Electrode assembly, battery cell, battery and power consuming device

The electrode assembly with bent portions and stoppers between bends addresses lithium precipitation and active material shedding, enhancing battery cell safety and performance.

JP7594107B2Active Publication Date: 2024-12-03CONTEMPORARY AMPEREX TECHNOLOGY (HONG KONG) LIMITED
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023528305
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-05-12
Publication Date
2024-12-03
Estimated Expiration
2041-05-12

AI Technical Summary

Technical Problem

The safety issues of battery cells, particularly due to lithium precipitation and active material shedding during bending, are not adequately addressed in existing technologies, leading to reduced performance and increased safety risks.

Method used

An electrode assembly design with bent portions featuring first stops or stoppers positioned between bends to block ion absorption and support the bent regions, reducing lithium precipitation and active material fallout.

Benefits of technology

The proposed design effectively reduces lithium precipitation and enhances the safety performance of battery cells by minimizing ion absorption and active material shedding, thereby improving overall safety and reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007594107000001
    Figure 0007594107000001
  • Figure 0007594107000002
    Figure 0007594107000002
  • Figure 0007594107000003
    Figure 0007594107000003
Patent Text Reader

Abstract

The present application provides an electrode assembly, a battery cell, a battery, and a power consumption device. The electrode assembly of the present application includes a positive electrode plate and a negative electrode plate, the positive electrode plate and the negative electrode plate being wound along a winding direction to form a wound structure, the wound structure including a bent region. The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, at least one bent portion in the positive electrode plate being a first bent portion, and at least one bent portion in the negative electrode plate being a second bent portion adjacent to the first bent portion. The electrode assembly is provided with first stoppers, at least some of which are located between the first bent portion and the second bent portion, and the first stoppers are used to prevent at least some ions released from the first bent portion from being absorbed into the second bent portion. In a first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction. The present application can improve the safety performance of battery cells.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to the field of battery technology, and more particularly to an electrode assembly and a manufacturing method and system thereof, a battery cell, a battery, and a power consuming device. [Background technology]

[0002] Battery cells are widely applied in electronic devices, such as mobile phones, notebook computers, battery cars, electric cars, electric airplanes, electric steamships, electric toy cars, electric toy steamships, electric toy airplanes and power tools, etc. The battery cells may include nickel-cadmium battery cells, nickel-hydride battery cells, lithium-ion battery cells and secondary alkaline zinc-manganese battery cells, etc.

[0003] In the development of battery technology, apart from the improvement of battery cell performance, safety issues are also one of the issues that cannot be ignored. If the safety issues of a battery cell cannot be ensured, the battery cell cannot be used. Therefore, how to reinforce the safety of battery cells is one of the technical issues in battery technology that needs to be solved as soon as possible. Summary of the Invention

[0004] The present application provides an electrode assembly capable of enhancing the safety of a battery cell, a manufacturing method and manufacturing system thereof, a battery cell, a battery, and a power consuming device.

[0005] According to a first aspect, an embodiment of the present application provides an electrode assembly, the electrode assembly including a positive electrode plate and a negative electrode plate, the positive electrode plate and the negative electrode plate being wound along a winding direction to form a wound structure, the wound structure including a bent region. The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion. The electrode assembly includes a first stopper, at least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion. In a first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction.

[0006] In the above solution, the first stopper is installed between the first bent portion and the second bent portion, thereby effectively reducing the lithium precipitation phenomenon. During charging, at least a part of the ions released from the positive electrode active material layer of the first bent portion is blocked by the first stopper, so that the ions blocked by the first stopper cannot be absorbed in the negative electrode active material layer of the second bent portion, thereby reducing the occurrence of lithium precipitation when the negative electrode active material falls off at the second bent portion. The part of the first stopper that protrudes beyond the first bent portion and the second bent portion can play a supporting role, effectively reducing the vibration width of the first bent portion and the second bent portion, reducing the impact force received by the first bent portion and the second bent portion, and reducing the fall off of the active material, thereby reducing the occurrence of lithium precipitation and improving the safety performance of the battery cell.

[0007] In some embodiments, the first bent portion has a first stopper attached thereto. The first stopper can be attached to a surface of the first bent portion in an adhesive manner.

[0008] In some embodiments, the first stopper includes a first base layer and a first adhesive layer, and the first adhesive layer is disposed on a surface of the first base layer facing the first bent portion. The first base layer includes a first body portion and a first support portion connected to the first body portion, and the first adhesive layer is used to bond at least a portion of the first body portion to the first bent portion, and the first support portion protrudes from the first bent portion in a first direction. The first body portion is used to reduce the occurrence of lithium precipitation by blocking at least a portion of ions released from the positive electrode active material layer of the first bent portion. The first support portion performs a supporting function, effectively reducing the vibration amplitude of the first bent portion and the second bent portion, reducing the impact force received by the first bent portion and the second bent portion, and reducing the falling off of the active material, thereby reducing the occurrence of lithium precipitation and improving the safety performance of the battery cell.

[0009] In some embodiments, at least a portion of the surface of the first support facing the first bend is free of the first adhesive layer, and since the first support protrudes beyond the first bend and does not need to be adhered to the first bend, the first adhesive layer on the surface of the first support can be omitted, thus saving material and improving energy density.

[0010] In some embodiments, a first stopper is attached to each of the two surfaces of the first bend portion, the first body portions of the two first stoppers are respectively disposed on both sides of the first bend portion, and none of the first support portions of the two first stoppers has a first adhesive layer disposed thereon.

[0011] In some embodiments, at least a portion of a surface of the first support facing the first flexure portion is provided with a first adhesive layer.

[0012] In some embodiments, the first stoppers are attached to both surfaces of the first bent portion, the first body portions of the two first stoppers are respectively disposed on both sides of the first bent portion, and the first support portions of the two first stoppers are connected by a first adhesive layer. The first support portions of the two first stoppers are connected by the first adhesive layer, so that the two first stoppers are adhered to each other, thereby reducing the risk that the first stoppers fall off the first bent portion and improving the reliability of the first stoppers during the service life of the battery cell.

[0013] In some embodiments, both ends of the first stopper protrude beyond the first bent portion in the first direction. The first stopper performs a supporting function along both ends in the first direction, thereby reducing the vibration amplitude of the first bent portion, reducing the impact force received by the first bent portion, and reducing the falling off of the active material.

[0014] In some embodiments, both ends of the first stopper protrude beyond the second bent portion in the first direction. The first stopper performs a supporting function along both ends in the first direction, thereby reducing the vibration amplitude of the second bent portion, reducing the impact force received by the second bent portion, and reducing the falling off of the active material.

[0015] In some embodiments, the electrode assembly further includes a second stopper, at least a portion of the second stopper being located between the first bent portion and the second bent portion, the first stopper and the second stopper being spaced apart along the first direction, an end of the first stopper remote from the second stopper extending beyond one end of the first bent portion, and an end of the second stopper remote from the first stopper extending beyond the other end of the first bent portion.

[0016] In some embodiments, the electrode assembly further includes a separator for isolating the first plate and the second plate, and both ends of the separator extend beyond the first bent portion and the second bent portion in the first direction. The separator separates the first bent portion and the second bent portion, and can reduce a risk of electrical conduction between the first bent portion and the second bent portion.

[0017] In some embodiments, the porosity of the first stopper is less than the porosity of the separator such that the first stopper can more effectively block the passage of lithium ions.

[0018] In some embodiments, the hardness of the first stopper is greater than the hardness of the separator. The first stopper has a relatively large hardness, can withstand a large impact force, and reduces deformation of the first stopper when the first stopper receives the impact force, thereby effectively reducing the vibration amplitude of the first bent portion and the second bent portion, reducing the impact force received by the first bent portion and the second bent portion, and reducing the falling off of the active material.

[0019] In some embodiments, both ends of the separator extend beyond the first stop in the first direction. In this manner, the first stop increases the energy density of the electrode assembly without increasing the maximum size of the first direction of the electrode assembly.

[0020] In some embodiments, the separator has a first stopper attached to a surface thereof.

[0021] In some embodiments, the wound structure further includes a straight region connected to the bent region, and both ends of the first stopper along the winding direction are located in the bent region, or one end of the first stopper along the winding direction is located in the bent region and the other end of the first stopper along the winding direction is located in the straight region, or both ends of the first stopper along the winding direction are located in the straight region.

