Screen printing mask

The screen printing mask's innovative recessed and protruding design enhances bonding strength by mechanical interlocking, preventing peeling and damage, and enabling precise, lightweight construction.

JP7595118B2Active Publication Date: 2024-12-05MAXELL LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023111292
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-07-06
Publication Date
2024-12-05
Estimated Expiration
2039-04-26

AI Technical Summary

Technical Problem

Conventional screen printing masks with a metal lower layer and resin upper layer face issues with peeling due to adhesive forces, leading to damage during printing, as the resin layer is not securely fixed to the metal layer.

Method used

The screen printing mask design incorporates a recessed portion between the upper and lower layers, featuring a biting protrusion and receiving recess with a sloped contact surface, enhancing the bonding strength through both adhesive and mechanical interlocking mechanisms.

Benefits of technology

This design prevents peeling and damage by increasing the contact area and structural strength, allowing for more reliable printing and reducing the risk of buckling, while also enabling lighter and more precise mask construction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595118000001
    Figure 0007595118000001
  • Figure 0007595118000002
    Figure 0007595118000002
  • Figure 0007595118000003
    Figure 0007595118000003
Patent Text Reader

Abstract

To strongly and closely fix an upper layer made of metal and a lower layer made of a resin, and prevent damage of a printing mask caused by peeling of the upper and lower layers.SOLUTION: A mask for screen printing includes a lower layer 2 which has a group of pattern openings 3 and is made of resin, and an upper layer 1 which has a group of adjustment openings 4 corresponding to the pattern openings 3 and is made of metal, and has a biting part 13 provided between the upper layer 1 and the lower layer 2, wherein the biting part 13 includes a receiving recess 16 formed so as to be recessed between the adjacent adjustment openings 4 on the lower surface of the upper layer 1, and a biting projection 15 which is formed so as to project from the upper surface of the lower layer 2 and bites into the receiving recess 16.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This invention is a method for fine printing of internal electrodes of ceramic capacitors and multilayer chip inductors. The present invention relates to a screen printing mask used when forming a pattern by a screen printing method, Among them, screen printing substrates with a laminated structure of an upper layer made of metal and a lower layer made of resin are Regarding masks. [Background technology]

[0002] This type of screen printing mask is disclosed in, for example, Patent Document 1. The mask described in is made of a metal plating (electroforming) having a plurality of mesh patterns. It is composed of a metal layer and a lower resin layer made of photosensitive resin having multiple printed patterns. The upper and lower surfaces of the metal layer are flat, and the resin layer is fixed to the lower surface of the metal layer. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2008-162277 A Summary of the Invention [Problem to be solved by the invention]

[0004] As in Patent Document 1, a mask in which the lower layer having a print pattern is formed of a resin layer is used. In this case, the thickness of the lower layer can be made thinner and more uniform than when the lower layer is made of a metal layer. This improves the printing accuracy of the mask and also makes it possible to make the entire mask thinner and lighter. However, in the mask of Patent Document 1, the lower surface of the metal layer, which is a flat surface, is made of a photosensitive resin. The resin layer is fixed in place only by the adhesive force. The pressure applied by the squeegee and the bending deformation of the mask caused by the pressure applied repeatedly When the mask is exposed to the heat, the upper and lower layers can peel off and separate, damaging the mask. There is a risk of this happening.

[0005] The present invention relates to a method for manufacturing a metal-made upper layer and a resin-made lower layer, which are firmly bonded together to form a metal-made upper layer and a resin-made lower layer. The purpose of this invention is to prevent damage to the mask due to peeling off of the mask. [Means for solving the problem]

[0006] The screen printing mask of the present invention has a resin substrate having a group of pattern openings 3. a layer 2 and an upper layer 1 made of metal having a group of alignment openings 4 corresponding to the pattern openings 3; The upper layer 1 partially penetrates into the lower layer 2 between the upper layer 1 and the lower layer 2. The upper layer 1 is provided with a penetration portion 13, or a penetration portion 13 where the lower layer 2 partially penetrates into the upper layer 1. It is characterized by the fact that

[0007] The biting portion 13 is a receiving portion formed as a recess between adjacent adjustment openings 4 on the lower surface of the upper layer 1. a receiving recess 16, and a biting protrusion 15 formed on the upper surface of the lower layer 2 and biting into the receiving recess 16; It is composed of:

[0008] The biting portion 13 is provided in a recess 16 formed in the upper surface of the lower layer 2 and in a lower surface of the upper layer 1. and a biting protrusion 15 that is formed between the adjacent adjustment openings 4 and bites into the receiving recess 16. It is composed of:

[0009] At the contact surface between the biting projection 15 and the receiving recess 16 at the rising portion 17 of the biting projection 15 A gradient is provided.

[0010] The opposing raised portions 17·17 of the biting protrusion 15 are flared tapered portions that flare out toward the protruding tip. It is formed into a pearl shape.

[0011] The lower layer 2 may be made of a photocurable resin or a thermosetting resin.

