Vertical type gateless, capacitorless memory device, and its manufacturing mehtod
A vertical gateless and capacitorless memory device using two-dimensional materials addresses reliability and durability issues by eliminating the gate and capacitor, enhancing integration density and enabling low-power operation.
Patent Information
- Application Number
- KR1020240134863
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-10-04
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2044-10-04
AI Technical Summary
Existing capacitorless DRAM devices face issues with reduced memory reliability and durability due to gate insulating film degradation and structural instability, limiting miniaturization and integration density.
A vertical gateless and capacitorless memory device utilizing two-dimensional materials for the emitter, base, and collector layers, eliminating the need for a gate and capacitor, and employing a two-terminal structure to enhance reliability and integration.
The solution improves memory reliability by preventing gate insulating film degradation, enables high integration density, and allows for low-power operation with a simplified manufacturing process.
Smart Images

Figure 112024108108165-PAT00004_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a vertical gateless and capacitorless memory device and a method for manufacturing the same through two-dimensional material-based bandgap engineering.
[0002] Meanwhile, the present invention is the result of the Nano and Materials Technology Development Project (Research Project Name: Development of High-Performance Ultra-High Bandgap Energy Semiconductor to Overcome Space Environments through Extreme Defect Control; RS-2024-00460372) conducted with funding from the Ministry of Science and ICT and support from the National Research Foundation of Korea, and the Science and Technology-based Innovation Startup University Development Project (Research Project Name: 2023 Laboratory-Specialized Startup Leading University Project (Jeonbuk National University); RS-2023-00254730; 2710002608) conducted with funding from the Ministry of Science and ICT and support from the Korea Science and Technology Commercialization Agency. Background Technology
[0003] In the information society, semiconductors are essential components responsible for the processing and storage of information. To date, many computers and various digital devices operate by incorporating numerous semiconductors.
[0004] Dynamic Random Access Memory (DRAM), an example of a transistor that stores information, stores data in unit cells and is controlled by word lines and bit lines. Each unit cell consists of serially connected transistors and charge storage electrodes, and the capacity of the charge storage electrodes is directly related to the electrical characteristics and reliability of the DRAM memory cell.
[0005] In the case of memory devices, increasing the number of cells per unit area yields superior commercial and economic benefits; therefore, miniaturizing cells is the biggest challenge that the memory industry must address. To achieve cell miniaturization, reducing the size of transistors or capacitors in conventional DRAM cell structures has been a core technology in the memory industry. While technological advancements have made it possible to reduce transistor size, miniaturizing capacitors while maintaining capacitance has faced technical limitations. To resolve this issue, capacitorless DRAM has been proposed. In capacitorless DRAM, a unit cell consists of only a single transistor without a capacitor, which is advantageous for cell miniaturization. In other words, miniaturization allows for high integration density, and the simple manufacturing process makes it favorable for commercialization. However, capacitorless DRAM requires high driving voltages during memory write and read operations, leading to degradation of the gate insulation layer. Consequently, this presents critical issues regarding reliability and durability among memory operational characteristics.
[0006] Patent Document 1 relates to a semiconductor device and a method for manufacturing the same, and discloses a semiconductor device having a two-terminal structure without a gate. However, in the case of the semiconductor device disclosed in Patent Document 1, Si or Si is present in each of the drain region, body region, and source region. 1-x Ge x It includes, but the above Si 1-x Ge x In the case of, there was a disadvantage in that it was difficult to form a vertical stacked structure due to structural instability in the vertical direction. In addition, the above Si 1-x Ge xIn the case of [the device], there were limitations in bandgap engineering as the electron concentration in a fixed bandgap was controlled through doping, and furthermore, the process of doping Si and Ge was difficult to form abrupt junctions, which had the disadvantage of weakening memory characteristics due to leakage charge. Prior art literature
[0007] Korean Registered Patent No. 10-2424557 The problem to be solved
[0008] The present invention has been devised to solve the aforementioned problems and aims to present a vertical gateless and capacitorless memory device utilizing a two-dimensional material and a method for manufacturing the same, in order to solve the problem of reduced memory reliability and durability caused by the degradation of the gate insulating film. means of solving the problem
[0009] The present invention discloses a memory device comprising a plurality of unit cells, each comprising: an emitter layer formed on a substrate; a base layer formed on the emitter layer; and a collector layer formed on the base layer, wherein the emitter layer, the base layer, and the collector layer are all made of a two-dimensional material, as a means to achieve the above-described purpose.
