A semiconductor device
The semiconductor device addresses interference issues in highly integrated DRAMs by using oblique active patterns, device isolation, and sidewall barrier impurities to prevent charge leakage, improving operational reliability and data retention.
Patent Information
- Application Number
- KR1020220078640
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-06-28
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2042-06-28
AI Technical Summary
As DRAM devices become highly integrated, the reduced spacing between gate structures leads to malfunction and operational failure of recessed channel transistors due to interference, affecting the unit cell's performance.
A semiconductor device design featuring a first active pattern with an oblique direction, device isolation patterns within trenches, and a barrier impurity region on the sidewalls of the active pattern to prevent charge leakage, combined with a gate structure and impurity regions to enhance operational reliability.
The design reduces operational failures by suppressing charge movement and leakage, maintaining data integrity in the capacitor, thereby enhancing the DRAM device's operating characteristics.
Smart Images

Figure R1020220078640_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a semiconductor device. More specifically, the present invention relates to a DRAM device. Background Technology
[0002] In a DRAM device, a unit cell may include a recessed channel transistor and a capacitor. The recessed channel transistor may include a gate structure embedded within an active pattern and a device isolation pattern. As the DRAM device becomes highly integrated, the spacing between the gate structures may be reduced. Consequently, malfunction of the recessed channel transistor due to interference from the gate structures may occur, and operational failure of the unit cell may occur. The problem to be solved
[0003] The objective of the present invention is to provide a semiconductor device having excellent operating characteristics. means of solving the problem
[0004] A semiconductor device according to embodiments of the present invention for achieving the above-mentioned objectives is provided with a first active pattern having an isolated shape that is included on the substrate of a memory cell region and extends such that a direction oblique to a first direction becomes the long axis direction. A first device isolation pattern is provided within a first trench included in the substrate of the memory cell region and covers the sidewall of the first active pattern. A first gate structure is provided inside a gate trench extending in the first direction above the first active pattern and the first device isolation pattern. A barrier impurity region is selectively formed only on the surface of both sidewalls of the long axis of the first active pattern. First and second impurity regions are provided above the first active pattern adjacent to both sides of the first gate structure.
[0005] A semiconductor device according to embodiments of the present invention for achieving the above-mentioned objectives comprises a substrate including a memory cell region, a core ferri region, and a boundary region between the memory cell region and the core ferri region. A first active pattern and a first device isolation pattern are provided on the substrate of the memory cell region. A second device isolation pattern is provided to fill the interior of a second trench included in the substrate of the boundary region between the memory cell region and the core ferri region. A third device isolation pattern is provided to fill the interior of a third trench included in the substrate of the core ferri region. A first gate structure is provided within a gate trench extending in a first direction on the upper surface of the first active pattern and the first device isolation pattern. A barrier impurity region is selectively provided only on the surface of both sidewalls of the long axis of the first active pattern. First and second impurity regions are provided on the upper surface of the first active pattern adjacent to both sides of the first gate structure. The bottom surface of the second trench is not flat and has a step.
[0006] A semiconductor device according to embodiments of the present invention for achieving the above-mentioned objectives comprises a substrate including a memory cell region, a core ferri region, and a boundary region between the memory cell region and the core ferri region. A first active pattern and a first device isolation pattern are provided on the substrate of the memory cell region. A second device isolation pattern is provided to fill the interior of a second trench included in the substrate of the boundary region between the memory cell region and the core ferri region. A third device isolation pattern is provided to fill the interior of a third trench included in the substrate of the core ferri region. A first gate structure is provided within a gate trench extending in a first direction on the upper portion of the first active pattern and the first device isolation pattern. A barrier impurity region doped with germanium or fluorine is provided, which is selectively formed only on the surface of both sidewalls of the long axis of the first active pattern. First and second impurity regions are provided on the upper portion of the first active pattern adjacent to both sides of the first gate structure. A bit line structure electrically connected to the first impurity region is provided. A capacitor electrically connected to the above second impurity region is provided. Effects of the invention
[0007] In a semiconductor device according to exemplary embodiments, a barrier impurity region is selectively provided only on the surfaces of both sidewalls along the long axis of the first active pattern. By providing the barrier impurity region, charges can be suppressed from moving and flowing out from the first active pattern below the second impurity region to the bottom surface of the gate structure. Accordingly, operational failures caused by interference in the transistor can be reduced. Brief explanation of the drawing
[0008] FIGS. 1 and FIGS. 2 are a plan view and a cross-sectional view showing a DRAM device according to exemplary embodiments. FIGS. 3 and FIGS. 4 are a plan view and a perspective view showing a first active pattern and a first gate structure of a memory cell region of a DRAM device. FIGS. 5 to 7 are cross-sectional views showing the active patterns and device isolation patterns of the memory cell region, core region, and boundary region of a DRAM device according to exemplary embodiments. FIGS. 8 to 21 are cross-sectional and plan views illustrating a method for forming active patterns of a semiconductor device according to an exemplary embodiment. FIG. 22 is a cross-sectional view showing the active patterns and device isolation patterns of the memory cell region, core region, and boundary region of a DRAM device according to exemplary embodiments. FIGS. 23 to 26 are cross-sectional views illustrating a method for manufacturing a DRAM device according to exemplary embodiments. Specific details for implementing the invention
[0009] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the attached drawings.
[0010] In the following, two directions parallel to the upper surface of the substrate and perpendicular to each other are respectively referred to as the first direction and the second direction. Additionally, a direction parallel to the upper surface of the substrate and oblique to the first direction (i.e., diagonal direction) is referred to as the third direction, and a direction parallel to the upper surface of the substrate and perpendicular to the third direction is referred to as the fourth direction.