[0012] The lower layer 2 is made of a photocurable resin, and the photocurable resin is made of a photocurable emulsion resin 34. has been formed. Effect of the Invention

[0013] As in the screen printing mask according to the present invention, a layer is formed between the upper layer 1 and the lower layer 2, and the layer is formed against the lower layer 2. The upper layer 1 partially penetrates into the bite portion 13, or the lower layer 2 partially penetrates into the upper layer 1. When the penetrating biting portion 13 is provided, in addition to the adhesive strength derived from the photocurable resin, etc., The upper layer 1 is joined to the upper layer 2 by the joining force generated by the penetration part 13 where one of the upper and lower layers 1 and 2 penetrates into the other. The screen printing mass according to the present invention can be fixed to the lower layer 2 in close contact with each other. According to the company, compared to conventional masks that fix a resin layer to the flat surface of a metal layer, the upper layer and the lower layer This allows the upper and lower layers 1 and 2 to be more firmly attached to each other, preventing the mask from peeling off and breaking. In addition, the resin constituting the lower layer 2 is resistant to light and heat. It is preferable to use a resin that hardens in response to the above reaction.

[0014] The biting portion 13 is a receiving portion formed as a recess between adjacent adjustment openings 4 on the lower surface of the upper layer 1. a receiving recess 16, and a biting protrusion 15 formed on the upper surface of the lower layer 2 and biting into the receiving recess 16; According to the bite portion 13, the mask can be made of a material that is more flexible than the conventional mask. The upper and lower layers 1 are in contact with each other by the amount of contact between the outer peripheral side surface of the biting protrusion 15 and the inner peripheral side surface of the receiving recess 16. This increases the contact area between the two parts, so that the two parts 1 and 2 can be fixed more firmly. In addition, the specific gravity of the resin constituting the lower layer 2 is greater than the specific gravity of the metal constituting the upper layer 1. If it is small, the proportion of the lower layer 2 made of resin increases by the amount of the biting portion 13. The mask can be made lighter.

[0015] The biting portion 13 is provided in a recess 16 formed in the upper surface of the lower layer 2 and in a lower surface of the upper layer 1. and a biting protrusion 15 that is formed between the adjacent adjustment openings 4 and bites into the receiving recess 16. According to the bite portion 13, the mask can be made of a material that is more flexible than the conventional mask. The upper and lower layers 1 are in contact with each other by the amount of contact between the outer peripheral side surface of the biting protrusion 15 and the inner peripheral side surface of the receiving recess 16. This increases the contact area between the two parts, so that the two parts 1 and 2 can be fixed more firmly. In addition, the proportion of the upper layer 1 made of a metal layer increases by the amount of the biting portion 13. This increases the structural strength of the mask and suppresses damage to the mask due to buckling.

[0016] At the contact surface between the biting projection 15 and the receiving recess 16 at the rising portion 17 of the biting projection 15 If a gradient is provided, the contact surface will have a gradient of 0.01 mm, assuming that the protruding height of the rising portion 17 is the same. The length of the contact surface can be increased with the gradient compared to without the gradient. The contact area of ​​1·2 can be further increased.

[0017] The rising portion 17 of the biting protrusion 15 is formed in a tapered shape that widens toward the protruding tip side. In this way, the biting projection 15 and the receiving recess 16 can be engaged in a dovetail shape. This allows the upper and lower layers 1 and 2 to be fixed even more firmly in place.

[0018] The lower layer 2 made of a photocurable resin can be used to form a complex planar shape by photolithography. The lower layer 2 can be easily and precisely formed. According to the lower layer 2, the thermosetting resin has superior chemical resistance and solvent resistance compared to the photocurable resin. Even in printing environments where printing pastes containing acids, alkalis, or solvents are used, It can be used preferably with cleaning agents containing acids, alkalis, or solvents to clean the mask after use. It is also advantageous in that it can be used.

[0019] The lower layer 2 is made of a photocurable resin, and the photocurable resin is made of a photocurable emulsion resin 34. When the receiving recess 16 is formed, the surface of the upper layer 1 on which the receiving recess 16 is formed is oriented upward, and the upper surface By pouring photocurable emulsion resin 34 into the cavity, the fluidity of the emulsion is utilized to form the receiving cavity. While filling the portion 16 with the resin 34, the emulsion resin 34 is simply applied so that the surface of the emulsion resin 34 becomes smooth. By simply irradiating it with light and curing it, the adhesive can be provided with the protruding portions 15 and can be used as a base material. In this way, a lower layer 2 having a uniform thickness from the lower surface of the upper layer 1 can be obtained. The surface on which the projections 15 are formed is oriented upward, and a photocurable emulsion resin 34 is poured onto the upper surface. By filling the resin 34 with the emulsion, the surface of the resin 34 is covered with the fluidity of the emulsion. It can be easily applied to make it smooth. Simply expose it to light and let it harden. The lower layer 2 is provided with a receiving recess 16 and has a uniform thickness from the lower surface of the upper layer 1. do. [Brief description of the drawings]

