Semiconductor device, power conversion device, and manufacturing method for semiconductor device

JPWO2024024073A5Active Publication Date: 2024-11-28MITSUBISHI ELECTRIC CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024536721
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-07-29
Filing Date
2022-07-29
Publication Date
2024-11-28
Estimated Expiration
2042-07-29

AI Technical Summary

Technical Problem

Variations in the width and depth of gate trenches in trench-gate MOSFETs lead to difficulties in maintaining charge balance between p-type and n-type pillar regions, affecting the breakdown voltage characteristics and the ability to achieve low resistance and high breakdown voltage in semi-superjunction structures.

Method used

Implanting dopants into a second pillar region under the gate trench to suppress the implantation of dopants into the first pillar region, maintaining charge balance and forming a semi-superjunction structure with p-type and n-type pillar regions that are extended deep into the drift layer, where the n-type pillar region consists of high and low concentration regions for improved charge balance.

Benefits of technology

This approach prevents charge imbalance and enhances the semi-superjunction structure's performance by achieving lower resistance and higher withstand voltage, while also reducing conduction losses and stabilizing the electric field applied to the gate insulating film.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This semiconductor device comprises second-conductive-type first pillar regions (13) that are formed below a plurality of gate trenches (6) in which gate electrodes (8) are embedded, and first-conductive-type second pillar regions (14) that are formed between the adjacent first pillar regions (13) and have a peak impurity concentration higher than that of a drift layer (2). The second pillar regions (14) are each formed of a high-concentration region (14a) and a low-concentration region (14b) that is provided on at least one side of the second pillar region (14) and has a peak impurity concentration lower than that of the high-concentration region (14a).
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor device, power conversion device, and method of manufacturing the semiconductor device

[0001] The present disclosure relates to a semiconductor device, and more particularly to a trench gate type semiconductor device.

[0002] In power electronics devices, it is necessary to switch on and off the power supply to drive a load such as an electric motor, and for this purpose, switching elements such as silicon-based IGBTs (Insulated Gate Bipolar Transistors) or MOSFETs (Metal Oxide Semiconductor Field Effect Transistors) are used.

[0003] Vertical MOSFETs and IGBTs, known as "vertical MOSFETs" and "vertical IGBTs," are often used as switching devices for power semiconductor devices. Vertical MOSFETs and vertical IGBTs are further classified into planar gate and trench gate types depending on their gate structure.

[0004] In a trench-gate MOSFET having a trench (hereinafter referred to as a "gate trench") in which a gate electrode is embedded in an active region of a drift layer of a first conductivity type (e.g., n-type), due to its structure, a high electric field is applied to the gate insulating film at the bottom of the gate trench when the MOSFET is off, which may cause breakdown of the gate insulating film at the bottom of the gate trench.

[0005] To solve this problem, for example, Patent Document 1 discloses a technique for alleviating the electric field applied to the gate insulating film at the bottom of the gate trench by providing a "trench bottom protection layer," which is a second conductivity type (e.g., p-type) electric field alleviation region, covering the bottom of the gate trench. Furthermore, Patent Document 1 also discloses a "depletion suppression layer," which is a first conductivity type current diffusion layer, on the side of the gate trench, preventing the trench bottom protection layer from narrowing the on-current path between the gate trenches and reducing conduction loss during on-state. The depletion suppression layer in Patent Document 1 is formed by implanting donor impurities of the first conductivity type into the side of the gate trench by oblique ion implantation.

[0006] Patent No. 6377309

[0007] By extending the trench bottom protection layer and the depletion suppression layer deep into the drift layer and using them as the p-type pillar region and the n-type pillar region of the semi-superjunction structure, it is possible to achieve low resistance and high breakdown voltage for the trench-gate MOSFET. Note that the semi-superjunction structure refers to a superjunction structure in which the p-type pillar region and the n-type pillar region are formed halfway down the semiconductor layer.

[0008] However, when the n-type pillar region serving as a depletion suppression layer is formed at a shallow position in the gate trench by oblique ion implantation, variations in the width and depth of the gate trench result in a large amount of donors (n-type dopants) being implanted into the p-type pillar region serving as a trench bottom protection layer. This makes it difficult to achieve a charge balance between the p-type pillar region and the n-type pillar region, resulting in variations in the breakdown voltage characteristics of the semiconductor device, and therefore preventing the full benefits of the low resistance and high breakdown voltage achieved by the semi-superjunction structure.

[0009] The present disclosure has been made to solve the above-mentioned problems, and aims to prevent dopants from the second pillar region from being implanted into the first pillar region below the gate trench in a semiconductor device having a semi-superjunction structure.

[0010] a first conductivity type well region formed in a surface layer portion of the semiconductor layer; a first conductivity type source region formed in a surface layer portion of the well region; a source electrode electrically connected to the well region and the source region; a plurality of gate trenches penetrating the source region and the well region and having gate electrodes embedded therein via gate insulating films; first conductivity type first pillar regions formed below the plurality of gate trenches; and second conductivity type second pillar regions formed between adjacent first pillar regions and having a higher peak impurity concentration than the drift layer, wherein the second pillar region is composed of a high concentration region and a low concentration region provided on at least one side of the second pillar region and having a lower peak impurity concentration than the high concentration region.

[0011] The semiconductor device according to the present disclosure can prevent dopants from the second pillar region from being implanted into the first pillar region below the gate trench, thereby preventing the charge balance between the first pillar region and the second pillar region from being disrupted and contributing to lower resistance and higher breakdown voltage achieved by the semi-superjunction structure.

[0012] The objects, features, aspects, and advantages of the present disclosure will become more apparent from the following detailed description and the accompanying drawings.

