Method for changing running sheet thickness

JPWO2024147346A5Active Publication Date: 2024-12-03JFE STEEL CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024529328
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-05-16
Publication Date
2024-12-03
Estimated Expiration
2044-01-04

AI Technical Summary

Technical Problem

Existing methods for changing plate thickness during rolling in cold rolling processes face challenges with large tension fluctuations, particularly when rolling high deformation resistance materials, leading to increased risk of breakage and low prediction accuracy due to neglecting differences in rolling conditions and material properties.

Method used

A method that continuously measures plate thickness or speed between rolling stands, detects the plate thickness change position near the joint, and adjusts the roll gap at the target stand based on these measurements to synchronize the plate thickness change, eliminating the need for an intermediate thickness and reducing tension fluctuations.

Benefits of technology

This approach reduces tension fluctuations, prevents breakage, and allows for stable manufacturing by accurately adjusting the roll gap settings during the transition from one material standard to another, maintaining efficient rolling without the need for an intermediate thickness, thus improving the overall process stability.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Provided is a method for changing running sheet thickness, with which it is possible to shorten sheet-thickness off-gauge length and reduce tension fluctuation. This method for changing running sheet thickness is for continuous rolling of a rolling target material (6) in which a leading material (61) and a succeeding material (62), which are metal sheets, are joined by a tandem mill 2. In this method, the sheet thickness or the sheet speed of the rolling target material 6 is continuously measured in a target stand interval between a subject stand (e.g., second stand (2B)) which is a rolling stand where the sheet thickness is changed and a preceding-stage stand (e.g., first stand (2A)) which is a rolling stand in a stage preceding to the subject stand. A sheet-thickness changing position in the vicinity of a joint portion between the leading material (61) and the succeeding material (62) is detected from a sheet-thickness measurement result or tracked from a sheet-speed measurement result. Then, at the timing when said sheet-thickness changing position reaches the subject stand, the roll gap of the subject stand is changed.
Need to check novelty before this filing date? Find Prior Art

Description

How to change plate thickness while running

[0001] The present invention relates to a method for varying gauge while running.

[0002] In cold rolling of steel plates, a technique called "flying gauge change" is used to continue rolling without stopping the rolling mill as much as possible, with the aim of improving efficiency and yield. Flying gauge change involves continuously changing the actuator settings from the preceding coil to the following coil when rolling welds of coils of different specifications, thereby allowing continuous rolling without stopping the rolling mill. When changing the actuator settings for a flying gauge change, particularly when the amount of change in the reduction position is large, it takes time to change the settings, temporarily disrupting the steady state and causing tension instability, which can lead to plate breakage.

[0003] Conventionally, a method of providing an intermediate thickness has been used to suppress tension fluctuations during on-the-fly thickness changes. For example, Patent Document 1 discloses a method of determining an intermediate thickness to suppress tension fluctuations by creating an evaluation function with the thickness fluctuation amount as a variable and determining the intermediate thickness so that the evaluation function falls within a certain threshold. Furthermore, Patent Document 2 discloses a means of suppressing tension fluctuations by determining a tension fluctuation value and resetting the on-the-fly thickness change time during which the set values ​​of the roll gap and roll peripheral speed are changed from pass schedule A to pass schedule B. In Patent Document 2, the tension fluctuation value is determined based on a tension fluctuation value predicted by a tension fluctuation learning means using a neural network that has learned tension fluctuations during actual on-the-fly thickness changes as training data.

[0004] JP2022-12423A JP10-249423A

[0005] Due to recent technological innovations and the expansion of steel sheet applications, various steel sheets (especially electromagnetic steel sheets and high deformation resistance materials such as high tensile strength steel sheets) are now being rolled, and thickness changes during rolling are now being implemented at the joining of coils with significantly different specifications (plate thickness, deformation resistance, etc.). As a result, tension fluctuations during thickness changes during rolling have become large, and solutions using the conventional techniques described above have been attempted.

[0006] However, the method disclosed in Patent Document 1 has a problem in that the thickness-off-gauge length becomes long because an intermediate thickness is provided. Furthermore, the method disclosed in Patent Document 2 does not necessarily take into consideration the influence of changes in rolling conditions before and after the joining zone, such as differences in thickness and deformation resistance between the preceding and succeeding strips, which affect tension fluctuations when passing through the joining zone. Therefore, the method disclosed in Patent Document 2 has low prediction accuracy for tension fluctuations, resulting in large tension fluctuations.

