RF tag laminate manufacturing method and RF tag laminate

By inclining RF tags on a rubber sheet and using a roller crimping method with aligned antennas, the method addresses air retention issues, resulting in a durable and efficiently produced RF tag laminate for rubber articles.

JP7610476B2Active Publication Date: 2025-01-08BRIDGESTONE CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021109730
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-06-30
Publication Date
2025-01-08
Estimated Expiration
2041-06-30

AI Technical Summary

Technical Problem

When manufacturing RF tag laminates for rubber articles like tires, air remains between the rubber sheet layers and the RF tags, reducing the durability of the laminate.

Method used

The method involves arranging RF tags on a rubber sheet layer with their long sides inclined relative to the roller's direction, using a roller to crimp the layers together, ensuring the antenna extends parallel to the long side of the IC chip, and employing a strip-shaped rubber sheet for efficient stacking.

Benefits of technology

This approach produces an RF tag laminate with high durability and productivity by effectively removing air during the manufacturing process, enhancing the laminate's structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007610476000001
    Figure 0007610476000001
  • Figure 0007610476000002
    Figure 0007610476000002
  • Figure 0007610476000003
    Figure 0007610476000003
Patent Text Reader

Abstract

To provide a production method of an RF tag laminate capable of obtaining durable RF tag laminate with high productivity, and a durable RF tag laminate.SOLUTION: A disclosed production method of an RF tag laminate includes: an RF tag placement step; a second rubber sheet layer lamination step; and a roller crimping step. In the RF tag placement step, in plan view, multiple RF tags 10 are placed on a first rubber sheet layer 11a so that a long side 10aL of a rectangle in an IC chip 10a of each of the multiple RF tags 10 is inclined with respect to the direction RMV perpendicular to the relative movement direction RM of the first roller 3a.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing an RF tag laminate and a method for producing an RF tag laminate. [Background technology]

[0002] Conventionally, a configuration has been known in which an RF tag equipped with a memory unit capable of storing unique identification information and the like is embedded inside a rubber article such as a tire (for example, Patent Document 1). With this configuration, for example, various information acquired from the memory unit of the RF tag can be utilized for maintenance services for the rubber article such as the tire. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-132292 A Summary of the Invention [Problem to be solved by the invention]

[0004] When embedding an RF tag inside a rubber article such as a tire, the RF tag may be embedded inside the rubber article as an RF tag laminate in which the RF tag is sandwiched between covering rubber and laminated, in order to improve durability and adhesion to the rubber components that make up the rubber article. When manufacturing such an RF tag laminate, for example, multiple RF tags are placed on a rubber sheet layer, and then another rubber sheet layer is placed on top of that and pressed together, thereby enabling multiple RF tag laminates to be obtained together with good productivity. However, in this process, air may remain between the rubber sheet layer and the RF tags, which may reduce the durability of the obtained RF tag laminate.

[0005] Therefore, an object of the present invention is to provide a method for producing an RF tag laminate that can produce an RF tag laminate with excellent durability with high productivity, and to provide an RF tag laminate with excellent durability. [Means for solving the problem]

[0006] The method for producing the RF tag laminate of the present invention comprises the steps of: A method for producing an RF tag laminate, comprising: an RF tag having an IC chip that is rectangular in plan view and an antenna connected to at least one short side of the rectangle of the IC chip; and a covering rubber that is laminated on the RF tag and covers an outer surface of the RF tag, the method comprising the steps of: an RF tag arrangement step of arranging a plurality of the RF tags on a first rubber sheet layer that becomes a part of the coating rubber, the RF tags being spaced apart from one another; a second rubber sheet layer laminating step of laminating a second rubber sheet layer, which becomes another part of the coated rubber, on the first rubber sheet layer and the plurality of RF tags after the RF tag arrangement step; a roller pressing step of pressing the first rubber sheet layer, the plurality of RF tags, and the second rubber sheet layer against each other by a first roller that moves relatively over the first rubber sheet layer, the plurality of RF tags, and the second rubber sheet layer after the second rubber sheet layer lamination step; Including, The RF tag placement process is characterized in that the multiple RF tags are placed on the first rubber sheet layer so that, in a plan view, the long side of the rectangle in the IC chip of each of the multiple RF tags is inclined with respect to a direction perpendicular to the relative traveling direction of the first roller. According to the method for producing an RF tag laminate of the present invention, an RF tag laminate having excellent durability can be obtained with high productivity.

[0007] In the method for producing the RF tag laminate of the present invention, In the RF tag placement step, the RF tags are arranged on the first rubber sheet layer such that the long sides of the rectangular shapes of the respective IC chips face each other and are spaced apart from each other; In the roller pressing step, it is preferable that the first roller relatively advances over the first rubber sheet layer, the plurality of RF tags, and the second rubber sheet layer in a direction intersecting with a long side of the rectangle of the IC chip. This further increases the productivity of the RF tag laminate.

[0008] In the method for producing the RF tag laminate of the present invention, In the RF tag placement step, the inclination angle of the long side of the rectangle with respect to a direction perpendicular to the relative traveling direction of the first roller is preferably 8 to 15 degrees in a plan view. This makes it possible to more effectively obtain an RF tag laminate having excellent durability with high productivity.

[0009] In the method for producing the RF tag laminate of the present invention, In a plan view, it is preferable that the entire longitudinal direction of the antenna of the RF tag extends in a direction parallel to the extension direction of the long side of the rectangle of the IC chip. This makes it possible to more effectively obtain an RF tag laminate having excellent durability.

