Casting Method and Casting Apparatus for DC casting
Patent Information
- Application Number
- NO20190143
- Authority / Receiving Office
- NO · NO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2019-02-01
- Publication Date
- 2020-08-03
- Estimated Expiration
- 2039-02-01
AI Technical Summary
The semi-continuous DC casting process is plagued by 'bleed-out' phenomena, where molten metal spills out uncontrollably from the mold, posing risks to personnel and causing equipment damage, with the underlying mechanisms not fully understood.
A method and apparatus that utilize a thermal camera to record temperature ranges of the cast product, determining peak temperatures and controlling the casting process by adjusting metal supply and starter block movement, with defined temperature ranges for normal operation, maintenance, and emergency shutdown to prevent bleed-outs.
The solution effectively reduces the risk of bleed-outs, ensuring safer operations and minimizing equipment damage by automatically or manually aborting the process when critical temperature thresholds are exceeded, thereby enhancing the efficiency and reliability of the DC casting process.
Abstract
Description
Casting Method and Casting Apparatus for DC castingTechnical FieldThe present invention relates to an apparatus and a method for the efficient casting of longitudinal cast products such as rolling ingots or extrusion ingots or forging stockTechnical BackgroundCasting of longitudinal casting products is carried out using a direct chill (DC) casting apparatus. Such a DC casting apparatus comprises a mold that is configured to at least partially solidify molten metal that is introduced into the mold via a top opening. The at least partially solidified molten metal, which corresponds to the cast product, exits the mold via a bottom opening and is supported by a vertically moveable starter block. Thelongitudinal cast product is produced by continuously supplying molten metal into mold while moving the starter block that supports the cast product produced from the molten metal vertically downwards. A cast product may for example have a length of 1 to 5 meter, although the cast product may have any length. After casting a cast product, the flow of molten metal into the mold is interrupted, the cast product is removed from the starter block, and the starter block is moved vertically upwards to close the bottom opening of the mold. Starting from this configuration, the next cast product can be cast.As each cast product individually is cast in a continuous steady-state manner and as thereare interruptions between casting of subsequent cast products, the process is referred to as a “semi-continuous casting process”. In the following, it will also be referred to as “DC casting” or “casting”. A slab or rolling slab is a cast product that is subsequently used in rolling process to e.g. produce foil or sheet metal and the like and that may have a rectangular cross-section. An extrusion billet is a cast product that is subsequently used for extrusion and may have a circular cross-section. However, the cast products producible by DC casting are not limited to subsequent use for rolling or extrusion bumay also be used for forging or other forming methods.A common problem during DC casting is a phenomenon known as “bleed-out”. A bleeout occurs when the molten metal spills out of the bottom opening of the mold in uncontrolled and undesired manner. A bleed-out may put personnel at risk and alsomight permanently damage the casting apparatus and cause production down-time. Figure 1 shows a visible-light image of a bleed-out in a DC casting apparatus while casting of a cast product that is intended to have a circular cross-section. So far, the reasons and mechanisms that lead to a bleed-out have not been fully established.Short Description of the InventionIt is an objective of the present invention to enable a more efficient semi-continuous casting process. To solve this and other objects, the present invention provides a methofor casting longitudinal cast products comprising: casting longitudinal cast products in semi-continuous manner using a DC casting apparatus having a mold, wherein the moldhas top and bottom openings and is configured to at least partially solidify molten metathat is entered into the mold via the top opening and to output the cast product via thbottom opening, recording a thermal image of the cast product that is output via the bottom opening, determining at least three non-overlapping temperature ranges comprising a first temperature range, a second temperature range and a third temperature range, determining a peak temperature in the thermal image; comparing the peak temperature with the at least three temperature ranges; and a.) when the peak temperature is comprised in the first temperature range, casting the cast product, b.) when the peak temperature is comprised in the second temperature range, displaying an information indicative of a maintenance requirement of the casting apparatus and carrying out maintenance of the casting apparatus after the cast product is cast and before a subsequent casting operation is carried out, c.) when the peak temperature is comprised in the third temperature range, aborting the casting of the currently cast cast product and displaying an information indicative of an emergency shutdown. Accordembodiments of the method, the aborting may be carried out automatically (e.g. using an electronic control unit). According to embodiments of the method according to the invention, the aborting may be carried out by an operator (that is, by a person) based on the displaying of the information indicative of an emergency shutdown. According toembodiments, the invention provides an apparatus for carrying out the method descriherein.According to embodiments of the method according to the invention, the first temperature range comprises temperatures up to but not including 70°C.According to embodiments of the method according to the invention, the second temperature range comprises temperatures between 70°C and 90°C.According to embodiments of the method according to the invention, the third temperature range comprises temperatures higher than and not including 90°C.According to a further aspect, the invention provides a aasting apparatus for semi- continuous direct chill