Method of checking defect of lithium ion secondary battery and lithium ion secondary battery manufactured by the same method

The pressurized aging process improves defect sorting in lithium-ion secondary batteries by applying pressure to identify internal micro-short defects, addressing the inadequacies of conventional methods and enhancing defect detection efficiency.

KR103044740B1Active Publication Date: 2026-11-06HYUNDAI MOTOR CO LTD +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
KR1020190154790
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2019-11-27
Publication Date
2026-11-06
Estimated Expiration
2039-11-27

AI Technical Summary

Technical Problem

Existing methods for sorting internal micro-short defects in lithium-ion secondary batteries during the aging process are inadequate, leading to frequent occurrences of cells with unusually reduced Open Circuit Voltage (OCV) and increased process time, necessitating improved defect sorting capability.

Method used

A method involving a pressurized aging process with applied pressure greater than 0.2 to 5 kg/cm² and elevated temperature (45 to 60 degrees) to identify defects by measuring OCV and IR before and after applying pressure, and comparing these values to detect deviations from a preset normal range.

Benefits of technology

Enhances the ability to identify internal micro-short defects caused by high-resistance protruding or growing particles, reduces aging time, and improves overall product quality by minimizing defective products in the market.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112019122575455-PAT00001_ABST
    Figure 112019122575455-PAT00001_ABST
Patent Text Reader

Abstract

A method for sorting defects in a lithium-ion secondary battery according to the present invention is a method for sorting internal micro-short defects in a lithium-ion secondary battery during an aging process in a manufacturing process of a lithium-ion secondary battery, and may include: a step of performing a first charge and degassing after manufacturing the lithium-ion secondary battery; a step of measuring one or more of the Open Circuit Voltage (OCV) and Internal Resistance (IR) of the lithium-ion secondary battery cell after a second charge and discharge of the lithium-ion secondary battery; a pressurized aging step of aging the lithium-ion secondary battery while applying pressure greater than a certain amount; and a defect sorting step of sorting defects in the lithium-ion secondary battery by re-measuring one or more of the OCV and IR of the lithium-ion secondary battery cell and comparing the result with the previously measured OCV and IR.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to a method for sorting defects in a lithium-ion secondary battery and a lithium-ion secondary battery manufactured thereby. More specifically, the invention relates to a method for sorting defects in a lithium-ion secondary battery capable of improving the sorting capability for internal micro-short defects in a lithium-ion secondary battery during the aging process in the manufacturing process of a lithium-ion secondary battery, and a lithium-ion secondary battery manufactured thereby. Background Technology

[0003] Recently, there has been an urgent demand to reduce carbon dioxide emissions in order to address air pollution and global warming. The automotive industry is focusing its expectations on reducing carbon dioxide emissions through the introduction of electric vehicles and hybrid electric vehicles, and active development is underway for lithium-ion rechargeable batteries for motor drives, which hold the key to their practical application.

[0004] Meanwhile, the sorting of internal short-circuit defects in lithium-ion secondary batteries is carried out during the formation process of lithium-ion secondary batteries. Generally, defects are sorted based on the Open Circuit Voltage (OCV) or Internal Resistance (IR) after charging and discharging following secondary battery manufacturing, the Open Circuit Voltage or Internal Resistance after aging, the difference between the Open Circuit Voltage or Internal Resistance before and after aging, or the fluctuation amount of OCV per unit of aging time. At this time, to increase the defect sorting capability of secondary batteries, methods such as increasing the aging time or temperature, or adding a separate process of repeating charging and discharging during the formation process have been used.