[0022] In some embodiments, the positive electrode plate further includes a first flat portion located in the straight region and a positive electrode tab connected to the first flat portion, the first flat portion being connected to the first bent portion, and the positive electrode tab being connected to one end of the first flat portion along the first direction. In the first direction, an end of the first stopper approaching the positive electrode tab protrudes beyond the first bent portion and the second bent portion. The first stopper can reduce the vibration amplitude of the electrode assembly on the positive electrode tab side, thereby reducing the risk of the positive electrode tab being torn.

[0023] In some embodiments, at least one innermost bend in the positive plate is a first bend, and at least one innermost bend in the negative plate is a second bend, and a first stopper is provided between the two innermost bends in the bend region, thus reducing the lithium precipitation phenomenon between the two innermost bends in the bend region and improving safety performance.

[0024] According to a second aspect, an embodiment of the present application provides a battery cell, the battery cell including a housing and an electrode assembly according to any one of the embodiments of the first aspect, the electrode assembly being accommodated within the housing.

[0025] According to a third aspect, an embodiment of the present application provides a battery, the battery including a housing and a battery cell of the second aspect, the battery cell being housed within the housing.

[0026] According to a fourth aspect, an embodiment of the present application provides a power consuming device, said power consuming device including a battery according to the third aspect, the battery being for providing electrical energy.

[0027] According to a fifth aspect, an embodiment of the present application provides a method for manufacturing an electrode assembly, the method including providing a positive electrode plate, a negative electrode plate, and a first stopper, and winding the positive electrode plate and the negative electrode plate along a winding direction to form a wound structure. The wound structure includes a bent region. The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, and at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion. At least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of ions released from the first bent portion from being occluded in the second bent portion. In a first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction.

[0028] According to a sixth aspect, an embodiment of the present application provides a manufacturing system for an electrode assembly, the manufacturing system including a first providing device for providing a positive electrode plate, a second providing device for providing a negative electrode plate, a third providing device for providing a first stopper, and an assembly device for winding the positive electrode plate and the negative electrode plate along a winding direction to form a wound structure. The wound structure includes a bent region. The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, and at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion. At least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion. At least one end of the first stopper protrudes beyond the first bent portion and the second bent portion in the first direction, and the first direction is perpendicular to the winding direction. [Brief description of the drawings]

[0029] In order to more clearly explain the technical solutions of the embodiments of the present application, the following briefly introduces the drawings that need to be used in the embodiments of the present application. It is obvious that the drawings described below are only some embodiments of the present application, and those skilled in the art can also obtain other drawings based on the drawings without exerting creative efforts. [Figure 1] 1 is a structural schematic diagram of a vehicle according to some embodiments of the present application. [Diagram 2] FIG. 2 is a schematic diagram of a battery explosion according to some embodiments of the present application. [Diagram 3] FIG. 3 is a structural schematic diagram of the battery module shown in FIG. 2. [Figure 4] 1 is a schematic diagram of a battery cell explosion according to some embodiments of the present application. [Diagram 5] 1 is a structural schematic diagram of an electrode assembly according to some embodiments of the present application. [Figure 6] 1 is a structural schematic diagram of an electrode assembly according to some further embodiments of the present application. [Figure 7] 1 is a schematic diagram of a local structure of an electrode assembly according to some embodiments of the present application. [Figure 8] FIG. 8 is a cross-sectional schematic view taken along line DD of the electrode assembly shown in FIG. 7. [Figure 9] FIG. 9 is an enlarged schematic view of block F of the electrode assembly shown in FIG. 8. [Figure 10] FIG. 8 is a cross-sectional schematic view of the electrode assembly shown in FIG. 7 taken along line EE. [Figure 11] FIG. 2 is a schematic diagram of the local structure of a positive electrode plate of an electrode assembly according to some embodiments of the present application in an expanded state. [Figure 12] 1 is a schematic cross-sectional view of an electrode assembly according to some further embodiments of the present application. [Figure 13] 11A-11C are schematic local cross-sectional views of electrode assemblies according to further some embodiments of the present application. [Figure 14] 11A-11C are schematic local cross-sectional views of electrode assemblies according to further some embodiments of the present application. [Figure 15]1 is a schematic diagram of a local structure of an electrode assembly according to some further embodiments of the present application. [Figure 16] 13A-13C are schematic topographical diagrams of electrode assemblies according to further some embodiments of the present application. [Figure 17] 1 is a schematic diagram of a local structure of an electrode assembly according to some further embodiments of the present application. [Figure 18] 13A-13C are schematic topographical diagrams of electrode assemblies according to further some embodiments of the present application. [Figure 19] 1 is a flow diagram of a method for manufacturing an electrode assembly according to some embodiments of the present application. [Figure 20] 1 is a schematic block diagram of a manufacturing system for an electrode assembly according to some embodiments of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0030] In order to make the objectives, technical solutions and advantages of the embodiments of the present application clearer, the following will clearly describe the technical solutions in the embodiments of the present application in conjunction with the drawings in the embodiments of the present application, and it is obvious that the described embodiments are only some of the embodiments of the present application, and not all of the embodiments. All other embodiments obtained based on the embodiments of the present application without the need for creative efforts by those skilled in the art are all within the scope of protection of the present application.

[0031] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as commonly understood by those skilled in the art in the technical field of this application, and the terms used in the specification of this application are only for describing specific embodiments and are not intended to limit this application, and the terms "comprise" and "have" and any variations thereof in the specification and claims of this application and the above drawings are intended to cover non-exclusive "comprises". The terms "first", "second", etc. in the specification and claims of this application or the above drawings are not intended to describe a specific order or subordinate relationship, but are intended to distinguish different objects.

[0032] An "embodiment" referred to in this application means that a particular feature, structure, or characteristic described in connection with the embodiment may be included in at least one embodiment of the application. The appearances of this phrase in various places in the specification are not necessarily all referring to the same embodiment, nor are they mutually exclusive separate or alternative embodiments of other embodiments.

[0033] In the description of the present application, it should be explained that unless otherwise clearly defined or limited, the terms "attached", "connected", "connected" and "attached" should be understood in a broad sense, for example, may be a fixed connection, a removable connection, or an integral connection, may be a direct connection, may be an indirect connection through an intermediate medium, or may be communication between the insides of two elements. Those skilled in the art can understand the specific meaning of the above terms in the present application according to the specific situation.

[0034] The term "and / or" in this application merely describes the relationship between related objects and indicates that three relationships may exist, for example, A and / or B may represent three cases: A alone, A and B in combination, and B alone. In addition, the character " / " in this application generally indicates that the related objects before and after are in an "or" relationship.

[0035] In the embodiments of the present application, the same reference numerals represent the same elements, and for the sake of brevity, detailed descriptions of the same elements in different embodiments are omitted. It should be understood that the thickness, length, width, etc. of various elements in the embodiments of the present application shown in the drawings, and the overall thickness, length, width, etc. of the integrated device are illustrative descriptions, and should not be construed as any limitation to the present application.

[0036] The term "plurality" as used herein refers to two or more (including two).

[0037] In the present application, the battery cell may include a lithium ion secondary battery cell, a lithium ion primary battery cell, a lithium sulfur battery cell, a sodium lithium ion battery cell, a sodium ion battery cell, or a magnesium ion battery cell, etc., and the embodiments of the present application are not limited thereto. The battery cell may have a cylindrical shape, a flat shape, a rectangular shape, or other shapes, and the embodiments of the present application are not limited thereto. Generally, the battery cell is divided into three types according to the packaging method, namely, a cylindrical battery cell, a rectangular battery cell, and a pouch battery cell, and the embodiments of the present application are not limited thereto.

[0038] The battery referred to in the embodiments of the present application refers to a single physical module that includes one or more battery cells to provide higher voltage and capacity. For example, the battery referred to in the present application may include a battery module or a battery pack. The battery generally includes a housing for packaging one or more battery cells. The housing can prevent liquid or other foreign matter from affecting the charging or discharging of the battery cells.

