Coating method and coating apparatus
The coating method employs laser cladding with curvature-matched laser beams and angled material injection to achieve a durable, uniform, and thin film on curved surfaces, addressing uneven temperature distribution and heat transfer issues.
Patent Information
- Application Number
- JP2022096596
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-06-15
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2042-06-15
AI Technical Summary
Existing coating methods struggle to achieve a uniform, thin, and durable film on curved surfaces, particularly in boiler tubes, due to uneven temperature distribution and increased thickness leading to deteriorated heat transfer.
A coating method using laser cladding with laser beams split by a diffractive optical element to match the curvature, combined with molten material injection at appropriate angles, ensuring uniform heat transfer and film thickness.
Enables a highly durable, thin, and uniform coating on curved surfaces at low cost, with increased film deposition rate and reduced heat input.
Smart Images

Figure 0007948528000001 
Figure 0007948528000002 
Figure 0007948528000003
Abstract
Description
Technical Field
[0001] The present invention relates to a coating method and a coating apparatus for coating the surface of a target object.
Background Art
[0002] As a method for coating the surface of a target object such as a boiler tube, a method using thermal spraying is known. In the method using thermal spraying, the film formation rate is high and the film formation area per unit time is large, so that coating can be performed at low cost. In addition, the thickness of the film formed on the surface of the target object can be reduced, and the film thickness can also be adjusted. However, the service life of the film formed by thermal spraying is generally about 1 to 2 years, and the durability is low.
[0003] As another coating method, a method using build-up welding is also conceivable (see, for example, Patent Document 1 below). In the method using build-up welding, although a highly durable film can be formed, the film formation rate is slow, and it is difficult to reduce the film thickness. When the target object is a boiler tube, there is also a problem that an increased coating film thickness increases the thickness of the boiler tube, leading to deteriorated heat transfer.
Prior Art Documents
Patent Documents
[0004]
Patent Document 1
Summary of the Invention
Problems to be Solved by the Invention
[0005] When the surface of an object includes curved surfaces, it is difficult to apply a coating with a uniform film thickness. That is, on curved surfaces, the distance from the light source is uneven, so the temperature distribution on the curved surface tends to be uneven, and as a result, the thickness of the film formed on the curved surface also tends to be uneven. For example, if the object has a circular cross-section, such as a boiler tube, if a film is deposited from above onto the outer surface of a horizontally extending boiler tube, the temperature will be higher in the center of the outer surface of the boiler (the part closest to the light source), and the temperature distribution on the outer surface (on the curved surface) will be uneven.
[0006] This invention has been made in view of the above circumstances, and aims to provide a coating method and a coating apparatus that can achieve a highly durable, thin, and uniform coating on the surface of an object having a curved surface at low cost. [Means for solving the problem]
[0007] (1) The coating method according to the present invention is a coating method for coating the surface of an object having a curved surface, and includes a laser output step, a laser branching step, and a coating step. In the laser output step, laser light is output from a light source. In the laser branching step, the laser light output from the light source is branched into a plurality of laser beams. In the coating step, while irradiating the plurality of laser beams toward the surface of the object, a molten material is sprayed into the optical path of the plurality of laser beams until they reach the surface of the object and melted, and fixed to the surface of the object, thereby coating the surface of the object, including the curved surface, by laser cladding. In the laser branching step, the laser light is branched such that the plurality of laser beams have an intensity corresponding to the shape of the curved surface.
[0008] With this configuration, when the laser light output from the light source is split into multiple laser beams and irradiated onto the surface of an object with a curved surface, the laser light is split so that each of the multiple laser beams has an intensity corresponding to the shape of the curved surface. This makes it possible to uniformly transfer heat to the curved surface, thus enabling coating with a uniform film thickness.
[0009] Furthermore, because the surface of the object is coated by laser cladding, it has high durability. In addition, since the molten material is injected into the optical path of multiple laser beams before reaching the surface of the object and melted, it is fixed to the surface of the object, allowing for the formation of a thin film thickness without the formation of a molten pool. Moreover, the heat input to the object can be reduced, and as a result, the film deposition rate can be increased. Therefore, a highly durable coating with a thin and uniform film thickness can be realized at low cost.
[0010] (2) In the laser branching step, the laser light output from the light source may be branched into multiple laser beams by a diffractive optical element.