[0005] However, despite research and development aimed at minimizing leakage defects by strengthening conditions for defect sorting, problems such as cells with unusually reduced OCV are frequently occurring in the actual market. Accordingly, there is a need to develop technology that can improve the defect sorting capability of secondary batteries. Prior art literature

[0007] KR 10-1471775 The problem to be solved

[0008] The present invention, proposed to solve the aforementioned problems, aims to provide a method for sorting defects in a lithium-ion secondary battery and a lithium-ion secondary battery manufactured through the same, which can improve the sorting capability for internal micro-short defects in a lithium-ion secondary battery by applying pressure greater than a certain amount to the lithium-ion secondary battery during the aging process in the manufacturing process of the lithium secondary battery. means of solving the problem

[0010] A method for sorting defects in a lithium-ion secondary battery according to the present invention for achieving the above-described purpose is a method for sorting internal micro-short defects in a lithium-ion secondary battery during an aging process in a manufacturing process of a lithium-ion secondary battery, and may include: a step of performing a first charge and degassing after manufacturing the lithium-ion secondary battery; a step of measuring one or more of the Open Circuit Voltage (OCV) and Internal Resistance (IR) of the lithium-ion secondary battery cell after a second charge and discharge of the lithium-ion secondary battery; a pressurized aging step of aging the lithium-ion secondary battery while applying pressure greater than a certain amount; and a defect sorting step of sorting defects in the lithium-ion secondary battery by re-measuring one or more of the OCV and IR of the lithium-ion secondary battery cell and comparing the result with the previously measured OCV and IR.

[0011] In the above pressurized aging step,

[0012] The pressure applied to the above lithium-ion secondary battery is 0.2 to 5 kg / cm² 2 It could be.

[0013] In the above pressurized aging step, the temperature can be raised to 45 to 60 degrees.

[0014] In the above pressurized aging step,

[0015] The lithium-ion secondary battery can be pressurized by placing it between pressure plates spaced apart by a certain distance and then moving each pressure plate in a direction facing each other.

[0016] In the above pressurized aging step,

[0017] After accommodating the lithium-ion secondary battery in a pressure chamber, the lithium-ion secondary battery can be pressurized by increasing the pressure of the gas in the pressure chamber.

[0018] In the above defective sorting step,

[0019] If the difference between the OCV of a lithium-ion secondary battery cell measured before the pressurized aging step and the OCV of a lithium-ion secondary battery cell re-measured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0020] In the above defective sorting step,

[0021] If the difference between the IR of a lithium-ion secondary battery cell measured before the pressurized aging step and the IR of a lithium-ion secondary battery cell re-measured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0022] After the second charge and discharge of the lithium-ion secondary battery, the method may further include the step of measuring one or more of the Open Circuit Voltage (OCV) and Internal Resistance (IR) of the lithium-ion secondary battery cell, and then the step of re-measuring one or more of the OCV and IR of the lithium-ion secondary battery cell while applying a certain pressure to the lithium-ion secondary battery; the step of deriving a variation amount of one or more of the OCV and IR based on one or more of the previously measured values ​​of the OCV and IR and one or more of the re-measured values ​​of the OCV and IR; and the step of identifying defects in the lithium-ion secondary battery cell based on the derived variation amount.

[0023] Prior to the secondary charging and discharging of the above lithium-ion secondary battery,

[0024] The method may further include the step of pressurizing the lithium-ion secondary battery to a pressure greater than a certain size.

[0025] In the step of screening defects in the lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR,

[0026] If the difference between the variation amount of the OCV derived above and the variation amount of the preset OCV deviates from the preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0027] In the step of screening defects in the lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR,

[0028] If the difference between the variation amount of the IR derived above and the preset variation amount of the IR deviates from the preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0029] In the step of screening defects in the lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR,

[0030] If the difference between the variation amount of the derived OCV and IR and the preset variation amount of the OCV and IR deviates from the preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0031] In the above defective sorting step,

[0032] If the OCV and IR of the lithium-ion secondary battery cell measured after the second charge and discharge of the lithium-ion secondary battery deviate from the preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0033] A lithium-ion secondary battery manufactured by a method for sorting defective lithium-ion secondary batteries. Effects of the invention

[0035] According to the present invention, the ability to select short defects by particles that come into contact between the positive and negative electrodes only when pressure is applied can be improved.

[0036] In addition, the ability to sort out short defects can be improved by high-resistance protruding particles or growing particles.

