Waterproof Planting Planter Using ABS Plate and Manufacturing Method Thereof

The waterproof plant structure using ABS sheets and MC solution with triangular brackets addresses weight, watertightness, and stability issues, offering lightweight, durable, and aesthetically pleasing designs with enhanced bonding strength and antibacterial properties.

KR103043960B1Active Publication Date: 2026-11-10주비오시스
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
KR1020260005205
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2026-01-12
Publication Date
2026-11-10
Estimated Expiration
2046-01-12

AI Technical Summary

Technical Problem

Conventional planting systems face issues with weight, watertightness, structural stability, and aesthetic appeal due to the use of heavy materials like concrete and plastic, which deform under water and soil pressure, leading to leakage and high production costs.

Method used

A waterproof plant structure using ABS sheets fused with an MC solution and reinforced with triangular brackets, combined with a viscous layer of MC solution and ABS resin powder, to enhance bonding strength and prevent deformation.

Benefits of technology

The structure provides superior watertightness, structural stability, and lightweight design, allowing for curved shapes and reduced production time, while maintaining aesthetic appeal through CNC machining and antibacterial properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112026003998012-PAT00001_ABST
    Figure 112026003998012-PAT00001_ABST
Patent Text Reader

Abstract

The present invention relates to a waterproofing plant using ABS sheet material and a method for manufacturing the same, comprising: a bottom plate made of ABS sheet material; a side plate made of ABS sheet material that is fused and bonded with an MC solution and positioned vertically at the edge of the bottom plate; and a reinforcing bracket made of a triangular ABS sheet material that is fused and bonded with an MC solution and positioned on the inner side of the corner where the bottom plate and the side plate meet, wherein the reinforcing bracket is extended to at least 60% of the height of the side plate to prevent the side plate from deforming outward. According to the present invention, excellent watertightness can be secured through fusion bonding using an MC solution, structural stability can be improved with a reinforcing bracket, and a viscous mixture of an ABS strip, an MC solution, and ABS resin powder in a weight ratio of 3:1 to 5:1 can be applied to the joint to enable long-term use without leakage.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to a waterproof plant for planting, and more specifically, to a waterproof plant for indoor and outdoor planting that secures long-term watertightness and structural stability by fusing ABS (acrylonitrile-butadiene-styrene) plates with an MC (methylene chloride) solution and providing a reinforcing bracket, and a method for manufacturing the same. Background Technology

[0003] Recently, various types of planting systems, terrariums, vivariums, and paludariums are being installed to enhance the comfort and aesthetics of indoor spaces. Since these structures must retain water or soil for extended periods, excellent watertightness is required. Conventional planting systems were primarily manufactured from materials such as concrete, metal, and plastic, but they presented the following problems. First, concrete and metal materials were excessively heavy, making indoor installation difficult; they also limited the realization of curved designs and involved long production times and high costs. Second, general plastic materials were prone to leakage at joints and easily deformed due to water or soil pressure, leading to reduced structural stability during long-term use. Third, existing plastic welding methods had weak joint strength, resulting in a high risk of leakage, and the rough finish of the joints was aesthetically unpleasing. Fourth, in the case of plants with high height or large volume, deformation occurs where the sides are pushed outward due to water pressure or earth pressure, which reduces structural stability and causes leakage. Therefore, there is a need to develop a new waterproof plant structure and manufacturing method that is lightweight, possesses excellent watertightness and structural stability, can be manufactured in various shapes such as curves, and can reduce manufacturing time and costs. The problem to be solved

[0005] The present invention was devised to solve the problems of the conventional technology described above, and aims to provide a waterproof plant and a method for manufacturing the same that can be used stably for a long period of time by securing excellent watertightness by fusing ABS plates with an MC solution and preventing deformation caused by water pressure and earth pressure by providing a triangular reinforcing bracket.

[0006] In addition, the present invention aims to provide a waterproof plant and a method for manufacturing the same, which further improves bonding strength and watertightness by attaching an ABS sheet strip to the joint and applying a mixed liquid of MC solution and ABS resin powder.

[0007] In addition, the present invention aims to provide a waterproof plant and a method for manufacturing the same, which enables the production of precise curved shapes through CNC machining and allows the application of various finishing materials. means of solving the problem

[0009] According to one embodiment of the present invention, a waterproofing plant is provided comprising: a bottom plate made of ABS sheet material; a side plate made of ABS sheet material that is fused and bonded with an MC solution and positioned vertically at the edge of the bottom plate; and a reinforcing bracket made of a triangular ABS sheet material that is fused and bonded with an MC solution and positioned on the inner side of the corner where the bottom plate and the side plate meet, wherein the reinforcing bracket extends up to 60% or more of the height of the side plate to prevent the side plate from deforming outward.

[0010] In the present invention, ABS sheet metal strips are attached to the fused joints of the bottom plate and the side plate and the fused joints of the reinforcing bracket.

[0011] In the present invention, the fusion joint portion of the bottom plate, side plate, and reinforcing bracket is provided with a viscous layer formed from a mixture of MC solution and ABS resin powder, wherein the MC solution and ABS resin powder are mixed in a weight ratio of 3:1 to 5:1, and the viscous layer functions as (i) a first functional layer that assists the fusion joint strength, (ii) a second buffering layer that absorbs microcracks, and (iii) a third interface layer that relieves stress due to differences in thermal expansion, and the viscous layer is formed with a thickness of 0.5 mm to 2.5 mm after curing.

[0012] In the present invention, the reinforcing bracket is formed with a tapered structure in which the thickness gradually decreases from the bottom to the top, and the lower thickness of the reinforcing bracket is formed to have a range of 1.3 to 3 times the upper thickness, so as to preferentially support the stress generated by water pressure and earth pressure from the bottom and distribute it to the top.

