Composition containing a large amount of polyol

A composition with cationic polymers and nonpolymeric acids forms a gel film to reduce stickiness and enhance moisturization in cosmetic products with high polyol content, improving user experience and efficacy.

JP7948808B2Active Publication Date: 2026-11-11LOREAL SA
View PDF 54 Cites 0 Cited by

Patent Information

Application Number
JP2022160348
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-10-04
Publication Date
2026-11-11
Estimated Expiration
2042-10-04

AI Technical Summary

Technical Problem

Cosmetic compositions containing large amounts of polyols like glycerin tend to be sticky, which affects their usability and user experience.

Method used

A composition comprising a cationic polymer, nonpolymeric acids or salts with multiple pKa values, a polyol, and water, where the polyol content is 10% or more by mass, forms a gel film or coacervate that reduces stickiness while maintaining the polyol on keratinous substances.

Benefits of technology

The composition achieves reduced stickiness and improved texture with enhanced moisturizing effects, allowing easy application and retention of polyols on the skin.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007948808000001
    Figure 0007948808000001
  • Figure 0007948808000002
    Figure 0007948808000002
  • Figure 0007948808000003
    Figure 0007948808000003
Patent Text Reader

Abstract

To provide a composition capable of exhibiting reduced stickiness while containing a large amount, i.e., 10 mass% or more, of a polyol such as glycerin based on the total mass of the composition.SOLUTION: The present invention relates to a composition containing: (a) at least one cationic polymer; (b) at least one non-polymeric acid or a salt thereof having two or more pKa values; (c) at least one polyol; and (d) water, the amount of (c) polyol in the composition being 10 mass% or more based on the total mass of the composition. Although the composition according to the invention contains a large amount of a polyol such as glycerin, it can exhibit reduced stickiness.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a composition containing a relatively large amount of polyol, and a cosmetic method using the composition. [Background technology]

[0002] Polyion complexes, which may be in the form of particles and can be formed from cationic and anionic polymers, are already known.

[0003] For example, WO2021 / 125069 discloses a composition useful for cosmetic treatments, comprising, in one embodiment, at least one polyion complex particle comprising at least one cationic polymer, at least one hyaluronic acid-based anionic polymer, and at least one nonpolymeric acid or salt thereof having two or more pKa values. WO2021 / 125069 also discloses a specific composition comprising 5% by mass of glycerin.

[0004] For example, WO2022 / 131351 discloses a composition useful for cosmetic treatments, which in one embodiment includes at least one polyion complex particle comprising at least one cationic polymer, at least one anionic polymer, at least one nonpolymeric acid or salt thereof having two or more pKa values, and at least one filler. WO2022 / 131351 also discloses a specific composition comprising 5% by mass of glycerin.

[0005] Polyols such as glycerin are often used for cosmetic purposes on keratinic substances in the skin. However, compositions containing large amounts of polyols such as glycerin, i.e., 10% or more by mass relative to the total mass of the composition, tend to be sticky. [Prior art documents] [Patent Documents]

[0006] [Patent Document 1] WO2021 / 125069 Patent Document 2 WO2022 / 131351 Patent Document 3 European Patent Application No. 0080976 Patent Document 4 French Patent No. 2077143 Patent Document 5 French Patent No. 2393573 Patent Document 6 French Patent No. 1492597 Patent Document 7 U.S. Patent No. 4,131,576 Patent Document 8 U.S. Patent No. 3,589,578 Patent Document 9 U.S. Patent No. 4,031,307 Patent Document 10 French Patent No. 2162025 Patent Document 11 French Patent No. 2280361 Patent Document 12 French Patent No. 2252840 Patent Document 13 French Patent No. 2368508 Patent Document 14 French Patent No. 1,583,363 Patent Document 15 U.S. Patent No. 3,227,615 Patent Document 16 U.S. Patent No. 2,961,347 Patent Document 17 French Patent No. 2080759 Patent Document 18 French Patent No. 2320330 Patent Document 19 French Patent No. 2270846 Patent Document 20 French Patent No. 2316271 Patent Document 21 French Patent No. 2336434 Patent Document 22 French Patent No. 2413907 [Patent Document 23] U.S. Patent No. 2,273,780 [Patent Document 24] U.S. No. 2,375,853 [Patent Document 25] U.S. Patent No. 2,388,614 [Patent Document 26] U.S. Patent No. 2,454,547 [Patent Document 27] U.S. Patent No. 3,206,462 [Patent Document 28] U.S. Patent No. 2,261,002 [Patent Document 29] U.S. Patent No. 2,271,378 [Patent Document 30] U.S. Patent No. 3,874,870 [Patent Document 31] U.S. Patent No. 4,001,432 [Patent Document 32] U.S. Patent No. 3,929,990 [Patent Document 33] U.S. Patent No. 3,966,904 [Patent Document 34] U.S. Patent No. 4,005,193 [Patent Document 35] U.S. Patent No. 4,025,617 [Patent Document 36] U.S. Patent No. 4,025,627 [Patent Document 37] U.S. Patent No. 4,025,653 [Patent Document 38] U.S. Patent No. 4,026,945 [Patent Document 39] U.S. Patent No. 4,027,020 [Patent Document 40] European Patent Application No. 0122324 [Patent Document 41] EP-A-0750899 [Patent Document 42] EP-A-1069172 [Patent Document 43] EP-A-0173109 [Non-patent literature]

[0007] [Non-Patent Document 1] "Micelle formation of random copolymers of sodium 2-(acrylamido)-2-methylpropanesulfonate and nonionic surfactant macromonomer in water as studied by fluorescence and dynamic light scattering" - Macromolecules, 2000, Vol. 33, No. 10-3694~3704 [Non-Patent Document 2] "Hyaluronan fragments: an information-rich system", R. Stern et al., European Journal of Cell Biology 58 (2006), pp. 699-715 [Non-Patent Document 3] D. Campoccia et al., "Semisynthetic resorbable materials from hyaluronan esterification", Biomaterials 19 (1998) pp. 2101-2127 [Overview of the Initiative] [Problems that the invention aims to solve]

[0008] Therefore, the object of the present invention is to provide a composition that can exhibit reduced stickiness while containing a large amount of polyol such as glycerin, i.e., 10% by mass or more relative to the total mass of the composition. [Means for solving the problem]

[0009] The above objective of the present invention is, (a) at least one cationic polymer, (b) Nonpolymeric acids or salts thereof having at least one of two or more pKa values, (c) at least one polyol, and (d) water A composition comprising, This can be achieved by a composition in which the amount of (c) polyol in the composition is 10% by mass or more relative to the total mass of the composition.

[0010] (a) The cationic polymer may be crosslinked with (b) two or more nonpolymeric acids or salts thereof having pKa values.

[0011] (a) The cationic polymer may have at least one positive charge selected from the group consisting of primary, secondary, or tertiary amino groups, quaternary ammonium groups, guanidine groups, biguanide groups, imidazole groups, imino groups, and pyridyl groups, and / or may have a positively charged moiety.

[0012] (a) The cationic polymer can be selected from the group consisting of alkyldiallylamine cyclopolymers and dialkyldiallylammonium cyclopolymers, e.g., (co)polydiallyldialkylammonium chloride, (co)polyamines, e.g., chitosan and (co)polylysine, cationic (co)polyamino acids, e.g., collagen, cationic cellulose polymers, and salts thereof.

[0013] (a) The cationic polymer may be more preferably selected from the group consisting of polylysine, chitosan, and mixtures thereof.

[0014] The amount of (a) cationic polymer in the composition according to the present invention may be 0.01% to 15% by mass, preferably 0.05% to 10% by mass, and more preferably 0.1% to 5% by mass, based on the total mass of the composition.

[0015] (b) The nonpolymeric acid or salt thereof having two or more pKa values ​​may be an organic acid or salt thereof, preferably a hydrophilic or water-soluble organic acid or salt thereof, more preferably phytic acid or salt thereof, terephthalylidene dicamfersulfonic acid or salt thereof, or a mixture thereof.

[0016] The amount of (b) a nonpolymeric acid or salt thereof having two or more pKa values ​​in the composition according to the present invention may be 0.01% to 15% by mass, preferably 0.05% to 10% by mass, and more preferably 0.1% to 5% by mass, based on the total mass of the composition.

[0017] (c) The polyol may preferably be glycerin.

[0018] The amount of (c) polyol in the composition according to the present invention may be 95% by mass or less of the total mass of the composition.

[0019] The composition according to the present invention may further contain (e) at least one anionic polymer.

[0020] (e) The anionic polymer may be selected from polysaccharides, preferably hyaluronic acid and its derivatives, cellulose polymers and their salts, and mixtures thereof, more preferably hyaluronic acid and its salts, carboxymethylcellulose and its salts, and mixtures thereof.

[0021] The amount of (e) anionic polymer in the composition according to the present invention may be 0.01% to 15% by mass, preferably 0.05% to 10% by mass, and more preferably 0.1% to 5% by mass, based on the total mass of the composition.

[0022] The composition according to the present invention may be a cosmetic composition, preferably a care cosmetic composition, and more preferably a skin care or hair care cosmetic composition.

[0023] The present invention also relates to a cosmetic method for keratin substances, A step of applying the composition according to the present invention to a keratin substance, The present invention also relates to a cosmetic method, which includes the step of drying the composition to form a cosmetic film on a keratin substance. [Modes for carrying out the invention]

[0024] As a result of diligent research, the inventors have discovered that it is possible to provide a composition that exhibits reduced stickiness while containing a large amount of polyol such as glycerin, i.e., 10% by mass or more relative to the total mass of the composition.

[0025] Therefore, the composition according to the present invention, (a) at least one cationic polymer, (b) Nonpolymeric acids or salts thereof having at least one of two or more pKa values, (c) at least one polyol, and (d) water Includes, The amount of (c) polyol in the composition is 10% by mass or more relative to the total mass of the composition.

