Semiconductor device and method for manufacturing same
Patent Information
- Application Number
- JP2024509885
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Priority Date
- 2023-02-28
- Filing Date
- 2023-02-28
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing semiconductor devices using gallium oxide substrates are expensive and have low thermal conductivity, which limits their cost-effectiveness and performance.
A semiconductor device is designed using a silicon substrate with a gallium oxide-based drift layer and a configuration of trenches and electrodes that satisfy specific resistance and aperture ratio conditions, allowing for ohmic and Schottky contacts, thereby reducing costs and enhancing thermal conductivity.
The solution results in a semiconductor device that is inexpensive and has high thermal conductivity, with reduced resistance in the current path, improving overall performance.
Abstract
Description
Semiconductor device and manufacturing method thereof
[0001] The present disclosure relates to a semiconductor device and a method for manufacturing the same.
[0002] Patent Document 1 describes a method for producing gallium oxide (Ga 2 O 3 The Schottky barrier diode described in Patent Document 1 includes a semiconductor substrate made of gallium oxide and a gallium oxide (Ga) layer formed on the semiconductor substrate. 2 O 3 anode electrode in Schottky contact with the drift layer; and a cathode electrode in ohmic contact with the semiconductor substrate.
[0003] Japanese Patent Application Laid-Open No. 2019-179815
[0004] The Schottky barrier diode described in Patent Document 1 uses a relatively expensive gallium oxide substrate as the semiconductor substrate, and therefore has problems of being expensive and having low thermal conductivity.
[0005] An object of the present disclosure is to provide a semiconductor device that is inexpensive and has high thermal conductivity, and a method for manufacturing the same.
[0006] One embodiment of the present disclosure provides a semiconductor device including a Si substrate having a first main surface and a second main surface opposite to the first main surface, a drift layer disposed on the first main surface and made of a gallium oxide-based semiconductor layer, a plurality of trenches formed by digging from the second main surface toward the first main surface, extending parallel to each other at equal intervals in a predetermined direction along the second main surface, and reaching the drift layer, and a first electrode formed on a side surface and a bottom surface of each trench and making ohmic contact with the drift layer, wherein the thickness of the Si substrate is d t [cm], and the resistivity of the Si substrate is ρ s [Ω cm], the width of each trench is W t [cm], the thickness of the first electrode formed on the side surface of each trench is t m [cm], and the resistivity of the first electrode is ρ m [Ω cm], and the interface resistance between the first electrode and the Si substrate is Rms [Ω cm 2 ], and the interface resistance between the first electrode and the drift layer is R mg [Ω cm 2 ], and the interface resistance between the Si substrate and the drift layer is R sg [Ω cm 2 ], the total number of the trenches is n, the length of the Si substrate in the predetermined direction is W x [cm], (n·W t / W x ) is the aperture ratio α, t The above t m The ratio t m / W t The present invention provides a semiconductor device in which the following formula (a) is satisfied:
[0007] t m / W t >ρ m ・d t / {2α(R ms +ρ s ・d t +R sg )-2R mg} (a) With this configuration, a semiconductor device can be obtained that is inexpensive and has high thermal conductivity.
[0008] One embodiment of the present disclosure includes a step of forming a drift layer on a first main surface of a Si substrate having a first main surface and a second main surface opposite the first main surface; a step of forming a second electrode in Schottky contact with a surface of the drift layer opposite the substrate side; a step of digging from the second main surface toward the first main surface to form a plurality of trenches extending parallel to each other at equal intervals in a predetermined direction along the second main surface and reaching the drift layer; and a step of forming a first electrode in ohmic contact with the drift layer on a side surface and a bottom surface of each trench, wherein the thickness of the Si substrate is set to d t [cm], and the resistivity of the Si substrate is ρ s [Ω cm], the width of each trench is W t [cm], the thickness of the first electrode formed on the side surface of each trench is t m [cm], and the resistivity of the first electrode is ρ m [Ω cm], and the interface resistance between the first electrode and the Si substrate is Rms [Ω cm 2 ], and the interface resistance between the first electrode and the drift layer is R mg [Ω cm 2 ], and the interface resistance between the Si substrate and the drift layer is R sg [Ω cm 2 ], the total number of the trenches is n, the length of the Si substrate in the predetermined direction is W x , (n·W t / W x ) is the aperture ratio α, t The above t m The ratio t m / W t The present invention provides a method for manufacturing a semiconductor device, wherein the following formula (a) is satisfied:
[0009] t m / W t >ρ m ・d t / {2α(R ms +ρ s ・d t +R sg )-2R mg ...(a) This manufacturing method makes it possible to manufacture semiconductor devices that are inexpensive and have high thermal conductivity.
[0010] The above and other objects, features, and advantages of the present disclosure will become apparent from the following description of the embodiments with reference to the accompanying drawings.