[0037] In addition, by shortening the aging period, process costs can be reduced, and overall product quality can be improved by minimizing the leakage of defective products into the market. Brief explanation of the drawing

[0039] FIG. 1 is a flowchart of a method for sorting defective lithium-ion secondary batteries according to an embodiment of the present invention. FIG. 2 is a drawing showing the appearance of pressurized aging in a method for sorting defective lithium-ion secondary batteries according to an embodiment of the present invention. FIG. 3 is a diagram showing the appearance of pressurized aging in a method for sorting defective lithium-ion secondary batteries according to another embodiment of the present invention. FIG. 4 is a flowchart of a method for sorting defective lithium-ion secondary batteries according to another embodiment of the present invention. Specific details for implementing the invention

[0040] Hereinafter, the present invention will be described in detail with reference to the drawings. Terms and words used in this specification and claims shall not be interpreted as being limited to their ordinary or dictionary meanings, but shall be interpreted in a meaning and concept consistent with the technical spirit of the present invention, based on the principle that the inventor may appropriately define the concept of the terms to best describe his invention.

[0041] Therefore, the embodiments described in this specification and the configurations described in the drawings are merely the most preferred embodiments of the present invention and do not represent all of the technical ideas of the present invention; thus, it should be understood that various equivalent modifications that can replace them may exist at the time of filing this application.

[0042] FIG. 1 is a flowchart of a method for sorting defects in a lithium-ion secondary battery according to an embodiment of the present invention. The present invention is a method for sorting internal micro-short defects in a lithium-ion secondary battery during an aging process in a manufacturing process of a lithium-ion secondary battery, and as shown in FIG. 1, it may include a step (S100) of performing primary charging and degassing after manufacturing a lithium-ion secondary battery, a step (S200) of measuring one or more of OCV (Open Circuit Voltage) and IR (Internal Resistance) of a lithium-ion secondary battery cell after secondary charging and discharging of the lithium-ion secondary battery, a pressurized aging step (S300) of aging while applying pressure greater than a certain amount to the lithium-ion secondary battery, and a defect sorting step (S400) of sorting defects in the lithium-ion secondary battery by re-measuring one or more of OCV and IR of the lithium-ion secondary battery cell and comparing them with the previously measured OCV and IR.

[0043] Specifically, in the step (S100) of performing primary charging and degassing after manufacturing a lithium-ion secondary battery, an initial charge, which is the first charge of the manufactured lithium-ion secondary battery, may be performed. At this time, during the initial charge, the battery may be charged up to a preset State of Charge (SOC). According to an embodiment, the initial charge may be performed up to 30% of the SOC, but this is merely an example, and the SOC can be set to a different value.

[0044] In addition, in the step (S100) of performing primary charging and degassing, degassing can be performed to remove the gas generated as gas is generated in the lithium-ion secondary battery during primary charging.

[0045] In the step (S200) of measuring one or more of the OCV and IR of the lithium-ion secondary battery cell after the secondary charge and discharge of the lithium-ion secondary battery, the charging capacity can be measured after charging the lithium-ion secondary battery to SOC 100% after degassing, and the discharge capacity can be measured after discharging the lithium-ion secondary battery to SOC 0% after confirming the charging capacity. In addition, after measuring the discharge capacity, at least one of the OCV and IR of the lithium-ion secondary battery can be measured after meeting preset aging conditions.

[0046] In other words, in step S200, after matching the preset aging conditions, the OCV of the lithium-ion secondary battery cell or the IR value of the lithium-ion secondary battery cell can be measured according to the embodiment, and the values ​​of the OCV and IR of the lithium-ion secondary battery cell can be measured according to another embodiment.

[0047] In the pressurized aging step (S300) in which aging is performed while applying pressure greater than a certain amount to the lithium-ion secondary battery, pressure greater than a certain amount may be applied to the lithium-ion secondary battery. Here, the pressure applied to the lithium-ion secondary battery is 0.2 to 5 kg / cm² 2It is desirable that the temperature of the lithium-ion secondary battery be raised to 40 to 60 degrees during the pressurized aging step (S300).