[0010] Here, the emitter layer and the collector layer may be made of an n+ type two-dimensional material, and the base layer may be made of a p+ type two-dimensional material.
[0011] Here, the emitter layer and the collector layer may be made of an n+ type two-dimensional material, and the base layer may be made of an n++ type two-dimensional material.
[0012] Here, the emitter layer and the collector layer may be made of a p+ type two-dimensional material, and the base layer may be made of an n+ type two-dimensional material.
[0013] Here, the memory device may be composed of WS2 / MoS2 / WS2, WS2 / MoTe2 / WS2, or MoS2 / WSe2 / MoS2.
[0014] Here, it may further include bit lines connected to two or more emitter layers and arranged in a first direction, and word lines connected to two or more collector layers and arranged in a second direction different from the first direction.
[0015] Here, the memory device can be driven through the energy bandgap difference of different two-dimensional materials provided in the emitter layer, the base layer, and the collector layer.
[0016] Here, the integration density of the above unit cell is 4F 2 It may be less than.
[0017] In addition, the present invention discloses a method for manufacturing a memory device comprising the steps of: forming an emitter layer on a substrate; forming a base layer on the emitter layer; and forming a collector layer on the base layer as a means to achieve the above-described purpose, wherein the emitter layer, the base layer, and the collector layer are all formed using a two-dimensional material.
[0018] Herein, the manufacturing method may further include the step of forming a bit line in a first direction so that two or more emitter layers are electrically connected; and the step of forming a word line in a second direction different from the first direction so that two or more collector layers are electrically connected. Effects of the invention
[0019] The memory device of the present invention can fundamentally solve the problem of gate insulating film degradation occurring in capacitorless devices having three or more terminals, thereby improving the reliability of the device.
[0020] In addition, the memory device of the present invention can provide a highly integrated semiconductor device by manufacturing a capacitorless semiconductor device in a vertical configuration to reduce the size of the device.
[0021] In addition, since the memory device of the present invention can store charge in the base layer without a capacitor, it is possible to achieve high integration while simplifying the manufacturing process, and subsequently expect the effect of being able to operate even at low power.
[0022] In addition, the memory device of the present invention can achieve bandgap engineering through a more simplified process by utilizing a two-dimensional material. Brief explanation of the drawing
[0023] Figure 1 is a schematic diagram illustrating the appearance of a unit cell of the present invention. Figure 2 is a schematic diagram illustrating the band gap diagram of a two-dimensional material forming the unit cell. Figure 3 is a schematic diagram illustrating the appearance of a memory device of the present invention. FIG. 4 is a plan view illustrating the appearance of the memory element of the present invention. FIG. 5 is a flowchart illustrating the manufacturing process of the memory device of the present invention. Figure 6 is a Raman spectrum of a unit cell manufactured according to one embodiment of the present invention. Figure 7 is a CV curve of a memory device manufactured according to one embodiment of the present invention. FIG. 8 is a CV curve of a memory device manufactured according to one embodiment of the present invention. Specific details for implementing the invention
[0024] The present invention is capable of various modifications and may have various embodiments, and specific embodiments are illustrated in the drawings and described in detail in the detailed description. However, this is not intended to limit the invention to specific embodiments, and it should be understood that the invention includes all modifications, equivalents, and substitutions that fall within the spirit and scope of the invention.
[0025] Throughout this specification, when a part is described as "comprising" a certain component, this means that, unless specifically stated otherwise, it does not exclude other components but may include additional components.
[0026] As used herein, terms of degree such as “about,” “substantially,” etc., are used to mean at or near the stated value when inherent manufacturing material tolerances are presented in the said sense, and are used to prevent unscrupulous infringers from unfairly exploiting the disclosed content in which precise or absolute values are mentioned to aid in understanding the invention. Furthermore, throughout this specification, “a step of” or “a step of” does not mean “a step for”.