[0011] FIG. 1 is a schematic plan view illustrating the configuration of a semiconductor device according to a first embodiment of the present disclosure. FIG. 2 is a schematic cross-sectional view taken along line II-II in FIG. 1. FIG. 3 is a partially enlarged cross-sectional view illustrating an enlarged portion A in FIG. 2. FIG. 4 is a schematic cross-sectional view illustrating the configuration of a semiconductor device according to a comparative example. FIG. 5A is a cross-sectional view illustrating a part of a manufacturing process of the semiconductor device illustrated in FIGS. 1 to 3, corresponding to the cross section of FIG. 2. FIG. 5B is a cross-sectional view illustrating a step subsequent to FIG. 5A. FIG. 5C is a cross-sectional view illustrating a step subsequent to FIG. 5B. FIG. 5D is a cross-sectional view illustrating a step subsequent to FIG. 5C. FIG. 5E is a cross-sectional view illustrating a step subsequent to FIG. 5D. FIG. 5F is a cross-sectional view illustrating a step subsequent to FIG. 5E. FIG. 5G is a cross-sectional view illustrating a step subsequent to FIG. 5F. FIG. 6 is a schematic cross-sectional view illustrating the configuration of a semiconductor device according to a second embodiment of the present disclosure, corresponding to the cross section of FIG. 2.
[0012] [Description of an embodiment of the present disclosure] One embodiment of the present disclosure relates to a semiconductor device including a Si substrate having a first main surface and a second main surface opposite to the first main surface, a drift layer disposed on the first main surface and made of a gallium oxide based semiconductor layer, a plurality of trenches formed by digging down from the second main surface toward the first main surface, extending parallel to each other at equal intervals in a predetermined direction along the second main surface, and reaching the drift layer, and a first electrode formed on a side surface and a bottom surface of each trench and making ohmic contact with the drift layer, wherein the thickness of the Si substrate is d t [cm], and the resistivity of the Si substrate is ρ s [Ω cm], the width of each trench is W t [cm], the thickness of the first electrode formed on the side surface of each trench is t m [cm], and the resistivity of the first electrode is ρ m [Ω cm], and the interface resistance between the first electrode and the Si substrate is R ms [Ω cm 2 ], and the interface resistance between the first electrode and the drift layer is R mg [Ω cm 2 ], and the interface resistance between the Si substrate and the drift layer is R sg [Ω cm 2], the total number of the trenches is n, the length of the Si substrate in the predetermined direction is W x [cm], (n·W t / W x ) is the aperture ratio α, t The above t m The ratio t m / W t The present invention provides a semiconductor device in which the following formula (a) is satisfied:
[0013] t m / W t >ρ m ・d t / {2α(R ms +ρ s ・d t +R sg )-2R mg} (a) With this configuration, a semiconductor device can be obtained that is inexpensive and has high thermal conductivity.
[0014] In one embodiment of the present disclosure, the drift layer is doped with a first n-type impurity, and the concentration of the first n-type impurity in the drift layer is 4×10 16 cm -3 1x10 or more 17 cm -3 The following is the result.
[0015] In one embodiment of the present disclosure, the drift layer includes a first drift layer arranged on the first main surface and a second drift layer formed on the first drift layer, the first drift layer and the second drift layer are each doped with a first n-type impurity, and the concentration of the first n-type impurity in the first drift layer is higher than the concentration of the first n-type impurity in the second drift layer.
[0016] In one embodiment of the present disclosure, the concentration of the first n-type impurity in the first drift layer is 1×10 17 cm -3 1x10 or more 18 cm -3 the concentration of the first n-type impurity in the second drift layer is 1×10 or less 16 cm -3 1x10 or more 17 cm -3 The following is the result.
[0017] In one embodiment of the present disclosure, the first n-type impurity is silicon (Si) or tin (Sn).
[0018] In one embodiment of the present disclosure, the first main surface is a (111) surface of the Si substrate.
[0019] In one embodiment of the present disclosure, the Si substrate is doped with a second n-type impurity, and the concentration of the second n-type impurity is 1×10 16 cm -3 1x10 or more 20 cm -3 The following is the result.
[0020] In one embodiment of the present disclosure, the second n-type impurity is phosphorus (P).
[0021] In one embodiment of the present disclosure, the gallium oxide based semiconductor layer is x1 Ga 1-x1 ) 2 O 3 (0≦x1<1) layer or (Al x2 Ga 1-x2 ) 2 O 3 It consists of (0≦x2<1) layers.
[0022] In one embodiment of the present disclosure, an insulating film is formed on a surface layer portion of the side surface of each of the trenches in the Si substrate.
[0023] In one embodiment of the present disclosure, the Si substrate has a thickness of 50 μm or more and 1000 μm or less, and the drift layer has a thickness of 1 μm or more and 100 μm or less.
[0024] A second electrode is included that is in Schottky contact with the surface of the drift layer opposite to the Si substrate side.
[0025] In one embodiment of the present disclosure, the first electrode includes an ohmic metal formed on the side and bottom surfaces of the trench and making ohmic contact with the drift layer, and a first electrode metal stacked on the ohmic metal, and the second electrode includes a Schottky metal making Schottky contact with the surface of the drift layer opposite to the Si substrate side, and a second electrode metal stacked on the Schottky metal.