[0013] In the present invention, the ABS is a copolymer of acrylonitrile, butadiene, and styrene, and the MC solution is methylene chloride.

[0014] In the present invention, the inner surface of the waterproof plant is further provided with an antibacterial layer formed on top of a mucus layer, wherein the antibacterial layer is formed from an antibacterial composition comprising an antibacterial particle containing one or more of silver (Ag), copper (Cu), and zinc (Zn), and an acrylic or urethane-based binder, and the antibacterial composition contains 0.1% to 5% by weight of the antibacterial particle and is formed on top of the mucus layer by coating or spraying.

[0015] In the present invention, a plurality of waterproof plant modules are arranged adjacent to each other, and the joints between the modules are joined in a structure including MC solution fusion, ABS sheet metal strips, and a mucus layer to form a single large waterproof plant structure.

[0016] According to another embodiment of the present invention, the method comprises: (a) cutting an ABS sheet to form a bottom plate and a side plate; (b) fusing the edge of the bottom plate and the side plate with an MC solution; (c) fusing a triangular-shaped ABS sheet with an MC solution to the inner corner where the bottom plate and the side plate meet to form a reinforcing bracket; and (d) forming a viscous layer by mixing an MC solution and ABS resin powder at the fused joint, wherein the MC solution and ABS resin powder are mixed in a weight ratio of 3:1 to 5:1; and wherein the reinforcing bracket is formed to extend up to 60% or more of the height of the side plate.

[0017] In the present invention, in steps (b) and (c), an ABS sheet metal strip is attached to the joint during fusion bonding, and in step (d), the viscous layer is formed to function as (i) a first functional layer that assists the fusion bonding strength, (ii) a second buffer layer that absorbs microcracks, and (iii) a third interface layer that relieves stress due to differences in thermal expansion, and the viscous layer is formed with a thickness of 0.5 mm to 2.5 mm based on the curing state.

[0018] In the present invention, in step (b), the MC solution is injected from one end of the bonding surface to the opposite end or from top to bottom to prevent bubble formation.

[0019] In the present invention, in steps (b) and (c), pressure is applied using a clamp or weight until the fused surface hardens.

[0020] In the present invention, the inner surface of the waterproofing plant is further provided with an antibacterial layer formed on top of a mucus layer, wherein the antibacterial layer is formed from an antibacterial composition comprising an antibacterial particle containing one or more of silver (Ag), copper (Cu), and zinc (Zn) and an acrylic or urethane-based binder, and wherein the antibacterial composition contains 0.1% to 5% by weight of the antibacterial particle, and further includes the step of forming the antibacterial layer on top of the mucus layer by coating or spraying. Effects of the invention

[0022] The waterproof plant and the method for manufacturing the same according to the present invention have the following effects.

[0023] First, by fusing ABS sheets with MC solution, superior water tightness and bonding strength can be secured compared to conventional adhesive or bolt fastening methods.

[0024] Second, by placing triangular reinforcing brackets up to more than 60% of the height of the side plate, deformation of the side plate due to water pressure and earth pressure can be effectively prevented, thereby maintaining structural stability for a long period.

[0025] Third, watertightness can be further enhanced by attaching ABS sheet metal strips to the joints and applying a mixture of MC solution and ABS resin powder to prevent the formation of microcracks and bubbles.

[0026] Fourth, due to the lightweight nature of ABS panels, the weight is significantly reduced compared to concrete or metal materials, making indoor installation easy and minimizing the load applied to the structure.

[0027] Fifth, CNC machining enables the production of precise curved shapes, allowing for the realization of various designs, and the application of various finishing materials such as interior films and artificial marble can enhance aesthetics.

[0028] Sixth, on-site production is possible and the production period is short, which can shorten the construction period and reduce costs. Brief explanation of the drawing

[0029] FIG. 1 is a cross-sectional view of a waterproofing plant according to one embodiment of the present invention. FIG. 2 is a schematic perspective view of a waterproofing plant according to one embodiment of the present invention. FIG. 3 is a schematic diagram of a reinforcing bracket installation according to one embodiment of the present invention. FIG. 4 is a schematic diagram of a corner joint according to one embodiment of the present invention. FIG. 5 is a schematic diagram of a surface bonding according to one embodiment of the present invention. FIG. 6 is a schematic diagram of a reinforcing joint during lateral joining according to one embodiment of the present invention. FIG. 7 is a flowchart of a manufacturing process according to one embodiment of the present invention. Specific details for implementing the invention

[0030] Specific details of other embodiments are included in the detailed description and drawings.

[0031] The advantages and features of the present invention and the methods for achieving them will become clear by referring to the embodiments described below in detail together with the accompanying drawings. However, the present invention is not limited to the embodiments disclosed below but may be implemented in various different forms. Unless otherwise specified in the following description, all numbers, values, and / or expressions representing components, reaction conditions, and the content of components in the present invention should be understood as being modified by the term "approximately" in all cases, as these numbers are approximations reflecting the various uncertainties of measurement that occur in obtaining these values ​​among essentially different things. Furthermore, where a numerical range is disclosed in this description, such range is continuous and, unless otherwise indicated, includes all values ​​from the minimum value of such range to the maximum value including said maximum value. Furthermore, where such range refers to an integer, unless otherwise indicated, it includes all integers including from the minimum value to said maximum value including said maximum value.