[0027] Since a person skilled in the art can make various applications through the gist of the present invention, the scope of the rights of the present invention is not limited to the following embodiments. The scope of the rights of the present invention extends to parts that are obvious to a person skilled in the art who can easily substitute or modify using prior art based on the matters described in the specific claims.
[0028] The present invention will be described in more detail below with reference to the attached drawings, where necessary.
[0030] The present invention discloses a memory device comprising a plurality of unit cells, each comprising: an emitter layer formed on a substrate; a base layer formed on the emitter layer; and a collector layer formed on the base layer, wherein the emitter layer, the base layer, and the collector layer are all made of a two-dimensional material, as a means to achieve the above-described purpose.
[0031] That is, the memory device of the present invention can be formed with a structure without a gate, a gate insulating film, and a capacitor, and in particular, since there is no gate insulating film made of metal oxide, the problem of reduced device reliability due to insulating film degradation can be fundamentally prevented.
[0032] FIG. 1 is a schematic diagram illustrating the appearance of a unit cell of the present invention. Referring to FIG. 1, it can be seen that the unit cell forming the memory element of the present invention has an emitter layer (10a), a base layer (10b), and a collector layer (10c) formed vertically on a substrate (100). The phrase "formed vertically" means that each layer is arranged to form a vertical column shape. Additionally, the emitter layer (10a), the base layer (10b), and the collector layer (10c) may each be made of a two-dimensional material.
[0033] Each layer forming the unit cell may be composed of a two-dimensional material as described above. The two-dimensional material may be, for example, graphene, transition metal chalcogenides, etc. The transition metal chalcogenides refer to compounds having a composition of MX2 (M is a transition metal, X is a chalcogen atom) in which the atomic plane of a transition metal is sandwiched between two atomic planes of chalcogen atoms (S, Se, and Te). More specific examples of the transition metal chalcogenides may include MoS2, MoSe2, MoTe2, WS2, WSe2, WTe2, SnS2, etc., but are not limited thereto.
[0034] In the present invention, several advantages can be secured by using the aforementioned two-dimensional material in each layer forming the unit cell. For example, the two-dimensional material has the advantage of being free from defects as it does not possess the dangling bonds found in conventional silicon, and is easy to separate layer by layer by van der Waals forces. In addition, the two-dimensional material has the advantage of being an ultrathin film with a monolayer of 1 nm or less, and the band gap can be controlled by adjusting the number of layers, thus facilitating band gap engineering. For example, the two-dimensional material, particularly transition metal chalcogenides, is characterized by having different band gaps when in a monolayer and when in a bulk state. For example, in the case of MoS2, the band gap when in a monolayer is approximately 1.9 eV, and the band gap when in a bulk state is approximately 1.3 eV.
[0035] In addition, the above transition metal chalcogenides may exhibit n-type or p-type semiconductor characteristics depending on their type. The above n-type semiconductor refers to a material in which the Fermi level is located near the conduction band within the band gap, and the above p-type semiconductor refers to a material in which the Fermi level is located near the valence band within the band gap. For example, transition metal chalcogenides exhibiting n-type semiconductor characteristics may include WS2, MoS2, etc., and transition metal chalcogenides exhibiting p-type semiconductor characteristics may include MoTe2, WSe2, etc.
[0036] In the present invention, the emitter layer / base layer / collector layer of each unit cell may heterojunction two-dimensional materials exhibiting different semiconductor characteristics. Here, the memory device may be driven through the difference in energy band gaps between the different two-dimensional materials provided in the emitter layer, the base layer, and the collector layer. That is, the emitter layer / base layer / collector layer of each unit cell may be formed of [p-type two-dimensional material / n-type two-dimensional material / p-type two-dimensional material] or [n-type two-dimensional material / p-type two-dimensional material / n-type two-dimensional material].