[0020] [Figure 1]1 is a vertical sectional side view of a screen printing mask according to a first embodiment of the present invention. [Diagram 2] 1 is an overall plan view of a screen printing mask according to a first embodiment, and an enlarged view of a pattern opening and an adjustment opening. [Diagram 3] FIG. 2 is an explanatory diagram showing a primary electroforming step in the method for producing a screen printing mask according to the first embodiment. [Figure 4] FIG. 3 is an explanatory diagram showing a secondary electroforming step in the method for producing a screen printing mask according to the first embodiment. [Diagram 5] 4 is an explanatory diagram showing a resin layer forming step in the method for producing a screen printing mask according to Example 1. FIG. [Figure 6] FIG. 6 is a longitudinal sectional view of a main portion of a screen printing mask according to a second embodiment of the present invention. [Figure 7] FIG. 11 is a vertical sectional side view of a main portion of a screen printing mask according to a third embodiment of the present invention. [Figure 8] FIG. 11 is an explanatory diagram showing an etching step in the method for producing a screen printing mask according to Example 3. [Figure 9] FIG. 11 is a vertical sectional side view of a screen printing mask according to Example 4 of the present invention. [Figure 10] FIG. 10 is an explanatory diagram showing a primary electroforming step in the method for producing a screen printing mask according to Example 4. [Figure 11] FIG. 10 is an explanatory diagram showing a secondary electroforming step in the method for producing a screen printing mask according to Example 4. [Figure 12] 13 is an explanatory view showing a resin layer forming step in the method for producing a screen printing mask according to Example 4. FIG. [Figure 13] FIG. 11 is a longitudinal sectional view of a main portion of a screen printing mask according to a fifth embodiment of the present invention. [Figure 14] FIG. 1 is a vertical cross-sectional view showing a reference example of a screen printing mask in which an upper layer made of metal and a lower layer made of resin are laminated. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] (Example 1) FIG. 1 to FIG. 5 show a screen printing mask according to the present invention (hereinafter, simply referred to as a printing mask). In the present invention, the terms front, back, left, right, top and bottom refer to the same as those in FIG. Also follow the crossed arrows shown in Figure 2 and the indications of front, back, left, right, up and down written near each arrow. The dimensions such as thickness and width in each drawing of the following examples do not represent the actual state. Each is shown diagrammatically.

[0022] The printing mask is a multi-layer ceramic capacitor applied to the surface of the ceramic film to be printed. It is used to print and form the internal electrodes that make up the capacitor by screen printing. The printing mask is formed in a square shape with each side measuring 250 mm, and the mask is divided into four quadrants. When the substrate is divided, a pattern forming area M for printing an electrode pattern is defined in each quadrant. Further, a process after screen printing is performed so as to surround the periphery of the pattern forming region M. A cutter for printing cut marks used when cutting the printed object into a specified shape. The printing mask is divided into four areas, the mark forming area C, and the mask is printed by itself or on the four periphery. With the frame fixed, the mask is attached to a mask fixing portion of a screen printing device.

[0023] As shown in Figure 1, the printing mask is made up of an upper layer 1 made of metal and a lower layer 2 made of synthetic resin (resin). The lower layer 2 has a group of pattern openings 3. The upper layer 1 is provided with a group of adjustment openings 4 corresponding to the pattern openings 3. The outer shape of the adjustment opening 4 is the same as the opening shape of the pattern opening 3 or It may also be formed to be slightly larger than the opening shape.

[0024] As shown in FIG. 2, the pattern opening 3 formed in the lower layer 2 has a rectangular shape that is long from left to right. The pattern forming regions M are arranged in a matrix. The adjustment opening 4 formed in the upper layer 1 above the opening 3 has a lattice-shaped adjustment rib 5 inside. The adjustment opening 4 has an outer shape similar to that of the pattern opening 3. The adjustment rib 5 is formed slightly smaller than the opening shape. It is provided to adjust the amount of printing paste supplied.

[0025] Although not shown in the figure, the cut mark forming area C has a long and narrow rectangular shape formed on the lower layer 2. A cut mark opening is formed, and a cover is formed on the upper layer 1 above the cut mark opening. The adjustment opening is formed with a lattice-shaped adjustment rib inside. The cut mark opening is formed into a mesh-like opening, and the outer shape of the cut mark opening is The opening shape is slightly smaller than that of the cut mark opening. The outer shape of the opening is the same as the opening shape of the cut mark opening, or It can also be formed slightly larger than the shape. The opening shape in the mark formation area C may be made different.

[0026] The upper surface of the upper layer 1 constitutes a squeegee surface 6, and during printing, the printing material placed on the squeegee surface 6 is By squeegeeing the paste with the squeegee S, the pattern opening 3 and the cutter The print paste is filled into the openings, and an electrode pattern that matches the pattern openings 3 is printed on the surface to be printed. A printing layer is formed with a cut pattern that matches the cut mark openings. The squeegee S is moved from the front to the rear of the printing mask with its tip in contact with the squeegee surface 6. The "printing paste" mentioned here is solder paste, This concept includes ream solder, liquid solder, conductive ink, etc.

