Stator, rotating electric machine, and method of manufacturing the stator
The stator design with a thermosetting resin layer on the slot inner surface enhances space utilization and insulation, improving motor performance and efficiency.
Patent Information
- Application Number
- JP2022536767
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-04-09
- Filing Date
- 2021-12-08
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2041-12-08
AI Technical Summary
Existing technologies face challenges in improving the space utilization efficiency of slots in rotating electric machines by accurately arranging coils while maintaining proper insulation, which affects the performance and efficiency of motors and generators.
A stator design featuring a resin layer with a thermosetting resin having a glass transition temperature of 120°C or higher, applied on the inner surface of the slot parallel to the rotation axis, enhancing space utilization and insulation efficiency.
The solution improves slot space utilization, allowing for increased coil arrangement and motor output, while ensuring high-temperature resistance and insulation reliability.
Smart Images

Figure 0007594011000003 
Figure 0007594011000004 
Figure 0007594011000005
Abstract
Description
[Technical Field]
[0001] The present invention relates to a stator, a rotating electric machine, and a method for manufacturing a stator. [Background technology]
[0002] In rotating electrical machines such as motors and generators, when a coil is accommodated in a slot provided in a stator, a technique is known in which insulating paper or resin material is filled into the slot to ensure insulation between the slot and the coil (see, for example, Patent Document 1). Patent Document 1 discloses a technique in which a resin is injected between a conductor (coil) and a peripheral wall of a slot and hardened to form an insulating layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 6814568 Summary of the Invention [Problem to be solved by the invention]
[0004] Meanwhile, in order to improve motor performance, there was a demand for technology that would allow coils to be positioned accurately while maintaining proper insulation, as well as improve the space utilization efficiency of the slots, i.e., technology that would allow the coils to occupy a larger proportion of the slot.
[0005] The present invention has been made in view of the above circumstances, and has as its object to provide a technique capable of improving the space utilization efficiency of slots. [Means for solving the problem]
[0006] According to the present invention, A stator having a stator core having a plurality of teeth, slots provided between the teeth and accommodating coils, and the coils accommodated in the slots, a resin layer provided on an inner surface of the slot and made of an insulating resin composition; a wall surface of the resin layer on the slot inner side is provided parallel to the rotation axis direction, the resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120°C or higher. A stator is provided. According to the present invention, there is provided a rotating electric machine having the above-described stator. According to the present invention, A method for manufacturing a stator used in a rotating electric machine, the stator having a stator core having a plurality of teeth, slots provided between the teeth and accommodating coils, and the coils accommodated in the slots, comprising: a resin layer forming step of forming a resin layer made of an insulating resin composition on the inner surface of the slot; a coil placement step of placing the coil in the slot provided with the resin layer; and a wall surface of the resin layer on the slot inner side is provided parallel to the direction of the rotation axis of the rotating electric machine, the resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120°C or higher. A method for manufacturing a stator is provided. [Effects of the Invention]
[0007] According to the present invention, it is possible to provide a technique that can improve the space utilization efficiency of slots. [Brief explanation of the drawings]
[0008] [Figure 1] 1 is a cross-sectional view of a motor according to a first embodiment taken along a direction perpendicular to the rotation axis of the motor. [Figure 2]1 is a vertical cross-sectional view of a motor according to a first embodiment taken along a rotation axis thereof. [Figure 3] FIG. 2 is an enlarged view showing the periphery of a slot according to the first embodiment. [Figure 4] FIG. 4 is an enlarged view of the periphery of the slot according to the first embodiment, showing the coils and resin-sealed portions in the slot from FIG. 3. [Figure 5] 4 is a cross-sectional view of the periphery of the slot according to the first embodiment, taken along the line AA in FIG. 3. FIG. [Figure 6] 5 is a cross-sectional view of the periphery of the slot according to the first embodiment, taken along line BB in FIG. 4. [Figure 7] FIG. 10 is a cross-sectional view of a motor according to a second embodiment taken along a direction perpendicular to the rotation axis of the motor. [Figure 8] FIG. 10 is a vertical cross-sectional view of a motor according to a second embodiment taken along the rotation axis. [Figure 9] FIG. 10 is an enlarged view showing the periphery of a slot according to a second embodiment. [Figure 10] FIG. 10 is an enlarged view showing the periphery of a slot according to a third embodiment. [Figure 11] 10A and 10B are diagrams showing the shapes of four types of liner members according to the third embodiment. [Figure 12] FIG. 10 is a schematic diagram of a power module according to a fourth embodiment. [Figure 13] FIG. 10 is a schematic view of a small-diameter resin pipe according to a fourth embodiment. [Figure 14] 10 is a flowchart showing a method for manufacturing a small-diameter resin pipe according to a fourth embodiment. DETAILED DESCRIPTION OF THE INVENTION
[0009] <<First embodiment>> <Summary> In this embodiment, an example will be described in which the present invention is applied to an electric motor (motor) as a rotating electric machine (electric motor, generator, or dual-purpose motor / generator). FIG. 1 is a schematic cross-sectional view of the motor 100 taken perpendicular to the rotational axis direction. FIG. 2 is a schematic cross-sectional view of the motor 100 taken along the rotational axis direction. FIG. 3 is an enlarged view of the slot periphery (area X in FIG. 1), showing a cross-sectional view of a portion where the coil 9 protrudes from the end of the slot 8. FIG. 4 is a diagram of FIG. 3 with the coil 9 in the slot 8 and the resin sealing portion 65 omitted. FIG. 5 is a cross-sectional view taken along the line AA in FIG. 3. FIG. 6 is a cross-sectional view taken along the line BB in FIG. 4. Note that in FIGS. 3, 4, and FIG. 7 (described later), the resin layer 50 is indicated by black ink for convenience. In the following description, the rotating shaft 3 side of the motor 100 will be referred to as the inner periphery side (or rotating shaft side), and the case 1 side will be referred to as the outer periphery side.
[0010] The outline of this embodiment is as follows. In a motor 100, wall surfaces 72 of slots 8 (teeth portions 7) of a stator 4 are covered with a resin layer 50 made of an insulating resin composition. At this time, the wall surfaces of the resin layer 50 (i.e., the resin layer surface 55 of the inner surface resin layer 51) are parallel to the rotation axis of the motor 100. In other words, as shown in FIGS. 5 and 6, when viewed in cross section, the resin layer surface 55 is linear from one (upper) end 55a to the other (lower) end 55b, as indicated by the straight line L in FIG. 6, without being tapered. The resin composition of the resin layer 50 contains a thermosetting resin, and its glass transition temperature Tg is 120°C or higher. This will be explained in detail below.
[0011] <Basic structure of motor 100> The motor 100 includes a case 1, and a rotor 2, a stator 4, and a coil 9 housed inside the case 1.
[0012] <Case 1> The case 1 is configured to have a cylindrical portion 1a and side plate portions 1b, 1c that close both axial ends of the cylindrical portion 1a. The case 1 can be made of a material such as an aluminum alloy (cast metal product), a resin material, or a combination thereof.
[0013] <Rotor 2> The rotor 2 is housed inside the case 1. A rotating shaft 3 is attached to the center of the rotor 2 as an output shaft. Both ends of the rotating shaft 3 are supported by the side plate portions 1b and 1c via bearings 3a. This allows the rotor 2 to rotate freely around the rotating shaft 3.
[0014] Permanent magnets 5 are installed inside the rotor 2. Specifically, as shown in Fig. 1, multiple (eight in this example) permanent magnets 5 are arranged at equal intervals on the same circumference. At this time, the magnetic poles of adjacent permanent magnets 5 are set to be different from each other.
[0015] A cylindrical stator 4 is disposed and fixed on the inner periphery of the cylindrical portion 1a so as to surround the outer periphery of the rotor 2. A minute gap (air gap) is provided between the inner periphery of the stator 4 and the outer periphery of the rotor 2.
[0016] <Stator 4> The stator 4 is formed by stacking multiple electromagnetic steel sheets in the axial direction and closely fixing them together. When viewed from the axial end as shown in FIG. 1, the stator 4 has an annular yoke portion 6 and multiple teeth portions 7 extending from the yoke portion 6 toward the rotor 2 (inner circumference). The multiple teeth portions 7 are arranged at equal intervals in the circumferential direction. In this example, as shown in FIG. 1, 24 teeth portions 7 are provided. Slots 8 are provided between each tooth portion 7. The teeth portions 7 are also provided with a thin resin layer 50 formed by wrapping a resin composition around them to cover them.
[0017] <Coil 9> The coil 9 is a U-shaped rectangular wire wound so as to be housed in two spaced apart slots 8 across the teeth 7. Here, the coil 9 is housed in a distributed winding in a liner member 20 arranged in the slot 8. The coil 9 has a coil body 91 made of a good conductor such as copper and having a rectangular cross section, and a resin coating layer 92 that coats the surface of the coil body 91. The resin coating layer 92 can be made of the same material as the resin material of the resin layer 50, which will be described later.
[0018] <Teeth part 7> The teeth 7 are provided to correspond to the permanent magnets 5 of the rotor 2 described above, and by sequentially exciting each coil 9, the rotor 2 rotates due to attraction and repulsion with the corresponding permanent magnets 5.
[0019] The teeth 7 are tapered, with a larger circumferential width on the outer periphery and a smaller width on the inner periphery. Teeth tips 71 are formed at the inner periphery end of the teeth 7, facing each other in the circumferential direction so as to reduce the width of the slots 8.
[0020] <Slot 8> The slots 8 are spaces between adjacent teeth 7, and as shown in Figures 3 and 4, are arranged so that wall surfaces 72 of teeth 7 that face each other in the radial direction are parallel to each other. The space between the tooth tips 71 forms the inner peripheral opening of the slots 8. The slots 8 are equipped with multiple coils 9 arranged on the outer peripheral side (the yoke portion 6 side) and a resin sealing portion 65 arranged on the inner peripheral side (the tooth tip 71 side).
[0021] <Resin layer 50> As shown in Figures 5 and 6, the resin layer 50 is integrally wrapped around the periphery of the tooth portion 7 with a resin composition, and has an inner surface resin layer 51 that covers the wall surface 72 of the tooth portion 7, and an outer surface resin layer 52 that covers the upper surface 75a and lower surface 75b of the tooth portion 7.
[0022] Resin layer 50 is formed thinly around teeth 7 by insert molding to cover them, thereby tightly fixing stator 4, more specifically the plurality of stacked electromagnetic steel plates in teeth 7.
[0023] As shown in FIGS. 5 and 6 , the surface of the inner resin layer 51 covering the wall surfaces 72 of the teeth 7, facing the interior of the slot 8, i.e., the resin layer surface 55, is linear (specifically, along the straight line L in FIG. 6 ) from one (upper) end 55a to the other (lower) end 55b without any tapered shape. A tapered shape requires a certain thickness to accommodate the shape. However, in this embodiment, no tapered shape is provided, so the thickness of the inner resin layer 51 can be reduced. As a result, the usable space within the slot 8 can be increased. For example, the area occupied by the coil 9 can be increased, which allows for a larger diameter or an increased number of coils, thereby increasing the output of the motor 100.
[0024] The thickness of the inner surface resin layer 51 of the resin layer 50 is 50 μm or more and 500 μm or less. The lower limit of the thickness is preferably 100 μm or more, and more preferably 150 μm or more. The upper limit of the thickness is preferably 400 μm or less, and more preferably 300 μm or less. The thickness of the outer surface resin layer 52 is not particularly limited, but can be approximately the same as that of the inner surface resin layer 51. It is preferable that the lower limit of the thickness be within the above range from the viewpoint of ensuring the fluidity of the resin composition in the extremely narrow portion between the mold and the tooth portion 7 (wall surface 72) relative to the axial length of the stator (i.e., the thickness of the stator 4) during insert molding. In a structure in which the coil 9 is wound around the tooth portion 7 and placed in the slot 8, it is preferable to set the upper limit of the thickness within the above range from the viewpoint of increasing the space utilization efficiency within the slot 8, ensuring the degree of freedom in the size of the coil 9 that can be used, and ensuring performance such as magnetic flux density.