[0010] In the method for producing the RF tag laminate of the present invention, In the RF tag placement step, the first rubber sheet layer has a rectangular shape having a predetermined width and extending in a longitudinal direction, In the RF tag arrangement step, the plurality of RF tags are preferably arranged side by side along the longitudinal direction of the first rubber sheet layer. This allows for efficient manufacturing of the RF tag laminate.

[0011] The RF tag laminate of the present invention is characterized in that it is produced by any one of the above-mentioned methods for producing an RF tag laminate. The RF tag laminate of the present invention has excellent durability. Effect of the Invention

[0012] According to the present invention, it is possible to provide a method for producing an RF tag laminate with excellent durability and with high productivity, and an RF tag laminate with excellent durability. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1 is a perspective view that shows, in outline, one example of an RF tag laminate obtained by a method for producing an RF tag laminate according to an embodiment of the present invention. [Diagram 2] 1 is a plan view that illustrates an example of an RF tag in an RF tag laminate obtained by a method for producing an RF tag laminate according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a plan view for explaining an RF tag arrangement step in the manufacturing method of the RF tag laminate according to one embodiment of the present invention. [Figure 4] 4 is a partial cross-sectional side view corresponding to the AA section in FIG. 3, for illustrating a roller pressing step in a manufacturing method for an RF tag laminate according to one embodiment of the present invention. FIG. [Diagram 5] 4 is a flowchart for explaining a method for manufacturing an RF tag laminate according to one embodiment of the present invention. [Figure 6] FIG. 11 is a plan view for explaining an RF tag arrangement step in the manufacturing method of the RF tag laminate according to the comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] The RF tag laminate obtained by the method for producing an RF tag laminate of the present invention is suitable for use in any rubber article, and is particularly suitable for use in tires.

[0015] Hereinafter, an embodiment of a method for producing an RF tag laminate according to the present invention and an embodiment of an RF tag laminate will be described with reference to the drawings. The same components are designated by the same reference numerals in the various figures.

[0016] First, the RF tag laminate to be obtained by the manufacturing method of the RF tag laminate of the present invention, and thus obtained by the manufacturing method, will be described with reference to Figs. 1 and 2. Fig. 1 is a perspective view that shows an example of an RF tag laminate obtained by a method for producing an RF tag laminate according to any embodiment of the present invention, and Fig. 2 is a plan view that shows an example of an RF tag in an RF tag laminate obtained by a method for producing an RF tag laminate according to any embodiment of the present invention.

[0017] As shown in FIG. 1, the RF tag laminate 1 of this example includes an RF tag 10 and a covering rubber 11. The RF tag 10 has an IC chip 10a (in other words, the outer contour of the IC chip 10a is rectangular in a plan view) (see Figure 2, etc.) (in this example, a rectangle in the narrow sense of the word) and an antenna 10b connected to at least one of the short sides 10aS (in this example, both) of the rectangle in the IC chip 10a. An "RF tag" is also commonly called an "RFID (Radio Frequency Identification) tag." The RF tag can be configured to be capable of wireless communication with the outside. In this specification, the term "rectangle" refers to a rectangle in the narrow sense (hereinafter simply referred to as a "rectangle") and a square. When the rectangle is a square, the "long side of the rectangle" refers to any one side of the square, and the "short side of the rectangle" refers to the other side adjacent to the one side. Note that the vertices of the rectangle may be slightly rounded from the viewpoint of suppressing damage to other members adjacent to the IC chip. In this specification, the direction parallel to the extension direction of the long side 10aL of the rectangle in a plan view (see FIG. 2, etc.) of the RF tag is referred to as the "long side direction LD," the direction parallel to the extension direction of the short side 10aS of the rectangle in a plan view is referred to as the "short side direction LS," and the direction perpendicular to the long side direction LD and the short side direction LS is referred to as the "thickness direction TD." "Plan view" refers to the RF tag 10 viewed from the thickness direction TD. Furthermore, in this specification, for example, "antenna 10b is connected to the short side 10aS of the rectangle in the IC chip 10a when viewed in a plane" or "antenna 10b is connected to the short side 10aS of the rectangle in the IC chip 10a when viewed in a plane" more specifically means "antenna 10b is connected to the end face of the IC chip 10a that includes the short side 10aS of the rectangle (in a planar view) of the IC chip 10a but does not include the long side 10aL of the rectangle," but to avoid complexity of expression, the former two expressions will be used unless otherwise specified.

[0018] The covering rubber 11 is laminated on the RF tag 10 and covers the outer surface of the RF tag 10 . The covering rubber 11 has a first rubber sheet layer 11a covering the RF tag 10 from one side in the thickness direction TD (more specifically, in this example, the lower side during manufacturing described later), and a second rubber sheet layer 11b covering the RF tag 10 from the other side in the thickness direction TD (more specifically, in this example, the upper side during manufacturing described later). The first rubber sheet layer 11a and the second rubber sheet layer 11b can be formed from unvulcanized raw rubber. By forming the first rubber sheet layer 11a and the second rubber sheet layer 11b from unvulcanized raw rubber, the first rubber sheet layer 11a and the second rubber sheet layer 11b, and further the first rubber sheet layer 11a, the RF tag 10, and the second rubber sheet layer 11b can be firmly fixed to each other by pressing with a roller during manufacturing, which will be described later, for example, without using an adhesive, due to their adhesive strength. The first rubber sheet layer 11a and the second rubber sheet layer 11b are preferably made of the same rubber from the viewpoint of adhesion etc. However, the first rubber sheet layer 11a and the second rubber sheet layer 11b may be made of different rubbers. As will be described later, when the RF tag laminate 1 is manufactured, the first rubber sheet layer 11a and the second rubber sheet layer 11b may be formed into a predetermined planar shape different from that shown in FIG.