[0026] The composition according to the present invention contains a large amount of polyol such as glycerin, but can exhibit reduced stickiness.

[0027] The stickiness of the composition according to the present invention is less than that of a composition containing component (c) in an amount of 10% by mass or more relative to the total mass of the composition, and not containing components (a) and (b).

[0028] Therefore, the composition according to the present invention can provide an improved texture, such as a smoother feel.

[0029] Polyols such as glycerin are hydrophilic and therefore can be easily washed off the surface of keratinous substances with water. However, components (a) and (b) in the composition according to the present invention can form a gel film or coacervate that can effectively maintain the polyol on keratinous substances such as skin.

[0030] Therefore, the composition according to the present invention can also provide enhanced cosmetic effects derived from polyols, such as enhanced moisturizing effects.

[0031] The compositions and methods according to the present invention will be described in more detail below.

[0032] (cationic polymer) The composition according to the present invention comprises (a) at least one cationic polymer.

[0033] (a) There are no limitations on the type of cationic polymer. Two or more different types of cationic polymers may be used in combination. Therefore, a single type of cationic polymer or a combination of different types of cationic polymers can be used.

[0034] Cationic polymers have a positive charge density. (a) The charge density of the cationic polymer may be 0.01 meq / g to 20 meq / g, preferably 0.05 to 15 meq / g, and more preferably 0.1 to 10 meq / g.

[0035] (a) It is preferable that the molecular weight of the cationic polymer is 1,000 or more, preferably 2,000 or more, more preferably 3,000 or more, and even more preferably 4,000 or more.

[0036] Unless otherwise defined in the explanation, "molecular weight" refers to the number-average molecular weight.

[0037] (a) The cationic polymer may have at least one positively charged moiety selected from the group consisting of primary, secondary, or tertiary amino groups, quaternary ammonium groups, guanidine groups, biguanide groups, imidazole groups, imino groups, and pyridyl groups. The term (primary) "amino group" as used herein means an -NH2 group.

[0038] (a) The cationic polymer may be a homopolymer or a copolymer. The term “copolymer” is understood to mean both copolymers obtained from two monomers and terpolymers obtained from more than two monomers, for example, three monomers.

[0039] (a) Cationic polymers may be selected from natural and synthetic cationic polymers. (a) Non-limiting examples of cationic polymers are as follows:

[0040] (1) Homopolymers and copolymers are defined by the following units:

[0041] [ka]

[0042] (In the formula: R1 and R2 may be the same or different, and are selected from hydrogen and alkyl groups containing 1 to 6 carbon atoms, such as methyl and ethyl groups. R3 may be the same or different, and is selected from hydrogen and CH3. Symbol A may be the same or different, and is selected from linear or branched alkyl groups containing 1 to 6 carbon atoms, for example, 2 to 3 carbon atoms, and hydroxyalkyl groups containing 1 to 4 carbon atoms. R4, R5, and R6 may be the same or different, and are selected from alkyl groups containing 1 to 18 carbon atoms, benzyl groups, and, in at least one embodiment, alkyl groups containing 1 to 6 carbon atoms. X is derived from esters and amides of acrylic acid or methacrylic acid, comprising at least one unit selected from anions derived from inorganic or organic acids (e.g., methsulfate anions, and halide ions such as chloride ions and bromide ions).

[0043] The copolymers of Family (1) described above may also comprise at least one unit derived from a comonomer, which can be selected from acrylamide, methacrylamide, diacetoneacrylamide, acrylamide and methacrylamide in which the nitrogen atom is substituted with a (C1-C4) lower alkyl group, a group derived from acrylic acid or methacrylic acid and its esters, vinyl lactams, such as vinylpyrrolidone and vinylcaprolactam, and vinyl esters.

[0044] Examples of copolymers in Family (1) include, but are not limited to, the following: Copolymers of acrylamide and dimethylaminoethyl methacrylate quaternized with dimethyl sulfate or dimethyl halogen, e.g., described in European Patent Application No. 0080976; copolymers of acrylamide and methacryloyloxyethyltrimethylammonium chloride; copolymers of acrylamide and methacryloyloxyethyltrimethylammonium methosulfate, e.g., described in French Patents No. 2077143 and 2393573; quaternized or non-quaternized vinylpyrrolidone / acrylic acid or dialkylaminoalkyl methacrylate copolymers; dimethylaminoethyl methacrylate / vinylcaprolactam / vinyl Examples include pyrrolidone polymers, vinylpyrrolidone / methacrylamidopropyldimethylamine copolymers, quaternized vinylpyrrolidone / dimethylaminopropylmethacrylamido copolymers, and crosslinked methacryloyloxy(C1-C4)alkyltri(C1-C4)alkylammonium salt polymers, such as homopolymers of dimethylaminoethyl methacrylate quaternized with methyl chloride, or copolymers of acrylamide and dimethylaminoethyl methacrylate quaternized with methyl chloride, or polymers obtained by crosslinking the homopolymer or copolymer with a compound containing olefinic unsaturation, such as methylenebisacrylamide.

[0045] (2) Cationic cellulose polymers, such as cellulose ether derivatives containing one or more quaternary ammonium groups, as described in French Patent No. 1492597, and polymers sold by Union Carbide Corporation under the names "JR" (JR 400, JR 125, JR 30M) or "LR" (LR 400, LR 30M). These polymers are also defined in the CTFA dictionary as quaternary ammonium of hydroxyethylcellulose reacted with an epoxide substituted with a trimethylammonium group.

[0046] It is preferable that the cationic cellulose polymer has at least one quaternary ammonium group, preferably a quaternary trialkylammonium group, and more preferably a quaternary trimethylammonium group.

[0047] The quaternary ammonium group has the following chemical formula (I):

[0048] [ka]

[0049] (In the formula, Each of R1 and R2 represents a C1-C3 alkyl group, preferably a methyl group or an ethyl group, more preferably a methyl group. R3 is C1~C 24 The alkyl group is preferably a methyl group or an ethyl group, more preferably a methyl group. X- represents an anion, preferably a halide ion, more preferably a chloride ion. n represents an integer between 0 and 30, preferably between 0 and 10, more preferably 0. R4 may be present in a quaternary ammonium group-containing group that can be represented by a C1-C4 alkylene group, preferably an ethylene group or a propylene group.

[0050] The leftmost ether bond (-O-) in the above chemical formula (I) can bond to the sugar ring of a polysaccharide.

[0051] The quaternary ammonium group-containing group is -O-CH2-CH(OH)-CH2-N + (CH3)3 is preferred.

[0052] (3) Cationic cellulose polymers such as cellulose copolymers and cellulose derivatives described in, for example, U.S. Patent No. 4,131,576, grafted with water-soluble monomers of quaternary ammonium, such as hydroxyalkylcellulose, for example, hydroxymethyl-, hydroxyethyl-, and hydroxypropylcellulose grafted with salts selected from, for example, methacryloylethyltrimethylammonium salt, methacrylamidopropyltrimethylammonium salt, and dimethyldiallylammonium salt.

[0053] Examples of commercially available products equivalent to these polymers include those sold by National Starch under the names "Celquat® L 200" and "Celquat® H 100".

[0054] (4) Non-cellulose cationic polysaccharides as described in U.S. Patents No. 3,589,578 and No. 4,031,307, such as guar gum containing a cationic trialkylammonium group, cationic hyaluronic acid, and dextran hydroxypropyltrimonium chloride. Guar gum modified with salts, such as 2,3-epoxypropyltrimethylammonium chloride (guar hydroxypropyltrimonium chloride), may also be used.

[0055] Such products are sold by MEYHALL, for example, under the product names JAGUAR®C13 S, JAGUAR®C15, JAGUAR®C17, and JAGUAR®C162.

[0056] (5) Polymers comprising a divalent alkylene or hydroxyalkylene group comprising a piperazinyl unit and a linear or branched chain optionally interposed by at least one entity selected from oxygen, sulfur, nitrogen, aromatic rings and heterocycles, as well as oxidation and / or quaternization products of these polymers. Such polymers are described, for example, in French Patent Nos. 2162025 and 2280361.

[0057] (6) For example, water-soluble polyaminoamides prepared by polycondensation of an acidic compound with a polyamine, these polyaminoamides may be crosslinked with an oligomer obtained from the reaction of a bifunctional compound that is reactive with an entity selected from an entity selected from bishalohydrins, bisazetidinium, bishaloacyldiamines, bisalkyl halides, bishalohydrins, bisazetidinium, bishaloacyldiamines, bisalkyl halides, epihalohydrins, diexides and bisunsaturated derivatives; the crosslinking agent is used in an amount ranging from 0.025 to 0.35 mol per amine group of the polyaminoamide; these polyaminoamides may optionally be alkylated, or if they contain at least one tertiary amine functional group, they may be quaternized. Such polymers are described, for example, in French Patent Nos. 2252840 and 2368508.

[0058] (7) Polyaminoamide derivatives obtained by condensing a polyalkylene polyamine with a polycarboxylic acid and subsequently alkylating it with a bifunctional agent, such as adipic acid / dialkylaminohydroxyalkyldialkylentriamine polymers, in which the alkyl group contains 1 to 4 carbon atoms, such as methyl, ethyl, and propyl groups, and the alkylene group contains 1 to 4 carbon atoms, such as an ethylene group. Such polymers are described, for example, in French Patent No. 1,583,363. In at least one embodiment, these derivatives may be selected from adipic acid / dimethylaminohydroxypropyldiethylenetriamine polymers.

[0059] (8) A polymer obtained by the reaction of a polyalkylene polyamine containing two primary amine groups and at least one secondary amine group with diglycolic acid and a dicarboxylic acid selected from saturated aliphatic dicarboxylic acids containing 3 to 8 carbon atoms. The molar ratio of the polyalkylene polyamine to the dicarboxylic acid may be in the range of 0.8:1 to 1.4:1, and the resulting polyaminoamide is reacted with epichlorohydrin in a molar ratio of epichlorohydrin to the secondary amine groups of the polyaminoamide in the range of 0.5:1 to 1.8:1. Such polymers are described, for example, in U.S. Patent Nos. 3,227,615 and 2,961,347.