[0026] One embodiment of the present disclosure includes a step of forming a drift layer on a first main surface of a Si substrate having a first main surface and a second main surface opposite the first main surface; a step of forming a second electrode in Schottky contact with a surface of the drift layer opposite the substrate side; a step of digging from the second main surface toward the first main surface to form a plurality of trenches extending parallel to each other at equal intervals in a predetermined direction along the second main surface and reaching the drift layer; and a step of forming a first electrode in ohmic contact with the drift layer on a side surface and a bottom surface of each trench, wherein the thickness of the Si substrate is set to d t [cm], and the resistivity of the Si substrate is ρ s [Ω cm], the width of each trench is W t [cm], the thickness of the first electrode formed on the side surface of each trench is t m [cm], and the resistivity of the first electrode is ρ m [Ω cm], and the interface resistance between the first electrode and the Si substrate is R ms [Ω cm 2 ], and the interface resistance between the first electrode and the drift layer is R mg [Ω cm 2 ], and the interface resistance between the Si substrate and the drift layer is R sg [Ω cm 2 ], the total number of the trenches is n, the length of the Si substrate in the predetermined direction is W x , (n·W t / W x ) is the aperture ratio α, t The above t m The ratio t m / W t The present invention provides a method for manufacturing a semiconductor device, wherein the following formula (a) is satisfied:
[0027] t m / W t >ρ m ・d t / {2α(R ms +ρ s ・d t +R sg )-2R mg ...(a) This manufacturing method makes it possible to manufacture semiconductor devices that are inexpensive and have high thermal conductivity.
[0028] DETAILED DESCRIPTION OF EMBODIMENTS OF THE PRESENT DISCLOSURE Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings.
[0029] Fig. 1 is a schematic plan view for explaining the configuration of a semiconductor device according to a first embodiment of the present disclosure. Fig. 2 is a schematic cross-sectional view taken along line II-II in Fig. 1. Fig. 3 is a partially enlarged cross-sectional view showing an enlarged portion A in Fig. 2. However, for convenience of explanation, Fig. 2 depicts the ratio of the trench width to the semiconductor device width as being larger than the actual ratio. Therefore, Fig. 2 depicts fewer trenches than the actual number.
[0030] In the following description, the left-right direction on the paper surface of FIG. 1 will be referred to as the X direction, and the up-down direction on the paper surface of FIG. 1 will be referred to as the Y direction.
[0031] The semiconductor device 1 is a Schottky barrier diode. For example, as shown in FIG. 1 , the semiconductor device 1 is formed in the shape of a rectangular chip having two sides parallel to the X direction and two sides parallel to the Y direction in a plan view. The length Wx in the X direction and the length Wy in the Y direction of the semiconductor device 1 in a plan view are, for example, several millimeters. In this embodiment, the length Wx in the X direction and the length Wy in the Y direction are 1 mm (1000 μm).
[0032] The semiconductor device 1 includes a Si substrate (silicon substrate) 2 having a first main surface (front surface) 2a and a second main surface (back surface) 2b and made mainly of Si. The semiconductor device 1 also includes a gallium oxide (Ga 2 O 3 The drift layer 3 includes a first main surface (front surface) 3 a and a second main surface (back surface) 3 b.
[0033] The Si substrate 2 is doped with n-type impurities. Phosphorus (P) or the like is used as the n-type impurity. The n-type impurity concentration in the Si substrate 2 is, for example, 1×10 16 cm -3 1x10 or more 20 cm -3 In this embodiment, the n-type impurity concentration in the Si substrate 2 may be 1×10 19 cm -3 The first and second main surfaces 2a and 2b of the Si substrate 2 are (111) surfaces. The thickness d of the Si substrate 2 is t In this embodiment, the thickness d of the Si substrate 2 is, for example, 50 μm or more and 1000 μm or less. t is 100 μm.
[0034] The Si substrate 2 has a plurality of trenches 4 formed by digging down from the second main surface 2b of the Si substrate 2 toward the second main surface 3b of the drift layer 3, penetrating the Si substrate 2 and reaching the second main surface 3b of the drift layer 3. The trenches 4 are formed to reduce the resistance of a current path from the second main surface 3b of the drift layer 3 to a cathode electrode 5 on the second main surface 2b of the Si substrate 2, which will be described later. In this embodiment, the bottom surface of the trenches 4 is formed by the second main surface 3b of the drift layer 3.
[0035] In this embodiment, the trenches 4 are arranged at equal intervals in the X direction and extend parallel to one another in the Y direction. An insulating film 2c made of a thermal oxide film is formed on the surface layer of the side surfaces of the trenches 4 and on the surface layer of the second main surface 2b of the Si substrate 2. Therefore, in this embodiment, the side surfaces of the trenches 4 are formed by the outer surfaces of the insulating films 2c formed on the surface layer of the side surfaces of the trenches 4 in the Si substrate 2. Furthermore, the second main surface 2b of the Si substrate 2 is formed by the outer surface of the insulating film 2c formed on the surface layer of the second main surface 2b of the Si substrate 2.