[0025] <Physical Properties of Resin Layer 50> The physical properties of the cured resin material that forms the resin layer 50 are, for example, as follows. The thermal conductivity of the cured resin material is 0.5 W / (m·K) or more. The lower limit of the thermal conductivity is preferably 1.0 W / (m·K) or more, and more preferably 2 W / (m·K) or more. The upper limit of the thermal conductivity is not particularly limited, but a practical value is 10 W / (m·K).
[0026] The glass transition temperature Tg of the resin composition of the resin layer 50 is 120° C. or higher, preferably 140° C. or higher, and more preferably 160° C. or higher. By setting the glass transition temperature Tg within the above range, the motor 100 can be used at high temperatures, and the motor 100 is more resistant to heat generation in the coil 9, allowing it to be used at high output. The resin composition of the resin layer 50 will be specifically described below.
[0027] <Material of Resin Layer 50> The resin composition of the resin layer 50 preferably contains a thermosetting resin (A), a filler (B), a curing agent (C), and the like.
[0028] [Thermosetting resin (A)] Examples of the thermosetting resin (A) include epoxy resins, cyanate resins, polyimide resins, benzoxazine resins, unsaturated polyester resins, phenolic resins, melamine resins, silicone resins, bismaleimide resins, phenoxy resins, and acrylic resins. As the thermosetting resin (A), one of these may be used alone, or two or more may be used in combination. Among these, epoxy resins, phenolic resins, and phenoxy resins are preferred as the thermosetting resin (A) from the viewpoint of high insulating properties, and epoxy resins are particularly preferred from the viewpoint of ensuring flow in extremely narrow sections during molding.
[0029] Examples of epoxy resins include bisphenol type epoxy resins such as bisphenol A type epoxy resin, bisphenol F type epoxy resin, bisphenol E type epoxy resin, bisphenol S type epoxy resin, bisphenol M type epoxy resin (4,4'-(1,3-phenylenediisopridiene)bisphenol type epoxy resin), bisphenol P type epoxy resin (4,4'-(1,4-phenylenediisopridiene)bisphenol type epoxy resin), and bisphenol Z type epoxy resin (4,4'-cyclohexidienebisphenol type epoxy resin); phenol novolac type epoxy resin, cresol novolac type epoxy resin, trisphenol methane type novolac type epoxy resin, tetraphenol group ethoxylated epoxy resin, and the like. Examples of epoxy resins include novolac-type epoxy resins such as benzophenone-type novolac-type epoxy resins and novolac-type epoxy resins having a condensed ring aromatic hydrocarbon structure; biphenyl-type epoxy resins; aryl alkylene-type epoxy resins such as xylylene-type epoxy resins and biphenyl aralkyl-type epoxy resins; naphthalene-type epoxy resins such as naphthylene ether-type epoxy resins, naphthol-type epoxy resins, naphthalene diol-type epoxy resins, bifunctional to tetrafunctional epoxy-type naphthalene resins, binaphthyl-type epoxy resins, and naphthalene aralkyl-type epoxy resins; anthracene-type epoxy resins; phenoxy-type epoxy resins; dicyclopentadiene-type epoxy resins; norbornene-type epoxy resins; adamantane-type epoxy resins; and fluorene-type epoxy resins. These may be used alone or in combination of two or more.
[0030] Among the epoxy resins, from the viewpoint of further improving heat resistance and insulation reliability, it is preferable to use one or more types selected from the group consisting of bisphenol-type epoxy resins, novolac-type epoxy resins, biphenyl-type epoxy resins, aryl alkylene-type epoxy resins, naphthalene-type epoxy resins, anthracene-type epoxy resins, and dicyclopentadiene-type epoxy resins.
[0031] Examples of phenolic resins include novolac-type phenolic resins such as phenol novolac resin, cresol novolac resin, and bisphenol A novolac resin, and resol-type phenolic resins, etc. One of these may be used alone, or two or more may be used in combination. Among the phenolic resins, phenolic novolac resins are preferred.
[0032] The content of the thermosetting resin (A) is preferably 1% by mass or more, and more preferably 5% by mass or more, based on the total amount of the resin composition of the resin layer 50. On the other hand, the content is preferably 30% by mass or less, and more preferably 20% by mass or less, based on the total amount of the resin composition of the resin layer 50. When the content of the thermosetting resin (A) is equal to or greater than the above lower limit, the handleability of the entire resin composition of the resin layer 50 improves, making it easier to form the inner surface resin layer 51 and improving the strength of the inner surface resin layer 51. When the content of the thermosetting resin (A) is equal to or less than the upper limit, the linear expansion coefficient and elastic modulus of the inner surface resin layer 51 are further improved, and the thermal conductivity is further improved.
[0033] [Filler (B)] The filler (B) in this embodiment is used from the viewpoint of improving the thermal conductivity of the resin layer 50 (more specifically, the inner surface resin layer 51) and obtaining strength.
[0034] As the filler (B), an inorganic filler is preferred, and a thermally conductive filler is particularly preferred. More specifically, from the viewpoint of achieving a balance between thermal conductivity and electrical insulation, examples of the filler (B) include silica, alumina, boron nitride, aluminum nitride, and silicon carbide. These may be used alone or in combination of two or more. Of these, alumina and boron nitride are preferred as the filler (B).
[0035] The content of the filler (B), ie, the content of the above filler, is preferably 60% by mass or more based on the total amount of the resin composition.
[0036] [Hardening agent (C)] When an epoxy resin or a phenolic resin is used as the thermosetting resin (A), the resin composition preferably further contains a curing agent (C).
[0037] As the curing agent (C), one or more selected from the curing catalyst (C-1) and the phenol-based curing agent (C-2) can be used. Examples of the curing catalyst (C-1) include organic metal salts such as zinc naphthenate, cobalt naphthenate, tin octoate, cobalt octoate, bisacetylacetonate cobalt(II), and trisacetylacetonate cobalt(III); tertiary amines such as triethylamine, tributylamine, and 1,4-diazabicyclo[2.2.2]octane; 2-phenyl-4-methylimidazole, 2-ethyl-4-methylimidazole, 2,4-diethylimidazole, and 2-phenyl-4-methyl-5-hydroxyimidazole; Examples of suitable curing catalysts include imidazoles such as 2-phenyl-4,5-dihydroxymethylimidazole; organic phosphorus compounds such as triphenylphosphine, tri-p-tolylphosphine, tetraphenylphosphonium tetraphenylborate, triphenylphosphine triphenylborane, and 1,2-bis-(diphenylphosphino)ethane; phenolic compounds such as phenol, bisphenol A, and nonylphenol; and organic acids such as acetic acid, benzoic acid, salicylic acid, and p-toluenesulfonic acid, or mixtures thereof. The curing catalyst (C-1) can be used alone or in combination with two or more of these, including their derivatives. The content of the curing catalyst (C-1) is not particularly limited, but is preferably 0.001% by mass or more and 1% by mass or less based on the total amount of the resin composition.
[0038] Examples of the phenolic curing agent (C-2) include novolac-type phenolic resins such as phenol novolac resin, cresol novolac resin, trisphenolmethane-type novolac resin, naphthol novolac resin, and aminotriazine novolac resin; modified phenolic resins such as terpene-modified phenolic resin and dicyclopentadiene-modified phenolic resin; aralkyl-type resins such as phenol aralkyl resins having a phenylene skeleton and / or biphenylene skeleton and naphthol aralkyl resins having a phenylene skeleton and / or biphenylene skeleton; bisphenol compounds such as bisphenol A and bisphenol F; and resol-type phenolic resins, and these may be used alone or in combination of two or more. Among these, from the viewpoint of improving the glass transition temperature and reducing the linear expansion coefficient, the phenolic curing agent (C-2) is preferably a novolac type phenolic resin or a resol type phenolic resin.
[0039] The content of the phenolic curing agent (C-2) is not particularly limited, but is preferably 1% by mass or more, more preferably 5% by mass or more, based on the total amount of the resin composition, and is preferably 30% by mass or less, more preferably 15% by mass or less, based on the total amount of the resin composition.
[0040] [Coupling agent (D)] The resin composition may contain a coupling agent (D), which can improve the wettability at the interface between the thermosetting resin (A) and the filler (B).
[0041] The coupling agent (D) is not particularly limited, but it is preferable to use one or more coupling agents selected from, for example, epoxy silane coupling agents, cationic silane coupling agents, amino silane coupling agents, titanate-based coupling agents, and silicone oil-type coupling agents. The content of the coupling agent (D) is not particularly limited, but is preferably 0.05% by mass or more, more preferably 0.1% by mass or more, relative to 100% by mass of the filler (B), and is preferably 3% by mass or less, more preferably 2% by mass or less, relative to 100% by mass of the filler (B).
[0042] [Phenoxy resin (E)] Furthermore, the resin composition may contain a phenoxy resin (E). By containing the phenoxy resin (E), the flex resistance of the resin layer 50 can be improved, and the elastic modulus can be reduced, thereby improving the stress relaxation force of the resin layer 50.
[0043] Furthermore, when the resin layer 50 contains the phenoxy resin (E), the viscosity increases, reducing the flowability and preventing the occurrence of voids, etc. Furthermore, when the resin layer 50 is used in close contact with a metal member (i.e., the teeth portion 7), the adhesion between the metal and the cured resin composition can be improved.
[0044] The phenoxy resin (E) may be, for example, a phenoxy resin having a bisphenol skeleton. Examples of suitable phenoxy resins include phenoxy resins having a naphthalene skeleton, phenoxy resins having an anthracene skeleton, and phenoxy resins having a biphenyl skeleton. Phenoxy resins having a structure containing a plurality of these skeletons can also be used.
[0045] The content of the phenoxy resin (E) is preferably, for example, 3% by mass or more and 10% by mass or less relative to the total amount of the resin composition.
[0046] [Release agent] The resin composition preferably contains a mold release agent, which can improve mold releasability after molding. Examples of mold release agents include natural waxes such as carnauba wax, synthetic waxes such as Montan acid ester wax and oxidized polyethylene wax, higher fatty acids such as zinc stearate and their metal salts, and paraffin. These may be used alone or in combination of two or more.
[0047] When a mold release agent is used, its content in the entire resin molding material is preferably 0.01 to 3 mass %, more preferably 0.05 to 2 mass %. This ensures improved mold releasability. As a result, the molding precision of the inner resin layer 51 of the resin layer 50 can be improved.
[0048] [Other ingredients] The resin composition may also contain other additives such as an antioxidant and a leveling agent, provided that the effects of the present invention are not impaired.
[0049] <Resin sealing part 65> The resin sealing portion 65 is provided on the inner circumferential side of the slot 8 (toward the tooth tip 71). The resin sealing portion 65 may be provided by insert molding or may be provided as a separate part. The resin material used for the resin sealing portion 65 may be the same as that described for the resin layer 50.
[0050] <Method for manufacturing stator 4> A method for manufacturing the stator 4 of this embodiment will be described. First, a stator 4 is prepared by stacking a plurality of electromagnetic steel plates in the axial direction and closely fixing them together (stator preparation step). Next, the periphery of the teeth 7 (wall surface 73, upper surface 75a, and lower surface 75b) is integrally covered with an insulating resin composition by insert molding to form the resin layer 50 (resin layer forming step). Next, the coil 9 is placed in the slot 8 provided with the resin layer 50 (coil placement step). After all the coils 9 are accommodated, a resin material is filled into the inner peripheral region of the slot 8 and insert-molded to obtain a resin-sealed portion 65 (resin filling step). Through the above steps, the stator 4 shown in FIG. 3 is obtained.
