Solid oxide cell stack with a pressure difference between anode and cathode compartments

The SOC stack design addresses the mechanical vulnerability of ceramic-based cells by supporting the low-pressure side to withstand pressure differences, enabling efficient operation and cost savings by eliminating the need for additional compressors and buffer tanks.

JP7948836B2Active Publication Date: 2026-11-11HALDOR TOPSOE AS
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022516695
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-10-28
Filing Date
2020-10-07
Publication Date
2026-11-11
Estimated Expiration
2040-10-07

AI Technical Summary

Technical Problem

Solid oxide cells (SOCs) are brittle and prone to mechanical failure due to pressure differences between the fuel and oxygen compartments, leading to stack failures, which are exacerbated by the brittleness of ceramic materials used in their construction, necessitating the avoidance of any pressure differences during operation to maintain stack integrity.

Method used

A solid oxide cell stack design that provides mechanical support on the low-pressure side by selecting the distance between contact points/ribs such that the maximum tensile stress due to pressure differences is below the Weibull strength of the SOC, allowing for operation with a non-zero pressure difference between compartments.

Benefits of technology

Enables operation with a pressure difference between fuel and oxygen compartments, reducing the need for expensive pressure control devices and compressors, simplifying system design, and achieving cost savings in capital and operational expenditures (CAPEX and OPEX).

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007948836000003
    Figure 0007948836000003
  • Figure 0007948836000001
    Figure 0007948836000001
  • Figure 0007948836000002
    Figure 0007948836000002
Patent Text Reader

Abstract

The SOC stack has interconnects with a maximum distance between contact points that is designed to offset pressure differences between one side of the interconnect and the other.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to solid oxide cell (SOC) stacks, and more particularly to solid oxide fuel cell (SOFC) or solid oxide electrolytic cell (SOEC) units (especially for SOC stacks having a pressure difference between the fuel compartment and the oxygen compartment of the SOC units stacked together to form an SOC stack). [Background technology]

[0002] The present invention proposes a design for a solid oxide cell (SOC) stack that is mechanically robust to operation involving a pressure difference between the fuel compartment and the oxygen compartment of the stack. This is achieved by selecting the distance between the contact points / ribs on the low-pressure side of the SOC such that the maximum tensile stress experienced by the SOC due to the pressure difference applied between the two cells is well below the Weibull strength of the SOC.

[0003] Solid oxide cells (SOCs) typically contain layers of ceramic material and metal-ceramic composite material (cermet). Regardless of the selected cell shape (cylindrical, planar, integrated planar, etc.), one of the cell layers is typically considerably thicker than the others, providing mechanical support for the thinner layers. For example, in an electrolyte-supported cell, the airtight electrolyte layer (e.g., consisting of stabilized zirconia or doped ceria) is typically the thickest layer in the cell. The mechanical strength of such a cell is determined by the properties of the electrolyte. In a fuel electrode-supported cell, the fuel electrode is the thickest layer in the cell, and the mechanical properties of the cell are determined by the fuel electrode. The fuel electrode is typically a cermet material containing metallic Ni and an oxygen ion-conducting material, such as stabilized zirconia or doped ceria. Due to the use of ceramic materials, SOCs are brittle. A material is considered brittle if, when subjected to stress, it fractures or breaks with little or no plastic deformation. In contrast, ductile materials can undergo significant plastic deformation before fracture when subjected to stress.

[0004] To increase the output of an SOC unit, several SOCs are connected in series to form an SOC stack. A mechanical failure in a single SOC in a stack usually leads to the failure of the entire stack. The more cells there are in a stack, the lower the acceptable failure rate of the cells. For example, if the cell failure rate is 1 / 1000, the corresponding stack failure rate is 1 / 100 for a 10-cell stack, but 1 / 10 for a 100-cell stack. To achieve a low cell failure rate, the strength of the cells (typically characterized in terms of Weibull strength and Weibull coefficient) should be maximized. It should be understood that the strength of ceramic materials is not an intrinsic property but depends on the size and distribution of defects that occur during the manufacturing process and act as stress concentration points. As a result, the probability of failure of such a sample is statistically distributed and is generally characterized using the Weibull distribution. The Weibull distribution quantifies the variability of the strength of a sample derived from the distribution of defect sizes. According to this distribution, the probability of failure P f teeth, Pf =1-exp[-(σ / σ0)] m ] (In the formula, σ is the applied stress, σ0 is the Weibull strength, and m is the Weibull coefficient) The Weibull strength and Weibull coefficient can be estimated using many methods, such as ball-on-ring, four-point bending, ring-on-ring, etc.

