Asphalt-based waterproofing material and construction method thereof
The asphalt-based waterproof material, using asphalt, stone powder, and sand, addresses strength and installation challenges in deep water by forming block-shaped materials that deform and adhere without divers, ensuring effective water-shielding and safety.
Patent Information
- Application Number
- JP2022201353
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-12-16
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2038-11-14
AI Technical Summary
Conventional asphalt mastic used in water depths of 20 m or more lacks strength and requires divers for installation, leading to reduced work efficiency and increased risk, necessitating a mechanized solution.
An asphalt-based waterproof material composed of specific ratios of asphalt, stone powder, and sand, combined with a construction method that forms and installs block-shaped materials without diver intervention, using techniques like quicklime exothermic reaction or mechanical deformation.
The material maintains strength and water-shielding properties in deep water environments, ensuring reaction force against structural loads and eliminating the need for diver-assisted installation, enhancing safety and efficiency.
Smart Images

Figure 0007593986000001 
Figure 0007593986000002 
Figure 0007593986000003
Abstract
Description
[Technical field]
[0001] The present invention relates to an asphalt-based waterproof material applied to waterproofing technology at great depths (for example, 20 m or deeper) in the field of marine engineering, and to a method for applying the asphalt-based waterproof material. [Background technology]
[0002] In general, the use of the ocean has been limited to the construction of port facilities (breakwaters, quays, offshore airports, offshore wind power generation facilities, managed waste sea surface disposal sites, etc.) at depths of approximately 20m or less. In recent years, however, research and development has been carried out at depths of 100m or more in order to mine seabed resources, and there is a demand for the development of construction techniques for such great depths.
[0003] When constructing an undersea dome or offshore hydroelectric dam at a depth of more than 20m, it is necessary to seal between structural components (for example, the joints between the foundation ground and the side walls of the structure) to prevent seawater from flooding into the facility. Conventional waterproofing materials for water depths of less than 20m are rubber materials such as rubber gaskets, which are used for the joints of submerged tunnels. However, in water areas more than 20m deep, rubber materials cannot necessarily accommodate large displacements on the seabed caused by the accumulation of small displacements that continue over time, or large instantaneous displacements during earthquakes. Furthermore, maintenance-free materials are desired for waterproofing materials used in such large-scale structures.
[0004] Therefore, asphalt mastic (asphalt-based waterproofing material) is adopted as a deformation-conforming waterproofing material in managed sea surface disposal sites constructed at a depth of about 20 m or less. The asphalt mastic contains straight asphalt (penetration 60-80), stone powder (less than 75 μm), and sand (grain size less than 2.5 mm). For example, this asphalt mastic is heated to a temperature of about 150°C in a mixture factory and mixed in a weight ratio (%) of straight asphalt:stone powder:sand of 20:30:50. The weight ratio of this straight asphalt is the highest (20%) within the range of 16% to 20% by weight of straight asphalt set by the port standards. In addition, this asphalt mastic is a material that has been confirmed to not deteriorate even after about 40 years.
[0005] The strength characteristics of asphalt mastic are characterized by an increase in strength with a decrease in the amount of straight asphalt, a decrease in temperature, and an increase in the displacement speed. This strength development is thought to be mainly due to the gradual increase in shear friction caused by the sand particles coming into contact with each other during deformation. In this way, asphalt mastic is a material whose strength increases with displacement. For this reason, as mentioned above, a mix in which straight asphalt is mixed at a weight ratio of 20% has a relatively high asphalt content and a low sand content, so it is known to be relatively strong and compliant with deformation without developing strength. However, in deformation at low speeds, the sand moves and displaces smoothly through the asphalt, so there are fewer opportunities for friction between the sand particles, making it difficult for strength to develop. Therefore, if a load in one direction acts on a structure adjacent to the asphalt mastic and the asphalt mastic deforms slowly and significantly, there is a concern that the reaction force (strength that can withstand the load) may not be fully exerted.