[0007] Therefore, the present invention has been made in consideration of the above-mentioned problems, and aims to provide a method for changing the thickness of a running strip, which can reduce tension fluctuations.

[0008] (1) According to one aspect of the present invention, there is provided a method for changing the thickness of a rolling material, which is formed by joining a preceding material and a following material that are metal plates, using a tandem rolling mill. The method continuously measures the thickness or speed of the rolling material between a target stand, which is a rolling stand that performs the thickness change, and a preceding stand, which is a rolling stand preceding the target stand. The method detects a thickness change position near the joint between the preceding material and the following material from the thickness measurement results or tracks the thickness change position from the speed measurement results. The method changes the roll gap of the target stand at the timing when the thickness change position reaches the target stand.

[0009] (2) In the configuration of (1) above, the length of the tapered plate thickness portion after rolling in the preceding stand is calculated using the plate speed measured between the target stands, the length of the tapered plate thickness portion is divided by the amount of change in the reduction position in the target stand to calculate the rate of change in the reduction position, and the roll gap of the target stand is changed by the calculated rate of change.

[0010] (3) In the configuration of (1) or (2) above, the material to be rolled is a high deformation resistance steel plate.

[0011] According to one aspect of the present invention, there is provided a method for varying thickness while running, which can reduce tension fluctuations.

[0012] 1 is a schematic diagram showing a cold rolling facility according to a first embodiment of the present invention. FIG. 2 is an explanatory diagram showing a conventional method for changing the thickness of a rolling mill while it is running, and FIG. 3A shows a thickness changing position S 1 indicates a state where the stand is located upstream of the first stand, and (B) indicates a thickness change position S 1 (C) shows the state where the joint has reached the first stand, and (D) shows the plate thickness change position S 1 indicates the state where the plate has reached the second stand, and (E) indicates the plate thickness change position S 2 (A) shows a state where the thickness change position is located upstream of the first stand, (B) shows a state where the thickness change position has reached the first stand, (C) shows a state where the joint has reached the first stand, (D) shows a state where the thickness change position has reached the second stand, and (E) shows a state where the joint has reached the second stand. FIG. 1 is a graph showing a change in tension between the first stand and the second stand in a conventional method for changing thickness while flying. FIG. 2 is an explanatory diagram showing a method for changing thickness while flying according to a first embodiment, where (A) shows a state where the thickness change position is located upstream of the first stand, (B) shows a state where the thickness change position has reached the first stand, (C) shows a state where the joint has reached the first stand, (D) shows a state where the thickness change position has reached the second stand, and (E) shows a state where the joint has reached the second stand. FIG. 2 is a schematic diagram showing cold rolling equipment in a second embodiment of the present invention. 1 is an explanatory diagram showing a method for changing the thickness of a running steel sheet according to a second embodiment of the present invention, where (A) shows a state in which the thickness change position is upstream of the first stand, (B) shows a state in which the thickness change position has reached the first stand, (C) shows a state in which the joint has reached the first stand, (D) shows a state in which the joint has passed the first stand and the thickness change position is upstream of the second stand, (E) shows a state in which the thickness change position has reached the second stand, and (F) shows a state in which the joint has reached the second stand.

[0023] FIG. 1 is a flowchart showing a method for changing the thickness of a running steel sheet according to a second embodiment of the present invention.

[0024] FIG. 2 is a graph showing the change in tension between the first stand and the second stand when changing the thickness of a running steel sheet ends early.

[0013] In the following detailed description, embodiments of the present invention will be described with reference to the drawings. In the description of the drawings, identical or similar parts are designated by identical or similar reference numerals, and redundant explanations will be omitted. The drawings are schematic and may differ from the actual product. Furthermore, the embodiments shown below exemplify devices and methods for embodying the technical concept of the present invention, and the technical concept of the present invention does not specify the materials, structure, arrangement, etc. of component parts as described below. The technical concept of the present invention can be modified in various ways within the technical scope defined by the claims.

