Secondary battery and method of manufacturing the same, electrode member and method of manufacturing the same, and method of manufacturing current collector

The electrode member design with striped grooves and layered conductive structures addresses the risk of conductive layer detachment, ensuring improved performance and safety by releasing stress and maintaining structural integrity during manufacturing and operation.

JP7595688B2Active Publication Date: 2024-12-06CONTEMPORARY AMPEREX TECHNOLOGY (HONG KONG) LIMITED
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023003604
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-10-11
Filing Date
2023-01-13
Publication Date
2024-12-06
Estimated Expiration
2039-10-08

AI Technical Summary

Technical Problem

The risk of the conductive layer coming off the insulating substrate during the manufacturing process of secondary battery electrode members due to stress concentration and mismatched elastic properties between the insulating base and conductive layer, affecting the performance and safety of the electrode member.

Method used

The electrode member design includes a first conductive layer with striped grooves extending in the height direction, a second conductive layer with portions within and outside the grooves, and a protective layer, along with a manufacturing process that forms these layers and applies active and insulating materials to enhance bonding and stress relief.

Benefits of technology

The design effectively reduces the risk of the conductive layer detachment, ensures uniform active material distribution, and enhances the overall performance and safety of the secondary battery by releasing stress and maintaining structural integrity during manufacturing and operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595688000001
    Figure 0007595688000001
  • Figure 0007595688000002
    Figure 0007595688000002
  • Figure 0007595688000003
    Figure 0007595688000003
Patent Text Reader

Abstract

Provided are a secondary battery and a method for manufacturing the same, an electrode member and a method for manufacturing the same, and a current collector, which can reduce stress concentration, reduce the risk of a conductive layer coming off, and ensure the performance of the electrode member. [Solution] The electrode member (1) includes an insulating substrate (11), a first conductive layer (12), and an active material layer (13). The first conductive layer is provided on the surface of the insulating substrate, and the active material layer is provided on the side of the first conductive layer farther from the insulating substrate. The first conductive layer has stripe-shaped grooves extending in the height direction. The stripe-shaped grooves are used to release stress in the first conductive layer. A secondary battery includes an electrode assembly including the electrode member.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the field of batteries, and in particular to a secondary battery and a method for manufacturing the same, an electrode member and a method for manufacturing the same, and a method for manufacturing a current collector. [Background technology]

[0002] The electrode member of a secondary battery generally includes a current collector and an active material layer coated on the surface of the current collector. In order to improve the safety performance of the secondary battery, some electrode members select a current collector with a multi-layer structure, as shown in Figures 1 to 3, the current collector includes an insulating substrate 11 and a conductive layer 12 connected to the surface of the insulating substrate 11, and an active material layer 13 is coated on the surface of the conductive layer 12.

[0003] In the manufacturing process of the electrode member, it is necessary to roll press the active material layer 13 so as to make the active material layer 13 thin and increase the energy density. The insulating base 11 is made of a relatively soft material (e.g., PET plastic), while the conductive layer 12 is usually made of a metal material. The elastic modulus of the insulating base 11 is smaller than that of the conductive layer 12, so that the ductility of the insulating base 11 is higher than that of the conductive layer 12. In the process of the insulating base 11 expanding, the insulating base 11 applies a force to the conductive layer 12, but the connection force between the insulating base 11 and the conductive layer 12 is small, so that when the conductive layer 12 expands to a certain extent, the conductive layer 12 may come off the surface of the insulating base 11, which may affect the performance of the electrode member. Summary of the Invention [Problem to be solved by the invention]

[0004] The present invention has been made in consideration of the problems in the background art, and aims to provide a secondary battery and a manufacturing method thereof, an electrode member and a manufacturing method thereof, and a manufacturing method of a current collector that can reduce stress concentration, decrease the risk of a conductive layer coming off, and ensure the performance of the electrode member. [Means for solving the problem]

[0005] In order to achieve the above object, the present invention provides an electrode member for a secondary battery.

[0006] The electrode member includes an insulating base, a first conductive layer, and an active material layer. The first conductive layer is provided on a surface of the insulating base, and the active material layer is provided on a side of the first conductive layer farther from the insulating base. The first conductive layer is provided with stripe-shaped grooves extending in a height direction.

[0007] The electrode member further includes a second conductive layer having a first portion located in the stripe groove.

[0008] The second conductive layer is provided on a side of the first conductive layer away from the insulating base and further comprises a second portion connected to the first portion, and the active material layer is provided on a side of the second portion away from the first conductive layer.

[0009] The first conductive layer includes a main body on which the active material layer is applied and a protrusion extending from the main body on which the active material layer is not applied, The stripe-shaped groove includes a first groove formed in the protrusion, and at least a part of the second portion is located on a surface of the protrusion remote from the insulating base.

[0010] The stripe-shaped grooves further include a second groove formed in the main body portion, and the first groove and the second groove communicate with each other.

[0011] The electrode member further includes a protective layer provided on a surface of the second portion remote from the protrusion and connected to the active material layer, and the first groove does not protrude from the protective layer.

[0012] The second conductive layer has a stiffness less than the stiffness of the first conductive layer.

[0013] The stripe-shaped groove penetrates the first conductive layer along the thickness direction, and the first portion of the second conductive layer is connected to the insulating base.

[0014] The stripe-shaped grooves are plural, and the plural stripe-shaped grooves are arranged at intervals in the width direction.

[0015] In order to achieve the above object, the present invention further provides a secondary battery, comprising an electrode assembly including the electrode member.

[0016] In order to achieve the above object, the present invention further provides a method for producing a current collector, the method including the steps of preparing an insulating base, and adhering a conductive material to a surface of the insulating base to form a first conductive layer, the first conductive layer being provided with stripe-shaped grooves extending in a height direction.

[0017] The conductive material is fixed to the surface of the insulating substrate by vapor deposition or electroless plating.

[0018] The method for producing the current collector further includes applying a conductive slurry to a partial area of ​​the surface of the first conductive layer, filling the stripe-shaped grooves with the conductive slurry, and forming a second conductive layer after hardening the conductive slurry.