[0036] In this embodiment, the width W of the trench 4 t (hereinafter referred to as "trench width W t ") is 10 μm, and the interval W between adjacent trenches 4 in the Y direction is i (hereinafter referred to as "trench spacing W i") is 10 μm.
[0037] If the number of trenches 4 is n, the opening ratio α of the trenches 4 is α=n·(W t / W x ) The trench width W t and trench spacing W i can be set arbitrarily within a range that satisfies the condition of equation (5) described later.
[0038] A cathode electrode 5 is formed on the entire inner surface (bottom and side surfaces) of the trench 4 and on the entire second main surface 2b of the Si substrate 2. In this embodiment, the thickness t m (More specifically, the thickness t of the cathode electrode 5 formed on the side surface of the trench 4 m ) is 1 μm.
[0039] In this embodiment, the cathode electrode 5 is made of an ohmic metal 6 formed on the entire inner surface of the trench 4 and the entire second main surface 2 b of the Si substrate 2 , and an electrode metal 7 laminated on the ohmic metal 6 .
[0040] The ohmic metal 6 is made of a metal (e.g., titanium (Ti)) that is in ohmic contact with the second main surface 3b of the drift layer 3. The film thickness of the ohmic metal 6 is, for example, about 0.3 nm to 300 nm. The electrode metal 7 is made of gold (Au), copper (Cu), or the like. In this embodiment, the electrode metal 7 is made of gold (Au). The film thickness of the electrode metal 7 is larger than that of the ohmic metal 6, and is, for example, not less than 1 μm and not more than 100 μm.
[0041] The region of the second main surface 3b of the drift layer 3 that corresponds to the bottom surface of the trench 4 is covered with the cathode electrode 5 (ohmic metal 6). In other words, the region of the second main surface 3b of the drift layer 3 that corresponds to the bottom surface of the trench 4 is in contact with the cathode electrode 5. The other region of the second main surface 3b of the drift layer 3 (the region where the trench 4 is not formed in plan view) is in contact with the first main surface 2a of the Si substrate 2. Trench width W t can be defined as the length in the X direction of the portion of the trench 4 where the cathode electrode 5 is in contact with the drift layer 3 .
[0042] The drift layer 3 is made of (In x1 Ga 1-x1 ) 2 O 3 (0≦x1<1) layer, (Al x2 Ga 1-x2 ) 2 O 3 In this embodiment, the drift layer 3 is made of a gallium oxide-based semiconductor layer such as a gallium oxide (Ga 2 O 3 In this embodiment, the Ga 2 O 3 is β-Ga 2 O 3 The drift layer 3 is doped with n-type impurities. Examples of n-type impurities include silicon (Si) and tin (Sn). In this embodiment, the n-type impurity is silicon (Si).
[0043] The n-type impurity concentration in the drift layer 3 is, for example, 4×10 16 cm -3 1x10 or more 17 cm -3 In this embodiment, the n-type impurity concentration in the drift layer 3 may be 5×10 16 cm -3 That's about it.
[0044] The thickness of the drift layer 3 is, for example, not less than 1 μm and not more than 100 μm. In this embodiment, the thickness of the drift layer 3 is 5.5 μm.
[0045] The first main surface 3 a of the drift layer 3 is made of, for example, silicon oxide (SiO 2 A field insulating film 8 made of a SiO 2 film is laminated on the semiconductor substrate. The thickness of the field insulating film 8 is, for example, 100 nm or more, preferably 700 nm or more and 4000 nm or less. In this embodiment, the thickness of the field insulating film 8 is 500 nm. The field insulating film 8 may be made of other insulating materials such as silicon nitride (SiN).
[0046] An opening 9 that exposes the center of the drift layer 3 is formed in the field insulating film 8. In this embodiment, the opening 9 has a circular shape in a plan view. In this embodiment, the diameter of the opening 9 is about 400 μm. An anode electrode 10 is formed on the field insulating film 8.
[0047] The anode electrode 10 fills the opening 9 in the field insulating film 8 and projects outward from the opening 9 in a flange-like shape so as to cover the peripheral edge 8 a of the opening 9 in the field insulating film 8 from above. That is, the peripheral edge 8 a of the opening 9 in the field insulating film 8 is sandwiched from above and below by the drift layer 3 and the anode electrode 10 along its entire periphery. In this embodiment, the anode electrode 10 has a circular shape in a plan view. In this embodiment, the diameter of the anode electrode 10 is 800 μm. In this embodiment, the film thickness of the anode electrode 10 is 1 μm.
[0048] In this embodiment, the anode electrode 10 has a multilayer structure (a two-layer structure in this embodiment) of a Schottky metal 11 joined to the drift layer 3 within the opening 9 of the field insulating film 8 and an electrode metal 12 laminated on this Schottky metal 11.
