Repair painting method

The spray can method with polyvinylidene fluoride and thermoplastic acrylic resin composition addresses the issue of noticeable repair marks on metal siding, achieving a uniform and aesthetically pleasing finish.

JP7594957B2Active Publication Date: 2024-12-05LIXIL CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021055031
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-29
Publication Date
2024-12-05
Estimated Expiration
2041-03-29

AI Technical Summary

Technical Problem

Conventional methods of applying paint to metal siding using brushes or spray cans result in noticeable repair marks, making it difficult to achieve a natural finished appearance.

Method used

A repair coating method using a spray can with a first container for a gaseous propellant and a second container for a paint composition containing polyvinylidene fluoride resin and thermoplastic acrylic resin, applied in a specific mass ratio, to ensure even application and minimize repair marks.

Benefits of technology

The method provides a uniform coating that reduces the visibility of repair marks, resulting in a desirable finish on metal siding materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007594957000003
    Figure 0007594957000003
  • Figure 0007594957000004
    Figure 0007594957000004
  • Figure 0007594957000005
    Figure 0007594957000005
Patent Text Reader

Abstract

To provide a repair coating method for a metal siding material which makes repair marks after repair inconspicuous.SOLUTION: This invention is a repair coating method which is a repair coating method using a spray can having a first container which reserves a gas and a second container which reserves a liquid, and the second container reserves a coating composition (C). The coating composition (C) contains a polyvinylidene fluoride resin (A) and a thermoplastic acrylic resin (B), where the mass ratio of the polyvinylidene resin (A) to the total mass of the polyvinylidene resin (A) and the thermoplastic acrylic resin (B) is 30 mass % or more. A metal siding material is repair-coated with the coating composition (C) by using a spray can.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a repair painting method. [Background technology]

[0002] Conventionally, metal siding has been attached to the exterior walls of buildings as an exterior material. Metal siding materials may be damaged by external stimuli and may require repair. The repair is performed by applying a repair paint to the surface of the metal siding material. The repair is performed, for example, by applying the paint with a brush or paint brush.

[0003] A fluororesin paint may be applied to the surface of metal siding materials for the purpose of improving heat insulation, durability, etc. As a paint for repairing a film formed by applying a fluororesin paint, a technique related to a paint for repairing a polyvinylidene fluoride coating film is known (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 61-238863 Summary of the Invention [Problem to be solved by the invention]

[0005] The method of applying paint using a brush or paint brush has the problem that the repair marks are easily noticeable and a natural finish appearance after repair cannot be obtained. Therefore, it is considered to apply repair paint to the part of the metal siding to be repaired using a spray can having a container that stores gas and a container that stores liquid. However, a method of repair painting of metal siding material using a spray can has not been considered so far.

[0006] The present disclosure has been made in consideration of the above, and aims to provide a repair painting method for metal siding material in which repair marks are less noticeable after repair. [Means for solving the problem]

[0007] A repair painting method using a spray can having a first container in which a gas is stored and a second container in which a liquid is stored, the second container storing a paint composition, the paint composition containing a polyvinylidene fluoride resin and a thermoplastic acrylic resin, a mass ratio of the polyvinylidene fluoride resin to a total mass of the polyvinylidene fluoride resin and the thermoplastic acrylic resin being 30 mass% or more, and the paint composition being repair-painted onto a metal siding material using the spray can. [Brief description of the drawings]

[0008] [Figure 1] FIG. 2 is a front view showing the spray can according to the embodiment. [Diagram 2] FIG. 2 is an exploded view showing the spray can according to the embodiment. [Diagram 3] FIG. 2 is an enlarged vertical cross-sectional view of the spray can according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] <Spray can> The spray can 1 according to this embodiment is used for repairing metal siding materials. The metal siding materials are used, for example, as exterior materials for the outer walls of buildings. As shown in FIG. 1, the spray can 1 has a first container 20 in which a propellant as a gas is stored, and a second container 30 in which a coating composition (C) for repairing metal siding materials as a liquid is stored. The first container 20 and the second container 30 are connected, for example, by a connecting member 10. The following description is an example of the configuration of the spray can 1, and the second container 30 may be connected to the first container 20 without the connecting member 10.

[0010] (1st container) The first container 20 has a cylinder 21 made of, for example, a metal, filled with a propellant, and a holder 22 attached to the cylinder 21.