[0019] In order to achieve the above object, the present invention further provides a method for manufacturing an electrode member, which includes the steps of: preparing a current collector manufactured by the current collector manufacturing method; applying a slurry containing an active material to a partial area of ​​the surface of the first conductive layer and filling the striped grooves with the slurry containing the active material; forming an active material layer after hardening the slurry containing the active material, and roll-pressing the active material layer; welding a metal foil material to the area of ​​the first conductive layer where the active material layer is not applied; and removing a part of the metal foil material and a part of the current collector to form a plurality of spaced conductive structures and a plurality of spaced electrical guide portions.

[0020] The method for manufacturing the electrode member further includes applying a slurry containing an insulating material to a partial area of ​​a surface of the first conductive layer, and forming a protective layer after hardening the slurry containing the insulating material. The protective layer is formed before welding the metal foil material.

[0021] In order to achieve the above object, the present invention further provides a method for manufacturing a secondary battery, the method for manufacturing the secondary battery comprising: preparing a positive electrode member, a negative electrode member, and a diaphragm, winding the positive electrode member, the diaphragm, and the negative electrode member together to form an electrode assembly, at least one of the positive electrode member and the negative electrode member being manufactured by the method for manufacturing an electrode member, preparing an adapter piece, stacking a plurality of conductive structures of the electrode assembly and welding them to the adapter piece, preparing a top cover plate and an electrode terminal fixed to the top cover plate, welding the adapter piece to the electrode terminal, preparing a case, placing the electrode assembly in the case, and connecting the top cover plate to the case.

[0022] In order to achieve the above object, the present invention provides another method for manufacturing an electrode member, comprising the steps of: preparing a current collector manufactured by the current collector manufacturing method; applying a slurry containing an active material to a partial area of ​​a surface of the second conductive layer; forming an active material layer after hardening the slurry containing the active material, and roll-pressing the active material layer; welding a metal foil material to the area of ​​the first conductive layer where the second conductive layer is not applied; and removing a part of the metal foil material and a part of the current collector to form a plurality of spaced conductive structures and a plurality of spaced electrical guide portions.

[0023] The method for manufacturing the electrode member further includes applying a slurry containing an insulating material to a partial area of ​​a surface of the second conductive layer, and then curing the slurry containing the insulating material to form a protective layer before welding the metal foil material.

[0024] In order to achieve the above object, the present invention provides another method for manufacturing a secondary battery, which includes: preparing a positive electrode member, a negative electrode member, and a diaphragm, winding the positive electrode member, the diaphragm, and the negative electrode member together to form an electrode assembly, at least one of the positive electrode member and the negative electrode member being manufactured by the method for manufacturing another electrode member, preparing an adapter piece, stacking a plurality of conductive structures of the electrode assembly and welding them to the adapter piece, preparing a top cover plate and an electrode terminal fixed to the top cover plate, welding the adapter piece to the electrode terminal, preparing a case, placing the electrode assembly in the case, and connecting the cover plate to the case. Effect of the Invention

[0025] The present application has the following beneficial effects: In the present application, the first conductive layer is formed with stripe-shaped grooves, which effectively release the force applied to the first conductive layer, reduce stress concentration, and effectively reduce the risk of the first conductive layer coming off the surface of the insulating substrate, thereby ensuring the performance of the electrode member. [Brief description of the drawings]

[0026] [Figure 1] FIG. 1 is a schematic diagram of an electrode member according to the prior art. [Diagram 2] FIG. 2 is a schematic diagram showing a process of roll-pressing the electrode member of FIG. 1. [Diagram 3] 2 is a schematic diagram of an insulating base material and a conductive layer of the electrode member in FIG. 1 before roll pressing. FIG. [Figure 4] 2 is a schematic diagram of the insulating substrate and the conductive layer of the electrode member in FIG. 1 after roll pressing. FIG. [Diagram 5] 1 is a schematic diagram of a secondary battery according to the present invention. [Figure 6] 1 is a cross-sectional view of an electrode assembly according to the present invention. [Figure 7] FIG. 1 is a schematic diagram of a first embodiment of an electrode member according to the present invention. [Figure 8] FIG. 8 is a cross-sectional view taken along line AA in FIG. [Figure 9] FIG. 8 is a schematic diagram of the electrode member of FIG. 7 during molding. [Figure 10] 8 is another schematic view of the electrode member of FIG. 7 during molding. FIG. [Figure 11] FIG. 11 is a schematic view of the first conductive layer of FIG. 10 after roll pressing. [Figure 12] 8 is yet another schematic view of the electrode member of FIG. 7 during molding. FIG. [Figure 13] FIG. 8 is a schematic diagram of the electrode member in FIG. 7 after being wound. [Figure 14] FIG. 4 is a schematic diagram of a second embodiment of an electrode member according to the present invention. [Figure 15] FIG. 15 is a cross-sectional view taken along line BB in FIG. [Figure 16] 16 is a schematic diagram of the insulating base and the first conductive layer in FIG. 15. [Figure 17] FIG. 4 is a schematic diagram of a third embodiment of an electrode member according to the present invention. [Figure 18] FIG. 18 is a cross-sectional view taken along line CC in FIG. [Figure 19] FIG. 11 is a schematic diagram of a fourth embodiment of an electrode member according to the present invention. [Figure 20] FIG. 20 is a cross-sectional view taken along line DD in FIG. 19. [Figure 21] 20 is a schematic diagram of a first conductive layer of the electrode member of FIG. 19. [Figure 22] FIG. 11 is a schematic diagram of a fifth embodiment of an electrode member according to the present invention. [Figure 23] 23 is a cross-sectional view taken along line EE in FIG. 22. [Figure 24] 23 is a schematic diagram of a first conductive layer of the electrode member of FIG. 22. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0027] The technical solutions in the embodiments of the present application will be clearly and completely described below with reference to the drawings in the embodiments of the present application. Obviously, the described embodiments are only a part of the embodiments of the present application, not all the embodiments. The following description of at least one exemplary embodiment is merely exemplary in nature, and does not limit the present application and its application or use. Based on the embodiments of the present application, all other embodiments obtained by those skilled in the art without performing creative work are included in the protection scope of the present application.