[0039] The battery cell includes an electrode assembly and an electrolyte, and the electrode assembly includes a positive electrode plate, a negative electrode plate, and a separator. The battery cell is operated mainly by the movement of metal ions between the positive electrode plate and the negative electrode plate. The positive electrode plate includes a positive electrode collector and a positive electrode active material layer, and the positive electrode active material layer is coated on the surface of the positive electrode collector. The positive electrode collector includes a positive electrode collector part and a positive electrode protrusion protruding from the positive electrode collector part, and the positive electrode collector part is coated with the positive electrode active material layer, and at least a part of the positive electrode protrusion is not coated with the positive electrode active material layer, and the positive electrode protrusion is a positive electrode tab. Taking a lithium ion battery as an example, the material of the positive electrode collector may be aluminum, the positive electrode active material layer includes a positive electrode active material, and the positive electrode active material may be lithium cobalt oxide, lithium iron phosphate, ternary lithium, or lithium manganate, etc. The negative electrode plate includes a negative electrode collector and a negative electrode active material layer, and the negative electrode active material layer is coated on the surface of the negative electrode collector. The negative electrode collector includes a negative electrode collector and a negative electrode protrusion protruding from the negative electrode collector. The negative electrode collector is coated with the negative electrode active material layer, and at least a part of the negative electrode protrusion is not coated with the negative electrode active material layer, and the negative electrode protrusion is a negative electrode tab. The material of the negative electrode collector may be copper, and the negative electrode active material layer includes a negative electrode active material, and the negative electrode active material may be carbon or silicon, etc. In order to ensure that the positive electrode tabs do not melt even when a large current is applied, the number of positive electrode tabs is multiple and they are stacked, and the number of negative electrode tabs is multiple and they are stacked. The material of the separator may be PP (polypropylene) or PE (polyethylene), etc. In addition, the electrode assembly may have a wound type structure or a laminated type structure, and the embodiment of the present application is not limited thereto.

[0040] In a lithium-ion battery cell, when charging, lithium ions are released from the positive electrode active material layer and absorbed in the negative electrode active material layer, but some abnormalities may occur, such as when the lithium absorption space in the negative electrode active material layer is insufficient, the resistance of the lithium ions to be absorbed in the negative electrode active material layer is too large, or the lithium ions are released from the positive electrode active material layer too quickly, so that the released lithium ions cannot be absorbed in the negative electrode active material layer of the negative electrode plate in equal amounts, and the lithium ions that cannot be absorbed in the negative electrode plate can only obtain electrons on the surface of the negative electrode plate, thereby forming metallic lithium elements, which is the lithium precipitation phenomenon. Lithium precipitation not only reduces the performance of the lithium-ion battery cell and significantly shortens the cycle life, but also limits the high-speed charging capacity of the lithium-ion battery cell. In addition, when lithium precipitation occurs in a lithium-ion battery cell, the precipitated lithium metal is very active and can react with the electrolyte at low temperatures, resulting in a decrease in the self-heating start temperature of the battery cell and an increase in the self-heating rate, which seriously harms the safety of the battery cell. In addition, if the lithium deposition is serious, the released lithium ions can form lithium crystals on the surface of the negative electrode plate. The lithium crystals are likely to destroy the separator, and there is a risk of short-circuiting the adjacent positive and negative electrodes.

[0041] In the course of research and development, the inventors found that when the electrode assembly is subjected to vibration or extrusion, the active material of the positive electrode plate or the active material of the negative electrode plate falls off, which is called the powder falling phenomenon. Due to the falling off of the active material, especially the falling off of the active material on the negative electrode plate, the number of lithium absorption sites in the negative electrode active material layer of this negative electrode plate becomes less than the number of lithium ions that can be provided by the positive electrode active material layer of the adjacent positive electrode plate, so that the lithium ion battery cell is prone to the lithium deposition phenomenon during charging.

[0042] In the course of research and development, the inventors further found that the lithium deposition phenomenon is more likely to occur in the bending region of a wound electrode assembly, and as a result of further investigation, the inventors found that the cause of this lithium deposition phenomenon is that the positive electrode plate and the negative electrode plate, which are mainly located in the bending region, need to be bent, but the positive electrode active material layer and the negative electrode active material layer are prone to stress concentration during the bending process, and the active materials of each are prone to fall off. Falling off of the active material, particularly the active material on the negative electrode plate, can cause the lithium absorption sites of the negative electrode active material layer of this negative electrode plate to be fewer than the number of lithium ions that can be provided by the positive electrode active material layer of the adjacent positive electrode plate, which can cause the lithium deposition phenomenon.

[0043] In view of this, the embodiment of the present application provides a technical solution, in which the electrode assembly includes a positive electrode plate and a negative electrode plate, the positive electrode plate and the negative electrode plate are wound along a winding direction to form a wound structure, and the wound structure includes a bent region. The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, and at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion. The electrode assembly is provided with a first stopper, and at least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being absorbed into the second bent portion. In the first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction. A battery cell having such a structure can reduce lithium deposition and reduce safety risks.

[0044] The technical solutions described in the embodiments of the present application are applicable to batteries and power consuming devices that use batteries.

[0045] The power consumption device may be a vehicle, a mobile phone, a portable device, a notebook computer, a steamship, a spacecraft, an electric toy and an electric tool, etc. The vehicle may be a fuel oil vehicle, a gas vehicle or a new energy vehicle, the new energy vehicle may be a pure electric vehicle, a hybrid vehicle or a range extender vehicle, etc., the spacecraft includes an airplane, a rocket, a space shuttle and a spaceship, etc., the electric toy includes a stationary or mobile electric toy, such as a game console, an electric car toy, an electric steamship toy and an electric airplane toy, etc., and the electric tool includes a metal cutting electric tool, a polishing electric tool, an assembly electric tool and a railway electric tool, such as an electric drill, an electric grinder, an electric wrench, an electric screwdriver, an electric hammer, a hammer drill, a concrete vibrator and an electric planer, etc. The embodiment of the present application does not particularly limit the above power consumption device.

[0046] In the following embodiment, for convenience of explanation, the power consuming device is a vehicle.

[0047] 1 is a structural schematic diagram of a vehicle according to some embodiments of the present application. As shown in FIG. 1, a battery 2 is installed inside the vehicle 1, and the battery 2 may be installed at the bottom, head, or tail of the vehicle 1. The battery 2 may be used to supply power to the vehicle 1, for example, the battery 2 may be an operating power source for the vehicle 1.

[0048] The vehicle 1 may further include a controller 3 and a motor 4, where the controller 3 is used to control the battery 2 to power the motor 4, for example for start-up, navigation and operating power consumption needs of the vehicle 1 during driving.

[0049] In some embodiments of the present application, the battery 2 can be used not only as an operating power source for the vehicle 1, but also as a drive power source for the vehicle 1, providing drive power to the vehicle 1 in place of, or in place of, gasoline or natural gas.

[0050] 2 is a schematic diagram of an explosion of a battery according to some embodiments of the present application. As shown in FIG. 2, the battery 2 includes a housing 5 and a battery cell (not shown in FIG. 2), and the battery cell is housed in the housing 5.

[0051] The housing 5 is used to house the battery cells, and the housing 5 may have various structures. In some embodiments, the housing 5 may include a first housing portion 51 and a second housing portion 52, and the first housing portion 51 and the second housing portion 52 are placed over each other, and the first housing portion 51 and the second housing portion 52 together define a housing space 53 for housing the battery cells. The second housing portion 52 may have a hollow structure with an opening at one end, and the first housing portion 51 has a plate-like structure, and the first housing portion 51 is placed over the opening side of the second housing portion 52 to form the housing 5 having the housing space 53, and the first housing portion 51 and the second housing portion 52 may both have a hollow structure with an opening at one end, and the opening side of the first housing portion 51 is placed over the opening side of the second housing portion 52 to form the housing 5 having the housing space 53. Of course, the first housing part 51 and the second housing part 52 may have various shapes, for example, a cylinder, a rectangular parallelepiped, and the like.

[0052] In order to improve the sealing property after the first housing part 51 and the second housing part 52 are connected, a sealing material, such as a sealing rubber or a sealing ring, may be provided between the first housing part 51 and the second housing part 52.

[0053] If the first housing part 51 is placed on top of the second housing part 52, the first housing part 51 may be referred to as an upper housing cover, and the second housing part 52 may be referred to as a lower housing.

[0054] The battery 2 may have one or more battery cells. When there are multiple battery cells, the multiple battery cells may be connected in series, in parallel, or in series-parallel, and series-parallel connection means that the multiple battery cells are connected in series and in parallel. The multiple battery cells may be directly connected in series, in parallel, or in series-parallel, and then the entire battery cell assembly may be housed in the housing 5. Alternatively, the multiple battery cells may first be connected in series, in parallel, or in series-parallel to form a battery module 6, and the multiple battery modules 6 may then be connected in series, in parallel, or in series-parallel to form a whole battery module, which is then housed in the housing 5.

