AI Technical Summary
Existing processes for fabricating 3D integrated circuit devices, such as flip-chip, lack precise control over the separation, relative orientation, and alignment of individual dies, limiting flexibility and component density in qubit chip design.
A method involving etching substrates to form raised and recessed alignment structures on both substrates, positioning them to align oppositely with controlled depth, and bonding using flip-chip bumps or indium films, ensuring precise alignment and orientation through trapezoidal cross-sections and thermocompression bonding.
Enables precise control of die separation and alignment, enhancing flexibility and component density in qubit chip design, facilitating the formation of quantum circuit components like qubits and through-substrate vias.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Chip manufacturing methods and products This invention relates to the field of chip manufacturing, and more particularly to the manufacture of superconducting integrated circuits for use in quantum computers. In 3D integrated circuit devices, integrated circuit components not only occupy a single substrate side but are also distributed on both sides of the substrate and / or on the sides of multiple uniform dies, such as in a stack. The distribution of circuit components on different layers or design surfaces provides greater flexibility and higher component density for qubit wafer design. However, existing processes for manufacturing 3D integrated circuit devices such as flip-chip do not allow for precise control over the separation of individual wafers, the relative orientation (i.e., tilting) of individual wafers, or the alignment (i.e., lateral offset or rotation) of individual wafers. According to a first aspect of the present invention, a method is provided. The method includes: ● etching a first substrate to form a raised alignment structure extending above a first surface of the first substrate; ● etching a second substrate to form a recessed alignment structure extending below the first surface of the second substrate; and ● positioning the raised alignment structure and the recessed alignment structure relative to each other such that the first surface of the first substrate and the first surface of the second substrate are opposite and parallel, and such that the raised alignment structure is at least partially positioned within the recessed alignment structure; ● wherein the raised alignment structure and the recessed alignment structure are shaped such that the raised alignment structure extends at least partially within the recessed alignment structure to a predetermined depth, and such that when the raised alignment structure is positioned within the recessed alignment structure at the predetermined depth, the first substrate is constrained to move toward and relative to the second substrate along at least one axis parallel to the first surfaces of the first substrate and the second substrate. Before positioning the raised alignment structure relative to the recessed alignment structure, the method may further include depositing at least one of the following: ● a plurality of flip-chip bumps on at least one of a first surface of a first substrate or a first surface of a second substrate; or ● an indium film on the raised alignment structure and / or within the recessed alignment structure, and positioning the raised alignment structure relative to the recessed alignment structure further includes bonding the first substrate to the second substrate via the flip-chip bumps or the indium film. Bonding the first substrate to the second substrate may include thermoforming. When the protrusion alignment structure is positioned at a set depth within the recessed alignment structure, the height of the deposited flip-chip bump can be greater than the distance between the first surface of the first substrate and the first surface of the second substrate, and after compression bonding, the protrusion alignment structure can be positioned at a set depth within the recessed alignment structure. The cross-sections of the raised alignment structure and the recessed alignment structure along at least one plane perpendicular to the first surface of each substrate can be trapezoidal, such that the cross-section of the raised alignment structure is a trapezoid extending from the first surface of the first substrate, and the cross-section of the recessed alignment structure is a trapezoid extending into the first surface of the second substrate. The longest base of the raised alignment structure trapezoid can be longer than the longest base of the recessed alignment structure trapezoid, and when the first surface of the first substrate is parallel to the first surface of the second substrate, each waist of the raised alignment structure trapezoid can be parallel to the adjacent waist of the recessed alignment structure trapezoid. The protruding alignment structure and the recessed alignment structure can be isosceles trapezoids. When the protruding alignment structure extends to a set depth within the recessed alignment structure, the distance between the first surface of the first substrate and the first surface of the second substrate... It can be given by the following equation: in Let be the interior angle between the leg and the longest base of each trapezoid. The length of the longest bottom edge of the protrusion aligned with the structure and It is the length of the longest bottom edge of the concave alignment structure. The cross-sections of the protruding alignment structure and the recessed alignment structure along the two vertical planes perpendicular to the first surface of each substrate can be trapezoidal, such that the protruding alignment structure is a square or rectangular frustum extending from the first surface of the first substrate, and the recessed alignment structure is a square or rectangular frustum