[0051] <Summary of the First Embodiment> The features of this embodiment can be summarized as follows. (1) The stator 4 is a stator having a stator core 41 having a plurality of teeth 7, slots 8 provided between the teeth 7 and accommodating coils 9, and the coils 9 accommodated in the slots 8, a resin layer 50 formed on the inner surface of the slot 8 and made of an insulating resin composition; The wall surface of the resin layer 50 on the inner side of the slot 8 (the resin layer surface 55 of the inner surface resin layer 51) is provided parallel to the rotation axis direction, The resin composition of the resin layer 50 includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120°C or higher. Because the resin layer surface 55 is parallel to the rotation axis direction, i.e., is linear and not tapered, the inner resin layer 51 can be made thin. Furthermore, by using a thermosetting resin with a glass transition temperature Tg of 120°C or higher, the motor 100 can be used at high temperatures. It can also accommodate increased heat generation due to increased motor 100 output. (2) The resin composition of the resin layer 50 contains wax as a mold release agent, which improves mold release properties after molding and prevents molding defects even when the inner resin layer 51 is made thin. (3) The resin composition of the resin layer 50 contains a filler as a filler, which can increase the strength of the resin layer 50. (4) The resin composition of the resin layer 50 contains 60% by volume or more of the filler relative to the total volume of the resin composition, thereby increasing the strength of the resin layer 50. (5) The thickness of the resin layer 50 is 50 μm or more and 500 μm or less, which makes it possible to improve the space utilization efficiency within the slot 8 and ensure the fluidity of the resin composition in the extremely narrow portion. (6) The thermal conductivity of the resin layer 50 is 0.5 W / (m·K) or more. This allows the heat of the coil 9 to be smoothly transferred to the stator 4. (7) The thermosetting resin is epoxy resin, which provides high heat resistance and insulation reliability. (8) The coil 9 has a resin coating layer 92 in which the coil surface (coil body 91) is coated with resin, thereby ensuring good insulation of the coil 9. (9) A rotating electric machine (motor 100) having the above-described stator 4. (10) A method for manufacturing a stator 4 used in a rotating electric machine (here, a motor 100) having a stator core 41 having a plurality of teeth 7, slots 8 provided between the teeth 7 and accommodating coils 9, and the coils 9 accommodated in the slots 8, the method comprising: a resin layer forming step of forming a resin layer 50 made of an insulating resin composition on the inner surface of the slot 8, i.e., the wall surface 72 of the tooth portion 7; a coil placement step of placing the coil 9 in the slot 8 provided with the resin layer 50; and The wall surface of the resin layer 50 on the inside of the slot 8 (the resin layer surface 55 of the inner surface resin layer 51) is provided parallel to the rotation axis direction of the rotating electric machine (motor 100), The resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120°C or higher.
[0052] <<Second embodiment>> The second embodiment will be described with reference to Figures 7 to 9. Figure 7 is a schematic cross-sectional view of motor 100 taken in a direction perpendicular to the rotational axis direction. Figure 8 is a schematic cross-sectional view of motor 100 taken in the rotational axis direction. Figure 9 is an enlarged view of the periphery of the slot (area Y in Figure 7), and is a schematic cross-sectional view of the portion where coil 9 protrudes from the end of slot 8. The following describes the differences from the first embodiment. Unlike the first embodiment, this embodiment is provided with a cooling water channel 10 in the resin sealing portion 65, and an external connection channel 17 that connects the case 1 to an external cooling channel via a connecting member 12. This will be described in detail below.
[0053] In this embodiment, the side plate portions 1b and 1c of the case 1 are provided with external connection flow paths 17 that connect the cooling water paths 10 in the slots 8 to external cooling flow paths via connecting members 12.
[0054] The resin sealing portion 65 is provided with a cooling water passage 10 extending in the axial direction. A coolant, for example, cooling water, circulates through the cooling water passage 10. The cooling water passage 10 can be formed by a method of directly molding a resin material, or by a method of inserting a cylindrical part into the slot 8 and filling the surrounding area with a resin material.
[0055] The number of cooling water channels 10 arranged in one slot 8 may be one or more, but in a situation where the spatial width of the slot 8 is narrow, it is preferable to have a small number of channels so that the cross-sectional area of the channel is large, taking into account the flow resistance when the coolant passes through. The cross-sectional shape of the cooling water channel 10 can be circular as in this embodiment, or it can be square or matched to the shape of the slot 8.
[0056] <Method for manufacturing stator 4> A method for manufacturing the stator 4 of this embodiment will be described. As in the first embodiment, the stator preparation process, resin layer formation process, and coil arrangement process are performed. Next, after all the coils 9 are accommodated, a mold structure (nested structure) corresponding to the cooling water channels 10 is arranged in a predetermined region on the inner periphery of the slot 8, and insert molding is performed to obtain a resin sealing portion 65 having the cooling water channels 10 (resin filling process). Through the above steps, the stator 4 shown in FIGS. 7 to 9 is obtained.
[0057] The features of this embodiment can be summarized as follows. This embodiment has the same features as the features (1) to (10) of the first embodiment. Furthermore, by providing the cooling water passage 10 as a configuration for cooling the coil 9, it is possible to accommodate higher output of the motor 100.
[0058] <<Third embodiment>> The third embodiment will be described with reference to FIGS. 10 is an enlarged view of the periphery of the slot. The following describes the differences from the second embodiment. Unlike the second embodiment, this embodiment uses a liner member 20 when accommodating the coil 9 in the slot 8.
[0059] <Liner member 20> The liner member 20 is a cylindrical member made of a resin material, elongated in the direction of the rotation axis, and having a frame-like cross section. The interior of the frame of the liner member 20 forms a coil accommodating section 21 that accommodates the coil 9.
[0060] The longitudinal ends of the liner member 20 extend outward by a predetermined length from both ends of the stator 4 (i.e., both ends of the slot 8). The liner member 20 is manufactured in advance as a separate member by, for example, extrusion molding, and is placed in the slot 8 when the motor 100 is manufactured.
[0061] As shown in FIG. 10 , the liner member 20 has a square-shaped cross section. When the liner member 20 is placed in the slot 8, the outer circumferential surface of the liner member 20 is in close contact with the wall surfaces 72 and 73 of the slot 8 and the resin sealing portion 65. Here, the outer circumferential surface of the liner member 20, like the inner surface resin layer 51, is linearly arranged parallel to the rotational axis direction. This allows the inner surface resin layer 51 and the liner member 20 to be in close contact with each other overall, improving the heat transfer characteristics from the liner member 20 to the resin layer 50. In other words, the resin layer surface 55 of the inner surface resin layer 51 is not tapered and is linearly arranged parallel to the rotational axis direction, and the outer circumferential surface of the liner member 20 (the region in contact with the resin layer surface 55) is also not tapered and is linearly arranged parallel to the rotational axis direction. This allows the liner member 20 and the resin layer surface 55 to be in close contact with each other without any gaps.
[0062] The thickness of the liner member 20 is, for example, about 0.3 mm at the thinnest region (between the wall surfaces 72, 73 and the inner surface of the liner member 20).
[0063] <Material of the liner member 20> The material of the liner member 20 may be the same as that described as the material of the resin layer 50 in the first embodiment.
[0064] <Types of Shapes of Liner Member 20> 11 shows examples of the shape of the liner member 20. Four types of cross-sectional shapes are shown here. The liner member 20A of FIG. 11(a) corresponds to the shape of the liner member 20 shown in FIG. 10, and has a cross section in the shape of a square frame, with a plurality of coils 9 housed in a common coil housing portion 21. 11(b) is provided with a frame-shaped cross section in the shape of a U. When the liner member 20 is accommodated in the slot 8, the open end side is positioned on the resin sealing portion 65 side. The liner member 20C in Fig. 11(c) has a shape in which a plurality of (here, five) coil accommodating portions 21, each of which has a square-shaped cross section, are connected together. A coil 9 is accommodated in each of the coil accommodating portions 21. This ensures insulation between the coils 9. A liner member 20D in FIG. 11(d) has a configuration in which the liner member 20 of the first embodiment and a resin sealing portion 65 are integrated together.
[0065] The features of this embodiment can be summarized as follows. The present embodiment has the same features as the features (1) to (10) of the first embodiment, and also has the following feature (11). (11) The rotating electric machine (motor 100) has a resin liner member 20 (20A, 20B, 20C, 20D) that accommodates the coil 9, The coil 9 is housed in the slot 8 while being housed in the liner member 20 . This allows the coil 9 to be accurately accommodated in the slot 8. As a result, the output efficiency of the motor 100 can be improved, and vibration and noise can also be suppressed.
[0066] <<Fourth embodiment>> In this embodiment, a resin hollow body, a module, a method for manufacturing a resin hollow body, and a method for manufacturing a module will be described.
[0067] Hollow resin bodies such as resin pipe products and pipe parts are lighter and easier to mold than metal pipes, and so have been used in a variety of fields, and various technologies have been proposed for them. For example, a technology has been proposed to increase the degree of design freedom when manufacturing resin pipes with one end closed by injection molding (e.g., Patent No. 5864373).
[0068] In recent years, due to the characteristics of resin pipes as described above, there has been a demand for realizing various products by applying resin hollow bodies such as resin pipes. In particular, there is a growing demand for applying resin hollow bodies with a small diameter pipe structure to products that operate in high temperature ranges, such as power modules and the motor 100 described in the second embodiment. Generally, when manufacturing small diameter pipes, if the length L is long relative to the inner diameter D (i.e., if L / D is large), a manufacturing method using extrusion molding, more specifically, a molded product using a plastic product, has been used. However, this method may not be able to meet the specifications required for products that operate in high temperature ranges, and therefore a technology using thermosetting resins has been desired.
[0069] In this embodiment, a resin hollow body having a long, linear pipe structure made of a thermosetting resin, a module using the same, and a manufacturing method for the same will be described.
[0070] The outline of this embodiment is as follows. 1. A resin hollow body having a long, linear pipe structure made of a thermosetting resin, The hollow resin body has a ratio L / D1 of an inner diameter D1 to a length L of the pipe structure of 20 or more and 125 or less. 2. The hollow resin body according to 1., wherein the end of the inner surface of the pipe structure is formed straight without any tapered shape. 3. The hollow resin body according to 1. or 2., wherein the thermosetting resin is an epoxy resin. 4. A resin hollow body according to any one of 1. to 3., wherein the inner diameter D1 of the pipe structure is 1.8 mm or more and 3.5 mm or less. 5. A resin hollow body according to any one of 1. to 4., wherein the wall thickness t of the pipe structure is 0.10 mm or more and 1 mm or less. 6. A resin hollow body according to any one of 1. to 5., wherein the outer diameter D2 of the pipe structure is 2.0 mm or more and 4.5 mm or less. 7. A module comprising a hollow resin body according to any one of 1. to 6. above. 8. The module according to 7., wherein the hollow resin body is provided as a cooling water channel. 9. A method for manufacturing a resin hollow body having a long, linear pipe structure, comprising: a resin filling step of filling a molding die having a long, linear die pin having an outer peripheral surface corresponding to the inner peripheral surface of the pipe structure with a thermosetting resin; a mold pin removal step of removing the mold pin; and The method for producing a hollow resin body, wherein the ratio L / D1 of the inner diameter D1 to the length L of the pipe structure is 20 or more and 125 or less. 10. The method for producing a hollow resin body according to 9., wherein the mold pin does not have a tapered shape for extraction. 11. The method for producing a hollow resin body according to 9. or 10., wherein the thermosetting resin is an epoxy resin. 12. A method for manufacturing a resin hollow body according to any one of 9. to 11., wherein the inner diameter D1 of the pipe structure is 1.8 mm or more and 3.5 mm or less. 13. A method for producing a resin hollow body according to any one of 9. to 12., wherein the wall thickness t of the pipe structure is 0.10 mm or more and 1 mm or less. 14. A method for manufacturing a resin hollow body according to any one of 9. to 13., wherein the outer diameter D2 of the pipe structure is 2.0 mm or more and 4.5 mm or less. 15. A method for producing a resin hollow body according to any one of 9. to 14., wherein the filling pressure when filling the thermosetting resin into the molding die is 10 MPa or more and 12 MPa or less. 16. A method for manufacturing a module, comprising using the method for manufacturing a hollow resin body according to any one of items 9 to 15 above to manufacture a module having the hollow resin body. 17. The method for manufacturing a module according to 16, wherein the hollow resin body is manufactured as a cooling water channel.