[0060] (9) Cyclopolymers of alkyldiallylamines and cyclopolymers of dialkyldiallylammonium, for example, with formulas (Ia) and (Ib) as the main components of the chain:

[0061] [ka]

[0062] (In the formula: k and t may be the same or different, and are equal to 0 or 1, and their sum k+t is equal to 1. R 12 It is selected from hydrogen and methyl groups, R 10 and R 11 These may be the same or different, and are selected from alkyl groups containing 1 to 6 carbon atoms, hydroxyalkyl groups in which the alkyl group contains, for example, 1 to 5 carbon atoms, and lower (C1 to C4) amide alkyl groups, or R 10 and R 11 These may, together with the nitrogen atom to which they are bonded, form heterocyclic groups, such as piperidinyl and morpholinyl. Y' is an anion, for example, selected from bromide ion, chloride ion, acetate ion, borate ion, citrate ion, tartrate ion, bisulfate ion, hydrogen sulfite ion, sulfate ion and phosphate ion), homopolymers and copolymers comprising at least one unit selected from the units. These polymers are described, for example, in French Patent No. 2080759 and its additional patent No. 2190406.

[0063] In one embodiment, R 10 and R 11 may be the same or different and are selected from alkyl groups containing 1 to 4 carbon atoms.

[0064] Examples of such polymers include, but are not limited to, (co-)polydiallyldialkylammonium chlorides, for example, the dimethyldiallylammonium chloride homopolymer (Polyquaternium-6) sold by CALGON under the name "MERQUAT (registered trademark) 100" (and its homologs of low weight-average molecular weight), as well as the copolymer of diallyldimethylammonium chloride and acrylamide sold under the name "MERQUAT (registered trademark) 550".

[0065] (10) Formula (II):

[0066] [Formula]

[0067] (wherein: R 13 , R 14 , R 15 and R 16 may be the same or different and are selected from aliphatic, alicyclic and araliphatic groups containing 1 to 20 carbon atoms, as well as lower hydroxyalkyl aliphatic groups, or alternatively, R 13 , R 14 , R 15 and R 16These may form a heterocycle containing, either together with or separately from the nitrogen atom to which they are bonded, a second heteroatom other than nitrogen of any choice, or R 13 , R 14 , R 15 and R 16 These may be the same or different, and include nitrile groups, ester groups, acyl groups, amide groups, and -CO-OR groups. 17 -E group and -CO-NH-R 17 -E group (in the formula, R 17 (where is an alkylene group and E is a quaternary ammonium group) is selected from linear or branched C1-C6 alkyl groups which are substituted with at least one group selected from the above, A1 and B1 may be the same or different, selected from a polymethylene group containing 2 to 20 carbon atoms, which may be linear or branched, saturated or unsaturated, and which may contain, linked to or inserted into the main chain, at least one entity selected from an aromatic ring, oxygen, sulfur, sulfoxide group, sulfone group, disulfide group, amino group, alkylamino group, hydroxyl group, quaternary ammonium group, ureido group, amide group, and ester group. X - These are anions derived from inorganic or organic acids, A1, R 13 and R 15 These may also form a piperazine ring together with the two nitrogen atoms to which they are bonded. If A1 is selected from linear or branched, saturated or unsaturated alkylene or hydroxyalkylene groups, then B1 is as follows: -(CH2) n -CO-E'-OC-(CH2) n - [In the formula, E' is as follows: a) Glycol residue of formula -OZO- {wherein Z is a linear or branched hydrocarbon group, and the following formula: -(CH2-CH2-O) x -CH2-CH2- -[CH2-CH(CH3)-O] y -CH2-CH(CH3)- (In the formula, x and y may be the same or different, and are selected from integers in the range of 1 to 4 representing a defined unique degree of polymerization, and numbers in the range of 1 to 4 representing the average degree of polymerization.) Selected from the base}, b) Bis-secondary diamine residues, e.g., piperazine derivatives, c) Bis-primary diamine residues of the formula -NH-Y-NH- (wherein Y is selected from linear or branched hydrocarbon groups and divalent groups -CH2-CH2-SS-CH2-CH2-), and d) Urylene group of formula -NH-CO-NH- A quaternary diammonium polymer comprising at least one repeating unit of [selected from] (may be selected from).

[0068] In at least one embodiment, X - These are anions, such as chloride ions or bromide ions.

[0069] This type of polymer is, for example, described in French Patent Nos. 2320330, 2270846, 2316271, 2336434 and 2413907, and US Patent Nos. 2,273,780, 2,375,853, 2,388,614, 2,454,547, 3,206,462 and 2,261,000. It is described in No. 2, No. 2,271,378, No. 3,874,870, No. 4,001,432, No. 3,929,990, No. 3,966,904, No. 4,005,193, No. 4,025,617, No. 4,025,627, No. 4,025,653, No. 4,026,945, and No. 4,027,020.

[0070] A non-limiting example of such a polymer is equation (III):

[0071] [ka]

[0072] (In the formula, R 13, R 14 , R 15 and R 16 n and p may be the same or different, selected from alkyl groups and hydroxyalkyl groups containing 1 to 4 carbon atoms, n and p may be the same or different, integers in the range of 2 to 20, X - Examples include those containing at least one repeating unit of an anion derived from an inorganic or organic acid.

[0073] (11) Formula (IV):

[0074] [ka]

[0075] (In the formula: R 18 , R 19 , R 20 and R 21 These may be the same or different, and include hydrogen, methyl group, ethyl group, propyl group, β-hydroxyethyl group, β-hydroxypropyl group, and -CH2CH2(OCH2CH2). p The OH group is selected from the OH group (where p is an integer in the range of 0 to 6), however, R 18 , R 19 , R 20 and R 21 They cannot be hydrogen at the same time. r and s may be the same or different, and are selected from integers in the range of 1 to 6. q is selected from integers in the range of 0 to 34. X - These are anions, such as halide ions. A is a polyquaternary ammonium polymer containing units (selected from dihalide and -CH2-CH2-O-CH2-CH2- groups).

[0076] Such compounds are described, for example, in European Patent Application No. 0122324.

[0077] (12) Quaternary polymer of vinylpyrrolidone and vinylimidazole.

[0078] Other suitable cationic polymers include, but are not limited to, cationic proteins and cationic protein hydrolysates, polyalkyleneimines such as polyethyleneimine, polymers containing units selected from vinylpyridine units and vinylpyridinium units, condensates of polyamines and epichlorohydrins, quaternary polyurenes, and chitin derivatives.

[0079] According to one embodiment of the present invention, (a) the cationic polymer is selected from cellulose ether derivatives containing quaternary ammonium groups, such as the product sold by UNION CARBIDE CORPORATION under the name "JR 400", cationic cyclopolymers, such as homopolymers and copolymers of dimethyldiallylammonium chloride sold by CALGON under the names MERQUAT® 100, MERQUAT® 550 and MERQUAT® S, guar gum modified with 2,3-epoxypropyltrimethylammonium salt, and quaternary polymers of vinylpyrrolidone and vinylimidazole.

[0080] (13) Polyamines (a) As the cationic polymer, a (co)polyamine may be used, which may be a homopolymer or copolymer having multiple amino groups. The amino groups may be primary, secondary, tertiary, or quaternary amino groups. The amino groups may be present in the polymer backbone of the (co)polyamine, or in the pendant groups, if present.

[0081] Examples of (co)polyamines include chitosan, (co)polyallylamine, (co)polyvinylamine, (co)polyaniline, (co)polyvinylimidazole, (co)polydimethylaminoethylene methacrylate, (co)polyvinylpyridine, e.g., (co)poly-1-methyl-2-vinylpyridine, (co)polyimines, e.g., (co)polyethyleneimine, (co)polypyridine, e.g., (co)poly(quaternary pyridine), (co)polybiguanides, e.g., (co)polyaminopropylbiguanides, (co)polylysine, (co)polyornithine, (co)polyarginine, (co)polyhistidine, aminodextran, aminocellulose, amino(co)polyvinylacetal, and salts thereof.

[0082] (a) The cationic polymer may preferably be selected from chitosan.

[0083] (a) The cationic polymer may preferably be selected from (co)polylysine.

[0084] Polylysine is well known. Polylysine may be a natural homopolymer of L-lysine that can be produced by bacterial fermentation. For example, polylysine may be α-poly-L-lysine and ε-poly-L-lysine, which are typically used as natural preservatives in food. Polylysine is a polyelectrolyte soluble in polar solvents, such as water, propylene glycol, and glycerol. Polylysine is commercially available in various forms, such as poly-D-lysine and poly-L-lysine. Polylysine may also be in the form of a salt and / or solution.

[0085] (14) Cationic polyamino acids (a) As the cationic polymer, it may be possible to use a cationic polyamino acid which may be a cationic homopolymer or copolymer having multiple amino groups and carboxyl groups. The amino groups may be primary, secondary, tertiary, or quaternary amino groups. The amino groups may be present in the polymer backbone of the cationic polyamino acid, or in the pendant groups if present. The carboxyl groups may be present in the pendant groups of the cationic polyamino acid if present.

[0086] Examples of cationic polyamino acids include cationized collagen, cationized gelatin, steardimonium hydroxypropyl hydrolyzed wheat protein, cocodimonium hydroxypropyl hydrolyzed wheat protein, hydroxypropyltrimonium hydrolyzed conchiolin protein, steardimonium hydroxypropyl hydrolyzed soy protein, hydroxypropyltrimonium hydrolyzed soy protein, and cocodimonium hydroxypropyl hydrolyzed soy protein.

[0087] The following description relates to (a) preferred embodiments of cationic polymers.