[0011] FIGS. 1 and 2 are a plan view and a cross-sectional view showing a DRAM device according to exemplary embodiments. FIGS. 3 and 4 are a plan view and a perspective view showing a first active pattern and a first gate structure of a memory cell region of a DRAM device. FIGS. 5 to 7 are cross-sectional views showing active patterns and device isolation patterns of a memory cell region, a core ferri region, and a boundary region of a DRAM device according to exemplary embodiments.
[0012] FIG. 2 is a cross-sectional view taken along II' and II-II' of FIG. 1. In FIG. 2, the cross-sectional view taken along I-I' is taken along the barrier impurity region.
[0013] Referring to FIGS. 1 to 4, a substrate (100) is provided. The substrate (100) may include a memory cell region (A), a core periphery region (B), and a boundary region (C) located between them.
[0014] The substrate (100) may include a single-crystal semiconductor material. In an exemplary embodiment, the substrate (100) may be single-crystal silicon.
[0015] The above-mentioned core periphery region (B) may have a shape that surrounds the memory cell region (A) while being spaced apart from the edge of the memory cell region (A). The above-mentioned boundary region (C) may be a region for distinguishing the memory cell region (A) and the core periphery region (B).
[0016] The substrate (100) is provided with trenches, and an insulating material is embedded within the trenches to form a device isolation pattern. The area where the device isolation pattern is formed can be provided as a device isolation area. The portion of the substrate (100) protruding between the trenches can be defined as an active pattern. The upper surface of the active pattern can be provided as an active area.
[0017] A first trench (120) is provided in the substrate (100) of the memory cell region (A). First active patterns (130) may be formed between the first trenches (120) of the memory cell region (A). A first device isolation pattern (170a) may be provided within the first trench (120). The first device isolation pattern (170a) may cover the sidewall of the first active pattern (130).
[0018] Each first active pattern (130) may have an isolated shape extending in the third direction. That is, the third direction may be the length direction of the first active pattern (130) of the memory cell region (A), i.e., the major axis direction. The fourth direction may be the minor axis direction of the first active pattern (130). The first active pattern (130) may include first and second sidewalls of the major axis and third and fourth sidewalls of the minor axis. The first active patterns (130) may be regularly arranged spaced apart from each other along the first and second directions.
[0019] A second trench (122a) may be provided across the entire substrate (100) of the boundary region (C), and a second device isolation pattern (170b) may be provided within the second trench (122a). The boundary region (C) may have a sufficient width to distinguish between the memory cell region (A) and the core ferri region (B). Accordingly, the width of the second trench (122a) may be wider than the width of the first trench (120).
[0020] The bottom surface of the second trench (122a) may not be flat and may have a step. The second trench (122a) may include a first portion adjacent to the memory cell area (A) in the boundary area (C), a second portion adjacent to the core periphery area (B) in the boundary area (C), and a third portion between the first portion and the second portion. In an exemplary embodiment, in the boundary area (C), the bottom surface of the first portion may have a first step, the bottom surface of the second portion may have a second step, and the bottom surface of the third portion may have a third step lower than the first and second steps. The step may refer to the height of the bottom surface.
[0021] For example, as illustrated in FIG. 5, the first step and the second step may be substantially the same, and the third step may be lower than the first and second steps.
[0022] As another example, as shown in FIG. 6, the second step may be higher than the first step, and the third step may be lower than the first and second steps.
[0023] As another example, as shown in FIG. 7, the second step may be lower than the first step, and the third step may be lower than the first and second steps.
[0024] A third trench (124) is provided in the substrate (100) of the above-mentioned core ferri region (B), and a third device isolation pattern (170c) may be provided within the third trench (124). The portion of the substrate (100) where the third device isolation pattern (170c) is not formed may become a third active pattern. The upper surface of the third active pattern may be provided as an active region.
[0025] The first element isolation pattern (170a), the second element isolation pattern (170b), and the third element isolation pattern (170c) may include an insulating material. In an exemplary embodiment, the first to third element isolation patterns (170a, 170b, 170c) may include silicon oxide and / or silicon nitride.
[0026] A barrier impurity region (140) may be selectively provided only on the first and second sidewall surfaces along the long axis of the first active patterns (130) of the memory cell region (A). In an exemplary embodiment, the barrier impurity region (140) may include an impurity having a negative charge when doped into the substrate (100). In an exemplary embodiment, the impurity of the barrier impurity region (140) may include fluorine or germanium.
[0027] Since the barrier impurity region (140) is formed on the first and second sidewall surfaces of the long axis facing the fourth direction in the first active pattern (130), the barrier impurity region (140) can be arranged to face each other in the fourth direction. Accordingly, the barrier impurity region (140) may be formed at the edge of the fourth direction of the first active pattern (130) and may not be formed at the center of the fourth direction of the first active pattern (130).
[0028] Additionally, the barrier impurity region (140) may not be formed on the third and fourth sidewall surfaces of the short axis of the first active pattern (130). That is, the barrier impurity region (140) may not be formed on the sidewall of the end of the third direction of the first active pattern (130).
[0029] Meanwhile, the barrier impurity region (140) may not be formed in the third active pattern of the core ferri region (B). A recessed channel transistor may not be provided on the core ferri region (B), and only a planar type transistor may be provided. That is, a gate structure with a structure embedded in the substrate may not be provided in the core ferri region (B). Therefore, the barrier impurity region (140) is not required.