[0071] Below, we will specifically explain the configuration in which a resin pipe (hollow resin body) is applied to cooling a power module (power semiconductor chip), but it can also be applied to, for example, the cooling water passage 10 of the motor 100 of the second embodiment described above.
[0072] <Power Module 201> A power module 201 according to this embodiment will be described. 12 is a schematic cross-sectional view of a power module 201 according to this embodiment. FIG. 13 is a schematic view of a small-diameter resin pipe 200.
[0073] The power module 201 has a power semiconductor chip 202, a sintering layer 203, a Cu circuit 204, a heat dissipation sheet 205, a Cu base plate 206, and a lead frame 207, and is sealed with a resin sealing layer 209 (sealing material). Furthermore, the power module 201 has a first cooling water channel 210 provided in the resin sealing layer 209 and a second cooling water channel 220 provided in the Cu base plate 206.
[0074] <Power semiconductor chip 202> The power semiconductor chip 202 is, for example, an insulated gate bipolar transistor (IGBT), a diode, etc. An electrode pattern (not shown) is formed on the upper surface of the power semiconductor chip 202, and a conductive pattern (not shown) is formed on the lower surface of the power semiconductor chip 202.
[0075] The lower surface of the power semiconductor chip 202 is joined to one surface of the Cu circuit 204 via a sintering layer 203 which is a joining layer. The electrode pattern on the upper surface of the power semiconductor chip 202 is electrically connected to the lead frame 207.
[0076] <Sintering layer 203> The sintering layer 203 is a joining layer formed by sintering a sintering paste containing metal particles. As the sintering paste, any one of an Ag sintering paste containing silver particles, an AL sintering paste containing aluminum particles, and a Cu sintering paste containing copper particles can be used.
[0077] The above-mentioned sintering paste is provided and laminated between the power semiconductor chip 202 and the Cu circuit 204, and the power semiconductor chip 202 and the Cu circuit 204 are joined by the sintering layer 203 through a sintering process. Also, the lead frame 207 and the Cu circuit 204 are joined by the sintering layer 203.
[0078] In the sintering layer 203, a sintering network (metal bonding bus) by metal particles is formed, and high thermal conductivity and low electrical resistance are realized. From the viewpoint of improving the joining property by the sintering layer 203, the Cu circuit 204 and the lead frame 207 may be subjected to a surface treatment of plating with the metal contained in the sintering paste. Specifically, in this embodiment, the surfaces of the Cu circuit 204 and the lead frame 207 may be subjected to Ag plating.
[0079] <Cu circuit 204> The Cu circuit 204 is a metal circuit board made of a conductive metal material. The power semiconductor chip 202 is provided on a circuit pattern formed on one surface (the upper surface in the drawing) of the Cu circuit 204 via a sintering layer 203 which is a joining layer.
[0080] The Cu circuit 204 is a circuit board patterned from a metal material, and has a thickness of, for example, 0.3 mm to 5 mm. For example, thick copper (rolled copper) can be suitably used as the metal material constituting the Cu circuit 204. This allows the Cu circuit 204 to have a relatively low resistance. At least a portion of the Cu circuit 204 may be covered with a solder resist layer.
[0081] The Cu circuit 204 is formed, for example, by processing a metal layer (such as thick copper) laminated on the upper surface of the Cu base plate 206 via a heat dissipation sheet 205 into a predetermined pattern by cutting and etching, or by attaching the metal layer to the Cu circuit 204 with the heat dissipation sheet 205 after being processed into a predetermined pattern in advance.
[0082] The lower limit of the thickness of the Cu circuit 204 is, for example, 0.3 mm or more. If the thickness is equal to or greater than this value, heat generation in the circuit pattern can be suppressed even in applications requiring high current. Furthermore, the upper limit of the thickness of the circuit pattern is, for example, 5.0 mm or less, preferably 4.0 mm or less, and more preferably 3.0 mm or less. If the thickness is equal to or less than this value, circuit processability can be improved, and the substrate as a whole can be made thinner.
[0083] <Heat dissipation sheet 205> The heat dissipation sheet 205 is disposed between the Cu circuit 204 and the Cu base plate 206. The heat from the power semiconductor chip 202 is received by the Cu circuit 204, and is then transferred via the heat dissipation sheet 205 to the Cu base plate 206, which is heat dissipation means.
[0084] The planar shape of heat dissipation sheet 205 is not particularly limited and can be selected appropriately to match the shapes of Cu circuit 204 and Cu base plate 206, but can be rectangular, for example. Heat dissipation sheet 205 has a thickness of, for example, 50 μm or more and 250 μm or less. This allows for more effective transfer of heat from Cu circuit 204 to Cu base plate 206 while improving mechanical strength and heat resistance. Furthermore, heat dissipation sheet 205 has an excellent balance of heat dissipation and insulation properties. The thermal conductivity of heat dissipation sheet 205 is not particularly limited, but is preferably 10 W / mK (175°C) or more, more preferably 15 W / mK (175°C) or more.
[0085] [Material of heat dissipation sheet 205] The heat dissipation sheet 205 is, for example, a resin sheet, and is formed using a resin composition for a sheet. The resin composition for a sheet will be described below. In this embodiment, the resin composition for the sheet preferably contains a thermosetting resin (A), a filler (B), a curing agent (C), etc. When the resin composition contains a thermosetting resin, the heat dissipation sheet 205 is made by B-stage the thermosetting resin (A).
[0086] [Thermosetting resin (A)] Examples of the thermosetting resin (A) include epoxy resins, cyanate resins, polyimide resins, benzoxazine resins, unsaturated polyester resins, phenolic resins, melamine resins, silicone resins, bismaleimide resins, phenoxy resins, and acrylic resins. As the thermosetting resin (A), one of these may be used alone, or two or more may be used in combination. Among these, from the viewpoint of high insulating properties, epoxy resin, phenol resin, and phenoxy resin are preferred as the thermosetting resin (A).
[0087] Examples of epoxy resins include bisphenol type epoxy resins such as bisphenol A type epoxy resin, bisphenol F type epoxy resin, bisphenol E type epoxy resin, bisphenol S type epoxy resin, bisphenol M type epoxy resin (4,4'-(1,3-phenylenediisopridiene)bisphenol type epoxy resin), bisphenol P type epoxy resin (4,4'-(1,4-phenylenediisopridiene)bisphenol type epoxy resin), and bisphenol Z type epoxy resin (4,4'-cyclohexidienebisphenol type epoxy resin); phenol novolac type epoxy resin, cresol novolac type epoxy resin, trisphenol methane type novolac type epoxy resin, tetraphenol group ethoxylated epoxy resin, and the like. Examples of epoxy resins include novolac-type epoxy resins such as benzophenone-type novolac-type epoxy resins and novolac-type epoxy resins having a condensed ring aromatic hydrocarbon structure; biphenyl-type epoxy resins; aryl alkylene-type epoxy resins such as xylylene-type epoxy resins and biphenyl aralkyl-type epoxy resins; naphthalene-type epoxy resins such as naphthylene ether-type epoxy resins, naphthol-type epoxy resins, naphthalene diol-type epoxy resins, bifunctional to tetrafunctional epoxy-type naphthalene resins, binaphthyl-type epoxy resins, and naphthalene aralkyl-type epoxy resins; anthracene-type epoxy resins; phenoxy-type epoxy resins; dicyclopentadiene-type epoxy resins; norbornene-type epoxy resins; adamantane-type epoxy resins; and fluorene-type epoxy resins. These may be used alone or in combination of two or more.
[0088] Among the epoxy resins, from the viewpoint of further improving heat resistance and insulation reliability, it is preferable to use one or more types selected from the group consisting of bisphenol-type epoxy resins, novolac-type epoxy resins, biphenyl-type epoxy resins, aryl alkylene-type epoxy resins, naphthalene-type epoxy resins, anthracene-type epoxy resins, and dicyclopentadiene-type epoxy resins.
[0089] Examples of phenolic resins include novolac-type phenolic resins such as phenol novolac resin, cresol novolac resin, and bisphenol A novolac resin, and resol-type phenolic resins, etc. One of these may be used alone, or two or more may be used in combination. Among the phenolic resins, phenolic novolac resins are preferred.
[0090] The content of the thermosetting resin (A) is preferably 1% by mass or more, more preferably 5% by mass or more, based on the total amount of the resin composition for the sheet, while the content is preferably 30% by mass or less, more preferably 20% by mass or less, based on the total amount of the resin composition for the sheet. When the content of the thermosetting resin (A) is at least the above lower limit, the handleability of the sheet resin composition improves, the heat radiation insulation sheet can be easily formed, and the strength of the heat radiation insulation sheet is improved. When the content of the thermosetting resin (A) is at most the above upper limit, the linear expansion coefficient and elastic modulus of the heat radiation insulation sheet are further improved, and the thermal conductivity is further improved.
[0091] [Filler (B)] The filler (B) in this embodiment is used from the viewpoint of improving the thermal conductivity of the heat dissipation sheet 205 and also obtaining strength.
[0092] The filler (B) is preferably a thermally conductive filler. More specifically, from the viewpoint of achieving a balance between thermal conductivity and electrical insulation, examples of the filler (B) include silica, alumina, boron nitride, aluminum nitride, and silicon carbide. These may be used alone or in combination of two or more. Of these, the filler (B) is preferably alumina or boron nitride.
[0093] The content of the filler (B) is preferably 90% by mass or less, more preferably 80% by mass or less, based on the total amount of the resin composition for the sheet, while from the viewpoint of thermal conductivity, the content is preferably 40% by mass or more, more preferably 50% by mass or more, based on the total amount of the resin composition for the sheet.
[0094] [Hardening agent (C)] When an epoxy resin or a phenol resin is used as the thermosetting resin (A), the resin composition for a sheet preferably further contains a curing agent (C).
[0095] As the curing agent (C), one or more selected from the curing catalyst (C-1) and the phenol-based curing agent (C-2) can be used. Examples of the curing catalyst (C-1) include organic metal salts such as zinc naphthenate, cobalt naphthenate, tin octoate, cobalt octoate, bisacetylacetonate cobalt(II), and trisacetylacetonate cobalt(III); tertiary amines such as triethylamine, tributylamine, and 1,4-diazabicyclo[2.2.2]octane; 2-phenyl-4-methylimidazole, 2-ethyl-4-methylimidazole, 2,4-diethylimidazole, and 2-phenyl-4-methyl-5-hydroxyimidazole; Examples of suitable curing catalysts include imidazoles such as 2-phenyl-4,5-dihydroxymethylimidazole; organic phosphorus compounds such as triphenylphosphine, tri-p-tolylphosphine, tetraphenylphosphonium tetraphenylborate, triphenylphosphine triphenylborane, and 1,2-bis-(diphenylphosphino)ethane; phenolic compounds such as phenol, bisphenol A, and nonylphenol; and organic acids such as acetic acid, benzoic acid, salicylic acid, and p-toluenesulfonic acid, or mixtures thereof. The curing catalyst (C-1) can be used alone or in combination with two or more of these, including their derivatives. The content of the curing catalyst (C-1) is not particularly limited, but is preferably 0.001% by mass or more and 1% by mass or less based on the total amount of the resin composition for a sheet.