[0014] <First embodiment> (Configuration of tandem cold rolling mill) First, a running gauge method according to a first embodiment of the present invention will be described. Fig. 1 is a schematic configuration diagram showing an example of continuous cold rolling equipment 1 in the first embodiment of the present invention. Note that Fig. 1 does not show other devices incidental to the equipment (for example, an unwinder, a welder, and a looper on the entry side, and devices such as a cutter and a winder on the delivery side).

[0015] As shown in FIG. 1 , the continuous cold rolling facility 1 includes a tandem rolling mill 2, a plurality of plate thickness measuring devices 3, a rolling control controller (PLC) 4 that controls the tandem rolling mill 2, and a control computer (process computer) 5 that manages the continuous cold rolling facility including the rolling control controller 4.

[0016] The tandem rolling mill 2 is a continuous cold tandem rolling mill having, in order from the entry side in the strip threading direction, a first stand 2A to a fifth stand 2E.

[0017] Each of the first stand 2A to the fifth stand 2E is equipped with a work roll 21, a roll speed control device 22 which is an electric motor that changes the roll speed of the work roll 21, and a roll gap control device 23 that changes the roll gap between the upper and lower work rolls 21.

[0018] The multiple thickness measuring devices 3 are installed between adjacent stands (between stands) of the first stand 2A to the fifth stand 2E, and continuously measure the thickness of the rolled material 6, which is a metal plate, passing between the stands. There are no particular limitations on the method of measuring the thickness using the thickness measuring devices 3, but one possible method is to use a measuring device that irradiates the object with gamma rays or X-rays, measures the attenuation of the gamma rays (X-rays) that pass through the object, and converts the attenuation into thickness. The thickness measurement results from the thickness measuring devices 3 are sent to the control computer 5.

[0019] The control computer 5 sets the roll gap value, roll gap change amount, roll speed, roll speed change amount, etc. of each stand. Then, the rolling controller 4 executes calculations and processing online to control the roll speed control device 22 of each stand of the first stand 2A to the fifth stand 2E and the roll gap control device 23 of each stand, based on each value acquired from the control computer 5.

[0020] In this cold rolling facility 1, the tail end of the preceding strip 61 and the leading end of the following strip 62 are joined at a joint W by a welding machine (not shown) disposed on the entry side of the tandem rolling mill 2. The rolled strip 6 is then rolled sequentially from the first stand 2A of the cold rolling mill to the fifth stand 2E, which is the final stand, until it is rolled to a predetermined finished thickness. Thereafter, the rolled strip 6 is cut by a flying cut-off machine at or near the joint W between the preceding strip 61 and the following strip 62, and the cut following strip 52 is taken up by a tension reel separate from that for the preceding strip 51.

[0021] Here, if the rolling conditions such as the base plate thickness, finished plate thickness, deformation resistance, etc. are different between the preceding material 61 and the succeeding material 62, when the preceding material 61 and the succeeding material 62 are continuously rolled in a cold rolling mill, the rolling conditions are changed while the material to be rolled 6 is in flight (i.e., while the material to be rolled 6 is being transported within the tandem rolling mill 2), and a thickness change while the material is in flight is performed.

[0022] In a typical conventional method, the roll gap setting value is changed based on the tracking of the joint W (using the joint W as the reference) when the thickness change position, which is set a predetermined distance away from the joint toward the preceding material 61, reaches the stand. Specifically, the thickness change while running is performed using the method shown in Figures 2(A) to 2(F). The tension fluctuation between the first stand 2A and the second stand 2B at this time is shown in Figure 3. The timings (a) to (f) in Figure 3 correspond to the timings in the states of Figures 2(A) to 2(F), respectively.

[0023] First, as shown in FIG. 2A, rolling is performed with the roll gap value of each stand set to that for the preceding material 61. In FIG. 2A, the S 1 The position indicated by is the position where the roll gap setting value is changed in the first stand 2A.

[0024] As the rolling progresses further, the thickness change position S 1 reaches the first stand 2A, and the change of the roll gap setting value of the first stand 2A is started so that the roll gap setting value of the first stand 2A becomes that for the succeeding material 62. 1 is set at a position spaced a predetermined distance from the joint W on the tail end side of the preceding material 61. 1 The position is set depending on the time required to change the roll gap, the speed of the strip, etc., as will be described later.

