, the isocyanate-terminated urethane prepolymer has an unreacted isocyanate (NCO) concentration of 2 to 10 wt % (more preferably, 4 to 8 wt %; most preferably, 6 to 7 wt %). Examples of commercially available PTMEG-based isocyanate-terminated urethane prepolymers include Imuthane® prepolymers (available from COIM USA, Inc., e.g., PET-80A, PET-85A, PET-90A, PET-93A, PET-95A, PET-60D, PET-70D, PET-75D); Adiprene® prepolymers (available from Chemtura, e.g., LF800A, LF900A, LF910A, LF930A, LF931A, LF939A, LF950A, LF952A, LF600D, LF601D, LF650D, LF667, LF700D, LF750D, LF751D, LF752D, LF753D, and L325); Andur® prepolymers (available from Anderson Development Available from Company, for example, 70APLF, 80APLF, 85APLF, 90APLF, 95APLF, 60DPLF, 70APLF, 75APLF).

[0030] Preferably, when the prepolymer polyol is PPG, the isocyanate-terminated urethane prepolymer has an unreacted isocyanate (NCO) concentration of 3-9 wt% (more preferably, 4-8 wt%, most preferably, 5-6 wt%). Examples of commercially available PPG-based isocyanate-terminated urethane prepolymers include Imuthane® prepolymers (available from COIM USA, Inc., e.g., PPT-80A, PPT-90A, PPT-95A, PPT-65D, PPT-75D); Adiprene® prepolymers (available from Chemtura, e.g., LFG963A, LFG964A, LFG740D); and Andur® prepolymers (available from Anderson Development Company, e.g., 8000APLF, 9500APLF, 6500DPLF, 7501DPLF).

[0031] Preferably, the isocyanate-terminated urethane prepolymer used in forming the polishing layer of the chemical mechanical polishing pad of the present invention is a low free isocyanate-terminated urethane prepolymer having a free toluene diisocyanate (TDI) monomer content of less than 0.1 wt %.

[0032] Non-TDI-based isocyanate-terminated urethane prepolymers can also be used. For example, isocyanate-terminated urethane prepolymers are acceptable, including those formed by the reaction of 4,4'-diphenylmethane diisocyanate (MDI) and a polyol such as polytetramethylene glycol (PTMEG) with any diol such as 1,4-butanediol (BDO). When such an isocyanate-terminated urethane prepolymer is used, the unreacted isocyanate (NCO) concentration is preferably 4-10 wt% (more preferably 4-10 wt%, most preferably 5-10 wt%). Examples of commercially available isocyanate-terminated urethane prepolymers in this category include Imuthane® prepolymers (available from COIM USA, Inc., e.g., 27-85A, 27-90A, 27-95A); Andur® prepolymers (available from Anderson Development Company, e.g., IE75AP, IE80AP, IE85AP, IE90AP, IE95AP, IE98AP); and Vibrathane® prepolymers (available from Chemtura, e.g., B625, B635, B821).

[0033] The base layer may include a composite of a polymeric material with another material. Examples of such composites include polymers filled with carbon or inorganic fillers, and fiber mats, e.g., glass or carbon fibers, impregnated with a polymer. Any of the aforementioned polymers or epoxy resins may be used in such composites. Alternatively, the base may include a non-polymeric material, such as ceramic, glass, metal, stone, or wood. The base may include one layer, or may include two or more layers, of any suitable material, such as those listed above. The base may be provided on a subpad. For example, the base layer may be attached to the subpad via a mechanical fastener or by an adhesive. The subpad may be made of any suitable material, including, for example, materials useful in base layers. The base layer may have a thickness of at least 0.5 or 1 mm in some aspects. The base layer may have a thickness of no more than 5 or 3 or 2 mm in some aspects. The base layer may be provided in any shape, but may conveniently have a circular or disc shape with a diameter in the range of at least 10 or 20 or 30 or 40 or 50 cm to 100 or 90 or 80 cm. According to certain embodiments, the base of the pad is manufactured from a material having one or more of the following properties: a Young's modulus in the range of at least 2 or 2.5 or 5 or 10 or 50 MPa to 700 or 600 or 500 or 400 or 300 or 200 or 100 MPa, for example as determined by ASTM D412-16; a Poisson's ratio of at least 0.05 or 0.08 or 0.1 to 0.6 or 0.5, for example as determined by ASTM E132015; a density of 0.4 or 0.5 to 1.7 or 1.5 or 1.3 g / cm 3 Density.