[0088] (a) It may be preferable that the cationic polymer is selected from the group consisting of alkyldiallylamine cyclopolymers and dialkyldiallylammonium cyclopolymers, such as (co)polydiallyldialkylammonium chloride, (co)polyamines, such as chitosan and (co)polylysine, cationic (co)polyamino acids, such as cationized collagen, cationic cellulose polymers, and salts thereof.

[0089] (a) The cationic polymer may be more preferably selected from the group consisting of polylysine, chitosan, and mixtures thereof.

[0090] The amount of (a) cationic polymer in the composition according to the present invention may be 0.01% by mass or more, preferably 0.05% by mass or more, and more preferably 0.1% by mass or more, based on the total mass of the composition.

[0091] The amount of (a) cationic polymer in the composition according to the present invention may be 15% by mass or less, preferably 10% by mass or less, and more preferably 5% by mass or less, based on the total mass of the composition.

[0092] The amount of (a) cationic polymer in the composition according to the present invention may be 0.01% to 15% by mass, preferably 0.05% to 10% by mass, and more preferably 0.1% to 5% by mass, based on the total mass of the composition.

[0093] (Anionic polymer) The composition according to the present invention may (e) contain at least one anionic polymer.

[0094] If the composition according to the present invention contains (e) an anionic polymer, (a) a cationic polymer can form a polyionic complex together with (e) the anionic polymer.

[0095] (e) There are no limitations on the type of anionic polymer. Two or more different types of anionic polymers may be used in combination. Therefore, a single type of anionic polymer or a combination of different types of anionic polymers can be used.

[0096] The anionic polymer has a positive charge density. (e) If the anionic polymer is a synthetic anionic polymer, the charge density of the anionic polymer may be 0.1 meq / g to 20 meq / g, preferably 1 to 15 meq / g, more preferably 4 to 10 meq / g, and (e) if the anionic polymer is a natural anionic polymer, the average degree of substitution of the anionic polymer may be 0.1 to 3.0, preferably 0.2 to 2.7, more preferably 0.3 to 2.5.

[0097] (e) The molecular weight of the anionic polymer is preferably 1,000 or more, more preferably 3,000 or more, more preferably 5,000 or more, more preferably 10,000 or more, more preferably 50,000 or more, more preferably 100,000 or more, and more preferably 1,000,000 or more.

[0098] Unless otherwise defined in the explanation, "molecular weight" can refer to the number-average molecular weight.

[0099] (e) The anionic polymer may have at least one negatively charged and / or a negatively charged moiety selected from the group consisting of sulfate groups, sulfate groups, sulfonic acid groups, sulfonate groups, phosphoric acid groups, phosphate groups, phosphonic acid groups, phosphonate groups, carboxylic acid groups, and carboxylate groups.

[0100] (e) The anionic polymer may be a homopolymer or a copolymer. The term “copolymer” is understood to mean both copolymers obtained from two monomers and terpolymers obtained from more than two monomers, for example, three monomers.

[0101] (e) The anionic polymer can be selected from natural and synthetic anionic polymers.

[0102] (e) The anionic polymer may contain at least one hydrophobic chain.

[0103] An anionic polymer that may contain at least one hydrophobic chain can be obtained by copolymerizing monomer (a), selected from carboxylic acid containing α,β-ethylenically unsaturated compounds (monomer a') and 2-acrylamido-2-methylpropanesulfonic acid (monomer a''), with monomer (c), which contains ethylenically unsaturated compounds obtained by reacting an acrylic monomer containing α,β-monoethylenically unsaturated compounds or an isocyanate monomer containing monoethylenically unsaturated compounds with a monovalent nonionic amphiphilic component or a primary or secondary fatty amine.

[0104] Therefore, anionic polymers having at least one hydrophobic chain can be synthesized through two pathways: - Copolymerization of monomer (a') and (c), or (a') and (b) and (c), or (a'') and (c), or (a'') and (b) and (c), - Modification with monomer (a'), or monomer (a') and (b), or copolymer formed from (a'') and (b), or primary or secondary fatty amine (specifically esterification or amidation), It can be obtained by one of the following methods.

[0105] Examples of 2-acrylamido-2-methylpropanesulfonic acid copolymers include those disclosed in the paper "Micelle formation of random copolymers of sodium 2-(acrylamido)-2-methylpropanesulfonate and nonionic surfactant macromonomer in water as studied by fluorescence and dynamic light scattering - Macromolecules, 2000, Vol. 33, No. 10, pp. 3694-3704" and applications EP-A-0750899 and EP-A-1069172.

[0106] The carboxylic acid containing α,β-monoethylenically unsaturated compounds that constitute monomer (a') can be selected from a number of acids, particularly acrylic acid, methacrylic acid, crotonic acid, itaconic acid, and maleic acid. Preferably, this is acrylic acid or methacrylic acid.

[0107] The copolymer may contain monomer (b) which is monoethylenically unsaturated and does not possess surfactant properties. Preferred monomers are those which yield a water-insoluble polymer when homopolymerized. These can be selected from, for example, acrylic acids and alkyl (C1-C4) methacrylates, such as methyl acrylate, ethyl acrylate, butyl acrylate, or the corresponding methacrylate. More particularly preferred monomers are methyl acrylate and ethyl acrylate. Other monomers that can be used are, for example, styrene, vinyltoluene, vinyl acetate, acrylonitrile, and vinylidene chloride. Non-reactive monomers are preferred, in which a single ethylenic group is the only group that is reactive under polymerization conditions. However, monomers containing a group that reacts under the action of heat, such as hydroxyethyl acrylate, can be optionally used.

[0108] Monomer (c) is obtained by the reaction of an acrylic monomer containing α,β-monoethylene unsaturated compounds, such as (a), or an isocyanate monomer containing monoethylene unsaturated compounds, with a monovalent nonionic amphiphilic compound or a primary or secondary fatty amine.

[0109] Monovalent nonionic amphiphilic compounds or primary or secondary fatty amines used to produce nonionic monomers (c) are well known. Monovalent nonionic amphiphilic compounds are generally alkoxylated hydrophobic compounds containing alkylene oxides that form the hydrophilic portion of the molecule. Hydrophobic compounds are generally composed of aliphatic alcohols or alkylphenols, in which a carbon chain containing at least six carbon atoms constitutes the hydrophobic portion of the amphiphilic compound.

[0110] A preferred monovalent nonionic amphiphilic compound is given by the following formula (V): R-(OCH2CHR') m -(OCH2CH2) n -OH (V) (In the formula, R is selected from alkyl or alkylene groups containing 6 to 30 carbon atoms and alkylaryl groups having alkyl groups containing 8 to 30 carbon atoms, R' is selected from alkyl groups containing 1 to 4 carbon atoms, n is an average number in the range of approximately 1 to 150, and m is an average number in the range of approximately 0 to 50, provided that n is at least the same magnitude as m) is a compound having this configuration.

[0111] Preferably, in the compound of formula (V), the R group is an alkyl group containing 12 to 26 carbon atoms and the alkyl group is C8-C 13 The alkylphenyl group is selected from the R' group, the R' group is a methyl group, m=0, and n=1 to 25.

[0112] Preferred primary and secondary fatty amines consist of one or two alkyl chains containing 6 to 30 carbon atoms.

[0113] The monomer used to form the nonionic urethane monomer (c) can be selected from a wide variety of compounds. Any compound may be used, including copolymerizable unsaturated compounds, such as acrylic, methacrylic, or allyl unsaturated compounds. Monomer (c) can be obtained, in particular, from isocyanates containing monoethylene unsaturated compounds, such as α,α-dimethyl-m-isopropenylbenzyl isocyanate.

[0114] Monomer (c) is particularly involved in oxyethylene (1 to 50 EO) C6~C 30 Acrylates, methacrylates, or itaconates of fatty alcohols, such as steareth-20 methacrylate, oxyethylene-(25EO)behenyl methacrylate, oxyethylene-(20EO)monocetyl itaconate, oxyethylene-(20EO)monostealyl itaconate, or polyoxyethylene-(25EO)C 12~C 24 From alcohol-modified acrylates, and oxyethylene (1 to 50 EO) C6~C 30 Dimethyl-m-isopropenylbenzyl isocyanates of fatty alcohols may be selected, for example, particularly dimethyl-m-isopropenylbenzyl isocyanates of oxyethylene-behenyl alcohols.

[0115] According to a particular embodiment of the present invention, (e) the anionic polymer is selected from (a) a carboxylic acid containing α,β-ethylenically unsaturated compounds, (b) a non-surface-active monomer containing ethylenically unsaturated compounds other than those in (a), and (c) an acrylic polymer obtained from a nonionic urethane monomer which is a reaction product of a monovalent nonionic amphiphilic compound and an isocyanate containing monoethylenically unsaturated compounds.

[0116] Anionic polymers containing at least one hydrophobic chain include, in particular, acrylic acid / ethyl acrylate / alkyl acrylate terpolymer, e.g., a product sold by Rohm & Haas under the name Acusol 823 as a 30% aqueous dispersion; acrylate / steareth-20 methacrylate copolymer, e.g., a product sold by Rohm & Haas under the name Aculyn 22; (meth)acrylic acid / ethyl acrylate / oxyethylene-(25EO) behenyl methacrylate terpolymer, e.g., a product sold by Rohm & Haas under the name Aculyn 28 as an aqueous emulsion; acrylic acid / oxyethylene-(20EO) monocetyl itaconate copolymer, e.g., a product sold by National Starch under the name Structure 3001 as a 30% aqueous dispersion; acrylic acid / oxyethylene-(20EO) monostearyl itaconate copolymer, e.g., a product sold by National Starch under the name Structure Product sold in 2001 as a 30% aqueous dispersion; acrylate / polyoxyethylene (25EO)C 12 ~C 24Examples include copolymers of alcohol-modified acrylates, such as the 30-32% copolymer latex sold by 3V SA under the name Synthalen W2000; or terpolymers of dimethyl-meth-isopropenylbenzyl isocyanate of methacrylic acid / methyl acrylate / ethoxylated behenyl alcohol, such as the product as a 24% aqueous dispersion containing 40 ethylene oxide groups disclosed in reference EP-A-0173109.