[0019] In this example, the IC chip 10a constituting the RF tag 10 has a rectangular shape in plan view as shown in Figures 1 and 2. That is, in this example, the IC chip 10a has a rectangular parallelepiped shape. However, the IC chip 10a may have a square shape in a plan view, that is, the IC chip 10a may have a cubic shape. The IC chip 10a has, in a plan view, two long sides 10aL facing each other and two short sides 10aS facing each other. The IC chip 10a can constitute a control unit and / or a storage unit when the RF tag 10 performs wireless communication. The IC chip 10a may be operated by induced electromotive force generated by electromagnetic waves received by one or more antennas.

[0020] 1 and 2, in this example, the antenna 10b constituting the RF tag 10 is connected to both (i.e., two opposing) short sides 10aS of the rectangle of the IC chip 10a in a plan view. In other words, the antenna 10b has a first antenna 10b1 connected to one short side 10aS of the IC chip 10a and a second antenna 10b2 connected to the other short side 10aS of the IC chip 10a. However, the antenna 10b may be connected to only one of the short sides 10aS of the rectangle of the IC chip 10a in a plan view. In other words, the antenna 10b may have only one of the first antenna 10b1 and the second antenna 10b2. That is, the antenna 10b may be connected to at least one of the short sides 10aS of the rectangle of the IC chip 10a in a plan view. When antenna 10b has a first antenna 10b1 and a second antenna 10b2, their extension direction (the overall extension direction, not the direction along a spiral or the like shown in the example of FIG. 2), shape (the shape of the spiral or the like shown in the example of FIG. 2) and length (the length in the antenna extension direction, i.e., the distance between both ends of the antenna) can be the same as in the examples of FIGS. 1 and 2, but at least one of these may be different.

[0021] In this example, as shown in FIG. 2, each of the antennas 10b (first antenna 10b1 and second antenna 10b2) extends from the short side 10aS of the IC chip 10a in a spiral shape over the entire longitudinal direction. However, the antenna 10b (first antenna 10b1 and / or second antenna 10b2) may extend from the short side 10aS of the IC chip 10a in such a way that its entire longitudinal direction is a straight line, a wavy line (approximately two-dimensional wavy line; same below), or a zigzag line (approximately two-dimensional zigzag line; same below). Furthermore, the antenna 10b (first antenna 10b1 and / or second antenna 10b2) may extend from the short side 10aS of the IC chip 10a in any two or more of the following shapes: a spiral, a straight line, a wavy line, and a zigzag line, in any order. For example, antenna 10b (first antenna 10b1 and / or second antenna 10b2) may be one that first extends from short side 10aS of IC chip 10a in a spiral (or a wavy line or a zigzag line) and then extends from the end of the short side in a straight line, or one that first extends from short side 10aS of IC chip 10a in a straight line and then extends from the end of the short side in a spiral (or a wavy line or a zigzag line), or one that first extends from short side 10aS of IC chip 10a in a spiral (or a wavy line or a zigzag line), then extends from the end of the short side in a straight line and then extends from the end of the short side in a spiral (or a wavy line or a zigzag line). However, from the standpoint of air escaping through antenna 10b during manufacturing, which will be described later, it is preferable that at least a portion of antenna 10b extends in a spiral shape, since air tends to move inside the spiral, and it is preferable that the entire length of antenna 10b extends in a spiral shape, as in the example of Figure 2.

[0022] 1 and 2, in the plan view, the antennas 10b (the first antenna 10b1 and the second antenna 10b2) each extend from the short side 10aS of the IC chip 10a along the long side direction LD (i.e., in a direction parallel to the extending direction of the rectangular long side 10aL of the IC chip 10a). In other words, in the plan view, the antennas 10b (the first antenna 10b1 and the second antenna 10b2) each extend in a linear extension form with the entirety of their longitudinal direction extending along the long side direction LD. However, antenna 10b (first antenna 10b1 and / or second antenna 10b2) does not have to extend in a straight line extending along the long side direction LD in its entirety, and may extend in a broken line or curved line extending in a direction different from the long side direction LD in part of its longitudinal direction. However, from the viewpoint of allowing air to escape along antenna 10b during manufacturing (more specifically, during the roller pressing process) described below, it is preferable that the entire longitudinal direction of antenna 10b extends along the long side direction LD (i.e., in a direction parallel to the extension direction of rectangular long side 10aL of IC chip 10a).

[0023] The antenna 10b (the first antenna 10b1 and / or the second antenna 10b2) may be made of metal. The antenna 10b (the first antenna 10b1 and / or the second antenna 10b2) can be configured to perform a communication function when the RF tag performs wireless communication with the outside.