[0032] Additionally, when a range is described for a variable in the present invention, it will be understood that the variable includes all values ​​within the described range, including the described endpoints of the range. For example, the range "5 to 10" will be understood to include not only the values ​​5, 6, 7, 8, 9, and 10, but also any sub-ranges such as 6 to 10, 7 to 10, 6 to 9, 7 to 9, etc., and any values ​​between integers valid for the category of the described range, such as 5.5, 6.5, 7.5, 5.5 to 8.5, and 6.5 to 9. For example, the range “10% to 30%” will be understood to include all integers including values ​​such as 10%, 11%, 12%, 13%, etc. and up to 30%, as well as any sub-range such as 10% to 15%, 12% to 18%, 20% to 30%, etc., and any value between valid integers within the stated range category such as 10.5%, 15.5%, 25.5%, etc.

[0034] The present invention first comprises a bottom plate made of ABS sheet material; a side plate made of ABS sheet material positioned vertically at the edge of the bottom plate and fused and bonded with an MC solution; and

[0035] A waterproof plant is provided, comprising a reinforcing bracket made of a triangular ABS plate material fused and bonded with an MC solution, positioned on the inner side of the corner where the bottom plate and the side plate meet, wherein the reinforcing bracket extends to at least 60% of the height of the side plate to prevent the side plate from deforming outward.

[0036] ABS sheet metal strips may be attached to the fused joints of the bottom plate and side plate and the fused joints of the reinforcing bracket.

[0037] In addition, in the present invention, the fusion joint portion of the bottom plate, side plate, and reinforcing bracket is provided with a viscous layer formed from a mixture of MC solution and ABS resin powder, wherein the MC solution and ABS resin powder are mixed in a weight ratio of 3:1 to 5:1, and the viscous layer functions as (i) a first functional layer that assists the fusion joint strength, (ii) a second buffer layer that absorbs microcracks, and (iii) a third interface layer that relieves stress due to differences in thermal expansion, and the viscous layer is formed with a thickness of 0.5 mm to 2.5 mm based on the curing state.

[0038] It is preferable that the above reinforcing bracket be formed with a tapered structure in which the thickness gradually decreases from the bottom to the top, and that the lower thickness of the reinforcing bracket be formed to have a range of 1.3 to 3 times the upper thickness, so as to be configured to preferentially support the stress generated by water pressure and earth pressure at the bottom and distribute it to the top. The above ABS is a copolymer of acrylonitrile, butadiene, and styrene, and the above MC solution is methylene chloride.

[0039] The inner surface of the above waterproof plant is further provided with an antibacterial layer formed on top of a mucus layer, wherein the antibacterial layer is formed of an antibacterial composition comprising an antibacterial particle containing one or more of silver (Ag), copper (Cu), and zinc (Zn), and an acrylic or urethane-based binder, and the antibacterial composition contains 0.1% to 5% by weight of the antibacterial particle and can be formed on top of the mucus layer by coating or spraying.

[0040] In another embodiment of the present invention, a modular waterproofing plant system may be provided in which a plurality of waterproofing plant modules are arranged adjacent to each other, and the joints between the modules are joined in a structure including MC solution fusion, ABS sheet metal strips, and a mucus layer to form a single large waterproofing plant structure.

[0042] Embodiments of the present invention will be described in detail below with reference to the attached drawings.

[0043] FIG. 1 is a cross-sectional view of a waterproofing plant according to one embodiment of the present invention, FIG. 2 is a schematic perspective view of a waterproofing plant according to one embodiment of the present invention, and FIG. 3 is a schematic diagram of a reinforcing bracket installation according to one embodiment of the present invention.

[0044] First, in this invention, T5 ABS panels are used; however, depending on soil and water pressure, N-layer panels or thicker panels such as T7 or T10 may be used, and the use of recycled ABS panels is discouraged. Additionally, MC solution may be used when bonding ABS panels. However, since it evaporates easily at room temperature, caution is required as vapor may remain in the workplace if ventilation is insufficient during storage and use.

[0045] Referring to FIGS. 1 to 3, a waterproof plant according to one embodiment of the present invention includes a bottom plate (10), a side plate (20), and a reinforcing bracket (30).

[0046] The bottom plate (10) is a horizontal structure capable of filling or containing water or soil within the planned plant linearity and must have durability against water pressure or soil pressure according to the planned volume. In the present invention, it is made of an ABS plate with a thickness of 5 mm and forms a horizontal structure capable of containing water or soil. If the floor is uneven or structurally unstable, two or more layers of T5 plates may be overlapped, or a thick plate of T10 or thicker may be used.

[0047] The side plate (20) is positioned vertically at the edge of the bottom plate (10) and fused with MC solution. The side plate (20) may selectively use thicknesses such as T5, T7, T10, etc. to have durability against water pressure or earth pressure according to the planned volume, and if necessary, two or more layers of T5 plate material may be used.

[0048] The reinforcing bracket (30) is reinforced by fixing the side and bottom surfaces together to prevent the side from being pushed outward, thereby providing structural stability and durability to withstand water pressure or earth pressure according to the plant height and volume. An ABS plate of T5 or larger can be cut into a triangular shape and vertically joined to the bottom and side, and the size and thickness of the reinforcing bracket can be adjusted according to the plant height, volume, water pressure, and earth pressure.

[0049] This reinforcing bracket (30) has a triangular shape and is placed on the inner side of the corner where the bottom plate (10) and the side plate (20) meet. The reinforcing bracket (30) is fused to the bottom plate (10) and the side plate (20) with MC solution and extends more than 60% of the height of the side plate (20), preferably 60 to 80%, to prevent the side plate (20) from being pushed outward by water pressure and earth pressure.

[0050] The size and thickness of the reinforcing bracket (30) can be adjusted according to the height and volume of the plant, water pressure, and earth pressure, and generally, ABS plates of T5 or higher are used. In large plants or high-pressure environments, T7 or T10 plates may be used.