[0005] During operation, a reactant gas is supplied to the solid oxide cell. For example, when the SOC is operating in solid oxide fuel cell mode, a fuel such as hydrogen, methane, natural gas, or synthesis gas can be supplied to the fuel side of the SOC, and an oxidizer such as air can be supplied to the oxygen side of the SOC. When the SOC is operating in solid oxide electrolysis mode, for example, water vapor and / or carbon dioxide can be supplied to the fuel side of the SOC, while a flash gas such as oxygen, water vapor, nitrogen, or carbon dioxide can be supplied to the oxygen side.

[0006] The gas pressure on each side of the SOC can, in principle, be freely selected. However, due to the brittleness of the SOC, it is common practice in the field to completely avoid any pressure differences during operation. Nevertheless, if possible, operating an SOC stack with a non-zero pressure difference between the fuel and oxygen sides of the stack would offer significant advantages.

[0007] For example, US6902840B2 (Patent Document 1) teaches that it is desirable to minimize the pressure difference of the gas passing through the anode and cathode sides of the stack, and proposes the use of a mixer / educator to manipulate and mix the exhaust fuel gas and supply the oxidizer gas so as to reduce the difference between the pressure of the exhaust fuel gas at the anode outlet and the pressure of the oxidizer gas at the cathode inlet.

[0008] In another example, US2011 / 0027683A1 (Patent Document 2) proposes the use of a sealing material having a meandering seal shape to avoid seal failure, electrolyte failure (fracture induced by stress from wrinkles, bends, or undulations in the electrolyte sheet), or device failure due to differences in gas pressure and interactions between the device, seal, and cell support frame. [Prior art documents] [Patent Documents]

[0009] [Patent Document 1] US6902840B2 [Patent Document 2] US2011 / 0027683A1 [Overview of the project] [Problems that the invention aims to solve]

[0010] This study found that by providing sufficient mechanical support on the low-pressure side of the SOC, it is possible to operate an SOC stack with a pressure difference between the fuel side and the oxygen side of the stack. More specifically, the present invention proposes a stack design in which the distance between contact points / ribs on the low-pressure side of the SOC is selected such that the maximum tensile stress experienced by the SOC due to the pressure difference applied between the two sides of the cell is well below the Weibull strength of the SOC. [Means for solving the problem]

[0011] Operating the SOC stack under either a steady state or a transient pressure difference between the fuel and oxygen compartments offers several advantages.

[0012] Temporary pressure differences between compartments can occur during stack operation, for example, when the flow rate changes or when the blower / compressor is started / stopped. A stack design that is robust against such temporary pressure differences allows for the use of less expensive pressure control devices to monitor / control the inlet pressures of the oxygen and fuel compartments. Furthermore, the present invention minimizes the need for buffer tanks (e.g., for steam) that are often used to smooth out temporary pressure differences.

[0013] In solid oxide electrolysis mode, the fuel-side supply gas (e.g., water vapor, CO2, or a mixture thereof) is typically supplied under pressurized conditions, and the resulting products (H2, CO, or synthesis gas) will also be pressurized. Therefore, it is desirable to operate the fuel-side compartment of the stack at an elevated pressure to avoid both additional depressurization of the gas before it enters the stack and repressurization of the product gas after it leaves the stack. According to the state of the art, this means that the oxygen-side compartment of the stack must be pressurized to the same pressure as the fuel-side compartment. Thus, an additional compressor is required to pressurize the oxygen-side gas before it enters the stack. The proposed invention eliminates the need for an oxygen-side compressor and thus results in significant cost savings in both CAPEX and OPEX. Furthermore, in a stack constructed according to the present invention, it is not necessary to precisely match the inlet pressures of the oxygen-side and fuel-side gases, which simplifies the system design and eliminates the need for buffer tanks.