[0030] The memory cell region (A) of the above-mentioned DRAM device may include a recessed channel transistor, a bit line structure (226), a contact plug (252), a landing pad (254), and a capacitor (280). The unit memory cell of the DRAM device may include a recessed channel transistor and a capacitor (280).
[0031] A gate trench (180) extending in the first direction may be provided on the upper portion of the first active pattern (130) and the first device isolation pattern (170a) of the memory cell region (A). A first gate structure (190) may be provided inside the gate trench (180). The first gate structure (190) may extend in the first direction. The first gate structure (190) may include a first portion formed within the first active pattern (130) and a second portion formed within the first device isolation pattern (170a).
[0032] Two first gate structures (190) may be spaced apart from each other in a single unit first active pattern (130). Two recessed channel transistors may be formed in a single unit first active pattern (130). One first gate structure (190) may be disposed in each of the first device isolation patterns (170a) that contact both ends (i.e., both ends in the long axis direction) of the single unit first active pattern (130).
[0033] A first portion of the first gate structure (190) disposed within the first active pattern (130) may be provided as a main gate structure (190a) of a recessed transistor. A second portion of the first gate structure (190) disposed within the first device isolation pattern (170a) may be provided as a pass gate structure (190b) that does not operate as an actual transistor.
[0034] The first gate structure (190) may include a gate insulating film (192), a gate electrode (194), and a capping pattern (196).
[0035] First and second impurity regions (120a, 120b) provided as source / drain regions may be provided on the upper portion of the first active pattern (130) adjacent to both sides of the first gate structure (190). The first and second impurity regions (120a, 120b) may be provided on the upper portion of the first active pattern (130) between the first gate structures (190). The first gate structure (190) and the first and second impurity regions (120a, 120b) may be provided as recessed channel transistors, which are select transistors of memory cells.
[0036] The first impurity region (120a) may be located at the center of the long axis direction of the first active pattern (130), and the second impurity region (120b) may be located at both edges of the long axis direction of the first active pattern (130).
[0037] A first insulating pattern (210) and a second insulating pattern (212) may be laminated on the substrate (100) of the memory cell region (A), the first device isolation pattern (170a), and the first gate structure (190). For example, the first insulating pattern (210) may include an oxide such as silicon oxide, and the second insulating pattern (212) may include a nitride such as silicon nitride.
[0038] In the memory cell region (A) above, a recess may be included in a portion of the substrate (100) where the first insulating pattern (210) and the second insulating pattern (212) are not formed. The upper surface of the first impurity region (120a) may be exposed on the bottom surface of the recess.
[0039] The barrier impurity region (140) may be provided as a barrier to prevent charges that have moved to the first active pattern (130) from flowing out below the main gate structure (190a). Therefore, the bottom surface of the barrier impurity region (140) may be located lower than the bottom surface of the first gate structure (190). For example, the barrier impurity region (140) may extend from the top surface of the first active pattern (130) to below the bottom surface of the first device isolation pattern (170a). The barrier impurity region (140) may be positioned to overlap with a portion of the first and second impurity regions (120a, 120b).
[0040] In the memory cell region (A), a bit line structure (226) may be provided on the second insulation pattern (212) and the recess. The bit line structure (226) may be electrically connected to the first impurity region (120a).
[0041] The bit line structure (226) may include a first conductive pattern (220), a first barrier metal pattern (not shown), a first metal pattern (222), and a first hard mask pattern (224).
[0042] The first conductive pattern (220) may include, for example, impurity-doped polysilicon. The first barrier metal pattern may include, for example, tungsten nitride, titanium nitride, titanium, tantalum nitride, tantalum, or TiSiN. The first metal pattern (222) may include, for example, tungsten. The first hard mask pattern (224) may include, for example, silicon nitride.
[0043] The bit line structure (226) may be extended in the second direction and may be formed in multiple numbers along the first direction. In exemplary embodiments, a spacer (not shown) may be provided on the side wall of the bit line structure (226). Although not shown, the spacer may have a structure in which multiple spacers are stacked laterally.
[0044] A planar-type second gate structure (236) may be provided on the substrate (100) of the above-mentioned core ferri region (B). The second gate structure (236) may have a stacked structure of a gate insulating film pattern (228), a second conductive pattern (230), a second barrier metal pattern (not shown), a second metal pattern (232), and a second hard mask pattern (234). A spacer (240) may be provided on the side wall of the second gate structure (236).
[0045] In an exemplary embodiment, the stacked structure of the first conductive pattern (220), the first barrier metal pattern, the first metal pattern (222), and the first hard mask pattern (224) of the bit line structure (226) and the stacked structure of the second conductive pattern (230), the second barrier metal pattern, the second metal pattern (232), and the second hard mask pattern (234) of the second gate structure (236) may be identical to each other.
[0046] A first interlayer insulating film (not shown) may be provided to fill between the bit line structures (226) and to cover the bit line structures (226) and the second gate structure (236).
[0047] On the memory cell region (A), a contact plug (252) and a landing pad (254) may be provided, which penetrate the first interlayer insulating film, the second insulating pattern (212), and the first insulating pattern (210) to contact the second impurity region (120b). The contact plug (252) may be positioned between the bit line structures (226). The landing pad (254) may be formed on the contact plug (252). An insulating pattern (256) may be provided between the landing pads (254).
[0048] An etch stop layer (260) may be provided on the above-mentioned landing pad (254), insulation pattern (256), and first interlayer insulating film. A capacitor (280) may be provided that penetrates the etch stop layer (260) and contacts the landing pad (254).