hollow extending to the first surface of the second substrate. The dimensions of the protruding alignment structure and the recessed alignment structure can conform to the following equation: in This refers to the distance between the first surface of the first substrate and the first surface of the second substrate when the protruding alignment structure extends to a set depth within the recessed alignment structure. It is the interior angle between the waist side and the longest base side of the trapezoid along the first axis parallel to the first surface of the first substrate and the second substrate. The length of the longest base of the trapezoid aligned with the first axis of the protrusion is given. It is the length of the longest base of the trapezoidal alignment structure recessed along the first axis. It is the interior angle between the waist and the longest base of a trapezoid that is parallel to the first surface of the first substrate and the second substrate and perpendicular to the second axis. It is the length of the longest base of the trapezoid along the second axis of the structure aligned with the protrusion, and It is the length of the longest base of the trapezoidal alignment structure recessed along the second axis. Etching a first substrate to form a raised alignment structure may include: ● forming a hard mask or resist on a first region of the first substrate; ● etching the first substrate in an anisotropic manner; and ● removing the hard mask or resist. The size, etching time, and / or etchant concentration of the first area on which a hard mask or resist is formed can be controlled in order to control the size of the trapezoidal / frustum shape of the protrusion alignment structure. Etching a second substrate to form a recessed alignment structure may include: ● forming a hard mask or resist on an upper surface of the second substrate, the hard mask or resist including at least one opening defining an open region of the second substrate; ● etching the second substrate anisotropically through the opening in the hard mask or resist; and ● removing the hard mask or resist. The size of the open area, etching time, and / or etchant concentration on the second substrate can be controlled to control the size of the trapezoidal / frustum shape of the recessed alignment structure. Etching the first substrate to form a raised alignment structure may include forming a plurality of raised alignment structures on the first substrate, and etching the second substrate to form a recessed alignment structure may include forming a plurality of recessed alignment structures on the second substrate. The first substrate may be a die on a first wafer containing multiple dies, and the second substrate may be a die on a second wafer containing multiple dies. Etching the first substrate to form multiple raised alignment structures may include etching the first wafer to form multiple raised alignment structures on each die on the first wafer, and etching the second substrate to form multiple recessed alignment structures may include etching the second wafer to form multiple recessed alignment structures on each die on the second wafer. Etching a first wafer to form a plurality of raised alignment structures may be included in each quadrant of each die on the first wafer to form raised alignment structures and / or etching a second wafer to form a plurality of recessed alignment structures may be included in each quadrant of each die on the second wafer to form recessed alignment structures. Multiple raised alignment structures may be disposed on a first substrate, and multiple recessed alignment structures may be disposed on a second substrate, such that positioning the raised alignment structures and the recessed alignment structures relative to each other includes positioning each raised alignment structure and the recessed alignment structure relative to each other, such that each raised alignment structure extends at least partially within the opposing recessed alignment structure to a predetermined depth. The method may further include forming quantum circuit components on a first substrate and / or a second substrate prior to the step of positioning the protruding alignment structure and the recessed alignment structure relative to each other. Forming a quantum circuit assembly may include: ● forming qubits on a raised alignment structure; ● forming a through-substrate via in a second substrate, the through-substrate via extending from a recessed alignment structure through the second substrate to a second surface of the second substrate; and ● metallizing the sidewalls of the through-substrate via. Positioning the raised alignment structure relative to the recessed alignment structure can create a capacitor between the sidewall metallization through the through-hole in the substrate and the qubits formed on the raised alignment structure. Forming qubits on a raised alignment structure can include forming qubits on the upper surface of the raised alignment structure. Forming a through-substrate via can include forming a hard mask or resist within a recessed alignment portion and etching the through-substrate via an opening in the hard mask or resist. Sidewall metallizations can be formed by chemical vapor deposition or physical vapor deposition before the hard mask or resist is removed. The method may further include: ● forming a plurality of raised alignment structures and a plurality of recessed alignment structures; ● forming qubits on the raised alignment structures, including forming qubits on a first subset of the raised alignment structures; ● forming through-substrate vias, including forming through-substrate vias extending from the first subset of the recessed alignment structures, the first subset of the recessed alignment structures including recessed alignment structures positioned relative to the raised alignment structures in the first subset