Energy storage cell
The electrode body with axial grooves and varying spacing and width in the electrode sheets addresses cracking and peeling issues in lithium secondary batteries, enhancing durability and capacity.
Patent Information
- Application Number
- JP2023188445
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-11-02
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2043-11-02
AI Technical Summary
The electrode mixture layers in wound-type lithium secondary batteries are prone to cracking and peeling due to variations in winding radius, particularly at the center where the radius is smallest.
The electrode body is designed with grooves extending along the winding axis, with closer spacing and narrower widths on the inner side to mitigate bending stress, and the grooves on the inner side face each other to reduce lithium precipitation.
This design effectively suppresses cracking and peeling of the electrode mixture layers while maintaining capacity by distributing stress uniformly and minimizing lithium precipitation.
Smart Images

Figure 0007948135000001 
Figure 0007948135000002 
Figure 0007948135000003
Abstract
Description
Technical Field
[0001] The present disclosure relates to an electricity storage cell.
Background Art
[0002] Patent Document 1 (Japanese Unexamined Patent Application Publication No. 2001-6749) discloses a lithium secondary battery provided with a wound-type internal electrode body in which a positive electrode metal foil body and a negative electrode metal foil body are arranged with a separator interposed therebetween. The internal electrode body is formed by winding a positive electrode sheet, a separator, and a negative electrode sheet.
Prior Art Documents
Patent Documents
[0003]
Patent Document 1
Summary of the Invention
Problem to be Solved by the Invention
[0004] The electrode body of the lithium secondary battery configured as described above is formed by winding each sheet.
[0005] For example, on the winding center side of the electrode body, the winding radius is small. As a result, on the winding center side, the winding radius of the positive electrode mixture layer of the positive electrode sheet is also small, which may cause the positive electrode mixture layer to peel off or crack. A similar problem also occurs in the negative electrode mixture layer of the negative electrode sheet.
[0006] The present disclosure has been made in view of the above problems, and an object thereof is to provide an electricity storage cell in which the occurrence of cracks and the like in the electrode mixture layer is suppressed.
Means for Solving the Problem
[0007] [1] An electrode body formed by winding a sheet body so as to surround the periphery of a winding axis, and A case in which the electrode body is housed, Equipped with, The sheet body includes an electrode sheet and a separator. The electrode sheet includes a current collector plate and an electrode composite layer formed on the current collector plate. The electrode sheet has grooves extending in the direction of the winding axis, where the electrode composite layer is not formed, Multiple grooves are formed in the direction in which the electrode sheet extends. A storage cell in which the spacing between grooves on the inner side of the winding is smaller than the spacing between grooves on the outer side of the winding.
[0008] [2] The electrode body has a starting end portion of the winding body of the electrode body and a terminal end portion of the winding body of the electrode body, The energy storage cell according to [1], wherein the spacing between the grooves increases from the starting end to the ending end.
[0009] [3] The energy storage cell according to [1] or [2], wherein the groove width of the groove portion on the inner side of the winding is smaller than the groove width of the groove portion on the outer side of the winding.
[0010] [4] The electrode sheet includes a positive electrode sheet and a negative electrode sheet, The positive electrode sheet includes a positive electrode current collector plate and a positive electrode composite material layer formed on the positive electrode current collector plate. The positive electrode sheet has a positive electrode groove portion that extends in the direction of the winding axis and on which the positive electrode composite layer is not formed, The negative electrode sheet includes a negative electrode current collector plate and a negative electrode composite material layer formed on the negative electrode current collector plate. The negative electrode sheet has a negative electrode groove portion that extends in the direction of the winding axis and on which the negative electrode composite layer is not formed, The energy storage cell according to any one of [1] to [3], wherein the positive electrode groove and the negative electrode groove are formed to face each other.
[0011] [5] The energy storage cell according to [4], wherein the groove width of the negative electrode groove is smaller than the groove width of the positive electrode groove. [Effects of the Invention]
[0012] According to the power storage cell according to the present disclosure, occurrence of cracks and the like in the electrode mixture layer can be suppressed. [Brief Description of the Drawings]
[0013] [Figure 1] It is a cross-sectional view showing the power storage cell 1 according to the present embodiment. [Figure 2] It is a perspective view schematically showing the electrode body 10. [Figure 3] It is a plan view showing the positive electrode sheet 22. [Figure 4] It is a plan view showing the negative electrode sheet 24. [Figure 5] It is a developed view showing a state where the sheet body 20 is developed and the respective sheets are arranged side by side. [Figure 6] It is a cross-sectional view showing the positive electrode sheet 22, the negative electrode sheet 24, the separator 21 and the separator 23 in FIG. 5. [Mode for Carrying Out the Invention]
[0014] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. Note that the same reference numerals are assigned to the same or corresponding parts in the drawings, and descriptions thereof will not be repeated.