[0028] In the description of this application, the use of terms such as "first" and "second" to define components is intended to facilitate distinction between the components, and unless otherwise specified, the above terms do not have any particular meaning and should not be construed as limiting the scope of protection of this application.

[0029] The secondary battery of the present invention includes an electrode assembly. Referring to Fig. 6, the electrode assembly includes a positive electrode member 2, a negative electrode member 3, and a diaphragm 4 provided between the positive electrode member 2 and the negative electrode member 3. The positive electrode member 2, the diaphragm 4, and the negative electrode member 3 are laminated and wound in a flat shape. The electrode assembly is a core component for realizing the charge / discharge function of the secondary battery.

[0030] The secondary battery of the present invention may be a soft-pack battery in which an electrode assembly formed by winding the positive electrode member 2, the diaphragm 4, and the negative electrode member 3 is directly sealed in a packaging bag. The packaging bag may be made of aluminum plastic film.

[0031] Of course, the secondary battery of the present application may be a hard-shell battery. Specifically, referring to FIG. 5, the secondary battery mainly includes an electrode assembly, a case 5, a top cover plate 6, an electrode terminal 7, and an adapter piece 8.

[0032] The case 5 may have a hexahedral shape or another shape. A cavity for accommodating the electrode assembly and the electrolyte is formed inside the case 5. The case 5 has an opening at one end, and the electrode assembly may be placed in the accommodation chamber of the case 5 through the opening. The case 5 may be made of a conductive metal material such as aluminum or an aluminum alloy, or may be made of an insulating material such as plastic.

[0033] The top cover plate 6 is provided on the case 5 and covers the opening of the case 5, thereby enclosing the electrode assembly within the case 5. The electrode terminal 7 is provided on the top cover plate 6, and the upper end of the electrode terminal 7 protrudes above the top cover plate 6 and the lower end extends through the top cover plate 6 into the case 5. The adapter piece 8 is provided inside the case 5 and fixed to the electrode terminal 7. There are two electrode terminals 7 and two adapter pieces 8, and the positive electrode member 2 is electrically connected to one electrode terminal 7 via one adapter piece 8, and the negative electrode member 3 is electrically connected to the other electrode terminal 7 via the other adapter piece 8. The adapter piece 8 is welded to the electrode terminal 7.

[0034] In the secondary battery, at least one of the positive electrode member 2 and the negative electrode member 3 uses an electrode member 1 which will be described later.

[0035] 7 to 13 are schematic diagrams of a first embodiment of an electrode member 1 according to the present invention. With reference to Fig. 7 and Fig. 8, the electrode member 1 of the first embodiment includes an insulating base 11, a first conductive layer 12, and an active material layer 13. The first conductive layer 12 is provided on both sides of the insulating base 11, and the active material layer 13 is provided on the side of the first conductive layer 12 remote from the insulating base 11.

[0036] The material of the insulating base material 11 may be a PET (polyethylene terephthalate) film or a PP (polypropylene) film.

[0037] The material of the first conductive layer 12 is at least one of a metal conductive material and a carbon-based conductive material. The metal conductive material is preferably at least one of aluminum, copper, nickel, titanium, silver, a nickel-copper alloy, and an aluminum-zirconium alloy. The carbon-based conductive material is preferably at least one of graphite, acetylene black, graphene, and carbon nanotubes.

[0038] The first conductive layer 12 can be formed on the surface of the insulating base 11 by at least one of a vapor deposition method and an electroless plating method. Among these, as the vapor deposition method, a physical vapor deposition method (PVD), for example, a thermal evaporation deposition method, is preferable.

[0039] The active material layer 13 can also be provided by coating on the surface of the first conductive layer 12. The active material layer 13 can be formed by making a slurry from an active material such as lithium manganate or lithium iron phosphate, an adhesive, a conductive agent, and a solvent, coating the slurry on the outer surfaces of the two first conductive layers 12, and curing the slurry.

[0040] 9, the first conductive layer 12 is provided with stripe-shaped grooves G that extend substantially along the height direction Z and release stress in the first conductive layer 12. The length of the stripe-shaped grooves G along the width direction X is 0.001 mm to 1 mm, and is sufficiently shorter than the length of the stripe-shaped grooves G along the height direction Z. The stripe-shaped grooves G may be linear or curved, and may extend substantially along the height direction Z as a whole; that is, there may be a small angle between the extension direction of the stripe-shaped grooves G and the height direction Z (for example, the angle may be less than 10°).

[0041] The thickness of the insulating base 11 can be 1 μm to 20 μm, and the thickness of the first conductive layer 12 can be 0.1 μm to 10 μm. Since the first conductive layer 12 is thin, burrs generated on the first conductive layer 12 when the electrode member 1 is cut are small, and it is difficult to break through the diaphragm 4 of several tens of μm, so that a short circuit can be avoided and safety performance can be improved. In addition, when a foreign object breaks through the electrode member 1 of the secondary battery, since the thickness of the first conductive layer 12 is small, burrs generated at the place where the foreign object breaks through the first conductive layer 12 are small, and it is difficult to break through the diaphragm 4, so that a short circuit can be avoided and safety performance can be improved.

[0042] The first conductive layer 12 has a main body portion 121 to which the active material layer 13 is applied, and a protrusion 122 extending from the main body portion 121 to which the active material layer 13 is not applied. The active material layer 13 may be applied directly to the surface of the main body portion 121. Of course, another material may alternatively be provided between the main body portion 121 and the active material layer 13.

[0043] The protrusions 122 and the portions of the insulating base 11 corresponding to the protrusions 122 form an electrical guide portion P. The electrical guide portions P may be arranged at intervals in the width direction X. With reference to Fig. 13, when the electrode member 1 is rolled, the electrical guide portions P are arranged in a stacked manner in the thickness direction Y.

[0044] The electrode member 1 further includes a protective layer 15 provided on the side of the protrusion 122 remote from the insulating base 11 and connected to the active material layer 13 .

[0045] The protective layer 15 includes an adhesive and an insulating material. The insulating material includes at least one of aluminum trioxide and aluminum oxyhydroxide. The adhesive, the insulating material, and a solvent are mixed to prepare a slurry that is applied to the surface of the protrusion 122 and cured to form the protective layer 15. The hardness of the protective layer 15 is greater than the hardness of the protrusion 122.