[0006] The conventional method of applying the above-mentioned asphalt mastic is as follows. That is, the asphalt mastic is manufactured at a mix factory with the above-mentioned mixture. Next, the asphalt mastic, which has cooled and become less fluid during transportation from the mix factory to the application site, is reheated in the air at the application site to increase its fluidity. Next, this asphalt mastic with increased fluidity is poured into a pouring bucket (for example, a bucket with a capacity of 4 m) that is capable of maintaining a constant temperature. 3 The asphalt mastic is then transferred to a pouring bucket (a bucket with a bottom opening). This pouring bucket is then guided by a crane to the vicinity of the specified construction site in the seawater and lowered. Next, in the seawater, a diver operates the bottom opening lever of the pouring bucket, causing the fluidized asphalt mastic to flow out from the bottom of the pouring bucket and fill the specified construction site. By repeating this operation, a constant volume of asphalt mastic is poured to construct a continuous water shielding body (see Patent Document 1). Note that the diver who performs this operation must be trained in the pouring management of asphalt mastic.
[0007] However, when pouring (filling) asphalt mastic into water 20m or deeper using this conventional construction method, the diver must dive deep and the diving time is short, which reduces work efficiency and increases the risk of the diver developing decompression sickness. In other words, when a diver works underwater, decompression control is required according to the water depth. Therefore, the time that underwater work can be done without decompression stop (time to wait underwater to safely discharge nitrogen dissolved in the body during diving work) is about 6 hours for diving at a depth of 10m or shallower, but about 100 minutes at a depth of 15m, 50 minutes at a depth of 21m, and 25 minutes at a depth of 30m.
[0008] In this way, as the water depth increases, the time that divers can work underwater decreases, so even if the underwater work is the same, the work progress (work efficiency) decreases with the same number of divers as the water depth increases. As a countermeasure to this, the number of divers can be increased and divers can be replaced during work to ensure the same work progress in the process, but this inevitably leads to a decrease in work efficiency and increases costs. Meanwhile, when working at depths of 40m or more, special gases (helium mixed gas) are used for breathing, and when the water depth is even deeper (for example, 100m), saturation diving may be performed. Since these tasks can be dangerous, divers who have been specially educated and trained are required, and the costs are high. Thus, it is desirable to mechanize (unmann) underwater work at great depths of 20m or more without relying on divers. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] Japanese Patent Application Publication No. 6-228961 Summary of the Invention [Problem to be solved by the invention]
[0010] As mentioned above, in places where water pressure is strong at depths of 20m or more, conventional asphalt mastics containing a relatively large amount of straight asphalt are prone to deformation, and there are concerns about their insufficient strength. Moreover, pouring (filling) asphalt mastics at depths of 20m or more requires divers to dive to great depths and their diving time is short, which reduces work efficiency and increases the risk to the divers. For this reason, underwater work at great depths of 20m or more needs to be mechanized, without relying on divers.
[0011] The present invention has been made in consideration of the above-mentioned points, and has an object to provide an asphalt-based waterproofing material that has the strength to withstand the environment, even when filled in construction sites at depths of 20 m or more, and a construction method for the asphalt-based waterproofing material that can be filled in construction sites at depths of 20 m or more without relying on the work of divers. [Means for solving the problem]
[0012] As a means for solving the above problems, the first asphalt-based waterproofing material is made of asphalt, stone powder and sand. only An asphalt-based waterproofing material comprising: The asphalt-based waterproofing material is used at water depths of 20m or more. The asphalt has a penetration 20~40 The straight asphalt is the same as that of claim 1.