[0117] (e) The anionic polymer may also be polyester-5, for example, a product sold by Eastman Chemical under the name Eastman AQ(trademark) 55S Polymer, having the following chemical formula:

[0118] [ka]

[0119] A: Dicarboxylic acid portion G: Glycol portion SO3 - Na + : Sodium sulfo group OH: Hydroxyl group

[0120] (e) It may be preferable that the anionic polymer is selected from the group consisting of polysaccharides, such as alginic acid, hyaluronic acid and cellulose polymers (e.g., carboxymethylcellulose and cellulose gum), anionic (co)polyamino acids, such as (co)polyglutamic acid, (co)poly(meth)acrylic acid, (co)polyamine acid, (co)polystyrene sulfonate, (co)poly(vinyl sulfate), dextran sulfate, chondroitin sulfate, (co)polymaleic acid, (co)polyfumaric acid, maleic acid (co)polymer, and salts thereof.

[0121] The maleic acid copolymer may comprise one or more maleic acid comonomers, as well as one or more comonomers selected from vinyl acetate, vinyl alcohol, vinylpyrrolidone, olefins containing 2 to 20 carbon atoms, and styrene.

[0122] Therefore, "maleic acid copolymer" is understood to mean any polymer obtained by copolymerizing one or more maleic acid comonomers with one or more comonomers selected from vinyl acetate, vinyl alcohol, vinylpyrrolidone, olefins containing 2 to 20 carbon atoms, such as octadecene, ethylene, isobutylene, diisobutylene or isooctylene, and styrene, wherein the maleic acid comonomers are optionally partially or completely hydrolyzed. Preferably, hydrophilic polymers, i.e., polymers having a water solubility of 2 g / l or more, are used.

[0123] In an advantageous embodiment of the present invention, the maleic acid copolymer may have a mole fraction of maleic acid units between 0.1 and 1, more preferably between 0.4 and 0.9.

[0124] The mass-average molar mass of the maleic acid copolymer may be between 1,000 and 500,000, preferably between 1,000 and 50,000.

[0125] The maleic acid copolymer is preferably a styrene / maleic acid copolymer, and more preferably a sodium styrene / maleic acid copolymer.

[0126] Preferably, a copolymer of styrene and maleic acid in a 50 / 50 ratio is used.

[0127] For example, styrene / maleic acid (50 / 50) copolymer in the form of an ammonium salt at 30% in water, sold by Cray Valley under the reference name SMA1000H®, or styrene / maleic acid (50 / 50) copolymer in the form of a sodium salt at 40% in water, sold by Cray Valley under the reference name SMA1000HNa®, may be used.

[0128] The use of styrene / maleic acid copolymers, such as sodium styrene / maleic acid copolymer, can improve the wettability of films prepared by the compositions according to the present invention.

[0129] According to one embodiment of the present invention, (e) the anionic polymer is preferably selected from hyaluronic acid and its derivatives.

[0130] Hyaluronic acid can be represented by the following chemical formula:

[0131] [ka]

[0132] In the context of this invention, the term "hyaluronic acid" specifically refers to the following formula:

[0133] [ka]

[0134] It contains the basic units of hyaluronic acid.

[0135] This is the smallest portion of hyaluronic acid, containing a disaccharide dimer, namely D-glucuronic acid and N-acetylglucosamine.

[0136] The term "hyaluronic acid and its derivatives" also, in the context of the present invention, includes linear polymers comprising the above polymer units linked together in the chain via alternating β(1,4) and β(1,3) glucosidic bonds, having a molecular weight (MW) that can range between 380 and 13,000,000 daltons. This molecular weight depends primarily on the source and / or preparation method from which the hyaluronic acid is obtained.

[0137] The term "hyaluronic acid and its derivatives" also includes hyaluronic acid salts in the context of this invention. Examples of salts include alkali metal salts such as sodium salts and potassium salts, alkaline earth metal salts such as magnesium salts, ammonium salts, and mixtures thereof.

[0138] In its natural state, hyaluronic acid is present in the pericellular gel within the connective tissue substrate of vertebrate organs, such as the dermis and epithelial tissue. Specifically, it is found in the epidermis, synovial fluid of joints, vitreous fluid, human umbilical cord, and cockscomb process.

[0139] Therefore, the term "hyaluronic acid and its derivatives" includes all fractions or subunits of hyaluronic acid having molecular weights within the molecular weight range recalled above.

[0140] In the context of the present invention, it is preferable to use a hyaluronic acid fraction that does not have inflammatory activity.

[0141] For an overview of the listed biological activities of hyaluronic acid according to its molecular weight, through examples of various hyaluronic acid fractions, please refer to the paper "Hyaluronan fragments: an information-rich system" by R. Stern et al., European Journal of Cell Biology 58 (2006), pp. 699-715.

[0142] According to a preferred embodiment of the present invention, the hyaluronic acid fraction suitable for use, as encompassed by the present invention, has a molecular weight between 50,000 and 5,000,000, particularly between 100,000 and 5,000,000, and especially between 400,000 and 5,000,000 Da. In this case, the term used is high molecular weight hyaluronic acid.

[0143] Alternatively, a hyaluronic acid fraction that may be suitable for use as encompassed in the present invention has a molecular weight between 50,000 and 400,000 Da. In this case, the term used is intermediate molecular weight hyaluronic acid.

[0144] Furthermore, a hyaluronic acid fraction that may be suitable for use as encompassed in the present invention has a molecular weight of less than 50,000 Da. In this case, the term used is low molecular weight hyaluronic acid.

[0145] Finally, the term “hyaluronic acid and its derivatives” also includes hyaluronic acid esters, specifically those containing 1 to 20 carbon atoms, in particular those with a degree of substitution at the D-glucuronic acid level of hyaluronic acid ranging from 0.5 to 50%, in which all or part of the carboxylic acid groups of the acidic functional group are esterified with an oxyethylene alkyl or alcohol.

[0146] In particular, methyl, ethyl, n-propyl, n-pentyl, benzyl, and dodecyl esters of hyaluronic acid can be mentioned. Such esters are described in detail in D. Campoccia et al., "Semisynthetic resorbable materials from hyaluronan esterification," Biomaterials 19 (1998), pp. 2101-2127.

[0147] The hyaluronic acid derivative may be, for example, acetylated hyaluronic acid or a salt thereof.

[0148] The molecular weights shown above are also effective for hyaluronic acid esters.

[0149] Hyaluronic acid is particularly sold under the brand name CPN (MW: 10-150kDa) by Hyactive and under the brand name Cristalhyal (MW: 1.1×10) by Soliance. 6 ), or hyaluronic acid supplied by Bioland under the name Nutra HA (MW: 820,000 Da), Bioland under the name Nutra AF (MW: 69,000 Da), Bioland under the name Oligo HA (MW: 6100 Da), or Vam Farmacos Metica under the name D Factor (MW: 380 Da).

[0150] (e) The anionic polymer may preferably be selected from natural anionic polymers, more preferably from polysaccharides.

[0151] (e) The anionic polymer may more preferably be selected from the group consisting of hyaluronic acid and its derivatives, cellulose polymers and their salts, such as carboxymethylcellulose and cellulose gum (sodium carboxymethylcellulose), and mixtures thereof.

[0152] Therefore, (e) the anionic polymer may be selected from polysaccharides, preferably hyaluronic acid and its derivatives, cellulose polymers and their salts, and mixtures thereof, more preferably hyaluronic acid and its salts (e.g., sodium hyaluronate), carboxymethylcellulose and its salts, e.g., cellulose gum, and mixtures thereof.

[0153] The amount of (e) anionic polymer in the composition according to the present invention may be 0.01% by mass or more, preferably 0.05% by mass or more, and more preferably 0.1% by mass or more, based on the total mass of the composition.

[0154] The amount of (e) anionic polymer in the composition according to the present invention may be 15% by mass or less, preferably 10% by mass or less, and more preferably 5% by mass or less, based on the total mass of the composition.

[0155] The amount of (e) anionic polymer in the composition according to the present invention may be 0.01% to 15% by mass, preferably 0.05% to 10% by mass, and more preferably 0.1% to 5% by mass, based on the total mass of the composition.

[0156] The total amount of (a) cationic polymer and (e) anionic polymer in the composition according to the present invention may be 0.1% by mass or more, preferably 0.5% by mass or more, and more preferably 1% by mass or more, based on the total mass of the composition.

[0157] The total amount of (a) cationic polymer and (e) anionic polymer in the composition according to the present invention may be 20% by mass or less, preferably 15% by mass or less, and more preferably 10% by mass or less, based on the total mass of the composition.

[0158] The total amount of (a) cationic polymer and (e) anionic polymer in the composition according to the present invention may be 0.1% to 20% by mass, preferably 0.5% to 15% by mass, and more preferably 1% to 10% by mass, based on the total mass of the composition.

[0159] The ratio of (a) cationic polymer to (e) anionic polymer, for example, the ratio of chemical equivalents, may be 0.05 to 18, preferably 0.1 to 10, and more preferably 0.5 to 5.0. More specifically, it may be preferable that the ratio of the number of cationic groups in (a) cationic polymer to the number of anionic groups in (e) anionic polymer is 0.05 to 18, more preferably 0.1 to 10, and even more preferably 0.5 to 5.0.

[0160] (Non-polymeric acids with two or more acid dissociation constants) The composition according to the present invention comprises (b) a nonpolymeric acid or salt thereof having at least one pair of pKa values, i.e., a nonpolymeric acid or salt thereof having at least one pair of acid dissociation constants. The pKa value (acid dissociation constant) is well known to those skilled in the art and should be determined at a certain temperature, for example, 25°C.