[0049] The Schottky metal 11 is made of a metal that forms a Schottky junction with the gallium oxide-based semiconductor layer. In this embodiment, the Schottky metal 11 is made of nickel (Ni). The Schottky metal 11 that is joined to the drift layer 3 forms a Schottky barrier (potential barrier) between itself and the gallium oxide-based semiconductor layer that constitutes the drift layer 3. In this embodiment, the thickness of the Schottky metal 11 is, for example, not less than 0.02 μm and not more than 0.20 μm.
[0050] The electrode metal 12 is a portion of the anode electrode 10 that is exposed on the outermost surface of the semiconductor device 1 and to which a bonding wire or the like is bonded. The electrode metal 12 is made of gold (Au), copper (Cu), or the like. In this embodiment, the electrode metal 12 is made of gold (Au). In this embodiment, the thickness of the electrode metal 12 is greater than that of the Schottky metal 11, and is, for example, not less than 0.5 μm and not more than 5.0 μm.
[0051] Note that, of the surface of the drift layer 3, the region where the Schottky metal 11 makes Schottky contact with the surface of the drift layer 3 is sometimes called an active region, and the region surrounding the active region is sometimes called a peripheral region.
[0052] In the following, the semiconductor device 101 shown in Fig. 4 will be referred to as a comparative example. In Fig. 4, the same reference numerals as in Fig. 2 are used to denote the same parts as in Fig. 2.
[0053] 1 to 3, the semiconductor device 101 of the comparative example differs from the semiconductor device 1 of the present embodiment shown in FIGS. 1 to 3 in that no trenches 4 are formed and no insulating film is formed on the surface layer of the exposed surface of the Si substrate 2. In the semiconductor device 101 of the comparative example, since no trenches 4 are formed, the second main surface 2b of the Si substrate 2 is flat. A cathode electrode 5 is formed over the entire second main surface 2b of the Si substrate 2.
[0054] The length W in the X direction of the semiconductor device 101 of the comparative example x and the Y-direction length W y and the length W in the X direction of the semiconductor device 1 of this embodiment. x and the Y-direction length W y The thickness d of the Si substrate 2 in the semiconductor device 101 of the comparative example is the same as t , the thickness of the drift layer 3, the thickness of the cathode electrode 5, and the thickness of the anode electrode 10 are respectively the thickness d t , the thickness of the drift layer 3 , the thickness of the cathode electrode 5 , and the thickness of the anode electrode 10 .
[0055] In the comparative example, the resistance R of the current path from the interface between the Si substrate 2 and the drift layer 3 to the cathode electrode 5 on the second main surface 2 b of the Si substrate 2 wo [Ω] is expressed by the following equation (1).
[0056] R wo [Ω] = (R ms +ρ s d t +R sg ) / (W x ・W y ) ... (1) In formula (1), Wx , W y , d t The unit of is [cm]. ms [Ω cm 2 ] is the interface resistance between the cathode electrode 5 and the Si substrate 2, and ρ s [Ω cm] is the resistivity of the Si substrate 2, and R sg [Ω cm 2 ] is the interface resistance between the Si substrate 2 and the drift layer 3 .
[0057] R in the comparative example ms [Ω cm 2 ], ρ s [Ω cm] and R sg [Ω cm 2 ] are the interface resistance R between the cathode electrode 5 and the Si substrate 2 in the semiconductor device 1 of this embodiment. ms [Ω cm 2 ], resistivity ρ of the Si substrate 2 s [Ω·cm] and the interface resistance R between the Si substrate 2 and the drift layer 3 sg [Ω cm 2 ] is the same as
[0058] On the right side of equation (1) (W x ・W y ), the unit area (1 cm ) is calculated as shown in the following formula (2): 2 ) resistance R wo [Ω cm 2 ] is required.
[0059] R wo [Ω cm 2 ]=R ms +ρ s d t +R sg ...(2) In this embodiment, the resistance R of the current path from the interface between the cathode electrode 5 and the drift layer 3 to the cathode electrode 5 on the second main surface 2 b of the Si substrate 2 w [Ω] is expressed by the following equation (3).
[0060] R w [Ω] = (ρ m d t / 2nt m W y ) + (R mg / αWx ・W y ) = {(ρ m d t W t / 2t m α) + (R mg / α)} / (W x ・W y ) ... (3) In equation (3), W x , W y , d t , t m The unit of is [cm]. Furthermore, n is the number of trenches 4, and α is the aperture ratio (= n·W t / W x ) and ρ m [Ω cm] is the resistivity of the cathode electrode 5, and R mg [Ω cm 2 ] is the interface resistance between the cathode electrode 5 and the drift layer 3 .
[0061] On the right side of equation (3) (W x ・W y ), the unit area (1 cm ) is calculated as shown in the following formula (4): 2 ) resistance R w [Ω cm 2 ] is required.
[0062] R w [Ω cm 2 ]=(ρ m d t W t / 2t m α) + (R mg / α) (4) From the formulas (2) and (4), the resistance R w [Ω cm 2 ] is the resistance R ms [Ω cm 2 The condition for the value to be smaller than [0.01] is expressed by the following equation (5).