[0037] Furthermore, in the memory device of the present invention, the emitter layer, base layer, and collector layer constituting each unit cell may all be formed of an n-type two-dimensional material or all of a p-type two-dimensional material. Even if they are the same n-type two-dimensional material or p-type two-dimensional material, since each material has a different band gap, each layer of the unit cell can be formed using a different band gap among the same n-type or p-type two-dimensional material. That is, among the n-type two-dimensional materials, a material in which the Fermi level is located relatively closer to the conduction band can be called an n++-type two-dimensional material, and a material in which the Fermi level is located less close to the conduction band can be called an n+-type two-dimensional material. In addition, among the p-type two-dimensional materials, a material in which the Fermi level is located relatively closer to the valence band can be called a p+-type two-dimensional material, and a material in which the Fermi level is located less close to the valence band can be called a p++-type two-dimensional material. In other words, in the semiconductor device of the present invention, the unit cell may form, for example, a [n+ / n++ / n+] structure or a [p++ / p+ / p++] structure. More specifically, the memory device may be composed of WS2 / MoS2 / WS2, WS2 / MoTe2 / WS2, or MoS2 / WSe2 / MoS2, but is not limited thereto.
[0038] In addition, the above-mentioned two-dimensional material may be used after additional doping treatment depending on the purpose of the device.
[0039] FIG. 2 is a schematic diagram illustrating the band gap diagram of a two-dimensional material forming a unit cell of the present invention. More specifically, FIG. 2a illustrates the band gap diagram in a unit cell with a [n+ / n++ / n+] structure, and FIG. 2b illustrates the band gap diagram in a unit cell with a [n+ / p+ / n+] structure.
[0040] Hereinafter, the operation method of the memory element of the present invention will be explained with reference to FIG. 2.
[0041] First, the operation method of the memory device having a bandgap illustrated in FIG. 2a is as follows. When a voltage is applied to two n+ type regions, the n++ type region sandwiched between the two n+ types can be electrically floating. Consequently, electrons, which are majority carriers, accumulate in the n++ type region, and depending on the presence or absence of accumulated electrons (difference in threshold voltage), a bistable current-voltage characteristic can be obtained. If electrons accumulate in the n++ type region, the threshold voltage is lowered and detected as a "1" state, and if electrons are not accumulated, the threshold voltage rises and is detected as a "0" state. At this time, the driving current differs depending on the different threshold voltages, and this can be used as memory.
[0042] Next, the operation method of the memory device having a bandgap illustrated in FIG. 2b is as follows. When a voltage is applied to two n+ type regions, the p+ type region sandwiched between the two n+ types can be electrically floating. Consequently, holes, which are majority carriers, accumulate in the p+ type region, and a bistable current-voltage characteristic can be exhibited depending on the presence or absence of accumulated holes (difference in threshold voltage). If holes accumulate in the p+ type region, the threshold voltage is lowered and detected as a "1" state, and if holes are not accumulated, the threshold voltage rises and is detected as a "0" state. At this time, the driving current differs depending on the different threshold voltages, and this can be used as memory.
[0043] In the memory device of the present invention, the semiconductor located in the base layer is electrically floated, so an external voltage cannot be applied. Since the gate has been removed, it has become a two-terminal transistor; however, if the voltage between the two terminals is increased, electron-hole pairs are generated by collisional ionization, just as in the conventional method. In the case of an n+ / n++ / n+ structure, electrons accumulate in the base layer region, and in the case of an n+ / p+ / n+ structure, holes accumulate. When the voltage reaches a specific value, a large current flows, similar to how an NPN bipolar transistor (BJT) with an open base (=gate) enters the breakdown region. At this point, as long as a voltage above a specific value is applied, the large current is maintained (latched). When the voltage is reduced again, the generation of electron-hole pairs decreases, causing the device to move out of the breakdown region and the current value to drop sharply. At this time, the voltage at which the device moves out of the breakdown region (Latch Down voltage) is smaller than the voltage at which breakdown occurs (Latch Up voltage), exhibiting bistable current-voltage characteristics between the two voltages. Consequently, "1" and "0" are distinguished by comparing the amount of current generated depending on whether holes or electrons accumulate in the base layer. Since the gate is removed using the following method, the gate insulating film is also naturally removed, thereby fundamentally preventing the degradation of device reliability and durability caused by impact ionization.
[0044] Here, the memory element of the present invention may further include a bit line connected to two or more emitter layers and arranged in a first direction, and a word line connected to two or more collector layers and arranged in a second direction different from the first direction.