[0096] Examples of the phenolic curing agent (C-2) include novolac-type phenolic resins such as phenol novolac resin, cresol novolac resin, trisphenolmethane-type novolac resin, naphthol novolac resin, and aminotriazine novolac resin; modified phenolic resins such as terpene-modified phenolic resin and dicyclopentadiene-modified phenolic resin; aralkyl-type resins such as phenol aralkyl resins having a phenylene skeleton and / or biphenylene skeleton and naphthol aralkyl resins having a phenylene skeleton and / or biphenylene skeleton; bisphenol compounds such as bisphenol A and bisphenol F; and resol-type phenolic resins, and these may be used alone or in combination of two or more. Among these, from the viewpoint of improving the glass transition temperature and reducing the linear expansion coefficient, the phenolic curing agent (C-2) is preferably a novolac type phenolic resin or a resol type phenolic resin.
[0097] The content of the phenolic curing agent (C-2) is not particularly limited, but is preferably 1% by mass or more, more preferably 5% by mass or more, based on the total amount of the resin composition for sheets, while the content is preferably 30% by mass or less, more preferably 15% by mass or less, based on the total amount of the resin composition for sheets.
[0098] [Coupling agent (D)] The resin composition for a sheet may contain a coupling agent (D), which can improve the wettability at the interface between the thermosetting resin (A) and the filler (B).
[0099] The coupling agent (D) is not particularly limited, but it is preferable to use one or more coupling agents selected from, for example, epoxy silane coupling agents, cationic silane coupling agents, amino silane coupling agents, titanate-based coupling agents, and silicone oil-type coupling agents. The content of the coupling agent (D) is not particularly limited, but is preferably 0.05% by mass or more, more preferably 0.1% by mass or more, relative to 100% by mass of the filler (B), and is preferably 3% by mass or less, more preferably 2% by mass or less, relative to 100% by mass of the filler (B).
[0100] [Phenoxy resin (E)] Furthermore, the resin composition for the sheet may contain a phenoxy resin (E). By containing the phenoxy resin (E), the bending resistance of the heat dissipation sheet 205 can be improved. Furthermore, by including the phenoxy resin (E), it is possible to reduce the elastic modulus of heat dissipation sheet 205, and the stress relaxation force of heat dissipation sheet 205 can be improved.
[0101] Furthermore, when the phenoxy resin (E) is contained, the viscosity increases, reducing fluidity and preventing voids. Furthermore, when the heat dissipation sheet 205 is used in close contact with a metal member, the adhesion between the metal and the cured resin composition for the sheet can be improved. These synergistic effects further enhance the insulation reliability of the power module 201.
[0102] The phenoxy resin (E) may be, for example, a phenoxy resin having a bisphenol skeleton. Examples of suitable phenoxy resins include phenoxy resins having a naphthalene skeleton, phenoxy resins having an anthracene skeleton, and phenoxy resins having a biphenyl skeleton. Phenoxy resins having a structure containing a plurality of these skeletons can also be used.
[0103] The content of the phenoxy resin (E) is preferably, for example, 3% by mass or more and 10% by mass or less relative to the total amount of the resin composition for a sheet.
[0104] [Other ingredients] The resin composition for sheets may also contain other additives such as antioxidants and leveling agents, as long as the effects of the present invention are not impaired.
[0105] <1st cooling waterway 210> A first cooling water channel 210 extending left and right as shown is provided above the power semiconductor chip 202 and the lead frame 207. The first cooling water channel 210 is provided as a configuration in which a small diameter resin pipe 200, which will be described later, is embedded in the resin sealing layer 209. A plurality of small diameter resin pipes 200 are provided depending on the required heat dissipation conditions. A refrigerant (e.g., cooling water) circulates through the first cooling water channel 210, and heat generated by the power semiconductor chip 202 is dissipated to the outside.
[0106] <Small diameter resin pipe 200 (hollow resin body)> The small-diameter resin pipe 200 is a hollow resin body having a long, straight pipe structure made of a thermosetting resin (A). In this embodiment, the small-diameter resin pipe 200 (hollow resin body) is used to cool the power semiconductor chip 202, but it can also be used, for example, in the cooling water passage 10 of the motor 100 of the second embodiment.
[0107] Examples of the thermosetting resin (A) include epoxy resins, cyanate resins, polyimide resins, benzoxazine resins, unsaturated polyester resins, phenolic resins, melamine resins, silicone resins, bismaleimide resins, phenoxy resins, and acrylic resins. As the thermosetting resin (A), one of these may be used alone, or two or more may be used in combination, but epoxy resins are preferred.
[0108] Examples of epoxy resins include bisphenol type epoxy resins such as bisphenol A type epoxy resin, bisphenol F type epoxy resin, bisphenol E type epoxy resin, bisphenol S type epoxy resin, bisphenol M type epoxy resin (4,4'-(1,3-phenylenediisopridiene)bisphenol type epoxy resin), bisphenol P type epoxy resin (4,4'-(1,4-phenylenediisopridiene)bisphenol type epoxy resin), and bisphenol Z type epoxy resin (4,4'-cyclohexidienebisphenol type epoxy resin); phenol novolac type epoxy resin, cresol novolac type epoxy resin, trisphenol methane type novolac type epoxy resin, tetraphenol group ethoxylated epoxy resin, and the like. Examples of epoxy resins include novolac-type epoxy resins such as benzophenone-type novolac-type epoxy resins and novolac-type epoxy resins having a condensed ring aromatic hydrocarbon structure; biphenyl-type epoxy resins; aryl alkylene-type epoxy resins such as xylylene-type epoxy resins and biphenyl aralkyl-type epoxy resins; naphthalene-type epoxy resins such as naphthylene ether-type epoxy resins, naphthol-type epoxy resins, naphthalene diol-type epoxy resins, bifunctional to tetrafunctional epoxy-type naphthalene resins, binaphthyl-type epoxy resins, and naphthalene aralkyl-type epoxy resins; anthracene-type epoxy resins; phenoxy-type epoxy resins; dicyclopentadiene-type epoxy resins; norbornene-type epoxy resins; adamantane-type epoxy resins; and fluorene-type epoxy resins. These may be used alone or in combination of two or more.
[0109] Among the epoxy resins, from the viewpoint of further improving heat resistance and insulation reliability, it is preferable to use one or more types selected from the group consisting of bisphenol-type epoxy resins, novolac-type epoxy resins, biphenyl-type epoxy resins, aryl alkylene-type epoxy resins, naphthalene-type epoxy resins, anthracene-type epoxy resins, and dicyclopentadiene-type epoxy resins.
[0110] Examples of phenolic resins include novolac-type phenolic resins such as phenol novolac resin, cresol novolac resin, and bisphenol A novolac resin, and resol-type phenolic resins, etc. One of these may be used alone, or two or more may be used in combination. Among the phenolic resins, phenolic novolac resins are preferred.
[0111] The content of the thermosetting resin (A) is preferably 1% by mass or more, more preferably 5% by mass or more, based on the total amount of the resin composition for a hollow resin body, while the content is preferably 30% by mass or less, more preferably 20% by mass or less, based on the total amount of the resin composition for a hollow resin body. When the content of the thermosetting resin (A) is equal to or greater than the above lower limit, the handleability of the resin composition for a resin hollow body is improved, making it easier to form a small-diameter resin pipe 200 (a resin hollow body), and improving the strength of the small-diameter resin pipe 200. When the content of the thermosetting resin (A) is equal to or less than the upper limit, the linear expansion coefficient and elastic modulus of the small diameter resin pipe 200 are further improved, and the thermal conductivity is further improved.
[0112] [Filler (B)] The filler (B) in this embodiment is used from the viewpoint of improving the thermal conductivity of the small-diameter resin pipe 200 and obtaining strength.
[0113] The filler (B) is preferably a thermally conductive filler. More specifically, from the viewpoint of achieving a balance between thermal conductivity and electrical insulation, examples of the filler (B) include silica, alumina, boron nitride, aluminum nitride, and silicon carbide. These may be used alone or in combination of two or more. Of these, the filler (B) is preferably alumina or boron nitride.
[0114] The content of the filler (B) is preferably 90% by mass or less, more preferably 80% by mass or less, based on the total amount of the resin composition for a resin hollow body, while from the viewpoint of thermal conductivity, the content is preferably 40% by mass or more, more preferably 50% by mass or more, based on the total amount of the resin composition for a resin hollow body.
[0115] [Hardening agent (C)] When an epoxy resin or a phenol resin is used as the thermosetting resin (A), the resin composition for a hollow resin body preferably further contains a curing agent (C).
[0116] As the curing agent (C), one or more selected from the curing catalyst (C-1) and the phenol-based curing agent (C-2) can be used. Examples of the curing catalyst (C-1) include organic metal salts such as zinc naphthenate, cobalt naphthenate, tin octoate, cobalt octoate, bisacetylacetonate cobalt(II), and trisacetylacetonate cobalt(III); tertiary amines such as triethylamine, tributylamine, and 1,4-diazabicyclo[2.2.2]octane; 2-phenyl-4-methylimidazole, 2-ethyl-4-methylimidazole, 2,4-diethylimidazole, and 2-phenyl-4-methyl-5-hydroxyimidazole; Examples of suitable curing catalysts include imidazoles such as 2-phenyl-4,5-dihydroxymethylimidazole; organic phosphorus compounds such as triphenylphosphine, tri-p-tolylphosphine, tetraphenylphosphonium tetraphenylborate, triphenylphosphine triphenylborane, and 1,2-bis-(diphenylphosphino)ethane; phenolic compounds such as phenol, bisphenol A, and nonylphenol; and organic acids such as acetic acid, benzoic acid, salicylic acid, and p-toluenesulfonic acid, or mixtures thereof. The curing catalyst (C-1) can be used alone or in combination with two or more of these, including their derivatives. The content of the curing catalyst (C-1) is not particularly limited, but is preferably 0.001% by mass or more and 1% by mass or less based on the total amount of the resin composition for a hollow resin body.
[0117] Examples of the phenolic curing agent (C-2) include novolac-type phenolic resins such as phenol novolac resin, cresol novolac resin, trisphenolmethane-type novolac resin, naphthol novolac resin, and aminotriazine novolac resin; modified phenolic resins such as terpene-modified phenolic resin and dicyclopentadiene-modified phenolic resin; aralkyl-type resins such as phenol aralkyl resins having a phenylene skeleton and / or biphenylene skeleton and naphthol aralkyl resins having a phenylene skeleton and / or biphenylene skeleton; bisphenol compounds such as bisphenol A and bisphenol F; and resol-type phenolic resins, and these may be used alone or in combination of two or more. Among these, from the viewpoint of improving the glass transition temperature and reducing the linear expansion coefficient, the phenolic curing agent (C-2) is preferably a novolac type phenolic resin or a resol type phenolic resin.
[0118] The content of the phenolic curing agent (C-2) is not particularly limited, but is preferably 1% by mass or more, more preferably 5% by mass or more, based on the total amount of the resin composition for a resin hollow body, and is preferably 30% by mass or less, more preferably 15% by mass or less, based on the total amount of the resin composition for a sheet.
[0119] [Coupling agent (D)] The resin composition for a resin hollow body may contain a coupling agent (D), which can improve the wettability at the interface between the thermosetting resin (A) and the filler (B).
[0120] The coupling agent (D) is not particularly limited, but it is preferable to use one or more coupling agents selected from, for example, epoxy silane coupling agents, cationic silane coupling agents, amino silane coupling agents, titanate-based coupling agents, and silicone oil-type coupling agents. The content of the coupling agent (D) is not particularly limited, but is preferably 0.05% by mass or more, more preferably 0.1% by mass or more, relative to 100% by mass of the filler (B), and is preferably 3% by mass or less, more preferably 2% by mass or less, relative to 100% by mass of the filler (B).