[0025] As the rolling progresses further, as shown in FIG. 2(C), the change in the roll gap setting value of the first stand 2A is completed, and the first stand 2A starts rolling the following material 62. 1 is set so that the change in the roll gap setting value is completed before the joint W reaches the first stand 2A. By changing the roll gap setting value as shown in Figures 2(B) and 2(C), the plate thickness changes in a tapered shape from the tail end of the preceding material 61 to the joint W.

[0026] As the rolling progresses further, the thickness change position S 1 reaches the second stand 2B. As will be described later, the roll gap setting value at the second stand 2B is changed by setting the thickness change position S 2 The thickness change position S 2 is the plate thickness change position S 1 Similarly, the thickness change position S of the first stand 2A is set at a position a predetermined distance away from the joint W on the tail end side of the preceding material 61. As shown in FIG. 2(D), the preceding material 61 that has passed through the first stand 2A is rolled and its length in the longitudinal direction is extended. 1 and the plate thickness changing position S of the second stand 2B 2 It will be a different position.

[0027] In the state shown in Figure 2(D), the tapered thickness portion of the rolled material 6 reaches the second stand 2B before the roll gap of the second stand 2B is changed. At this time, the roll gap setting value of the second stand 2B is set to that for the preceding material 61, so the tension between the first stand 2A and the second stand 2B decreases, as shown in Figure 3. This causes large tension fluctuations and increases the risk of breakage.

[0028] As the rolling progresses further, the thickness change position S 2 reaches the second stand 2B, and the change in the roll gap setting value of the second stand 2B starts so that the roll gap setting value of the second stand 2B becomes that for the following material 62.

[0029] Furthermore, as shown in Figure 2 (F), the change in the roll gap setting value of the second stand 2B is completed, and the second stand 2B starts rolling the following material 62. For the third stand 2C and onwards, the roll gap setting value is changed in the same way as for the second stand 2B, thereby changing the running thickness. That is, for each stand from the third stand 2C onwards, the roll gap setting value is changed as the thickness change position S that is set for each stand passes through that stand. Note that in each stand, the change in the roll peripheral speed setting is made in synchronization with this change in the roll gap setting.

[0030] (Method of changing the thickness of a running strip) Figures 4(A) to 4(E) are explanatory diagrams showing a method of changing the thickness of a running strip according to the first embodiment. Figures 4(A) to 4(C) show a change in the roll gap set value of the first stand 2A, and the roll gap set value is changed in the same manner as in Figures 2(A) to 2(C). Figure 5 shows the tension fluctuation between the first stand 2A and the second stand 2B at this time. Note that the timings (a) to (e) in Figure 5 correspond to the timings in the states of Figures 4(A) to 4(E), respectively.

[0031] In the first embodiment, a thickness measuring device 3 is provided between the first stand 2A and the second stand 2B, and continuously measures the thickness of the material 6 to be rolled passing between the stands. The control computer 5 detects a thickness change position S at which the thickness of the material 6 to be rolled changes, based on the measurement results of the thickness measuring device 3. The detected thickness change position S is the thickness change position S set in the first stand 2A, and is the position at which the thickness changes in a tapered shape.

[0032] Next, when a thickness change position S is detected between the first stand 2A and the second stand 2B, the control computer 5 changes the roll gap set value of the second stand 2B at the timing when the thickness change position S reaches the second stand 2B, as shown in Figure 4(D). At this time, the roll gap set value of the second stand 2B is changed from the set value for the preceding material 61 to the set value for the following material 62. Because the roll gap set value of the second stand 2B is changed at the thickness change position S, as shown in Figure 5, even if the tapered thickness portion reaches the second stand 2B, the decrease in tension is compensated for, and the risk of breakage due to the decrease in tension can be reduced.

[0033] As rolling progresses, as shown in Figure 4 (E), the change in the roll gap setting value for the second stand 2B is completed, and the second stand 2B starts rolling the following material 62. For the third stand 2C and beyond, the roll gap setting value is changed in the same way as for the second stand 2B, thereby changing the running thickness. That is, for each stand from the third stand 2C onwards, the thickness change position S is detected from the measurement results of the thickness measuring device 3 provided between each stand, and the roll gap setting value is changed when the thickness change position S reaches each stand. In addition, in each stand, the setting of the roll peripheral speed is changed in synchronization with this change in the roll gap setting.