[0011] With this configuration, a simple setup using a diffractive optical element can split the laser light output from a light source into multiple laser beams, which can then irradiate the surface of an object with a curved surface. Furthermore, by designing the diffractive optical element so that each of the multiple laser beams has an intensity corresponding to the shape of the curved surface, the multiple laser beams can be irradiated onto the surface of the object with appropriate intensity.
[0012] (3) The coating method may further include an element placement step. In the element placement step, a diffractive optical element corresponding to the shape of the curved surface may be selected and placed in the optical path of the laser light output from the light source. In the laser branching step, the laser light output from the light source may be branched into a plurality of laser beams by the diffractive optical element placed in the element placement step.
[0013] With this configuration, by selecting a diffractive optical element that corresponds to the shape of the curved surface and placing it in the optical path of the laser light output from the light source, multiple laser beams can be irradiated onto the surface of the object with appropriate intensity.
[0014] (4) In the coating step, the solvent may be sprayed at an angle corresponding to the shape of the curved surface.
[0015] With this configuration, the welding material can be irradiated onto a curved surface at an appropriate angle corresponding to its shape, resulting in a more uniform coating thickness.
[0016] (5) The coating apparatus according to the present invention is a coating apparatus for coating the surface of an object having a curved surface, and comprises a light source, a laser branching mechanism, and a molten material spraying mechanism. The light source outputs laser light. The laser branching mechanism branches the laser light output from the light source into a plurality of laser beams. The molten material spraying mechanism sprays a molten material. The coating apparatus irradiates the surface of the object with the plurality of laser beams, and sprays molten material from the molten material spraying mechanism into the optical path of the plurality of laser beams until they reach the surface of the object, melting and fixing it to the surface of the object, thereby coating the surface of the object, including the curved surface, by laser cladding. The laser branching mechanism branches the laser light such that the plurality of laser beams have an intensity corresponding to the shape of the curved surface.
[0017] With this configuration, when the laser light output from the light source is split into multiple laser beams and irradiated onto the surface of an object with a curved surface, the laser light is split so that each of the multiple laser beams has an intensity corresponding to the shape of the curved surface. This makes it possible to uniformly transfer heat to the curved surface, thus enabling coating with a uniform film thickness.
[0018] Furthermore, since the surface of the object is coated by laser cladding, the durability is high. Moreover, the filler material is injected into the optical path before the plurality of laser beams reach the surface of the object to be melted and adhered to the surface of the object, so that a film can be formed with a thin film thickness without forming a molten pool. In addition, the heat input to the object can be reduced, and as a result, the film forming rate can be increased. Therefore, a coating with high durability, a thin and uniform film thickness can be realized at low cost.
[0019] (6) The laser branching mechanism may include a diffractive optical element.
[0020] According to such a configuration, with a simple configuration using the diffractive optical element, the laser light output from the light source can be split into a plurality of laser beams to irradiate the surface of the object having a curved surface. Further, if the diffractive optical element is designed so that the plurality of laser beams have an intensity corresponding to the shape of the curved surface, the surface of the object can be irradiated with the plurality of laser beams at an appropriate intensity.
[0021] (7) The filler material injection mechanism may inject the filler material at an angle corresponding to the shape of the curved surface.
[0022] According to such a configuration, since the filler material can be injected onto the curved surface at an appropriate angle corresponding to its shape, coating with a more uniform film thickness can be achieved. [Advantageous Effects of the Invention]
[0023] According to the present invention, a coating with high durability, a thin and uniform film thickness can be realized at low cost on the surface of an object having a curved surface. [Brief Description of the Drawings]
[0024] [Figure 1] It is a schematic diagram showing a configuration example in the vicinity of a nozzle of a coating apparatus according to an embodiment of the present invention. [Figure 2] It is a schematic diagram for explaining the overall configuration of the coating apparatus. [Figure 3] This is a schematic diagram of the coating apparatus as viewed along the scanning direction. [Figure 4A] This diagram illustrates the intensity of each laser beam. [Figure 4B] This diagram illustrates the intensity of each laser beam. [Figure 5] This is a schematic diagram illustrating the direction of welding material injection. [Modes for carrying out the invention]
[0025] 1. Configuration of the coating apparatus Figure 1 is a schematic diagram showing an example of the configuration near the nozzle 100 of a coating apparatus according to one embodiment of the present invention. In this coating apparatus, coating is performed on the surface 11 of the object 1 using laser cladding.