[0049] The above etching stop layer (260) may include, for example, silicon nitride, silicon oxynitride, etc.
[0050] The capacitor (280) may include a lower electrode (270), a dielectric film (272), and an upper electrode (274). The bottom surface of the lower electrode (270) may come into contact with the landing pad (254). Thus, the capacitor (280) may be electrically connected to the second impurity region (120b).
[0051] In an exemplary embodiment, the lower electrode (270) may comprise titanium nitride (TiN) or titanium (Ti). In an exemplary embodiment, the dielectric film (272) may comprise a metal oxide having a high dielectric constant, for example, the dielectric film (272) may be HfO2, ZrO2, TiO2, TaO, or ,It may include La2O3. The upper electrode (274) may include, for example, at least one selected from titanium nitride (TiN), titanium (Ti), tantalum (Ta), tantalum nitride (TaN), ruthenium (Ru), tungsten, tungsten nitride, Nb, NbN, ITO (indium tin oxide), Ta-doped SnO2, Nb-doped SnO2, Sb-doped SnO2, and V-doped SnO2.
[0052] The operation of a memory cell of a DRAM device having the above structure is described below.
[0053] First, the main gate structure (190a) of the recessed channel transistor corresponding to the selected memory cell is turned on, and charge can be charged to the capacitor (280) electrically connected to the recessed channel transistor. Afterward, the main gate structure (190a) is turned off, and data can be written by the charge charged to the capacitor (280).
[0054] Meanwhile, a pass gate structure (190b) may be provided within the first device isolation pattern (170a) which is positioned adjacent to the first active pattern (130) of the selected memory cell. As the DRAM device is integrated, the pass gate structure (190b) is positioned adjacent to the second impurity region (200b) of the first active pattern (130), and accordingly, the pass gate structure (190b) can perform a disturbance operation that turns on and off similarly to an actual transistor.
[0055] In this way, when the interference transistor by the pass gate structure (190b) is turned on, the charges stored in the capacitor (280) can move to the second impurity region (200b) and the first active pattern (130) below it through the landing pad (254) and the contact plug (252). Additionally, when the interference transistor by the pass gate structure (190b) is turned off, the charges that have moved to the first active pattern (130) area can move back to the capacitor (280) and be charged within the capacitor (280).
[0056] However, the charges may move to the first active pattern (130) between the main gate structure (190a) and the first device isolation pattern (170a), and then flow out from the bottom of the first active pattern (130) to the bottom surface of the main gate structure (190a). In this case, since the charges cannot move back to the capacitor (280), the number of charges stored in the capacitor (280) decreases, and the data stored in the capacitor (280) may change.
[0057] In the case of the memory cell described above, barrier impurity regions (140) may be provided on the first and second sidewalls of the long axis of the first active pattern (130). In some exemplary embodiments, the barrier impurity regions (140) may have a negative charge. Additionally, barrier impurity regions (140) may not be provided on the third and fourth sidewalls of the short axis of the first active pattern (130).
[0058] Accordingly, an electric field is applied so that the charge moved from the capacitor (280) to the first active pattern (130) repels each other from the first and second sidewalls of the long axis of the first active pattern (130), thereby preventing it from flowing out below the bottom surface of the main gate structure (190a) through the first and second sidewalls of the first active pattern (130). Additionally, since barrier impurity regions (140) are not provided on the third and fourth sidewalls of the short axis of the first active pattern (130), an electric field may not be applied to cause the charge moved from the capacitor (280) to the first active pattern (130) to move to the center of the first active pattern (130).
[0059] Therefore, even if charge moves from the capacitor (280) to the first active pattern (130), it does not leak out below the bottom surface of the main gate structure (190a) and can move back to the capacitor (280). Consequently, the data stored in the capacitor (280) can be maintained.
[0060] FIGS. 8 to 21 are cross-sectional and plan views illustrating a method for forming active patterns of a semiconductor device according to an exemplary embodiment.
[0061] FIGS. 8, 9, 11, and FIGS. 13 to 16 are cross-sectional views taken along the III-III' portion of FIG. 1. FIGS. 10 and 12 are plan views of the memory cell region. FIGS. 17 to 21 are cross-sectional views taken along the II' portion and the II-II' portion of FIG. 1.
[0062] Referring to FIG. 8, a substrate (100) is provided, comprising a memory cell region (A), a core periphery region (B), and a boundary region (C) between the memory region (A) and the core periphery region (B). A mask pattern structure (106) for forming a trench is formed on the substrate (100).
[0063] The mask pattern structure (106) formed on the substrate (100) of the memory cell region (A) may cover the area for forming the first active pattern. That is, the area between the mask pattern structures (106) may be the area for forming the first device isolation pattern (170a). The mask pattern structure (106) may cover the entire substrate (100) of the core periphery region (B). Additionally, the mask pattern structure (106) may cover a part of the substrate (100) of the boundary region (C) adjacent to the core periphery region (B) and expose the entire remaining substrate (100) of the boundary region (C).
[0064] In an exemplary embodiment, the mask pattern structure (106) may have a structure in which at least two mask patterns are stacked. At least one pattern included in the mask pattern structure (106) may include a material having a selectivity ratio with respect to the substrate (100). In an exemplary embodiment, the mask pattern structure (106) may have a structure in which a silicon oxide pattern (102) and a polysilicon pattern (104) are stacked.
[0065] In an exemplary embodiment, the mask pattern structure (106) can be formed through a Quadruple Patterning Technique (QPT) process or a Double Patterning Technique (DPT) process.