[0014] In addition, the construction method of asphalt-based waterproofing material is as follows: No. 1 The method includes a forming step of forming the asphalt-based waterproof material into a block shape, an installation step of guiding the block-shaped asphalt-based waterproof material to the underwater installation site and installing it thereafter without relying on the work of a diver, and a deformation and filling step of promoting the deformation of the block-shaped asphalt-based waterproof material, without relying on the work of a diver, and filling the installation site to ensure waterproofing (see claim 2 (corresponding to the invention of Effect of the Invention
[0015] The asphalt-based waterproof material according to the present invention has a strength that can withstand the environment even in construction locations at depths of 20 m or more. That is, the asphalt-based waterproof material according to the present invention can ensure waterproofing by tolerating and following slight displacements of the structure, while fully exerting (imparting) a reaction force against the load received from the structure. Furthermore, the construction method of the asphalt-based waterproof material according to the present invention makes it possible to fill the construction location with the asphalt-based waterproof material without relying on the work of divers, even in construction locations at depths of 20 m or more. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is a schematic diagram showing an example of a construction site of the asphalt-based waterproofing material according to the first to third embodiments of the present invention. [Diagram 2] FIG. 2 is a schematic diagram showing an example of a construction site of the asphalt-based waterproofing materials according to the first to third embodiments of the present invention. [Diagram 3] FIG. 3(a) is a schematic diagram showing an example of a construction site of the asphalt-based waterproofing material according to the first to third embodiments of the present invention, and (b) is an enlarged view of part A in FIG. 3(a). [Figure 4] FIG. 4 is a schematic diagram showing how the asphalt-based waterproof material according to the first to third embodiments of the present invention is filled into a formwork. [Diagram 5] FIG. 5 is a schematic diagram showing how the asphalt-based waterproofing material according to the first to third embodiments of the present invention is removed from a formwork. [Figure 6] FIG. 6 is a perspective view of the asphalt-based waterproof material according to the first to third embodiments of the present invention with integrated hanging hardware. [Figure 7] FIG. 7 is a diagram for explaining a first embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 8] FIG. 8 is a diagram for explaining a first embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 9] FIG. 9 is a diagram for explaining a second embodiment of the deformation and filling step in the application method of the asphalt-based waterproof material according to the first to third embodiments. [Figure 10] FIG. 10 is a diagram for explaining a second embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 11] FIG. 11 is a diagram for explaining a third embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 12]FIG. 12 is a diagram for explaining a third embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 13] FIG. 13 is a diagram for explaining a fourth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 14] FIG. 14 is a diagram for explaining a fifth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 15] FIG. 15 is a diagram for explaining a fifth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 16] FIG. 16 is a diagram for explaining a sixth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 17] FIG. 17 is a diagram for explaining a sixth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 18] FIG. 18 is a diagram for explaining a sixth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 19] FIG. 19 is a diagram for explaining a seventh embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 20] FIG. 20 is a diagram for explaining a seventh embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. [Figure 21] FIG. 21 is a diagram for explaining an eighth embodiment of the deformation and filling step in the application method for the asphalt-based waterproof material according to the first to third embodiments. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, an embodiment of the present invention will be described in detail with reference to Figs. First, an asphalt-based waterproof material 1A according to a first embodiment of the present invention will be described. The asphalt-based waterproof material 1A according to the first embodiment is composed of straight asphalt, stone powder, and sand. The straight asphalt has a penetration of 60 to 80. The stone powder has a particle size of less than 75 μm. The sand has a particle size of less than 2.5 mm. In the mix ratio (wt %) of the asphalt-based waterproof material 1A according to the first embodiment, the straight asphalt having a penetration of 60 to 80 is set to less than 16%. For example, a specific mixing ratio (by weight) is straight asphalt with a penetration of 60 to 80: stone powder: sand = 12:18:70.
[0018] Next, an asphalt-based waterproof material 1B according to a second embodiment of the present invention will be described. The asphalt-based waterproof material 1B according to the second embodiment is composed of straight asphalt, stone powder, and sand. The straight asphalt has a penetration of 40 to 60 or 20 to 40. The stone powder has a particle size of less than 75 μm. The sand has a particle size of less than 2.5 mm. In the asphalt-based waterproof material 1B according to the second embodiment, for example, the mixing ratio (wt %) is straight asphalt with a penetration of 40-60 or 20-40:stone powder:sand=8-20:12-30:50-80.
[0019] More specifically, the first compounding ratio (wt %) is straight asphalt having a penetration of 40 to 60 or 20 to 40:stone powder:sand=20:30:50. The second mixing ratio (wt %) is straight asphalt with a penetration of 40 to 60 or 20 to 40:stone powder:sand=16:24:60. The third mixing ratio (wt %) is straight asphalt with a penetration of 40 to 60 or 20 to 40:stone powder:sand=12:18:70. The fourth mixing ratio (wt %) is straight asphalt with a penetration of 40 to 60 or 20 to 40:stone powder:sand=8:12:80.
[0020] The asphalt-based waterproof material 1C according to the third embodiment is composed of blown asphalt, stone powder, and sand. The blown asphalt has a penetration of 20 to 40. The stone powder has a particle size of less than 75 μm. The sand has a particle size of less than 2.5 mm. In the asphalt-based waterproof material 1C according to the third embodiment, for example, the first blending ratio (wt %) is blown asphalt having a penetration of 20 to 40:stone powder:sand=16:24:60. The second mixing ratio (wt %) is blown asphalt with a penetration of 20 to 40:stone powder:sand=12:18:70.