[0048] Specifically, referring to FIG. 2, according to an embodiment, in the pressurized aging step (S300), the lithium-ion secondary battery can be pressurized by placing it between pressure plates (200) spaced apart at a certain distance and then moving each pressure plate in a direction facing each other. Although not illustrated in detail in the drawings, according to an embodiment, the pressure plates are driven by a cylinder or a motor, etc., to a pressure of 0.2 to 5 kg / cm² 2 The pressure can be applied to the lithium-ion secondary battery.

[0049] Additionally, referring to FIG. 3, according to another embodiment, in the pressurized aging step (S300), the lithium-ion secondary battery can be pressurized by receiving the lithium-ion secondary battery in the pressure chamber (300) and then increasing the pressure of the gas in the pressure chamber.

[0050] However, the lithium-ion secondary battery pressurization method illustrated in FIGS. 2 and FIGS. 3 is merely one example, and various other pressurization methods may be used in the present invention as long as a preset pressure can be applied to the lithium-ion secondary battery during the aging process.

[0051] Depending on the pressurization method, it may be possible to pressurize the cell before or after the second charge / discharge. In such cases, it is possible to induce defects in potential defective cells to increase defect sorting ability in subsequent processes, as well as minimize the gap between the separator and the electrode and minimize bending or wrinkling of the electrode to minimize thickness variation of the cell and improve cell characteristics by inducing a uniform reaction of the electrode.

[0052] According to the embodiment, in the defect screening step (S400) for screening defects in a lithium-ion secondary battery by re-measuring one or more of the OCV and IR of a lithium-ion secondary battery cell and comparing them with the previously measured OCV and IR, if the difference between the OCV of the lithium-ion secondary battery cell measured before the pressurized aging step and the OCV of the lithium-ion secondary battery cell re-measured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0053] According to another embodiment, in a defect screening step (S400) in which one or more of the OCV and IR of a lithium-ion secondary battery cell are remeasured and compared with the previously measured OCV and IR to screen for defects in the lithium-ion secondary battery, if the difference between the IR of the lithium-ion secondary battery cell measured before the pressurized aging step and the IR of the lithium-ion secondary battery cell remeasured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0054] According to another embodiment, in a defect screening step (S400) in which one or more of the OCV and IR of a lithium-ion secondary battery cell are remeasured and compared with the previously measured OCV and IR to screen for defects in the lithium-ion secondary battery, if the difference between the OCV and IR of the lithium-ion secondary battery cell measured before the pressurized aging step and the OCV and IR of the lithium-ion secondary battery cell remeasured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0055] In other words, in the defect screening step (S400) for screening defects in a lithium-ion secondary battery by re-measuring one or more of the OCV and IR of a lithium-ion secondary battery cell and comparing them with the previously measured OCV and IR, the difference between the values ​​of the OCV and IR of the lithium-ion secondary battery cell measured in S200 and the values ​​of the OCV and IR of the lithium-ion secondary battery cell measured in step S400 is calculated, and if the calculated value deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0056] FIG. 4 is a flowchart of a method for sorting defects in a lithium-ion secondary battery according to another embodiment of the present invention. Referring to FIG. 4, the method for sorting defects in a lithium-ion secondary battery according to another embodiment of the present invention may further include, after the step (S200) of measuring one or more of the Open Circuit Voltage (OCV) and Internal Resistance (IR) of a lithium-ion secondary battery cell after secondary charging and discharging of the lithium-ion secondary battery, a step (S500) of re-measuring one or more of the OCV and IR of a lithium-ion secondary battery cell while applying a certain pressure to the lithium-ion secondary battery, a step (S600) of deriving a variation amount of one or more of the OCV and IR based on one or more of the previously measured values ​​of OCV and IR and one or more of the re-measured values ​​of OCV and IR, and a step (S700) of sorting defects in the lithium-ion secondary battery cell based on the derived variation amount.

[0057] Specifically, in the step (S700) of screening for defects in a lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR, according to the embodiment, if the difference between the variation of the derived OCV and the preset variation of the OCV deviates from a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0058] In addition, in the step (S700) of screening for defects in a lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR, according to another embodiment, if the difference between the variation of the derived IR and the variation of the preset IR deviates from the preset normal range, the lithium-ion secondary battery cell may be determined to be defective.