[0013] 9 is a cross-sectional view schematically showing the structure of a semiconductor device according to a first embodiment. 10 is a cross-sectional view schematically showing the structure of a semiconductor device according to a modification of the first embodiment. 11 is a cross-sectional view schematically showing the structure of a semiconductor device according to a modification of the first embodiment. 12 is a cross-sectional view schematically showing the structure of a semiconductor device according to a modification of the first embodiment. 13 is a cross-sectional view schematically showing the structure of a semiconductor device according to a modification of the first embodiment. 14 is a cross-sectional view schematically showing a method for manufacturing a semiconductor device according to the first embodiment. 15 is a cross-sectional view schematically showing a method for manufacturing a semiconductor device according to the first embodiment. 16 is a cross-sectional view schematically showing a method for manufacturing a semiconductor device according to the first embodiment. 17 is a plan view schematically showing the structure of a semiconductor device according to a second embodiment. 18 is a cross-sectional view taken along line A1-A2 of FIG. 14. 19 is a cross-sectional view taken along line B1-B2 of FIG. 14. 20 is a cross-sectional view taken along line C1-C2 of FIG. 21. 22 is a cross-sectional view schematically showing the structure of a semiconductor device according to a third embodiment. 23 is a plan view schematically showing the structure of a semiconductor device according to a fourth embodiment. 24 is a cross-sectional view taken along line A1-A2 of FIG. 22. 25 is a cross-sectional view taken along line B1-B2 of FIG. 23. 26 is a cross-sectional view taken along line C1-C2 of FIG. 24. FIG. 10 is a block diagram showing the configuration of a power conversion system according to a fifth embodiment.

[0014] Hereinafter, embodiments of the technology according to the present disclosure will be described with reference to the drawings. Note that the drawings are schematic, and the relative sizes and positions of components shown in different drawings are not necessarily accurately depicted and may be changed as appropriate. Furthermore, identical or corresponding components in different drawings are denoted by the same reference numerals, and redundant descriptions thereof may be omitted. Furthermore, terms indicating positions or directions, such as "top," "bottom," "side," "bottom," "front," or "back," are used for convenience in the description to facilitate understanding and do not necessarily represent positions or directions in actual use.

[0015] In addition, in the following embodiments, the first conductivity type is n-type and the second conductivity type is p-type, but the first conductivity type may be p-type and the second conductivity type may be n-type.

[0016] 1 is a cross-sectional view schematically illustrating the structure of a semiconductor device according to a first embodiment. In the first embodiment, a vertical trench-gate silicon carbide MOSFET is shown as an example of the semiconductor device. The semiconductor device according to the first embodiment has an active region in which MOSFET cells (active unit cells) are arranged side by side, and a termination region outside the active region, and FIG. 1 shows the configuration of the active region.

[0017] The semiconductor device according to the first embodiment is formed using an n-type (first conductivity type) semiconductor substrate 1 made of silicon carbide having a 4H polytype. A semiconductor layer 20 made of silicon carbide is formed on the semiconductor substrate 1. The upper surface of the semiconductor substrate 1 is a (0001) plane having an off-angle θ tilting toward the [11-20] axis direction. The off-angle θ may be 10 degrees or less. An n-type drift layer 2 having a lower peak impurity concentration than the semiconductor substrate 1 is formed in the semiconductor layer 20.

[0018] In the active region, a p-type (second conductivity type) well region 3 is formed in a surface layer portion of the semiconductor layer 20. An n-type source region 4 and a p-type well contact region 5 having a higher peak impurity concentration than the well region 3 are selectively (i.e., partially) formed in a surface layer portion of the well region 3. The well contact region 5 is provided so as to be in contact with the source region 4, and electrically connects a source electrode 10 (described later) and the well region 3.

[0019] Furthermore, a gate trench 6 is formed in the semiconductor layer 20 so as to penetrate the source region 4 and the well region 3. A gate insulating film 7 is formed on the side and bottom surfaces of the gate trench 6. A gate electrode 8 is formed on the gate insulating film 7 so as to be embedded in the gate trench 6. The top surface of the gate electrode 8 is located deeper than the surface of the semiconductor layer 20. In other words, the top surface of the gate electrode 8 is located deeper than the upper end of the gate trench 6. An interlayer insulating film 9 is formed in the upper part of the gate trench 6 so as to cover the gate electrode 8.

[0020] In this embodiment, the gate trench 6 penetrates the source region 4, and therefore the edge portion of the gate trench 6 in the semiconductor layer 20 becomes the source region 4. However, the gate electrode 8 is not formed on the upper end portion of the gate trench 6, and the gate insulating film 7 in that portion is covered with the interlayer insulating film 9. Therefore, the source region 4 and the gate electrode 8 do not face each other at the edge portion of the gate trench 6.

[0021] A source electrode 10 is formed on the semiconductor layer 20. The source electrode 10 is electrically connected to the source region 4 and the well region 3. In this embodiment, a silicide layer 15 is formed on the surfaces of the source region 4 and the well contact region 5, and a barrier metal 16 is provided on the bottom surface of the source electrode 10. Therefore, the source electrode 10 is connected to the source region 4 and the well contact region 5 via the silicide layer 15 and the barrier metal 16. Furthermore, a drain electrode 11 electrically connected to the semiconductor substrate 1 is formed on the lower surface of the semiconductor substrate 1.

[0022] A p-type trench bottom protection layer 12 is formed at the bottom of the gate trench 6 in the semiconductor layer 20. The trench bottom protection layer 12 is electrically connected to the source electrode 10. The trench bottom protection layer 12 functions to reduce the electric field applied to the bottom and side surfaces of the gate trench 6 when the MOSFET is turned off. It is desirable that the trench bottom protection layer 12 be in contact with the gate trench 6.