[0034] In the first embodiment, the material 6 to be rolled is a metal plate, and is preferably a steel plate, particularly a high deformation resistance steel plate. High deformation resistance steel plates include, for example, steel plates of electromagnetic materials or high-tensile strength materials. Such high deformation resistance steel plates require a large amount of reduction during thickness change while running, and the thickness of the front portion of the weld zone due to thickness change while running in the upstream stand significantly deviates from the set thickness, resulting in large tension fluctuations. Therefore, by applying the method for thickness change while running according to the first embodiment, problems such as breakage can be prevented, and stable production can be achieved.

[0035] The method for changing the thickness of a running material according to the first embodiment is a method for changing the thickness of a running material when a tandem rolling mill 2 is continuously rolling a material 6 to be rolled, which is a metal plate consisting of a leading material 61 and a trailing material 62 joined together. The method continuously measures the thickness of the material between target stands, detects a thickness change position S near the joint W, and changes the roll gap of the target stand when the thickness change position reaches the target stand. The target stand is the rolling stand that performs the thickness change, and the preceding stand is the rolling stand installed adjacent to the target stand on the upstream side in the rolling direction. For example, in FIG. 4 , when changing the roll gap of the second stand 2B, the second stand 2B is the target stand and the first stand 2A is the preceding stand.

[0036] According to the method for varying the thickness on the fly of the first embodiment, it is not necessary to provide an intermediate thickness, and therefore the thickness off-gauge length can be shortened, compared to the method described in Patent Document 1. Furthermore, according to the method for varying the thickness on the fly of the first embodiment, the roll gap is changed using the thickness change point in the front stand as the thickness change point in the rear stand, and therefore tension fluctuations can be suppressed regardless of the material or specifications of the rolled material 6.

[0037] <Second embodiment> (Configuration of tandem cold rolling mill) Next, a running gauge method according to a second embodiment of the present invention will be described. Fig. 6 is a schematic configuration diagram showing an example of continuous cold rolling equipment 1 according to the second embodiment of the present invention. Note that in Fig. 6, similar to Fig. 1, other devices incidental to the equipment are not shown.

[0038] As shown in FIG. 6 , the continuous cold rolling facility 1 includes a tandem rolling mill 2, a rolling control controller (PLC) 4 that controls the tandem rolling mill 2, a control computer (process computer) 5 that manages the continuous cold rolling facility including the rolling control controller 4, and a plurality of strip speed meters 7.

[0039] The tandem rolling mill 2 is a continuous cold tandem rolling mill having, in order from the entry side in the strip threading direction, a first stand 2A to a fifth stand 2E.

[0040] Each of the first stand 2A to the fifth stand 2E is equipped with a work roll 21, a roll speed control device 22 which is an electric motor that changes the roll speed of the work roll 21, and a roll gap control device 23 that changes the roll gap between the upper and lower work rolls 21.

[0041] The control computer 5 sets the roll gap value, roll gap change amount, roll speed, roll speed change amount, etc. of each stand. Then, the rolling controller 4 executes calculations and processing online to control the roll speed control device 22 of each stand of the first stand 2A to the fifth stand 2E and the roll gap control device 23 of each stand, based on each value acquired from the control computer 5.

[0042] The plurality of strip speed meters 7 are provided between adjacent stands (between stands) of the first stand 2A to the fifth stand 2E, and continuously measure the strip speed, which is the speed in the conveying direction of the rolled material 6, which is a metal plate, passing between the stands. There are no particular restrictions on the method for measuring the strip speed using the strip speed meters 7, but a laser Doppler velocimeter, for example, is conceivable. The results of measurement of the strip speed by the strip speed meters 7 are sent to the control computer 5.

[0043] As in the first embodiment, in the cold rolling facility 1, the tail end of the preceding strip 61 and the leading end of the following strip 62 are joined at a joint W by a welding machine (not shown) disposed on the entry side of the tandem rolling mill 2. The rolled strip 6 is then rolled sequentially from the first stand 2A of the cold rolling mill to the final stand, the fifth stand 2E, until it is rolled to a predetermined finished thickness. The rolled strip 6 is then cut by a flying cut-off machine at or near the joint W between the preceding strip 61 and the following strip 62, and the cut following strip 52 is reeled up by a tension reel separate from that for the preceding strip 51. As in the first embodiment, if the rolling conditions, such as the base strip thickness, the finished strip thickness, and the deformation resistance, differ between the preceding strip 61 and the following strip 62, a flying thickness change is performed.