[0015] FIG. 1 is a cross-sectional view showing the power storage cell 1 according to the present embodiment. The power storage cell 1 includes a cylindrical electrode body 10 formed so as to surround the periphery of a winding axis O, a case 11, a positive electrode current collecting member 12, a negative electrode current collecting member 13, insulating members 14 and 15, and a positive electrode terminal 16.
[0016] Note that in FIG. 1 and the like, "Z" indicates the direction in which the winding axis O extends. "Z1" indicates one direction in the Z direction. "Z2" indicates the other direction in the Z direction. "R" indicates the radial direction of the electrode body 10.
[0017] The case 11 includes a top plate 17, a bottom plate 18, and a peripheral wall 19. The case 11 is made of a metal material. The top plate 17 is located at one end of the case 11, and the bottom plate 18 is located at the other end of the case 11. The peripheral wall 19 is positioned between the top plate 17 and the bottom plate 18.
[0018] Through holes 7 are formed in the top plate 17. The insulating member 14 is placed on the outer surface of the top plate 17, and through holes are formed in the insulating member 14.
[0019] The insulating member 15 includes a top plate portion 2 and a peripheral wall 3 provided on the outer peripheral edge of the top plate portion 2. The top plate portion 2 is located on the inner surface of the top plate 17. The peripheral wall 3 is located on the inner peripheral surface of the peripheral wall 19. Through holes are formed in the top plate 17.
[0020] The positive terminal 16 includes a flat plate 50 and a shaft 51. The flat plate 50 is positioned on the insulating member 14. The shaft 51 is connected to the flat plate 50 and is formed to extend in the Z2 direction. The shaft 51 is inserted into the case 11 through through holes 7 formed in the insulating member 14 and through holes formed in the insulating member 15.
[0021] The positive electrode current collector 12 is positioned on the Z2 direction side relative to the insulating member 15. The positive electrode current collector 12 is formed in a plate shape, and the lower end of the shaft 51 is welded to the upper surface of the positive electrode current collector 12. The positive electrode current collector 12 is made of, for example, aluminum.
[0022] The negative electrode current collector 13 is positioned on the inner surface of the bottom plate 18. The negative electrode current collector 13 is formed in a plate shape and is made of a metal material such as copper.
[0023] The electrode body 10 is positioned within the case 11 between the positive electrode current collector 12 and the negative electrode current collector 13.
[0024] The electrode body 10 includes a first end 5 located on the Z1 direction side, and a positive electrode current collector 12 is disposed on the first end 5. The electrode body 10 includes a second end 6 located on the Z2 direction side, and a negative electrode current collector 13 is disposed on the second end 6. The electrode body 10 is formed in a hollow shape, and a hollow portion 43 is formed. The hollow portion 43 is formed at a position passing through the winding axis O.
[0025] Figure 2 is a schematic perspective view of the electrode body 10. The electrode body 10 includes a sheet body 20 formed to surround the winding axis O. Note that "D" is the direction in which the sheet body 20 extends in the wound electrode body 10.
[0026] The sheet body 20 is formed in an elongated shape in the winding direction D of the electrode body 10. The sheet body 20 includes a separator 21, a positive electrode sheet 22, a separator 23, and a negative electrode sheet 24.
[0027] Figure 3 is a plan view showing the positive electrode sheet 22. The positive electrode sheet 22 shown in Figure 3 is in a state where it has been unwound from being wound around the electrode body 10 and spread out. The positive electrode sheet 22 includes long sides 30, 31 and short sides 32, 33. The long sides 30, 31 extend in the L1 direction from which the positive electrode sheet 22 extends. Note that the L1 direction corresponds to the winding direction D in the wound state of the electrode body 10. The long side 30 is located at the first end 5 of the wound electrode body 10, and the long side 31 is located at the second end 6 of the wound electrode body 10.