[0121] [Phenoxy resin (E)] Furthermore, the resin composition for a hollow resin body may contain a phenoxy resin (E). By containing the phenoxy resin (E), the bending resistance of the small-diameter resin pipe 200 can be improved. Furthermore, by including the phenoxy resin (E), it is possible to reduce the elastic modulus of the small diameter resin pipe 200, and the stress relaxation force of the small diameter resin pipe 200 can be improved.
[0122] Furthermore, when the phenoxy resin (E) is contained, the viscosity increases, which reduces the flowability and prevents the occurrence of voids and the like.
[0123] The phenoxy resin (E) may be, for example, a phenoxy resin having a bisphenol skeleton. Examples of suitable phenoxy resins include phenoxy resins having a naphthalene skeleton, phenoxy resins having an anthracene skeleton, and phenoxy resins having a biphenyl skeleton. Phenoxy resins having a structure containing a plurality of these skeletons can also be used.
[0124] The content of the phenoxy resin (E) is preferably, for example, 3% by mass or more and 10% by mass or less relative to the total amount of the resin composition for a hollow resin body.
[0125] [Other ingredients] The resin composition for a hollow resin body may also contain other additives such as an antioxidant and a leveling agent, provided that the effects of the present invention are not impaired.
[0126] <Pipe structure of small diameter resin pipe 200> The small diameter resin pipe 200 has the following pipe structure features. The small-diameter resin pipe 200 is a cylindrical pipe in which an end 212 of an inner surface 211 is formed straight and not tapered. In this embodiment, a cylindrical pipe with a circular cross section is exemplified, but the small-diameter resin pipe 200 may be a pipe with an irregular cross section such as an ellipse or a polygon.
[0127] The inner diameter D1 of the small-diameter resin pipe 200 is 1.8 mm or more and 3.5 mm or less. If the small-diameter resin pipe 200 is a non-circular pipe, the narrowest width of the inner diameter is taken as D1. The lower limit of the inner diameter D1 is preferably 1.9 mm or more, and more preferably 2.0 mm or more. The upper limit is preferably 3.2 mm or less, and more preferably 3.0 mm or less.
[0128] The outer diameter D2 of the small diameter resin pipe 200 is 2.0 mm or more and 4.5 mm or less, preferably 2.1 mm or more, and more preferably 2.2 mm or more. The upper limit is preferably 4.2 mm or less, and more preferably 4.0 mm or less.
[0129] The wall thickness t (=(D2-D1) / 2) of the small diameter resin pipe 200 is 0.10 mm or more and 1 mm or less. The lower limit of the wall thickness t is preferably 0.15 mm or more, more preferably 0.20 mm or more. The upper limit is preferably 0.9 mm or less, more preferably 0.8 mm or less.
[0130] The length L of the small diameter resin pipe 200 is 60 mm or more and 250 mm or less. The lower limit of the length L is preferably 70 mm or more, and more preferably 80 mm or more. The upper limit is preferably 230 mm or less, and more preferably 200 mm or less.
[0131] The ratio L / D1 of the inner diameter D1 to the length L of the small diameter resin pipe 200 is 20 or more and 125 or less. The lower limit of the ratio L / D1 is preferably 25 or more, more preferably 30 or more. The upper limit is preferably 120 or less, more preferably 100 or less. For example, when the length L is 60 mm and the inner diameter D1 is 3 mm, the ratio L / D1 is 20. When the length L is 250 mm and the inner diameter D1 is 2 mm, the ratio L / D1 is 125.
[0132] <Cuベースプレート206> The Cu base plate 206 is a type of heat dissipation member, and has a copper plate-shaped base and a second cooling water channel 220 provided in the lower region of the base as shown in the drawing.
[0133] The heat dissipation member may be, for example, an aluminum base plate other than the Cu base plate 206. Furthermore, the heat dissipation member is not limited to a general heat dissipation member, and may be a part of another configuration (for example, a housing) as long as it has the function of obtaining heat generated by the power semiconductor chip 202 via the Cu circuit 204 and dissipating it elsewhere.
[0134] <Second cooling waterway 220> Similar to the first cooling water channel 210, the second cooling water channel 220 has a function of circulating a coolant therein and releasing heat from the Cu base plate 206 to the outside. The second cooling water channel 220 may be formed by hollowing out the Cu base plate 206 so that all of the inner wall surfaces are configured as part of the Cu base plate 206, or the second cooling water channel 220 may be configured by disregarding the pipe arrangement structure in the Cu base plate 206 and arranging a resin hollow body similar to the small diameter resin pipe 200 there and filling the periphery with resin.
[0135] <Lead frame 207> The lead frame 207 supports and fixes the power semiconductor chip 202 and electrically connects it to external wiring, and is a component made by pressing or etching a thin plate of a metal material such as copper or iron.
[0136] <Resin sealing layer 209> The resin sealing layer 209 is, for example, a molded resin, and integrally seals the power semiconductor chip 202, the sintering layer 203, the Cu circuit 204, the heat dissipation sheet 205, the Cu base plate 206, the lead frame 207, and the first cooling water channel 210 therein.
[0137] Besides mold resin, silicone gel or the like may be used as resin sealing layer 209. The following describes a configuration in which the components are integrally sealed with mold resin.
[0138] In this sealing, a portion of the lead frame 207 is sealed, and the remaining unsealed portion is connected to an external device. Furthermore, with regard to the Cu base plate 206, the upper surface and side surfaces of the Cu base plate 206 are covered and sealed with a resin sealing layer 209. The lower surface of the Cu base plate 206 and the second cooling water channels 220 are not covered with the resin sealing layer 209. In other words, the resin sealing layer 209 covers and seals the power semiconductor chip 202 so as to cover part or all of the side surfaces of the base 5A of the Cu base plate 206 in the thickness direction. Here, a configuration in which all of the side surfaces of the base 5A of the Cu base plate 206 are covered with the resin sealing layer 209 is exemplified.
[0139] [Components of resin sealing layer 209 (mold resin)] The molding resin of the resin sealing layer 209 is a cured product of a thermosetting composition (C) containing a thermosetting resin (A) and an inorganic filler (B). The thermosetting composition (C) contains a curing accelerator (D).
[0140] [Curing accelerator (D)] The curing accelerator (D) of this embodiment has strong activity, which allows low-temperature curing to be achieved, but if used as is without any special measures, the reaction will proceed during storage, reducing the shelf life. Examples of the curing accelerator (D) include phosphorus atom-containing compounds such as organic phosphines, tetra-substituted phosphonium compounds, phosphobetaine compounds, adducts of phosphine compounds and quinone compounds, or adducts of phosphonium compounds and silane compounds; amidine compounds such as 1,8-diazabicyclo(5,4,0)undecene-7 and imidazole; and nitrogen atom-containing compounds such as tertiary amines such as benzyldimethylamine, amidinium salts, or ammonium salts. Among these, the curing accelerator (D) is preferably an imidazole-based curing accelerator or a phosphorus-based curing accelerator. The imidazole-based curing accelerator preferably contains, for example, an imidazole compound, which is an amidine-based compound. Examples of imidazole compounds include, but are not limited to, 2-methylimidazole, 2-phenylimidazole, imidazole-2-carbaldehyde, 5-azabenzimidazole, and 4-azabenzimidazole. Of these, 2-methylimidazole is preferably used.
[0141] The content of the curing accelerator (D) in the encapsulating resin composition is not particularly limited, but is preferably 0.1 mass % or more and 5 mass % or less, and more preferably 0.2 mass % or more and 4 mass % or less, based on the total encapsulating resin composition. By setting the content of the curing accelerator (D) to the above lower limit or more, the encapsulating resin composition can be appropriately cured. On the other hand, by setting the content of the curing accelerator (D) to the above upper limit or less, the molten state can be prolonged, and the low-viscosity state can be prolonged, which makes it easier to achieve low-temperature encapsulation.
[0142] [Thermosetting resin (A)] Examples of the thermosetting resin (A) include phenolic resin, epoxy resin, unsaturated polyester resin, melamine resin, and polyurethane. These may be used alone or in combination of two or more. Among these, it is preferable to contain at least one of a phenolic resin and an epoxy resin, and it is more preferable to contain an epoxy resin.
[0143] As the epoxy resin, any monomer, oligomer, or polymer having two or more epoxy groups in one molecule can be used, and there are no particular limitations on the molecular weight or molecular structure. Specific examples of epoxy resins include crystalline epoxy resins such as bisphenol-type epoxy resins (e.g., biphenyl-type epoxy resins, bisphenol A-type epoxy resins, bisphenol F-type epoxy resins, and tetramethylbisphenol F-type epoxy resins), stilbene-type epoxy resins, and hydroquinone-type epoxy resins; novolac-type epoxy resins (e.g., cresol novolac-type epoxy resins, phenol novolac-type epoxy resins, and naphthol novolac-type epoxy resins); aralkyl-type epoxy resins (e.g., phenylene-skeleton-containing phenol aralkyl-type epoxy resins, biphenylene-skeleton-containing phenol aralkyl-type epoxy resins, phenylene-skeleton-containing naphthol aralkyl-type epoxy resins, and alkoxynaphthalene-skeleton-containing phenol aralkyl-type epoxy resins); trifunctional epoxy resins (e.g., triphenolmethane-type epoxy resins and alkyl-modified triphenolmethane-type epoxy resins); modified phenol-type epoxy resins (e.g., dicyclopentadiene-modified phenol-type epoxy resins and terpene-modified phenol-type epoxy resins); and heterocycle-containing epoxy resins (e.g., triazine-nucleus-containing epoxy resins). These may be used alone or in combination of two or more. Among these, it is more preferable to use at least one of an aralkyl type epoxy resin and a naphthyl ether type epoxy resin from the viewpoint of improving the balance between the reliability and moldability of the aluminum electrolytic capacitor.
[0144] The ICI viscosity of the thermosetting resin (A) at 150°C is preferably set appropriately depending on the content of the inorganic filler (B), and for example, the upper limit is preferably 60 poise or less, more preferably 50 poise or less, and even more preferably 40 poise or less, thereby improving the fluidity of the encapsulating resin composition and facilitating low-temperature encapsulation. On the other hand, the lower limit of the ICI viscosity of the thermosetting resin (A) at 150° C. is not particularly limited, but may be, for example, 0.01 poise or more. Note that 1 poise is 0.1 Pa·s.
[0145] The content of the thermosetting resin (A) is not particularly limited, but is preferably 1% by mass or more and 50% by mass or less, more preferably 2% by mass or more and 30% by mass or less, and even more preferably 5% by mass or more and 20% by mass or less, based on the total encapsulating resin composition. By setting the content of the thermosetting resin (A) to the above lower limit or more, the flowability and moldability of the encapsulating resin composition can be more effectively improved, and by setting the content of the thermosetting resin (A) to the above upper limit or less, the reliability of the aluminum electrolytic capacitor can be more effectively improved.
[0146] [Inorganic filler (B)] Examples of the inorganic filler (B) include silica, alumina, kaolin, talc, clay, mica, rock wool, wollastonite, glass powder, glass flakes, glass beads, glass fiber, silicon carbide, silicon nitride, aluminum nitride, carbon black, graphite, titanium dioxide, calcium carbonate, calcium sulfate, barium carbonate, magnesium carbonate, magnesium sulfate, barium sulfate, cellulose, aramid, and wood, etc. These may be used alone or in combination of two or more.
[0147] Examples of the silica include crystalline silica (crushed crystalline silica), fused silica (crushed amorphous silica, spherical amorphous silica), and liquid encapsulated silica (spherical amorphous encapsulated silica for liquid encapsulation). Of these, fused spherical silica is preferred from the viewpoint of facilitating low-temperature, low-pressure encapsulation.