[0055] Fig. 3 is a structural schematic diagram of the battery module shown in Fig. 2. As shown in Fig. 3, in some embodiments, a plurality of battery cells 7 are provided, and the plurality of battery cells 7 are first connected in series, in parallel, or in series-parallel to form a battery module 6. Further, the plurality of battery modules 6 are connected in series, in parallel, or in series-parallel to form a whole, which is then housed in a housing.

[0056] The multiple battery cells 7 in the battery module 6 may be electrically connected to each other by bus bar components, thereby realizing parallel connection, series connection, or series-parallel connection of the multiple battery cells 7 in the battery module 6.

[0057] 4 is a schematic diagram of an explosion of a battery cell according to some embodiments of the present application. As shown in FIG. 4, a battery cell 7 according to an embodiment of the present application includes an electrode assembly 10 and a housing 20, and the electrode assembly 10 is housed in the housing 20.

[0058] In some embodiments, the housing 20 may further be used to house an electrolyte, such as an electrolyte solution. The housing 20 may be of various construction types.

[0059] In some embodiments, the housing 20 may include a case 21 and an end cap 22, where the case 21 is a hollow structure with an opening on one side, and the end cap 22 fits over the opening of the case 21 to form a sealed connection, thereby forming a sealed space for containing the electrode assembly 10 and the electrolyte.

[0060] The case 21 may have various shapes, for example, a cylinder, a rectangular parallelepiped, etc. The shape of the case 21 may be determined based on the specific shape of the electrode assembly 10. For example, if the electrode assembly 10 has a cylindrical structure, a cylindrical case may be selected, and if the electrode assembly 10 has a rectangular parallelepiped structure, a rectangular parallelepiped case may be selected. Of course, the end cap 22 may have various structures, for example, the end cap 22 may have a plate-like structure, a hollow structure with one end open, etc. Exemplarily, in FIG. 4, the case 21 has a rectangular parallelepiped structure, the end cap 22 has a plate-like structure, and the end cap 22 is placed over the opening at the top of the case 21.

[0061] In some embodiments, the battery cell 7 may further include a positive electrode terminal 30, a negative electrode terminal 40, and a pressure relief mechanism 50, where the positive electrode terminal 30, the negative electrode terminal 40, and the pressure relief mechanism 50 are all attached to the end cap 22. The positive electrode terminal 30 and the negative electrode terminal 40 are all used to electrically connect with the electrode assembly 10 to output the electric energy generated by the electrode assembly 10. The pressure relief mechanism 50 is used to release the pressure inside the battery cell 7 when the internal pressure or temperature of the battery cell 7 reaches a predetermined value.

[0062] Exemplarily, the pressure relief mechanism 50 is located between the positive electrode terminal 30 and the negative electrode terminal 40, and the pressure relief mechanism 50 may be, for example, a component such as an explosion-proof valve, an explosion-proof piece, an air valve, a pressure relief valve, or a safety valve, but is not limited thereto.

[0063] Of course, in some other embodiments, the housing 20 may have other structures, for example, the housing 20 includes a case 21 and two end caps 22, the case 21 is a hollow structure with openings on both opposing sides, and one end cap 22 is fitted over one opening of the case 21 to form a sealed connection, thereby forming a sealed space for accommodating the electrode assembly 10 and the electrolyte. In such a structure, the positive electrode terminal 30 and the negative electrode terminal 40 may be attached to the same end cap 22 or different end caps 22, and the pressure relief mechanism 50 may be attached to one end cap 22 or both end caps 22.

[0064] It should be noted that the battery cell 7 may have one or more electrode assemblies 10 housed in the housing 20. Exemplarily, in FIG. 4, there are two electrode assemblies 10.

[0065] FIG. 5 is a structural schematic diagram of an electrode assembly according to some embodiments of the present application.

[0066] As shown in FIG. 5, an electrode assembly 10 of an embodiment of the present application includes a positive electrode plate 11 and a negative electrode plate 12, and the positive electrode plate 11 and the negative electrode plate 12 are wound along a winding direction A to form a wound structure.

[0067] In the embodiment of the present application, the winding direction A is the direction in which the positive electrode plate 11 and the negative electrode plate 12 are wound circumferentially from the inside to the outside. In Fig. 5, the winding direction A is the clockwise direction.

[0068] In some embodiments, the electrode assembly 10 further includes a separator 13, which is used to isolate the positive electrode plate 11 from the negative electrode plate 12 to reduce the risk of short circuit between the positive electrode plate 11 and the negative electrode plate 12. The separator 13 has a large number of penetrating micropores, which can ensure the free passage of electrolyte ions, and has good permeability to lithium ions, so that the separator 13 can hardly block the passage of lithium ions. Exemplarily, the material of the separator 13 may be PP (polypropylene) or PE (polyethylene), etc.

[0069] The positive electrode plate 11, the negative electrode plate 12 and the separator 13 all have a strip-like structure. In the embodiment of the present application, the positive electrode plate 11, the separator 13 and the negative electrode plate 12 may be first stacked in order and then wound two or more times to form the electrode assembly 10.

[0070] The electrode assembly 10 may have a variety of shapes, for example, the electrode assembly 10 may be a cylinder, a flattened body, a prismatic body (eg, a triangular, square or hexagonal prism), or other shape.

[0071] In some embodiments, the wound structure includes a bent region B. Both the positive electrode plate 11 and the negative electrode plate 12 include a plurality of bent portions 14 located in the bent region B. The bent region B is a region having a bent structure of the electrode assembly 10, and the portion of the positive electrode plate 11 located in the bent region B (i.e., the bent portion 14 of the positive electrode plate 11) and the portion of the negative electrode plate 12 located in the bent region B (i.e., the bent portion 14 of the negative electrode plate 12) are both bent. Exemplarily, the bent portion 14 of the positive electrode plate 11 and the bent portion 14 of the negative electrode plate 12 are bent into a substantially arc shape.

[0072] Exemplarily, in the bending region B, the bent portions 14 of the positive electrode plate 11 and the bent portions 14 of the negative electrode plate 12 are arranged alternately, that is, in the bending region B, one bent portion 14 of the negative electrode plate 12, one bent portion 14 of the positive electrode plate 11, one bent portion 14 of the negative electrode plate 12, ... are arranged in this order. Optionally, the innermost bent portion 14 of the positive electrode plate 11 is located outside the innermost bent portion 14 of the negative electrode plate 12.

[0073] In some embodiments, the electrode assembly 10 has a flat body. Exemplarily, the wound structure further includes a straight region C connected to the bent region B. Both the positive electrode plate 11 and the negative electrode plate 12 include a plurality of flat portions 15 located in the straight region C. The straight region C is a region having a flat structure of the electrode assembly 10, and optionally, the bent region B is two and is connected to both ends of the straight region C, respectively.

[0074] A portion of the positive electrode plate 11 located in the straight region C (i.e., the flat portion 15 of the positive electrode plate 11) and a portion of the negative electrode plate 12 located in the straight region C (i.e., the flat portion 15 of the negative electrode plate 12) are disposed substantially flat. The surfaces of the flat portion 15 of the positive electrode plate 11 and the flat portion 15 of the negative electrode plate 12 are both substantially flat.

[0075] FIG. 6 is a structural schematic diagram of an electrode assembly according to some further embodiments of the present application.

[0076] 6, in some embodiments, the electrode assembly 10 is substantially cylindrical. Illustratively, the wound structure may have only the bent region B and no straight region. In the positive electrode plate 11, one turn of the positive electrode plate 11 is one bent portion 14, and in the negative electrode plate 12, one turn of the negative electrode plate 12 is one bent portion 14.

[0077] FIG. 7 is a schematic diagram of a local structure of an electrode assembly according to some embodiments of the present application, FIG. 8 is a schematic diagram of a cross section taken along line DD of the electrode assembly shown in FIG. 7, FIG. 9 is an enlarged schematic diagram of block F of the electrode assembly shown in FIG. 8, FIG. 10 is a schematic diagram of a cross section taken along line EE of the electrode assembly shown in FIG. 7, and FIG. 11 is a schematic diagram of a local structure of a positive electrode plate of the electrode assembly according to some embodiments of the present application in an expanded state.

[0078] 7 to 11, the positive electrode plate 11 includes a positive electrode collector 111 and a positive electrode coating 112 coated on the surface of the positive electrode collector 111, the positive electrode collector 111 includes a positive electrode collector portion 111a and a positive electrode tab 111b protruding from the positive electrode collector portion 111a, the positive electrode coating 112 includes a positive electrode active material layer 112a, two surfaces of the positive electrode collector portion 111a are coated with the positive electrode active material layer 112a, and at least a part of the positive electrode tab 111b is not coated with the positive electrode active material layer 112a. The part of the positive electrode tab 111b that is not coated with the positive electrode active material layer 112a is used for electrical connection to an electrode terminal.