[0023] The semiconductor layer 20 has a semi-superjunction structure in which p-type pillar regions 13, which are p-type first pillar regions, and n-type pillar regions 14, which are n-type second pillar regions, are alternately arranged. The p-type pillar regions 13 are formed below the trench bottom protection layer 12, and the n-type pillar regions 14 are formed between adjacent p-type pillar regions 13.

[0024] In this embodiment, the n-type pillar region 14 is composed of a high-concentration n-type pillar region 14a, which is a high-concentration region, and a low-concentration n-type pillar region 14b, which is a low-concentration region (for ease of illustration, the high-concentration n-type pillar region 14a in each drawing is hatched with a grain pattern). The peak impurity concentration of the high-concentration n-type pillar region 14a is higher than the peak impurity concentration of the low-concentration n-type pillar region 14b. The low-concentration n-type pillar region 14b is disposed on at least a part of the side of the n-type pillar region 14 (i.e., the portion in contact with the p-type pillar region 13). Hereinafter, the side of the n-type pillar region 14 may also be referred to as the "side of the high-concentration n-type pillar region 14a."

[0025] The n-type pillar region 14 has two sides because it is sandwiched between two p-type pillar regions 13. The low-concentration n-type pillar region 14b is formed on at least one of the two sides of the n-type pillar region 14. In other words, the high-concentration n-type pillar region 14a may be provided on only one side of the high-concentration n-type pillar region 14a.

[0026] In addition, in FIG. 1, the width of the top and the width of the bottom of the low-concentration n-type pillar region 14b are the same, but as shown in FIG. 2, for example, the top surface or side surface of the low-concentration n-type pillar region 14b may be inclined so that the width of the bottom of the low-concentration n-type pillar region 14b is wider than the width of the top.

[0027] Although details will be described later, the structure of the high-concentration n-type pillar region 14a and the low-concentration n-type pillar region 14b shown in Figures 1 and 2 is formed by performing oblique ion implantation on both side surfaces of the gate trench 6, that is, by performing ion implantation from a direction oblique to the depth direction of the semiconductor layer 20.

[0028] However, the n-type pillar region 14 consisting of the high-concentration n-type pillar region 14a and the low-concentration n-type pillar region 14b can also be formed by oblique ion implantation onto one side surface of the gate trench 6. In this case, as shown in FIG. 3 , FIG. 4 , or FIG. 5 , the bottom of the n-type pillar region 14 is inclined, and the depth of the n-type pillar region 14 becomes asymmetric. FIG. 3 shows an example in which the low-concentration n-type pillar region 14b is formed by implanting a high-concentration impurity from the side surface of the gate trench 6, which serves as the implantation surface, to a midpoint between the side surface and the adjacent gate trench 6. FIG. 4 shows an example in which the low-concentration n-type pillar region 14b is formed by implanting a high-concentration impurity from the side surface of the gate trench 6, which serves as the implantation surface for the oblique ion implantation, to a deep position (near the trench bottom protection layer 12 and the p-type pillar region 13 below the adjacent gate trench 6). FIG. 5 shows an example in which a low-concentration n-type pillar region 14 b is formed by implanting a high concentration of impurities into a shallow position (near the trench bottom protection layer 12 and the p-type pillar region 13 below the gate trench 6) from the side surface of the gate trench 6, which is the implantation surface of the oblique ion implantation.

[0029] Regarding the positional relationship between the p-type pillar region 13 and the n-type pillar region 14 in the depth direction from the top surface of the semiconductor layer 20, in order to avoid current constriction between adjacent p-type pillar regions 13, it is desirable that the lower end of the high-concentration n-type pillar region 14a or the low-concentration n-type pillar region 14b be located at the same depth as the lower end of the p-type pillar region 13 or even deeper.

[0030] Furthermore, it is desirable that the p-type pillar region 13 and the n-type pillar region 14 are formed to a position deeper than the distance between adjacent gate trenches 6, or to a position deeper than the distance between adjacent p-type pillar regions 13, based on the position of the bottom of the gate trench 6. In other words, it is desirable that the depth from the bottom of the gate trench 6 to the lower end of the p-type pillar region 13 and the depth from the bottom of the gate trench 6 to the lower end of the n-type pillar region 14 be longer than the distance between adjacent gate trenches 6 or the distance between adjacent p-type pillar regions 13.

[0031] A method for manufacturing the semiconductor device according to the first embodiment shown in FIG. 1 will now be described.

[0032] First, a relatively high-resistance n-type (n - The semiconductor layer 20 made of silicon carbide (type) is epitaxially grown. 14 [cm -3 ] or more 1 x 10 17 [cm -3 ] or less.

[0033] Next, an alignment mark is formed in the semiconductor layer 20 by reactive ion etching (RIE). The alignment mark may be formed simultaneously with the gate trench 6.

[0034] Thereafter, using the alignment marks as a reference, a p-type well region 3 and a relatively low-resistance n-type (n + The source region 4 (of the n-type) is formed by ion implantation. As an implantation mask for selectively forming the source region 4 by ion implantation, for example, a resist mask or the like can be used.

[0035] The source region 4 is 5×10 18 [cm -3 ] or more 5 x 10 20 [cm -3 ] or less, and the well region 3 has an n-type impurity concentration of 1×10 16 [cm -3 ] or more 3 x 10 19 [cm -3 ] or less. In order to form the source region 4 in the surface layer portion of the well region 3, the n-type impurity concentration of the source region 4 is set to be higher than the p-type impurity concentration of the well region 3. At this time, an n-type region in the semiconductor layer 20 where the well region 3 and the source region 4 are not formed remains as the drift layer 2.