[0024] The connection between the IC chip 10a and the antenna 10b is not particularly limited, and the antenna 10b may be connected to the IC chip 10a by, for example, soldering. Furthermore, although not shown, the RF tag 10 can have a coating resin that covers and reinforces the outer surfaces of at least a portion of the IC chip 10a and the antenna 10b (for example, the connection between the IC chip 10a and the antenna 10b, or the entire IC chip 10a and the connection between the IC chip 10a and the antenna 10b). This increases the durability of the RF tag 10 compared to when the RF tag 10 does not have a coating resin. When the RF tag 10 has a coating resin, the entire outer surfaces of the IC chip 10a, the antenna 10b, and the coating resin are covered with a coating rubber 11 to form the RF tag laminate 1. Furthermore, although not shown, the RF tag 10 may have an antenna (hereinafter also referred to as an "additional antenna") separate from the antenna 10b, which extends in the long side direction LD in a spiral shape (in other words, so that at least a part of the IC chip 10a and antenna 10b is included inside the spiral) so as to surround at least a part of the IC chip 10a and antenna 10b (for example, the entire IC chip 10a, or the entire IC chip 10a and at least a part of the antenna 10b) in addition to the IC chip 10a and antenna 10b, or, in the case where the RF tag 10 has the above-mentioned coating resin, in addition to the IC chip 10a and antenna 10b, if the RF tag 10 has the above-mentioned coating resin. The additional antenna may or may not be in contact or connected with the IC chip 10a. The additional antenna may be configured to function as a dipole antenna, in which case the communication strength can be improved. Since the additional antenna has a spiral structure, it can further promote air escape during manufacturing, which will be described later. When the RF tag 10 has the above-mentioned additional antenna, the entire outer surface of the IC chip 10a, antenna 10b, and additional antenna, or when the RF tag 10 has the above-mentioned coating resin, the entire outer surface of the IC chip 10a, antenna 10b, coating resin, and additional antenna are covered with coating rubber 11 to form the RF tag laminate 1.

[0025] Next, a method for producing an RF tag laminate according to one embodiment of the present invention will be described with reference to FIGS. Fig. 3 is a plan view for explaining an RF tag arrangement step in a method for producing an RF tag laminate according to one embodiment of the present invention. In Fig. 3, rollers used in a subsequent roller pressing step are also shown by dotted lines. Fig. 4 is a partial cross-sectional side view corresponding to section AA in Fig. 3 for explaining the roller pressing step in a method for producing an RF tag laminate according to one embodiment of the present invention. Fig. 5 is a flow chart for explaining a method for producing an RF tag laminate according to one embodiment of the present invention.

[0026] The manufacturing method of an RF tag laminate according to one embodiment of the present invention, which will be described below, includes, in this order, a first rubber sheet layer placing step (step S101), an RF tag arrangement step (step S102), a second rubber sheet layer lamination step (step S103), a roller pressing step (step S104), and an RF tag laminate cutting step (step S105).

[0027] (First rubber sheet layer placing step) First, in the first rubber sheet layer placing process, although not shown, the first rubber sheet layer 11a, which will become part of the coated rubber 11 in the RF tag laminate 1 obtained by the manufacturing method of this embodiment, is placed on an appropriate stand 2 (step S101). The base 2 may be any base as long as it can stably place the first rubber sheet layer 11a substantially horizontally.

[0028] (RF tag placement process) After the first rubber sheet layer placing step, in the RF tag placement step, as shown in FIG. 3, multiple RF tags 10 are placed side by side and spaced apart from each other on the first rubber sheet layer 11a which is to become part of the coated rubber 11 in the RF tag laminate 1 obtained by the manufacturing method of this embodiment and which has been placed on the table 2 in the first rubber sheet layer placing step (step S102). Any of the RF tags 10 described above with reference to Figs. 1 and 2 can be used as each of the RF tags 10. In the example shown in Figs. 3 and 4, each of the RF tags 10 has an IC chip 10a that is rectangular in plan view, a first antenna 10b1, and a second antenna 10b2, and the entire longitudinal direction of each of the first antenna 10b1 and the second antenna 10b2 extends along the long side direction LD (i.e., in a direction parallel to the extending direction of the rectangular long side 10aL of the IC chip 10a) in plan view, and has the antenna 10b shown in Fig. 2, which has the same shape and length. In the example shown in Figs. 3 and 4, all of the RF tags 10 have the same shape and size.

[0029] More specifically, in this embodiment, as shown in FIG. 3, in a plan view, a plurality of RF tags 10 are arranged on the first rubber sheet layer 11a so that the rectangular long sides 10aL of each IC chip 10a (in other words, the IC chips 10a of each adjacent RF tag 10) face each other and are spaced apart, and in the roller pressing process described below, the first roller 3a moves relatively over the first rubber sheet layer 11a, the plurality of RF tags 10 and the second rubber sheet layer 11b in a direction intersecting with the rectangular long sides 10aL of the IC chips 10a. However, the multiple RF tags 10 do not have to be arranged side by side such that the long sides 10aL of the rectangles of the respective IC chips 10a face each other and are spaced apart from each other. For example, the multiple RF tags 10 may be arranged side by side such that the entire longitudinal direction of each antenna 10b (first antenna 10b1 and second antenna 10b2) extends in a linear extension form along the long side direction LD, and the tips of the antennas 10b of adjacent RF tags 10 butt against each other and are spaced apart from each other. In other words, the multiple RF tags 10 may be arranged so that the entire longitudinal direction of each of them extends in a linear form along the relative traveling direction RM of the first roller 3a described later (in other words, so that the inclination angle θ described later is 90°). However, particularly from the viewpoint of productivity, it is preferable to arrange a plurality of RF tags 10 on the first rubber sheet layer 11a so that the long sides 10aL of the rectangles of the respective IC chips 10a face each other and are spaced apart from each other.