[0079] In some embodiments, the positive electrode current collector 111a is coated with the positive electrode active material layer 112a only in a part of the area, and the positive electrode tab 111b is not coated with the positive electrode active material layer 112a. The positive electrode coating 112 further includes an insulating layer 112b, which is located on the side of the positive electrode active material layer 112a that is closer to the positive electrode tab 111b, and the insulating layer 112b is coated on the area of ​​the positive electrode current collector 111a that is not coated with the positive electrode active material layer 112a. For example, the insulating layer 112b is also coated on the root part of the positive electrode tab 111b that is closer to the positive electrode current collector 111a.

[0080] At the bent portion of the positive electrode plate 11, both ends of the positive electrode coating 112 along the first direction X are flush with both ends of the positive electrode current collecting portion 111a along the first direction X. The first direction X is perpendicular to the winding direction A.

[0081] In some embodiments, the positive electrode tab 111b is connected to one end of the flat portion along the first direction X and protrudes from the flat portion. In the first direction X, both ends of the flat portion of the positive electrode plate 11 are flush with both ends of the bent portion of the positive electrode plate 11. In the positive electrode plate 11, the positive electrode tab 111b may be connected to some of the flat portions, or the positive electrode tab 111b may be connected to all of the flat portions. Exemplarily, the positive electrode tabs 111b are multiple and are stacked.

[0082] The negative electrode plate 12 includes a negative electrode current collector 121 and a negative electrode coating applied to the surface of the negative electrode current collector 121, the negative electrode current collector 121 includes a negative electrode current collector and a negative electrode tab protruding from the negative electrode current collector, the negative electrode coating includes a negative electrode active material layer 122, two surfaces of the negative electrode current collector are coated with the negative electrode active material layer 122, and at least a portion of the negative electrode tab is not coated with the negative electrode active material layer 122. The portion of the negative electrode tab that is not coated with the negative electrode active material layer 122 is used for electrical connection to an electrode terminal.

[0083] At the bent portion of the negative electrode plate 12, both ends of the negative electrode active material layer 122 along the first direction X are flush with both ends of the negative electrode current collecting portion along the first direction X.

[0084] In the first direction X, both ends of the negative electrode active material layer 122 protrude beyond the positive electrode active material layer 112a. The first direction X is perpendicular to the winding direction A. In the first direction X, one end of the positive electrode active material layer 112a is located inside one end of the negative electrode active material layer 122, and the other end of the positive electrode active material layer 112a is located inside the other end of the negative electrode active material layer 122. In this way, the negative electrode active material layer 122 covers the positive electrode active material layer 112a and provides more lithium absorption sites for the lithium ions released from the positive electrode active material layer 112a, thereby reducing the risk of lithium precipitation.

[0085] In some embodiments, at least one bent portion in the positive electrode plate 11 is a first bent portion 14a, and at least one bent portion in the negative electrode plate 12 is a second bent portion 14b adjacent to the first bent portion 14a. The electrode assembly 10 is provided with a first stopper 16, and at least a portion of the first stopper 16 is located between the first bent portion 14a and the second bent portion 14b, and the first stopper 16 is used to prevent at least a portion of the ions released from the first bent portion 14a from being occluded in the second bent portion 14b. At least one end of the first stopper 16 protrudes from the first bent portion 14a and the second bent portion 14b in the first direction X.

[0086] In the first direction X, one end of the first stopper 16 protrudes beyond the first bent portion 14a and the second bent portion 14b, while the other end of the first stopper 16 may protrude beyond the first bent portion 14a, may not protrude beyond the first bent portion 14a, may protrude beyond the second bent portion 14b, or may not protrude beyond the second bent portion 14b.

[0087] In the positive electrode plate 11, the first bent portion 14a may be one or more. In the positive electrode plate 11, all the bent portions may be the first bent portion 14a, or some of the bent portions may be the first bent portion 14a. For example, some of the bent portions in the positive electrode plate 11 are the first bent portion 14a, and other some of the bent portions are the third bent portions, and a first stopper 16 is provided between the first bent portion 14a and the second bent portion 14b, but no first stopper 16 is provided between the third bent portion and the bent portions of the adjacent negative electrode plates 12 on both sides.

[0088] In the negative electrode plate 12, the second bent portion 14b may be one or more. In the negative electrode plate 12, all the bent portions may be the second bent portion 14b, or some of the bent portions may be the second bent portion 14b. For example, some of the bent portions in the negative electrode plate 12 are the second bent portion 14b, and other some of the bent portions are the fourth bent portion, and a first stopper 16 is provided between the second bent portion 14b and the first bent portion 14a, but no first stopper 16 is provided between the fourth bent portion and the bent portions of the adjacent positive electrode plates 11 on both sides.

[0089] The number of first stoppers 16 between the first bent portion 14a and the second bent portion 14b may be one or more. Only the first stopper 16 may be provided between the first bent portion 14a and the second bent portion 14b, or other stoppers, such as a second stopper and a third stopper, may be provided at the same time.

[0090] The first stopper 16 may be entirely located in the curved region B, or only a portion of the first stopper 16 may be located in the curved region B. For example, in the case of an electrode assembly including a straight region C, the first stopper 16 may be entirely located in the curved region B, or a portion of the first stopper 16 may be located in the curved region B and another portion of the first stopper 16 may be located in the straight region C.

[0091] The first stopper 16 may be installed independently on the positive electrode plate 11 and the negative electrode plate 12, or may be attached to any surface of the positive electrode plate 11, any surface of the negative electrode plate 12, or any surface of the separator 13. The first stopper 16 being installed independently on the positive electrode plate 11 and the negative electrode plate 12 means that the first stopper 16 is separably stacked on the positive electrode plate 11 and the negative electrode plate 12, respectively, that is, does not have an adhesive or coating relationship. Attachment means that the first stopper 16 is connected by a method such as adhesion, coating, or spray coating.

[0092] In the second bent portion, stress concentration may occur during the bending process, which may cause the negative electrode active material to fall off, and the falling off of the negative electrode active material may cause the number of lithium absorption sites in the negative electrode active material layer in the second bent portion to be less than the number of lithium ions provided by the positive electrode active material layer in the first bent portion, which may cause lithium precipitation. If the battery cell is subject to vibration or extrusion during use, the negative electrode active material layer in the second bent portion will be in a bent state, and if the negative electrode active material layer in the second bent portion is subjected to vibration or extrusion, the falling off of the negative electrode active material is more likely to occur.

[0093] In the embodiment of the present application, the lithium deposition phenomenon can be effectively reduced by providing the first stopper 16 between the first bent portion 14a and the second bent portion 14b. During charging, at least a part of the ions released from the positive electrode active material layer 112a of the first bent portion 14a is blocked by the first stopper 16, so that the ions blocked by the first stopper 16 cannot be absorbed in the negative electrode active material layer 122 of the second bent portion 14b, and thus, when the negative electrode active material falls off in the second bent portion 14b, the occurrence of lithium deposition is reduced. In other words, the lithium absorption sites in the second bent portion 14b are reduced due to the fall off of the negative electrode active material, but the occurrence of lithium deposition is reduced by blocking at least a part of the ions released from the positive electrode active material layer 112a of the first bent portion 14a by the first stopper 16.

[0094] In the embodiment of the present application, at least one end of first stopper 16 in first direction X protrudes beyond first bent portion 14a and second bent portion 14b, but the portion of first stopper 16 protruding beyond first bent portion 14a and second bent portion 14b can perform a supporting function, effectively reducing the vibration amplitude of first bent portion 14a and second bent portion 14b, reducing the impact force received by first bent portion 14a and second bent portion 14b, and reducing the falling-off of active material, thereby reducing the occurrence of lithium precipitation and improving the safety performance of the battery cell.

[0095] In the embodiment of the present application, the first stopper 16 can reduce the loss of the positive electrode active material at the first bent portion 14a and the loss of the negative electrode active material at the second bent portion 14b, and can also block at least a portion of the ions released from the positive electrode active material layer 112a at the first bent portion 14a, thereby reducing the occurrence of lithium precipitation and improving the safety performance of the battery cell.

[0096] In some embodiments, both ends of the first stopper 16 protrude beyond the first bent portion 14a in the first direction X.