[0066] A first photoresist film is formed to cover the above mask pattern structure (106). The first photoresist film is patterned through a photolithography process to form a first photoresist pattern (110) that covers the mask pattern structure (106) on the core ferri region (B). At this time, the first photoresist pattern (110) may also be formed on the mask pattern structure (106) that is partially formed on the boundary region (C). Additionally, the first photoresist pattern (110) may not be formed on the substrate (100) of the boundary region (C), the substrate (100) of the memory cell region (A), and the mask pattern structure (106).
[0067] Referring to FIGS. 9 and 10, the upper surface of the substrate (100) is etched using the mask pattern structure (106) and the first photoresist pattern (110) as an etching mask to form trenches.
[0068] By the above process, a first trench (120) and a first active pattern (130) may be formed in the memory cell region (A). A second preliminary trench (122) may be formed in the boundary region (C). At this time, since the substrate (100) of the core ferri region (B) is covered by the mask pattern structure (106) and the first photoresist pattern (110), a trench may not be formed in the core ferri region (B).
[0069] The first active patterns (130) may have an isolated shape with the third direction as the length direction.
[0070] After performing the above etching process, the mask pattern structure (106) on the boundary region (C) and memory cell region (A) may be etched so that only a portion of its thickness remains. However, the mask pattern structure (106) on the substrate (100) of the core ferri region (B) may remain almost intact. The first photoresist pattern (110) may be removed by the above etching process.
[0071] Referring to FIGS. 11 and 12, a barrier impurity region (140) is formed by selectively doping a first impurity onto the first sidewall surface and the second sidewall surface along the long axis of the first active patterns (130) of the memory cell region (A).
[0072] In an exemplary embodiment, the process of doping the first impurity can be performed through a gradient ion implantation process. In the ion implantation process, the first impurity can be doped onto the first sidewall surface of the first active patterns (130) by ion implantation to have a first gradient, and the first impurity can be doped onto the second sidewall surface of the first active patterns (130) by ion implantation to have a second gradient. Accordingly, the first impurity can be doped onto the first and second sidewall surfaces facing each other in the fourth direction of the first active patterns (130).
[0073] The first impurity doped into the barrier impurity region (140) may include germanium or fluorine. In some exemplary embodiments, the barrier impurity region (140) may apply an electric field to prevent electrons moved from the capacitor (280) from moving down to the first gate structure (190) and being lost.
[0074] In each of the first active patterns (130) above, the barrier impurity region (140) is formed on the first and second sidewalls of the long axis, respectively, so that the barrier impurity region (140) can be arranged to face each other in the fourth direction. That is, the barrier impurity region (140) can be formed on the surfaces of both ends of the fourth direction.
[0075] When viewed in a plan view, the first impurity may be doped only in the edge portion of the fourth direction of the first active pattern (130), and the first impurity may not be doped in the center portion of the fourth direction of the first active pattern (130).
[0076] Additionally, the barrier impurity region (140) may not be formed on the third and fourth sidewall surfaces of the short axis of the first active pattern (130). That is, the barrier impurity region (140) may not be formed on the sidewalls of both ends of the third direction of the first active pattern (130).
[0077] When the first impurity is doped into the third and fourth sidewalls in the short-axis direction of the first active pattern (130), the first impurity applies an electric field in the direction of the center of the first active pattern (130), so electrons that have moved from the capacitor (280) may move down to the first gate structure (190) and be lost. Therefore, it is preferable that the barrier impurity region (140) is not formed on the third and fourth sidewalls in the short-axis direction of the first active pattern (130).
[0078] Meanwhile, since the substrate (100) of the above-mentioned core ferri region (B) is covered by the above-mentioned mask pattern structure (106), the above-mentioned first impurity may not be doped.
[0079] Referring to FIG. 13, a preliminary sacrificial layer is formed to completely fill the interior of the first trench (120) and the second preliminary trench (122). At this time, the preliminary sacrificial layer may cover the mask pattern structure (106). Afterward, the preliminary sacrificial layer may be flattened to form a sacrificial layer (150) so that the upper surface of the mask pattern structure (106) is exposed. The flattening process may include an etch-back and / or chemical mechanical polishing process.
[0080] The sacrificial layer (150) may be made of a material that has excellent gap-filling properties and can be easily removed through an etching process. In an exemplary embodiment, the sacrificial layer (150) may be formed using a spin-on hard mask material, silicon nitride, or silicon oxide.
[0081] Referring to FIG. 14, a second photoresist film is formed to cover the mask pattern structure (106) and the sacrificial film (150). The second photoresist film is patterned through a photolithography process to form a second photoresist pattern (160).
[0082] The second photoresist pattern (160) may cover a sacrificial film (150) on a portion of the memory cell region (A) and the boundary region (C) adjacent to the memory cell region (A). The sacrificial film (150) and the mask pattern structure (106) on the remaining portion of the boundary region (C) may be exposed by the second photoresist pattern (160).
[0083] Additionally, the second photoresist pattern (160) can selectively expose the area where the third device isolation pattern (170c) is to be formed on the substrate (100) of the core ferri region (B). That is, the second photoresist pattern (160) can cover the entire area corresponding to the active region in the core ferri region (B).
[0084] Referring to FIG. 15, the second photoresist pattern (160) is used as an etching mask to anisotropically etch the mask pattern structure (106) and the sacrificial film (150).
[0085] Next, the substrate (100) below the mask pattern structure (106) of the core ferri region (B) is etched to form a third trench (124). The portion of the substrate (100) of the core ferri region (B) where the third trench (124) is not formed can be provided as an active region.