[0148] The average particle size of the inorganic filler (B) is not particularly limited, but is typically 1 to 100 μm, preferably 1 to 50 μm, and more preferably 1 to 20 μm. It is believed that an appropriate average particle size contributes to the effect of more uniformly coating the shell containing the molten mixture in the granulation step described below. Furthermore, when the finally obtained core-shell particles are used as a semiconductor encapsulant, the filling ability around the semiconductor element in the mold cavity can be improved. The volumetric particle size distribution of the inorganic filler (B) can be measured using a commercially available laser particle size distribution analyzer (for example, SALD-7000 manufactured by Shimadzu Corporation).
[0149] The content of the inorganic filler (B) is not particularly limited, but is preferably 50% by mass or more and 95% by mass or less, more preferably 60% by mass or more and 95% by mass or less, and even more preferably 65% by mass or more and 85% by mass or less, based on the entire encapsulating resin composition. By setting the content of the inorganic filler (B) to the above lower limit or more, the reliability of the aluminum electrolytic capacitor encapsulated with the encapsulating resin composition can be effectively improved. Also, by setting the content of the inorganic filler (B) to the above upper limit or less, the flowability of the encapsulating resin composition can be improved, and the moldability can be more effectively improved.
[0150] The encapsulating resin composition of the present embodiment may contain the following components in addition to those described above. [Hardening agent (C)] The encapsulating resin composition may contain a curing agent (C). The curing agent (C) is not particularly limited as long as it reacts with the thermosetting resin (A) to cure it, but examples thereof include linear aliphatic diamines having 2 to 20 carbon atoms, such as ethylenediamine, trimethylenediamine, tetramethylenediamine, and hexamethylenediamine, as well as amines such as metaphenylenediamine, paraphenylenediamine, paraxylenediamine, 4,4'-diaminodiphenylmethane, 4,4'-diaminodiphenylpropane, 4,4'-diaminodiphenylether, 4,4'-diaminodiphenylsulfone, 4,4'-diaminodicyclohexane, bis(4-aminophenyl)phenylmethane, 1,5-diaminonaphthalene, metaxylenediamine, paraxylenediamine, 1,1-bis(4-aminophenyl)cyclohexane, and dicyanodiamide; resole-type phenolic resins, such as aniline-modified resole resins and dimethyl ether resole resins; phenol novolac resins; and cresol. Examples of suitable phenolic resins include novolac-type phenolic resins such as phenol novolac resins, tert-butylphenol novolac resins, and nonylphenol novolac resins; phenol aralkyl resins such as phenylene skeleton-containing phenol aralkyl resins and biphenylene skeleton-containing phenol aralkyl resins; phenolic resins having a condensed polycyclic structure such as a naphthalene skeleton or an anthracene skeleton; polyoxystyrenes such as polyparaoxystyrene; alicyclic acid anhydrides such as hexahydrophthalic anhydride (HHPA) and methyltetrahydrophthalic anhydride (MTHPA), and aromatic acid anhydrides such as trimellitic anhydride (TMA), pyromellitic anhydride (PMDA), and benzophenonetetracarboxylic acid (BTDA); polymercaptan compounds such as polysulfides, thioesters, and thioethers; isocyanate compounds such as isocyanate prepolymers and blocked isocyanates; and organic acids such as carboxylic acid-containing polyester resins. These may be used alone or in combination of two or more. Among these, from the viewpoint of realizing low-temperature and low-pressure sealing of the encapsulating resin composition, it is more preferable to use at least one of a novolac type phenolic resin and a phenol aralkyl resin.
[0151] The content of the curing agent (C) in the encapsulating resin composition is not particularly limited, but is preferably 1% by mass or more and 12% by mass or less, and more preferably 3% by mass or more and 10% by mass or less, based on the total mass of the encapsulating resin composition. By setting the content of the curing agent (C) to the above lower limit or more, the encapsulating resin composition can be easily cured appropriately, whereas by setting the content of the curing agent (C) to the above upper limit or less, the encapsulating resin composition can maintain appropriate fluidity, making it easier to achieve low-temperature, low-pressure encapsulation.
[0152] [Coupling agent (E)] The encapsulating resin composition may contain, for example, a coupling agent (E). Examples of the coupling agent (E) that can be used include known coupling agents such as various silane-based compounds, such as epoxysilane, mercaptosilane, aminosilane, alkylsilane, ureidosilane, and vinylsilane, titanium-based compounds, aluminum chelates, and aluminum / zirconium-based compounds. More specifically, vinyltrichlorosilane, vinyltrimethoxysilane, vinyltriethoxysilane, vinyltris(β-methoxyethoxy)silane, γ-methacryloxypropyltrimethoxysilane, β-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, γ-glycidoxypropyltrimethoxysilane, γ-glycidoxypropyltriethoxysilane, γ-glycidoxypropylmethyldimethoxysilane, γ-methacryloxypropylmethyldiethoxysilane, γ-methacryloxypropyltriethoxysilane, vinyltriacetoxysilane, γ-mercaptopropyltrimethoxysilane, γ-aminopropyltriethoxysilane, γ-anilinopropyltrimethoxysilane, γ-anilinopropylmethyldimethoxysilane, γ-[bis(β-hydroxyethyl)]aminopropyltriethoxysilane, N-β-(aminoethyl)-γ-aminopropyltrimethoxysilane, N-β-(aminoethyl) silane coupling agents such as -γ-aminopropyltriethoxysilane, N-β-(aminoethyl)-γ-aminopropylmethyldimethoxysilane, N-phenyl-γ-aminopropyltrimethoxysilane, γ-(β-aminoethyl)aminopropyldimethoxymethylsilane, N-(trimethoxysilylpropyl)ethylenediamine, N-(dimethoxymethylsilylisopropyl)ethylenediamine, methyltrimethoxysilane, dimethyldimethoxysilane, methyltriethoxysilane, N-β-(N-vinylbenzylaminoethyl)-γ-aminopropyltrimethoxysilane, γ-chloropropyltrimethoxysilane, hexamethyldisilane, vinyltrimethoxysilane, γ-mercaptopropylmethyldimethoxysilane, 3-isocyanatepropyltriethoxysilane, 3-acryloxypropyltrimethoxysilane, and 3-triethoxysilyl-N-(1,3-dimethylbutylidene)propylamine hydrolysate;Examples of titanate-based coupling agents include isopropyl triisostearoyl titanate, isopropyl tris (dioctyl pyrophosphate) titanate, isopropyl tri (N-aminoethyl - aminoethyl) titanate, tetraoctyl bis (ditridecyl phosphite) titanate, tetra (2,2-diallyloxymethyl-1-butyl) bis (ditridecyl) phosphite titanate, bis (dioctyl pyrophosphate) oxyacetate titanate, bis (dioctyl pyrophosphate) ethylene titanate, isopropyl trioctanoyl titanate, isopropyl dimethacryl isostearoyl titanate, isopropyl tridodecyl benzenesulfonyl titanate, isopropyl isostearoyl diacryl titanate, isopropyl tri (dioctyl phosphate) titanate, isopropyl tricumyl phenyl titanate, and tetraisopropyl bis (dioctyl phosphite) titanate. These may be used alone or in combination of two or more.
[0153] The content of the coupling agent (E) in the encapsulating resin composition is not particularly limited, but is preferably 0.05% by mass or more and 3% by mass or less, and more preferably 0.1% by mass or more and 2% by mass or less, based on the total encapsulating resin composition. By making the content of the coupling agent (E) equal to or greater than the above-mentioned lower limit, the dispersibility of the inorganic filler (B) in the encapsulating resin composition can be improved. Furthermore, by making the content of the coupling agent (E) equal to or less than the above-mentioned upper limit, the flowability of the encapsulating resin composition can be improved, thereby improving moldability.
[0154] Furthermore, in addition to the above components, the encapsulating resin composition of the present embodiment may contain various additives, such as a colorant such as carbon black; a release agent such as natural wax, synthetic wax, higher fatty acid or metal salts thereof, paraffin, or polyethylene oxide; an ion scavenger such as hydrotalcite; a stress reducing agent such as silicone oil or silicone rubber; a flame retardant such as aluminum hydroxide; and an antioxidant.
[0155] <Method for manufacturing small diameter resin pipe 200> The method for manufacturing the small diameter resin pipe 200 will be described with reference to the flowchart of FIG.
[0156] (Mold preparation process S10) A split mold having a recess formed on its mating surface is prepared as a mold for manufacturing the molded product of the small diameter resin pipe 200. The recess is cylindrical and corresponds to the outer peripheral shape of the small diameter resin pipe 200. For example, when the mold is made up of two split molds, the recess of each split mold corresponds to half of the outer peripheral shape of the small diameter resin pipe 200. A long, straight mold pin (core pin) is placed in the recess so as to extend in the axial direction (pipe length direction). The outer peripheral surface of the mold pin corresponds to the inner peripheral surface of the small-diameter resin pipe 200. Both ends of the core pin are supported to prevent the mold pin from shifting during resin filling. After the mold pin is placed and the mold is closed, the process moves to the next resin filling step S20.
[0157] (Resin filling process S20) The cavity defined by the recess and the mold pin (core pin) is filled with the above-mentioned thermosetting resin (e.g., epoxy resin) at high pressure. The filling pressure at this time is preferably 10 MPa or more and 12 MPa or less. Filling the thermosetting resin at such a filling pressure ensures a smooth and even flow of the resin, thereby preventing filling defects such as short shots.
[0158] (Mold pin removal process S30) Once the filled thermosetting resin has hardened, a predetermined jig is used to pull the mold pin out of the small diameter resin pipe 200. The pulling force can be, for example, 60 kgf to 130 kgf, and if the small diameter resin pipe 200 has a thin wall thickness, the pulling force is reduced to prevent buckling, surface scratches, etc., from occurring during mold release.
[0159] (Mold opening process S40) After the small diameter resin pipe 200 is released from the mold pin (S30), the mold is opened and the small diameter resin pipe 200 is taken out from the mold.
[0160] According to the above-described manufacturing method of the small diameter resin pipe 200, Because the resin flows smoothly during filling and is prevented from sticking to the recessed surface of the mold or the surfaces of the mold pins, the small-diameter resin pipe 200 can be smoothly removed from the mold, particularly when being pulled out from the mold pins. In other words, even if the small-diameter resin pipe 200 does not have a taper for pulling out (a mold-removal taper), the small-diameter resin pipe 200 can be pulled out without damage. That is, a straight small-diameter resin pipe 200 (a hollow resin body) without a mold-removal taper can be manufactured.
[0161] <Manufacturing Method of Power Module 201> A power module 201 is manufactured by placing a set of a power semiconductor chip 202, a sintering layer 203, a Cu circuit 204, a heat dissipation sheet 205, a Cu base plate 206 (including a second cooling water channel 220), and a lead frame 207 in a predetermined mold, and a small diameter resin pipe 200 manufactured by the above-mentioned manufacturing method, and sealing the set with a resin sealing layer 209.