[0045] FIG. 3 is a schematic diagram illustrating the appearance of a memory device of the present invention. More specifically, FIG. 3 is a diagram showing a configuration in which a plurality of unit cells disclosed in FIG. 1 are arranged.
[0046] Referring to FIG. 3, the memory device of the present invention comprises a plurality of unit cells arranged on a substrate, wherein the unit cells are composed of an emitter layer (10a), a base layer (10b), and a collector layer (10c), and it can be seen that a bit line (60) is arranged in a first direction of each unit cell. Additionally, it can be seen that a word line (70) is arranged in a second direction different from the first direction.
[0047] Furthermore, referring to FIG. 3, the memory device of the present invention is an array structure using two terminals, a collector and an emitter, which can block a sneak path. The sneak path problem refers to current flowing in an unwanted direction at a crossbar, and is a problem that occurs because gating is not performed in the crossbar structure. In other words, the memory device of the present invention [describes] the flow of current (I) flowing from a single emitter layer (10a) through a base layer (10b) to a collector layer (10c). FWD In the process, the reverse current (I) of an adjacent cell REV ) can be blocked to prevent sneak paths. This may be because the electrical characteristics between the two terminals are unidirectional.
[0048] In the memory device of the present invention, since each layer of each unit cell constituting the memory device is made of a two-dimensional material, it is possible to improve memory characteristics and reduce operating voltage and improve sensing margin. In addition, the memory device of the present invention can achieve high integration density by introducing a unit cell with a vertical structure. Here, the integration density of the unit cell is 4F 2 It may be less than.
[0049] FIG. 4 is a view of FIG. 3 from the 30 direction, showing a configuration where a bit line (60) and a word line (70) intersect. FIG. 3 also shows a bit line (60) and a word line (70) electrically connected to a single unit cell arranged vertically. The area occupied by the intersection point of the word line (60) and the bit line (70) is 2F in width and height, and through this, a single unit cell has a gateless-capacitorless structure and 4F 2 A vertical two-terminal structure with the same level of integration can be completed.
[0050] Since the memory device of the present invention has a vertical two-terminal structure, the integration density can be increased, and the cell pitch between unit cells can be configured to be 30 nm or less. Conventionally, the device size of a unit cell is at least 6F 2 However, by applying the embodiments of the present invention, high integration can be achieved by reducing the cell size vertically. In addition, by introducing a two-dimensional material into each layer constituting the unit cell, low operating voltage and high driving current can be realized.
[0052] In addition, the present invention discloses a method for manufacturing a memory device as a means to achieve the above-described purpose.
[0053] FIG. 5 is a flowchart illustrating the manufacturing process of a memory device of the present invention. Referring to FIG. 5, it can be seen that the method for manufacturing a memory device of the present invention includes the steps of: forming an emitter layer on a substrate; forming a base layer on the emitter layer; and forming a collector layer on the base layer.
[0054] Here, the emitter layer, the base layer, and the collector layer can all be formed using a two-dimensional material as described above. For example, the emitter layer, the base layer, and the collector layer can be formed with a structure of [n+ type two-dimensional material / n++ type two-dimensional material / n+ type two-dimensional material], [n+ type two-dimensional material / p+ type two-dimensional material / n+ type two-dimensional material], [p+ type two-dimensional material / n+ type two-dimensional material / p+ type two-dimensional material], or [p++ type two-dimensional material / p+ type two-dimensional material / p++ type two-dimensional material].
[0055] Here, known methods may be used to form each layer of the unit cell. For example, chemical vapor deposition, atomic layer deposition, ion-assisted deposition, plasma methods, etc., may be used, but are not limited thereto. According to one embodiment of the present invention, each layer of the unit cell may be formed using the MOCVD (Metal Organic Chemical Vapor Deposition) method.