[0014] In solid oxide fuel cell mode, the fuel-side supply gas (e.g., H2, CH4, natural gas, etc.) is often supplied under pressurized conditions, and the resulting product gas (CO2, steam), if pressurized, can advantageously be used to drive a gas turbine. Therefore, it is desirable to operate the fuel-side compartment of the stack at an increased pressure to avoid both additional depressurization of the gas before it enters the stack and repressurization of the product gas after it leaves the stack. According to the state of the art, this means that the oxygen-side compartment of the stack must be pressurized to the same pressure as the fuel-side compartment. Thus, an additional compressor is required to pressurize the oxygen-side gas before it enters the stack. The proposed invention eliminates the need for an oxygen-side compressor and therefore results in significant cost savings in both CAPEX and OPEX.

[0015] More specifically, the present invention solves the above-mentioned problems by providing a solid oxide cell stack comprising a plurality of stacked cell units as known in the art, in accordance with the claims. Each unit comprises a solid oxide cell in a cell layer and an interconnect in an interconnect layer. One interconnect layer separates one cell unit from adjacent cell units in the cell stack and thus provides a gas barrier between the cell units. The interconnect also serves to provide a gas flow channel and electrical contact between the cell units. This is solved by each interconnect, which includes one or more protruding contact regions on the first side of the interconnect and one or more protruding contact regions on the second side of the interconnect, adapted to provide mechanical and electrical contact between the interconnect and the solid oxide cell, as well as a gas flow channel between the contact regions on both the first and second sides of the interconnect. It should be understood that the contact regions on both sides of each interconnect protrude at least beyond the bottom of the gas flow channel. In particular with respect to the present invention, each solid oxide cell has a high-pressure side facing the first side of the adjacent interconnect and a low-pressure side facing the second side of the adjacent interconnect. The maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 2.5 mm, thereby the tensile stress experienced by the SOC due to the pressure difference applied between the first and second sides of the interconnect also has a maximum value, which is related to the applied pressure and the distance between the two adjacent edges of the contact area.

[0016] Accordingly, with respect to a given SOC unit having a given strength and given given operating conditions, the interconnect is designed, in accordance with the present invention, to provide the maximum tensile stress the SOC receives, which is determined by the maximum distance between two adjacent edges of the contact area on the second side of the interconnect. Accordingly, further embodiments of the present invention have various applications with respect to SOC strength and / or pressure difference, the said maximum difference can be 0.3 mm, 0.4 mm, 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, 1.0 mm, 1.2 mm, 1.5 mm, 1.8 mm, or 2.5 mm, depending on the above operating conditions and SOC strength.

[0017] According to another embodiment of the present invention, the maximum distance discussed above between two adjacent edges of the contact region on the first side of the interconnect is the same as or greater than the maximum distance between two adjacent edges of the contact region on the second side of the interconnect. In this way, the interconnect can be adapted to various process parameters and tensile stresses on both sides of the interconnect. That is, the distance between two adjacent edges of the contact region on one side is adapted to the pressure and and therefore the stress on that side, while the pressure and stress on the other side may be different, and therefore the distance discussed above on that side may also be different to satisfy the strength requirements.

[0018] In a further embodiment of the present invention, the interconnects of the SOC stack are each 15 cm 2 ~10,000cm 2 Preferably 64-500cm 2 It has an area of ​​.

[0019] In one embodiment of the present invention, the cell unit may be made of ceramic. The interconnect may also include one or more intermediate contact strengthening layers. In a particular embodiment of the present invention, the SOC stack is a solid oxide electrolytic cell stack.

[0020] According to one embodiment of the present invention, the pressure difference between the high pressure side and the low pressure side is at least 300 mBar. In a further embodiment of the present invention, said pressure difference is at least 1 Bar, preferably at least 5 Bar, or even at least 15 Bar. It should be understood that the maximum distance between two adjacent edges of the contact regions on the second side of the interconnect may vary such that the greater the pressure difference, the smaller the maximum distance between two adjacent edges of the contact regions.