[0036] The impurity concentration of the well region 3 may or may not be constant in the depth direction. For example, the impurity concentration may be distributed so that it is lower in the surface portion of the well region 3, or may have a peak in the deeper portion.

[0037] Next, a p-type well contact region 5 is formed by ion implantation. At this time, the well contact region 5 has a concentration of 1×10 19 [cm -3 ] or more 1 x 10 22 [cm -3 ] or less.

[0038] Next, an etching mask 18 (see FIG. 6 ) having a pattern in which an area where the gate trench 6 is to be formed is formed on the semiconductor layer 20, and by RIE using the etching mask 18, a gate trench 6 is formed in the semiconductor layer 20, penetrating the well region 3 and reaching the drift layer 2.

[0039] 6, a p-type trench bottom protection layer 12 and a p-type pillar region 13 are formed on the bottom surface of the gate trench 6 by ion implantation using the etching mask 18 as an implantation mask. At this time, the trench bottom protection layer 12 has a thickness of 1×10 17 [cm -3 ] or more 1 x 10 20 [cm -3 ] or less, and the p-type pillar region 13 has a p-type impurity concentration of 1×10 16 [cm -3 ] or more 1 x 10 18 [cm -3 ] or less.

[0040] After removing the etching mask 18, n-type pillar regions 14 consisting of high-concentration n-type pillar regions 14a and low-concentration n-type pillar regions 14b are formed by oblique ion implantation below the mesa-shaped semiconductor layer 20 between the gate trenches 6. Specifically, as shown in FIG. 7 , n-type impurities are first implanted into one side surface of the gate trench 6 by oblique ion implantation, thereby forming the low-concentration n-type pillar region 14b below the mesa-shaped semiconductor layer 20. Furthermore, as shown in FIG. 8 , n-type impurities are also implanted into the other side surface of the gate trench 6 by oblique ion implantation, thereby forming the low-concentration n-type pillar region 14b below the mesa-shaped semiconductor layer 20. The high-concentration n-type pillar region 14a is formed in the region where impurities are implanted in an overlapping manner by these two oblique ion implantations.

[0041] In the tilted ion implantation for forming the high-concentration n-type pillar region 14a and the low-concentration n-type pillar region 14b, it is important to implant n-type impurities from the side of each gate trench 6 to the vicinity of the trench bottom protection layer 12 and p-type pillar region 13 below the adjacent gate trench 6.

[0042] Furthermore, in this oblique ion implantation, the lower surface of the gate trench 6 is in the shadow of the mesa-shaped semiconductor layer 20, thereby suppressing implantation of n-type impurities into the lower surface of the gate trench 6. This suppresses donors from being implanted into the trench bottom protection layer 12 and the p-type pillar region 13 below the gate trench 6, thereby achieving a stable charge balance. As a structural feature, the concentration of n-type impurities contained in the p-type pillar region 13 is lower than the concentration of n-type impurities contained in the low-concentration n-type pillar region 14b.

[0043] The high-concentration n-type pillar region 14a is 1×10 15 [cm -3 ] or more 5 x 10 18 [cm -3 ] or less, and the low-concentration n-type pillar region 14b is formed to have an n-type impurity concentration of 5×10 14 [cm -3 ] or more 1 x 10 18 [cm -3 ] or less.

[0044] Thereafter, annealing is performed at a temperature in the range of 1500° C. to 2200° C. for 0.5 minutes to 60 minutes to activate the implanted ions.

[0045] Furthermore, an insulating film is formed on the surface of the semiconductor layer 20 by a thermal oxidation method or a chemical vapor deposition (CVD) method, and the insulating film is patterned by wet etching or dry etching to form a field insulating film (not shown) for protecting the termination region.

[0046] Next, the gate insulating film 7 is formed on the surface of the semiconductor layer 20 including the inside of the gate trench 6 by thermal oxidation, CVD, or the like.

[0047] Next, polysilicon or the like doped with impurities, which is the material of the gate electrode 8, is formed by CVD or the like over the entire surface of the semiconductor layer 20 on which the gate insulating film 7 has been formed. At this time, the inside of the gate trench 6 is filled with polysilicon. When polysilicon is formed by CVD, the polysilicon grows not only upward from the bottom surface of the gate trench 6 but also laterally within the gate trench 6, so that the gate trench 6 can be filled with polysilicon relatively easily.

[0048] Next, the polysilicon on the surface of the semiconductor layer 20 is removed by etching back. At this time, the polysilicon buried in the gate trench 6 remains without being removed, and becomes the gate electrode 8. Note that, in order to completely remove the polysilicon on the surface of the semiconductor layer 20, a certain amount of over-etching is required, and therefore the upper surface of the gate electrode 8 in the gate trench 6 is positioned deeper than the upper end of the gate trench 6.

[0049] Next, an interlayer insulating film 9 is formed so as to cover the termination region and gate electrode 8, and the source region 4 and well contact region 5 are exposed from the interlayer insulating film 9 by dry etching or the like. Then, a silicide layer 15 is formed on the well contact region 5 and the n-type source region 4. Furthermore, a gate contact hole (not shown) reaching the gate electrode 8 is formed in the interlayer insulating film 9 by dry etching, wet etching or the like.

[0050] Thereafter, the source electrode 10 is formed on the semiconductor layer 20. Also, a gate pad or a wiring for connection to the gate pad is formed to connect to the gate insulating film 7 through the gate contact hole.