[0056] In addition, as described above, since the band gap of each layer of the unit cell varies depending on the type and thickness of the two-dimensional material formed therein, the thickness of each layer is not limited to any specific numerical value; however, in the semiconductor device of the present invention, it is preferable that the emitter layer and the collector layer be formed to have a relatively large band gap so as to induce a large amount of charge in the base layer, and it is preferable that the base layer be formed to have a relatively small band gap. In the present invention, the two-dimensional material formed in each layer of the unit cell may exhibit a tendency to induce a narrower band gap as the thickness increases. Accordingly, it is preferable that the emitter layer and the collector layer be formed with a thickness of 0.1 to 10 nm more specifically, and it is preferable that the base layer be formed with a thickness of 100 nm or less more specifically. Since the amount of charge induced in the base layer increases as the base layer is formed to have a small band gap, an effect of increasing the possibility of sensing can be expected.
[0057] Furthermore, the memory device of the present invention can be vertically stacked through a more simplified process because it can be grown in a one-shot manner using the MOCVD method described above once only the two-dimensional materials forming the emitter layer, base layer, and collector layer are determined. In addition, since it is not necessary to perform a process of injecting additional impurities to form each layer of the unit cell, there is also an advantage that the memory device of the present invention can be manufactured through a more simplified process.
[0058] Herein, the manufacturing method may further include the step of forming a bit line in a first direction so that two or more emitter layers are electrically connected; and the step of forming a word line in a second direction different from the first direction so that two or more collector layers are electrically connected.
[0059] In addition, the manufacturing method of the present invention may further include the step of depositing an insulating material between the unit cells.
[0060] In addition, since the memory device of the present invention forms the emitter layer, base layer, and collector layer constituting each unit cell entirely from a two-dimensional material, the effect of not requiring a sensing amplifier can also be expected. The sensing amplifier was used in conventional memory devices to detect small differential input signals and amplify them into digital signals. However, in the case of the memory device of the present invention, since the unit cell is constructed by including a two-dimensional material, particularly a transition metal chalcogenide, a high On / Off current ratio, high field-effect mobility, and a low threshold swing can be expected from the wide bandgap originating from the two-dimensional material, high reliability can be achieved even without the aforementioned sensing amplifier.
[0061] Since there is no gate insulating film, breakdown of the gate oxide can be prevented, thereby improving the reliability of the device.
[0062] Furthermore, since the memory device of the present invention is devoid of capacitors, it can improve integration density and fundamentally eliminate capacitor-related issues. Accordingly, it has the advantage of being able to have high-density memory and operate at low power.
[0063] The memory device of the present invention can fundamentally solve the problem of gate insulating film degradation occurring in capacitorless devices having three or more terminals, thereby improving the reliability of the device.
[0064] The memory device of the present invention can provide a highly integrated semiconductor device by manufacturing a capacitorless semiconductor device in a vertical configuration to reduce the size of the device.
[0065] Since the memory device of the present invention can store charge in the base layer without a capacitor, it is possible to achieve high integration while simplifying the manufacturing process, and subsequently expect the effect of being able to operate even at low power.
[0067] Hereinafter, the claims of this specification will be explained in more detail with reference to the attached drawings and embodiments. However, as the drawings and embodiments presented in this specification may be modified in various ways by a person skilled in the art and may take various forms, the details described in this invention should not be limited to a specific disclosed form, but should be understood to include all equivalents and substitutions included within the spirit and scope of the invention. Furthermore, the attached drawings are presented to help a person skilled in the art understand the invention more accurately and may be depicted in an exaggerated or reduced size compared to the actual size.
[0069] {Examples and Evaluation}
[0070] <Example>
[0071] Example 1
[0072] First, the emitter, base, and collector layers were grown on a silicon oxide film using the MOCVD method. Nitrogen was used as the carrier gas, and hydrogen was used as the atmosphere gas. To form the emitter layer, a WS2 layer was formed by maintaining the flow rates of W(CO)6 and (C2H5)2S at 50 sccm and 5 sccm, respectively, at a growth temperature of 550 ℃ and a deposition time of 45 minutes. Next, a MoS2 layer was formed by maintaining the flow rates of Mo(CO)6 and (C2H5)2S at 50 sccm and 5 sccm, respectively, at a growth temperature of 550 ℃ and a deposition time of 90 minutes. Finally, a WS2 layer was formed by maintaining the flow rates of W(CO)6 and (C2H5)2S at 50 sccm and 5 sccm, respectively, at a growth temperature of 550 ℃ and a deposition time of 45 minutes.