[0028] The positive electrode sheet 22 includes a positive electrode current collector plate 25 and a positive electrode composite material layer 26. The positive electrode current collector plate 25 is formed of a metallic material such as aluminum or an aluminum alloy.
[0029] The positive electrode composite layer 26 contains a positive electrode active material and a binder. Examples of positive electrode active materials include LiCoO2, LiNo2, and LiMn2O4. The thickness of the positive electrode composite layer 26 is, for example, 0.1 μm or more and 1000 μm or less.
[0030] The positive electrode composite layer 26 may be formed on either the front or back surface of the positive electrode current collector plate 25, or on one surface. The positive electrode sheet 22 has positive electrode grooves 27 that extend in the direction of the winding axis O and where the positive electrode composite layer 26 is not formed. Multiple positive electrode grooves 27 are formed in the direction in which the positive electrode sheet 22 extends. The positive electrode composite layer 26 is separated by multiple positive electrode grooves 27. If the positive electrode composite layer 26 is formed on either the front or back surface of the positive electrode current collector plate 25, the positive electrode grooves 27 may be formed on either of the positive electrode composite layers 26 on the front or back surface, or on one surface. If the positive electrode grooves 27 are formed on one surface, it is preferable that this surface is formed on the side that faces outward from the winding.
[0031] Figure 4 is a plan view showing the negative electrode sheet 24. The negative electrode sheet 24 shown in Figure 4 is in a state where it has been unwound from being wound around the electrode body 10 and spread out. The negative electrode sheet 24 includes long sides 36 and 37 and short sides 38 and 39. The long sides 36 and 37 extend in the L2 direction from which the negative electrode sheet 24 extends. Note that the L2 direction corresponds to the winding direction D in the wound state of the electrode body 10. The long side 36 is located at the first end 5 of the wound electrode body 10, and the long side 37 is located at the second end 6 of the wound electrode body 10.
[0032] The negative electrode sheet 24 includes a negative electrode current collector plate 34 and a negative electrode composite material layer 35. The negative electrode current collector plate 34 includes, for example, a metallic material such as copper.
[0033] The negative electrode composite layer 35 contains a negative electrode active material and a binder. The negative electrode active material is, for example, graphite. The thickness of the negative electrode composite layer 35 is, for example, 0.1 μm or more and 1000 μm or less.
[0034] The negative electrode composite layer 35 may be formed on either the front or back surface of the negative electrode current collector plate 34, or on only one surface. The negative electrode sheet 24 has negative electrode grooves 40 that extend in the direction of the winding axis O, where the negative electrode composite layer 35 is not formed. Multiple negative electrode grooves 40 are formed in the direction in which the negative electrode sheet 24 extends. The negative electrode composite layer 35 is separated by multiple negative electrode grooves 40. If the negative electrode composite layer 35 is formed on either the front or back surface of the negative electrode current collector plate 34, the negative electrode grooves 40 may be formed on either the front or back surface of the negative electrode composite layer 35, or on only one surface. If the negative electrode grooves 40 are formed on one surface, it is preferable that this surface is formed on the side that faces outward from the winding.
[0035] In Figure 1, the length of the negative electrode composite layer 35 is formed to be longer than the length of the positive electrode composite layer 26 in the Z direction.
[0036] Figure 5 is an unfolded view showing the sheet body 20 with each sheet laid out. The sheet body 20 is formed by placing a separator 23 on top of the negative electrode sheet 24, placing a positive electrode sheet 22 on top of the separator 23, and placing a separator 21 on top of the positive electrode sheet 22. Note that the positions of the negative electrode sheet 24 and the positive electrode sheet 22 may be swapped.
[0037] Separators 21 and 23 are formed in an elongated shape. Separator 21 includes long sides 70, 71 and short sides 72, 73. Separator 23 includes long sides 75, 76 and short sides 77, 78.
[0038] In Figure 5, the electrode body 10 includes an electrode composite layer 45, and the electrode composite layer 45 includes a positive electrode composite layer 26 and a negative electrode composite layer 35. The electrode body 10 has a starting end S of the winding body of the electrode body 10 and an ending end E of the winding body of the electrode body 10.