[0046] The electrode member 1 further includes a conductive structure 16 welded to an area of ​​the protrusion 122 that is not covered by the protective layer 15. With reference to Figs. 7 and 8, a conductive structure 16 is fixed to both sides of each electrical guide portion P in the thickness direction Y. With reference to Fig. 13, after the electrode member 1 is wound and formed, all the conductive structures 16 are stacked and welded to the adapter piece 8 at the same time. With reference to Fig. 5, the current in the electrode member 1 can be output to the outside via the adapter piece 8 and the electrode terminal 7.

[0047] The electrode member 1 of the first embodiment can be formed by the following steps.

[0048] (1) A composite tape material is produced by forming a first conductive layer 12 by vapor deposition or electroless plating on the surface of an insulating substrate 11. As shown in Fig. 9, stripe-shaped grooves G are formed in advance in the first conductive layer 12 during the molding process.

[0049] (2) Referring to FIG. 10, active material layer 13 and protective layer 15 are simultaneously applied to the surface of first conductive layer 12.

[0050] (3) Active material layer 13 is roll-pressed to compact active material layer 13 and increase its density.

[0051] (4) Referring to FIG. 12, after roll pressing, a metal foil material (e.g., aluminum foil) is welded to the first conductive layer 12, and then a plurality of electrical guide portions P and a plurality of conductive structures 16 are cut out along the dashed lines in FIG. 12, thereby obtaining the electrode member 1 shown in FIG. 7.

[0052] In step (1), first conductive layer 12 can be formed on the surface of insulating base 11 by vapor phase growth or electroless plating. Therefore, the connection strength between first conductive layer 12 and insulating base 11 is small, and there is a risk that first conductive layer 12 may be easily peeled off from the surface of insulating base 11 due to an external force.

[0053] Since the elastic modulus of the insulating base 11 is smaller than that of the first conductive layer 12, the ductility of the insulating base 11 is higher than that of the first conductive layer 12. In step (3), the insulating base 11 is pressurized and stretched, and since the insulating base 11 has high ductility, the insulating base 11 applies a force to the first conductive layer 12. In the conventional technology, the force applied to the first conductive layer 12 cannot be released, so when the first conductive layer 12 stretches to a certain extent, the force applied to the first conductive layer 12 becomes larger than the connection force between the insulating base 11 and the first conductive layer 12, and the insulating base 11 and the first conductive layer 12 slide relative to each other, and the first conductive layer 12 comes off the surface of the insulating base 11, which affects the performance of the electrode member 1.

[0054] In the present application, a stripe-shaped groove G is formed in the first conductive layer 12, and the stripe-shaped groove G effectively releases the force applied to the first conductive layer 12, reduces stress concentration, and prevents the force applied to the first conductive layer 12 from being too large, thereby effectively reducing the risk of the first conductive layer 12 coming off the surface of the insulating base 11, and ensuring the performance of the electrode member 1.

[0055] 11 shows the state in which the first conductive layer 12 has been roll-pressed, and the dashed line shows the state of the stripe-shaped grooves G before being roll-pressed. In the roll-pressing step (3), the force applied to the first conductive layer 12 is gradually concentrated on the stripe-shaped grooves G, and when the force applied to the first conductive layer 12 is large, the first conductive layer 12 is torn along the stripe-shaped grooves G by the force, so that the stress is quickly released and it is possible to prevent the force applied to the first conductive layer 12 from being greater than the connection force between the insulating base 11 and the first conductive layer 12, thereby reducing the probability of the insulating base 11 and the first conductive layer 12 sliding relative to each other, and ensuring the performance of the electrode member 1.

[0056] In use of the secondary battery, the current generated in the active material layer 13 flows through the main body 121 to the protrusion 122, i.e., the current flows through the first conductive layer 12 approximately along the height direction Z, so that the overcurrent area of ​​the first conductive layer 12 depends on the area of ​​the cross section perpendicular to the height direction Z of the first conductive layer 12. In the present application, the stripe-shaped groove G extends approximately along the height direction Z, and the length of the width direction X is small. That is, the dimension of the stripe-shaped groove G along the height direction Z is larger than the dimension of the stripe-shaped groove G along the width direction X. Therefore, when the first conductive layer 12 is torn along the stripe-shaped groove G during the roll press process, the stripe-shaped groove G has little effect on the overcurrent area of ​​the first conductive layer 12, and thus the overcurrent capacity of the first conductive layer 12 can be sufficiently ensured.

[0057] In step (3), as the roll press proceeds, the force applied to the first conductive layer 12 gradually increases. Referring to FIG. 11, when the electrode member 1 is roll pressed at a certain length along the width direction X, the force applied to the first conductive layer 12 tears the first conductive layer 12 along the stripe-shaped grooves G, and the stress is quickly released. Since the first conductive layer 12 has a long length in the width direction X, it is preferable that the stripe-shaped grooves G are multiple and arranged at intervals in the width direction X. The multiple stripe-shaped grooves G can gradually release the stress during the roll press, and prevent the force applied to the first conductive layer 12 from becoming larger than the connection force between the insulating base 11 and the first conductive layer 12, thereby reducing the probability that the insulating base 11 and the first conductive layer 12 slide relative to each other, and ensuring the performance of the electrode member 1.

[0058] 8 and 9, the stripe-shaped grooves G penetrate the first conductive layer 12 in the thickness direction Y, i.e., the depth of the stripe-shaped grooves G is equal to the thickness of the first conductive layer 12 in the thickness direction Y. At this time, the first conductive layer 12 becomes easily torn along the stripe-shaped grooves G during roll pressing, and stress is quickly released.

[0059] In step (2), the active material layer 13 can be filled into the striped grooves G, so that the current on the active material layer 13 can flow to the first conductive layer 12 through the peripheral walls of the striped grooves G, thereby improving the current collecting ability of the first conductive layer 12. In step (3), even if the first conductive layer 12 is torn along the striped grooves G, the active material layer 13 is filled up to the torn parts by the force of the roll press.