[0021] The asphalt-based waterproof materials 1A to 1C according to the first to third embodiments described above (hereinafter referred to as the present asphalt-based waterproof materials 1A to 1C) are filled, for example, in construction locations as shown in Figs. 1 to 3. That is, the present asphalt-based waterproof materials 1A to 1C are filled in the lower side wall of an offshore hydroelectric dam 10 constructed, for example, at a depth of 20 m or more as shown in Figs. 1 and 2. That is, in the offshore hydroelectric dam 10, as shown in Fig. 1, a structure 11 such as a caisson is constructed on a riprap mound 14 composed of a large number of riprap stones provided on the seabed. Then, the present asphalt-based waterproof materials 1A to 1C are filled between the lower side wall surface of the structure 11 and a formwork structure 12 composed of blocks or the like.
[0022] As shown in Fig. 2, in an offshore hydroelectric dam 10, an installation recess 17 is provided on the seabed, a rubble mound 14 made of a large number of rubble stones is constructed on the bottom surface of the installation recess 17, and in the case where a structure 11 such as a caisson is constructed on the rubble mound 14, the present asphalt-based water shielding materials 1A to 1C are filled in the installation recess 17 between the lower side wall surface of the structure 11 and the inner wall surface of the installation recess 17. Furthermore, as shown in Fig. 3, when constructing an undersea dome 20 at a water depth of 20 m or more, for example, an annular recess 22 extending in a ring shape is formed on the seabed. A peripheral end 20B of a dome body 20A is installed on the bottom surface of the annular recess 22, and the present asphalt-based water shielding materials 1A to 1C are filled in the annular recess 22 so as to sandwich the peripheral end 20B of the dome body 20A from the outside and inside of the dome body 20A.
[0023] Furthermore, the asphalt-based waterproofing materials 1A to 1C according to the first to third embodiments described above can have higher strength than conventional asphalt-based waterproofing materials, that is, conventional asphalt-based waterproofing materials having a mixing ratio (by weight) of straight asphalt with a penetration of 60 to 80:stone powder:sand = 20:30:50. As a result, when the above-mentioned construction site, that is, the construction site is about 20m or more deep underwater and one side of the waterproofing material is used as a waterproofing material for a structure in which the water depth is an air part, if the conventional mix is used, there is a concern that the waterproofing material will continue to deform due to a large water pressure and the required waterproofing layer thickness will be lost and cannot be secured. However, in the asphalt-based waterproofing materials 1A to 1C according to the first to third embodiments, from the viewpoint of strength, even under a large water pressure, the waterproofing material will deform only at the initial displacement and fill the construction site, and for any further deformation, the viscosity of the straight asphalt increases, and in addition, the hydraulic pressure (Pascal pressure stress) of the asphalt-based waterproofing materials 1A to 1C increases, and the frictional resistance of the sand increases, so that the reaction force (strength) from the asphalt-based waterproofing materials 1A to 1C increases. As a result, deformation from the filled shape is suppressed. In addition, the asphalt-based waterproofing materials 1A to 1C are capable of following the displacement of the structure that occurs after construction. That is, the present asphalt-based waterproof materials 1A to 1C can be used in deep water environments and can be maintenance-free. The present asphalt-based waterproof materials 1A to 1C can be provided with a composition having such strength characteristics.
[0024] In short, the asphalt-based waterproofing materials 1A to 1C of the first to third embodiments can tolerate and follow the displacement of the structures 11, 12, even when the construction site is 20 m or deeper, ensuring their waterproofing, while also exerting sufficient reaction force against the deformation load received from the structures 11, 12 and the water pressure generated by the difference in water head between the inside and outside of the structures.