[0044] (Method of changing the thickness while running) Figures 7(A) to 7(F) and 8 are explanatory diagrams showing a method of changing the thickness while running according to the second embodiment. Figures 7(A) to 7(C) show a method of changing the roll gap set value of the first stand 2A (method of changing the thickness while running), and the roll gap set value is changed in the same way as in Figures 2(A) to 2(C).

[0045] In the following explanation, a method for changing the roll gap setting value of the second stand 2B, that is, a method for changing the flying strip thickness, will be described. The flying strip thickness change of the second stand 2B is performed in accordance with the processing flow shown in Figure 8. Note that the flying strip thickness change is also performed in the rolling stands after the second stand 2B in the same manner as the second stand 2B. Here, as in the first embodiment, the rolling stand that performs the flying strip thickness change is also referred to as the target stand, and the rolling stand preceding the target stand is also referred to as the preceding stand. Also, the processing flow shown in Figure 8 is started when the flying strip thickness change of the preceding stand (first stand 2A) begins, that is, when the state shown in Figure 7(B) is reached.

[0046] When a running thickness change is initiated at the first stand 2A, first, the strip speed meter 7 installed between the target stands is used to continuously measure the strip speed of the rolled material 6 passing between the target stands (S100). The target stands refer to the area between the target stand and the preceding stand. In the case where the target stand is the second stand 2B, this area is between the second stand 2B and the first stand 2A. Furthermore, strip speed measurement is continuously performed at least until a running thickness change is performed at the target stand. In other words, when the target stand is the second stand 2B, strip speed measurement is continuously performed at least from the time when the thickness change position S shown in FIG. 7(B) reaches the first stand 2A until the thickness change position S shown in FIG. 7(E) reaches the second stand 2B. Furthermore, the control computer 5 tracks the thickness change position S of the rolled material 6 based on the results of measurement of the strip speed between the target stands by the strip speed meter 7.

[0047] After step S100, the control computer 5 calculates the length L of the tapered plate thickness portion after rolling in the front stand. N-1 (S102). N indicates the number of the target stand (Nth stand). In other words, when the target stand is the second stand 2B, the length L of the tapered thickness portion after rolling in the first stand 2A is calculated. 1is calculated. The tapered thickness portion is a portion where the thickness of the material 6 to be rolled changes in a tapered manner due to a thickness change during rolling in the preceding stand. When the target stand is the second stand 2B, the tapered thickness portion is the portion from the thickness change position S to the joining portion W in Figure 7(D).

[0048] Length of tapered plate thickness L N-1 is calculated by integrating (the strip speed of the front stand) x (time) until the thickness change while running at the front stand is completed. Specifically, the length L of the tapered thickness portion N-1 is calculated using the following formula (1): In formula (1), the measurement timing of the strip speed is defined as a time step, and the strip speed v N-1(i) and time T i From the length L N-1 The number of time steps is 1 at the measurement timing of the start of the on-the-fly thickness change and m at the measurement timing of the end of the on-the-fly thickness change. i indicates the elapsed time from a predetermined timing as a starting point to each time step.

[0049] Here, T i : Time at time step i [s] v N-1(i) : Strip speed between target stands at time step i [m / s]

[0050] After step S102, the control computer 5 determines the time t until the tapered plate thickness portion enters the target stand. N In step S104, the strip speed between the target stands measured by the strip speed meter 7 immediately before the running strip thickness change is performed at the target stand, that is, immediately before step S104, and the length L calculated in step S102 are calculated. N-1 and time t N In the second embodiment, the time t N corresponds to the time from when the thickness changing position S of the rolled material 6 enters the target stand until when the welded portion W enters the target stand. N can be calculated using the following formula (2).