[0011] The propellant stored in the cylinder 21 is not particularly limited, and various known propellants used in aerosol products can be used. For example, liquefied gas, compressed gas, etc. can be used as the propellant. Examples of the liquefied gas include various liquefied petroleum gases, dimethyl ether, and liquefied gases obtained by mixing these. Examples of the compressed gas include compressed gases such as nitrogen gas and carbon dioxide gas. The propellant stored in the cylinder 21 can be ejected to the outside of the cylinder 21 by depressing a stem (not shown) provided at the top of the cylinder 21.

[0012] The holder 22 has a push button 221 and a head portion 222. The holder 22 is integrally molded from, for example, a synthetic resin etc. The holder 22 is attached to the upper portion of the cylinder 21 by, for example, a fitting method.

[0013] Push button 221 is attached to a stem provided at the top of cylinder 21. Inside push button 221, a flow path is provided that communicates with the stem and nozzle 223 described below. By pressing push button 221, the stem is pressed down. As a result, the propellant stored in cylinder 21 is sprayed from nozzle 223 via the flow path provided inside push button 221.

[0014] 1 and 2, the head portion 222 has an injection port 223 and a nozzle 224. As shown in Fig. 3, the head portion 222 has a circular opening that opens downward and into which a part of the connection member 10 can be inserted. A female screw portion 226 is formed on the inner circumferential surface of the opening as a first screw portion that can be screwed into the connection member 10. The opening communicates with the nozzle 224 as shown in Fig. 3.

[0015] From the nozzle 223, the propellant stored in the cylinder 21 is sprayed in the direction shown by the arrow in Fig. 3. From the nozzle 224, the coating composition stored in the second container 30 is discharged. As shown in Figs. 2 and 3, a tube 225 is connected to the nozzle 224. The tube 225 is a cylindrical member having a flow path therein through which the coating composition can flow. The coating composition is supplied to the nozzle 224 through the tube 225. The tip of the tube 225 is inserted into the coating composition stored in the second container 30. The tube 225 may be detachable from the nozzle 224.

[0016] (2nd container) The second container 30 is a container for storing a paint composition (C) for repairing metal siding. The second container 30 is configured to be detachable from the first container 20 via the connecting member 10. As the second container 30, an existing container used for storing the paint composition can be repurposed. The second container 30 has, for example, a cylindrical container body, and as shown in Figs. 2 and 3, a male screw portion 31 is formed on the top of the container body. After the paint composition is filled inside the second container 30, a female screw portion (not shown) formed inside the lid portion C is screwed into the male screw portion 31. As a result, the paint composition is sealed inside the second container 30. The male screw portion 31 is used for connection with the connecting member 10 as a third screw portion.

[0017] (Connection parts) The connection member 10 is a member that connects the first container 20 and the second container 30. The connection member 10 has a substantially cylindrical shape, as shown in Fig. 2 and Fig. 3. The cylindrical shape may have different diameters at both ends depending on the diameters of the first container 20 and the second container 30. The connection member 10 has a space therein through which the tube 225 can be inserted, as shown in Fig. 2 and Fig. 3.

[0018] A male screw portion 11 is formed as a second screw portion on the outer peripheral surface of one end of the connection member 10. The male screw portion 11 can be screwed into a female screw portion 226 formed on the inner surface of the head portion 222 of the first container 20. A female screw portion 12 is formed as a fourth screw portion on the inner peripheral surface of the other end of the connection member 10. The female screw portion 12 can be screwed into a male screw portion 31 formed on the top of the second container 30. This allows the connection member 10 to connect the second container 30 using the male screw portion 31 used to screw into the lid portion C of the second container 30. For this reason, for example, the work of transferring the coating composition to a dedicated container is not required, and workability during application can be improved.

[0019] The connection member 10 is integrally molded from, for example, synthetic resin. Therefore, the diameter of the inner circumferential surface on which the female thread portion 12 is formed can be adjusted according to the diameter of the male thread portion formed on the top of the second container 30. This allows the connection member 10 to be connected to a plurality of second containers 30 having different diameters. For example, by preparing a plurality of connection members 10 having different diameters of the inner circumferential surface according to the diameter of the existing second container 30, a plurality of second containers 30 having different diameters can be connected to the first container 20.

[0020] A procedure for connecting the first container 20 and the second container 30 using the connection member 10 will be described with reference to FIG. 2. First, a procedure for connecting the first container 20 and the connection member 10 will be described. A tube 225 is connected to the nozzle 224 of the first container 20. Next, the tube 225 is inserted into the connection member 10 from one end side. Next, one end side of the connection member 10 is inserted into the opening of the head part 222. Next, the male threaded part 11 of the connection member 10 and the female threaded part 226 formed on the inner surface of the opening are screwed together and fixed. In this state, the tube 225 protrudes from the other end side of the connection member 10.