[0073] Subsequently, a lower electrode (Cr / Au, 30 / 70 nm) is placed on a separate substrate at a depth of 100 μm A WS2 / MoS2 / WS2 layer formed by the above method was formed to a size of 100 μm and transferred onto the lower electrode. Subsequently, the WS2 / MoS2 / WS2 layer was patterned on the lower electrode through photolithography and etching processes, and then an upper electrode (Ti / Ni, 30 / 70 nm) was formed on the top surface to a size of 100 μm. A semiconductor device was manufactured by forming it to a size of 100 μm (hereinafter referred to as "Example 1").
[0074] Example 2
[0075] A semiconductor device was manufactured in the same manner as in Example 1, except that the lower electrode was Ti / Ni (30 / 70 nm) and the upper electrode was Cr / Au (30 / 70 nm) (hereinafter referred to as "Example 2").
[0076] Example 3
[0077] The size of the lower electrode and the upper electrode is 500 μm A semiconductor device was manufactured in the same manner as in Example 1, except that it was formed to a size of 500 μm (hereinafter referred to as "Example 3").
[0079] <Evaluation>
[0080] FIG. 6 is a Raman spectrum of a unit cell manufactured according to one embodiment of the present invention. More specifically, FIG. 6a compares the Raman spectra of MoS2, WS2, and a unit cell manufactured according to the above embodiment, and FIG. 6b compares the Raman spectra when the unit cell manufactured according to the above embodiment is stacked 2 to 10 times.
[0081] Referring to Fig. 6, it can be seen that in the unit cell fabricated by organometallic chemical vapor deposition, WS2 and MoS2 forming each layer are well formed without deformation of the molecular structure. In addition, it can be seen that the molecular structure of each layer is well maintained even when a multiple stacking process is performed.
[0082] FIG. 7 is a CV curve of a memory device manufactured according to one embodiment of the present invention. More specifically, it shows the CV curve of a memory device manufactured according to Examples 1 to 3. In FIG. 7, the substrate TE refers to the top electrode, and the substrate BE refers to the bottom electrode.
[0083] Referring to Fig. 7, it can be seen that the current increases proportionally with the size of the upper and lower electrodes, and the largest current value appears in Example 3. Additionally, it can be observed from the data in Fig. 7 that the curves of Example 1 and Example 2 are not identical, which means that the memory device of the present invention does not exhibit Fermi level pinning. The work function of a metal is a factor that determines the conductivity (current amount) of a semiconductor material, and in this case, the work function must be aligned with the Fermi level of the two-dimensional material. If Fermi level pinning occurs, it may be aligned at an energy level different from the theory. That is, since the above Examples 1 and 2 used Ti and Cr as electrodes, they should theoretically exhibit different current amounts, and since it can be confirmed that the experimental values also exhibit different current amounts similar to the theory, it can be inferred that the memory device of the present invention does not exhibit Fermi level pinning.
[0084] In addition, the structure of a conventional two-dimensional material transistor is formed with a lower electrode, a two-dimensional material (channel), and an upper electrode in a vertical structure, and additionally, an electrode is formed on the lower electrode in a horizontal structure with the two-dimensional material. At this time, non-uniform surfaces are generated on the side of the two-dimensional material due to cutting or other factors during thin film manufacturing, and as the additionally formed electrode is formed to contact this non-uniform two-dimensional material, the work function is fixed in the non-uniform surface, that is, in a non-uniform energy band, and there was a problem in which Fermi level pinning frequently occurred in the thickness portion of the two-dimensional material. In contrast, the memory device of the present invention can be free from problems such as Fermi level pinning because the emitter layer, base layer, and collector layer, which include the aforementioned electrode and two-dimensional material, all form a vertical structure.
[0085] FIG. 8 is a CV curve of a memory device manufactured according to one embodiment of the present invention. FIG. 8 is intended to verify the difference in device performance by region of a wafer on which the manufactured memory device is formed. More specifically, FIG. 8a shows wafer regions divided for performance testing of a memory device manufactured according to Example 3, and FIG. 8b shows the CV curve for each wafer region.