[0063] t m / W t >(ρ m ・d t ) / {2α(R ms +ρ s ・d t +R sg )-2R mg} (5) In this embodiment, the thickness t of the cathode electrode 5 is set to satisfy the condition of the formula (5). m and trench width W t is set.
[0064] ρ m [Ω cm], ρ s [Ω cm], R ms [Ω cm 2 ], R mg [Ω cm 2 ] and R sg [Ω cm 2 ] and an example of the value of d t [cm], W i [cm], t m [cm] and W t An example of a preferred value for [cm] is as follows:
[0065] ρ m =0.0000012 [Ω・cm] ρ s =0.001 [Ω・cm] R ms = 3 x 10 -7 [Ω cm 2 ] R mg = 5 x 10 -6 [Ω cm 2 ] R sg = 5.8 x 10 -6 [Ω cm 2 ] d t =0.01 [cm] W i =0.001[cm]t m =0.0001 [cm] W t In the semiconductor device 1 according to this embodiment, the Si substrate 2 is inexpensive and has a high thermal conductivity compared to a gallium oxide substrate, and therefore, a semiconductor device (Schottky barrier diode) 1 can be obtained that is inexpensive and has a high thermal conductivity.
[0066] In this embodiment, the thickness t m and trench width W tis set to satisfy the condition of formula (5), it is possible to reduce the resistance of the current path from the second main surface 3 b of the drift layer 3 to the cathode electrode 5 on the second main surface 2 b of the Si substrate 2. This results in a semiconductor device 1 with higher thermal conductivity.
[0067] 5A to 5G are cross-sectional views showing an example of a manufacturing process of the semiconductor device 1, and are cross-sectional views corresponding to the cross section of FIG.
[0068] An n-type silicon wafer (not shown) is prepared as the original substrate for the Si substrate 2. A plurality of element (Schottky barrier diode) regions corresponding to a plurality of semiconductor devices (Schottky barrier diodes) 1 are arranged in a matrix on the surface of the silicon wafer. Boundary regions (scribe lines) are provided between adjacent element regions. The boundary regions are strip-shaped regions with a substantially constant width, and are formed in a grid pattern extending in two perpendicular directions. After necessary processes are performed on the silicon wafer, the silicon wafer is cut along the boundary regions to obtain a plurality of semiconductor devices 1.
[0069] First, as shown in FIG. 5A, a gallium oxide (GaO) doped with n-type impurities is deposited on a first main surface 2a of an n-type Si substrate (n-type silicon wafer) 2 by, for example, CVD (chemical vapor deposition) or HVPE (hydride vapor phase epitaxy). 2 O 3 ) is formed.
[0070] Next, as shown in FIG. 5B, silicon oxide (SiO 2 ) is formed as a field insulating film 8.
[0071] Next, as shown in FIG. 5C , the field insulating film 8 is etched using a resist pattern (not shown) created by photolithography as a mask, thereby forming an opening 9 that exposes the central portion (active region) of the drift layer 3.
[0072] 5D , a material film 21 of the Schottky metal 11 is formed on the surfaces of the drift layer 3 and the field insulating film 8 by, for example, sputtering. The material film 21 is, for example, a nickel (Ni) layer. After that, a gold-plated seed layer is formed on the material film 21 by, for example, vapor deposition, and then a gold (Au) film is formed on the gold-plated seed layer by plating. As a result, a material film 22 of the electrode metal 12 is formed on the material film 21.
[0073] 5E , material film 22 is patterned by photolithography and etching to form electrode metal 12. Subsequently, material film 21 is patterned to form Schottky metal 11. Schottky metal 11 is formed so as to cover the entire first main surface 3 a of drift layer 3 within opening 9. In this way, anode electrode 10 made of Schottky metal 11 and electrode metal 12 is formed.
[0074] Next, as shown in FIG. 5F, a plurality of trenches 4 are formed in the Si substrate 2 by photolithography and etching, extending from the second main surface 2b of the Si substrate 2 to the second main surface 3b of the drift layer 3.
[0075] Next, as shown in FIG. 5G, an insulating film (silicon thermal oxide film) 2c made of a thermal oxide film is formed on the surface layer of the exposed surface of the Si substrate 2 by, for example, thermal oxidation.
[0076] Finally, a cathode electrode 5 is formed on the inner surface of the trench 4 and on the second main surface 2b of the Si substrate 2. In this way, the semiconductor device 1 shown in FIGS.
[0077] The cathode electrode 5 is formed as follows: First, a titanium (Ti) layer is formed on the inner surface of the trench 4 and on the second main surface 2 b of the Si substrate 2 by, for example, sputtering, thereby forming the ohmic metal 6. Then, a gold-plated seed layer is formed on the ohmic metal 6 by, for example, vapor deposition, and then a gold (Au) film is formed on the gold-plated seed layer by plating.
[0078] Fig. 6 is a schematic cross-sectional view for explaining the configuration of a semiconductor device according to a second embodiment of the present disclosure, and is a cross-sectional view corresponding to the cross section of Fig. 2. In Fig. 6, parts corresponding to those in Fig. 2 are denoted by the same reference numerals as in Fig. 2. Note that the plan view of the semiconductor device 1A according to the second embodiment is similar to the plan view of the semiconductor device 1 according to the first embodiment (Fig. 1).