[0021] Next, a procedure for connecting the second container 30 to the first container 20 to which the connection member 10 is connected will be described. First, the lid C of the second container 30 is removed. Next, the tube 225 is inserted into the second container 30 so that the tip of the tube 225 is submerged in the coating composition stored in the second container 30. Next, the female screw portion 12 of the connection member 10 and the male screw portion 31 of the second container 30 are screwed together and fixed. By the above procedure, the first container 20 and the second container 30 are connected by the connection member 10 as shown in FIG. 3. In this way, by connecting the first container 20 and the second container 30 by screwing them together using the connection member 10, the first container 20 and the second container 30 can be reliably connected. Therefore, even if the weight of the second container 30 is heavy or the viscosity of the coating composition is low, it is possible to prevent the second container 30 from coming off or the coating composition from leaking.

[0022] <Paint composition (C)> The coating composition (C) contains a polyvinylidene fluoride resin (A) and a thermoplastic acrylic resin (B). In addition to the above, the coating composition (C) may contain a pigment and a solvent that dissolves the polyvinylidene fluoride resin (A) and the thermoplastic acrylic resin (B).

[0023] (Polyvinylidene fluoride resin (A)) The polyvinylidene fluoride resin (A) is not particularly limited, but is preferably a vinylidene fluoride (VDF)-hexafluoropropylene (HFP) copolymer (hereinafter referred to as "VDF-HFP copolymer"). Commercially available products may be used as the VDF-HFP copolymer. Commercially available VDF-HFP copolymers include "KynarFlex 2751-00" (manufactured by Arkema), "KynarFlex 2801-00" (manufactured by Arkema), "KynarFlex 2821-00" (manufactured by Arkema), "Kynar ADS2" (manufactured by Arkema), "Solef 11008" (manufactured by Nippon Solvay Co., Ltd.), "Solef 11010" (manufactured by Nippon Solvay Co., Ltd.), and "Solef 21510" (manufactured by Nippon Solvay Co., Ltd.), all under their trade names.

[0024] (Thermoplastic acrylic resin (B)) The thermoplastic acrylic resin (B) is not particularly limited, but is preferably a non-polymerizable thermoplastic acrylic resin from the viewpoint of weather resistance and compatibility with the vinylidene fluoride resin (A). As the non-polymerizable thermoplastic acrylic resin, a commercially available product may be used. Examples of commercially available non-polymerizable thermoplastic acrylic resins include "Paraloid A-11", "Paraloid A-14", "Paraloid A-21", "Paraloid B-60", "Paraloid B-64", "Paraloid B-66", "Paraloid B-72", and "Paraloid B-82" (all manufactured by Dow Chemical Company), all under the trade name.

[0025] The mass ratio of the polyvinylidene fluoride resin (A) to the total mass of the polyvinylidene fluoride resin (A) and the thermoplastic acrylic resin (B) is 30 mass% or more. If the mass ratio of (A) is less than 30%, the adhesion of the film formed by the coating composition (C) to the metal siding material decreases.

[0026] (solvent) The solvent is not particularly limited as long as it can easily dissolve the polyvinylidene fluoride resin (A) and the thermoplastic acrylic resin (B) and does not adversely affect the properties of the resulting coating composition (C) or the film formed. Examples of the solvent include ketone solvents, ester solvents, furan solvents, polar solvents, etc. The above solvents may be used alone or in any combination of two or more solvents. From the viewpoint of solubility and coating workability, ketone solvents and polar solvents are preferred as the solvent.

[0027] Examples of ketone-based solvents include acetone (dimethyl ketone), MEK (methyl ethyl ketone), cyclohexanone, and MIBK (methyl isobutyl ketone). Examples of ester-based solvents include methyl acetate, ethyl acetate, and butyl acetate. Examples of furan-based solvents include THF (tetrahydrofuran). Examples of polar solvents include NMP (N-methyl-2-pyrrolidone).

[0028] (Pigments) The pigment is not particularly limited, and a pigment appropriately selected according to the color of the metal siding material to be repaired can be used. Examples of pigments include color pigments, extender pigments, and luster pigments. The above pigments may be used alone, or two or more pigments may be used in any combination.