[0060] Since the elastic modulus of the insulating base 11 is small, in step (3), the insulating base 11 corresponding to the main body 121 spreads under the protrusion 122, causing the insulating base 11 inside the protrusion 122 to swell and deform, making the protrusion 122 more susceptible to deformation by the acting force of the insulating base 11 and causing cracks. On the other hand, in the present application, the protective layer 15 has high strength and provides a supporting force to the protrusion 122 in the process of roll-pressing the electrode member 1, restricting the deformation of the protrusion 122, reducing the probability of cracks occurring in the protrusion 122, and improving the overcurrent capability of the electrode member 1.

[0061] Since there is a risk that the protrusions 122 may come off due to vibration or the like during operation of the secondary battery, by connecting the protective layer 15 to the active material layer 13, the protective layer 15 can be fixed to the active material layer 13, the bonding force of the protective layer 15 to the electrode member 1 is increased, the earthquake resistance is improved, and it is possible to prevent the protective layer 15 from coming off together with the protrusions 122. At the same time, since the protrusions 122 are most likely to swell near the base of the active material layer 13 (i.e., the boundary between the protrusions 122 and the main body portion 121), when the protective layer 15 and the active material layer 13 are connected, the deformation of the protrusions 122 is reduced, the probability of cracks occurring is reduced, and the overcurrent capability of the electrode member 1 can be improved.

[0062] Next, four other embodiments will be described. For simplicity, only the differences between the first embodiment and the other four embodiments will be described below, and the differences between the first embodiment and the other four embodiments will be described below with reference to the first embodiment.

[0063] 14 to 16 are schematic diagrams showing a second embodiment of an electrode member according to the present invention. With reference to Fig. 14 and Fig. 16, the depth of the stripe-shaped groove G along the thickness direction Y is smaller than the thickness of the first conductive layer 12. Compared to the first embodiment, the first conductive layer 12 of the second embodiment has a larger overcurrent area. The cross section of the stripe-shaped groove G may be U-shaped or V-shaped.

[0064] 17 and 18 are schematic diagrams showing a third embodiment of the electrode member according to the present invention. Referring to FIG. 17 and FIG. 18, the electrode member 1 of the third embodiment further includes a second conductive layer 14 having a first portion 141 located in the stripe-shaped groove G, compared with the first embodiment. The first portion 141 is filled in the stripe-shaped groove G, and the current around the stripe-shaped groove G can be transmitted through the first portion 141. In other words, the first portion 141 can restore the conductive area of ​​the first conductive layer 12, increase the overcurrent area, and ensure the overall overcurrent capacity of the electrode member 1.

[0065] In the first embodiment, since the active material layer 13 is filled in the striped grooves G, the distribution of the active material layer 13 is not uniform, that is, the thickness of the active material layer 13 in the striped grooves G is thicker than the thickness of other portions. During operation of the secondary battery, the active material layer 13 may dissolve lithium at positions corresponding to the striped grooves G. In the third embodiment, the first portions 141 are filled in the striped grooves G, thereby ensuring the flatness of the first conductive layer 12, improving the uniformity of the distribution of the active material layer 13, and reducing the risk of lithium dissolution.

[0066] The second conductive layer 14 is provided on the side of the first conductive layer 12 away from the insulating base 11 and further includes a second portion 142 connected to the first portion 141, and the active material layer 13 is provided on the surface of the second portion 142 away from the first conductive layer 12.

[0067] The second conductive layer 14 may be a metal material or a nonmetal material. The second conductive layer 14 is preferably a nonmetal material that is less likely to generate burrs in order to reduce burrs that are generated when a foreign object breaks through the electrode member 1. Specifically, first, conductive carbon, an adhesive, and a solvent are made into a slurry, and the slurry is applied to the first conductive layer 12 and hardened to form the second conductive layer 14. During application, the slurry is filled in the stripe-shaped grooves G to form the first portions 141.

[0068] In step (2), the slurry for second conductive layer 14 may be applied to first conductive layer 12, and then the slurry for active material layer 13 and the slurry for protective layer 15 may be applied to the surface of second conductive layer 14.

[0069] In step (3), even if the first conductive layer 12 is torn along the stripe-shaped groove G, the second portion 142 is filled up to the torn portion by the force of the roll press, thereby repairing the conductive area of ​​the first conductive layer 12, increasing the overcurrent area, and ensuring the overall overcurrent capacity of the electrode member 1.

[0070] When the second conductive layer 14 is provided only on the surface of the first conductive layer 12, the current of the second conductive layer 14 is only conducted to the first conductive layer 12 via the surface of the first conductive layer 12. In the present application, the first portion 141 of the second conductive layer 14 is embedded in the stripe-shaped groove G of the first conductive layer 12, so that the current is not only conducted to the first conductive layer 12 via the surface of the first conductive layer 12 but also conducted via the peripheral wall of the stripe groove G, thereby increasing multiple conductive paths, forming conductive areas at multiple locations, improving the conductive performance of the electrode member 1, reducing polarization of the electrode member 1 and the secondary battery, and improving the high-rate charge / discharge performance of the secondary battery.

[0071] The second portion 142 is at least partially disposed on a surface of the protrusion 122 remote from the insulating base 11. A protective layer 15 may be provided on a surface of the second portion 142 remote from the protrusion 122. The conductive structure 16 is welded to an area of ​​the protrusion 122 not covered by the second portion 142.

[0072] In step (3), the main body 121 is expanded by the insulating base material 11, but the protrusions 122 are hardly expanded. The main body 121 and the insulating base material 11 apply force to the protrusions 122 when expanding, but because the protrusions 122 are thin, the force causes microcracks in the protrusions 122. In contrast, in the present application, the second portions 142 are provided on the surfaces of the protrusions 122, so that even if cracks occur in the process of the protrusions 122 being roll-pressed, the current in the cracks can flow to the outside via the second portions 142, thereby realizing the repair of the conductive area and ensuring the overcurrent capacity of the entire electrode member 1.

[0073] The rigidity of the second conductive layer 14 is lower than the rigidity of the first conductive layer 12. That is, the second conductive layer 14 is more likely to deform when a force is applied. When the protrusion 122 deforms, the second portion 142 also deforms along with the protrusion 122. Even if the protrusion 122 deforms too much and tears, the second portion 142 will not tear, and the transmission of current is ensured.