casting of longitudinal cast products comprising a mold havingmold cavity and a top opening and a bottom opening that are in fluid communicationwith the mold cavity, wherein the mold is configured to at least partially solidify molten metal that is supplied into the mold cavity, a metal supply system for selectively supplying molten metal from a reservoir into the mold cavity via the top opening, a starter block that is configured such as to be vertically moveable between a high positionin which it closes the bottom opening of the mold and a low position, and wherein a caproduct is produced by vertically moving the starter block from the high position to low position while supplying molten metal into the mold cavity, a thermal camera, that is configured to record a thermal image of the cast product while the starter block is movedfrom the high position to the low position, an electronic control system that is configuto determine a peak temperature in the thermal image and compare the determined peak temperature with at least a first temperature range, a second temperature range and a third temperature range, to control metal supply via the metal supply system and to control a vertical movement of the starter block, an information output system for outputting an information, wherein the electronic control system controls the metal supply system and the starter block such as to produce a cast product when the peak temperature is comprised in the first temperature range, wherein the electronic control system controls the metal supply system and the starter block such as to produce a cast product and controls the information output system to output an information indicathat maintenance of the casting apparatus is necessary when the peak temperature is comprised in the second temperature range, wherein the electronic control system controls the metal supply system to stop supply of molten metal from the reservoir into the mold cavity such as to abort casting of the cast product, when the peak temperature comprised in the third temperature range.According to embodiments of the invention, the first temperature range comprises temperatures up to but not including 70°C.According to embodiments of the invention the second temperature range comprises temperatures between 70°C and 90°C.According to embodiments of the invention the third temperature range comprises temperatures higher than and not including 90°C.Short Description of the FiguresFig. 1 shows a bleed-out in a DC casting apparatus during casting of a cast product.Fig. 2 shows a schematic view of a DC casting apparatus according to embodiments of the invention for carrying out the method according to the invention.Fig. 3 shows a thermal image of a cast product shortly before a bleed out occurs.Detailed descriptionWith reference to Fig. 2, a DC casting apparatus 10 according to embodiments of the invention comprises a mold 30.The mold 30 has a top opening 31 and a bottom opening 32 and a mold cavity 33 thafluid communication with the top and bottom openings 31,32. The mold 30 may furthcomprise a cooling jacket 34 for circulating a cooling medium such as water. The cooling jacket 34 may serve to remove heat from the mold cavity 33 via heat conduction from thmold cavity into the cooling medium which transports heat away, e.g. to a heat exchang(not shown).The casting apparatus 10 further comprises a starter block 50. The starter block 50 is arranged such as to be able to selectively open or close the bottom opening 32 of the mold 30 by a vertical movement of the starter block 50. The starter block 50 is arranged below the bottom opening 32 and is vertically moveable to close the bottom opening (when it is in its top most position) and to open the bottom opening 32, (when it is movertically downwards). The double arrow in Fig. 2 indicates the vertical movability of thestarter block 50.The DC casting apparatus 10 further comprises a metal supply system 70 configured to supply liquid metal, in particular molten aluminium or molten aluminium alloy, from a reservoir, such as a melting furnace or crucible, into the mold cavity 33 via the top opening 31 of the mold 30. The metal supply system 70 may comprise means 75 for stopping the metal flow into the mold cavity 33. The means 75 for stopping the metal flow may for example be implemented as a valve, e.g. a gate valve or dam or as an opening-plug-combination, provided on a conduit connecting the reservoir and thcavity 33 as shown in Fig. 2. The means 75 may also be implemented in other ways, e.g. via an electro-magnetic field that counters flow of liquid metal into the mold 33, or the like.A casting operation using the casting apparatus 10 is carried out as follows. In the initial state, the starter block is in the top position such as to close the bottom opening 32 of tmold 30. Then, liquid metal is introduced into the mold cavity 33 via the metal supply system 70. The liquid metal is at least partially solidified by a heat transfer from the metal into the mold 30, e.g. the cooling jacket 34 thereof. At the same time, the starter block 50 is moved vertically downwards while liquid metal is continuously supplied into the moldcavity 33 via the metal supply system 70. In this way, a longitudinal cast product 90 is produced in a continuous manner. When the casting of the cast product 90 is finished,the supply of liquid metal into the mold cavity 33 is interrupted and the vertical movement of the starter block 50 is stopped. Then, the cast product 90 is removed from the starter block 50. The empty starter block 50 is then moved vertically upwards such as to close the bottom opening 32 of the mold 30 and to bring the casting apparatus 10 inthe initial state again. From this state, the next cast product 90 may be cast. With respect to terminology, the casting of a cast product 90 is referred to as “continuous casting” as the casting is carried out in a steady-state manner (“dynamic equilibrium”) while the subsequent casting of several cast products 90 is referred to as “semi-continuous” castingor the like, as there is a discontinuity between casting of subsequent cast products 90 when the starter block 50 is moved upwards to the top position.The present inventors have found and confirmed by experiments that the bleed-out phenomenon is related to a temperature increase on the