[0021] Features of the Invention 1. A solid oxide cell stack comprising a plurality of stacked cell units, each unit comprising a solid oxide cell in a cell layer and an interconnect in an interconnect layer, wherein one interconnect layer separates one cell layer from an adjacent cell layer in said cell stack, and each interconnect comprises one or more protruding contact regions on a first side of said interconnect and one or more protruding contact regions on a second side adapted to provide mechanical and electrical contact between the interconnect and the solid oxide cell, Each solid oxide cell has a high pressure side facing the first side of the adjacent interconnect, and a low pressure side facing the second side of the adjacent interconnect, and the maximum distance between two adjacent edges of the contact regions on the second side of said interconnect is 2.5 mm, the solid oxide cell stack.

[0022] 2. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact regions on the second side of the interconnect is 2.0 mm.

[0023] 3. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact regions on the second side of the interconnect is 1.8 mm.

[0024] 4. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact regions on the second side of the interconnect is 1.5 mm.

[0025] 5. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 1.2 mm.

[0026] 6. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 1.0 mm.

[0027] 7. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.9 mm.

[0028] 8. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.8 mm.

[0029] 9. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.7 mm.

[0030] 10. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.6 mm.

[0031] 11. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.5 mm.

[0032] 12. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.4 mm.

[0033] 13. The solid oxide cell stack according to feature 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.3 mm.

[0034] 14. The solid oxide cell stack according to any one of the preceding features, wherein the maximum distance between two adjacent edges of the contact region on the first side of the interconnect is equal to or greater than the maximum distance between two adjacent edges of the contact region on the second side of the interconnect.

[0035] 15. The solid oxide cell stack according to any one of the preceding features, wherein the area of each of the interconnects is 15 cm 2 ~10000 cm 2 , preferably 64 to 500 cm 2 .

[0036] 16. The solid oxide cell stack according to any one of the preceding features, wherein the solid oxide cell is a ceramic cell.

[0037] 17. The solid oxide cell stack according to any one of the preceding features, wherein the interconnect comprises one or a plurality of intermediate contact reinforcing layers.

[0038] 18. The solid oxide cell stack according to any one of the preceding features, wherein the solid oxide stack is a solid oxide electrolysis cell stack.

[0039] 19. The solid oxide cell stack according to any one of the preceding features, wherein the pressure difference between the high pressure side and the low pressure side is at least 300 mBar.

[0040] 20. The solid oxide cell stack according to any one of the preceding features, wherein the pressure difference between the high pressure side and the low pressure side is at least 1 Bar, preferably at least 5 Bar, preferably at least 15 Bar.

[0041] 21. The solid oxide cell stack according to any one of the preceding features, wherein the high pressure side is the fuel side.

[0042] Drawings Hereinafter, embodiments of the present invention will be described with reference to Figure 1. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] [Figure 1] Figure 1 shows a partial, principle-side cross-section of a portion of an SOC stack according to one embodiment of the present invention.

[0044] A portion of a solid oxide cell (SOC) 101 is shown together with a high-pressure side H and a low-pressure side L. It should be understood that several SOCs are stacked in layers within an SOC stack, and an interconnect 102 separates each SOC from the next in the cell stack. One SOC and one interconnect each form one cell unit 103. The high-pressure side of the SOC faces the first side of the interconnect, and the low-pressure side of the SOC faces the second side of the interconnect. The interconnect includes protruding contact regions on both the first and second sides of the interconnect. According to the present invention, the maximum distance M1 between two adjacent edges of the contact region on the second side of each interconnect is adapted to support the cell unit, such that it is 2.5 mm. The distance M2 between two adjacent edges of the contact region on the first side of each interconnect may be greater than M1 in one embodiment of the present invention because the high-pressure side of the SOC requires less support than the low-pressure side. In a further embodiment of the present invention, the high-pressure side of the SOC is the fuel side of the SOC. [Examples]

[0045] example The design of the present invention was tested in two short SOC stacks containing nine single repeating cell units. The contact point / rib distance on the low-pressure oxygen side was 1.3 mm, and the fuel side was pressurized up to a maximum of 1.75 bara, resulting in a pressure difference from the fuel side to the oxygen side of a maximum of 750 mbar.