[0079] In the semiconductor device 1A according to the second embodiment, the configuration of the drift layer 3 is different from that of the semiconductor device 1 according to the first embodiment.
[0080] In the semiconductor device 1A according to the second embodiment, the drift layer 3 includes a first drift layer 31 disposed on the first main surface 2 a of the Si substrate 2, and a second drift layer 32 formed on the first drift layer 31. The first drift layer 31 and the second drift layer 32 are made of (In x1 Ga 1-x1 ) 2 O 3 (0≦x1<1) layer, (Al x2 Ga 1-x2 ) 2 O 3 In this embodiment, the first drift layer 31 and the second drift layer 32 are made of a gallium oxide-based semiconductor layer such as a gallium oxide (Ga 2 O 3 In this embodiment, the Ga 2 O 3 is β-Ga 2 O 3 The first drift layer 31 and the second drift layer 32 are doped with n-type impurities. Examples of n-type impurities include silicon (Si) and tin (Sn). In this embodiment, the n-type impurity is silicon (Si).
[0081] The n-type impurity concentration in the first drift layer 31 is higher than the n-type impurity concentration in the second drift layer 32, and functions as a current spreading layer.
[0082] The n-type impurity concentration in the first drift layer 31 is, for example, 1×10 17 cm -3 1x10 or more 18 cm -3In this embodiment, the n-type impurity concentration in the first drift layer 31 is preferably 1×10 18 cm -3 The thickness of the first drift layer 31 is, for example, not less than 0.1 μm and not more than 10 μm. In this embodiment, the thickness of the first drift layer 31 is about 1 μm.
[0083] The n-type impurity concentration in the second drift layer 32 is, for example, 1×10 16 cm -3 1x10 or more 17 cm -3 In this embodiment, the n-type impurity concentration in the second drift layer 32 is preferably 5×10 16 cm -3 The thickness of the second drift layer 32 is, for example, not less than 1 μm and not more than 100 nm. In this embodiment, the thickness of the drift layer 3 is about 5.5 μm.
[0084] In the second embodiment, the thickness t of the cathode electrode 5 is set to satisfy the condition of the formula (5). m and trench width W t Therefore, the second embodiment also provides the same effects as the first embodiment.
[0085] Furthermore, in the second embodiment, the drift layer 3 includes the first drift layer 31 that functions as a current diffusion layer, which reduces the variation in current density in the X direction in the drift layer 3. This reduces the resistance of the drift layer 3.
[0086] Although the first and second embodiments of the present disclosure have been described above, the present disclosure can also be embodied in other forms. For example, in the first and second embodiments described above, the insulating film 2c made of a thermal oxide film is formed on the surface portion of the side surface of the trench 4 and the surface portion of the second main surface 2b of the Si substrate 2, but the insulating film 2c may not be formed.
[0087] In the first and second embodiments, the anode electrode 10 has a two-layer structure of the Schottky metal 11 and the electrode metal 12, but may have a single-layer structure or a three-layer or more layer structure. The materials for the Schottky metal 11 and the electrode metal 12 may be appropriately selected and used. The thicknesses of the Schottky metal 11 and the electrode metal 12 are merely examples, and appropriate values may be appropriately selected and used. The planar shape of the anode electrode 10 is circular, but it may also be a shape other than circular, such as an ellipse or a polygon.
[0088] In the first and second embodiments described above, the cathode electrode 5 has a two-layer structure of the ohmic metal 6 and the electrode metal 7, but may have a one-layer structure or a three-layer or more layer structure. The ohmic metal 6 and the electrode metal 7 may be made of suitable materials. The thicknesses of the ohmic metal 6 and the electrode metal 7 are merely examples, and suitable values may be selected and used.
[0089] Although the embodiments of the present disclosure have been described in detail above, these are merely specific examples used to clarify the technical content of the present disclosure, and the present disclosure should not be interpreted as being limited to these specific examples, and the scope of the present disclosure is limited only by the appended claims.
[0090] This application corresponds to Patent Application No. 2022-049157 filed with the Japan Patent Office on March 24, 2022, the entire disclosures of which are incorporated herein by reference.