[0025] Then, a construction method for filling the asphalt-based waterproof materials 1A to 1C in the above-mentioned construction location (see Figs. 1 to 3) will be described with reference to Figs. 4 to 21. First, in the molding process, the asphalt-based waterproof materials 1A to 1C are heated in a mixture plant or at a land yard such as a construction site to increase fluidity, and filled into a formwork 20 or the like as shown in FIG. 4. After time has passed, the materials are cooled to the air temperature and solidified to form a block shape. It is preferable to coat or attach a release material to the inner surface of the formwork 20 to facilitate release. When the asphalt-based waterproof materials 1A to 1C are molded into a block shape, for example, the area of the bottom surface is made smaller than the installation area of the construction site (for example, between structures 11 and 12) as shown in FIG. 10, and the height is increased accordingly so that the volume is the same as the volume when the materials are filled into the construction site. Next, as shown in FIG. 5, the formwork 20 is removed from the block-shaped asphalt-based waterproof materials 1A to 1C. As a result, the asphalt-based waterproof materials 1A to 1C are molded into a block shape that can be moved. The asphalt-based waterproof materials 1A to 1C have the basic shape of the block described above, but are formed into a shape corresponding to the deformation and filling step based on an embodiment in the deformation and filling step described later.
[0026] Next, an installation process is carried out. That is, in this installation process, the block-shaped asphalt-based water-shielding materials 1A to 1C are lifted and transported by the lifting fittings 26 (see FIG. 6) integrally connected thereto, for example, integrally molded when the asphalt-based water-shielding materials 1A to 1C are molded, and guided to the above-mentioned construction site (see FIG. 1 to FIG. 3) and installed. Note that the block-shaped asphalt-based water-shielding materials 1A to 1C are guided in water using technologies such as GPS surveying (not shown) of the crane position and a transponder (not shown), and the installation at the construction site is performed using an automatic crane removal device (not shown). Thus, in this installation process when the block-shaped asphalt-based water-shielding materials 1A to 1C are installed at the construction site, installation work by a diver is not required.
[0027] Next, a deformation and filling process is carried out. In this deformation and filling process, for example, the block-shaped asphalt-based waterproofing materials 1A-1C installed between the structures 11 and 12 as the construction site shown in Fig. 1 are made to be easily deformed, that is, to have a shape that promotes the deformation, so that the gap between the structures 11 and 12 at the construction site is filled in tightly without any gaps, thereby ensuring waterproofing. A specific embodiment of this is described below. First, a first embodiment of the deformation filling process will be described with reference to Fig. 7 and Fig. 8. In the first embodiment, after the molding process and before the installation process, a quicklime sealed bag 27 is attached to the bottom surface of the block-shaped present asphalt-based waterproof material 1A-1C at a mix plant or a land yard at the construction site as shown in Fig. 7. The quicklime sealed bag 27 is configured by sealing quicklime (calcium oxide) inside. Then, in the installation process, the present asphalt-based waterproof material 1A-1C is installed, for example, between the structures 11 and 12 at the construction site shown in Fig. 8(a) with the quicklime sealed bag 27 attached. Then, in the subsequent deformation filling process, the quicklime sealed bag 27 is crushed by the weight of the present asphalt-based waterproof material 1A-1C, and the bottom surface is broken by a protrusion or the like from the installation surface at the construction site, and water infiltrates from that point into the inside.
[0028] Thereafter, the block-shaped asphalt-based waterproofing materials 1A-1C are heated by an exothermic reaction of the quicklime (calcium oxide) due to contact with water that has entered the quicklime sealed bag 27. As a result, the block-shaped asphalt-based waterproofing materials 1A-1C installed at the construction site (for example, between structures 11 and 12) are heated and become easily deformed. Then, as shown in Fig. 8(b), the asphalt-based waterproofing materials 1A-1C are deformed and are brought into close contact with, for example, the structure 11 and 12 at the construction site, thereby ensuring waterproofing.
[0029] Next, a second embodiment of the deformation filling process will be described with reference to Figs. 9 and 10. In the second embodiment, after the molding process and before the installation process, a quicklime sealed bag 27 is attached to the bottom surface of the block-shaped present asphalt-based waterproof material 1A-1C at a mixer factory or a land yard at the construction site, as shown in Fig. 9. Also, just before the installation process, when the block-shaped asphalt-based asphalt 1A-1C is lifted up via a hoisting metal fitting 26, a punching tool 32 is suspended from the present asphalt-based waterproof material 1A-1C. The punching tool 32 has a shape similar to a thumb tack or the like, and is configured with a needle protruding from a circular head. When the punching tool 32 is suspended, it is suspended from the block-shaped present asphalt-based waterproof material 1A-1C so that the needle faces the quicklime sealed bag 27. Then, in the installation process, as shown in FIG. 10(a), with the quicklime sealed bag 27 and the punching tool 32 attached, the asphalt-based waterproofing material 1A-1C is installed, for example, between structures 11 and 12 at the construction site shown in FIG. 10(a).