[0030] As shown in FIG. 3, in this embodiment, the first rubber sheet layer 11a which is placed on the table 2 in the above-mentioned first rubber sheet layer placing process, and on which the RF tag 10 is placed in the RF tag placement process, is in the form of a strip in a plan view having a predetermined width (the width in the vertical direction of the paper in FIG. 3) and extending in the longitudinal direction (the horizontal direction of the paper in FIG. 3), and in the RF tag placement process, multiple RF tags 10 are placed along the longitudinal direction of the first rubber sheet layer 11a (i.e., lined up at intervals in a direction parallel to the longitudinal direction). This enables efficient production of RF tag laminates, for example, by reducing the amount of rubber that does not become part of the resulting RF tag laminate and is discarded, compared to when a first rubber sheet layer 11a having a shape other than a rectangular shape is used. The above-mentioned predetermined width of the first rubber sheet layer 11a may be any width as long as it is greater than the width of the first rubber sheet layer 11a of the RF tag arranged on the first rubber sheet layer 11a. However, from the viewpoint of reducing waste rubber in the RF tag laminate cutting process described later, the width of the first rubber sheet layer 11a is preferably 2 times or less, more preferably 1.5 times or less, of the width of the first rubber sheet layer 11a of the RF tag 10 arranged on the first rubber sheet layer 11a. Moreover, from the viewpoint of leaving a predetermined amount of covering rubber around the RF tag 10 in plan view in the manufactured RF tag laminate, the width of the first rubber sheet layer 11a is preferably 1.2 times or more, more preferably 1.3 times or more, of the width of the first rubber sheet layer 11a of the RF tag 10 arranged on the first rubber sheet layer 11a. In this embodiment, the width of the first rubber sheet layer 11a is constant along the longitudinal direction of the first rubber sheet layer 11a, as shown in Fig. 3. However, the width of the first rubber sheet layer 11a does not have to be constant along the longitudinal direction of the first rubber sheet layer 11a.

[0031] In the RF tag placement process, the multiple RF tags 10 are placed on the first rubber sheet layer 11a so that, in a plan view, the long side 10aL (and thus the long side direction LD) of the rectangle of the IC chip 10a of each of the multiple RF tags 10 placed on the first rubber sheet layer 11a is inclined with respect to the direction RMV perpendicular to the relative traveling direction RM of the first roller 3a in the roller pressing process described below (i.e., so that the inclination angle θ in Figure 3 is not 0°) (see Figure 3). The effects of this will be described in detail later. Here, the "relative moving direction RM of the first roller 3a" refers to the direction in which the first roller 3a moves relative to an object (in the example of FIG. 5 described later, the second rubber sheet layer 11b, and in turn, a laminated sheet in which the first rubber sheet layer 11a, the multiple RF tags 10, and the second rubber sheet layer 11b are laminated) that is pressed by the first roller 3a in the roller pressure bonding process described later. If the orientation of the relative moving direction RM of the first roller 3a is not taken into consideration, it is the same as (i.e., parallel to) the direction in which the laminated sheet in which the first rubber sheet layer 11a, the multiple RF tags 10, and the second rubber sheet layer 11b are laminated moves relative to the first roller 3a in the roller pressure bonding process described later (relative moving direction of the laminated sheet) SR (see FIGS. 3 and 4). If the orientation is taken into consideration, the relative moving direction RM of the first roller 3a and the relative moving direction SR of the laminated sheet are opposite to each other. In this embodiment, as shown in FIG. 3, the relative moving direction RM of the first roller 3a is the same as the longitudinal direction of the first rubber sheet layer 11a, and the direction RMV perpendicular to the relative moving direction RM of the first roller 3a is the same as the width direction of the first rubber sheet layer 11a and the direction parallel to the rotation axis of the first roller 3a.

[0032] In a plan view, in the RF tag placement process, the inclination angle θ (see Figure 3) of the rectangular long side 10aL (and thus the long side direction LD) of each IC chip 10a with respect to the direction RMV perpendicular to the relative moving direction RM of the first roller 3a may be any angle other than 0°, as long as adjacent RF tags 10 are placed with an appropriate gap between them and without touching each other. For example, the inclination angle θ may be 90°. However, from the viewpoint of a balance between production efficiency and air removal in the roller compression step described below, the inclination angle θ (the angle on the acute angle side) is preferably less than 90°, more preferably 8 to 15°, and most preferably about 10°. If the angle θ is 8° or more, air can be removed more effectively in the roller compression step, and if it is 15° or less, a more sufficient gap can be provided between adjacent RF tags, thereby improving production efficiency in the RF tag laminate cutting step described below and the like.

[0033] In the example of Figure 3, the extension direction (i.e., the long side direction LD) of the RF tags 10 arranged on the first rubber sheet layer 11a is the same among all of the multiple RF tags 10 (i.e., the extension directions of the long sides 10aL are all parallel to each other), but the extension directions (i.e., the long side direction LD) of the RF tags 10 may not be the same among all of the multiple RF tags 10 and may be partially different. In addition, in the example of Figure 3, the spacing between adjacent RF tags 10 arranged on the first rubber sheet layer 11a in the relative traveling direction RM of the first roller 3a (and thus the longitudinal direction of the first rubber sheet layer 11a) is all the same, but the spacing may not all be the same and some may be different. Furthermore, in the example of Figure 3, all of the multiple RF tags 10 arranged on the first rubber sheet layer 11a are arranged side by side along the longitudinal direction of the first rubber sheet layer 11a so that the longitudinal center of the IC chip 10a coincides with the widthwise center of the first rubber sheet layer 11a, but the IC chips 10a of at least some of the multiple RF tags 10 may be arranged so that the longitudinal centers do not coincide with the widthwise center of the first rubber sheet layer 11a, and the IC chips 10a of at least some of the multiple RF tags 10 may be arranged so that they are at different positions from each other in the width direction of the first rubber sheet layer 11a. However, from the viewpoint of easily obtaining multiple homogeneous RF tag laminates 1, it is preferable that the RF tag 10 is arranged on the first rubber sheet layer 11a in the RF tag arrangement process in a plan view as shown in FIG. 3.