[0086] Referring to FIG. 8, it can be seen that the memory device manufactured according to the above embodiment has almost no difference in current values depending on each wafer region, and that quantum wells are formed upon current application. In addition, it can be seen that the memory device of the present invention exhibits the same current value regardless of the direction of the applied voltage, so excellent stability of the device can be expected.
[0087] The memory device of the present invention can fundamentally solve the problem of gate insulating film degradation occurring in capacitorless devices having three or more terminals, thereby improving the reliability of the device.
[0088] In addition, the memory device of the present invention can provide a highly integrated semiconductor device by manufacturing a capacitorless semiconductor device in a vertical configuration to reduce the size of the device.
[0089] In addition, since the memory device of the present invention can store charge in the base layer without a capacitor, it is possible to achieve high integration while simplifying the manufacturing process, and subsequently expect the effect of being able to operate even at low power.
[0090] In addition, the memory device of the present invention can achieve bandgap engineering through a more simplified process by utilizing a two-dimensional material.
[0092] The above description is merely an illustrative explanation of the technical concept of the present invention, and those skilled in the art to which the present invention pertains will be able to make various modifications and variations within the scope of the essential characteristics of the present invention.
[0093] Accordingly, the embodiments disclosed in this invention are intended to illustrate, not limit, the technical concept of the invention, and the scope of the technical concept of the invention is not limited by these embodiments. The scope of protection of this invention shall be interpreted by the claims below, and all technical concepts within an equivalent scope shall be interpreted as being included within the scope of rights of this invention.
Claims
Claim 1 A memory device comprising a plurality of unit cells including an emitter layer formed on a substrate; a base layer formed on the emitter layer; and a collector layer formed on the base layer; wherein the emitter layer, the base layer, and the collector layer are all made of a two-dimensional material, and by distinguishing between "1" and "0" by comparing the amount of current generated with bistable current-voltage characteristics depending on whether holes or electrons are accumulated in the base layer by generating electron-hole pairs by collision ionization, the emitter layer, the base layer, and the collector layer, the memory device is driven through the difference in energy bandgap between the different two-dimensional materials provided in the emitter layer, the base layer, and the collector layer. Claim 2 A memory device according to claim 1, wherein the emitter layer and the collector layer are made of an n+ type two-dimensional material, and the base layer is made of a p+ type two-dimensional material. Claim 3 A memory device according to claim 1, wherein the emitter layer and the collector layer are made of an n+ type two-dimensional material, and the base layer is made of an n++ type two-dimensional material. Claim 4 A memory device according to claim 1, wherein the emitter layer and the collector layer are made of a p+ type two-dimensional material, and the base layer is made of an n+ type two-dimensional material. Claim 5 In claim 1, the memory element is a memory element composed of WS2 / MoS2 / WS2, WS2 / MoTe2 / WS2, or MoS2 / WSe2 / MoS2. Claim 6 A memory element according to claim 1, further comprising a bit line connected to two or more emitter layers and arranged in a first direction, and a word line connected to two or more collector layers and arranged in a second direction different from the first direction. Claim 7 In claim 1, the integration density of the unit cell is 4F 2 Lee Ha-in, memory device. Claim 8 A method for manufacturing a memory device comprising: a step of forming an emitter layer on a substrate; a step of forming a base layer on the emitter layer; and a step of forming a collector layer on the base layer; wherein the emitter layer, the base layer, and the collector layer are all formed using a two-dimensional material, and electron-hole pairs are generated by collision ionization, and a current amount is distinguished between "1" and "0" by comparing the amount of current generated with bistable current-voltage characteristics depending on whether holes or electrons are accumulated in the base layer, thereby driving through the difference in energy band gaps of different two-dimensional materials provided in the emitter layer, the base layer, and the collector layer. Claim 9 A method for manufacturing a memory device according to claim 8, further comprising: a step of forming a bit line in a first direction such that two or more emitter layers are electrically connected; and a step of forming a word line in a second direction different from the first direction such that two or more collector layers are electrically connected. Claim 10 delete
Citation Information
Patent Citations
Two-terminal biristor with poly-crystalline silicon emitter electrode and method for manufacturing thereof
KR1020200021419A
Semiconductor device, and method for manufacturing the same
KR102424557B1