[0039] In the example shown in Figure 5, the starting end S has short sides 33 and 39. The ending end E has short sides 32 and 38. Note that short sides 33 and 39 may be offset in the winding direction D. In this case, when wound, the side closer to the winding axis O becomes the starting end S. Similarly, if short sides 32 and 38 are offset in the winding direction D, the side further away from the winding axis O becomes the ending end E. In the example shown in Figure 5, the short sides 73 and 78 of separators 21 and 23 are also located at the starting end S, and short sides 72 and 73 are also located at the ending end E. On the other hand, separators 21 and 23 may be formed to be longer in the winding direction D than the positive electrode sheet 22 and the negative electrode sheet 24.
[0040] Figure 6 is a cross-sectional view showing the positive electrode sheet 22, negative electrode sheet 24, separator 21, and separator 23 in Figure 5. The positive electrode current collector plate 25 includes a main surface 80 and a main surface 81. The positive electrode composite layer 26 includes a one-sided positive electrode composite layer 82 formed on the main surface 80 and a one-sided positive electrode composite layer 83 formed on the main surface 81.
[0041] The negative electrode current collector plate 34 includes a main surface 84 and a main surface 85. The negative electrode composite layer 35 includes a one-sided negative electrode composite layer 86 formed on the main surface 84 and a one-sided negative electrode composite layer 87 formed on the main surface 85.
[0042] In the example shown in Figure 6, the starting end S on the inner side of the winding is located on the right, and the ending end E on the outer side of the winding is located on the left. The spacing between grooves on the inner side of the winding (right side of Figure 6) is smaller than the spacing between grooves on the outer side of the winding (left side of Figure 6). Note that in Figure 6, the inner side is denoted as D1 and the outer side as D2, but this is merely an example and not limiting.
[0043] The electrode body 10 is formed so as to surround the winding axis O from the starting end S. Therefore, in the wound state of the electrode body 10, the curvature on the inside of the winding is greater than the curvature on the outside of the winding, resulting in a greater bending stress.
[0044] Therefore, on the inner winding side, there is a risk that cracks may occur in the electrode mixture layer 45. On the other hand, in the power storage cell 1 according to the present embodiment, the electrode sheet has a plurality of groove portions where the electrode mixture layer 45 is not formed, and the interval between the groove portions on the inner winding side is smaller than the interval between the groove portions on the outer winding side, so that the occurrence of cracks and the like in the electrode mixture layer 45 is suppressed.
[0045] In the positive electrode sheet 22 shown in FIG. 6, the intervals W1, W2, W3 between the positive electrode groove portions 27 on the inner winding side are smaller than the intervals W4, W5, W6 between the positive electrode groove portions 27 on the outer winding side. In the negative electrode sheet 24, the intervals X1, X2, X3 between the negative electrode groove portions 40 on the inner winding side are smaller than the intervals X4, X5, X6 between the negative electrode groove portions 40 on the outer winding side.
[0046] It is preferable that the interval between the groove portions increases from the start end S toward the end end E. When the groove portions are provided in the electrode mixture layer 45, the active material contained in the electrode mixture layer 45 decreases, so that the capacity is reduced. Therefore, instead of providing the groove portions uniformly in the electrode mixture layer 45, the groove portions are provided more on the inner winding side where the bending stress is large, thereby suppressing the decrease in capacity.
[0047] In the positive electrode sheet 22 shown in FIG. 6, the intervals between the positive electrode groove portions 27 are preferably W1<W2<W3<W4<W5<W6. In the negative electrode sheet 24, the intervals between the negative electrode groove portions 40 are preferably X1<X2<X3<X4<X5<X6.
[0048] It is preferable that the groove width of the groove portions on the inner winding side is smaller than the groove width of the groove portions on the outer winding side. This is because, on the inner winding side where the bending stress is large, the occurrence of cracks and the like in the electrode mixture layer 45 can be sufficiently suppressed even if the groove width of the groove portions is small. This is also because the area where the electrode mixture layer 45 is formed can be sufficiently secured while providing the groove portions.
[0049] In the positive electrode sheet 22 shown in FIG. 6, it is preferable that the groove widths Y1, Y2, Y3, Y4 of the positive electrode groove portions 27 on the winding inner side are smaller than the groove widths Y5, Y6, Y7 between the positive electrode groove portions 27 on the winding outer side. In the negative electrode sheet 24, it is preferable that the groove widths Z1, Z2, Z3, Z4 of the negative electrode groove portions 40 on the winding inner side are smaller than the groove widths Z5, Z6, Z7 between the negative electrode groove portions 40 on the winding outer side.
[0050] The groove width of the groove portion preferably increases from the start end S toward the terminal end E. This is because the bending stress is larger closer to the start end S.