[0161] (b) Nonpolymeric acids having two or more pKa values ​​can function as crosslinking agents for (a) cationic polymers. (a) Cationic polymers may be ionically crosslinked with (b) nonpolymeric acids or salts thereof having two or more pKa values.

[0162] In this specification, the term "nonpolymer" means that the acid is not obtained by polymerizing two or more monomers. Therefore, nonpolymer acids do not correspond to acids obtained by polymerizing two or more monomers, such as polycarboxylic acids.

[0163] (b) The molecular weight of the nonpolymeric acid or salt thereof having two or more pKa values ​​is preferably 1,000 or less, preferably 800 or less, and more preferably 700 or less.

[0164] (b) There is no limitation on the type of nonpolymer acid or salt thereof having two or more pKa values. Two or more different types of nonpolymer acids or salts thereof having two or more pKa values ​​may be used in combination. Therefore, a single type of nonpolymer acid or salt thereof having two or more pKa values, or a combination of different types of nonpolymer acids or salts thereof having two or more pKa values, may be used.

[0165] In this specification, the term "salt" means a salt formed by adding a suitable base to a nonpolymeric acid having two or more pKa values, which can be obtained by reacting a nonpolymeric acid having two or more pKa values ​​with a base according to methods known to those skilled in the art. Examples of salts include metal salts, such as salts with alkali metals like Na and K, and salts with alkaline earth metals like Mg and Ca, as well as ammonium salts.

[0166] (b) The nonpolymeric acid or salt thereof having two or more pKa values ​​may be an organic acid or salt thereof, preferably a hydrophilic or water-soluble organic acid or salt thereof.

[0167] (b) Nonpolymeric acids having two or more pKa values ​​may have at least two acid groups selected from the group consisting of carboxylic acid groups, sulfate groups, sulfonic acid groups, phosphoric acid groups, phosphonic acid groups, phenolic hydroxyl groups, and mixtures thereof.

[0168] (b) The nonpolymeric acid having two or more pKa values ​​may be a nonpolymeric polyhydric acid.

[0169] (b) Nonpolymeric acids having two or more pKa values ​​can be selected from the group consisting of dicarboxylic acids, disulfonic acids, and diphosphates, as well as mixtures thereof.

[0170] (b) Nonpolymeric acids or salts thereof having two or more pKa values ​​include oxalic acid, malonic acid, succinic acid, glutaric acid, adipic acid, pimelic acid, suberic acid, azelaic acid, sebacic acid, fumaric acid, maleic acid, malic acid, citric acid, aconitic acid, oxaloacetate, tartaric acid, and salts thereof; aspartic acid, glutamic acid, and salts thereof; terephthalylidene dicamfersulfonic acid, or salts thereof (Mexoryl SX), Benzophenone-9; Phytic acid and its salts; Red 2 (Amaranth), Red 102 (New Coccine), Yellow 5 (Tartrazine), Yellow 6 (Sunset Yellow FCF), Green 3 (Fast Green FCF), Blue 1 (Brilliant Blue FCF), Blue 2 (Indigo Carmine), Red 201 (Lysol Rubin B), Red 202 (Lysol Rubin BCA), Red 204 (Lake Red CBA), Red 206 (Lysol Red CA), Red 207 (Lysol Red BA), Red 208 (Lysol Red SR), Red 219 (Brilliant Lake Red R), Red 220 (Deep Maroon), Red 227 (Fast Acid Magenta), Yellow 203 (Quinoline Yellow W) S), Green 201 (Alizanin Cyanine Green F), Green 204 (Pyranine Concentrate), Green 205 (Light Green SF Yellow), Blue 203 (Patent Blue CA), Blue 205 (Alphazrin FG), Red 401 (Violamin R), Red 405 (Permanent Red F5R), Red 502 (Ponceau 3R), Red 503 (Ponceau R), Red 504 (Ponceau SX), Green 401 (Naphthol Green B), Green 402 (Guinea Green B), and Black 401 (Naphthol Blue Black); Folic acid, ascorbic acid, erythorbic acid, and salts thereof; Cystine and its salts; EDTA and its salts; Glycyrrhizin and its salts; and mixtures thereof can be selected from the group.

[0171] (b) It may be preferable that the nonpolymeric acid or salt thereof having two or more pKa values ​​is selected from the group consisting of terephthalylidene dicamphor sulfonic acid and its salts (Mexoryl SX), Yellow No. 6 (Sunset Yellow FCF), ascorbic acid, phytic acid, and salts thereof, and mixtures thereof.

[0172] (b) It may be more preferable that the nonpolymeric acid or salt thereof having two or more pKa values ​​is selected from the group consisting of terephthalylidene dicamphor sulfonic acid and its salts (Mexoryl SX), phytic acid, and salts thereof, and mixtures thereof.

[0173] The amount of (b) a nonpolymeric acid or salt thereof having two or more pKa values ​​in the composition according to the present invention may be 0.01% by mass or more, preferably 0.05% by mass or more, and more preferably 0.1% by mass or more, based on the total mass of the composition.

[0174] The amount of (b) a nonpolymeric acid or salt thereof having two or more pKa values ​​in the composition according to the present invention may be 15% by mass or less, preferably 10% by mass or less, and more preferably 5% by mass or less, based on the total mass of the composition.

[0175] The amount of (b) a nonpolymeric acid or salt thereof having two or more pKa values ​​in the composition according to the present invention may be 0.01% to 15% by mass, preferably 0.05% to 10% by mass, and more preferably 0.1% to 5% by mass, based on the total mass of the composition.

[0176] [Polyol] The composition according to the present invention comprises (c) at least one polyol. If two or more polyols are used, they may be the same or different.

[0177] In this specification, the term "polyol" means an alcohol having two or more hydroxyl groups and does not include sugars or their derivatives. Examples of sugar derivatives include sugar alcohols obtained by reducing one or more carbonyl groups of a sugar, and sugars or sugar alcohols in which one or more hydrogen atoms in the hydroxyl groups are replaced by at least one substituent such as an alkyl group, hydroxyalkyl group, alkoxy group, acyl group, or carbonyl group.

[0178] The polyol used in this invention is liquid at atmospheric pressure (760 mmHg or 105 Pa) and room temperature such as 25°C.

[0179] (c) The polyol contains at least two hydroxyl groups, preferably two to five hydroxyl groups. 2~24 Polyol, preferably C 2~9 Polyols are also acceptable.

[0180] (c) The polyol may be a natural or synthetic polyol. The polyol may have a linear, branched, or cyclic molecular structure.

[0181] (c) Polyols may be selected from glycerin and its derivatives, and glycols and their derivatives. Polyols include glycerin, diglycerin, polyglycerin, ethylene glycol, diethylene glycol, propylene glycol, dipropylene glycol, butylene glycol, pentylene glycol, hexylene glycol, C6-C 24 The following can be selected: polyethylene glycol, 1,3-propanediol, 1,4-butanediol, and 1,5-pentanediol.

[0182] (c) The polyol is preferably glycerin.

[0183] The amount of (c) polyol in the composition used in the present invention is 10% by mass or more, preferably 15% by mass or more, and more preferably 20% by mass or more, based on the total mass of the composition.

[0184] On the other hand, the amount of (c) polyol in the composition used in the present invention may be 95% by mass or less, preferably 60% by mass or less, and more preferably 30% by mass or less, based on the total mass of the composition.

[0185] The amount of (c) polyol in the composition used in the present invention may be in the range of 10% to 95% by mass, preferably 10% to 60% by mass, and more preferably 10% to 30% by mass, based on the total mass of the composition.

[0186] [water] The composition according to the present invention comprises (d) water.

[0187] (d) The amount of water may be 1% by mass or more, preferably 30% by mass or more, and more preferably 50% by mass or more, based on the total mass of the composition.

[0188] (d) The amount of water may be 90% by mass or less, preferably 50% by mass or less, and more preferably 10% by mass or less, based on the total mass of the composition.

[0189] (d) The amount of water may be 1% to 90% by mass, preferably 30% to 90% by mass, and more preferably 50% to 90% by mass, based on the total mass of the composition.

[0190] [pH] The pH of the composition according to the present invention may be 9.0 or less, preferably 8.5 or less, and more preferably 8.1 or less.

[0191] The pH of the composition according to the present invention may be 3.0 or higher, preferably 3.3 or higher, and more preferably 3.5 or higher.

[0192] The pH of the composition according to the present invention may be 3.0 to 9.0, preferably 3.3 to 8.5, and more preferably 3.5 to 8.1.

[0193] At a pH of 3.0 to 9.0, the composition according to the present invention can be very stable.

[0194] The pH of the composition according to the present invention can be adjusted by (b) adding at least one alkaline agent and / or at least one acid other than a nonpolymeric acid or a salt thereof having two or more pKa values. The pH of the composition according to the present invention can also be adjusted by adding at least one buffering agent.

[0195] (Alkaline agent) The composition according to the present invention may contain at least one alkaline agent. Two or more alkaline agents may be used in combination. Therefore, a single type of alkaline agent or a combination of different types of alkaline agents can be used.

[0196] The alkaline agent may be an inorganic alkaline agent. The inorganic alkaline agent is preferably selected from the group consisting of ammonia, alkali metal hydroxides, alkaline earth metal hydroxides, alkali metal phosphates, and monohydrogen phosphates, such as sodium phosphate or monohydrogen phosphate.

[0197] Examples of inorganic alkali metal hydroxides include sodium hydroxide and potassium hydroxide. Examples of alkaline earth metal hydroxides include calcium hydroxide and magnesium hydroxide. Sodium hydroxide is preferred as the inorganic alkali agent.

[0198] The alkaline agent may be an organic alkaline agent. The organic alkaline agent is preferably selected from the group consisting of monoamines and their derivatives, diamines and their derivatives, polyamines and their derivatives, basic amino acids and their derivatives, oligomers and their derivatives of basic amino acids, polymers and their derivatives of basic amino acids, urea and its derivatives, and guanidine and its derivatives.