[0026] In laser cladding, a laser beam 101 is used as a heat source. The laser beam 101, continuously emitted from the nozzle 100, is irradiated onto the surface 11 of the object 1. At the irradiation position 104 of the laser beam 101 on the surface 11 of the object 1, a rectangular irradiation area of, for example, about 20 mm × 1 mm is formed. However, the irradiation area is not limited to a rectangle; it may also be a circular or elliptical shape. The laser beam 101 may be parallel light, or it may be focused toward the irradiation position 104.
[0027] From the nozzle 100, a laser beam 101 is emitted while continuously spraying a welding material 102 and shielding gas 103 toward the object 1. The welding material 102 is, for example, a powdered material containing Inconel. The particle size of the welding material 102 powder is 20 to 40 μm, more preferably about 30 μm. The welding material 102 may consist only of Inconel, or it may contain other materials. Furthermore, the welding material 102 may be composed of materials other than Inconel.
[0028] In this embodiment, the welding material 102 ejected from the nozzle 100 enters the laser beam 101 before the irradiation position 104 (on the nozzle 100 side). That is, the welding material 102 is ejected onto the laser beam 101 while it is in flight. As a result, while irradiating the surface 11 of the object 1 with the laser beam 101, the welding material 102 is ejected into the optical path of the laser beam 101 until it reaches the surface 11 of the object 1, causing it to melt. After adhering to the surface 11 of the object 1, it is allowed to cool naturally, thereby fixing the welding material 102 to the surface 11 of the object 1.
[0029] As the shielding gas 103, an inert gas such as argon or helium is used. The welding material 102 injected from the nozzle 100 is injected into the shielding gas 103, thereby suppressing oxidation during flight. However, the shielding gas 103 can be omitted.
[0030] The nozzle 100 is moved along a predetermined scanning direction parallel to the surface 11 of the object 1. Therefore, by scanning the laser beam 101 over the surface 11 of the object 1 and injecting and melting the molten material 102 into the laser beam 101, a continuous build-up layer 2 can be formed on the surface 11 of the object 1, thereby coating the surface 11 of the object 1 (coating process). However, instead of moving the nozzle 100, the object 1 may be moved to scan the surface 11 of the object 1 with the laser beam 101.
[0031] The scanning speed of laser beam 101 is 1.0 m 2 / h or more, more preferably 1.2m 2 The rate is 1 / h or higher. Furthermore, the thickness of the build-up layer 2 formed on the surface 11 of the object 1 is 0.3 to 0.8 mm, more preferably about 0.5 mm.
[0032] In this embodiment, the welding material 102 is incident on the laser beam 101 from both sides in the scanning direction, flanking the laser beam 101. That is, the welding material 102 is incident on the laser beam 101 from multiple directions (for example, two directions). The welding material 102 incident on the laser beam 101 from each direction intersects at the intersection point 105 in the laser beam 101. By incidenting the welding material 102 on both sides in the scanning direction, flanking the laser beam 101, the film deposition efficiency can be improved.
[0033] Figure 2 is a schematic diagram illustrating the overall configuration of the coating apparatus. While Figure 1 described in detail the coating method for a single laser beam 101, in this embodiment, multiple laser beams 101 are irradiated toward the surface 11 of the object 1. For this purpose, the coating apparatus is equipped with a light source 200 and a laser branching mechanism 210.
[0034] The light source 200 includes a laser device and outputs laser light 201 generated by the laser device (laser output process). A semiconductor laser, fiber laser, or disk laser can be used as the laser device. The laser light 201 output from the light source 200 is incident on the laser branching mechanism 210.
[0035] The laser branching mechanism 210 includes a diffractive optical element (DOE) 211. Laser light 201 from the light source 200 that enters the laser branching mechanism 210 is branched into multiple laser beams 101 by the diffractive optical element 211 (laser branching process). The multiple laser beams 101 branched by the diffractive optical element 211 are irradiated onto the surface 11 of the object 1 in a multi-row x multi-column matrix.
[0036] The rectangular irradiation areas at irradiation positions 104 for each laser beam 101 branched by the diffractive optical element 211 are all the same shape. However, the diffractive optical element 211 may be designed so that the shape of the irradiation area at irradiation position 104 for each laser beam 101 is different. Furthermore, the intensity of each laser beam 101 can be arbitrarily adjusted by the design of the diffractive optical element 211.