[0051] Meanwhile, in the present invention, the reinforcing bracket (30) may be formed with a tapered structure in which the thickness gradually decreases from the bottom to the top. This tapered structure serves to effectively disperse stress caused by water pressure and earth pressure. Specifically, the lower thickness of the reinforcing bracket (130) is formed to have a range of 1.3 to 3 times the upper thickness. For example, if the upper thickness is 5 mm (T5), the lower thickness may be formed in the range of 6.5 mm to 15 mm, and if the upper thickness is 7 mm (T7), the lower thickness may be formed in the range of 9.1 mm to 21 mm. The technical effects of such a tapered structure are as follows. First, the thickness is increased at the bottom where water pressure and earth pressure are highest to preferentially support stress, and the thickness is decreased towards the top to gradually disperse stress. Second, it achieves lightweighting by reducing the use of unnecessary materials while providing a concentrated reinforcement effect to the necessary parts. Third, the thicker part at the bottom increases the fusion bonding area with the floor plate, thereby improving the bonding strength. The tapered structure can be precisely fabricated through CNC machining. The taper can be formed stepwise by cutting ABS sheet metal at a predetermined angle or by laminating sheet metal of different thicknesses. The taper angle is generally set within the range of 3 to 15 degrees and can be adjusted according to the height and volume of the plant. If the lower thickness is less than 1.3 times the upper thickness, the stress-supporting effect of the lower section is insufficient; if it exceeds 3 times, the benefits of lightweighting are reduced and costs increase due to excessive weight gain. Therefore, a range of 1.3 to 3 times is the optimal range that satisfies both structural stability and economic efficiency.

[0052] Meanwhile, the finishing material of FIG. 1 functions as a cap / cover / sealing / protective material covering the cut surface or joint at the top of the side plate. It can serve as a coating or protective layer for the purpose of protecting sharp edges (safety) during use, blocking dust, moisture, and contaminants from entering through the top of the joint, and improving long-term durability (UV / chemicals). The finishing material can be implemented using silicone-based / urethane-based sealants, ABS caps, coating layers, etc. Additionally, the finishing material can reduce exposure of the joint, thereby reducing deterioration and peeling caused by the environment.

[0054] FIG. 4 is a schematic diagram of a corner joint according to one embodiment of the present invention, FIG. 5 is a schematic diagram of a face joint according to one embodiment of the present invention, and FIG. 6 is a schematic diagram of a reinforcing joint during a side joint according to one embodiment of the present invention.

[0055] Referring to FIGS. 4 to 6, the waterproofing plant of the present invention has a special structure at the fusion joint between ABS plates.

[0056] When fusing the bottom plate (10) and the side plate (10), as shown in FIG. 4, the bonding strength is improved by attaching an ABS sheet strip with a width of 10 to 30 mm to the inner side of the joint and fusing them. The MC solution is injected so that it flows from one end of the joint surface to the opposite end, or from top to bottom, to minimize the generation of bubbles.

[0057] After fusion, a viscous layer made by mixing MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 can be applied to the fusion joint. This viscous layer fills in micro-cracks or bubbles that may occur during the fusion process, thereby further enhancing watertightness. When fusion joining side plates (20), an ABS plate strip can be attached and the viscous layer applied in the same manner as shown in FIG. 4.

[0058] Referring to Fig. 5 (see planar joint in Fig. 1), when the floor plate is composed of two or more plates joined together rather than a single plate, the joint can be made on the same plane (horizontal plane). This enables the fabrication of large structures (expansion of width / length) that exceed the plate size limits, and facilitates modular fabrication and improved convenience for transportation and construction. Since the joint is located in the center of the floor, reliability of the joint can be ensured in terms of leakage and strength. The planar joint can be configured to ensure airtightness / watertightness and strength through MC solution fusion, reinforcement strips, or the formation of a viscous layer (mixed viscous layer). Additionally, since the planar joint is prone to microcracks caused by thermal expansion / contraction and repeated loading during long-term use, a viscous layer (cushioning / interface functional layer) can be added.

[0059] Meanwhile, looking at FIG. 6, an additional external reinforcing structure can be added to the outer surface of the reinforcing bracket. It is joined or fastened to the outer side of the side plate of the reinforcing bracket and is configured to reduce the bending moment acting on the joint between the bottom plate and the side plate. In addition, the inner reinforcing bracket (30) and the external reinforcing structure work together to disperse stress concentration at the joint and further reduce the risk of leakage.

[0060] The following describes in detail the multilayer functional structure of the mucus layer in the present invention.

[0061] In another embodiment of the present invention, a mucilage layer formed by mixing an MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 has a multilayer functional structure that goes beyond a simple filler. The mucilage layer acts as the following three functional layers.

[0062] (i) First functional layer: As a functional layer that assists in fusion bond strength, ABS resin powder is partially dissolved by the MC solution and forms a chemical bond at the interface of the fusion bond to improve bond strength. This layer serves to increase the tensile strength and shear strength of the bond.

[0063] (ii) Second buffer layer: As a buffer layer that absorbs microcracks, the mucus layer absorbs microcracks that may occur due to temperature changes, water pressure fluctuations, vibrations, etc., thereby blocking crack propagation. The particles of ABS resin powder form a network structure to disperse crack energy.

[0064] (iii) Third Interface Layer: As an interface layer that relieves stress caused by differences in thermal expansion, the viscous layer relieves interfacial stress resulting from differences in thermal expansion coefficients between different ABS plates, such as bottom plates, side plates, and reinforcing brackets. The appropriate elasticity of the viscous layer absorbs deformation caused by thermal expansion.