[0027] Between the upper layer 1 and the lower layer 2, there is a biting portion 13 for firmly fixing the two layers 1 and 2 in contact with each other. The upper layer 1 made of metal is provided with a first metal layer 11 on the upper side having a relatively large thickness. The second metal layer 12 is formed by laminating a second metal layer 13 having a relatively small thickness on the lower side. The layer 12 has a lattice-shaped cutout 14 formed between adjacent adjustment openings 4, 4, penetrating vertically. The upper surface of the cutout portion 14 is covered with the first metal layer 11. A receiving recess 16A (16) is formed to receive the biting protrusion 15A (15). The recesses 16A are formed in a lattice shape corresponding to the notches 14. The thickness of the upper layer 1 is set to 18 μm. The depth of the receiving recess 16A is set to 3 μm.

[0028] The lower layer 2 made of synthetic resin is fixed to the lower surface of the upper layer 1 and forms a pattern opening 3. The upper surface of the lower layer 2 is provided with a biting projection 15A which constitutes the biting portion 13 and projects upward. The opposing raised portions 17 are formed of parallel surfaces. The lower layer 2 has a biting protrusion 15A and the upper layer 1 has a receiving recess 16A. The layer 1 is provided with a biting portion 13 where the lower layer 2 partially penetrates into the layer 1. The thickness of the lower layer 2 excluding A is set to 3 μm. Therefore, the total thickness of the printing mask is 21 μm. is formed.

[0029] In this way, the receiving recess formed between the adjacent adjustment openings 4 on the lower surface of the upper layer 1 is The recess 16A is formed on the upper surface of the lower layer 2 and is engaged with the recess 16A. When the biting portion 13 composed of the portion 15A (15) is provided, it is more flexible than the conventional mask. The outer peripheral side surface of the biting protrusion 15A and the inner peripheral side surface of the receiving recess 16A are in contact with each other, and the upper and lower portions of the biting protrusion 15A and the inner peripheral side surface of the receiving recess 16A are in contact with each other. Since the contact area between the layers 1 and 2 can be increased, the layers 1 and 2 can be firmly fixed in contact with each other. In addition, the proportion of the lower layer 2 made of synthetic resin increases by the amount of the biting portion 13. This has the advantage of making the printing mask lighter. The contact area between the upper layer 1 and the lower layer 2 can be increased as the depth increases. If this occurs, the structural strength of the upper layer 1 will decrease, and the printing mask will be damaged, such as buckled, by the pressing force of the squeegee S during printing. Therefore, the depth of the receiving recess 16A is set to less than half the thickness of the upper layer 1. It is preferable to set

[0030] An example of a method for manufacturing a printing mask according to this embodiment is shown in FIG. 3 to FIG. 5. The primary electroforming process shown in (a) to (d), the secondary electroforming process shown in FIG. 4(a) to (d), and the secondary electroforming process shown in FIG. The resin layer is formed through the steps of forming a resin layer shown in (a) to (c). As shown in FIG. 3(a), a conductive flat plate-shaped electroforming mold 20 made of stainless steel is provided on the surface thereof. A negative type first photoresist layer 21 is formed. Next, the first photoresist layer 21 is A first pattern film 22 (photomask) is then adhered onto the top.

[0031] Next, the inside of the oven of the ultraviolet irradiation device equipped with the ultraviolet lamp 23 is heated to the oven temperature during the exposure operation. After the preheating is completed, the laminate shown in FIG. 3(a) is placed in the furnace of the ultraviolet irradiation device. After the laminate is acclimated to the temperature in the furnace, it is irradiated with ultraviolet light from an ultraviolet lamp 23. The first photoresist layer 21 is exposed through the first pattern film 22. The resulting laminate is taken out, and the first pattern film 22 is removed from the first photoresist layer 21. The unexposed portion of the first photoresist layer 21 is dissolved and removed (developed) to obtain the structure shown in FIG. As shown in (b), a primary pattern resist 24 is formed on the electroforming matrix 20. The line resist 24 is formed by adjusting the opening 4 for the pattern opening 3 and adjusting the opening 4 for the cut mark opening. It is made up of a resist body that corresponds to the mouth opening.

[0032] Next, as shown in FIG. 3(c), the electroforming matrix not covered with the primary pattern resist 24 is By subjecting the surface of the mold 20 to electroforming (plating) processing, the height of the primary pattern resist 24 is Within this range, a primary electroforming layer 25 that will become the first metal layer 11 is formed. After the primary electroforming layer 25 is formed, The surfaces of the primary pattern resist 24 and the primary electroforming layer 25 are polished and smoothed, as shown in FIG. The result will be in state d).

[0033] In the secondary electroforming process, as shown in FIG. 4(a), a primary pattern resist 24 and A negative type second photoresist layer 28 is then formed on the surface of the primary electroforming layer 25. 2. A second pattern film 29 (photomask) is adhered to the photoresist layer 28. The second pattern film 29 has a light-transmitting portion corresponding to the opening of the adjustment opening 4 and the notch 14. Next, ultraviolet light is irradiated from the ultraviolet lamp 23 to form a second pattern film. The second photoresist layer 28 is exposed through the film 29. After exposure, the second photoresist The second pattern film 29 is removed from the layer 28, and the unexposed portions of the second photoresist layer 28 are By dissolving and removing (developing) the resist, the primary pattern resist is formed as shown in FIG. 4(b). A secondary pattern resist 30 is formed on the primary electroforming layer 24 and the primary electroforming layer 25. The display 30 is a display for adjusting the opening 4 for the pattern opening 3 and the opening for adjusting the cut mark opening. It is composed of a resist body corresponding to the mouth portion and a resist body corresponding to the notch portion 14.