[0059] In addition, in the step (S700) of selecting defects in a lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR, according to another embodiment, if the difference between the variation of the derived OCV and IR and the preset variation of OCV and IR deviates from a preset normal range, the lithium-ion secondary battery cell may be determined to be defective.

[0060] In other words, in the step (S700) of screening for defects in a lithium-ion secondary battery cell based on one or more variations in OCV and IR derived, if the variation in one or more of the OCV and IR derived in step S600 based on the values ​​of OCV and IR of the lithium-ion secondary battery cell measured in step S200 and the values ​​of OCV and IR of the lithium-ion secondary battery cell re-measured in step S500 deviates from the variation amount of a preset normal range, the lithium-ion secondary battery cell can be determined to be defective.

[0061] Meanwhile, the reason for performing aging under pressure on the lithium-ion secondary battery during the aging process in the present invention is as follows.

[0062] Conventionally, aging was performed during the manufacturing process of lithium-ion secondary batteries to stabilize cell performance by stabilizing the film of the lithium-ion secondary battery and to identify defective cells based on measured OCV and IR. However, conventional aging processes had limitations in that they could not identify internal short circuit defects caused by high-resistance protruding particles or internal short circuit defects caused by growing particles that grow over time, and there was a limitation in that the aging process time had to be increased to detect these defects.

[0063] To solve the aforementioned problems, the present invention performs aging while applying pressure greater than a certain amount to the lithium-ion secondary battery during the aging process, thereby selecting internal short-circuit defects caused by high-resistance protruding particles or internal short-circuit defects caused by growth-type particles that grow over time, thereby improving the defect selection capability of the lithium-ion secondary battery and simultaneously shortening the aging time.

[0064] Specifically, in the case of high-resistance protruding particles, when a certain amount of pressure is applied to a lithium-ion secondary battery, the contact resistance decreases, so a short circuit can occur in a shorter time, and accordingly, fluctuations in OCV can occur rapidly, and as a result, short circuit defects can be detected during a shorter aging process.

[0065] In addition, in the case of growth particles located between the positive and negative electrodes, as time passes, the particles grow and connect the positive and negative electrodes, causing a short circuit. However, when a certain amount of pressure is applied to the lithium-ion secondary battery as in the present invention, the distance between the positive and negative electrodes decreases, so a short circuit between the positive and negative electrodes can occur due to the growth particles even when the growth particles have not grown sufficiently, and accordingly, short circuit defects can be selected during a shorter aging process.

[0066] Furthermore, although it was difficult to sort out defects caused by particles that come into contact between the anode and cathode only when pressure is applied through a conventional non-pressure aging process, according to the present invention, the ability to sort out defects caused by particles that come into contact between the anode and cathode only when pressure is applied can be enhanced.

[0067] In addition, by applying pressure exceeding a certain amount to the lithium-ion secondary battery, in the case of a lithium-ion secondary battery in which the bonding or physical bonding (tab welding defect, substrate crack, tab crack) of internal components is abnormal, the state of the bonding part changes, and based on said change, the defect sorting capability can be improved compared to conventional methods.

[0068] Meanwhile, the lithium-ion secondary battery manufactured by the defect sorting method for lithium-ion secondary batteries according to the present invention is manufactured through improved defect sorting capability, thereby improving cell stability and overall marketability. Explanation of the symbols

[0070] 100: Lithium-ion rechargeable battery 200: Pressure plate 300: Pressure chamber