[0065] The thickness of the mucus layer (150) is formed in a range of 0.5 mm to 2.5 mm based on the curing process. If the thickness is less than 0.5 mm, the effects of the three functional layers are not sufficiently expressed, and in particular, the micro-crack absorption and stress relief functions are reduced. If the thickness exceeds 2.5 mm, the curing time of the mucus layer becomes excessively long, and shrinkage occurs during the curing process, which may instead create new cracks. Additionally, the strength of the mucus layer itself may be lower than that of the base material, which may become a structural weakness. The optimal thickness of the mucus layer is 1.0 mm to 1.8 mm. In this range, the functions of the first functional layer, the second buffer layer, and the third interface layer are optimally expressed, the curing time is appropriate, and long-term watertightness is maintained most excellently.

[0066] The method for forming such a mucilage layer is as follows. After mixing the MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1, apply the mixture uniformly to the fusion joint using a spatula or a caulking gun. After application, let the mixture stand at room temperature for 30 minutes to 1 hour to flatten the mucilage layer, and then allow an additional curing time of 6 to 8 hours for complete curing. During the curing process, as the MC solution evaporates, the ABS resin powder fuses together to form a robust network structure.

[0068] The following describes a method for manufacturing a waterproofing plant according to the present invention.

[0069] First, the processing and fabrication of ABS sheet metal must be done in advance. For curved sections, cutting can be performed using CNC (Computerized Numerical Control, a method of creating products by controlling machine tools via a computer to cut raw materials) to ensure that the lines and dimensions match those in the CAD drawings. Furthermore, when cutting or shaping the sheet metal, care must be taken to prevent deformation, and a flatbed cutter should be used to ensure accurate dimensions and angles. Additionally, for on-site processing, appropriate tools must be used with caution to prevent safety accidents; tools approved by the site representative or supervisor must be used in the presence of the supervisor. Sharp edges on the cut surfaces should be smoothed using a router or deburring tool to prevent safety accidents, such as lacerations caused by hand scraping.

[0070] Next, in the case of forming, if there is a curved surface, a guide manufactured to match the linear shape and dimensions is attached to the bottom or side surface to join them.

[0071] For the finishing process, planned finishing materials such as interior film, artificial marble, galvanized steel sheets, and wood can be used for the finished surface.

[0072] FIG. 7 is a flowchart of a manufacturing process according to an embodiment of the present invention. Referring to FIG. 7, the manufacturing process of the waterproofing plant of the present invention is as follows.

[0073] (1) Cutting stage: ABS sheet metal is cut according to the CAD drawing. Curved shapes are precisely cut using CNC (Computerized Numerical Control) machining, and straight shapes are cut using a flatbed cutter. Sharp edges on the cut surface are trimmed using a router or deburring tool to prevent accidents.

[0074] (2) Bottom plate and side plate joining step: The edges of the bottom plate and the side plate are fused and joined using MC solution. When joining, an ABS plate strip is attached to the inside, and the MC solution is injected so that it flows from one end of the joint surface to the other. Pressure is applied using a clamp or weight until the fused surface hardens.

[0075] (3) Reinforcement bracket joining step: Place a triangular ABS sheet at the inner corner where the bottom plate and the side plate meet and fuse them together with MC solution. The reinforcement bracket is extended to at least 60% of the height of the side plate, and an ABS sheet strip is attached to the joint.

[0076] (4) Mucus application step: Mix MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 to make a mucus, and apply it sufficiently to all fusion joints. This fills micro-cracks and bubbles to enhance watertightness.

[0077] (5) Finishing step: If necessary, finishing materials such as interior film, artificial marble, galvanized steel plates, and wood are attached to the exterior to improve the appearance.

[0078] (6) Inspection step: After production is complete, fill with water for 1 to 3 days to conduct a leak test and check the waterproof performance.

[0079] In this invention, the design may incorporate the use of non-woven fabric, waterproof sheeting, root barrier sheeting, etc., to protect the paving finishing material of existing facilities before the installation of a waterproofing plant, thereby preventing damage or contamination.

[0080] In addition, before installation, contaminants, foreign substances, and protrusions on the floor surface are removed to eliminate causes that may impair long-term waterproofing performance. When joining all ABS panels and accessories, they must be joined using a fusion method with MC solution; when injecting the MC solution, it should be injected in a flowing manner from one end of the joint surface to the opposite end or from top to bottom to prevent the formation of air bubbles, and pressure must be applied using a hand, a clamp (a device for fixing a workpiece, such as a vise used to secure objects), a weight, or a tool until the fusion surface hardens. When joining floor or side panels, ABS panel strips are attached as shown in the figure below to enhance watertightness and physical stability, such as preventing cracks and deformation, and when joining accessories such as reinforcing brackets, to increase joint strength.

[0081] In particular, to ensure waterproofing performance and durability, and to prevent bubbles or microcracks that may occur in the jointed area formed by injecting MC solution, a viscous solution made by dissolving MC solution and ABS resin powder is sufficiently applied to the area where leakage may occur during the final stage of bonding (fusion) so that the main materials and the main materials, and the main materials and the components, can be tightly fused together.

[0082] Embodiments of the present invention are described below.

[0083] The waterproof plant according to the present invention can be manufactured in various sizes depending on the application and installation environment.

[0084] (Example 1: Plate thickness and reinforcing bracket usage by specification)

[0085] Height (mm) Length (mm) Width (mm) Floor plate thickness Side panel thickness Reinforcement bracket height 300 1000 500 T5 T5 180 500 2000 1000 T5 T7 300 700 3000 1500 T7 T10 420 1000 5000 2000 T10 T5 × 2 layers 600

[0086] In Table 1 above, the height of the reinforcing bracket is set to approximately 60% of the height of the side plate, and can be extended up to 70-80% as needed.