[0086] Additionally, in the above etching process, the substrate (100) under the sacrificial film (150) and mask pattern structure (106) of the boundary region (C) may be additionally etched so that a second trench (122a) may be formed in the boundary region (C). In the above etching process, the portion of the sidewall of the preliminary second trench (122) of the boundary region (C) that is doped with a first impurity may be removed.
[0087] When the above etching process is performed, the second photoresist pattern (160) and the mask pattern structure (106) can be mostly removed.
[0088] The second trench (122a) may include a portion already etched in the etching process for forming the first trench (120) and a portion additionally etched in the etching process for forming the third trench (124). In the etching process for forming the third trench (124), the etching rate of the sacrificial film (150) portion may be faster than that of the substrate (100) portion of the boundary region (C). Therefore, the portion of the substrate (100) below the sacrificial film (150) that is additionally etched may have the lowest bottom surface in the second trench (122a).
[0089] In this way, the bottom surface of the second trench (122a) may not be flat and may have a step. In an exemplary embodiment, the bottom surface of the first portion adjacent to the memory cell area (A) in the boundary area (C) may have a first step, the bottom surface of the second portion adjacent to the core ferri area (B) may have a second step, and the bottom surface of the third portion between the first portion and the second portion may have a third step lower than the first and second steps. The step may refer to the height of the upper surface of the bottom surface.
[0090] In the above etching process, the shape of the step on the bottom surface of the second trench (122a) may vary depending on the thickness of the substrate (100) being etched.
[0091] For example, the substrate (100) below the mask pattern structure (106) of the boundary region (C) may be etched to the same depth as the bottom surface of the first trench (120) adjacent to the boundary region (C). In this case, as shown in FIG. 15, the first step and the second step may be substantially the same, and the third step may be lower than the first and second steps.
[0092] As another example, the substrate (100) below the mask pattern structure (106) of the boundary region (C) may be etched to a position higher than the bottom surface of the first trench (120) adjacent to the boundary region (C). In this case, as shown in FIG. 6, the second step may be higher than the first step, and the third step may be lower than the first and second steps.
[0093] As another example, the substrate (100) below the mask pattern structure (106) of the boundary region (C) may be etched to a position lower than the bottom surface of the first trench (120) adjacent to the boundary region (C). In this case, as shown in FIG. 7, the second step may be lower than the first step, and the third step may be lower than the first and second steps.
[0094] Referring to FIG. 16, the sacrificial membrane (150) is removed. Additionally, the remaining mask pattern structure (106) is removed.
[0095] By forming an insulating film inside the first to third trenches (120, 122a, 124), first to third element isolation patterns (170a, 170b, 170c) are formed inside the first to third trenches (120, 122a, 124), respectively.
[0096] The following description refers to the cross-sectional views taken of II' and II-II' in FIG. 1.
[0097] Referring to FIG. 17, the upper portion of the first active pattern (130) and the first device isolation pattern (170a) of the memory cell region (A) is etched to form a gate trench (180) extending in the first direction. A first gate structure (190) is formed inside the gate trench (180).
[0098] N-type impurities are doped onto the upper portions of the first active pattern (130) on both sides of the first gate structure (190) to form first and second impurity regions (200a, 200b). The first and second impurity regions (200a, 200b) can be provided as the source / drain of a recessed channel transistor. The first impurity region (200a) may be located at the center portion along the long axis of the first active pattern (130), and the second impurity region (200b) may be located at both edge portions along the long axis of the first active pattern (130).
[0099] The first gate structure (190) may include a gate insulating film (192), a gate electrode (194), and a capping pattern (196). The first gate structure (190) disposed within the first active pattern (130) may be provided as a main gate structure (190a) of the recessed channel transistor included in the memory cell. The first gate structure (190) disposed within the first device isolation pattern (170a) may be provided as a pass gate structure (190b) that does not operate as an actual transistor.
[0100] Referring to FIG. 18, a first insulating pattern (210) and a second insulating pattern (212) can be formed on the substrate (100), first to third device isolation patterns (170a, 170b, 170c), and a first gate structure (190). A recess (not shown) may be formed in some parts of the substrate (100) where the first insulating pattern (210) and the second insulating pattern (212) are not formed. The upper surface of the first impurity region (200a) may be exposed on the bottom surface of the recess.
[0101] A bit line structure (226) extending in a second direction is formed on the second insulation pattern (212) and recess of the memory cell region (A). The bit line structure (226) can be electrically connected to the first impurity region (120a). Additionally, a planar-type second gate structure (236) is formed on the substrate (100) of the core ferri region (B).
[0102] The bit line structure (226) may have a stacked structure of a first conductive pattern (220), a barrier metal pattern (not shown), a first metal pattern (222), and a first hard mask pattern (224). The second gate structure (236) may have a stacked structure of a gate insulating film pattern (228), a second conductive pattern (230), a second barrier metal pattern (not shown), a second metal pattern (232), and a second hard mask pattern (234).
[0103] In exemplary embodiments, a spacer (240) may be formed on the side wall of the bit line structure (226) and the side wall of the second gate structure (236).
[0104] An impurity region (242) can be formed on the substrate (100) of the core ferri region (B) adjacent to both sides of the second gate structure (236).
[0105] Referring to FIG. 19, a first interlayer insulating film (250) is formed covering the bit line structures (226) and the second gate structure (236).