[0051] Finally, a drain electrode 11 is formed on the lower surface of the semiconductor substrate 1, thereby completing the semiconductor device having the structure shown in FIG.

[0052] The effects achieved by the semiconductor device according to the first embodiment will be described below.

[0053] First, we will describe the effect of the trench bottom protection layer 12. By providing the trench bottom protection layer 12 below the gate trench 6, it is possible to significantly reduce the electric field applied to the gate insulating film 7 when the MOSFET is in the off state.

[0054] Next, the effects of the p-type pillar regions 13 and the n-type pillar regions 14 (high-concentration n-type pillar regions 14a and low-concentration n-type pillar regions 14b) will be described. By providing the p-type pillar regions 13 and the n-type pillar regions 14 deep in the drift layer 2 and increasing their impurity concentrations above those of the drift layer 2 while maintaining a charge balance between the p-type pillar regions 13 and the n-type pillar regions 14, a superjunction effect can be achieved. That is, when the semiconductor device is off, a depletion layer extends laterally between the p-type pillar regions 13 and the n-type pillar regions 14, allowing the p-type pillar regions 13 and the n-type pillar regions 14 to share a larger electric field than the drift layer 2, thereby contributing to a higher breakdown voltage of the semiconductor device. Furthermore, when the semiconductor device is on, the n-type pillar regions 14, which have a lower resistance than the drift layer 2, serve as a current path, thereby contributing to a lower on-resistance of the semiconductor device.

[0055] Here, we will describe the effect of the n-type pillar region 14 being composed of the high-concentration n-type pillar region 14a and the low-concentration n-type pillar region 14b. In the superjunction effect described above, the high-concentration n-type pillar region 14a functions as a current path with lower resistance when the device is on, and the low-concentration n-type pillar region 14b functions as a region with higher breakdown voltage when the device is off, by making it easier to extend the depletion layer.

[0056] Next, the effects of the method for forming the high-concentration n-type pillar region 14 a and the low-concentration n-type pillar region 14 b will be described. When the high-concentration n-type pillar region 14 a and the low-concentration n-type pillar region 14 b are formed by oblique ion implantation, the lower surface of the gate trench 6 is in the shadow of the mesa-shaped semiconductor layer 20, thereby suppressing the implantation of n-type impurities into the lower surface of the gate trench 6. This suppresses the implantation of donors into the trench bottom protection layer 12 and the p-type pillar region 13 below the gate trench 6, thereby achieving a stable charge balance.

[0057] In order to obtain a higher superjunction effect, it is desirable that the p-type pillar region 13 and the n-type pillar region 14 be formed to a position deeper than the distance between adjacent gate trenches 6, or to a position deeper than the distance between adjacent p-type pillar regions 13, based on the position of the bottom of the gate trench 6.

[0058] The cell structure formed in the active region of the semiconductor device may have any structure, for example, a continuous stripe shape in plan view, or a partial lattice or T-shape formed by forming a bridge in the gate trench 6. Alternatively, a partial polygonal or wave-shaped structure may also be used.

[0059] The crystal orientation of the side surface of the gate trench 6 may be any crystal plane, such as the (11-20) plane, the (-1120) plane, the (1-100) plane, or the (-1100) plane, and is not limited thereto.

[0060] In addition, in the first embodiment, the surface of the semiconductor substrate 1 is a (0001) plane having an off-angle θ tilted toward the [11-20] axis, but even if the surface is a (000-1) plane having an off-angle θ tilted toward the [11-20] axis, a trench-gate MOSFET having a similar structure can be fabricated and the effects of the first embodiment can be obtained. Needless to say, the surface may also be a (1-100) plane or a (03-38) plane.

[0061] Furthermore, the semiconductor device is not limited to a MOSFET. For example, if the conductivity type of the semiconductor substrate 1 in the structure of Figure 1 is changed to p-type, or if the semiconductor substrate 1 is removed and a p-type impurity region is formed on the underside of the drift layer 2, an IGBT configuration can be obtained. In this case, the source region 4 corresponds to the emitter region of the IGBT, and the drain electrode 11 corresponds to the collector electrode of the IGBT. Even if the semiconductor device is an IGBT, the same effects as in the case of a MOSFET can be obtained.

[0062] In the first embodiment, silicon carbide (SiC) is used as the semiconductor material for the semiconductor device. However, other semiconductor materials may be used. Examples of the semiconductor material include silicon (Si) and wide band gap materials. Examples of wide band gap materials include SiC and Ga. 2 O 3 , GaN (Gallium Nitride), and diamond.

[0063] Semiconductor devices using wide band gap materials are expected to be used particularly at high temperatures and with high voltages. Since the reliability of insulating films is likely to decrease at high temperatures, the effect of applying the first embodiment is significant. Furthermore, as semiconductor devices are made to withstand higher voltages, the voltage applied to the insulating film also increases, so the effect of applying the first embodiment is significant.

[0064] Furthermore, it is known that in a silicon carbide semiconductor device, more electron traps are generated at the MOS interface between the gate insulating film 7 and the drift layer 2 than in a silicon (Si) semiconductor device, and the reliability of the MOS interface and the gate insulating film 7 is lower than in a silicon (Si) semiconductor device. Therefore, the application of the first embodiment, which can reduce the electric field applied to the gate insulating film 7, is very effective.

[0065] In the first embodiment, nitrogen, phosphorus, etc. are assumed as n-type impurities, and aluminum, boron, etc. are assumed as p-type impurities.