[0034] Next, as shown in FIG. 4(c), the primary electrode that is not covered with the secondary pattern resist 30 is By subjecting the surface of the casting layer 25 to electroforming (plating), the secondary pattern resist 30 is highly A secondary electroformed layer 31 that will become the second metal layer 12 is formed within the range of the thickness. After the secondary electroformed layer 31 is formed The surfaces of the secondary pattern resist 30 and the secondary electroforming layer 31 are polished and smoothed, and then the secondary When the next pattern resist 30 is removed and the electroforming mold 20 is also removed, the result is as shown in FIG. A mask precursor can be obtained. After removing the resist pattern 30 and the secondary electroforming layer 31, the surfaces of the secondary pattern resist 30 and the secondary electroforming layer 31 are polished to be smooth. Depending on the form of the printing mask, the secondary pattern resist 30 may be bimodal. The mesh of both adjustment openings may be formed so as to cover the entire area of ​​the adjustment opening. The secondary electroforming layer 31 is not formed in the corresponding portion. This can be done as needed.

[0035] In the resin layer forming process, the mask precursor is temporarily fixed on a surface plate, and as shown in FIG. Then, a photocurable emulsion resin (photocurable resin) 34 is poured onto the surface of the mask precursor body, and the emulsion Using the resulting fluidity, the primary and secondary electroforming layers 25·31 and the primary pattern resist are The emulsion resin 34 is then evenly applied to the surface of the substrate 24. A glass mask is then placed on the emulsion resin 34. Then, a third pattern film 35 (photomask) made of The emulsion resin 34 is exposed to ultraviolet light from the tap 23 through the third pattern film 35. After hardening, the third pattern film 35 is removed from the emulsion resin 34. By removing the unhardened portion of the grease 34, the primary and secondary A lower layer 2 having an opening corresponding to the pattern opening 3 is formed on the electroforming layer 25·31 as a mask precursor. Finally, the primary pattern resist 24 is removed, leaving the mark shown in FIG. The photocurable emulsion resin 34 reacts to ultraviolet light and hardens. In addition to those that cure in response to visible light, those that cure in response to heat may also be used. It may be a thermosetting emulsion resin (resin) that hardens.

[0036] Since the lower layer 2 in this embodiment is made of a photocurable resin, it is possible to form the lower layer 2 by a photolithography method. The lower layer 2 having a complex planar shape can be easily formed with high accuracy. The photocurable resin is formed from a photocurable emulsion resin 34. The surface on which the receiving recess 16A is formed is oriented upward, and a photocurable emulsion resin 34 is applied to the upper surface of the surface. By pouring the resin 34 into the receiving recess 16A, the resin 34 is poured into the receiving recess 16A by utilizing the fluidity of the emulsion. While filling, the emulsion resin 34 can be easily coated so as to make the surface smooth. By simply irradiating the upper layer 1 with light and curing it, the upper layer 1 is provided with the biting protrusions 15A and the lower surface of the upper layer 1 is A lower layer 2 having a uniform thickness can be obtained.

[0037] The lower layer 2 can also be made of a thermosetting resin. Thermosetting resins are more durable than photocurable resins. It has excellent chemical resistance and solvent resistance, so it is suitable for printing pastes containing acids, alkalis, or solvents. It can be used suitably in printing environments where acid, It is also advantageous in that cleaning agents containing alkali or solvents can be used.

[0038] In the above manufacturing method, the resin layer forming step is carried out without removing the primary pattern resist 24. After removing the primary pattern resist 24 at the same time as removing the secondary pattern resist 30, In this case, the resin layer forming step may be performed after removing the primary pattern resist 24. During the removal, the lower layer 2 can be prevented from falling off and being removed together with the primary pattern resist 24. In addition, the electroforming matrix 20 may be removed after the lower layer 2 is formed.

[0039] The resin layer forming step may be performed by the following method: A plastic resin plate is temporarily fixed on a surface plate or the surface of a mask precursor formed by electroforming on an electroforming mold 20. The softened thermoplastic resin plate is placed on the mask front body and pressed against the mask front body. A part of the thermoplastic resin plate is inserted into the receiving recess 16A. After the resin is cured, the unnecessary parts of the thermoplastic resin plate are removed by sublimation using a laser or by etching. The lower layer 2 is formed by melting and removing the pattern opening 3 through a chipping process.

[0040] Example 2 FIG. 6 shows a screen printing mask according to the present invention (hereinafter, simply referred to as a printing mask). In this embodiment, the opposing raised portions of the biting protrusions 15A (15) are The difference from the first embodiment is that the slope of the sloped portions 17·17 is provided. The slope of the rising portion 17 is the same as that of the second pattern level. When exposing the resist layer 28, the light transmitting holes corresponding to the notches 14 of the second pattern film 29 are The other parts are the same as in Example 1, so the same The same reference numerals are used to designate the same members, and the description thereof will be omitted. The same applies to the following embodiments.