[0097] One end of the first stopper 16 in the first direction X is located outside of one end of the first bent portion 14a in the first direction X, and the other end of the first stopper 16 in the first direction X is located outside of the other end of the first bent portion 14a in the first direction X.

[0098] In the first direction X, one end of the first stopper 16 protrudes beyond the second bent portion 14b, and the other end of the first stopper 16 may or may not protrude beyond the second bent portion 14b.

[0099] In this embodiment, both ends of the first stopper 16 along the first direction X perform a supporting function, thereby making it possible to reduce the vibration amplitude of the first bent portion 14a, reduce the impact force received by the first bent portion 14a, and reduce the falling off of the active material.

[0100] In some embodiments, both ends of the first stopper 16 protrude beyond the second bent portion 14b in the first direction X.

[0101] One end of the first stopper 16 in the first direction X is located outside of one end of the second bent portion 14b in the first direction X, and the other end of the first stopper 16 in the first direction X is located outside of the other end of the second bent portion 14b in the first direction X.

[0102] In this embodiment, both ends of the first stopper 16 along the first direction X perform a supporting function, reduce the vibration amplitude of the second bent portion 14 b, reduce the impact force received by the second bent portion 14 b, and reduce the falling off of the active material, thereby reducing the occurrence of lithium precipitation and improving the safety performance of the battery cell.

[0103] In some embodiments, at least one innermost bent portion of the positive electrode plate 11 is the first bent portion 14a, and at least one innermost bent portion of the negative electrode plate 12 is the second bent portion 14b. In other words, the first stopper 16 is provided between the two innermost bent portions of the bent region B.

[0104] The degree of bending of the innermost one of the bent portions of the positive electrode plate 11 is the largest, i.e., the phenomenon of the positive electrode active material falling off at the innermost one of the bent portions of the positive electrode plate 11 is the most serious, and the degree of bending of the innermost one of the bent portions of the negative electrode plate 12 is the largest, i.e., the phenomenon of the negative electrode active material falling off at the innermost one of the bent portions of the negative electrode plate 12 is the most serious. In the embodiment of the present application, at least the innermost one of the bent portions of the positive electrode plate 11 is set as the first bent portion 14a, and at least the innermost one of the bent portions of the negative electrode plate 12 is set as the second bent portion 14b, thus reducing the lithium deposition phenomenon between the two innermost bent portions of the bent region B and improving safety performance.

[0105] In some embodiments, the two or more bent portions of the negative electrode plate 12 extending from the inside to the outside are first bent portions 14a, and the two or more bent portions of the positive electrode plate 11 extending from the inside to the outside are second bent portions 14b. The first bent portions 14a and the second bent portions 14b are alternately arranged from the inside to the outside. A first stopper 16 is provided between the adjacent first bent portions 14a and second bent portions 14b.

[0106] In some embodiments, both ends of the first stopper 16 along the winding direction A are located in the curved region B, and, for example, both ends of the first stopper 16 along the winding direction A are located at the boundary between the curved region B and the straight region C, or both ends of the first stopper 16 along the winding direction A approach the boundary between the curved region B and the straight region C. In other embodiments, one end of the first stopper 16 along the winding direction A is located in the curved region B, and the other end of the first stopper 16 along the winding direction A is located in the straight region C. In still further embodiments, both ends of the first stopper 16 along the winding direction A are located in the straight region C.

[0107] In some embodiments, the positive electrode plate 11 further includes a first flat portion 15a located in the straight region C and a positive electrode tab 111b connected to the first flat portion 15a, the first flat portion 15a being connected to the first bent portion 14a, and the positive electrode tab 111b being connected to one end of the first flat portion 15a along the first direction X. In the first direction X, an end of the first stopper 16 approaching the positive electrode tab 111b protrudes beyond the first bent portion 14a and the second bent portion 14b.

[0108] Both ends of the first flat portion 15a along the first direction X are flush with both ends of the first bent portion 14a along the first direction X, and the positive electrode tab 111b protrudes from the first flat portion 15a.

[0109] When the electrode assembly 10 vibrates, the positive electrode tab 111b may be easily torn because it is thin, which affects the discharge capacity. Since the end of the first stopper 16 approaching the positive electrode tab 111b protrudes beyond the first bent portion 14a and the second bent portion 14b, the first stopper 16 can reduce the vibration amplitude of the electrode assembly 10 on the positive electrode tab 111b side, thereby reducing the risk of the positive electrode tab 111b being torn.

[0110] In some embodiments, the electrode assembly 10 further includes a separator 13 for isolating the first electrode plate 11 and the second electrode plate 12, and both ends of the separator 13 extend beyond the first bent portion 14a and the second bent portion 14b in the first direction X.

[0111] One end of separator 13 in the first direction X is located outside one end of first bent portion 14a in the first direction X and outside one end of second bent portion 14b in the first direction X, and the other end of separator 13 in the first direction X is located outside the other end of first bent portion 14a in the first direction X and outside the other end of second bent portion 14b in the first direction X.

[0112] In this embodiment, the separator 13 separates the first bent portion 14a and the second bent portion 14b, thereby reducing the risk of electrical conduction between the first bent portion 14a and the second bent portion 14b, and improving safety performance.

[0113] In some embodiments, the porosity of the first stopper 16 is less than the porosity of the separator 13 .

[0114] In the embodiment of the present application, the porosity of the first stopper 16 is smaller than that of the separator 13, so that the first stopper 16 can effectively block the passage of lithium ions. The porosity is the percentage of the void volume of a bulk material to the total volume of the material in its natural state. Generally, the test method for the porosity is the true density test method.

[0115] Illustratively, the porosity of the first stopper 16 is 10%-70%, alternatively, the porosity of the first stopper 16 is 20%-60%.

[0116] In some embodiments, the hardness of the first stopper 16 is greater than the hardness of the separator 13 .

[0117] The first stopper 16 has a relatively large hardness, can withstand a large impact force, and reduces deformation of the first stopper 16 when the first stopper 16 receives an impact force, thereby effectively reducing the vibration amplitude of the first bent portion 14a and the second bent portion 14b, reducing the impact force received by the first bent portion 14a and the second bent portion 14b, and reducing the falling off of the active material. For example, the Shore hardness of the first stopper 16 is larger than the Shore hardness of the separator 13.

[0118] The first stopper 16 has a relatively large hardness and supports the separator 13, and can also reduce the risk that the end of the separator 13 will be folded back between the first bent portion 14a and the second bent portion 14b.

[0119] In the first direction X, one end of the separator 13 may or may not protrude beyond the first stopper 16, and the other end of the separator 13 may or may not protrude beyond the first stopper 16.

[0120] In some embodiments, both ends of the separator 13 extend beyond the first stopper 16 in the first direction X.

[0121] One end of the separator 13 in the first direction X is located outside one end of the first stopper 16 in the first direction X, and the other end of the separator 13 in the first direction X is located outside the other end of the first stopper 16 in the first direction X.

[0122] In this embodiment, the first stopper 16 improves the energy density of the electrode assembly 10 without increasing the maximum size of the electrode assembly 10 in the first direction X.

[0123] In some embodiments, the surface of separator 13 is provided with a first stopper.

[0124] In some embodiments, the first bent portion 14a is provided with a first stopper 16. Exemplarily, the first stopper 16 can be attached to the surface of the first bent portion 14a in an adhesive manner.

[0125] In some embodiments, the material of the first stopper 16 includes at least one of an inorganic oxide and a polymer. Exemplarily, the inorganic oxide may be at least one of magnesium oxide (MgO), calcium oxide (CaO), boehmite, wollastonite, barium sulfate (BaSO4), calcium sulfate (CaSO4), calcium carbonate (CaCO3), aluminum oxide (Al2O3), and silicon dioxide (SiO2), and the polymer may be at least one of polypropylene, polychloroethylene, polyethylene, epoxy resin, polyacrylate, and polyurethane rubber.

[0126] In some other embodiments, the first stopper 16 includes a first base layer 161 and a first adhesive layer 162, and the first adhesive layer 162 is disposed on a surface of the first base layer 161 facing the first bending portion 14a. The first base layer 161 includes a first body portion 161a and a first support portion 161b connected to the first body portion 161a, and the first adhesive layer 162 is used to adhere at least a portion of the first body portion 161a to the first bending portion 14a, and the first support portion 161b protrudes in the first direction X beyond the first bending portion 14a.

[0127] The material of the first base layer 161 includes polyethylene and / or ethylene-vinyl acetate copolymer (EVA).