[0034] (Second rubber sheet layer lamination process) After the RF tag placement process, in the second rubber sheet layer lamination process, although not shown, a second rubber sheet layer 11b, which becomes another part of the coated rubber 11, is laminated on top of the first rubber sheet layer 11a and the multiple RF tags 10 that were arranged on top of each other in the RF tag placement process (step S103). The shape and dimensions of the second rubber sheet layer 11b used in the second rubber sheet layer lamination step are not particularly limited and may be any as long as the second rubber sheet layer 11b and the first rubber sheet layer 11a can completely cover the multiple RF tags 10 arranged on the first rubber sheet layer 11a. The second rubber sheet layer 11b may be, for example, a large single piece or may be divided. The second rubber sheet layer 11b may be, for example, a strip-like piece similar to the first rubber sheet layer 11a illustrated in FIG. 3, extending in the longitudinal direction with a width approximately equal to that of the first rubber sheet layer 11a illustrated in FIG. 3.

[0035] (Roller pressure bonding process) After the second rubber sheet layer lamination process, in the roller pressing process, as shown in FIG. 4, the first rubber sheet layer 11a, the multiple RF tags 10, and the second rubber sheet layer 11b (in other words, a laminated sheet consisting of the first rubber sheet layer 11a, the multiple RF tags 10, and the second rubber sheet layer 11b) (hereinafter, these are also collectively referred to as the "laminate sheet") laminated in the second rubber sheet layer lamination process are pressed together by a first roller 3a which moves relatively over the first rubber sheet layer 11a, the multiple RF tags 10, and the second rubber sheet layer 11b (laminate sheet) (step S104). In the roller pressing process, the first roller 3a, which moves relatively over the laminated sheet, gradually presses and adheres to the first rubber sheet layer 11a and the second rubber sheet layer 11b (see FIG. 4), which are spaced apart vertically with a gap S between adjacent RF tags 10 on the front side of the relative moving direction RM of the first roller 3a (on the left side of the paper in FIGS. 3 and 4), until the entire first rubber sheet layer 11a, the multiple RF tags 10 and the second rubber sheet layer 11b are pressed together and these components are adhered to each other.

[0036] In the roller pressure bonding step, the first roller 3a may advance relative to the laminated sheet. That is, in the roller pressure bonding step, the position of the first roller 3a may be fixed and the laminated sheet may advance (move) relative to the first roller 3a, or the position of the laminated sheet may be fixed and the first roller 3a may advance (move) relative to the laminated sheet. In the example shown in FIG. 4, the laminate sheet is passed between two rollers 3 (first roller 3a and second roller 3b) that rotate relative to each other and moved in the relative moving direction SR of the laminate sheet (when the direction is also taken into consideration, the direction is the opposite to the relative moving direction RM of the first roller 3a), thereby fixing the position of the first roller 3a and moving (moving) the laminate sheet relative to the first roller 3a. However, instead of using the second roller 3b, the position of the laminate sheet may be fixed on the base 2, and the first roller 3a may move over it in the relative moving direction RM of the first roller 3a, thereby fixing the position of the laminate sheet and moving (moving) the first roller 3a relative to the laminate sheet. In the example shown in FIG. 4, the first roller 3a does not actually move (move), so in FIG. 4, the relative moving direction RM of the first roller 3a is indicated by a dotted line.

[0037] The material of the first roller 3a (excluding the shaft body that serves as the rotating shaft) is not particularly limited and may be any material. The first roller 3a (excluding the shaft body that becomes the rotating shaft) may be, for example, a metal material such as iron whose surface is coated with a flexible resin such as urethane. In this case, the urethane coating or the like increases the flexibility of the roller surface, so that the roller can sufficiently follow the shape change of the second rubber sheet layer 11b when the rollers are pressed against each other, and the first rubber sheet layer 11a, the multiple RF tags 10, and the second rubber sheet layer 11b can be more effectively pressed against each other. When a second roller 3b is also used as illustrated in FIG. 4, the second roller 3b is similar to the first roller 3a described above.

[0038] The diameter of the first roller 3a is not particularly limited and may be any as long as the first roller 3a is configured so that the first rubber sheet layer 11a and the second rubber sheet layer 11b (see FIG. 4), which are spaced apart from each other in the vertical direction via the gap S between the adjacent RF tags 10, can come into contact with each other as the first roller 3a moves relative to each other. However, from the viewpoint of sufficiently removing the air in the gap S as the first roller 3a moves relative to each other (i.e., from the viewpoint of air removal), it is preferable that the diameter of the first roller 3a is such that the first roller 3a can completely drop into the gap S between the adjacent RF tags 10 as the first roller 3a moves relative to each other (i.e., does not come into contact with the second rubber sheet layer 11b above both of the RF tags 10 adjacent to each other via the gap S) as the first roller 3a moves relative to each other. When a second roller 3b is also used as illustrated in FIG. 4, the second roller 3b is similar to the first roller 3a described above.

[0039] (RF tag laminate cutting process) After the roller pressing process, in the RF tag laminate cutting process, although not shown, a laminate sheet in which the first rubber sheet layer 11a, multiple RF tags 10, and second rubber sheet layer 11b are pressed together and stacked is cut out in multiple portions consisting of the first rubber sheet layer 11a, one RF tag 10, and the second rubber sheet layer 11b as finished products of the RF tag laminate 1, thereby obtaining multiple RF tag laminates 1 (step S105). The method of cutting out the RF tag laminate in the RF tag laminate cutting step is not particularly limited and may be any method. For example, the RF tag laminate 1 may be cut out from the laminate sheet by die cutting. Also, for example, the RF tag laminate 1 may be cut out by cutting between adjacent RF tags 10 in the laminate sheet with a knife or the like.