[0199] Examples of organic alkaline agents include alkanolamines, such as mono-, di-, and tri-ethanolamines, and isopropanolamines; urea, guanidine, and their derivatives; basic amino acids, such as lysine, ornithine, or arginine; and diamines, such as those with the following structures:

[0200] [ka]

[0201] Examples of compounds that can be described as (wherein R represents an alkylene such as propylene which is optionally substituted with a hydroxyl group or a C1-C4 alkyl group, and R1, R2, R3 and R4 independently represent a hydrogen atom, an alkyl group or a C1-C4 hydroxyalkyl group) include 1,3-propanediamine and its derivatives. Arginine, urea and monoethanolamine are preferred.

[0202] Depending on their solubility, the alkaline agent can be used in a total amount of 0.01% to 15% by mass, preferably 0.02% to 10% by mass, and more preferably 0.03% to 5% by mass, relative to the total mass of the composition.

[0203] (acid) The composition according to the present invention may contain at least one acid. Two or more acids may be used in combination. Therefore, a single type of acid or a combination of different types of acids can be used.

[0204] Examples of acids include any inorganic or organic acid commonly used in cosmetics, preferably inorganic acids. Monohydric acids and / or polyhydric acids may be used. Monohydric acids such as citric acid, lactic acid, sulfuric acid, phosphoric acid, and hydrochloric acid (HCl) may be used. HCl is preferred.

[0205] The acid can be used in a total amount of 0.01% by mass to 15% by mass, preferably 0.02% by mass to 10% by mass, more preferably 0.03% by mass to 5% by mass, relative to the total mass of the composition, depending on their solubility.

[0206] (Buffering Agent) The composition according to the present invention may comprise at least one buffering agent. Two or more buffering agents may be used in combination. Therefore, a single type of buffering agent, or a combination of different types of buffering agents can be used.

[0207] Examples of the buffering agent may include acetate buffer (e.g., acetic acid + sodium acetate), phosphate buffer (e.g., sodium dihydrogen phosphate + disodium hydrogen phosphate), citrate buffer (e.g., citric acid + sodium citrate), borate buffer (e.g., boric acid + sodium borate), tartrate buffer (e.g., tartaric acid + sodium tartrate dihydrate), Tris buffer (e.g., tris(hydroxymethyl)aminomethane), and Hepes buffer (4-(2-hydroxyethyl)-1-piperazineethanesulfonic acid).

[0208] [Optional Components] In addition to the aforementioned essential components (components (a) to (d)), the composition according to the present invention may comprise optional components, for example, (e) anionic polymers, as well as components typically used in cosmetics, specifically surfactants (in particular nonionic surfactants) or emulsifiers, hydrophilic or lipophilic thickeners, organic volatile or non-volatile solvents other than component (c), hydrophilic or hydrophobic UV screening agents, silicones and silicone derivatives, natural extracts derived from animals or plants, oils, waxes and the like, within a range that does not impair the effects of the present invention.

[0209] The composition according to the present invention may comprise the above optional components in an amount of 0.01% by mass to 50% by mass, preferably 0.05% by mass to 30% by mass, more preferably 0.1% by mass to 10% by mass, relative to the total mass of the composition.

[0210] The composition according to the present invention may not contain a surfactant, or it may contain a limited amount of a surfactant, for example, less than 0.1% by mass, preferably less than 0.01% by mass, and more preferably less than 0.001% by mass, based on the total mass of the composition.

[0211] [Preparation] The composition according to the present invention can be prepared by mixing the essential components described above with optional components using conventional methods.

[0212] For example, the composition according to the present invention is (a) at least one cationic polymer, (b) Nonpolymeric acids or salts thereof having at least one of two or more pKa values, (c) at least one polyol, and (d) water It can be prepared by a method that includes the step of mixing, where the amount of (c) polyol in the composition is 10% by mass or more relative to the total mass of the composition.

[0213] Any of the optional components may be further mixed in. For example, (e) at least one anionic polymer may be mixed in.

[0214] The mixing can be carried out at any temperature, such as room temperature (e.g., 25°C), preferably without heating. Since the composition according to the present invention can be prepared without any heating steps, it may be environmentally friendly.

[0215] The cosmetic composition according to the present invention is preferably in liquid form at room temperature (for example, 25°C).

[0216] [coating] The composition according to the present invention can be used to easily prepare a coating.

[0217] Therefore, the present invention also provides a method for preparing a film, preferably a cosmetic film, having a thickness of preferably 10 nm or more, more preferably 50 nm or more, and even more preferably 100 nm or more, optionally. The present invention involves applying the composition to a substrate, preferably a keratin substance, more preferably skin and hair, The method may also include a step of drying the composition.

[0218] The upper limit of the thickness of the above-mentioned film is not limited. Therefore, for example, the thickness of the above-mentioned film may be 10 μm or less, preferably 5 μm or less, more preferably 3 μm or less, and even more preferably 1 μm or less.

[0219] Therefore, the present invention also relates to a film, preferably a cosmetic film, (a) at least one cationic polymer, (b) nonpolymeric acids or salts thereof having at least one of two or more pKa values, (c) at least one polyol This also relates to coatings, including those that make up a film.

[0220] The film may further contain (d) water.

[0221] The above-mentioned film, preferably a cosmetic film, is resistant to water with a pH of 7 or less and can be removed with water with a pH greater than 7, preferably 8 or higher, and more preferably 9 or higher.

[0222] In other words, the above-mentioned film, preferably a cosmetic film, can be water-resistant under neutral or acidic conditions such as a pH of 7 or less, preferably between 6 and 7, more preferably between 5 and 7, while the above-mentioned film, preferably a cosmetic film, can be removed under alkaline conditions such as a pH greater than 7, preferably 8 or more, more preferably 9 or more. The upper limit of the pH is preferably 13, more preferably 12, and even more preferably 11.

[0223] Accordingly, the above film, preferably a cosmetic film, can be water-resistant, so that it can remain on keratin substances such as the skin and hair even when the surface of the keratin substances is wet, for example, by sweat and rain. On the other hand, the above film, preferably a cosmetic film, can be easily removed from keratin substances under alkaline conditions. Therefore, the above film, preferably a cosmetic film, is difficult to remove with water, but it can be easily removed using, for example, soap that can provide alkaline conditions.

[0224] Furthermore, even when the above film does not contain any cosmetically active ingredients, due to the properties of the film, it can have cosmetic effects such as absorbing or adsorbing malodors, changing the appearance of keratin substances such as the skin and hair, changing the tactile feel of keratin substances, and / or protecting keratin substances from, for example, dirt or contaminants.

[0225] When the above film contains (c) at least one polyol such as glycerin, the film can have a cosmetic effect provided by the (c) polyol, for example, a moisturizing effect.

[0226] [Cosmetic Use and Cosmetic Method] The composition according to the present invention may be used as a cosmetic composition, preferably a care cosmetic composition, more preferably a skin care or hair care cosmetic composition.

[0227] Accordingly, the cosmetic composition according to the present invention may be intended for application to keratin substances. The keratin substance may be keratin fibers. As used herein, keratin fibers mean fibers containing keratin as a main constituent, and examples thereof include hair, eyelashes, eyebrows and the like. On the other hand, the keratin substance may be mucous membranes such as the skin and lips.

[0228] The composition according to the present invention can preferably be used as a leave-on or rinse-off cosmetic composition for keratin substances such as the skin and hair.

[0229] In this specification, "leave-on" means that the composition according to the present invention is not removed from keratinous materials such as skin and hair after being applied to them.

[0230] In this specification, "rinse-off" means that the composition according to the present invention is removed from keratinous materials such as skin and hair by rinsing after it has been applied to the keratinous material. Water may be used for rinsing. Even after rinsing off, the composition according to the present invention may remain and form a film or coating on keratinous materials such as skin and hair.

[0231] The present invention also relates to keratinous substances such as skin and hair, A step of applying the composition according to the present invention to a keratin substance, The process involves drying the composition to form a cosmetic film on the keratin material. Beauty methods including, For preparing a film, preferably a cosmetic film, The present invention involves applying the composition to keratinous material such as skin and hair, The present invention also relates to a method that includes a step of drying the composition.

[0232] In this specification, "cosmetic method" means a non-therapeutic cosmetic method for caring for keratinous substances such as skin and hair and / or for styling keratinous fibers such as hair.

[0233] The present invention may also relate to the use of the compositions according to the present invention for the preparation of cosmetic films on keratinous substances such as skin and hair.

[0234] The present invention also, (a) at least one cationic polymer, (b) A nonpolymeric acid or salt thereof having at least one of two or more pKa values, For keratinous substances in skin and hair, (c) at least one polyol, and (d) water This also relates to a use in a cosmetic composition containing (c) polyol to reduce the stickiness of the composition, wherein the amount of (c) polyol in the composition is 10% by mass or more relative to the total mass of the composition.

[0235] The use according to the present invention can reduce the stickiness of a composition containing components (c) and (d), wherein the amount of component (c) in the composition is 10% by mass or more of the total mass of the composition, by optionally combining components (a) and (b) with component (e).

[0236] The description of components (a) to (e) in the composition according to the present invention may be applied to the description of use according to the present invention. [Examples]

[0237] The present invention will be described in more detail by the examples provided. However, these should not be construed as limiting the scope of the invention.

[0238] (Examples 1-4 and Comparative Examples 1-4) [Preparation] Each of the compositions from Examples 1-4 and Comparative Examples 1-4 was prepared by mixing the components shown in Table 1 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 1 are based on the "mass%" of the raw materials.

[0239] [Table 1]

[0240] [evaluation] (Formation of a gel film) Each of the compositions from Examples 1-4 and Comparative Examples 1-4, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0241] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0242] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0243] The results are shown in Table 1.

[0244] (texture) Each of the compositions from Examples 1-4 and Comparative Examples 1-4, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0245] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0246] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0247] The results are shown in Table 1.