[0087] (Example 2: Application of antimicrobial layer)

[0088] In an embodiment of the present invention, a separate antimicrobial layer may be additionally formed on the inner surface of a waterproof plant on top of a mucus layer. The antimicrobial layer serves to maintain a hygienic environment by inhibiting the proliferation of microorganisms such as bacteria, fungi, and algae that may occur in a plant cultivation environment. The antimicrobial layer is formed from an antimicrobial composition comprising an antimicrobial particle containing one or more of silver (Ag), copper (Cu), and zinc (Zn), and an acrylic or urethane-based binder. The antimicrobial particle is used in the form of a nano-sized particle (10 to 500 nm), maximizing the surface area to enhance the antimicrobial effect.

[0089] The antimicrobial composition contains 0.1% to 5% by weight of antimicrobial particles. If the antimicrobial particle content is less than 0.1% by weight, the antimicrobial effect is insufficient, and if it exceeds 5% by weight, aggregation of the antimicrobial particles occurs, which actually reduces the antimicrobial effect and causes the cost to increase excessively. The optimal content is 0.5% to 2% by weight.

[0090] Acrylic binders have excellent adhesion and water resistance, while urethane binders have excellent elasticity and durability. The two binders can be used individually or mixed, and when mixed, the weight ratio of acrylic to urethane is preferably in the range of 7:3 to 3:7.

[0091] The method of forming the antimicrobial layer is carried out by application or spraying. After the mucus layer is completely cured, the antimicrobial composition is applied with a brush or roller, or sprayed using a spray gun. The application thickness is 20 to 100 µm, and if necessary, the antimicrobial layer is formed by applying it 2 to 3 times in layers.

[0092] The antibacterial effect of the antibacterial layer was evaluated by an antibacterial test according to the KS M 0146 standard. As a result of measuring the number of viable bacteria after 24 hours of incubation with Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus), the application of the antibacterial layer showed an antibacterial effect of over 99%.

[0093] The antimicrobial layer can be applied not only to waterproof plants for plant cultivation but also to various applications where microbial proliferation is a concern, such as hydroponic systems, fish farms, and vivariums. In particular, it is effective in maintaining a clean environment and extending maintenance cycles by inhibiting the growth of algae and bacteria in structures that retain water for extended periods.

[0094] (Example 3: Modular Waterproofing Plant)

[0095] In a specific embodiment of the present invention, a modular system can be implemented in which a plurality of waterproof plant modules are arranged adjacent to each other to form a single large waterproof plant structure.

[0096] Each waterproofing plant module is manufactured as an independent structure including a bottom plate (10), a side plate (20), and a reinforcing bracket (30), as described in Example 1. Multiple modules are arranged adjacently at the installation site, and the joints between the modules are joined using a structure including MC solution fusion, ABS plate strips, and a viscous layer to ensure watertightness and structural stability equivalent to a single waterproofing plant.

[0097] The technical advantages of the modular system are as follows. First, transportation and installation are facilitated by manufacturing standard-sized modules and assembling them on-site, rather than requiring the entire large-scale waterproofing plant to be fabricated in a factory. Second, standardizing module sizes enables mass production, and design flexibility is high as the number and placement of modules can be adjusted to suit the spatial conditions of the installation site. Third, maintenance is convenient as only the damaged modules can be replaced.

[0098] The method of joining modules is as follows. First, the side plates (20) of two adjacent modules are placed together. Second, ABS sheet metal strips with a width of 20 to 40 mm are placed on the inner and outer sides of the joint and fused with MC solution. Third, a liquid mixture of MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 is applied to the joint to ensure watertightness. Fourth, a reinforcing bracket (30) can be additionally installed at the joint to improve structural strength.

[0099] As a specific embodiment of the modular system, a large waterproof plant measuring 2000mm in width × 2000mm in length × 500mm in height can be constructed by connecting four standard modules of 1000mm in width × 1000mm in length × 500mm in height in a 2×2 array. Each module is manufactured from T7 ABS sheet metal, and T5 ABS strips and a viscous layer with a weight ratio of 3:1 are applied to the joints between modules.

[0100] As a result of conducting a long-term leak test to evaluate the watertightness of the joints between modules, the modular system demonstrated a level of watertightness equivalent to that of a single-structure waterproofing plant. No leakage occurred under conditions of a water depth of 500 mm for 90 days, and no deformation of the joints was observed.

[0101] The modular system is particularly useful when installing large waterproof plants with a length of 5m or more in large spaces such as shopping malls, office lobbies, and public buildings. In addition, when implementing large curved plants, a natural curved structure can be formed by arranging and connecting each module at a fine angle.

[0102] (Example 4: Evaluation of waterproof performance)

[0103] To evaluate the waterproofing performance of the waterproofing plant according to the present invention, the following tests were conducted.

[0104] Test items Test conditions Evaluation period result Initial leak test Depth 300mm, Room temperature 3 days No leaks Long-term leak test Depth 500mm, Room temperature 30 days No leaks High pressure test Depth 700mm, Room temperature 7 days No leaks Temperature change test Repeat at 10–40℃, depth 300mm 14th No cracks or leaks Earth pressure test Soil filling, height 500mm 30 days No deformation or leakage

[0105] As shown in Table 2 above, the waterproofing plant according to the present invention exhibited excellent waterproofing performance and structural stability under various conditions.

[0106] (Example 5: Optimization of Mixed Mucus of MC Solution and ABS Resin Powder)

[0107] In this invention, the physical properties and watertightness performance of the mucus were evaluated according to the mixing ratio of the MC solution and the ABS resin powder.

[0108] A mucus was prepared by mixing an MC solution (methylene chloride, purity 99.5% or higher) and ABS resin powder (particle size 50–200 µm) in various weight ratios. The specific manufacturing process is as follows:

[0109] (1) Measure the MC solution into a clean glass beaker.

[0110] (2) ABS resin powder is prepared by weighing it in a predetermined weight ratio.

