Method of welding and heat treatment of welded joints of martensitic steel with boron
PL250580B1Active Publication Date: 2026-11-16POLITECHNA WROCLAWSKA
View PDF 0 Cites 0 Cited by
Patent Information
- Application Number
- PL2023446047
- Authority / Receiving Office
- PL · PL
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-09-06
- Publication Date
- 2026-11-16
- Estimated Expiration
- 2043-09-06
Smart Images

Figure 00000007_0000 
Figure 00000007_0001 
Figure 00000008_0000
Abstract
The subject of the application is a method of welding and heat treatment of martensitic steel with boron, in the context of ensuring ballistic resistance against intermediate ammunition 7.62 x 39 mm nb. pattern 43 with PS class, in which to produce a welded joint a martensitic steel sheet with a thickness of 10 mm and the chemical composition expressed in weight percent: C – 0.17÷0.23; Si – 0.19÷0.32; Mn – 1.00÷1.10; P - max. 0.025; S – max. 0.010; Cr – 0.20÷0.37; Ni - max. 0.10; Mo – 0.05÷0.15; B - max.0.002 with a carbon equivalent CEV≤52, is welded by the SAW method (121) with an S3Ni2.5CrMO electrode wire and MgO+CaF2+Al2O3+SiO2 flux, using the following welding parameters: welding speed v≈60 cm / min, rated electric arc current I=530÷630 A, electric arc voltage U=31÷33 V, linear energy Q≤2.0 kJ / mm, interlayer temperature Ti<250°C, which is characterized in that after welding the sheet is thinned to a thickness of 4 to 5 mm, and the obtained joint is subjected to normalization by austenitizing at a temperature of 880°C÷900°C for 60 minutes and cooling in air; further hardening by austenitizing at 930°C÷950°C for 15÷20 minutes and cooling in water at ≤30°C; and tempering at 100°C for 5 hours, after which the joint is cooled in air.