[0066] <Second Preferred Embodiment> Fig. 9 is a plan view schematically showing the structure of a trench-gate MOSFET as a semiconductor device according to a second preferred embodiment. Fig. 10 is a cross-sectional view taken along line A1-A2 in Fig. 9, Fig. 11 is a cross-sectional view taken along line B1-B2 in Fig. 9, and Fig. 12 is a cross-sectional view taken along line C1-C2 in Fig. 9.

[0067] 10 , a p-type sidewall well region 17 is formed in a part of the sidewall of the gate trench 6. The sidewall well region 17 serves to electrically connect the trench bottom protection layer 12 or the p-type pillar region 13 to the well region 3 or the well contact region 5.

[0068] 9, some components are omitted to more clearly show the arrangement of the sidewall well regions 17. 10 to 12 show cross sections of the periodic structure of unit cells at positions in the active region that include the gate trench 6 in their cross sections.

[0069] 11, in the cross section taken along line B1-B2 in Fig. 9, sidewall well region 17 is not formed, but well contact region 5 is formed. As shown in Fig. 12, in the cross section taken along line C1-C2 in Fig. 9, neither sidewall well region 17 nor well contact region 5 is formed, and well region 3 reaches the surface of semiconductor layer 20. In this way, the semiconductor device according to the second embodiment may have a cross section in which there is no sidewall well region 17 but there is a well contact region 5, or a cross section in which there is neither sidewall well region 17 nor well contact region 5.

[0070] 10 to 12 may coexist in a cross section of the active region of the semiconductor device. That is, the cross-sectional structures shown in FIGS. 10 to 12 may each be local. There are no restrictions on the ratio at which the cross-sectional structures shown in FIGS. 10 to 12 are arranged, and the arrangement may be freely designed.

[0071] A method for manufacturing the p-type sidewall well region 17 will be described. The sidewall well region 17 can be formed by implanting p-type impurities into the sidewall of the gate trench 6 by oblique ion implantation or the like after forming the gate trench 6. The sidewall well region 17 may be formed simultaneously with the trench bottom protection layer 12, or may be formed separately. The sidewall well region 17 has a size of 1×10 17 [cm -3 ] or more 1 x 10 22 [cm -3 ] or less.

[0072] The effect of the sidewall well region 17 will be described. The sidewall well region 17 electrically connects the trench bottom protective layer 12 and the p-type pillar region 13 to the well region 3 or the well contact region 5. As a result, during switching operation of the MOSFET, a current path is secured for charging and discharging the pn junction formed between the trench bottom protective layer 12 and the p-type pillar region 13 and the n-type pillar region 14 and the drift layer 2, thereby reducing switching loss. Because the sidewall well region 17 is formed only on a portion of the sidewall of the gate trench 6, it does not significantly reduce the channel density, and as a result, it is possible to reduce the on-resistance.

[0073] The gate trenches 6 may be formed in a stripe shape parallel to the off-axis direction, and may have sidewalls on which the sidewall well regions 17 are not formed. In this case, an inversion channel with uniform channel characteristics is formed, which prevents current concentration on a specific channel surface and instability in the threshold voltage, thereby realizing a device with high operational stability.

[0074] 9 and 10 , an example has been shown in which the sidewall well region 17 is provided on only one sidewall of the gate trench 6, but the sidewall well region 17 may be provided on both sidewalls of the gate trench 6, and there are no restrictions on the position at which the sidewall well region 17 is formed. However, if the spacing between the sidewall well regions 17 is too narrow, there is a risk of a decrease in channel density, so the spacing between adjacent sidewall well regions 17 is preferably the same as or greater than the spacing between adjacent gate trenches 6.

[0075] 13 is a plan view schematically showing the structure of a trench-gate MOSFET as a semiconductor device according to the third embodiment. In the semiconductor device according to the third embodiment, the trench bottom protection layer 12 is omitted, and the p-type pillar region 13 is formed so as to contact the bottom of the gate trench 6. Therefore, in the third embodiment, the p-type pillar region 13 plays the role of the trench bottom protection layer 12, which relieves the electric field applied to the bottom and side surfaces of the gate trench 6.

[0076] According to the third embodiment, the manufacturing process is simplified and the manufacturing cost of the semiconductor device can be reduced because the formation of the trench bottom protection layer 12 can be omitted. Furthermore, instead of the trench bottom protection layer 12, the p-type pillar region 13 can alleviate the electric field applied to the bottom and side surfaces of the gate trench 6, thereby achieving the same effects as those of the first embodiment.

[0077] <Fourth Embodiment> Fig. 14 is a plan view schematically showing the structure of a trench-gate MOSFET as a semiconductor device of the fourth embodiment. Fig. 15 is a cross-sectional view taken along the line A1-A2 in Fig. 14, Fig. 16 is a cross-sectional view taken along the line B1-B2 in Fig. 14, and Fig. 17 is a cross-sectional view taken along the line C1-C2 in Fig. 14.

[0078] 14 , in the fourth embodiment, the well contact region 5 is formed in a line shape that is perpendicular to the gate trench 6. In other words, the well contact region 5 extends so as to be in contact with both of the adjacent gate trenches 6 and to cross the mesa-shaped semiconductor layer 20 therebetween.

[0079] Furthermore, in the fourth embodiment, the technique of the second embodiment is applied, and a sidewall well region 17 is provided on a part of the sidewall of the gate trench 6. The sidewall well region 17 serves to electrically connect the trench bottom protection layer 12 or the p-type pillar region 13 to the well region 3 or the well contact region 5.