[0111] (3) Slowly add ABS resin powder to the MC solution and stir uniformly with a glass rod for 3 to 5 minutes.

[0112] (4) Let stand at room temperature (20~25℃) for 10 minutes to remove bubbles.

[0113] (5) Once the viscosity of the mucus is uniformly formed, use it for application immediately.

[0114] The viscosity, curing time, and applicability of mucilages prepared with different mixing ratios of MC solution and ABS resin powder were evaluated. Viscosity was measured using a Brookfield viscometer (Spindle No. 3, 20 rpm), and curing time was measured as surface drying time and complete curing time. Applicability was evaluated on a 5-point scale regarding the ease of application by an operator using a spatula.

[0115] Table 3 below shows the properties of the mucus according to the mixing ratio of MC solution and ABS resin powder.

[0116] Mixing ratio (MC: ABS powder) Viscosity (cps) Surface drying time (minutes) Complete curing time (time) Coatability (5-point scale) note 1:1 12,500 8 3 2 Excessively high viscosity 2:1 7,800 12 4 3 Viscosity is somewhat high 3:1 4,200 15 5 5 optimal 4:1 2,800 18 6 5 Good 5:1 1,900 22 7 4 Good 6:1 1,200 28 8 3 Viscosity is somewhat low 7:1 850 35 10 2 Viscosity is excessively low

[0117] As shown in Table 3, when the weight ratio of MC solution to ABS resin powder was 3:1 to 5:1, the viscosity was appropriately formed in the range of 1,900 to 4,200 cps, resulting in excellent coating performance. At a mixing ratio of 1:1 to 2:1, the viscosity was excessively high, making it difficult to apply uniformly, and at a mixing ratio of 6:1 or higher, the viscosity was low, causing the problem of the solution flowing down at the joint.

[0118] To evaluate the bonding strength according to the mixing ratio of MC solution and ABS resin powder, T5 ABS plates were fusion-bonded with MC solution, then the solution of each mixing ratio was applied and cured for 7 days, after which a tensile shear test was performed. The test specimens were prepared according to the KS M 3734 standard, and the breaking strength was measured using a universal testing machine (UTM) under a tensile speed of 5 mm / min.

[0119] Table 4 below shows the bonding strength according to the mixing ratio of MC solution and ABS resin powder.

[0120] Mixing ratio (MC: ABS powder) Average bond strength (MPa) Standard deviation (MPa) fracture shape Mucus not applied 18.5 2.3 Joint interface fracture 1:1 22.3 1.8 Joint interface fracture 2:1 25.7 1.5 Joint interface fracture 3:1 28.9 1.2 Base material fracture 4:1 27.8 1.4 Base material fracture 5:1 26.2 1.6 Base material fracture 6:1 23.1 2.1 Joint interface fracture 7:1 20.4 2.5 Joint interface fracture

[0121] As shown in Table 4, when a mixture of MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 was applied, the bonding strength was excellent at 26.2 to 28.9 MPa, and it was confirmed that the strength of the bond was equal to or greater than the strength of the base material, as fracture occurred in the base material rather than the bond. When no mixture was applied, the bonding strength was low at 18.5 MPa, and when the mixing ratio fell outside the range of 3:1 to 5:1, the bonding strength decreased and fracture occurred at the interface of the bond.

[0122] Meanwhile, Table 5 shows the watertightness evaluation according to the mixing ratio of MC solution and ABS resin powder.

[0123] To evaluate watertightness according to the mixing ratio of MC solution and ABS resin powder, a small waterproof plant (300mm wide × 300mm long × 300mm high) was fabricated using T5 ABS sheet metal, and a long-term leakage test was conducted after applying the liquid of each mixing ratio.

[0124] Mixing ratio (MC: ABS powder) 7 days have passed 30 days have passed 60 days have passed 90 days elapsed Mucus not applied Micro leak Leakage occurred Worsening leak Joint separation 1:1 Good Good microcracks Micro leak 2:1 Good Good Good Good 3:1 excellence excellence excellence excellence 4:1 excellence excellence excellence excellence 5:1 excellence excellence Good Good 6:1 Good Good Micro leak Leakage occurred 7:1 Micro leak Leakage occurred Worsening leak Joint separation

[0125] As shown in Table 5, when a mixture of MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 was applied, excellent watertightness was maintained even after 90 days. In particular, the best long-term watertightness was observed at mixing ratios of 3:1 and 4:1. When no mixture was applied, micro-leakage occurred starting from the 7th day, and when the mixing ratio was 6:1 or higher, long-term watertightness was reduced because the viscosity of the mixture was low and insufficient filling was not achieved.

[0126] When the results of Examples 8-2, 8-3, and 8-4 above are combined, the viscosity, coating properties, bonding strength, and water tightness were all excellent when the MC solution and ABS resin powder were mixed in a weight ratio of 3:1 to 5:1. In particular, the best performance was observed at a weight ratio of 3:1, and sufficient performance for practical use could also be secured at mixing ratios of 4:1 and 5:1. Therefore, the present invention is characterized by mixing the MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1, and more preferably, mixing in a weight ratio of 3:1 to 4:1 is optimal.

[0128] Meanwhile, in the present invention, a waterproof plant was manufactured by fusing ABS sheet metal only with MC solution and omitting the ABS strip attachment and mucus coating, and its performance was evaluated.

[0129] Table 5 below shows the waterproof performance evaluation for such comparative examples.

[0130] Test items Test conditions Evaluation period result Initial leak test Depth 300mm, Room temperature 3 days Minor leak occurred Long-term leak test Depth 500mm, Room temperature 30 days Joint cracks, worsening leakage Temperature change test Repeat at 10–40℃, depth 300mm 14th Joint separation, leakage

[0131] In Comparative Example 1, the absence of ABS strips and a viscous layer resulted in microcracks in the fusion joint and exacerbated leakage during long-term use. This demonstrates that strips and a viscous layer play an important role in ensuring watertightness.