[0128] The first main body portion 161a is a portion of the first base layer 161 that overlaps with the first bent portion 14a in the thickness direction of the first bent portion 14a. Accordingly, the first support portion 161b does not overlap with the first bent portion 14a in the thickness direction of the first bent portion 14a. The first main body portion 161a is used to reduce the occurrence of lithium deposition by blocking at least a portion of the ions released from the positive electrode active material layer 112a of the first bent portion 14a. The first support portion 161b performs a supporting function, effectively reduces the vibration amplitude of the first bent portion 14a and the second bent portion 14b, reduces the impact force received by the first bent portion 14a and the second bent portion 14b, and reduces the falling off of the active material, thereby reducing the occurrence of lithium deposition and improving the safety performance of the battery cell.

[0129] In some embodiments, the entire first body portion 161a is adhered to the first bend portion 14a by the first adhesive layer 162. In other embodiments, a portion of the first body portion 161a is adhered to the first bend portion 14a by the first adhesive layer 162, and a portion of the first body portion 161a does not have the first adhesive layer 162 and is not adhered to the first bend portion 14a.

[0130] In some embodiments, the first adhesive layer 162 is not provided on at least a portion of the surface of the first support 161b facing the first bent portion 14a. The first support 161b protrudes from the first bent portion 14a and does not need to be adhered to the first bent portion 14a, so the first adhesive layer 162 on the surface of the first support 161b can be omitted, thus saving material and improving energy density. In addition, in this embodiment, the possibility that the first support 161b is adhered to the separator 13 can be reduced, and the risk of wrinkles occurring in the separator 13 due to the influence of the first support 161b can also be reduced.

[0131] FIG. 12 is a schematic cross-sectional view of an electrode assembly according to some further embodiments of the present application.

[0132] 12, in some embodiments, the first stoppers 16 are attached to both surfaces of the first bent portion 14a. Exemplarily, at least two first stoppers 16 are attached to the first bent portion 14a, and the first body portions 161a of the two first stoppers 16 are respectively installed on both sides of the first bent portion 14a, and none of the first adhesive layers 162 are installed on the first support portions 161b of the two first stoppers 16. The first body portions 161a of the two first stoppers 16 are respectively bonded to the two surfaces of the first bent portion 14a.

[0133] The first main body portions 161a of the two first stoppers 16 are used to block at least some of the ions released from the positive electrode active material layers 112a on both sides of the first bent portion 14a. The first support portions 161b of the two first stoppers 16 protect the first bent portion 14a from both sides and can reduce the impact force received by the first bent portion 14a.

[0134] FIG. 13 is a schematic cross-sectional view of a localized portion of an electrode assembly according to some further embodiments of the present application.

[0135] 13, in some embodiments, a first adhesive layer 162 is provided on at least a portion of the surface of the first support portion 161b facing the first bending portion 14a. The first adhesive layer 162 may adhere the first support portion 161b to a set component, as needed.

[0136] In some embodiments, the first support portion 161b may be bent and adhered to an end portion of the first bent portion 14a along the first direction X, thereby increasing the adhesion area between the first stopper 16 and the first bent portion 14a and reducing the risk that the first stopper 16 will fall off the first bent portion 14a.

[0137] In some embodiments, first stoppers 16 are attached to both surfaces of the first bending portion 14a, the first body portions 161a of the two first stoppers 16 are respectively installed on both sides of the first bending portion 14a, and the first support portions 161b of the two first stoppers 16 are connected by a first adhesive layer 162.

[0138] The first body portions 161a of the two first stoppers 16 are bonded to the two surfaces of the first bending portion 14a.

[0139] Before the two first stoppers 16 are bonded to the first bent portion 14a, the first adhesive layer 162 is provided on the first support portion 161b of one of the first stoppers 16, and the first adhesive layer 162 is not provided on the first support portion 161b of the other first stopper 16. After the two first stoppers 16 are bonded to the first bent portion 14a, the two first support portions 161b are pressed together and the two first support portions 161b are connected by the one first adhesive layer 162. In some other examples, before the two first stoppers 16 are bonded to the first bent portion 14a, the first adhesive layer 162 is provided on the first support portions 161b of the two first stoppers 16, and after the two first stoppers 16 are bonded to the first bent portion 14a, the two first support portions 161b are pressed together and the two first adhesive layers 162 are bonded together to connect the two first support portions 161b. The first support portions 161b of the two first stoppers 16 are connected by the first adhesive layer 162, thereby adhering the two first stoppers 16 to each other, thereby reducing the risk of the first stoppers 16 falling off from the first bending portions 14a and improving the reliability of the first stoppers 16 over the service life of the battery cell.

[0140] FIG. 14 is a schematic cross-sectional view of a localized portion of an electrode assembly according to some further embodiments of the present application.

[0141] In some embodiments, the electrode assembly 10 further includes a second stopper 17, and at least a portion of the second stopper 17 is located between the first bent portion 14a and the second bent portion 14b. The first stopper 16 and the second stopper 17 are spaced apart from each other along the first direction X, and an end of the first stopper 16 that is away from the second stopper 17 extends beyond one end of the first bent portion 14a, and an end of the second stopper 17 that is away from the first stopper 16 extends beyond the other end of the first bent portion 14a.

[0142] The first stopper 16 and the second stopper 17 are used to prevent at least a part of the ions released from the first bent portion 14a from being occluded in the second bent portion 14b.

[0143] The portion of first stopper 16 that protrudes beyond first bent portion 14a performs a supporting function, reduces the impact force that one end of first bent portion 14a receives during vibration, and can reduce the falling off of active material, while the portion of second stopper 17 that protrudes beyond first bent portion 14a performs a supporting function, reduces the impact force that the other end of first bent portion 14a receives during vibration, and can reduce the falling off of active material.

[0144] In some embodiments, the second stopper 17 is attached to the first bent portion 14a. The second stopper 17 and the first stopper 16 adopt the same structure. Exemplarily, the second stopper 17 includes a second base layer 171 and a second adhesive layer 172. The second adhesive layer 172 is disposed on a surface of the second base layer 171 facing the first bent portion 14a.

[0145] The second base layer 171 includes a second main body portion 171a and a second support portion 171b connected to the second main body portion 171a, and the second adhesive layer 172 is used to bond at least a part of the second main body portion 171a to the first bent portion 14a, and the second support portion 171b protrudes from the first bent portion 14a in the first direction X. In the thickness direction of the first bent portion 14a, the second main body portion 171a overlaps with the first bent portion 14a. The second main body portion 171a is used to reduce the occurrence of lithium deposition by blocking at least a part of the ions released from the positive electrode active material layer 112a of the first bent portion 14a. The second support portion 171b performs a supporting function, effectively reducing the vibration amplitude of the first bent portion 14a, reducing the impact force received by the first bent portion 14a, and reducing the falling off of the active material.

[0146] In some embodiments, the entire second body portion 171a is adhered to the first flex portion 14a by a second adhesive layer 172.

[0147] In some embodiments, at least a portion of the surface of the second support portion 171b facing the first bending portion 14a is not provided with the second adhesive layer 172. In other embodiments, the surface of the second support portion 171b facing the first bending portion 14a may be provided with the second adhesive layer 172.

[0148] In some embodiments, the electrode assembly 10 further includes a third stopper (not shown), which is attached to the first bend 14a and is located between the first stopper 16 and the second stopper 17.

[0149] FIG. 15 is a schematic diagram of a local structure of an electrode assembly according to some further embodiments of the present application.

[0150] 15, in some embodiments, a first stopper 16 is attached to the surface of the second bent portion 14b. Exemplarily, a first body portion of the first stopper 16 is bonded to the surface of the second bent portion 14b.

[0151] In some other embodiments, a first stopper 16 is attached to both the surface of the first bent portion 14a and the surface of the second bent portion 14b.

[0152] FIG. 16 is a schematic diagram of a topographical structure of an electrode assembly according to further some embodiments of the present application.

[0153] In some embodiments, the surface of the separator 13 is provided with a first stopper 16. Illustratively, the entire first stopper 16 is adhered to the surface of the separator 13.

[0154] FIG. 17 is a schematic diagram of a local structure of an electrode assembly according to some further embodiments of the present application.

[0155] 17, one end of the first stopper 16 along the winding direction A is located in a curved region B, and the other end of the first stopper 16 along the winding direction A is located in a straight region C. Exemplarily, the one end of the first stopper 16 along the winding direction A approaches the boundary between the curved region B and the straight region C.