surface of the cast product 90 exiting the bottom opening 32 of the mold 30. The present inventors have also foundcauses for a temperature increase on the surface of a cast product 90 and present a method and an apparatus for casting that allows efficient casting with no or at least a reduced risk for bleed-outs and related injuries and damages.Accordingly, the DC casting apparatus 10 further comprises a thermal imaging device or thermal camera 80 that is configured to record a thermal image (or a thermal vision video) of the cast product 90 during casting. A thermal image recorded by the thermal camera 80 may for example be an image of pixels arranged in a matrix (for example 320 columns and 240 rows or 1920 columns and 1080 rows), wherein a value of each pixel corresponds to thermal radiation that is incident on the thermal camera 80 on the corresponding location. The value of a pixel corresponds to the temperature of the recorded object. To record the thermal image, the thermal camera 80 may for example comprise a CCD detector. An example for a thermal camera 80 that can be used according to the present invention is for example the camera FLIR GF309 obtainable from FLIR Systems, Wilsonville, Oregon, USA. However, also other commercially available thermal cameras can be used as a thermal camera 80 according to the invention. The thermal camera 80 is arranged such that it records a thermal image of the cast product 90 exiting the bottom opening 33 of the mold 30. An example of a thermal imagerecorded using a thermal camera 80 according to the invention is shown in Fig. 3.The thermal camera 80 is connected to or comprises an electronic control system 100. The electronic control system 100 may be a computer, such as a standard PC. The electronic control system 100 may control the full operation of the cast apparatus 10. The electronic control system 100 determines a peak temperature of the cast product 90 that has exited the bottom opening 32 during a casting operation from the thermal image recorded by the thermal camera 80. The peak temperature is correspondingly the recorded maximum temperature of the cast product 90. The electronic control system 100 may according to embodiments also be connected to the metal supply system 70, e.g. the means 75 for stopping metal supply thereof. The electronic control system 100 is connected to an information output system (not shown), for example a computer displthat can display information, a warning lamp, an audio alarm, or the like. To determine the peak temperature, any suitable algorithm may be used. A very simple algorithm to determine the peak temperature may comprises iterating over all the rows and columns of pixels forming the thermal image and comparing a present value with a previous valueand when the present value is higher than the previous value, replacing the previous value with the present value. The final value when the iteration over all rows and columns took place corresponds in this case to the peak temperature. However, depending on the conditions, also other algorithms may be used.The electronic control system 100 is configured to execute the following actions depending on the maximum temperature that is determined by the electronic control system 100 based on the thermal image recorded by the thermal camera 80. When the maximum temperature falls within a first temperature range, no additional action is taken, and the casting operation is executed in a semi-continuous manner as described above. When the maximum temperature falls within a second temperature range, the casting process for the presently cast cast product 90 is carried out normally, but a signal is sent to the information output system that indicates that maintenance of the casting apparatus 10 is necessary. When the maximum temperature falls within the third temperature range, a corresponding signal is sent to the information output system andthe currently carried out cast process is interrupted, e.g. automatically or by an operator, by interrupting the metal flow into the mold cavity 33. The third temperature range is higher than the second temperature range and the second temperature range is higher than the first temperature range, wherein none of the temperature ranges are overlapping. The first temperature range is also referred to as the normal operation temperature range, the second temperature range is also referred to as the maintenance required temperature range and the third temperature range is also referred to as the emergency shutdown temperature range. By careful analysis and experimentation, the present inventors have found that in the case of casting of aluminium or aluminium alloy(an aluminium alloy as described herein is an alloy comprising at least 70wt-% Al), the following temperature ranges using an emissivity of 1 for the thermal image may be used for efficient casting that safely prevents bleed-out:First temperature range: up to 70°C: normal operationSecond temperature range 70 to 90°C: maintenance requiredThird temperature range: higher than 90°C: emergency shutdown temperatureHowever, the temperatures may be optimized and adapted according to the used castingapparatus 10, the casting parameters, the alloy, the cast house temperature, cast dimensions, etc.The inventors have found that the following maintenance should be carried out on thcasting apparatus 10 when the peak temperature is in the maintenance required temperature range or in the emergency shutdown temperature range. In particular, two types of maintenance may be carried out according to the invention: a.) it should be ensured that the cooling medium supply is sufficient, and b.) it should be ensured thatwall of the mold 30 that enclosed the mold cavity 33 is free of contaminants. With respect to a.), for example, the flow rate may be limited by dirt that accumulates in the cooling jacket of the mold 30. With respect to b.), it has been found that often metal residue or other dirt on the wall of the mold 30 that surrounds the mold cavity 33 results in hotspots on the cast products 90 that in turn develop into a bleed-out. Accordingly, castinaccording to the present invention may involve removing dirt from the cooling jacketand / or cleaning the wall of the mold 30 when the peak temperature is in the second temperature range or the third temperature range.