[0037] A welding material 102 is injected into each laser beam 101 from the welding material injection mechanism 300. That is, the welding material injection mechanism 300 is configured to inject the welding material 102 individually into each laser beam 101. The incidence angle of the welding material 102 to each laser beam 101 may be the same or different. In this embodiment, the welding material injection mechanism 300 injects the welding material 102 into each laser beam 101 from both sides in the scanning direction, flanking each laser beam 101.
[0038] In this embodiment, multiple laser beams 101 are directed toward the surface 11 of the object 1, and a melting agent 102 is injected into the optical path of each laser beam 101 until it reaches the surface 11 of the object 1, causing it to melt and simultaneously fix to multiple irradiation positions 104 on the surface 11 of the object 1.
[0039] 2. Coating for curved surfaces Figure 3 is a schematic diagram of the coating apparatus as viewed along the scanning direction. As shown in Figure 3, for example, if the object 1 is a member with a circular cross-section, such as a boiler pipe used in a boiler panel, the surface 11 of the object 1 has a curved surface (arc surface) 111.
[0040] The optical path length of each laser beam 101 irradiated onto the curved surface 111 to the irradiation position 104 is non-uniform in the width direction perpendicular to the scanning direction, so the temperature distribution on the curved surface 111 is also likely to be non-uniform. Therefore, when the surface 11 of the object 1 includes a curved surface 111, it is difficult to apply a coating with a uniform film thickness. However, in this embodiment, the laser branching mechanism 210 (diffractive optical element 211) is designed to enable coating with a uniform film thickness.
[0041] Specifically, the laser splitting mechanism 210 splits the laser beam 201 so that the intensity of the laser beam 101 increases with the distance to the irradiation position 104 on the curved surface 111. As shown in the example in Figure 3, when the curved surface 111 is arc-shaped, the laser splitting mechanism 210 (diffractive optical element 211) is designed so that the intensity of the laser beam 101 is lowest when irradiated to the center of the curved surface 111, and the intensity of the laser beam 101 gradually increases as it moves toward both sides in the width direction (both sides in the circumferential direction) relative to this center.
[0042] In this way, by splitting the laser light 201 in the laser branching mechanism 210 so that multiple laser beams 101 have an intensity corresponding to the shape of the curved surface 111, heat can be uniformly transferred to the curved surface 111. However, "intensity corresponding to the shape of the curved surface 111" means, for example, that the longer the optical path length of each laser beam 101 to the irradiation position 104, the greater the intensity (power density (W / cm²)) of each laser beam 101. 2 This means that the ratio of the intensities of each laser beam 101 does not need to perfectly match the ratio of the optical path lengths to the irradiation position 104 of each laser beam 101. 4 W / cm 2 It is preferable that the above conditions are met.
[0043] As shown in Figure 3, it is preferable that the diffractive optical element 211 is configured to split the laser light 201 over a wide area so that each laser beam 101 irradiates the entire width of the surface 11 (top surface) of the object 1. In this case, the surface 11 (top surface) of the object 1 can be coated at once by scanning each laser beam 101 once in the scanning direction. However, the configuration is not limited to coating the surface 11 (top surface) of the object 1 in one scan, but may also be configured to coat it by scanning multiple times.
[0044] Figures 4A and 4B are diagrams illustrating the intensity of each laser beam 101. Figure 4A shows the case where the target object 1, a boiler tube, is relatively large in diameter, and Figure 4B shows the case where the target object 1, a boiler tube, is relatively small in diameter. In Figures 4A and 4B, the irradiation area corresponding to each laser beam 101 is shown as a rectangle, and the hatching applied to each irradiation area is shown as the intensity of each laser beam 101 increases with the density of the hatching.
[0045] As shown in Figure 4A, when the boiler tube, which is the object 1, has a relatively large diameter, the curvature of the curved surface 111 on the surface 11 of the object 1 becomes relatively small. Therefore, the change in intensity of each laser beam 101 along the width direction of the curved surface 111 is relatively gradual. Also, when attempting to coat the surface 11 (top surface) of the object 1 in a single scan, the width of the irradiation range R of the multiple laser beams 101 becomes relatively large.
[0046] On the other hand, as shown in Figure 4B, when the boiler tube, which is the object 1, has a relatively small diameter, the curvature of the curved surface 111 on the surface 11 of the object 1 becomes relatively large. Therefore, the change in intensity of each laser beam 101 along the width direction of the curved surface 111 becomes relatively steep. Also, even when attempting to coat the surface 11 (top surface) of the object 1 in one scan, the width of the irradiation range R of the multiple laser beams 101 is relatively small.