[0030] Then, in the subsequent deformation and filling step, the needle of the punching tool 32 perforates the bottom surface of the quicklime sealed bag 27, and water infiltrates into the inside through the hole. Then, the quicklime (calcium oxide) comes into contact with the water that has infiltrated into the quicklime sealed bag 27 and generates an exothermic reaction, heating the block-shaped asphalt-based waterproof material 1A-1C. As a result, the block-shaped asphalt-based waterproof material 1A-1C installed at the construction site (for example, between the structures 11 and 12) is heated and becomes easily deformed. Then, as shown in FIG. 10(b), the asphalt-based waterproof material 1A-1C is deformed and is brought into close contact with, for example, the structures 11 and 12 at the construction site, ensuring waterproofing.
[0031] Next, a third embodiment of the deformation filling step will be described with reference to Figs. 11 and 12. In the third embodiment, a weakened line 34 is provided on the bottom surface (the surface that contacts the installation surface of the construction site) of the quicklime sealed bag 27 so that the quicklime sealed bag 27 can be easily torn by the weight of the asphalt-based waterproof materials 1A to 1C after the installation step. The weakened line 34 is formed by forming a number of cuts such as perforations along the longitudinal direction on the bottom surface of the quicklime sealed bag 27. Note that a plurality of weakened lines 34 may be provided at intervals. As a result, when the asphalt-based waterproof materials 1A to 1C are installed at the construction site (for example, between the structures 11 and 12) during the installation step as shown in Fig. 12(a), the quicklime sealed bag 27 is crushed by its own weight in the subsequent deformation filling step, and the quicklime sealed bag 27 is torn along the weakened line 34, allowing water to penetrate inside.
[0032] Thereafter, the block-shaped asphalt-based waterproof materials 1A-1C are heated and put into a state where they are easily deformed due to an exothermic reaction of the quicklime (calcium oxide) caused by contact with water that has entered the quicklime sealed bag 27. Then, as shown in Fig. 12(b), the block-shaped asphalt-based waterproof materials 1A-1C are brought into close contact with, for example, structures 11, 12 at the construction site due to the deformation, thereby ensuring waterproofing. In this embodiment, it is preferable to set the peripheral length L' of the quicklime sealed bag 27 so that 2L>L' holds, where L is the width of the block-shaped asphalt-based waterproof materials 1A-1C as viewed from the front, and L' is the peripheral length of the quicklime sealed bag 27. As a result, when the quicklime sealed bag 27 is crushed by the weight of the asphalt-based waterproof material 1A-1C and the quicklime sealed bag 27 is torn along the weakened line 34, the exothermic reaction of the quicklime (calcium oxide) is effectively distributed throughout the entire bottom surface of the asphalt-based waterproof material 1A-1C without escaping outward from the bottom surface.
[0033] Next, a fourth embodiment of the deformation and filling step will be described with reference to Fig. 13. In the fourth embodiment, a plurality of thermocouples 28 are integrated into the interior or surface of the block-shaped present asphalt-based water-shielding materials 1A-1C during the molding step or before the installation step. The cables (electric wires) 29 extending from the thermocouples 28 are arranged to extend upward from the upper surfaces of the block-shaped present asphalt-based water-shielding materials 1A-1C, so that when the block-shaped present asphalt-based water-shielding materials 1A-1C are installed at the construction site (for example, between the structures 11 and 12), the cables 29 can be prevented from interfering with the adjacent structures 11, 12, etc. In the deformation and filling step after the installation step, electricity is applied to the thermocouples 28 in the block-shaped present asphalt-based water-shielding materials 1A-1C via the cables 29 at sea, so that the block-shaped present asphalt-based water-shielding materials 1A-1C are heated and put into a state in which they are easily deformed. The asphalt-based waterproof materials 1A-1C can be deformed to fit closely between structures 11, 12 at the construction site, for example, and ensure waterproofing. In this embodiment, a covered cable 29 is used to prevent electrical leakage and heat leakage in the underwater area.