[0041] As described above, the biting projection 15A and the receiving recess 15B at the rising portion 17 of the biting projection 15A are Since a gradient is provided on the contact surface with the portion 16A, when it is assumed that the protruding height of the rising portion 17 is the same, When comparing the contact surface with and without a gradient, the contact surface can be made longer with a gradient. Therefore, the contact area between the upper and lower layers 1 and 2 can be increased. Since the rising portion 17 of A is formed in a tapered shape, the biting projection 15A and the receiving recess 16A can be engaged in a dovetail shape, so that the upper and lower layers 1 and 2 can be sealed even more firmly. Can be fastened.

[0042] (Example 3) FIG. 7 and FIG. 8 show a screen printing mask according to the present invention (hereinafter, simply referred to as a printing mask). In this embodiment, the upper layer 1 is formed only by the first metal layer 11. The difference from Example 1 is that the first electroforming process and the resin layer formation process are the same in the manufacturing method. However, it differs from Example 1 in that an etching process is carried out instead of the secondary electroforming process.

[0043] In the etching process, as shown in FIG. 8(a), the primary pattern resist 24 and Then, a negative type second photoresist layer 28 is formed on the surface of the primary electroforming layer 25. An etching pattern film 38 (photomask) is applied on the second photoresist layer 28. The etching pattern film 38 has a light transmitting hole corresponding to the receiving recess 16A. Next, ultraviolet light is irradiated from the ultraviolet lamp 23 to form an etching pattern. The second photoresist layer 28 is exposed through the film 38. After exposure, the second photoresist The etching pattern film 38 is removed from the second photoresist layer 28. The unexposed parts are dissolved and removed (developed) to leave the primary pattern as shown in Figure 8(b). An etching pattern resist 39 is formed on the resist 24 and the primary electroforming layer 25 . The etching pattern resist 39 is composed of a resist body corresponding to the receiving recess 16A. do.

[0044] Next, as shown in FIG. 8(c), the area not covered with the etching pattern resist 39 is The surface of the primary electroforming layer 25 is etched to form a receiving recess in the primary electroforming layer 25. After the etching process, the etching pattern resist 39 is removed, and When the electroforming matrix 20 is then removed, the mask precursor shown in FIG. 8(d) can be obtained.

[0045] In this embodiment, the upper layer 1 is composed of only the first metal layer 11. Since the structural strength of the upper layer 1 of the first embodiment is improved compared to that of the upper layer 1 of the first embodiment, which is composed of the layers 11 and 12, the present embodiment can be carried out. The resistance to bending deformation can be improved as compared with the printing masks of Examples 1 and 2.

[0046] Example 4 FIGS. 9 to 12 show a screen printing mask according to the present invention (hereinafter, simply referred to as a printing mask). In this embodiment, the configuration of the bite portion 13 is the same as in the first embodiment. Specifically, as shown in FIG. 9, a biting protrusion 15B (15) is formed on the upper layer 1. The lower layer 2 has a receiving recess 16B (16). The upper layer 1 is made of metal and has a thickness of A relatively large upper first metal layer 11 and a relatively small lower second metal layer 12 The second metal layer 12 is formed by laminating the first metal On the lower surface of the layer 11, a lattice-like shape is formed between the adjacent adjustment openings 4, and this The upper surface of the lower layer 2 made of synthetic resin is formed of the metal layer 12 as a biting protrusion 15B. The receiving recess 16B (16) for receiving the biting protrusion 15B is formed in the The biting projection 15B bites into the receiving recess 16B, and the lower surface and rising surface of the biting projection 15B The portion 17 is covered with the lower layer 2. In this embodiment, the biting protrusion 15B provided on the upper layer 1 and The upper layer 1 partially penetrates into the lower layer 2 by the receiving recess 16B provided in the lower layer 2. The thickness of the first metal layer 11 is set to 18 μm, and the thickness of the lower layer 2 is set to 18 μm. The thickness is set to 3 μm. Therefore, the total thickness of the printing mask is set to 21 μm. The thickness of the second metal layer 12, ie, the protruding portion 15B, is set to 1.5 μm.

[0047] As described above, the receiving recess 16B (16) formed in the upper surface of the lower layer 2 and the upper layer 1 A protruding portion is formed between adjacent adjustment openings 4 on the lower surface and bites into the receiving recess 16B. The bite portion 13 formed by the protrusion 15B (15) is more bite-in than the conventional mask. The upper and lower layers 15B and 16B are in contact with each other by the outer peripheral side surface of the protrusion 15B and the inner peripheral side surface of the receiving recess 16B. Since the contact area of ​​2 can be increased, 1 and 2 can be firmly fixed in contact with each other. Since the proportion of the upper layer 1 made of a metal layer increases by the portion of the biting portion 13, the structural strength is increased. There is also the advantage that damage to the printing mask due to buckling can be suppressed.