[0047] Thus, the irradiation range R of the multiple laser beams 101 and the change in intensity of each laser beam 101 within the irradiation range R differ depending on the shape of the curved surface 111 on the surface 11 of the object 1. Therefore, the design of the optimal diffractive optical element 211 also differs depending on the shape of the curved surface 111. By preparing multiple diffractive optical elements 211 with different designs in advance and selecting the diffractive optical element 211 that corresponds to the shape of the curved surface 111, and placing it in the optical path of the laser light 201 output from the light source 200 (element placement step), the laser light 201 can be branched using the optimal diffractive optical element 211.
[0048] Figure 5 is a schematic diagram illustrating the injection direction of the welding material 102. Each laser beam 101 is irradiated onto the surface 11 of the object 1 so as to extend parallel to each other, but the angles of the welding material 102 injected into each laser beam 101 do not have to be parallel to each other, as shown in Figure 5.
[0049] In the coating process, it is preferable that the welding material 102 is sprayed from the welding material spraying mechanism 300 at an angle corresponding to the shape of the curved surface 111 on the surface 11 of the object 1. The "angle corresponding to the shape of the curved surface 111" means, for example, that the larger the incident angle of each laser beam 101 with respect to the irradiation position 104, the larger the spraying angle θ of the welding material 102 with respect to each laser beam 101. The ratio of the incident angles of each laser beam 101 does not need to perfectly match the ratio of the spraying angles of the welding material 102 with respect to each laser beam 101.
[0050] Note that the incident angle of each laser beam 101 with respect to the irradiation position 104 refers to the inclination angle of each laser beam 101 with respect to the direction perpendicular to the curved surface 111 at the irradiation position 104. That is, when the curved surface 111 is arc-shaped, as in the example in Figure 5, the incident angle of the laser beam 101 irradiated to the center of the curved surface 111 is smallest, and the incident angle of the laser beam 101 gradually increases as it moves toward both sides in the width direction (both sides in the circumferential direction) relative to this center. Consequently, the injection angle θ of the welding material 102 with respect to the laser beam 101 irradiated to the center of the curved surface 111 is smallest, and the injection angle θ of the welding material 102 with respect to the laser beam 101 gradually increases as it moves toward both sides in the width direction (both sides in the circumferential direction) relative to this center.
[0051] 3. Effects In this embodiment, as illustrated in Figures 2 and 3, when the laser light 201 output from the light source 200 is split into multiple laser beams 101 and irradiated onto the surface 11 of an object 1 having a curved surface 111, the laser light 201 is split so that the multiple laser beams 101 have an intensity corresponding to the shape of the curved surface 111. This makes it possible to uniformly transfer heat to the curved surface 111, thereby enabling coating with a uniform film thickness.
[0052] Furthermore, as illustrated in Figure 1, the coating is highly durable because a build-up layer 2 is formed on the surface 11 of the object 1 by laser cladding. In addition, since a molten material 102 is injected into the optical path of multiple laser beams 101 before reaching the surface 11 of the object 1 and melted, and then fixed to the surface 11 of the object 1, a thin film thickness (e.g., 1 mm or less) can be formed without forming a molten pool. Also, the heat input to the object 1 can be reduced, and as a result, the film deposition rate can be increased. Therefore, a highly durable coating with a thin and uniform film thickness can be realized at low cost.
[0053] In particular, in this embodiment, a simple configuration using a diffractive optical element 211 allows the laser light 201 output from the light source 200 to be split into multiple laser beams 101 and irradiated onto the surface 11 of an object 1 having a curved surface 111. Furthermore, by designing the diffractive optical element 211 so that the multiple laser beams 101 have an intensity corresponding to the shape of the curved surface 111, the multiple laser beams 101 can be irradiated onto the surface 11 of the object 1 with an appropriate intensity.
[0054] Furthermore, in this embodiment, as illustrated in Figures 4A and 4B, by selecting a diffractive optical element 211 corresponding to the shape of the curved surface 111 and arranging it in the optical path of the laser light 201 output from the light source 200, multiple laser beams 101 can be irradiated onto the surface 11 of the object 1 with appropriate intensity.