[0074] The stripe-shaped grooves G penetrate the first conductive layer 12 in the thickness direction Y, and the first portion 141 of the second conductive layer 14 is connected to the insulating base 11. The first portion 141 is fitted into the stripe-shaped grooves G and adhered to the insulating base 11, thereby increasing the connection strength between the first conductive layer 12, the second conductive layer 14, and the insulating base 11.

[0075] 19 to 21 are schematic diagrams showing a fourth embodiment of an electrode member according to the present invention. With reference to Fig. 19 to 21, the stripe-shaped grooves G of the fourth embodiment include a first groove G1 formed in the protrusion 122, as compared with the third embodiment.

[0076] In step (3), the portion of the insulating base 11 corresponding to the main body 121 is roll-pressed and stretched, and the portion of the insulating base 11 corresponding to the main body 121 applies force to the portion of the insulating base 11 corresponding to the protrusion 122, thereby stretching the portion of the insulating base 11 corresponding to the protrusion 122. On the other hand, the protrusion 122 is hardly stretched because it is restricted by the protective layer 15, and the portion of the insulating base 11 corresponding to the protrusion 122 applies force to the protrusion 122 during stretching. If the force applied is greater than the connecting force between the insulating base 11 and the protrusion 122, the protrusion 122 is likely to come off the insulating base 11. In contrast, in the present application, the first groove G1 effectively releases the force applied to the protrusion 122, reduces stress concentration, prevents the force applied to the protrusion 122 from becoming excessive, effectively reduces the probability of the protrusion 122 coming off, and ensures the performance of the electrode member 1.

[0077] Preferably, the first groove G1 does not protrude from the protective layer 15 in the direction away from the active material layer 13. The area of ​​the protrusion 122 covered by the protective layer 15 receives the greatest stress, and therefore the first groove G1 may be provided in the area of ​​the protrusion 122 covered by the protective layer 15. On the other hand, the area of ​​the protrusion 122 not covered by the protective layer 15 receives a small force and is unlikely to come off; however, if the first groove G1 extends to the area of ​​the protrusion 122 not covered by the protective layer 15, the overcurrent capability of the protrusion 122 will be reduced.

[0078] The stripe-shaped grooves G further include a second groove G2 formed in the main body portion 121, and the first groove G1 and the second groove G2 communicate with each other.

[0079] In step (3), the main body 121 expands due to the force applied by the insulating base 11. The protrusion 122 is restricted by the protective layer 15, and the protrusion 122 does not expand much, so that the region of the main body 121 close to the protrusion 122 receives the reaction force of the protrusion 122. In other words, the region of the main body 121 close to the protrusion 122 receives the acting forces of the insulating base 11 and the protrusion 122 at the same time, so that the region of the main body 121 close to the protrusion 122 is likely to come off from the insulating base 11. In contrast, in the present application, the second groove G2 extends to the region of the main body 121 close to the protrusion 122, so that the force applied to the main body 121 is effectively released, stress concentration is reduced, and the probability of the insulating base 11 and the main body 121 sliding relative to each other is effectively reduced, and the performance of the electrode member 1 is ensured.

[0080] The stripe-shaped grooves G include a plurality of third grooves G3 formed in the main body 121 and arranged at intervals in the width direction X. In the width direction X, each third groove G3 is located between two adjacent second grooves G2, and in the height direction Z, the third grooves G3 and the second grooves G2 are offset from each other.

[0081] 22 to 24 are schematic diagrams showing a fifth embodiment of an electrode member according to the present invention. With reference to Fig. 22 to 24, the stripe-shaped grooves G of the fifth embodiment include a third groove G3 and a fourth groove G4 formed in a main body portion 121. There are multiple third grooves G3 and they are spaced apart in the width direction X, and there are multiple fourth grooves G4 and they are spaced apart in the width direction X.

[0082] In the width direction X, each third groove G3 is located between two adjacent fourth grooves G4. In the height direction Z, the third groove G3 and the fourth groove G4 are offset from each other. The third groove G3 and the fourth groove G4 are arranged in a dispersed manner in the width direction X and the height direction Z, which can improve the effect of releasing stress and improve uniformity.

[0083] The present application provides a method for manufacturing a secondary battery that can further improve the safety performance of the secondary battery. The method for manufacturing a secondary battery includes preparing a positive electrode member 2, a negative electrode member 3, and a diaphragm 4, winding the positive electrode member 2, the diaphragm 4, and the negative electrode member 3 together to form an electrode assembly, using the electrode member 1 for at least one of the positive electrode member 2 and the negative electrode member 3, preparing an adapter piece 8, stacking a plurality of conductive structures 16 of the electrode assembly and welding them to the adapter piece 8, preparing a top cover plate 6 and an electrode terminal 7 fixed to the top cover plate 6, welding the adapter piece 8 to the electrode terminal 7, preparing a case 5, placing the electrode assembly in the case 5, and connecting the top cover plate 6 to the case 5.

[0084] In the electrode member 1 used in the fabricated secondary battery, the thickness of the first conductive layer 12 is thin, and when a foreign object breaks through the electrode member 1 of the secondary battery, the first conductive layer 12 generates small burrs at the breakthrough point, making it difficult for the foreign object to break through the diaphragm 4, thus avoiding a short circuit and improving safety performance. In addition, the first conductive layer 12 has stripe-shaped grooves G formed therein, which effectively release the force applied to the first conductive layer 12, reduce stress concentration, and effectively reduce the risk of the first conductive layer 12 coming off the surface of the insulating base 11, thereby ensuring the performance of the electrode member 1 and the secondary battery. [Explanation of symbols]

[0085] In the following, reference numerals will be used to explain the drawing. 1 electrode member, 5 case, 11 insulating base, 6 top cover plate, 12 first conductive layer, 7 electrode terminal, 121 main body, 8 adapter piece, 122 protrusion, 9 roller, 13 active material layer, G stripe-shaped groove, 14 second conductive layer, G1 first groove, 141 first portion, G2 second groove, 142 second portion, G3 third groove, 15 protective layer, G4 fourth groove, 16 conductive structure, P electrical guide portion, 2 positive electrode member, X width direction, 3 negative electrode member, Y thickness direction, 4 diaphragm, Z height direction.