[0106] By etching a portion of the first interlayer insulating film (250) between the bit line structures (226), a contact hole is formed that exposes a second impurity region (200b) of the substrate (100). A contact plug (252) and a landing pad (254) are formed to fill the inside of the contact hole. An insulating pattern (256) is formed between the landing pads (254).
[0107] Referring to FIG. 20, an etch stop layer (260) is formed on the first interlayer insulating film (250), landing pad (254), and insulating pattern (256). The etch stop layer (260) may include, for example, silicon nitride, silicon oxynitride, etc.
[0108] A mold film (262) is formed on the etch stop film (260). The mold film (262) and the etch stop film (260) are anisotropically etched to form holes for forming a capacitor. The upper surface of the landing pad (254) may be exposed on the bottom surface of the holes. The holes may be arranged in a honeycomb structure located at the vertices and center of the hexagon, respectively.
[0109] A lower electrode film is formed on the mold film (262) to completely fill the inside of the holes. In an exemplary embodiment, the lower electrode film may include titanium nitride (TiN) or titanium (Ti). Afterward, the lower electrode film is etched back to form a lower electrode (270) inside the holes.
[0110] Referring to FIG. 21, the mold film (262) is removed. The removal process includes an isotropic etching process, and may include, for example, a wet etching process.
[0111] A dielectric film (272) is formed on the surface of the lower electrode (270) and on the etching stop layer (260). The dielectric film (272) may include a metal oxide having a high dielectric constant, for example, the dielectric film (272) may be HfO2, ZrO2, TiO2, TaO, or , La2O3 may be included. An upper electrode (274) is formed on the dielectric film (272). Thus, a capacitor (280) comprising a lower electrode (270), a dielectric film (272), and an upper electrode (274) may be formed. The capacitor (280) may be electrically connected to the second impurity region (120b).
[0112] A DRAM device can be manufactured by the above process. In the DRAM device, the barrier impurity region (140) may be formed on the first and second sidewall surfaces along the long axis of the first active pattern (130) of the memory cell region (A). Accordingly, even if the charge stored in the capacitor (280) moves to the first active pattern (130) through the landing pad (254) and the contact plug (252), the barrier impurity region (140) can prevent the charge from moving and being lost below the bottom surface of the first gate structure (190). Therefore, the operational failure of the memory cell of the DRAM device can be reduced.
[0113] FIG. 22 is a cross-sectional view showing the active patterns and device isolation patterns of the memory cell region, core region, and boundary region of a DRAM device according to exemplary embodiments.
[0114] The DRAM device described below may have the same structure as the DRAM device described with reference to FIGS. 1 and 2. However, only the shape of the step on the bottom surface of the second trench of the boundary region differs. Therefore, the step on the bottom surface of the second trench of the boundary region will be described mainly.
[0115] Referring to FIG. 22, the bottom surface of the second trench (322a) may not be flat and may have a step. The second trench (322a) may include a first portion adjacent to the memory cell area (A) in the boundary area (C) and a second portion adjacent to the core periphery area (B) in the boundary area (C).
[0116] In an exemplary embodiment, in the boundary region (C), the bottom surface of the first portion may have a first step, and the bottom surface of the second portion may have a second step lower than the first step. Accordingly, the bottom surface of the second trench (322a) may have a stepped shape when viewed in cross-section.
[0117] The DRAM device illustrated in FIG. 22 can be formed in a manner similar to the method of manufacturing the DRAM device described with reference to FIG. 8 to FIG. 21. However, the position of the etching mask may differ slightly.
[0118] FIGS. 23 to 26 are cross-sectional views illustrating a method for manufacturing a DRAM device according to exemplary embodiments.
[0119] Referring to FIG. 23, a substrate (100) is provided, comprising a memory cell region (A), a core periphery region (B), and a boundary region (C) between the memory region (A) and the core periphery region (B). A mask pattern structure (306) for forming a trench is formed on the substrate (100).
[0120] The mask pattern structure (306) formed on the substrate (100) of the memory cell region (A) can cover the area for forming the first active pattern. That is, the area between the mask pattern structures (306) may be the area for forming the first device isolation pattern. The mask pattern structure (306) can cover the entire substrate (100) of the core ferri region (B). Additionally, the mask pattern structure (106) can expose the entire substrate (100) of the boundary region (C).
[0121] Afterwards, a first photoresist pattern (110) is formed to cover the mask pattern structure (306) on the core ferri region. The first photoresist pattern (110) may not be formed on the substrate (100) and the mask pattern structure (306) on the boundary region (C) and the memory cell region (A).
[0122] Referring to FIG. 24, the upper surface of the substrate (100) is etched using the mask pattern structure (306) and the first photoresist pattern (110) as an etching mask to form trenches.
[0123] By the above process, a first trench (120) and a first active pattern (130) may be formed in the memory cell region (A). A preliminary second trench (322) may be formed in the boundary region (C). At this time, since the substrate (100) of the core ferri region (B) is covered by the mask pattern structure (106) and the first photoresist pattern (110), a trench may not be formed in the core ferri region (B).
[0124] Afterwards, a barrier impurity region (140) is formed by selectively doping the first and second sidewall surfaces of the long axis of the first active patterns (130) of the memory cell region (A).
[0125] At this time, the barrier impurity region (140) may also be formed on the side wall of the preliminary second trench (322) adjacent to the core ferry region (B).
[0126] Referring to FIG. 25, a preliminary sacrificial membrane is formed to completely fill the interior of the first trench (120) and the preliminary second trench (322). Afterward, the preliminary sacrificial membrane can be flattened to form a sacrificial membrane (150) so that the upper surface of the mask pattern structure (306) is exposed.