of the raised alignment structures during the positioning step; and ● depositing a spacer material layer on a second subset of the raised alignment structures and / or the second subset of the recessed alignment structures before positioning the raised alignment structures and the recessed alignment structures relative to each other. After the raised alignment structure and the recessed alignment structure are positioned relative to each other, the distance between the first substrate and the second substrate can be determined at least in part by the thickness of the spacer material layer deposited on the second subset of the raised alignment structure and / or the second subset of the recessed alignment structure. The method may further include forming a metallization around the qubit at least on the sidewall of the raised alignment structure, and positioning the raised alignment structure and the recessed alignment structure relative to each other may further include making the metallization on the sidewall of the through-hole of the substrate electrically contact the metallization on the sidewall of the raised alignment structure. The method may further include: ● forming a plurality of raised alignment structures and a plurality of recessed alignment structures; ● forming qubits on the raised alignment structures, including forming qubits on at least two of the raised alignment structures and forming a coupler on at least one of the raised alignment structures; ● forming a connection element connecting at least two qubits to at least one coupler; ● forming a through-substrate via, including forming a through-substrate via extending from a subset of the recessed alignment structures, the subset of the recessed alignment structures including the recessed alignment structures positioned relative to the raised alignment structures on which the qubits are formed. A qubit can be a Josephson junction-based qubit, such as a transmon qubit. According to a second aspect of the present invention, a product is provided. The product comprises: ● a first substrate having at least one raised alignment structure extending above a first surface of the first substrate; and ● a second substrate having at least one recessed alignment structure extending below the first surface of the second substrate; ● wherein the raised alignment structure and the recessed alignment structure are positioned relative to each other such that the first surface of the first substrate is opposite to and parallel to the first surface of the second substrate, and such that the raised alignment structure is at least partially positioned within the recessed alignment structure; and ● wherein the raised alignment structure and the recessed alignment structure are shaped such that the raised alignment structure extends at least partially within the recessed alignment structure to a predetermined depth, and such that the first substrate is restricted to move toward and relative to the second substrate along at least one axis parallel to the first surfaces of the first substrate and the second substrate. The product may further include: ● a plurality of flip-chip bumps connecting a first surface of a first substrate and a first surface of a second substrate; and / or ● an indium film on a raised alignment structure and / or within a recessed alignment structure. The cross-sections of the raised alignment structure and the recessed alignment structure along at least one axis parallel to the first surface of each substrate can be trapezoidal, such that the cross-section of the raised alignment structure is a trapezoid extending from the first surface of the first substrate, and the cross-section of the recessed alignment structure can be a trapezoid extending into the first surface of the second substrate. The longest base of the convex alignment trapezoid can be longer than the longest base of the concave alignment trapezoid, and each side of the convex alignment trapezoid can be parallel to the adjacent side of the concave alignment trapezoid. The protruding alignment structure and the recessed alignment structure can be isosceles trapezoids. When the protruding alignment structure extends to a set depth within the recessed alignment structure, the spacing between the first substrate and the second substrate... It can be given by the following equation: in Let be the interior angle between the leg and the longest base of each trapezoid. The length of the longest bottom edge of the protrusion aligned with the structure and It is the length of the longest bottom edge of the concave alignment structure. The cross-sections of the raised alignment structure and the recessed alignment structure along the two vertical axes parallel to the first surface of each substrate can be trapezoidal, such that the raised alignment structure is a square or rectangular frustum extending from the first surface of the first substrate, and the recessed alignment structure is a square or rectangular frustum hollow extending into the first surface of the second substrate. The dimensions of the protruding alignment structure and the recessed alignment structure can conform to the following equation: Wherein d represents the distance between the first surface of the first substrate and the first surface of the second substrate when the protruding alignment structure extends to a set depth within the recessed alignment structure. It is the interior angle between the waist side and the longest base side of the trapezoid along the first axis parallel to the first surface of the first substrate and the second substrate. The length of the longest base of the trapezoid aligned with the first axis of the protrusion is given. It is the length of the longest base of the trapezoidal alignment structure recessed along the first axis. It is the interior angle between the waist and the longest base of a trapezoid that is parallel to the first surface