[0046] The first test was conducted in electrolytic mode using fuel containing 5% hydrogen in water vapor. The oxygen side was flushed with air, and the ambient pressure (1.013 bara) was maintained throughout the test. The inlet gas was heated to 750°C, and the stack was placed in a furnace where the temperature around the stack was kept stable at 750°C. The stack was operated at a current density of approximately 0.75 A / cm². The following table shows the average cell voltage at the selected operating point as the fuel side pressure was increased.

[0047] [Table 1]

[0048] As can be seen from the table, the average cell voltage decreases as the fuel-side pressure increases, which corresponds to improved performance in SOEC mode. This increased performance at this operating point corresponds to a reduction in power consumption of slightly more than 1%.

[0049] The second test was conducted in SOFC mode with 60% hydrogen and 40% nitrogen fuel. Again, the oxygen side was flushed with air, and the ambient pressure (1.013 bara) was maintained throughout the test. The inlet gas was heated to 700°C, and the SOC stack was placed in a reactor where the temperature around the SOC stack was kept stable at 700°C. The SOC stack was operated at a current density of approximately 0.28 A / cm². The following table shows the average cell voltage at the selected operating point as the fuel-side pressure was increased.

[0050] [Table 2]

[0051] As can be seen from the table, the average cell voltage increases as the fuel-side pressure increases, which corresponds to improved performance in SOFC mode. This increased performance at this operating point corresponds to an increase in power output of approximately 0.6%.

Claims

1. A solid oxide cell stack comprising a plurality of stacked cell units, each unit comprising a cell layer containing solid oxide cells and an interconnect layer containing interconnects, wherein one interconnect layer separates one cell layer from an adjacent cell layer in the cell stack, and each interconnect includes one or more protruding contact regions on a first side and one or more protruding contact regions on a second side of the interconnect, adapted to provide mechanical and electrical contact between the interconnect and the solid oxide cell. Each solid oxide cell has a high-pressure side facing the first side of the adjacent interconnect and a low-pressure side facing the second side of the adjacent interconnect, and the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 2.5 mm. The pressure difference between the high-pressure side and the low-pressure side is at least 300 mBar. The maximum distance between two adjacent edges of the contact area on the first side of the interconnect is greater than the maximum distance between two adjacent edges of the contact area on the second side of the interconnect. The high-pressure side is the fuel side. Solid oxide cell stack.

2. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 2.0 mm.

3. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 1.8 mm.

4. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 1.5 mm.

5. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 1.2 mm.

6. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 1.0 mm.

7. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.9 mm.

8. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.8 mm.

9. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.7 mm.

10. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.6 mm.

11. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.5 mm.

12. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.4 mm.

13. The solid oxide cell stack according to claim 1, wherein the maximum distance between two adjacent edges of the contact area on the second side of the interconnect is 0.3 mm.

14. Each interconnect has an area of ​​15 cm². 2 ~10,000 cm 2 The solid oxide cell stack according to any one of claims 1 to 13.

15. The solid oxide cell stack according to any one of claims 1 to 14, wherein the solid oxide cell is a ceramic cell.

16. The solid oxide cell stack according to any one of claims 1 to 15, wherein the solid oxide cell stack is a solid oxide electrolytic cell stack.

17. The solid oxide cell stack according to any one of claims 1 to 16, wherein the pressure difference between the high-pressure side and the low-pressure side is at least 1 Bar.

Citation Information

Patent Citations

  • Fuel cell

    JP2007115413A

  • Gas sealing structure and gas sealing method for solid-oxide fuel cell

    JP2007287585A

  • Components constituting HTE electrolytic cell interconnection members or SOFC fuel cell interconnection members, and their manufacturing method.

    JP2015537329A

  • Solid Oxide Fuel Cell Devices With Serpentine Seal Geometry

    US20110027683A1

  • Fuel cell system with mixer / eductor