[0127] A second photoresist film is formed to cover the mask pattern structure (306) and the sacrificial film (150). The second photoresist film is patterned through a photolithography process to form a second photoresist pattern (160).
[0128] The second photoresist pattern (160) may cover a sacrificial film (150) on a portion of the memory cell region (A) and the boundary region (C) adjacent to the memory cell region (A). The sacrificial film (150) and the mask pattern structure (306) on the remaining portion of the boundary region (C) may be exposed by the second photoresist pattern.
[0129] Additionally, the second photoresist pattern (160) can selectively expose the area where the third device isolation pattern is to be formed on the substrate of the core ferri region (B). That is, the second photoresist pattern (160) can cover the entire area corresponding to the active region in the core ferri region (B).
[0130] Referring to FIG. 26, the second photoresist pattern (160) is used as an etching mask to anisotropically etch the mask pattern structure (106) and the sacrificial film (150).
[0131] Next, the substrate (100) below the mask pattern structure (106) of the core ferri region (B) is etched to form a third trench (124). The portion of the substrate (100) of the core ferri region (B) where the third trench (124) is not formed can be provided as an active region.
[0132] In addition, in the above etching process, the sacrificial film (150) of the boundary region (C) and the substrate (100) below the sacrificial film may be additionally etched so that a second trench (322a) may be formed in the boundary region (C).
[0133] The second trench (322a) may include a portion already etched in the etching process for forming the first trench (120) and a portion etched in the etching process for forming the third trench (124).
[0134] As such, the bottom surface of the second trench (322a) may not be flat and may have a step. In an exemplary embodiment, the second trench (322a) may include a first portion adjacent to the memory cell area (A) in the boundary area (C) and a second portion adjacent to the core periphery area (B) in the boundary area (C).
[0135] In an exemplary embodiment, in the boundary region (C), the bottom surface of the first portion may have a first step, and the bottom surface of the second portion may have a second step lower than the first step. Accordingly, the bottom surface of the second trench (322a) may have a stepped shape when viewed in cross-section.
[0136] Afterwards, a DRAM device can be manufactured by performing the same process as described with reference to FIGS. 16 to 21. Explanation of the symbols
[0137] 100 : Substrate 120 : 1st trench 122a : 2nd Trench 124 : 3rd Trench 130: First active pattern 120a: First impurity region 120b: Second impurity region 140: Barrier impurity region 170a: First element isolation pattern 170b: Second element isolation pattern 170c: Third device isolation pattern 190: First gate structure 236 : Second gate structure 280 : Capacitor
Claims
Claim 1 A semiconductor device comprising: a first active pattern having an isolated shape that is included on the substrate of a memory cell region, includes single-crystal silicon, and extends such that a direction oblique to a first direction becomes the long axis direction; a first device isolation pattern provided within a first trench included in the substrate of the memory cell region and covering the sidewall of the first active pattern; a first gate structure provided inside a gate trench extending in the first direction above the first active pattern and the first device isolation pattern; a barrier impurity region selectively formed only on the surface of both sidewalls of the long axis of the first active pattern; and first and second impurity regions provided above the first active pattern adjacent to both sides of the first gate structure. Claim 2 delete Claim 3 In claim 1, the impurity included in the barrier impurity region is a semiconductor device comprising germanium or fluorine. Claim 4 A semiconductor device according to claim 1, wherein the barrier impurity region is not formed on the sidewall of the short axis. Claim 5 A semiconductor device according to claim 1, wherein the bottom surface of the barrier impurity region is positioned lower than the bottom surface of the first gate structure. Claim 6 A semiconductor device according to claim 1, wherein the barrier impurity region extends from the upper surface of the first active pattern to below the lower surface of the first device isolation pattern. Claim 7 A semiconductor device according to claim 1, wherein two first gate structures are spaced apart from each other in a first active pattern, and one first gate structure is disposed in each of the first device isolation patterns that contact both ends in the long axis direction of the first active pattern. Claim 8 A semiconductor device according to claim 1, wherein the first impurity region is located at the center of the long axis direction of the first active pattern and the second impurity region is located at both edges of the long axis direction of the first active pattern, and further comprising a bit line structure electrically connected to the first impurity region; and a capacitor electrically connected to the second impurity region. Claim 9 A semiconductor device according to claim 1, wherein the substrate of the boundary region in contact with the edge of the memory cell region includes a second trench, and a second element isolation pattern filling the interior of the second trench is provided, and the bottom surface of the second trench is not flat and has a step. Claim 10 A semiconductor device comprising: a substrate including a memory cell region, a core ferri region, and a boundary region between the memory cell region and the core ferri region, and including single-crystal silicon; a first active pattern and a first device isolation pattern provided on the substrate of the memory cell region; a second device isolation pattern filling the interior of a second trench included in the substrate of the boundary region between the memory cell region and the core ferri region; a third device isolation pattern filling the interior of a third trench included in the substrate of the core ferri region; a first gate structure provided in a gate trench extending in a first direction on the upper portion of the first active pattern and the first device isolation pattern; a barrier impurity region selectively formed only on the surface of both sidewalls of the long axis of the first active pattern; and first and second impurity regions provided on the upper portion of the first active pattern adjacent to both sides of the first gate structure, wherein the bottom surface of the second trench is not flat and has a step.
Citation Information
Patent Citations
Semiconductor device having a device isolation structure
KR1020110052206A
Semiconductor devices and methods of manufacturing the same
KR1020140062601A
Semiconductor device and method for fabricating the same
KR1020210047032A