[0029] Examples of the color pigment include inorganic pigments such as carbon black, yellow iron oxide, red iron oxide, composite oxides (nickel-titanium, chromium-titanium, bismuth-vanadium, cobalt-aluminum, cobalt-aluminum-chromium, ultramarine blue, etc.), and titanium oxide, as well as organic pigments such as quinacridone, diketopyrol, benzimidazolone, isoindolinone, anthrapyrimidine, phthalocyanine, threne, dioxazine, and azo. From the viewpoint of weather resistance, it is preferable to use inorganic pigments.

[0030] Examples of the extender pigment include clay, kaolin, barium sulfate, barium carbonate, calcium carbonate, talc, silica, and alumina white.

[0031] Examples of the luster pigment include aluminum (including vapor-deposited aluminum), copper, zinc, brass, nickel, glass flakes, aluminum oxide, mica, aluminum oxide coated with at least one of titanium oxide and iron oxide, mica coated with at least one of titanium oxide and iron oxide, etc. As the aluminum pigment, either a non-leafing type aluminum pigment or a leafing type aluminum pigment can be used.

[0032] The pigment may be added directly to the coating composition (C), or may be mixed and dispersed with a pigment dispersant and a pigment dispersing resin to form a paste, which may then be blended into the coating composition (C). There are no particular limitations on the pigment dispersant, pigment dispersing resin, or dispersion method, and known materials and methods may be used.

[0033] (Other Ingredients) The coating composition (C) may contain components other than those described above. Examples of the components other than those described above include known coating additives such as ultraviolet absorbers (e.g., benzotriazole-based absorbers, triazine-based absorbers, salicylic acid derivative-based absorbers, benzophenone-based absorbers, etc.), light stabilizers (e.g., hindered amines, etc.), thickeners (non-aqueous dispersion-type acrylic thickeners, polymer fine particle-type thickeners, urethane association-type thickeners, urea-type thickeners, mineral-type thickeners, etc.), defoamers, surface conditioners, anti-settling agents, rust inhibitors, chelating agents (e.g., acetylacetone), dehydrating agents, neutralizing agents, and plasticizers.

[0034] [Paint viscosity] The paint viscosity of the paint composition (C) is preferably 8 seconds or more and 15 seconds or less. If the paint viscosity is less than 8 seconds, sagging occurs on the painted surface, resulting in an uneven appearance and poor appearance. If the paint viscosity exceeds 15 seconds, the spraying state is poor, resulting in lumps on the painted surface and poor appearance. From the above viewpoint, it is preferable that the paint viscosity is 10 seconds or more and 12 seconds or less. The paint viscosity of the paint composition (C) is measured by the flow cup method using Iwata Cup NK-2 (manufactured by Anest Iwata Corporation). Specifically, the cup is placed in the paint composition (C), and then the cup is pulled up, and the outflow time is measured from when the paint starts to flow out of the hole at the bottom of the cup until the paint stops flowing out.

[0035] (Metal siding material) The metal siding material to be repaired by the repair coating method according to this embodiment is not particularly limited, and any known metal siding material used in the exterior wall structure of a building can be repaired.

[0036] <Method of repair painting for metal siding> The repair coating method for metal siding material according to this embodiment includes a spray coating step of spray coating a paint composition onto the metal siding material to be repaired, using the above-mentioned spray can 1. This allows the paint composition to be applied uniformly to the repaired portion of the metal siding material, as compared with the conventional repair coating method using brush painting, so that repair marks after repair are less noticeable and a favorable finished appearance can be obtained.

[0037] A method of spray coating using the spray can 1 according to this embodiment will be described below. A user of the spray can 1 (hereinafter, referred to as "user") selects a paint composition (C) corresponding to the color of the metal siding material to be repaired, stores it in the second container 30, and connects the first container 20 and the second container 30. The second container 30 may be a container in which the paint composition (C) is stored beforehand. Next, in the spray coating process, the user aims the nozzle 223 of the spray can 1 at the repair location and presses the push button 221. As a result, the paint composition stored in the second container 30 is spray-coated evenly to the repair location.

[0038] When a user presses push button 221, propellant is sprayed from nozzle 223 in the direction shown by the arrow in Fig. 3. This generates a negative pressure due to the spray airflow of the propellant. This negative pressure generates a suction force in tube 225, and the paint composition stored in second container 30 is sucked up through tube 225. The sucked up paint composition is discharged from nozzle 224 and sprayed in the direction of the arrow in Fig. 3 together with the propellant sprayed from nozzle 223. This allows the paint composition to be sprayed evenly onto the repaired portion of the metal siding material.