[0040] Next, the effects of the above-mentioned method for producing an RF tag laminate according to one embodiment of the present invention will be described. First, according to this embodiment, in the RF tag arrangement step, a plurality of RF tags 10 are arranged on the first rubber sheet layer 11a, and in the second rubber sheet layer lamination step, the second rubber sheet layer 11b is laminated on the first rubber sheet layer 11a and the plurality of RF tags 10. This allows a plurality of RF tag laminates 1 to be obtained collectively in a later RF tag laminate cutting step or the like, and therefore the productivity of the RF tag laminate 1 can be improved compared to the case where the first rubber sheet layer 11a of a certain shape, one RF tag 10, and the second rubber sheet layer 11b of a certain shape are prepared and laminated to obtain the RF tag laminates 1 one by one. That is, according to this embodiment, the RF tag laminate 1 can be obtained with high productivity.

[0041] Next, according to this embodiment, in the RF tag placement process, the multiple RF tags 10 are placed on the first rubber sheet layer 11a so that, in a planar view, the rectangular long side 10aL of the IC chip 10a of each of the multiple RF tags 10 is inclined with respect to the direction RMV perpendicular to the relative moving direction RM of the first roller 3a (i.e., the inclination angle θ of the long side direction LD with respect to the direction RMV is not 0°) (Figure 3). The effect of this will be described in detail below. In the following description, the front side of the relative advancing direction RM of the first roller 3a (the left side of the paper in Figs. 3 to 5) will be simply referred to as the "front side", and the rear side of the relative advancing direction RM of the first roller 3a (the right side of the paper in Figs. 3 to 5) will be simply referred to as the "rear side". 6 shows a case where, unlike the above embodiment, in the RF tag placement step, the multiple RF tags 10 are placed on the first rubber sheet layer 11a so that the long side 10aL of the rectangle in each IC chip 10a of the multiple RF tags 10 is not inclined in a direction RMV perpendicular to the relative moving direction RM of the first roller 3a in a plan view (i.e., the inclination angle θ of the long side direction LD to the direction RMV is 0°, and the long side direction LD and the direction RMV are coincident). In this case, even if the subsequent roller pressing step is performed, the inventors have found that air remains in the gap S between the IC chips 10a of the adjacent RF tags 10 (the IC chip 10a has a predetermined thickness in the thickness direction TD, and therefore there is a gap S having a certain volume), particularly near the rear end (in other words, the end of the gap S adjacent to the front side of the rear IC chip 10a. Hereinafter, it is also referred to as "the end of the gap S on the IC chip front side") Sf (see FIGS. 3 to 4 and 6), and that the air does not easily escape. The reason that air remains near the end Sf of the gap S on the front side of the IC chip and does not easily escape is that the air in the gap S is gradually pushed forward as the first roller 3a moves relative to one another in the roller pressing process, but for one gap S, the first rubber sheet layer 11a and the second rubber sheet layer 11b on the front side that form the gap S come into close contact first as the first roller 3a moves relative to one another, so that air remains near the end Sf of the rear side of the gap S (the end Sf of the gap S on the front side of the IC chip). On the other hand, in the example of Figure 6, in the RF tag placement process, the long side 10aL of the IC chip 10a is not inclined with respect to the direction RMV (the inclination angle θ of the long side direction LD with respect to the direction RMV is 0°), so in the roller pressing process, the first roller 3a reaches the entire area in the direction RMV of the end Sf of the gap S simultaneously in a planar view (see Figure 6) as it progresses relative to the first roller 3a. Even if there is pressure due to the relative progress of the first roller 3a, the air remaining near the end Sf of the gap S cannot move at all, which is thought to be the reason why the air does not easily escape. On the other hand, in this embodiment, in the RF tag placement process, the long side 10aL of the IC chip 10a is inclined with respect to the direction RMV (the inclination angle θ of the long side direction LD with respect to the direction RMV is not 0°), so that in the roller pressing process, as the first roller 3a progresses relative to itself, it will first reach one side of the end Sf of the gap S in the direction RMV in a planar view (see Figure 3).The air near the end Sf of the gap S will move to one side in the direction RMV due to the pressure caused by the relative progress of the first roller 3a, and the antenna 10b (first antenna 10b1 and / or second antenna 10b2) will promote the air to be discharged to the outside along the antenna 10b (first antenna 10b1 and / or second antenna 10b2). That is, according to this embodiment, air escape during the production of the RF tag laminate 1 is promoted, and air is prevented from remaining inside the obtained RF tag laminate 1, so that it is possible to obtain an RF tag laminate 1 with excellent durability. Note that if air remains inside the RF tag laminate 1, the air may act as a nucleus to cause damage to the RF tag 10, and ultimately the durability of the RF tag laminate 1 may decrease. As described above, in this embodiment, antenna 10b (first antenna 10b1 and second antenna 10b2) also has the function of providing an escape route for air when compressed, and from that viewpoint, it is preferable that antenna 10b (first antenna 10b1 and / or second antenna 10b2) extends in a spiral shape, as illustrated in FIG. 2.

[0042] As described above, according to the method for producing an RF tag laminate according to this embodiment, the RF tag laminate 1 having excellent durability can be obtained with high productivity.