[0132] The following Comparative Example 2 shows the deformation evaluation in a state without reinforcing brackets.

[0133] A waterproof plant consisting only of a floor plate and side plates, without installing reinforcing brackets, was fabricated and its performance evaluated.

[0134] Height (mm) Water depth (mm) Evaluation period Lateral deformation (mm) 300 300 7 days 2.5 500 500 7 days 8.3 700 700 7 days 15.7

[0135] In Comparative Example 2, it was found that the side plate deformed outward due to water pressure because there was no reinforcing bracket. In particular, the amount of deformation increased rapidly as the height increased, and there is a concern about separation of the joint and leakage during long-term use.

[0136] The waterproof plant according to the present invention can be utilized in various fields such as indoor and outdoor landscaping, terrariums, vivariums, paludariums, hydroponics, and fish farms. In particular, it can be applied as a planting plant that is lightweight yet has excellent waterproof performance in indoor spaces such as shopping malls, offices, and public buildings, and improves the aesthetics of the space through various shapes and finishing materials.

[0137] A person skilled in the art to which the present invention pertains will understand that the present invention may be implemented in other specific forms without altering its technical concept or essential features. Therefore, the embodiments described above should be understood as illustrative in all respects and not restrictive. The scope of the present invention is defined by the claims set forth below rather than by the detailed description above, and all modifications or variations derived from the meaning and scope of the claims and equivalent concepts should be interpreted as being included within the scope of the present invention.

Claims

Claim 1 A bottom plate made of ABS sheet material; a side plate made of ABS sheet material positioned vertically at the edge of the bottom plate and fused and bonded with an MC solution; and a reinforcing bracket made of a triangular ABS plate fused with an MC solution, disposed on the inner side of the corner where the bottom plate and the side plate meet; wherein the reinforcing bracket extends to at least 60% of the height of the side plate to prevent the side plate from deforming outward, and an ABS plate strip is attached to the fused joint of the bottom plate and the side plate and the fused joint of the reinforcing bracket, and a viscous layer formed of a mixed viscous mixture of MC solution and ABS resin powder is provided at the fused joint of the bottom plate, the side plate, and the reinforcing bracket, wherein the MC solution and the ABS resin powder are mixed in a weight ratio of 3:1 to 5:1, and the viscous layer functions as (i) a first functional layer that assists in fusion bonding strength, (ii) a second buffering layer that absorbs microcracks, and (iii) a third interface layer that relieves stress due to differences in thermal expansion, and the viscous layer is formed with a thickness of 0.5mm to 2.5mm based on the curing state. A waterproofing plant characterized by a fusion joint with a formed mucus layer, wherein fracture occurs in the base material rather than at the joint interface in a tensile shear test according to KS M 3734. Claim 2 delete Claim 3 delete Claim 4 A waterproofing plant according to claim 1, wherein the reinforcing bracket is formed with a tapered structure in which the thickness gradually decreases from the bottom to the top, and the lower thickness of the reinforcing bracket is formed to have a range of 1.3 to 3 times the upper thickness, and configured to preferentially support stress generated by water pressure and earth pressure from the bottom and distribute it to the top. Claim 5 delete Claim 6 A waterproofing plant according to claim 1, wherein the inner surface of the waterproofing plant further comprises an antibacterial layer formed on top of a mucus layer, wherein the antibacterial layer is formed from an antibacterial composition comprising an antibacterial particle containing one or more of silver (Ag), copper (Cu), and zinc (Zn) and an acrylic or urethane-based binder, wherein the antibacterial composition contains 0.1% to 5% by weight of the antibacterial particle and is formed on top of the mucus layer by a coating or spraying method. Claim 7 delete Claim 8 (a) a step of cutting an ABS sheet to form a bottom plate and a side plate; (b) a step of fusing the edge of the bottom plate and the side plate with an MC solution, wherein an ABS sheet strip is attached to the joint and fused; (c) a step of fusing a triangular-shaped ABS sheet to the inner side of the corner where the bottom plate and the side plate meet with an MC solution to form a reinforcing bracket, wherein an ABS sheet strip is attached to the joint and fused; and (d) forming a viscous layer by mixing an MC solution and ABS resin powder in a weight ratio of 3:1 to 5:1 on all of the above-mentioned fusion joints to a thickness of 0.5 mm to 2.5 mm after curing, wherein the viscous layer is formed to function as (i) a first functional layer that assists in fusion joint strength, (ii) a second buffer layer that absorbs microcracks, and (iii) a third interface layer that relieves stress due to differences in thermal expansion; wherein the reinforcing bracket is formed to extend up to 60% or more of the height of the side plate, a method for manufacturing a waterproofing plant. Claim 9 delete Claim 10 delete Claim 11 delete Claim 12 A method for manufacturing a waterproofing plant according to claim 8, wherein the inner surface of the waterproofing plant further comprises an antibacterial layer formed on top of a mucus layer, wherein the antibacterial layer is formed from an antibacterial composition comprising an antibacterial particle containing one or more of silver (Ag), copper (Cu), and zinc (Zn) and an acrylic or urethane-based binder, wherein the antibacterial composition contains 0.1% to 5% by weight of the antibacterial particle, and further comprises the step of forming the antibacterial layer on top of the mucus layer by coating or spraying.

Citation Information

Patent Citations

  • Planter for growing plants

    JP6724714B2

  • Reinforced vacuum forming products and forming methodthereof

    KR1020040101963A

  • Ag-Cu-CyD Antimicrobial

    KR1020120010340A

  • Underpinning case for flowerbed and plant pot

    KR200306740Y1