[0051]

[0052] After step S104, the control computer 5 calculates the change amount ΔS of the roll position in the target stand. N and time t N The speed of change of the pressing position R N is calculated (S106). The change amount of the roll gap in the target stand corresponds to the adjustment amount of the roll gap in the target stand, and is the amount of movement of the upper and lower work rolls 21 in the thickness direction of the material 6 to be rolled in accordance with the change in plate thickness. The change amount of plate thickness is a value that is set in advance. The change speed R of the roll gap in the target stand N is the moving speed of each work roll 21 when changing the rolling position (i.e., when changing the running thickness). N can be calculated using the following formula (3). The processes up to step S104 are performed before the thickness change position S reaches the target stand. It is also preferable that the processes of steps S102 and S104 be performed immediately before the tapered thickness portion reaches the target stand.

[0053]

[0054] After step S106, when the plate thickness change position S reaches the target stand, the control computer 5 calculates the change speed R N and plate thickness change amount Δs N The running strip thickness is changed, that is, the roll gap set value is changed (S108). As described above, the strip thickness change position S is tracked from the strip speed measurement results, and the control computer 5 changes the running strip thickness by detecting the arrival of the strip thickness change position S at the target stand from the tracking results. In step S108, the running strip thickness is changed at the change speed R N and plate thickness change amount Δs N By changing the thickness while flying, the change of the thickness while flying is completed when the welded portion W reaches the target stand. When the target stand is the second stand 2A, as shown in FIG. 7(D), the arrival of the thickness change position S at the second stand 2A is detected by tracking, and the roll gap setting value at the second stand 2B is changed. Then, in step S108, the change speed R Nand plate thickness change amount Δs N By changing the thickness while the welded joint is performed, the thickness change while the welded joint is completed when the welded joint W reaches the second stand 2B, as shown in FIG. 7(F).

[0055] As described above, the third stand 2C to the fifth stand 2E also undergo a running strip thickness change in the same manner as the second stand 2B. In this case, by using the results of measuring the strip speed between a plurality of target stands from the first stand 2A, the strip thickness change position S can be tracked within the line of the tandem rolling mill 2.

[0056] In the second embodiment, the material 6 to be rolled is a metal plate, and is preferably a steel plate, particularly a high deformation resistance steel plate. High deformation resistance steel plates include, for example, steel plates of electromagnetic materials or high-tensile strength materials. Such high deformation resistance steel plates require a large amount of reduction during thickness change while running, and the thickness of the front portion of the weld zone due to thickness change while running in the upstream stand significantly deviates from the set thickness, resulting in large tension fluctuations. Therefore, by applying the method for thickness change while running according to the second embodiment, problems such as breakage can be prevented, and stable production can be achieved.

[0057] The method for changing the thickness of a running material according to the second embodiment is a method for changing the thickness of a running material when a rolled material 6, which is made up of a leading material 61 and a trailing material 62 that are metal plates joined together, is continuously rolled by a tandem rolling mill 2, in which the plate speed of the rolled material is continuously measured between the target stands, the plate thickness change position S near the joint W is tracked, and the roll gap of the target stand is changed at the timing when the plate thickness change position reaches the target stand.

[0058] According to this method, as in the first embodiment, it is not necessary to provide an intermediate thickness, and therefore the thickness off-gauge length can be shortened. Furthermore, according to the method for changing the thickness on the fly according to the second embodiment, the roll gap is changed using the thickness change point in the front stand as the thickness change point in the rear stand, so tension fluctuations can be suppressed regardless of the material or specifications of the rolled material 6.

[0059] In addition, the method for changing the thickness of a running strip according to the second embodiment uses the strip speed measured between the target stands to calculate the length L of the tapered strip thickness portion after rolling in the front stand.N-1 Calculate the length L of the tapered plate thickness portion N-1 is divided by the change amount of the roll-down position in the target stand to obtain the roll-down position change speed R N is calculated, and the calculated change speed R N to change the roll gap of the target stand.

[0060] FIG. 9 shows the tension change between the first stand 2A and the second stand 2B when the on-the-fly thickness change in the second stand 2B ends midway through the tapered thickness portion, i.e., when the on-the-fly thickness change ends earlier than in the second embodiment. If the on-the-fly thickness change ends too early, as shown near timing (f) in FIG. 9 , the roll gap change ends midway through the tapered thickness portion, which may result in excessive tension in the subsequent rolling of the tapered thickness portion. However, according to the on-the-fly thickness change method of the second embodiment, the start and end timings of the roll gap change can be determined by the timings at which the start point (thickness change position S in FIG. 7 ) and end point (joint W in FIG. 7 ) of the tapered thickness portion pass through the target stand. As a result, the on-the-fly thickness change method of the second embodiment can prevent excessive tension.