[0156] Exemplarily, the first stopper 16 is attached to the first bent portion 14a and the first flat portion 15a simultaneously.

[0157] FIG. 18 is a schematic diagram of a topographical structure of an electrode assembly according to further some embodiments of the present application.

[0158] 18, both ends of the first stopper 16 along the winding direction A are located in the straight region C. Exemplarily, the first stopper 16 is attached to the first bent portion 14a and the first flat portion 15a at the same time.

[0159] FIG. 19 is a schematic flow diagram of a method for manufacturing an electrode assembly according to some embodiments of the present application.

[0160] As shown in FIG. 19, the manufacturing method of the electrode assembly of the embodiment of the present application includes the following steps.

[0161] S100, providing a positive electrode plate, a negative electrode plate, and a first stopper.

[0162] S200, winding a positive electrode plate and a negative electrode plate along a winding direction to form a wound structure.

[0163] The wound structure includes a bent region. Both the positive electrode plate and the negative electrode plate include a plurality of bent portions located in the bent region, and at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion. At least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion. In the first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction.

[0164] Step S100 includes providing a positive plate S110, providing a negative plate S120, and providing a first stopper S130.

[0165] It should be noted that for the relevant structure of the electrode assembly manufactured by the above manufacturing method of the electrode assembly, reference may be made to the electrode assemblies according to the above embodiments.

[0166] When assembling an electrode assembly based on the above-mentioned manufacturing method of an electrode assembly, the steps do not necessarily have to be performed in the above-mentioned order, that is, the steps may be performed in the order mentioned in the embodiment, or in an order different from the order mentioned in the embodiment, or some steps may be performed simultaneously. For example, step S110 and step S120 may be performed simultaneously, regardless of the order.

[0167] FIG. 20 is a schematic block diagram of a manufacturing system for an electrode assembly according to some embodiments of the present application.

[0168] As shown in FIG. 20 , the manufacturing system 8 of the electrode assembly of the embodiment of the present application includes a first providing device 81 for providing a positive electrode plate, a second providing device 82 for providing a negative electrode plate, a third providing device 83 for providing a first stopper, and an assembly device 84 for winding the positive electrode plate and the negative electrode plate along the winding direction to form a wound structure.

[0169] The wound structure includes a bent region. Both the positive electrode plate and the negative electrode plate include a plurality of bent portions located in the bent region, and at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion. At least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion. In the first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction.

[0170] For the relevant structure of the electrode assembly manufactured by the manufacturing system, please refer to the electrode assemblies according to the above embodiments.

[0171] It should be mentioned that, unless there is a conflict, the embodiments and features in the embodiments in the present application can be combined with each other.

[0172] Finally, it should be noted that the above examples are only for illustrating the technical solutions of the present application, and are not intended to limit the same. Although the present application has been described in detail with reference to the above examples, those skilled in the art may still modify the technical solutions described in the above examples or make equivalent replacements for some of the technical features thereof, but it should be understood that such modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application.

Claims

1. An electrode assembly including a positive electrode plate and a negative electrode plate, the positive electrode plate and the negative electrode plate being wound along a winding direction to form a wound structure, the wound structure including a bent region; The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion; A first stopper is provided on the electrode assembly, and at least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion; An electrode assembly, wherein at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion in a first direction, and the first direction is perpendicular to the winding direction.

2. The electrode assembly according to claim 1 , wherein the first bent portion is provided with the first stopper.

3. The first stopper includes a first base layer and a first adhesive layer, the first adhesive layer being disposed on a surface of the first base layer facing the first bend portion; 3. The electrode assembly of claim 2, wherein the first base layer includes a first body portion and a first support portion connected to the first body portion, the first adhesive layer is used to adhere at least a portion of the first body portion to the first bent portion, and the first support portion protrudes beyond the first bent portion in the first direction.

4. The electrode assembly according to claim 3 , wherein the first adhesive layer is not provided on at least a portion of a surface of the first support portion facing the first bent portion.

5. The electrode assembly according to claim 4, wherein the first stoppers are attached to two surfaces of the first bent portion, the first main body portions of the two first stoppers are respectively installed on both sides of the first bent portion, and the first adhesive layer is not installed on any of the first support portions of the two first stoppers.

6. The electrode assembly according to claim 3 , wherein the first adhesive layer is provided on at least a portion of a surface of the first support portion facing the first bent portion.

7. The electrode assembly according to claim 6, wherein the first stoppers are attached to two surfaces of the first bent portion, the first body portions of the two first stoppers are respectively installed on both sides of the first bent portion, and the first support portions of the two first stoppers are connected by the first adhesive layer.

8. The electrode assembly according to claim 1 , wherein both ends of the first stopper protrude beyond the first bent portion in the first direction.

9. The electrode assembly according to claim 8 , wherein both ends of the first stopper protrude beyond the second bent portion in the first direction.

10. The electrode assembly further includes a second stopper, and at least a portion of the second stopper is located between the first bent portion and the second bent portion; 8. The electrode assembly according to claim 1, wherein the first stopper and the second stopper are spaced apart along the first direction, an end of the first stopper that is away from the second stopper extends beyond one end of the first bent portion, and an end of the second stopper that is away from the first stopper extends beyond the other end of the first bent portion.

11. 11. The electrode assembly according to claim 1, further comprising a separator for isolating the positive electrode plate and the negative electrode plate, and both ends of the separator protrude beyond the first bent portion and the second bent portion in the first direction.

12. The electrode assembly of claim 11 , wherein the porosity of the first stopper is less than the porosity of the separator.

13. The electrode assembly according to claim 11 or 12, wherein the hardness of the first stopper is greater than the hardness of the separator.

14. The electrode assembly according to claim 11 , wherein both ends of the separator protrude beyond the first stopper in the first direction.

15. The electrode assembly according to claim 11 , wherein the first stopper is provided on a surface of the separator.

16. The wound structure further includes a straight region connected to the bent region, The electrode assembly according to any one of claims 1 to 15, wherein both ends of the first stopper along the winding direction are located in the curved region, or one end of the first stopper along the winding direction is located in the curved region and the other end of the first stopper along the winding direction is located in the straight region, or both ends of the first stopper along the winding direction are located in the straight region.

17. The positive electrode plate further includes a first flat portion located in the straight region and a positive electrode tab connected to the first flat portion, the first flat portion being connected to the first bent portion, and the positive electrode tab being connected to one end of the first flat portion along the first direction; The electrode assembly according to claim 16 , wherein an end of the first stopper approaching the positive electrode tab protrudes beyond the first bent portion and the second bent portion in the first direction.

18. 18. The electrode assembly according to claim 1, wherein at least one innermost bent portion of the positive electrode plate is the first bent portion, and at least one innermost bent portion of the negative electrode plate is the second bent portion.

19. A battery cell comprising a housing and the electrode assembly according to claim 1 , wherein the electrode assembly is contained within the housing.

20. 20. A battery comprising: a housing; and the battery cell of claim 19, said battery cell contained within said housing.

21. 21. A power consuming device comprising the battery of claim 20, the battery being for providing electrical energy.

22. 1. A method for manufacturing an electrode assembly, comprising: Providing a positive electrode plate, a negative electrode plate, and a first stopper; and winding the positive electrode plate and the negative electrode plate along a winding direction to form a wound structure; Here, the wound structure includes a bent region, The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion; At least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion; A method for manufacturing an electrode assembly, wherein in a first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction.

23. 1. A system for manufacturing an electrode assembly, comprising: a first providing device for providing a positive electrode plate; a second providing device for providing a negative electrode plate; a third providing device for providing the first stopper; an assembly device for winding the positive electrode plate and the negative electrode plate along a winding direction to form a wound structure; Here, the wound structure includes a bent region, The positive electrode plate and the negative electrode plate each include a plurality of bent portions located in the bent region, at least one bent portion in the positive electrode plate is a first bent portion, and at least one bent portion in the negative electrode plate is a second bent portion adjacent to the first bent portion; At least a portion of the first stopper is located between the first bent portion and the second bent portion, and the first stopper is used to prevent at least a portion of the ions released from the first bent portion from being occluded in the second bent portion; A manufacturing system for an electrode assembly, wherein in a first direction, at least one end of the first stopper protrudes beyond the first bent portion and the second bent portion, and the first direction is perpendicular to the winding direction.

Citation Information

Patent Citations

  • Electrode assembly, battery cell, battery and electric device

    CN212810367U