Claims

1. An electrode member (1) for a secondary battery, the electrode member (1) comprising: The battery includes an insulating substrate (11), a first conductive layer (12), and an active material layer (13), the first conductive layer (12) is provided on a surface of the insulating base (11), and the active material layer (13) is provided on a side of the first conductive layer (12) farther from the insulating base (11); The first conductive layer (12) is provided with a stripe-shaped groove (G) extending in a height direction (Z) of the electrode member (1), The first conductive layer (12) includes a main body portion (121) and a protrusion portion (122) extending from the main body portion (121), The stripe-shaped groove (G) includes a first groove (G1) formed in the protrusion (122), The stripe-shaped groove (G) further includes a second groove (G2) formed in the main body portion (121), and the first groove (G1) and the second groove (G2) are in communication with each other; The stripe-shaped grooves (G) further include a plurality of third grooves (G3) formed in the main body portion (121) and arranged at intervals in the width direction (X) of the electrode member (1), In the width direction (X) of the electrode member (1), each of the third grooves (G3) is located between two adjacent second grooves (G2), and in the height direction (Z) of the electrode member (1), the third grooves (G3) and the second grooves (G2) are offset from each other. An electrode member (1).

2. The second conductive layer (14) further includes a first portion (141) located in the stripe-shaped groove (G). Electrode member (1) according to claim 1 .

3. the second conductive layer (14) is provided on a surface of the first conductive layer (12) remote from the insulating base (11) and further includes a second portion (142) connected to the first portion (141), and the active material layer (13) is provided on a surface of the second portion (142) remote from the first conductive layer (12); Electrode member (1) according to claim 2.

4. The active material layer (13) is applied to the main body portion (121), and the active material layer (13) is not applied to the protrusion portion (122), At least a portion of the second portion (142) is located on a surface of the protrusion (122) away from the insulating base (11). Electrode member (1) according to claim 3.

5. The insulating substrate (11) is provided on a side of the protrusion (122) away from the insulating substrate (11) and is connected to the active material layer (13). The first groove (G1) does not protrude from the protective layer (15); Electrode member (1) according to any one of claims 1 to 4.

6. The stiffness of the second conductive layer (14) is less than the stiffness of the first conductive layer (12); Electrode member (1) according to claim 2.

7. A depth of the stripe-shaped groove (G) along a thickness direction (Y) of the electrode member (1) is smaller than a thickness of the first conductive layer (12). Electrode member (1) according to any one of claims 1 to 6.

8. the stripe-shaped groove (G) penetrates the first conductive layer (12) along the thickness direction (Y) of the electrode member (1), and the first portion (141) of the second conductive layer (14) is connected to the insulating base (11); Electrode member (1) according to claim 2.

9. An electrode member (1) for a secondary battery, the electrode member (1) comprising: The battery includes an insulating substrate (11), a first conductive layer (12), and an active material layer (13), the first conductive layer (12) is provided on a surface of the insulating base (11), and the active material layer (13) is provided on a side of the first conductive layer (12) farther from the insulating base (11); The first conductive layer (12) is provided with a stripe-shaped groove (G) extending in a height direction (Z) of the electrode member (1), The first conductive layer (12) includes a main body portion (121) and a protrusion portion (122) extending from the main body portion (121), The stripe-shaped grooves (G) include a third groove (G3) and a fourth groove (G4) formed in the main body portion (121), the third grooves (G3) are multiple and are arranged at intervals in the width direction (X) of the electrode member (1), the fourth grooves (G4) are multiple and are arranged at intervals in the width direction (X) of the electrode member (1), In the width direction (X) of the electrode member (1), each of the third grooves (G3) is located between two adjacent fourth grooves (G4), and in the height direction (Z) of the electrode member (1), the third groove (G3) and the fourth groove (G4) are offset from each other, and the third groove (G3) and the fourth groove (G4) are disposed in a dispersed manner in the width direction (X) and height direction (Z) of the electrode member (1); The second conductive layer (14) further includes a first portion (141) located in the stripe-shaped groove (G). An electrode member (1).

10. the second conductive layer (14) is provided on a surface of the first conductive layer (12) remote from the insulating base (11) and further includes a second portion (142) connected to the first portion (141), and the active material layer (13) is provided on a surface of the second portion (142) remote from the first conductive layer (12); 10. An electrode member (1) according to claim 9.

11. The active material layer (13) is applied to the main body portion (121), and the active material layer (13) is not applied to the protrusion portion (122), At least a portion of the second portion (142) is located on a surface of the protrusion (122) away from the insulating base (11). Electrode member (1) according to claim 10.

12. The insulating layer (11) is provided on the side of the protrusion (122) away from the insulating base (11) and is connected to the active material layer (13). Electrode member (1) according to any one of claims 9 to 11.

13. The stiffness of the second conductive layer (14) is less than the stiffness of the first conductive layer (12); 10. An electrode member (1) according to claim 9.

14. A depth of the stripe-shaped groove (G) along a thickness direction (Y) of the electrode member (1) is smaller than a thickness of the first conductive layer (12). Electrode member (1) according to any one of claims 9 to 13.

15. the stripe-shaped groove (G) penetrates the first conductive layer (12) along the thickness direction (Y) of the electrode member (1), and the first portion (141) of the second conductive layer (14) is connected to the insulating base (11); 10. An electrode member (1) according to claim 9.