[0034] At least a portion of the structures protruding from the surface have a shape (cross section and circumference) as defined by three or more lobes or six or more inflection points and by a delta parameter in a range as described herein, e.g., 0.2-0.75. According to one aspect, all of the protruding structures have a cross section defined by three or more lobes or six or more inflection points and by a delta parameter in a range as described herein, e.g., 0.2-0.75. All of the protruding structures may have the same cross section, or different protruding structures may have different cross sections. For example, some protruding structures may have longer or wider or shorter or thinner lobes than another protruding structure. For example, some of the protruding structures may have three lobes, while other protruding structures have four or more lobes. For example, the pad may include other protruding structures that may have other shapes such as circles, ellipses, or other polygons (squares, triangles, pyramids, etc.), so long as some of the protruding structures may have a cross-section defined by three or more lobes or six or more inflection points and by a delta parameter in the range of 0.2 to 0.75. Preferably, at least 50 to 60 or 70 or 80 percent of the protruding structures on the pad have a cross-section defined by three or more lobes or six or more inflection points and by a delta parameter in the range of 0.2 to 0.75. If the delta parameter is too low, the protruding structures may have arms or lobes that are too thin to provide the desired mechanical support. If the delta parameter is too high, the protruding structures may be too round and the time to achieve contact may be too long to provide the desired removal rate.

[0035] The protruding structures may be arranged in any configuration on the work surface. In one embodiment, they may be arranged in a hexagonal packing structure oriented in the same direction. In another embodiment, they may be arranged in a radial pattern with one lobe oriented along a radial. The protruding structures need not be oriented in a macroscale orientation. The macroscale orientation may be adjusted to achieve a desired removal rate, planarization effect, defect control, uniformity control, and, if necessary, a desired amount of slurry. As an example, see FIG. 5, which shows a plurality of three-lobed protruding structures in a hexagonal packing pattern on a portion of a pad.

[0036] Preferably, the protruding structures do not directly contact each other. The spacing between adjacent protruding structures can be, but need not be, constant. According to certain embodiments, the structures are spaced apart from the center of one protruding structure to the center of an adjacent protruding structure (i.e., pitch) by up to 50 or 20 or 10 or 7 or 5 or 4 times the longest dimension of the cross section of the protruding structures. According to certain embodiments, the structures are spaced apart from the center of one protruding structure to the center of an adjacent protruding structure by at least 1, 1.5 or 2 times the longest dimension of the cross section of the protruding structures. As an example of low pitch configurations, they can be arranged such that one lobe of a first protruding structure can be positioned between two lobes of an adjacent protruding structure without direct contact between the first protruding structure and the adjacent protruding structure. According to certain embodiments, the pitch (the distance from the center of one protruding structure to the center of an adjacent protruding structure) is at least 0.7 or 1 or 5 or 10 or 20 mm. According to certain embodiments, the pitch (the distance from the center of one protruding structure to the center of an adjacent protruding structure) is 150 mm or 100 mm or 50 mm or less. According to certain embodiments, the distance from the periphery of one protruding structure to the closest periphery of an adjacent protruding structure is at least 0.02 or 0.05 or 0.1 or 0.5 or 1 mm. According to certain embodiments, the distance from the periphery of one protruding structure to the closest periphery of an adjacent protruding structure is 100 or 50 or 20 or 10 or 5 mm or less.

[0037] According to one aspect, the protruding structure has its major axis of its height perpendicular or substantially perpendicular to the surface of the base. In that case, the angle α between the base 12 and the protruding structure 10 in FIG. 6 is 90 degrees. The top surface 11 of the protruding structure 10 is parallel to the top surface 13 of the base 12 according to a particular embodiment. According to another embodiment, the protruding structure may be inclined or tilted such that α is less than 90 degrees. However, α is preferably at least 20 or 40 or 60 or 70 or 80 degrees.

[0038] The contact area ratio is the cumulative surface contact area A cpsa , or multiple protruding structures with a base area A b The cumulative surface contact area can be calculated by adding up the areas of all the top surfaces 11 of the protruding structures. Since pads are traditionally circular, for traditional pad shapes, π(r b ) 2 , in the formula, r b is the radius of the pad. cpsa / A b is at least 0.1 or 0.2 or 0.3 or 0.4 and is not more than 0.8 or 0.75 or 0.7 or 0.65 or 0.6.