[0248] (Summary) The compositions from Examples 1-4 formed a gel film. The compositions from Examples 1 and 2 formed a better gel film than the compositions from Examples 3 and 4.

[0249] The compositions from Comparative Examples 1-4 failed to form any gel.

[0250] Since the compositions in Comparative Examples 2 and 4 did not contain glycerin, the texture of the compositions could not be evaluated.

[0251] It has been demonstrated that cationic polymers (polylysine and chitosan), crosslinking agents (phytic acid or terephthalylidene dicamphor sulfonic acid), and glycerin can form a gel film (coacervate) and reduce the stickiness inherent in glycerin.

[0252] (Examples 5-6 and Comparative Examples 5-6) [Preparation] The compositions of Examples 5-6 and Comparative Examples 5-6 were each prepared by mixing the components shown in Table 2 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 2 are based on the "mass%" of the raw materials.

[0253] [Table 2]

[0254] [evaluation] (Formation of a gel film) Each of the compositions from Examples 5-6 and Comparative Examples 5-6, in quantities of 10 g, was placed in a Petri dish and dried at 45°C for 24 hours.

[0255] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0256] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0257] The results are shown in Table 2.

[0258] (texture) Each of the compositions from Examples 5-6 and Comparative Examples 5-6, in quantities of 10 g, was placed in a Petri dish and dried at 45°C for 24 hours.

[0259] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0260] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0261] The results are shown in Table 2.

[0262] (Summary) The compositions from Examples 5-6 formed a uniform gel film. The gel film spread across the entire surface of the petri dish.

[0263] The compositions from Comparative Examples 5 and 6 failed to form any gel.

[0264] Since the composition in Comparative Example 5 did not contain glycerin, the stickiness of the composition could not be evaluated.

[0265] Anionic polymers (sodium hyaluronate and cellulose gum) can be added to a cationic polymer (polylysine), a crosslinking agent (phytic acid), and glycerin to form a gel film (coacervate), and it has been demonstrated that the gel film thus formed is more preferable (more uniform).

[0266] (Examples 7-8 and Comparative Examples 7-8) [Preparation] The compositions of Examples 7-8 and Comparative Examples 7-8 were each prepared by mixing the components shown in Table 3 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 3 are based on the "mass%" of the raw materials.

[0267] [Table 3]

[0268] [evaluation] (Formation of a gel film) Each of the compositions from Examples 7-8 and Comparative Examples 7-8, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0269] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0270] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0271] The results are shown in Table 3.

[0272] (texture) Each of the compositions from Examples 7-8 and Comparative Examples 7-8, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0273] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0274] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0275] The results are shown in Table 3.

[0276] (Summary) The compositions from Examples 7-8 formed a gel.

[0277] The compositions from Comparative Examples 7 and 8 failed to form any gel.

[0278] It has been demonstrated that a gel film (coacervate) can be formed using a large amount of glycerin.

[0279] (Example 9 and Comparative Example 9) [Preparation] The compositions of Example 9 and Comparative Example 9 were prepared by mixing the components shown in Table 4 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 4 are based on the "mass%" of the raw materials.

[0280] [Table 4]

[0281] [evaluation] (Formation of a gel film) 10g portions of each composition from Example 9 and Comparative Example 9 were placed in a Petri dish and dried at 45°C for 24 hours.

[0282] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0283] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0284] The results are shown in Table 4.

[0285] (texture) 10g portions of each composition from Example 9 and Comparative Example 9 were placed in a Petri dish and dried at 45°C for 24 hours.

[0286] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0287] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0288] The results are shown in Table 4.

[0289] (Summary) The composition according to Example 9 formed a gel.

[0290] The composition according to Comparative Example 9 failed to form any gel.

[0291] It has been demonstrated that a gel film (coacervate) can be formed using a large amount of cationic polymer and / or a large amount of crosslinking agent.

[0292] (Examples 10-16) [Preparation] Each of the compositions according to Examples 10-16 was prepared by mixing the components shown in Table 5 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 5 are based on the "mass%" of the raw materials.

[0293] [Table 5]

[0294] [evaluation] (Formation of a gel film) Each of the compositions from Examples 10-16, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0295] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0296] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0297] The results are shown in Table 5.

[0298] (texture) Each of the compositions from Examples 10-16, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0299] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0300] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0301] The results are shown in Table 5.

[0302] (Summary) The compositions from Examples 10-16 formed a gel.

[0303] It was demonstrated that the amount of crosslinking agent required to form the gel film (coacervate) can vary.

[0304] (Example 17 and Comparative Examples 10-14) [Preparation] Each of the compositions from Example 17 and Comparative Examples 10-14 was prepared by mixing the components shown in Table 6 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 6 are based on the "mass%" of the raw materials.

[0305] [Table 6]

[0306] [evaluation] (Formation of a gel film) Each of the compositions from Example 17 and Comparative Examples 10-14, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0307] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0308] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0309] The results are shown in Table 6.

[0310] (texture) Each of the compositions from Example 17 and Comparative Examples 10-14, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0311] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0312] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0313] The results are shown in Table 6.

[0314] (Summary) The composition according to Example 17 formed a gel.

[0315] The compositions from Comparative Examples 10-14 failed to form any gel.

[0316] It was demonstrated that the use of a monovalent acid (HCl) failed to form a gel film (coacervate). Therefore, it can be understood that the use of a polyvalent crosslinking agent (e.g., phytic acid) is essential.

[0317] (Examples 18-23) [Preparation] Each of the compositions from Examples 18 to 23 was prepared by mixing the components shown in Table 7 at room temperature (25°C). All numerical values ​​for the amounts of components in Table 7 are based on the "mass%" of the raw materials.

[0318] [Table 7]

[0319] [evaluation] (Formation of a gel film) Each of the compositions from Examples 18-23, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0320] Five experts evaluated the formation of gel films in petri dishes according to the following ranking system. 5. A uniform gel film was formed (the gel film was evenly distributed on the Petri dish). 4. A gel film was formed, but it was not uniform (the gel film was unevenly distributed on the petri dish). 3: A slight gel film has formed. 2: Only a very small amount of gel film was formed. 1: No gel film was formed.

[0321] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0322] The results are shown in Table 7.

[0323] (texture) Each of the compositions from Examples 18-23, in 10g quantities, was placed in a Petri dish and dried at 45°C for 24 hours.

[0324] Five experts evaluated the texture on the petri dish according to the following ranking system. 5: Non-sticky (very smooth) 4: Very slight stickiness (smooth) 3: Slightly sticky 2: Sticky 1: Very sticky

[0325] Next, we categorized them into the following categories based on the average of their ratings: 5: Very good 4: Good 3: Normal 2: Bad 1: Very poor

[0326] The results are shown in Table 7.

[0327] (Summary) The compositions from Examples 18-23 formed a gel.

[0328] It was demonstrated that the gel film can be formed at a pH of at least less than 8.1.

Claims

1. (a) at least one cationic polymer, (b) Nonpolymeric acids or salts thereof having at least one of two or more pKa values, (c) at least one polyol, and (d) water A composition comprising, The (b) nonpolymeric acid or salt thereof having two or more pKa values ​​is phytic acid or a salt thereof, terephthalylidene dicamfersulfonic acid or a salt thereof, or a mixture thereof. A composition wherein the amount of (c) polyol in the composition is 10% by mass or more relative to the total mass of the composition.

2. The composition according to claim 1, wherein the (a) cationic polymer is crosslinked with (b) a nonpolymeric acid or salt thereof having two or more pKa values.

3. The composition according to claim 1, wherein the cationic polymer (a) may have at least one positively charged and / or a positively charged moiety selected from the group consisting of primary, secondary, or tertiary amino groups, quaternary ammonium groups, guanidine groups, biguanide groups, imidazole groups, imino groups, and pyridyl groups.

4. The composition according to claim 1, wherein the cationic polymer (a) is selected from the group consisting of alkyldiallylamine cyclopolymers, dialkyldiallylammonium cyclopolymers, (co)polyamines, cationic (co)polyamino acids, cationic cellulose polymers, and salts thereof.

5. The composition according to claim 1, wherein the cationic polymer (a) is selected from the group consisting of polylysine, chitosan, and mixtures thereof.

6. The composition according to claim 1, wherein the amount of the cationic polymer (a) in the composition is 0.01% by mass to 15% by mass with respect to the total mass of the composition.

7. The composition according to claim 1, wherein the amount of (b) a nonpolymeric acid or salt thereof having two or more pKa values ​​in the composition is 0.01% by mass to 15% by mass with respect to the total mass of the composition.

8. The composition according to claim 1, wherein the (c) polyol is glycerin.

9. The composition according to claim 1, wherein the amount of the (c) polyol in the composition is 95% by mass or less with respect to the total mass of the composition.

10. (e) The composition according to claim 1, further comprising at least one anionic polymer.

11. The composition according to claim 10, wherein the (e) anionic polymer is selected from polysaccharides.

12. The composition according to claim 10, wherein the amount of the (e) anionic polymer in the composition is 0.01% by mass to 15% by mass with respect to the total mass of the composition.

13. The composition according to claim 1, which is a cosmetic composition.

14. This is a beauty method for keratin substances, A step of applying the composition according to any one of claims 1 to 13 to the keratin substance, The steps include drying the composition to form a cosmetic film on the keratin substance, and Beauty methods, including

Citation Information

Patent Citations

  • Specific skin cleaning liquid for infants

    CN105581922A

  • Mask containing vitamin C and preparation method thereof

    CN114246805A

  • Mixtures of quaternary polymeric acrylic ammonium salts, quaternary mono- or oligomeric ammonium salts and surfactants, their preparation and their use in cosmetic compositions

    EP0080976A1

  • Polyquaternary ammonium compounds and cosmetic compositions containing them

    EP0122324A1

  • Alkali soluble latex thickeners

    EP0173109A2