[0080] As shown in Fig. 15, in the cross section taken along line A1-A2 in Fig. 14, sidewall well region 17 is formed so as to contact well contact region 5. As shown in Fig. 16, in the cross section taken along line B1-B2 in Fig. 14, sidewall well region 17 is not formed, but well contact region 5 is formed. As shown in Fig. 17, in the cross section taken along line C1-C2 in Fig. 9, neither sidewall well region 17 nor well contact region 5 is formed, and well region 3 reaches the surface of semiconductor layer 20.

[0081] For example, when the well contact region 5 is island-shaped as shown in the plan view of FIG. 9 in the second embodiment, if there is a misalignment in the photolithography process, the position of the well contact region 5 relative to the gate trench 6 may be misaligned, which may result in variations in the channel characteristics.

[0082] In contrast, in the fourth embodiment, the well contact region 5 is linear and perpendicular to the gate trench 6, so even if there is a misalignment in the photolithography process, it does not affect the position of the well contact region 5 relative to the gate trench 6, thereby preventing variations in the channel characteristics.

[0083] Furthermore, since the sidewall well region 17 electrically connects the trench bottom protection layer 12 and the p-type pillar region 13 to the well contact region 5, a current path is secured for charging and discharging the pn junction formed between the trench bottom protection layer 12 and the p-type pillar region 13 and the n-type pillar region 14 and the drift layer 2 during switching operation of the MOSFET, thereby reducing switching loss.

[0084] Fifth Embodiment Fig. 18 is a block diagram showing the configuration of a power conversion system to which a power conversion apparatus according to a fifth embodiment is applied. The power conversion system shown in Fig. 18 is composed of a power supply 100, a power conversion apparatus 200, and a load 300. The power supply 100 is a DC power supply and supplies DC power to the power conversion apparatus 200. The power supply 100 can be composed of various components, such as a DC system, a solar cell, or a storage battery, or it may be composed of a rectifier circuit and an AC / DC converter connected to an AC system. Furthermore, the power supply 100 may be composed of a DC / DC converter that converts DC power output from the DC system into a predetermined power.

[0085] The power conversion device 200 is a three-phase inverter connected between the power source 100 and the load 300, and converts DC power supplied from the power source 100 into AC power and supplies the AC power to the load 300. As shown in Fig. 18 , the power conversion device 200 includes a main conversion circuit 201 that converts DC power into AC power and outputs it, a drive circuit 202 that outputs drive signals that drive each switching element of the main conversion circuit 201, and a control circuit 203 that outputs control signals to the drive circuit 202.

[0086] The load 300 is a three-phase electric motor driven by AC power supplied from the power conversion device 200. The load 300 is not limited to a specific application, but is an electric motor mounted on various electrical devices, and is used as an electric motor for, for example, a hybrid vehicle, an electric vehicle, a railroad car, an elevator, or an air conditioning device.

[0087] The power conversion device 200 will be described in detail below. The main conversion circuit 201 includes switching elements and freewheel diodes (not shown). The switching elements convert DC power supplied from the power supply 100 into AC power, which is supplied to the load 300. While the main conversion circuit 201 can have a variety of specific circuit configurations, the main conversion circuit 201 according to this embodiment is a two-level, three-phase full-bridge circuit that can be configured with six switching elements and six freewheel diodes connected in anti-parallel to each switching element. The semiconductor devices according to any of the first to fourth embodiments and their modifications described above are applied to each switching element of the main conversion circuit 201. Two switching elements are connected in series to form upper and lower arms, and each upper and lower arm constitutes one phase (U phase, V phase, and W phase) of the full-bridge circuit. The output terminals of each upper and lower arm, i.e., the three output terminals of the main conversion circuit 201, are connected to the load 300.

[0088] The drive circuit 202 generates drive signals for driving the switching elements of the main conversion circuit 201 and supplies them to the control electrodes of the switching elements of the main conversion circuit 201. Specifically, in accordance with control signals from a control circuit 203 (described later), the drive circuit 202 outputs to the control electrodes of each switching element a drive signal that turns the switching element on and a drive signal that turns the switching element off. When maintaining a switching element in the on state, the drive signal is a voltage signal (on signal) that is equal to or greater than the threshold voltage of the switching element, and when maintaining a switching element in the off state, the drive signal is a voltage signal (off signal) that is less than the threshold voltage of the switching element.

[0089] The control circuit 203 controls the switching elements of the main conversion circuit 201 so that the desired power is supplied to the load 300. Specifically, it calculates the time (on time) that each switching element of the main conversion circuit 201 should be in the on state based on the power to be supplied to the load 300. For example, the main conversion circuit 201 can be controlled by PWM control, which modulates the on time of the switching elements according to the voltage to be output. The control circuit 203 then outputs a control command (control signal) to the drive circuit 202 so that an on signal is output to the switching element that should be in the on state at each time, and an off signal is output to the switching element that should be in the off state at each time. In accordance with this control signal, the drive circuit 202 outputs an on signal or an off signal as a drive signal to the control electrode of each switching element.

[0090] In the power conversion device according to the present embodiment, the semiconductor devices according to the first to fourth embodiments are applied as switching elements of the main conversion circuit 201, so that a low-loss power conversion device can be realized.

[0091] In this embodiment, an example in which the semiconductor device according to the first to fourth embodiments is applied to a two-level three-phase inverter has been described, but the present invention is not limited to this and can be applied to various power conversion devices. In this embodiment, a two-level power conversion device is described, but a three-level or multi-level power conversion device may also be used, and the semiconductor device may be applied to a single-phase inverter when supplying power to a single-phase load. Furthermore, the semiconductor device may also be applied to a DC / DC converter or an AC / DC converter when supplying power to a DC load or the like.