[0051] In the positive electrode sheet 22 shown in FIG. 6, the groove widths of the positive electrode groove portions 27 preferably satisfy Y1<Y2<Y3<Y4<Y5<Y6<Y7. In the negative electrode sheet 24, the groove widths of the negative electrode groove portions 40 preferably satisfy Z1<Z2<Z3<Z4<Z5<Z6<Z7.
[0052] It is preferable that the positive electrode groove portions 27 and the negative electrode groove portions 40 are formed to face each other. When the negative electrode groove portions 40 are provided on the negative electrode sheet 24, the ratio at which the negative electrode groove portions 40 face the positive electrode sheet 22 increases, which may cause lithium to precipitate. Therefore, by forming the positive electrode groove portions 27 and the negative electrode groove portions 40 to face each other, the ratio at which the negative electrode groove portions 40 face the positive electrode sheet 22 is suppressed, whereby lithium precipitation can be suppressed.
[0053] In this case, the groove width of the negative electrode groove portion 40 is preferably smaller than the groove width of the opposing positive electrode groove portion 27. By doing this, lithium precipitation can be further suppressed.
[0054] In FIG. 6, it is preferable that Y1>Z1, Y2>Z2, Y3>Z3, Y4>Z4, Y5>Z5, Y6>Z6, and Y7>Z7.
[0055] The embodiments disclosed herein should be considered in all respects to be illustrative and not restrictive. This disclosure is indicated by the claims and is intended to include all modifications in the meaning and scope equivalent to the claims. [Explanation of Symbols]
[0056] 1 Energy storage cell, 2 Top plate, 3, 19 Peripheral wall, 5 First end, 6 Second end, 7 Through hole, 10, 10A Electrode body, 11 Case, 12 Positive electrode current collector, 13 Negative electrode current collector, 14, 15 Insulating member, 16 Positive electrode terminal, 17 Top plate, 18 Bottom plate, 20 Sheet body, 21, 23 Separator, 22 Positive electrode sheet, 24 Negative electrode sheet, 25 Positive electrode current collector plate, 26, 82, 83 Positive electrode composite layer, 27 Positive electrode groove, 30, 31, 36, 37, 70, 71, 75, 76 Long side, 32, 33, 38, 39, 72, 73, 77, 78 Short side, 34 Negative electrode current collector plate, 35, 86, 87 Negative electrode composite layer, 40 Negative electrode groove, 43 Hollow section, 45 electrode composite layer, 50 flat plate, 51 axis, 80, 81, 84, 85 main surface, D winding direction, D1 inside winding, D2 outside winding, E end section, O winding axis, S start end.
Claims
[Claim 1] An electrode body is wound around a winding axis, A case in which the electrode body is housed, Equipped with, The sheet body includes a positive electrode sheet, a negative electrode sheet, and a separator. The positive electrode sheet includes a positive electrode current collector plate and a positive electrode composite material layer formed on the positive electrode current collector plate. The positive electrode sheet has a positive electrode groove portion that extends in the direction of the winding axis and on which the positive electrode composite layer is not formed, Multiple positive electrode grooves are formed in the direction in which the positive electrode sheet extends. The negative electrode sheet includes a negative electrode current collector plate and a negative electrode composite material layer formed on the negative electrode current collector plate. The negative electrode sheet has a negative electrode groove portion that extends in the direction of the winding axis and on which the negative electrode composite layer is not formed, Multiple negative electrode grooves are formed in the direction in which the negative electrode sheet extends. The electrode body has a starting end portion of the winding body of the electrode body and a terminal end portion of the winding body of the electrode body, The spacing between the positive electrode grooves and the spacing between the negative electrode grooves increases from the starting end to the ending end. The groove width of the positive electrode groove and the groove width of the negative electrode groove increase from the starting end to the ending end. The positive electrode groove and the negative electrode groove are formed to face each other. The groove width of the negative electrode groove is smaller than the groove width of the opposing positive electrode groove. Energy storage cell.
Citation Information
Patent Citations
Rectangular battery and its manufacture
JP1998270068A
Lithium secondary battery
JP2001006749A
Storage battery element and its manufacturing method
JP2003257471A
Electrode group for nonaqueous secondary battery, and nonaqueous secondary battery using the same
JP2011146219A
Electrode structure for prismatic secondary battery
KR1020030031818A