[0043] In the RF tag placement process, multiple RF tags 10 are arranged on the first rubber sheet layer 11a so that the rectangular long sides 10aL of each IC chip 10a face each other and are spaced apart, and in the roller compression process, it is preferable that the first roller 3a moves relatively over the first rubber sheet layer 11a, the multiple RF tags 10 and the second rubber sheet layer 11b in a direction intersecting with the rectangular long sides 10aL of the IC chip 10a. This allows a greater number of RF tag laminates to be obtained from the first rubber sheet layer 11a of the same longitudinal length than when multiple RF tags 10 are arranged on the first rubber sheet layer 11a in the RF tag placement process, spaced apart from each other, so that their entirety extends linearly along the relative traveling direction RM of the first roller 3a (in other words, so that the inclination angle θ shown in Figure 3 is 90°), thereby further improving the productivity of the RF tag laminates.

[0044] In plan view, the inclination angle θ of the long side 10aL of the rectangle with respect to the direction RMV perpendicular to the relative moving direction RM of the first roller 3a in the roller pressing step in the RF tag placement step is preferably 8 to 15°. As a result, as mentioned above, air can be removed more effectively in the roller pressing process, and production efficiency can be improved in the RF tag laminate cutting process, etc., so that an RF tag laminate with excellent durability can be obtained more effectively and with high productivity.

[0045] In plan view, it is preferable that the entire longitudinal direction of the antenna 10b of the RF tag 10 extends in a direction parallel to the direction in which the rectangular long sides 10aL of the IC chip 10a extend (that is, the long side direction LD). According to this, air can be more effectively removed in the roller pressing step, so that an RF tag laminate having excellent durability can be obtained more effectively.

[0046] In a planar view during the RF tag placement process, the first rubber sheet layer 11a has a strip shape having a predetermined width and extending in the longitudinal direction, and in the RF tag placement process, it is preferable that the multiple RF tags 10 are arranged side by side along the longitudinal direction of the first rubber sheet layer 11a. This allows efficient production of the RF tag laminate, as described above.

[0047] Next, an RF tag laminate according to one embodiment of the present invention will be described. The RF tag laminate according to one embodiment of the present invention is manufactured by any of the above-mentioned methods for manufacturing an RF tag laminate. The RF tag laminate according to one embodiment of the present invention has excellent durability. [Industrial Applicability]

[0048] The RF tag laminate obtained by the manufacturing method for an RF tag laminate of the present invention, and therefore the RF tag laminate according to the present invention, is suitable for use in any rubber article, and is particularly suitable for use in tires. [Explanation of symbols]

[0049] 1: RF tag laminate, 10: RF tag, 10a: IC chip, 10aL: long side, 10aS: short side, 10b: antenna, 10b1: first antenna, 10b2: second antenna, 11: covering rubber, 11a: first rubber sheet layer, 11b: second rubber sheet layer, 2: stand, 3: roller, 3a: first roller, 3b: second roller, LD: Long side direction, SD: Short side direction, TD: Thickness direction, RM: relative moving direction of the first roller, RMV: direction perpendicular to the relative moving direction of the first roller, SR: Relative direction of stacked sheets, S: gap, Sf: IC chip front end of the gap, θ: Tilt angle

Claims

1. A method for producing an RF tag laminate, comprising: an RF tag having an IC chip that is rectangular in plan view and an antenna connected to at least one short side of the rectangle of the IC chip; and a covering rubber that is laminated on the RF tag and covers an outer surface of the RF tag, the method comprising the steps of: an RF tag arrangement step of arranging a plurality of the RF tags in a spaced relationship on a first rubber sheet layer that becomes a part of the coating rubber; a second rubber sheet layer laminating step of laminating a second rubber sheet layer, which becomes another part of the covering rubber, on the first rubber sheet layer and the plurality of RF tags after the RF tag arrangement step; a roller pressing step of pressing the first rubber sheet layer, the plurality of RF tags, and the second rubber sheet layer against each other by a first roller that moves relatively over the first rubber sheet layer, the plurality of RF tags, and the second rubber sheet layer after the second rubber sheet layer lamination step; Including, In the RF tag placement step, the RF tags are placed on the first rubber sheet layer such that, in a plan view, a long side of the rectangle in an IC chip of each of the RF tags is inclined with respect to a direction perpendicular to a relative advancing direction of the first roller; In addition, in the RF tag placement step, the RF tags are arranged on the first rubber sheet layer such that the long sides of the rectangular shapes of the respective IC chips face each other and are spaced apart from each other, A method for manufacturing an RF tag laminate, characterized in that in the roller compression process, the first roller moves relatively over the first rubber sheet layer, the multiple RF tags, and the second rubber sheet layer in a direction intersecting with the long side of the rectangle in the IC chip.

2. 2. The method for manufacturing an RF tag laminate as described in claim 1, wherein, in a plan view, in the RF tag placement process, the inclination angle of the long side of the rectangle with respect to a direction perpendicular to the relative traveling direction of the first roller is 8 to 15 degrees.

3. 3. The method for producing an RF tag laminate according to claim 1, wherein, in a plan view, the antenna of the RF tag extends, over its entire longitudinal direction, in a direction parallel to the direction in which the long side of the rectangle of the IC chip extends.

4. In a plan view during the RF tag placement step, the first rubber sheet layer has a rectangular shape having a predetermined width and extending in a longitudinal direction, 4. The method for manufacturing an RF tag laminate according to claim 1, wherein in the RF tag arrangement step, the plurality of RF tags are arranged side by side along the longitudinal direction of the first rubber sheet layer.

5. An RF tag laminate, characterized in that it is manufactured by the method for manufacturing an RF tag laminate according to any one of claims 1 to 4.

Citation Information

Patent Citations

  • Patch type RFID (Radio Frequency Identification Device) tire electronic tag device and manufacturing and mounting method thereof

    CN102054195A

  • Manufacture of ic card and ic card

    JP1999272831A

  • Fid tag built-in tire

    JP2017132292A

  • tire

    JP2020083044A