[0092] Furthermore, the power conversion device to which the semiconductor device according to any one of the first to fourth embodiments is applied is not limited to the case where the load described above is an electric motor, but can also be used, for example, as a power supply device for an electric discharge machine, a laser processing machine, an induction heating cooker, or a contactless power supply system, and can also be used as a power conditioner for a solar power generation system, a power storage system, etc.

[0093] It is possible to freely combine the embodiments, and to modify or omit the embodiments as appropriate.

[0094] The above description is illustrative in all respects, and it is understood that countless variations not illustrated can be envisioned.

[0095] 1 semiconductor substrate, 2 drift layer, 3 well region, 4 source region, 5 well contact region, 6 gate trench, 7 gate insulating film, 8 gate electrode, 9 interlayer insulating film, 10 source electrode, 11 drain electrode, 12 trench bottom protective layer, 13 p-type pillar region, 14 n-type pillar region, 14a high-concentration n-type pillar region, 14b low-concentration n-type pillar region, 15 silicide layer, 16 barrier metal, 17 sidewall well region, 18 etching mask, 20 semiconductor layer, 100 power supply, 200 power conversion device, 201 main conversion circuit, 202 drive circuit, 203 control circuit, 300 load.

Claims

1. A semiconductor layer; a drift layer of a first conductivity type formed in the semiconductor layer; a well region of a second conductivity type formed in a surface layer portion of the semiconductor layer; a first conductivity type source region formed in a surface layer portion of the well region; a source electrode electrically connected to the well region and the source region; a plurality of gate trenches each penetrating the source region and the well region and each having a gate electrode embedded therein via a gate insulating film; a first pillar region of a second conductivity type formed below the gate trenches; a second pillar region of a first conductivity type formed between adjacent first pillar regions and having a peak concentration of impurities higher than that of the drift layer; Equipped with the second pillar region is composed of a high concentration region and a low concentration region that is provided on at least one side of the second pillar region and has a peak impurity concentration lower than that of the high concentration region; the high concentration region and the low concentration region have different depths from the surface of the semiconductor layer; Semiconductor device.

2. A depth of a lower end of the second pillar region from a surface of the semiconductor layer is the same as or deeper than a lower end of the first pillar region. The semiconductor device according to claim 1 .

3. a trench bottom protection layer of a second conductivity type formed at a bottom of the gate trench and having a peak concentration of impurities higher than that of the first pillar region; The first pillar region is formed below the trench bottom protection layer.

3. The semiconductor device according to claim 1 or 2.

4. The low concentration regions are provided on both sides of the second pillar region.

3. The semiconductor device according to claim 1 or 2.

5. a concentration of the first conductivity type impurity contained in the first pillar region is lower than a concentration of the first conductivity type impurity contained in the low concentration region; 3. The semiconductor device according to claim 1 or 2.

6. a lower end of the low concentration region is located deeper from the surface of the semiconductor layer than a lower end of the first pillar region; 3. The semiconductor device according to claim 1 or 2.

7. a depth from a bottom of the gate trench to a lower end of the first pillar region is longer than a distance between adjacent gate trenches; 3. The semiconductor device according to claim 1 or 2.

8. a depth from a bottom of the gate trench to a lower end of the first pillar region is longer than a distance between adjacent first pillar regions; 3. The semiconductor device according to claim 1 or 2.

9. a well contact region of a second conductivity type formed in a surface layer portion of the well region so as to be in contact with the source region and having a peak concentration of impurities higher than that of the well region; 3. The semiconductor device according to claim 1 or 2.

10. The well contact region is formed in a line perpendicular to the gate trench. The semiconductor device according to claim 9.

11. a second conductivity type sidewall well region formed on a part of a sidewall of the gate trench for electrically connecting the trench bottom protection layer and the first pillar region to the source electrode; The semiconductor device according to claim 3 .

12. The distance between adjacent sidewall well regions is equal to or greater than the distance between adjacent gate trenches. The semiconductor device according to claim 11.

13. a well contact region of a second conductivity type formed in a surface layer portion of the well region so as to be in contact with the source region and having a peak concentration of impurities higher than that of the well region; the sidewall well region is in contact with the well contact region; The semiconductor device according to claim 11.

14. The well contact region is formed in a line perpendicular to the gate trench. The semiconductor device according to claim 13.

15. The gate trench is filled with an interlayer insulating film covering the gate electrode.

3. The semiconductor device according to claim 1 or 2.

16. a main conversion circuit including the semiconductor device according to claim 1 or 2, which converts input power and outputs the converted power; a drive circuit that outputs a drive signal for driving the semiconductor device to the semiconductor device; a control circuit that outputs a control signal to the drive circuit to control the drive circuit; A power conversion device comprising:

17. forming a semiconductor layer including a drift layer of a first conductivity type; forming a well region of a second conductivity type in a surface layer portion of the semiconductor layer; forming a first conductivity type source region in a surface layer portion of the well region; forming a plurality of gate trenches penetrating the source region and the well region; forming a first pillar region of a second conductivity type below a plurality of the gate trenches; forming a second pillar region of a first conductivity type between adjacent first pillar regions and having a peak concentration of impurities higher than that of the drift layer; forming gate electrodes in the gate trenches via gate insulating films; forming a source electrode electrically connected to the well region and the source region; Equipped with the second pillar region is composed of a high concentration region and a low concentration region that is provided on at least one side of the second pillar region and has a peak impurity concentration lower than that of the high concentration region; the high concentration region and the low concentration region are formed by injecting a first conductivity type impurity into the side surfaces of the plurality of gate trenches by ion implantation at an angle inclined with respect to a depth direction of the semiconductor layer; the high concentration region and the low concentration region have different depths from the surface of the semiconductor layer; A method for manufacturing a semiconductor device.