16. An electrode assembly including the electrode member (1) according to any one of claims 1 to 15. A secondary battery comprising:

17. A method for producing a current collector, the method comprising the steps of: Providing an insulating substrate (11); forming a first conductive layer (12) by adhering a conductive material to a surface of the insulating base (11), and providing a stripe-shaped groove (G) extending in a height direction (Z) of the current collector in the first conductive layer (12); The first conductive layer (12) includes a main body portion (121) and a protrusion portion (122) extending from the main body portion (121), The stripe-shaped groove (G) includes a first groove (G1) formed in the protrusion (122), The stripe-shaped groove (G) further includes a second groove (G2) formed in the main body portion (121), and the first groove (G1) and the second groove (G2) are in communication with each other; The stripe-shaped grooves (G) further include a plurality of third grooves (G3) formed in the main body portion (121) and arranged at intervals in the width direction (X) of the current collector, In a width direction (X) of the current collector, each of the third grooves (G3) is located between two adjacent second grooves (G2), and in a height direction (Z) of the current collector, the third grooves (G3) and the second grooves (G2) are shifted from each other. A manufacturing method comprising the steps of:

18. The conductive material is fixed to the surface of the insulating substrate (11) by vapor deposition or electroless plating. The method for producing a current collector according to claim 17 .

19. applying a conductive slurry to a surface of the main body (121) of the first conductive layer (12) and at least a part of the surface of the protrusion (122) and filling the stripe-shaped grooves with the conductive slurry; forming a second conductive layer (14) after curing of the conductive slurry; Further comprising: The method for producing a current collector according to claim 17 or 18.

20. A method for producing a current collector, the method comprising the steps of: Providing an insulating substrate (11); forming a first conductive layer (12) by adhering a conductive material to a surface of the insulating base (11), and providing a stripe-shaped groove (G) extending in a height direction (Z) of the current collector in the first conductive layer (12); The first conductive layer (12) includes a main body portion (121) and a protrusion portion (122) extending from the main body portion (121), The stripe-shaped grooves (G) include a third groove (G3) and a fourth groove (G4) formed in the main body portion (121), the third grooves (G3) are multiple and are arranged at intervals in the width direction (X) of the current collector, and the fourth grooves (G4) are multiple and are arranged at intervals in the width direction (X) of the current collector, In the width direction (X) of the current collector, each of the third grooves (G3) is located between two adjacent fourth grooves (G4), and in the height direction (Z) of the current collector, the third groove (G3) and the fourth groove (G4) are offset from each other, and the third groove (G3) and the fourth groove (G4) are disposed in a dispersed manner in the width direction (X) and height direction (Z) of the current collector, applying a conductive slurry to a surface of the main body (121) of the first conductive layer (12) and at least a part of the surface of the protrusion (122) and filling the stripe-shaped grooves with the conductive slurry; forming a second conductive layer (14) after curing of the conductive slurry; Further comprising: A manufacturing method comprising the steps of:

21. The conductive material is fixed to the surface of the insulating substrate (11) by vapor deposition or electroless plating. The method for producing a current collector according to claim 20 .

22. Preparing a current collector manufactured by the manufacturing method according to any one of claims 17 to 18 and 20 to 21; applying a slurry containing an active material to a surface of the main body portion (121) of the first conductive layer (12) and filling the stripe-shaped grooves (G) with the slurry containing the active material; forming an active material layer (13) after hardening the slurry containing the active material, and roll-pressing the active material layer (13); welding a metal foil material to an area of ​​the first conductive layer (12) where the active material layer (13) is not applied; removing a portion of the metal foil material and a portion of the current collector to form a plurality of spaced apart conductive structures (16) and a plurality of spaced apart electrical guide portions (P); A method for manufacturing an electrode member, comprising:

23. Applying a slurry containing an insulating material to a partial area of ​​a surface of the first conductive layer (12), and forming a protective layer (15) after hardening the slurry containing the insulating material; The protective layer (15) is formed before welding the metal foil material. The method for manufacturing an electrode member according to claim 22 .

24. a positive electrode member (2), a negative electrode member (3), and a diaphragm (4); and forming an electrode assembly by winding the positive electrode member (2), the diaphragm (4), and the negative electrode member (3) together, and at least one of the positive electrode member (2) and the negative electrode member (3) is manufactured by the manufacturing method of an electrode member according to claim 22 or 23; providing an adapter piece (8) and stacking and welding a plurality of conductive structures (16) of the electrode assembly to the adapter piece (8); preparing a top cover plate (6) and an electrode terminal (7) fixed to the top cover plate (6), and fixing the adapter piece (8) to the electrode terminal (7); preparing a case (5), placing the electrode assembly in the case (5), and connecting the top cover plate (6) to the case (5); A method for manufacturing a secondary battery comprising the steps of:

25. Preparing a current collector manufactured by the manufacturing method according to claim 19 or 20; Applying a slurry containing an active material to a partial area of ​​the surface of the second conductive layer (14); After hardening the slurry containing the active material, an active material layer (13) is formed, and the active material layer (13) is roll-pressed; welding a metal foil material to the first conductive layer (12) in an area where the second conductive layer (14) is not applied; removing a portion of the metal foil material and a portion of the current collector to form a plurality of spaced apart conductive structures (16) and a plurality of spaced apart electrical guide portions (P); A method for manufacturing an electrode member, comprising:

26. applying a slurry containing an insulating material to a partial area of ​​the surface of the second conductive layer (14), and then curing the slurry containing the insulating material to form a protective layer (15); The protective layer (15) is formed before welding the metal foil material. The method for manufacturing an electrode member according to claim 25 .

27. a positive electrode member (2), a negative electrode member (3), and a diaphragm (4); and forming an electrode assembly by winding the positive electrode member (2), the diaphragm (4), and the negative electrode member (3) together, and at least one of the positive electrode member (2) and the negative electrode member (3) is manufactured by the manufacturing method of an electrode member according to claim 25 or 26; providing an adapter piece (8) and stacking and welding a plurality of conductive structures (16) of the electrode assembly to the adapter piece (8); preparing a top cover plate (6) and an electrode terminal (7) fixed to the top cover plate (6), and fixing the adapter piece (8) to the electrode terminal (7); preparing a case (5), placing the electrode assembly in the case (5), and connecting the top cover plate (6) to the case (5); A method for manufacturing a secondary battery comprising the steps of:

Citation Information

Patent Citations

  • Secondary battery and pole piece thereof

    CN108598491A

  • Mass flow body, pole piece and battery

    CN207818780U

  • Thin film electrode, its manufacturing method, lithium secondary battery using it

    JP2005085570A

  • Anode and battery

    JP2008153015A

  • Electrode sheet for li-ion battery and li-ion battery including the same

    US20170214036A1