[0048] An example of a method for manufacturing a printing mask according to this embodiment is shown in FIG. 10 to FIG. 12. The primary electroforming process shown in FIG. 10(a) to (d) and the secondary electroforming process shown in FIG. 11(a) to (d) The resin layer is formed through the steps of forming a resin layer shown in Fig. 12(a) to (c). As shown in FIG. 10(a), a conductive flat plate-shaped electroforming mold made of stainless steel is used. A negative type first photoresist layer 21 is then formed on the surface of the first photoresist layer 20. The first pattern film 22 is adhered to the top of the band layer 21. The first photoresist layer 21 is formed thicker in proportion to the thickness of the metal layer 11 .

[0049] Next, the inside of the oven of the ultraviolet irradiation device equipped with the ultraviolet lamp 23 is heated to the oven temperature during the exposure operation. After the preheating is completed, the laminate shown in FIG. 10(a) is placed in the furnace of the ultraviolet irradiation device. After the laminate is allowed to acclimate to the temperature inside the furnace, it is irradiated with ultraviolet light from an ultraviolet lamp 23. Thus, the first photoresist layer 21 is exposed through the first pattern film 22. The laminate after the irradiation is taken out, and the first pattern film 22 is removed from the first photoresist layer 21. The unexposed portion of the first photoresist layer 21 is dissolved and removed (developed), thereby forming a photoresist pattern. As shown in FIG. 10(b), a primary pattern resist 24 is formed on the electroforming matrix 20. The pattern resist 24 includes an adjustment opening 4 for the pattern opening 3 and an adjustment opening for the cut mark opening. The alignment hole is made of a resist material that corresponds to the opening of the alignment hole.

[0050] Next, as shown in FIG. 10(c), the electroformed portion not covered with the primary pattern resist 24 is By performing electroforming (plating) on ​​the surface of the matrix 20, the primary pattern resist 24 is highly A primary electroforming layer 25 that will become the first metal layer 11 is formed within the range of the thickness. After the primary electroforming layer 25 is formed The surfaces of the primary pattern resist 24 and the primary electroforming layer 25 are polished and smoothed, as shown in FIG. The state becomes 0(d).

[0051] In the secondary electroforming process, as shown in FIG. 11(a), a primary pattern resist 24 and Then, a negative type second photoresist layer 28 is formed on the surface of the primary electroforming layer 25. A second pattern film 29 is adhered to the second photoresist layer 28. The insulating film 29 is provided with a light transmitting hole corresponding to the second metal layer 12 (the bite-in protrusion 15B). Next, ultraviolet light is irradiated from the ultraviolet lamp 23 to cause ultraviolet light to be emitted through the second pattern film 29. After exposure, the second photoresist layer 28 is exposed to a second The pattern film 29 is removed, and the unexposed portion of the second photoresist layer 28 is dissolved and removed ( By performing the development process, as shown in FIG. 11(b), the primary pattern resist 24 and the primary pattern resist 25 are formed. A secondary pattern resist 30 is formed on the secondary electroforming layer 25. The secondary pattern resist 30 is , the second metal layer 12 is made of a resist material corresponding to the second metal layer 12 .

[0052] Next, as shown in FIG. 11(c), the primary pattern resist 30 that is not covered with the secondary pattern resist 30 is By performing electroforming (plating) on ​​the surface of the electroformed layer 25, the secondary pattern resist 30 is formed. A secondary electroformed layer 31 that will become the second metal layer 12 is formed within the height range. Formation of the secondary electroformed layer 31 Thereafter, the surfaces of the secondary pattern resist 30 and the secondary electroforming layer 31 are polished and smoothed, and then When the secondary pattern resist 30 is removed and the electroforming mold 20 is also removed, the result is as shown in FIG. The mask precursor shown in FIG. 1 can be obtained. After removing the secondary pattern resist 30, the surfaces of the secondary electroforming layer 31 and the secondary pattern resist 30 are polished. It is also possible to smooth the surface. Note that a recess corresponding to the second metal layer 12 (the protruding portion 15B) is formed. The electroforming mold is used to form a primary electroforming layer 25, which will become the second metal layer 12, in the recess in the primary electroforming process. After forming the first metal layer 11, a secondary electroforming layer 31 that becomes the first metal layer 11 is formed in a secondary electroforming process. Can

[0053] In the resin layer forming process, the mask precursor is temporarily fixed on a surface plate, and as shown in FIG. In this way, a photocurable emulsion resin (photocurable resin) 34 is poured onto the surface of the mask precursor body. The fluidity derived from the primary and secondary electroformed layers 25·31 and the primary pattern register are utilized. The emulsion resin 34 is evenly applied to the surface of the mold 24. Next, the third pattern is applied to the emulsion resin 34. Next, ultraviolet light is irradiated from the ultraviolet lamp 23 to form a third panel. The emulsion resin 34 is exposed to light through the turn film 35 and hardened. After hardening, the emulsion resin 34 Then, the third pattern film 35 is removed, and the uncured portion of the emulsion resin 34 is removed. As a result, as shown in FIG. 12(b), pattern openings are formed on the primary and secondary electroformed layers 25 and 31. A lower layer 2 is formed on the mask precursor, which has an opening corresponding to the primary pattern register 3. By removing the mask 24, the finished printing mask shown in FIG. 12(c) can be obtained. Cut.