[0039] In the above spray coating process, the distance between the part of the metal siding material to be repaired and the nozzle 223 of the spray can 1 is preferably 3 cm or more and 15 cm or less, and more preferably 5 cm or more and 10 cm or less. This makes it possible to obtain a desirable finished appearance after the repair coating.

[0040] The preferred embodiments of the present disclosure have been described above. The present disclosure is not limited to the above embodiments, and modifications and improvements are included in the present disclosure. EXAMPLES

[0041] The present disclosure will be described in more detail below with reference to examples, but the present disclosure is not limited to the following examples.

[0042] (Preparation of Coating Composition (C)) KynarFlex2801-00 (Arkema) was used as the polyvinylidene fluoride resin (A), and Paraloid A-21 (Dow Chemical) was used as the thermoplastic acrylic resin (B). The mass ratio of the polyvinylidene fluoride resin (A) to the total mass of the polyvinylidene fluoride resin (A) and the thermoplastic acrylic resin (B) was 55%. A white pigment (Tipaque CR-97, Ishihara Sangyo Kaisha) was used as the pigment. Flowlen AC-300, Kyoeisha Chemical Co., Ltd. was used as the additive. Techpolymer EXM-8, Sekisui Chemical Co., Ltd. was used as the gloss adjuster. Using MEK (methyl ethyl ketone), cyclohexanone, and NMP (N-methyl-2-pyrrolidone) as solvents, the paint viscosity of the paint composition was adjusted to 5 seconds, 8 seconds, 11 seconds, 15 seconds, and 18 seconds, respectively, to prepare the paint composition (C) according to each example. The paint viscosity was measured by a flow cup method using an Iwata Cup NK-2 (manufactured by Anest Iwata Corporation). In detail, the Iwata Cup NK-2 was placed in each paint composition, and then the cup was lifted up, and the paint viscosity was measured as the outflow time from when the paint composition started to flow out of the hole at the bottom of the cup until the outflow of the paint composition stopped.

[0043] (Repair coating with coating composition (C)) The paint composition (C) prepared above was stored in the second container of a spray can having a first container and a second container, and repair painting was performed by spray painting with the distances between the nozzle of the spray can and the repair site of the metal siding material to be repaired being 1 cm, 3 cm, 5 cm, 9 cm, 15 cm, and 17 cm, respectively.

[0044] [Appearance evaluation] The appearance of the metal siding material repaired with the coating composition (C) was visually evaluated according to the following criteria. The results are shown in Tables 1 and 2. 3: Repair marks are hardly noticeable, resulting in a very good appearance 2: Repair marks are less noticeable, resulting in a good appearance 1: Repair marks are less noticeable

[0045] [Table 1]

[0046] [Table 2]

[0047] From the results of Tables 1 and 2, it was confirmed that the metal siding material repaired by the repair painting method according to each Example had less noticeable repair marks after repair painting. It was also confirmed that a desirable appearance of the metal siding material after repair painting can be obtained by setting the paint viscosity of the paint composition to 8 seconds or more and 15 seconds or less, and setting the distance between the repaired part and the nozzle of the spray can to 3 cm or more and 15 cm or less. [Explanation of symbols]

[0048] 1 spray can, 20 first container, 30 second container

Claims

1. A repair painting method using a spray can having a first container in which a gas is stored and a second container in which a liquid is stored, The second container contains a coating composition, The coating composition includes a polyvinylidene fluoride resin and a thermoplastic acrylic resin, a mass ratio of the polyvinylidene fluoride resin to a total mass of the polyvinylidene fluoride resin and the thermoplastic acrylic resin is 30 mass% or more; A repair coating method comprising applying the coating composition to a metal siding material using the spray can.

2. 2. The repair coating method according to claim 1, wherein the coating composition has a coating viscosity of 8 seconds or more and 15 seconds or less.

3. 3. The repair coating method according to claim 1, wherein the distance between the part to be repaired and the spray can is 3 cm or more and 15 cm or less.

Citation Information

Patent Citations

  • Paint for repair

    JP1986238863A

  • Paint composition

    JP1993320563A

  • Polymer composition for fluorine-containing coating material

    JP1994057196A

  • Simplified spray gun

    JP1998305243A

  • Plastic molded product coated with surface hydrophilicity imparting coating material

    JP2000301054A