of the first substrate and the second substrate and perpendicular to the second axis. It is the length of the longest base of the trapezoid along the second axis of the structure aligned with the protrusion, and It is the length of the longest base of the trapezoidal alignment structure recessed along the second axis. The product may include multiple raised alignment structures and multiple recessed alignment structures, such that each raised alignment structure extends at least partially within the corresponding recessed alignment structure to a set depth. At least one raised alignment structure and at least one recessed alignment structure may exist in each quadrant of the substrate. The product may further include qubits on the raised alignment structure, and the through-hole in the substrate may extend from the recessed alignment structure to the second surface of the second substrate, and the sidewalls of the through-hole in the substrate may be metallized. Quantum bits and metallizations that penetrate the sidewalls of the substrate can serve as electrodes for capacitors. Quantum bits can be positioned on the upper surface of the protrusion alignment structure. The product comprises multiple raised alignment structures and multiple recessed alignment structures. Quantum bits can be positioned on each of the raised alignment structures in a first subset of the raised alignment structures. Through-substrate vias can extend from the first subset of the recessed alignment structures. The first subset of the recessed alignment structures includes recessed alignment structures positioned relative to the raised alignment structures in the first subset of the raised alignment structures. A spacer layer can be positioned on a second subset of the raised alignment structures and / or the second subset of the recessed alignment structures. The distance between the first substrate and the second substrate can be determined by the thickness of the spacer material layer located on the second subset of the (etc.) raised alignment structure and / or the second subset of the (etc.) recessed alignment structure. The product may further include metallization surrounding the qubit at least on the sidewall of the protrusion alignment structure, and the metallization on the sidewall of the through-hole in the substrate may be in electrical contact with the metallization on the sidewall of the protrusion alignment structure. The product may include multiple raised alignment structures and multiple recessed alignment structures. Quantum bits may be positioned on at least two of the raised alignment structures and a coupler may be positioned on at least one of the raised alignment structures. A connecting element may connect at least two qubits to at least one coupler and may extend through a substrate via from a subset of the recessed alignment structures. The subset of the recessed alignment structures includes recessed alignment structures positioned relative to the raised alignment structures on which qubits are positioned. Figure 1 is a flowchart illustrating a method for aligning substrates. This method can be part of a broader process in which components of integrated circuit devices (e.g., superconducting qubits) are formed on one or more substrates. The term "substrate" refers to a base material that can be patterned to form integrated circuit components and structures. For example, the substrate can be a silicon wafer. When using the term "substrate," it can refer to the entire wafer, i.e., the wafer before dicing, or individual dies. The steps of this method can be performed simultaneously in multiple regions of each substrate to form several substantially identical individual dies from each substrate. In step 101, the first substrate 210 is etched to form a raised alignment structure 201 extending above the first surface 211 of the first substrate 210. The phrase "extending above" means that the raised alignment structure 201 extends away from the first surface 211 of the first substrate 210 in a direction away from the interior of the substrate 210, such that the raised alignment structure 201 is a protrusion extending from the first surface 211 of the first substrate 210. In step 102, the second substrate 220 is etched to form a recessed alignment structure 202 extending below the first surface 221 of the second substrate 220. The phrase "extending below" means that the recessed alignment structure 202 extends away from the first surface 221 of the second substrate 220 in a direction toward the interior of the substrate 220, such that the recessed alignment structure 202 is a recessed area within the second substrate 220 extending from the first surface 221 of the first substrate 220. Steps 101 and 102 can be performed in any order or simultaneously in separate processes. Steps 101 and 102 are shown in FIG2A, where the dashed sections indicate the areas of the first substrate 210 and the second substrate 220 that are removed during the etching process. In step 103, the protruding alignment structure 201 and the recessed alignment structure 202 are positioned relative to each other, such that the first surface 211 of the first substrate 210 and the first surface 221 of the second substrate 220 are opposite to and parallel to each other, and the protruding alignment structure 201 is at least partially positioned within the recessed alignment structure 202. The raised alignment structure 201 and the recessed alignment structure 202 are shaped such that the raised alignment structure 201 extends at least partially within the recessed alignment structure 202 to a predetermined depth. In this context, "at least partially within" means that at least a portion of the raised alignment structure 201 extends within the recessed alignment structure 202, that is, extends below the plane of the first surface 221 of the second substrate 220. Furthermore, when the raised alignment structure 