[0162] <Summary of features of the embodiment> The features of this embodiment can be summarized as follows. (1) The small-diameter resin pipe 200 is a hollow resin body having a long, linear pipe structure made of a thermosetting resin, The ratio L / D1 of the inner diameter D1 to the length L of the pipe structure (that is, the small diameter resin pipe 200) is 20 or more and 125 or less. When molding a resin hollow body having a long, straight pipe structure using a thermosetting resin, by setting the ratio L / D1 of the inner diameter D1 to the length L within the above range, the material of the thermosetting resin and the molding pressure can be adjusted, and a small-diameter resin pipe 200 can be molded without quality problems. Since the small diameter resin pipe 200 is made of a thermosetting resin, it can be applied to products that are expected to be used in high temperature regions. (2) In the small diameter resin pipe 200, the end 102 on the inner surface of the pipe structure is formed straight without a tapered shape. As described above, by setting the ratio L / D1 of the inner diameter D1 to the length L within the above range, and adjusting the thermosetting resin material and molding pressure, the inner surface of the pipe can be made straight and not tapered during molding. (3) In the small diameter resin pipe 200, the thermosetting resin is made of epoxy resin. In particular, by using epoxy resin with high thermal conductivity, it can be used for the first cooling water channel 210 of the power module 201, the cooling water channel of the motor, etc., and a structure with excellent insulation performance and thermal efficiency (thermal conductivity) can be realized. (4) In the small diameter resin pipe 200, the inner diameter D1 of the pipe structure is 1.8 mm or more and 3.5 mm or less. Since a small-diameter resin hollow body having an inner diameter D1 within the above range, i.e., the small-diameter resin pipe 200, can be molded from a thermosetting resin, various products having a small-diameter pipe shape as a resin hollow body can be realized. (5) In the small diameter resin pipe 200, the wall thickness t of the pipe structure is 0.10 mm or more and 1 mm or less. Since a small-diameter, thin-walled hollow resin body having a wall thickness t within the above range, i.e., the small-diameter resin pipe 200, can be molded from a thermosetting resin, various products having a small-diameter, thin-walled pipe shape as a hollow resin body can be realized. (6) In the small diameter resin pipe 200, the outer diameter D2 of the pipe structure is 2.0 mm or more and 4.5 mm or less. Since a small diameter resin hollow body with an outer diameter D2 within the above range, i.e., a small diameter resin pipe 200, can be molded from a thermosetting resin, various products having a small diameter pipe shape as a resin hollow body with both an inner diameter D1 and an outer diameter D2 can be realized. (7) In the small diameter resin pipe 200, a module (here, a power module 201) is provided integrally with the above-mentioned resin hollow body. This makes it easy to apply the small diameter resin pipe 200 and other similar pipe-shaped modules to various other shapes. (8) In the small diameter resin pipe 200, a resin hollow body is provided as a cooling water channel (first cooling water channel 210). In modules such as the power module 201 and motors, a cooling structure (water channel structure) with excellent insulation performance and thermal efficiency (thermal conductivity) can be realized. (9) A method for manufacturing a resin hollow body (small diameter resin pipe 200) having a long, linear pipe structure, comprising: a resin filling step (S20) of filling a molding die having a long, straight die pin with a thermosetting resin, the die having an outer peripheral surface corresponding to the inner peripheral surface of the pipe structure; a die pin removal step (S30) of removing the die pin; and The ratio L / D1 of the inner diameter D1 to the length L of the pipe structure is 20 or more and 125 or less. Since the hollow resin body can be manufactured using a mold (molding mold) with mold pins, productivity can be significantly improved compared to manufacturing methods in which a structure equivalent to the inner diameter of the pipe is inserted using sacrificial material, which is then removed after molding. (10) In the method for manufacturing the small-diameter resin pipe 200, the die pin does not have a tapered shape for extraction. As described above, by setting the ratio L / D1 of the inner diameter D1 to the length L within the above range, and adjusting the thermosetting resin material and molding pressure, the inner surface of the pipe can be made straight and not tapered during molding. By setting the pulling force to, for example, 60 to 130 kgf, even in a structure without a tapered shape, molding defects such as cracks in the resin can be avoided and mold release can be achieved. (11) In the method for manufacturing the small-diameter resin pipe 200, the thermosetting resin is made of epoxy resin. In particular, by using epoxy resin with high thermal conductivity, it can be used for the first cooling water channel 210 of the power module 201, the cooling water channel of the motor, etc., and a structure with excellent insulation performance and thermal efficiency (thermal conductivity) can be realized. (12) In the method for manufacturing the small-diameter resin pipe 200, the inner diameter D1 of the pipe structure is 1.8 mm or more and 3.5 mm or less. Since a small-diameter resin hollow body having an inner diameter D1 within the above range, i.e., the small-diameter resin pipe 200, can be molded from a thermosetting resin, various products having a small-diameter pipe shape as a resin hollow body can be realized. (13) In the method for manufacturing the small-diameter resin pipe 200, the wall thickness t of the pipe structure is 0.10 mm or more and 1 mm or less. Since a small-diameter, thin-walled hollow resin body having a wall thickness t within the above range, i.e., the small-diameter resin pipe 200, can be molded from a thermosetting resin, various products having a small-diameter, thin-walled pipe shape as a hollow resin body can be realized. (14) In the method for manufacturing the small-diameter resin pipe 200, the outer diameter D2 of the pipe structure is 2.0 mm or more and 4.5 mm or less. Since a small diameter resin hollow body with an outer diameter D2 within the above range, i.e., a small diameter resin pipe 200, can be molded from a thermosetting resin, various products having a small diameter pipe shape as a resin hollow body with both an inner diameter D1 and an outer diameter D2 can be realized. (15) In the method for manufacturing the small-diameter resin pipe 200, the filling pressure when filling the thermosetting resin into the molding die is 10 MPa or more and 12 MPa or less. By controlling the filling pressure within the above range and filling the curable resin, the flow of the resin during filling can be made smooth and even, and filling defects such as short shots can be suppressed. (16) A method for manufacturing a module (power module 201) having a hollow resin body using the above-described method for manufacturing a hollow resin body (small diameter resin pipe 200). It becomes easy to apply to various modules corresponding to various shapes based on a pipe shape such as the small diameter resin pipe 200. (17) In the method for manufacturing the power module 201, a resin hollow body is manufactured as the cooling water channel (first cooling water channel 210).
[0163] Although the embodiments of the present invention have been described above with reference to the drawings, these are merely examples of the present invention, and various other configurations can also be adopted. [Example]
[0164] The fourth embodiment of the present invention will be described in detail based on examples, although the present invention is not limited to these examples.
[0165] Table 1 shows examples (wt%) of thermosetting resin blends used in Examples 1 to 6, which are molded products (Examples 1 to 6) of resin pipes (hollow resin bodies) corresponding to the small-diameter resin pipe 200 of the fourth embodiment described above. Examples 1 to 3 use a 3W high-thermal-conductivity epoxy material (silica-based), and Examples 4 to 6 use a 5W high-thermal-conductivity epoxy material (alumina-based). Table 2 shows the evaluation results for Examples 1 to 6.
[0166] The manufacturing conditions for the resin pipes (hollow resin bodies) of Examples 1 to 6 are as follows. Molding method: Transfer molding Mold temperature: 170℃ Tablet diameter: φ30mm Plunger diameter: φ35mm Tablet preheat temperature: 90℃ Material injection pressure: 8MPa Material injection time: 8 seconds Curing time: 180 seconds
[0167] In Examples 1 and 4, the resin filling property in the resin filling step was good, and no pin damage occurred in the mold pin removal step. It was confirmed that mold release was possible with a removal force of 130 kg or less.
[0168] In Examples 2 and 5, the resin filling property in the resin filling step was good, and there was no pin damage or molding defects in the mold pin removal step. It was confirmed that the mold could be released with a removal force of 60 kg or less.
[0169] In Examples 3 and 6, the resin filling was good during the resin filling process, and there was no pin damage during the mold pin removal process. It was confirmed that demolding was possible with a removal force of 60 kg or less. However, buckling sometimes occurred during demolding, which is thought to be due to the thin wall.
[0170] [Table 1] [Table 2]
[0171] This application claims priority based on Japanese Patent Application No. 2020-203912, filed December 9, 2020, and Japanese Patent Application No. 2021-066387, filed April 9, 2021, the disclosures of which are incorporated herein in their entireties. [Explanation of symbols]
[0172] 100 motor 1 case 2 rotors 4 Stator 5. Permanent magnets 6. Yoke 7 Teeth 8 slots 9 coils 10 Cooling channel 20, 20A, 20B, 20C, 20D Liner material 21 Coil housing 50 resin layer 51 Inner resin layer 52 Outer resin layer 55 Resin layer surface 55a, 55b ends 65 Resin sealing part 71 Teeth tip 72, 73 Wall 75a Top side 75b Bottom side 100 motor 200 Resin Pipe 201 Power Module 202 Power Semiconductor Chip 203 Sintering layer 204 Cu circuit 205 Heat dissipation sheet 206 Cu base plate 210 1st cooling waterway 220 2nd cooling waterway 211 Inside 212 End
Claims
1. A stator including a stator core having a plurality of teeth, a slot provided between the teeth and accommodating a coil, and a coil accommodated in the slot, A resin layer is provided on an inner surface of the slot and is made of an insulating resin composition, The wall surface of the resin layer on the inside of the slot is provided parallel to the rotation axis direction, The resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120° C. or higher, The thermal conductivity of the resin layer is 0.5 W / (m K) or more, There is no adhesive layer between the coil and the resin layer, a resin liner member that houses the coil, The coil is housed in the slot while being housed in the liner member.
2. The stator according to claim 1 , wherein the resin composition contains a filler as a filler.
3. The stator according to claim 2 , wherein the resin composition has a filler content of 60% by volume or more based on the total volume of the resin composition.
4. A stator including a stator core having a plurality of teeth, a slot provided between the teeth and accommodating a coil, and a coil accommodated in the slot, A resin layer is provided on an inner surface of the slot and is made of an insulating resin composition, The wall surface of the resin layer on the inside of the slot is provided parallel to the rotation axis direction, The resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120° C. or higher, The thermal conductivity of the resin layer is 0.5 W / (m K) or more, The resin composition contains a filler as a filler, The filler content of the resin composition is 60% by volume or more based on the total amount of the resin composition, The filler of the resin composition includes silica, a resin liner member that houses the coil, The coil is housed in the slot while being housed in the liner member.
5. The stator according to claim 1 , wherein the resin composition contains a wax as a release agent.
6. The stator according to claim 1 , wherein the resin layer has a thickness of 50 μm or more and 500 μm or less.
7. 7. The stator according to claim 1, wherein the thermosetting resin is an epoxy resin.
8. The stator according to claim 1 , wherein the coil has a resin coating layer in which a surface of the coil is coated with a resin.
9. A rotating electric motor having a stator described in any one of claims 1 to 8.
10. A method for manufacturing a stator used in a rotating electric machine having a stator core having a plurality of teeth, slots provided between the teeth and receiving coils, and the coils received in the slots, comprising: a resin layer forming step of forming a resin layer made of an insulating resin composition on the inner surface of the slot; a coil placement step of placing the coil in the slot in which the resin layer is provided; having a wall surface of the resin layer on an inner side of the slot is provided parallel to a direction of a rotation axis of the rotating electric machine, The resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120° C. or higher, The thermal conductivity of the resin layer is 0.5 W / (m K) or more, There is no adhesive layer between the coil and the resin layer, a resin liner member that houses the coil, A method for manufacturing a stator, in which the coil is housed in the slot while being housed in the liner member.
11. A method for manufacturing a stator used in a rotating electric machine having a stator core having a plurality of teeth, slots provided between the teeth and receiving coils, and the coils received in the slots, comprising: a resin layer forming step of forming a resin layer made of an insulating resin composition on the inner surface of the slot; a coil placement step of placing the coil in the slot in which the resin layer is provided; having a wall surface of the resin layer on an inner side of the slot is provided parallel to a direction of a rotation axis of the rotating electric machine, The resin composition includes a thermosetting resin, The glass transition temperature Tg of the thermosetting resin is 120° C. or higher, The thermal conductivity of the resin layer is 0.5 W / (m K) or more, The resin composition contains a filler as a filler, The filler content of the resin composition is 60% by volume or more based on the total amount of the resin composition, The filler of the resin composition includes silica, a resin liner member that houses the coil, A method for manufacturing a stator, in which the coil is housed in the slot while being housed in the liner member.
Citation Information
Patent Citations
Rotary machine
JP2003158842A
Electric rotating machine and its manufacturing method
JP2003284277A
Crow-teeth rotating electric machine and manufacturing method of stator
JP2008029142A
Generator stator core with small cap
JP2008503993A
Electric machine with slot liner
JP2015033323A