[0061] The thickness in the first embodiment and the strip speed in the second embodiment are also collectively referred to as operation data. In other words, the method for changing the thickness while rolling according to the present invention detects or tracks the thickness change position S from the operation data of the rolled material 6 measured between the target stands, thereby changing the thickness while rolling at the timing when the thickness change position S reaches the target stand.

[0062] <Modifications> Although the present invention has been described above with reference to specific embodiments, it is not intended that the invention be limited by these descriptions. By referring to the description of the present invention, other embodiments of the present invention that include various modifications in addition to the disclosed embodiments will be apparent to those skilled in the art. Therefore, it should be understood that the embodiments of the invention described in the claims also encompass embodiments that include these modifications described herein, either alone or in combination.

[0063] For example, in the first and second embodiments, the tandem rolling mill 2 shown in Fig. 1 is a rolling mill having five stands, but the present invention is not limited to such an example. The number of stands in the tandem rolling mill 2 may be two or more, and may be six or more. In the case of a general tandem rolling mill 2, the upper limit of the number of stands is six.

[0064] Furthermore, in the first and second embodiments, a case has been described in which the thickness of the following material 62 in the rolled material 6 is thinner than the thickness of the preceding material 61, but the present invention is not limited to such an example. The thickness of the following material 62 in the rolled material 6 may be thicker than the thickness of the preceding material 61. In this case, the tension between the stands fluctuates to increase.

[0065] Furthermore, in the first and second embodiments, four thickness measuring devices 3 or strip speed meters 7 are provided, and the roll gap setting values ​​at the second stand 2B to the fifth stand 2E are changed based on the measurement results of the four thickness measuring devices 3 or strip speed meters 7. However, the present invention is not limited to such an example. For example, the roll gap setting values ​​may be changed only between stands where large tension fluctuations are a problem, as in the above embodiment, and the roll gap setting values ​​for other stands may be changed using a control method similar to that of the conventional method. In this case, thickness measuring devices 3 or strip speed meters 7 may be provided only between necessary stands. Furthermore, thickness measuring devices 3 and strip speed meters 7 may be provided between different stands, and the running thickness may be changed for each target stand according to the thickness measuring devices 3 or strip speed meters 7 provided between the stands, as in the first or second embodiment.

[0066] Furthermore, in the second embodiment, the plate speed meter 7 is used as a method for measuring the plate speed, but the present invention is not limited to this example. For example, the plate speed may be calculated by calculating the motor rotation speed of each rolling stand measured by a PLG or an absocorder and the forward slip calculated from operational data. Note that, in consideration of measurement accuracy, it is preferable to measure the plate speed using the plate speed meter 7.

[0067] REFERENCE SIGNS LIST 1 cold rolling mill equipment 2 tandem rolling mills 2A to 2E first stand to fifth stand 21 work roll 22 roll speed control device 23 roll reduction control device 3 plate thickness measuring device 4 rolling control controller 5 control computer 6 rolled material 61 preceding material 62 succeeding material 7 plate speed meter

Claims

1. A method for changing a thickness of a rolling material in a continuous rolling process using a tandem rolling mill, the method comprising the steps of: The thickness or speed of the rolled material is continuously measured between a target stand which is a rolling stand performing a thickness change and a front stand which is a rolling stand preceding the target stand, A plate thickness change position in the vicinity of the joint between the preceding material and the following material is detected from the plate thickness measurement result or tracked from the plate speed measurement result; Calculate the length of the tapered plate thickness portion after rolling in the front-stage stand using the plate speed measured between the target stands; Calculating a speed of change of the reduction position by dividing the length of the tapered plate thickness portion by an amount of change of the reduction position in the target stand; A method for changing a thickness while running, the method comprising: changing a roll gap of the target stand at the calculated change speed at a timing when the thickness change position reaches the target stand.

2. The method for varying thickness while rolling according to claim 1, wherein the material to be rolled is a high deformation resistance steel plate.