[0054] Since the lower layer 2 in this embodiment is made of a photocurable resin, it is possible to form the lower layer 2 by a photolithography method. The lower layer 2 having a complex planar shape can be easily formed with high accuracy. The photocurable resin is formed from a photocurable emulsion resin 34. The surface on which the protruding portion 15B is formed is oriented upward, and a photocurable emulsion resin 34 is applied to the upper surface. By pouring the emulsion resin 34 into the mold, the biting protrusion 15B is covered with the fluidity derived from the emulsion. It can be easily applied to make the surface of the product smooth. It is then cured by irradiating it with light. By doing so, a lower layer 2 having a receiving recess 16B and a uniform thickness from the lower surface of the upper layer 1 can be obtained. In this embodiment, the electroforming matrix 20 is removed after the lower layer 2 is formed. But that's okay.

[0055] (Example 5) FIG. 13 shows a screen printing mask according to the present invention (hereinafter, simply referred to as a printing mask). In this embodiment, the shape of the biting protrusion 15B (15) is the same as that of the embodiment. Unlike the example 4, three (multiple) protrusions 15B are formed on the upper layer 1, and each protrusion 15B The receiving recesses 16B at both ends are formed in the lower layer 2. One side surface is open on the pattern opening 3 side. By providing a plurality of bite portions 13 in this way, Therefore, the contact area between the upper layer 1 and the lower layer 2 can be increased, so that the contact area between the upper layer 1 and the lower layer 2 can be further increased. It can be firmly attached and fixed.

[0056] As described above, in the printing mask of each of the above-mentioned examples, between the upper layer 1 and the lower layer 2, The upper layer 1 partially penetrates into the bite portion 13, or the lower layer 2 partially penetrates into the upper layer 1. The intruding biting portion 13 is provided, so in addition to the adhesive strength derived from the photocurable synthetic resin, The upper layer 1 and the lower layer 2 are bonded together by the bonding force that results from one of the layers 1 and 2 penetrating into the other. Therefore, compared with the conventional mask in which a resin layer is fixed to the flat surface of a metal layer, Since the upper and lower layers 1 and 2 are more firmly attached to each other, the damage caused by peeling of the upper and lower layers 1 and 2 is reduced. This can prevent damage to the disk.

[0057] The biting projection 15 and the receiving recess 16 constituting the biting portion 13 in each of the above-mentioned embodiments are formed without a step. However, it can be formed with multiple protrusions and recesses. The printing mask of the present invention is not limited to the above-mentioned embodiment. The present invention is not limited to the printing mask used for printing the internal electrodes of a capacitor. The mask structure is a deposition mask, a solder ball mounting mask, and a solder ball adsorption mask. It is also possible to repurpose it as a

[0058] FIG. 14 shows a screen printing mass in which an upper layer 1 made of metal and a lower layer 2 made of resin are laminated. In this reference example, the biting portion 13 of the present invention is not provided, and In Example 4, the lower layer 2 is formed only on the lower surface of the second metal layer 12. In the oil layer forming process, after applying the photo-curable emulsion resin 34, the second metal A pattern film corresponding to the layer 12 is attached to the substrate 12. The substrate 12 is irradiated with ultraviolet light by an ultraviolet lamp 23. After the emulsion resin 34 is exposed to light and hardened, the pattern film and the unhardened emulsion resin 34 are The photoresist-treated portion is then removed, and the printing mask according to the reference example is obtained. [Explanation of symbols]

[0059] 1 upper layer 2 Lower layer 3 Pattern opening 4 Adjustment aperture 13. Biting section 15 Biting protrusion 16 Receiving recess 17 Rising section 34 Emulsion Resin

Claims

1. a lower layer (2) made of resin having a group of pattern openings (3); a top layer (1) made of metal having a set of alignment openings (4) corresponding to the pattern openings (3); A biting portion (13) is provided between the upper layer (1) and the lower layer (2), The biting portion (13) includes a receiving recess (16) recessed between adjacent adjustment openings (4) on the lower surface of the upper layer (1), and a biting protrusion (15) protrudingly formed on the upper surface of the lower layer (2) and biting into the receiving recess (16), A screen printing mask characterized in that a slope is provided on the contact surface between a biting protrusion (15) and a receiving recess (16) at a rising portion (17) of the biting protrusion (15).

2. 2. A screen printing mask according to claim 1, wherein the opposing raised portions (17, 17) of the biting protrusion (15) are formed in a tapered shape that widens toward the protruding tip side.

3. 3. The screen printing mask according to claim 1, wherein the lower layer (2) is made of a photocurable resin or a thermosetting resin.

4. 4. The screen printing mask according to claim 3, wherein the lower layer (2) is made of a photocurable resin and is formed from a photocurable emulsion resin (34).

Citation Information

Patent Citations

  • Metal mask and manufacture thereof

    JP1997315026A

  • Mask for screen printing, its manufacture, and method for using it

    JP1999042867A

  • Screen mask, method for manufacturing thick film printing base using it and thick film printing base

    JP2004195858A

  • Mask and its manufacturing method

    JP2008162277A

  • Screen mask and method for producing screen mask

    JP2018144284A