[0055] Furthermore, in this embodiment, as illustrated in Figure 5, by spraying the welding material 102 at an angle corresponding to the shape of the curved surface 111, the welding material 102 can be irradiated onto the curved surface 111 at an appropriate angle corresponding to its shape, thereby enabling coating with a more uniform film thickness.
[0056] 4. Variations In the embodiments described above, a configuration was described in which the welding material 102 is incident into the laser beam 101 from both sides in the scanning direction, with the laser beam 101 in between. However, the configuration is not limited to this, and a configuration in which the welding material 102 is incident into the laser beam 101 from one direction may also be used, or a configuration in which the welding material 102 is incident into the laser beam 101 from three or more directions may also be used.
[0057] The laser branching mechanism 210 is not limited to a configuration that includes a diffractive optical element 211, but may also be configured to branch the laser light 201 into multiple laser beams 101 using components other than the diffractive optical element 211. [Explanation of Symbols]
[0058] 1. Object 2 Overlay layer 100 nozzles 101 Laser Beam 102 Welding material 103 Shielding gas 104 Irradiation position 105 intersection 111 Curved surface 200 light source 201 Laser light 210 Laser branching mechanism 211 Diffractive optical elements 300 Solvent injection mechanism
Claims
1. A coating method for coating the surface of an object having a curved surface, The laser output process involves outputting laser light from a light source, A laser branching step in which the laser light output from the light source is split into multiple laser beams extending parallel to each other, The process includes a coating step in which the surface of the object, including the curved surface, is coated by laser cladding by irradiating the surface of the object with the plurality of laser beams, injecting a molten material into the optical path of the plurality of laser beams until they reach the surface of the object, melting it, and fixing it to the surface of the object, A coating method comprising the laser branching step, in which the laser light is branched such that the multiple laser beams have an intensity corresponding to the shape of the curved surface, thereby branching the laser light so that the intensity of the laser beam increases with the distance to the irradiation position on the curved surface.
2. The coating method according to claim 1, wherein in the laser branching step, a diffractive optical element is used to branch the laser light output from the light source into a plurality of laser beams.
3. The process further includes selecting the diffractive optical element corresponding to the shape of the curved surface and arranging it in the optical path of the laser light output from the light source, The coating method according to claim 2, wherein in the laser branching step, the laser light output from the light source is branched into a plurality of laser beams by the diffractive optical element arranged in the element arrangement step.
4. The coating method according to claim 1, wherein in the coating step, the molten material is sprayed at an angle corresponding to the shape of the curved surface.
5. The coating method according to claim 1, wherein in the coating step, the plurality of laser beams are irradiated toward the surface of the object, and a molten material is sprayed individually toward each laser beam and from both sides in the scanning direction on either side of each laser beam in the optical path until the plurality of laser beams reach the surface of the object, melting and fixing the material to the surface of the object, thereby coating the surface of the object, including the curved surface, by laser cladding.
6. A coating apparatus for coating the surface of an object having a curved surface, A light source that emits laser light, A laser branching mechanism that splits the laser light output from the light source into multiple laser beams extending parallel to each other, It is equipped with a welding material injection mechanism that sprays the welding material, The method involves irradiating the surface of the object with the plurality of laser beams, and then injecting a molten material from the molten material injection mechanism into the optical path of the plurality of laser beams until they reach the surface of the object, melting it, and fixing it to the surface of the object, thereby coating the surface of the object, including the curved surface, by laser cladding. The laser branching mechanism is a coating apparatus that branches the laser light so that the multiple laser beams have an intensity corresponding to the shape of the curved surface, thereby branching the laser light so that the intensity of the laser beam increases with the distance to the irradiation position on the curved surface.
7. The coating apparatus according to claim 6, wherein the laser branching mechanism includes a diffractive optical element.
8. The coating apparatus according to claim 6, wherein the welding material injection mechanism injects the welding material at an angle corresponding to the shape of the curved surface.
9. The coating apparatus according to claim 6, wherein the surface of the object, including the curved surface, is coated by laser cladding by individually spraying a molten material onto each laser beam and from both sides in the scanning direction on either side of each laser beam in the optical path until the multiple laser beams reach the surface of the object, thereby fixing the molten material to the surface of the object.
Citation Information
Patent Citations
Seal machine for box body
JP1980029434A
Padding valve seat and padding method therefor
JP1998141132A
Apparatus and method for laser beam machining
JP2006320938A
Laser processing device
JP2012170985A
Laser processing apparatus, laser processing method, optical system, and padding finished article
JP2017113766A