Claims

Claim 1 A method for screening internal micro-short defects of a lithium-ion secondary battery during an aging process in a manufacturing process of a lithium-ion secondary battery, comprising: a step of performing a first charge and degassing after manufacturing the lithium-ion secondary battery; a step of measuring one or more of the Open Circuit Voltage (OCV) and Internal Resistance (IR) of the lithium-ion secondary battery cell after a second charge and discharge of the lithium-ion secondary battery; and a defect screening step of screening defects of the lithium-ion secondary battery by comparing the results with the previously measured OCV and IR after aging while applying pressure greater than a certain magnitude to the lithium-ion secondary battery. After the step of measuring one or more of the Open Circuit Voltage (OCV) and Internal Resistance (IR) of the lithium-ion secondary battery cell after a second charge and discharge of the lithium-ion secondary battery, the lithium-ion secondary battery [is subjected to] a certain pressure while [is subjected to] the lithium-ion secondary battery A method for sorting defects in a lithium-ion secondary battery, further comprising: a step of remeasuring one or more of the OCV and IR of a cell; a step of deriving a variation amount of one or more of the OCV and IR based on one or more of the previously measured values ​​of the OCV and IR and one or more of the remeasured values ​​of the OCV and IR; and a step of sorting defects in the lithium-ion secondary battery cell based on the derived variation amount. Claim 2 In claim 1, the pressure applied to the lithium-ion secondary battery in the pressurized aging step is 0.2 to 5 kg / cm² 2 A method for sorting defective lithium-ion secondary batteries characterized by the following. Claim 3 A method for sorting defective lithium-ion secondary batteries according to claim 1, characterized in that, in the pressurized aging step, the temperature is raised to 45 to 60 degrees. Claim 4 A method for sorting defective lithium-ion secondary batteries according to claim 1, wherein in the pressurized aging step, the lithium-ion secondary battery is placed between pressure plates spaced apart by a certain distance, and then the lithium-ion secondary battery is pressurized by moving each pressure plate in a direction facing each other. Claim 5 A method for sorting defective lithium-ion secondary batteries according to claim 1, wherein in the pressurized aging step, the lithium-ion secondary battery is pressurized by receiving the lithium-ion secondary battery in a pressure chamber and then increasing the pressure of the gas in the pressure chamber. Claim 6 A method for sorting defects in a lithium-ion secondary battery according to claim 1, characterized in that, in the defect sorting step, if the difference between the OCV of a lithium-ion secondary battery cell measured before the pressurized aging step and the OCV of a lithium-ion secondary battery cell re-measured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell is determined to be defective. Claim 7 A method for sorting defects in a lithium-ion secondary battery according to claim 1, wherein in the defect sorting step, if the difference between the IR of the lithium-ion secondary battery cell measured before the pressurized aging step and the IR of the lithium-ion secondary battery cell re-measured after the pressurized aging step deviates from a preset normal range, the lithium-ion secondary battery cell is determined to be defective. Claim 8 delete Claim 9 A method for sorting defective lithium secondary batteries according to claim 1, further comprising the step of pressurizing the lithium-ion secondary battery to a pressure greater than a certain magnitude prior to the secondary charging and discharging of the lithium-ion secondary battery. Claim 10 A method for detecting defects in a lithium-ion secondary battery according to claim 1, wherein in the step of detecting defects in the lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR, the lithium-ion secondary battery cell is determined to be defective if the difference between the variation of the derived OCV and the variation of a preset OCV deviates from a preset normal range. Claim 11 A method for detecting defects in a lithium-ion secondary battery according to claim 1, wherein in the step of detecting defects in the lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR, the lithium-ion secondary battery cell is determined to be defective if the difference between the variation of the derived IR and the variation of a preset IR deviates from a preset normal range. Claim 12 A method for detecting defects in a lithium-ion secondary battery according to claim 1, wherein in the step of detecting defects in the lithium-ion secondary battery cell based on one or more variations of the derived OCV and IR, the lithium-ion secondary battery cell is determined to be defective if the difference between the variation of the derived OCV and IR and the preset variation of OCV and IR deviates from a preset normal range. Claim 13 A method for sorting defects in a lithium-ion secondary battery according to claim 1, characterized in that, in the defect sorting step, if the OCV and IR of the lithium-ion secondary battery cell measured after the secondary charge and discharge of the lithium-ion secondary battery deviate from a preset normal range, the lithium-ion secondary battery cell is determined to be defective. Claim 14 A lithium-ion secondary battery manufactured by the method for sorting defective lithium-ion secondary batteries of claim 1.

Citation Information

Patent Citations

  • Method for preparing lithium secondary battery having high-temperature storage properties

    KR1020180087162A

  • Multicell battery monitoring system

    US5675234A