[0091] REFERENCE SIGNS LIST 1, 1A Semiconductor device 2 Si substrate 2a First main surface 2b Second main surface 3 Drift layer 3a First main surface 3b Second main surface 4 Trench 5 Cathode electrode 6 Ohmic metal 7 Electrode metal 8 Field insulating film 8a Periphery 9 Opening 10 Anode electrode 11 Schottky metal 12 Electrode metal 21, 22 Material film 31 First drift layer 32 Second drift layer
Claims
1. a Si substrate having a first main surface and a second main surface opposite to the first main surface; a drift layer disposed on the first principal surface and made of a gallium oxide based semiconductor layer; a plurality of trenches formed by digging from the second main surface toward the first main surface, extending parallel to one another at equal intervals in a predetermined direction along the second main surface, and reaching the drift layer; a first electrode formed on a side surface and a bottom surface of each of the trenches and in ohmic contact with the drift layer; The thickness of the Si substrate is d t [cm], and the resistivity of the Si substrate is ρ s [Ω cm], the width of each trench is W t [cm], the thickness of the first electrode formed on the side surface of each trench is t m [cm], and the resistivity of the first electrode is ρ m [Ω cm], and the interface resistance between the first electrode and the Si substrate is R ms [Ω cm 2 ], and the interface resistance between the first electrode and the drift layer is R mg [Ω cm 2 ], and the interface resistance between the Si substrate and the drift layer is R sg [Ω cm 2 ], the total number of the trenches is n, the length of the Si substrate in the predetermined direction is W x [cm], (n·W t / W x ) is the aperture ratio α, The W t The above t m The ratio of t m / W t The semiconductor device satisfies the condition of the following formula (a). t m / W t >ρ m ・d t / {2α(R ms +ρ s ・d t +R sg )-2R mg } …(a)
2. the drift layer is doped with a first n-type impurity, The concentration of the first n-type impurity in the drift layer is 4×10 16 cm -3 Above 1 x 10 17 cm -3 2. The semiconductor device according to claim 1, wherein:
3. the drift layer includes a first drift layer disposed on the first main surface; a second drift layer formed on the first drift layer, the first drift layer and the second drift layer are each doped with a first n-type impurity, The semiconductor device according to claim 1 , wherein a concentration of the first n-type impurity in the first drift layer is higher than a concentration of the first n-type impurity in the second drift layer.
4. The concentration of the first n-type impurity in the first drift layer is 1×10 17 cm -3 Above 1 x 10 18 cm -3 is as follows: The concentration of the first n-type impurity in the second drift layer is 1×10 16 cm -3 Above 1 x 10 17 cm -3 4. The semiconductor device according to claim 3, wherein:
5. 3. The semiconductor device according to claim 2, wherein the first n-type impurity is silicon (Si) or tin (Sn).
6. 6. The semiconductor device according to claim 1, wherein the first main surface is a (111) surface of the Si substrate.
7. The Si substrate is doped with a second n-type impurity, and the concentration of the second n-type impurity is 1×10 16 cm -3 Above 1 x 10 20 cm -3 The semiconductor device according to any one of claims 1 to 5, wherein:
8. 8. The semiconductor device according to claim 7, wherein the second n-type impurity is phosphorus (P).
9. The gallium oxide based semiconductor layer is x1 G 1-x1 ) 2 O 3 (0≦x1<1) layer or (Al x2 G 1-x2 ) 2 O 3 6. The semiconductor device according to claim 1, comprising a (0≦x2<1) layer.
10. 6. The semiconductor device according to claim 1, wherein an insulating film is formed on a surface layer portion of a side surface of each of said trenches in said Si substrate.
11. The thickness of the Si substrate is 50 μm or more and 1000 μm or less, 6. The semiconductor device according to claim 1, wherein the drift layer has a thickness of 1 μm or more and 100 μm or less.
12. 6. The semiconductor device according to claim 1, further comprising a second electrode in Schottky contact with a surface of said drift layer opposite to said Si substrate.
13. the first electrode includes an ohmic metal formed on a side surface and a bottom surface of the trench and in ohmic contact with the drift layer, and a first electrode metal stacked on the ohmic metal; 13 . The semiconductor device according to claim 12 , wherein the second electrode includes a Schottky metal in Schottky contact with a surface of the drift layer opposite to the Si substrate, and a second electrode metal stacked on the Schottky metal.
14. forming a drift layer on a first main surface of a Si substrate having a first main surface and a second main surface opposite to the first main surface; forming a second electrode in Schottky contact with a surface of the drift layer opposite to the substrate; forming a plurality of trenches extending parallel to one another at equal intervals in a predetermined direction along the second main surface by digging down from the second main surface toward the first main surface and reaching the drift layer; forming a first electrode on a side surface and a bottom surface of each of the trenches, the first electrode being in ohmic contact with the drift layer; The thickness of the Si substrate is d t [cm], and the resistivity of the Si substrate is ρ s [Ω cm], the width of each trench is W t [cm], the thickness of the first electrode formed on the side surface of each trench is t m [cm], and the resistivity of the first electrode is ρ m [Ω cm], and the interface resistance between the first electrode and the Si substrate is R ms [Ω cm 2 ], and the interface resistance between the first electrode and the drift layer is R mg [Ω cm 2 ], and the interface resistance between the Si substrate and the drift layer is R sg [Ω cm 2 ], the total number of the trenches is n, the length of the Si substrate in the predetermined direction is W x , (n·W t / W x ) is the aperture ratio α, The W t The above t m The ratio of t m / W t A method for manufacturing a semiconductor device, wherein the following formula (a) is satisfied: t m / W t >ρ m ・d t / {2α(R ms +ρ s ・d t +R sg )-2R mg …(a)