[0034] Next, a fifth embodiment of the deformation filling step will be described with reference to Fig. 14 and Fig. 15. In the fifth embodiment, immediately before the installation step, that is, immediately before the block-shaped present asphalt water-proofing materials 1A-1C are hoisted via the hoisting metal fittings 26, a weight 36 such as a substantially rectangular metal plate or concrete plate is placed on the upper surface of the present asphalt water-proofing materials 1A-1C as shown in Fig. 14. Thereafter, in the installation step, as shown in Fig. 15(a), the present asphalt water-proofing materials 1A-1C are hoisted via the hoisting metal fittings 26 together with the weight 36 and installed at the construction site (for example, between the structures 11 and 12). Then, in the subsequent deformation filling step, as shown in Fig. 15(b), the weight 36 deforms the present asphalt water-proofing materials 1A-1C so that their vertical heights are lowered, thereby making them adhere closely to the construction site between the structures 11 and 12, thereby ensuring water-proofing. The weight 36 is formed so that its short-side length (width) is longer than the short-side length (width) of the block-shaped asphalt water impermeable materials 1A-1C before the installation step, and its long-side length is longer than the long-side length of the block-shaped asphalt water impermeable materials 1A-1C. As a result, the weight 36 can deform the block-shaped asphalt water impermeable materials 1A-1C in the deformation filling step so that their vertical heights are reduced not locally but generally uniformly.
[0035] Next, a sixth embodiment of the deformation filling step will be described with reference to Figs. 16 to 18. In the sixth embodiment, as shown in Figs. 16 and 18, in the molding step, the asphalt-based water-proofing materials 1A to 1C are formed into a block shape in which the front view shape is a trapezoid with the top side length longer than the bottom side length and the side view shape is a parallelogram. Then, in the installation step, as shown in Fig. 17(a), the block-shaped asphalt-based water-proofing materials 1A to 1C are installed at the construction site (for example, between structures 11 and 12). Then, in the subsequent deformation filling step, as shown in Fig. 17(b), the asphalt-based water-proofing materials 1A to 1C deform under their own weight so that their height in the vertical direction decreases, and for example, they are closely attached to the construction site between structures 11 and 12, thereby ensuring water-proofing. Furthermore, when the asphalt-based waterproof materials 1A-1C are arranged in series along the longitudinal direction during the installation process, adjacent asphalt-based waterproof materials 1A-1C are arranged so as to overlap each other along the longitudinal direction, as shown in Fig. 18. Then, in the deformation and filling process after the installation process, the asphalt-based waterproof materials 1A-1C deform under their own weight so as to reduce their height in the up-down direction, and the ends of adjacent asphalt-based waterproof materials 1A-1C come into close contact with each other.
[0036] Next, a seventh embodiment of the deformation filling step will be described with reference to Fig. 19 and Fig. 20. In the seventh embodiment, in the molding step, as shown in Fig. 19, the asphalt-based waterproof material 1A-1C is molded into a block shape in which the top and bottom surfaces are formed into a downwardly convex arc shape in front view and the side view shape is a parallelogram. In front view, the perimeter L' of the arc-shaped bottom and top surfaces is set to, for example, the distance L between the structures 11 and 12 at the construction site. Then, in the installation step, as shown in Fig. 20(a), the block-shaped asphalt-based waterproof material 1A-1C is installed at the construction site (for example, between the structures 11 and 12). Then, in the subsequent deformation and filling step, as shown in Fig. 20(b), the asphalt-based water-shielding materials 1A to 1C deform under their own weight so that the vertical height of both sides decreases in front view while the overall vertical height decreases, so that they are in close contact with, for example, structures 11 and 12 at the construction site, thereby ensuring water-shielding. Furthermore, as in the sixth embodiment, when the asphalt-based water-shielding materials 1A to 1C are arranged in series along the longitudinal direction during the installation step, the adjacent asphalt-based water-shielding materials 1A to 1C are arranged so as to overlap each other along the longitudinal direction. As a result, the asphalt-based water-shielding materials 1A to 1C deform under their own weight so that the vertical height decreases, so that the ends of the adjacent asphalt-based water-shielding materials 1A to 1C come into close contact with each other.