Claims
1. Method for casting longitudinal cast products (90) comprising:casting longitudinal cast products (90) in a semi-continuous manner using a DC casting apparatus (10) having a mold (30), wherein the mold (30) has top (31) and botto(32) openings and is configured to at least partially solidify molten metal that is entered into the mold (30) via the top opening (31) and to output the cast product (90) via thebottom opening (32),recording a thermal image of the cast product (90) that is output via the bottom opening (32),determining at least three non-overlapping temperature ranges comprising a first temperature range, a second temperature range and a third temperature range, determining a peak temperature in the thermal image;comparing the peak temperature with the at least three temperature ranges; anda. ) when the peak temperature is comprised in the first temperature range, casting the cast product (90),b. ) when the peak temperature is comprised in the second temperature range, displaying an information indicative of a maintenance requirement of the casting apparatus (10) and carrying out maintenance of the casting apparatus (10) after the cast product (90) is cast and before a subsequent casting operation is carried out,c. ) when the peak temperature is comprised in the third temperature range, aborting the casting of the currently cast cast product (90) and displaying an information indicative of an emergency shutdown.
2. Method according to claim 1, wherein the first temperature range comprises temperatures up to but not including 70°C.
3. Method according to any preceding claim, wherein the second temperature range comprises temperatures between 70°C and 90°C.
4. Method according to any preceding claim, wherein the third temperature range comprises temperatures higher than and not including 90°C.
5. Method according to any previous claim, wherein the aborting the casting of the currently cast cast product (90) comprises stopping entering molten metal into the mold(30).
6. Casting apparatus (10) for semi-continuous direct chill casting of longitudinal cast products (90) comprisinga mold (30) having a mold cavity (33) and a top opening (31) and a bottom openi(32) that are in fluid communication with the mold cavity (33), wherein the mold (30) is configured to at least partially solidify molten metal that is supplied into the mold cavity(33) ,a metal supply system (70) for selectively supplying molten metal from a reservoir into the mold cavity (33) via the top opening (31),a starter block (50) that is configured such as to be vertically moveable between a high position in which it closes the bottom opening (32) of the mold (30) and a low position, and wherein a cast product (90) is produced by vertically moving the starter block (50) from the high position to the low position while supplying molten metal inthe mold cavity (33),a thermal camera (80), that is configured to record a thermal image of the cast product (90) while the starter block (50) is moved from the high position to the low position,an electronic control system (100) that is configured to determine a peak temperature in the thermal image and compare the determined peak temperature with at least a first temperature range, a second temperature range and a third temperature range, to control metal supply via the metal supply system and to control a vertical movement of the starter block (50),an information output system for outputting an information,wherein the electronic control system (100) controls the metal supply system (70) and the starter block (50) such as to produce the cast product (90) when the peak temperature is comprised in the first temperature range,wherein the electronic control system (100) controls the metal supply system (70) and the starter block (50) such as to produce the cast product (90) and controls the information output system to output an information indicating that maintenance of thcasting apparatus (10) is necessary when the peak temperature is comprised in the second temperature range,wherein the electronic control system (100) controls the metal supply system (70) to stop supply of molten metal from the reservoir into the mold cavity (33) such as to abort casting of the cast product (90), when the peak temperature is comprised in the third temperature range.
7. Casting apparatus (10) according to claim 6, wherein the first temperature range comprises temperatures up to but not including 70°C.
8. Casting apparatus (10) according to claim 6 or 7, wherein the second temperature range comprises temperatures between 70°C and 90°C.
9. Casting apparatus (10) according to any of claims 6 to 8, wherein the third temperature range comprises temperatures higher than and not including 90°C.Fig. 180Fig. 2Fig. 3
Citation Information
Patent Citations
Active temperature feedback control of continuous casting
EP1849539A1
Method of controlling continuous casting rate
US4306610A
Bleed out detector for direct chill casting
WO1997016273A1
Method and apparatus for controlling the temperature of an ingot during casting, particularly at start-up
WO1998056522A1