[0039] The protruding structures and base may be a unitary structure, or the protruding structures may be disposed on and adhered to the base.

[0040] The composition of the protruding structure may be the same as or different from the composition of the base. For example, the protruding structure may include or consist of a polymeric material. Examples of such polymeric materials include polycarbonate, polysulfone, nylon, polyether, epoxy resin, polyester, polystyrene, acrylic polymer, polymethylmethacrylate, polyvinyl chloride, polyvinyl fluoride, polyethylene, polypropylene, polybutadiene, polyethyleneimine, polyurethane, polyethersulfone, polyamide, polyetherimide, polyketone, epoxy, silicone, copolymers thereof (e.g., polyether-polyester copolymers), and combinations or blends thereof. The protruding structure may include composites of polymeric materials with other materials. Examples of such composites include polymers filled with carbon or inorganic fillers. According to certain embodiments, the protruding structure(s) are fabricated from a material having one or more of the following properties: a Young's modulus in the range of at least 2 or 2.5 or 5 or 10 or 50 MPa to 700 or 600 or 500 or 400 or 300 or 200 or 100 MPa, for example, as determined by ASTM D412-16; a Poisson's ratio of at least 0.05 or 0.08 or 0.1 to 0.6 or 0.5, for example, as determined by ASTM E132015; a viscosity of 0.4 or 0.5 to 1.7 or 1.5 or 1.3 g / cm 3 Density.

[0041] The pad can be manufactured by any suitable process. For example, the pad can be manufactured by molding, such as injection molding, where the mold contains indentations that are used to form the protruding structures of the pad. As another example, the pad can be manufactured by additive manufacturing according to known methods, whereby the protruding structures are built up on the base of the pad provided, or the entire pad can be manufactured by additive manufacturing.

[0042] The test methods are those in effect as of the filing date of this application.

Claims

1. A base and and a plurality of structures protruding from a base, the structures comprising: a portion of the plurality of structures has a perimeter defined by a height of a plane perpendicular to a plane of the base and a cross section defined by the perimeter, the area of ​​the cross section being defined by the perimeter; Here, the outer periphery is x:=(a1*sin(2*f1*π*t)+a3*sin(2*f3*π*t)+a5*sin(2*f5*π*t)) / G1 y:=(a2*cos(2*f2*π*t)+a4*cos(2*f4*π*t)+a6*cos(2*f6*π*t)) / G2 [In the formula, a1, a2, a3, a4, a5, and a6 each independently represent −10 12 ~10 12 and f1, f2, f3, f4, f5, and f6 are each a number between 0 and 10. 12 where t is a parametric independent variable that defines the perimeter and increases from 0 to 1 by delta t, and delta t is preferably 0.05 or less, and G1 and G2 are greater than 0 to 10. 12 where a1, a2, a3, a4, a5, a6; f1, f2, f3, f4, f5, f6 are selected such that the perimeter has six or more inflection points where it transitions from a concave to a convex curve, and the perimeter does not cross itself except at the points where it starts and ends; The cross-section is further characterized by a delta parameter equal to the distance from the farthest point inside the periphery and from the periphery to the closest point on the periphery divided by the equivalent radius of a circle having an area equal to the area of ​​the cross-section, the delta parameter being in the range of 0.20 to 0.

75.

2. The polishing pad as described in claim 1, wherein the outer periphery has six inflection points.

3. A base and and a plurality of structures protruding from a base, a portion of the plurality of structures having a perimeter defined by a height of a plane perpendicular to a plane of the base, a cross-section defined by the perimeter, and a lobe that is three or more lobes, the cross-section having an area defined by the perimeter; The cross-section is characterized by a delta parameter equal to (the distance from the point inside and farthest from the outer periphery to the closest point on the outer periphery) / (the equivalent radius of a circle having an area equal to the area of ​​the cross-section), the delta parameter being in the range of 0.3 to 0.

6.

4. The polishing pad of claim 3, wherein a portion of the multiple structures has three of the lobes.

Citation Information

Patent Citations

  • Method for planarizing the top surface of a semiconductor wafer

    JP2001523395A

  • Polishing pad and its use

    JP2004517480A

  • Polishing pad having polishing surface with continuous protrusions having tapered sidewalls

    US20140273777A1

  • Method to provide an abrasive product surface and abrasive products thereof

    US20160001423A1

  • Chemical mechanical planarization pad conditioner with elongated cutting edges

    US20170095903A1