[0037] The first to seventh embodiments of the deformation filling process described above may be combined as appropriate. For example, as an eighth embodiment of the deformation filling process, as shown in Fig. 21, the present asphalt-based water-shielding material 1A to 1C in the form of a block, which is formed in a downwardly convex arc shape with its upper and bottom surfaces in a front view as shown in Fig. 19 and which is used in the seventh embodiment, is used, and the quicklime sealed bags 27, 27 shown in Figs. 7, 9, and 11 used in the first to third embodiments are attached to the bottom and upper surfaces of the present asphalt-based water-shielding material 1A to 1C, respectively, and furthermore, the weight 36 shown in Fig. 14 used in the fifth embodiment is placed on the upper quicklime sealed bag 27.
[0038] Then, in an installation step, the present asphalt-based water-sealing materials 1A-1C in block form are installed at the construction site (for example, between structures 11 and 12). Then, in the subsequent deformation and filling step, the present asphalt-based water-sealing materials 1A-1C are deformed by the weight 36 so that their vertical height decreases, and each of the quicklime sealed bags 27, 27 arranged above and below is crushed and broken, and water penetrates into the inside of each of the quicklime sealed bags 27, 27, and the present asphalt-based water-sealing materials 1A-1C in block form are heated by the exothermic reaction of the quicklime. Then, the weight 36 and the heat generated by the exothermic reaction of the quicklime promote the deformation of the present asphalt-based water-sealing materials 1A-1C in block form, and the present asphalt-based water-sealing materials 1A-1C are reliably brought into close contact between structures 11 and 12 at the construction site, thereby ensuring water-sealing properties.
[0039] In the construction method of the asphalt-based waterproof materials 1A to 1C described above, in the forming step, the asphalt-based waterproof materials 1A to 1C are formed into a block shape. Then, in the installation step, the block-shaped asphalt-based waterproof materials 1A to 1C are installed at the construction site shown in FIG. 1, for example, without relying on the work of a diver. Then, in the deformation and filling step, the deformation of the block-shaped asphalt-based waterproof materials 1A to 1C is promoted without relying on the work of a diver, and the materials can be filled in the construction site (gaps, etc.) so as to be in close contact with the construction site. In this way, the construction method basically does not involve the work of a diver, and therefore safety is improved. Moreover, since the uncertainty in construction is reduced, a highly accurate process plan can be made, and construction can be carried out according to the process.
[0040] The construction method according to this embodiment is a method for filling the asphalt-based waterproofing materials 1A to 1C according to the first to third embodiments described above into the construction area, but it can also be applied as a method for filling the construction area with asphalt-based waterproofing materials manufactured with other mixing ratios, including conventional asphalt-based waterproofing materials having a mixing ratio (by weight) of straight asphalt with a penetration of 60 to 80:stone powder:sand = 20:30:50.
[0041] In addition, the construction method according to this embodiment is a construction method in which the asphalt-based waterproofing materials 1A to 1C according to the first to third embodiments are filled in construction locations at a water depth of 20 m or more, but it is of course also possible to adopt the asphalt-based waterproofing materials 1A to 1C according to the first to third embodiments as a construction method in which the asphalt-based waterproofing materials 1A to 1C according to the first to third embodiments are filled in construction locations at a water depth of 20 m or less. [Explanation of symbols]
[0042] 1A, 1B, 1C Asphalt-based waterproofing material, 27 Lime sealed bag, 36 Sinker
Claims
1. An asphalt-based waterproofing material consisting only of asphalt, stone powder and sand, The asphalt-based waterproof material is used at water depths of 20m or more, The asphalt-based waterproofing material is characterized in that the asphalt is straight asphalt having a penetration of 20 to 40.
2. A construction method for filling the asphalt-based waterproofing material according to claim 1 into a construction site underwater, comprising: A molding step of molding the asphalt-based waterproofing material into a block shape; After the forming step, an installation step is performed in which the block-shaped asphalt-based waterproofing material is guided to a construction site underwater and installed therein without relying on the work of a diver; a deformation and filling process for promoting the deformation of the block-shaped asphalt-based waterproof material without relying on the work of a diver after the installation process, and filling the block-shaped asphalt-based waterproof material in the construction area to ensure waterproofing; A method for applying an asphalt-based waterproofing material, comprising:
Citation Information
Patent Citations
JP1971019378Y1
Underwater placement device for asphalt or the like
JP1994228961A
Asphalt mixture suitable for underwater application and application apparatus
JP2000169720A
Block copolymer for modifying asphalt, and asphalt composition