201 is positioned at a predetermined depth within the recessed alignment structure 202, the movement of the first substrate 210 toward the second substrate 220 is limited by the contact between the raised alignment structure 201 and the recessed alignment structure 202, and the relative movement of the first substrate 210 and the second substrate 220 along at least one axis parallel to the first surfaces of the first and second substrates is also limited by the contact between the raised alignment structure 201 and the recessed alignment structure 202. The predetermined depth by which the protruding alignment structure 201 extends within the recessed alignment structure 202 is determined by the relative size of the protruding alignment structure 201 and the recessed alignment structure 202, as shown in FIG3. The protruding alignment structure 201 and the recessed alignment structure 202 preferably have trapezoidal cross-sections along at least one plane perpendicular to the first surfaces 211 and 221 of the first substrate 210 and the second substrate 220. When the first surface 211 of the first substrate 210 is parallel to the first surface 221 of the second substrate 220, the longest base of the trapezoid of the protruding alignment structure 201 is longer than the longest base of the trapezoid of the recessed alignment structure 202, and each side of the trapezoid of the protruding alignment structure 201 is parallel to the adjacent side of the trapezoid of the recessed alignment structure 202. Preferably, the protruding alignment structure 201 and the recessed alignment structure 202 are isosceles trapezoids. When substrates 210 and 220 are positioned and aligned such that the protruding alignment structure 201 and the recessed alignment structure 202 form hard stops, that is, when the protruding alignment structure 201 is at a set depth within the recessed alignment structure 202, the final distance between the first surface 211 of the first substrate 210 and the first surface 221 of the second substrate 220 is... Determined by the following equation: in Let be the interior angle between the leg and the longest base of each trapezoid. The length of the longest bottom edge of the protrusion aligned with the structure and This refers to the length of the longest bottom edge of the recessed alignment structure. This is shown in more detail in Figure 3. The protruding alignment structure 201 and the recessed alignment structure 202 have trapezoidal cross sections in two vertical planes. That is, when the protruding alignment structure 201 and the recessed alignment structure 202 are frustoconical, as shown in Figure 4, the dimensions of the protruding alignment structure and the recessed alignment structure conform to the following equation: in This refers to the distance between the first surface of the first substrate and the first surface of the second substrate when the protruding alignment structure extends to a set depth within the recessed alignment structure. It is the interior angle between the waist side and the longest base side of the trapezoid along the first axis parallel to the first surface of the first substrate and the second substrate. The length of the longest base of the trapezoid aligned with the first axis of the protrusion is given. It is the length of the longest base of the trapezoidal alignment structure recessed along the first axis. It is the interior angle between the waist and the longest base of a trapezoid that is parallel to the first surface of the first substrate and the second substrate and perpendicular to the second axis. It is the length of the longest base of the trapezoid along the second axis of the structure aligned with the protrusion, and It is the length of the longest base of the trapezoidal alignment structure recessed along the second axis. Etching the first substrate 210 in step 101 to form the raised alignment structure 201 may include: forming a hard mask or resist on a first region of the first substrate 210; etching the first substrate 210 anisotropically; and removing the hard mask or resist. The size of the first region on which the hard mask or resist is formed, as well as the etching time and / or etchant concentration, are controlled to control the size of the trapezoidal / frustum shape of the raised alignment structure 201. Etching the second substrate 220 to form the recessed alignment structure 202 may include: forming a hard mask or resist on the upper surface of the second substrate 220, the hard mask or resist including at least one opening defining an open region of the second substrate 220; anisotropically etching the second substrate through the opening in the hard mask or resist; and removing the hard mask or resist. The size of the open region on the second substrate 220, as well as the etching time and / or etchant concentration, are controlled to control the dimensions of the trapezoidal / frustum shape of the recessed alignment structure 202. When the first substrate 210 and the second substrate 220 are silicon substrates, anisotropic etching of the first substrate 210 and the second substrate 220 can be performed using a solution based on TMAH and KOH. Using a silicon substrate with a <100> crystal orientation, TMAH can be used to selectively etch the <110> direction (45°, relative to <100>), while the KOH solution can be used to selectively etch the <111> direction (54.7°, relative to <100>). Multiple raised alignment structures 201 and recessed alignment structures 202 may be formed on the same substrate, wherein the substrate is a wafer to be diced later, and multiple wafers may be formed on each individual die. Each substrate and / or die may include at least one pair of corresponding raised alignment structures 201 and recessed alignment structures 202 in each quadrant of the substrate / die, such as one in each corner, to provide both lateral and vertical alignment. In a minimum case, each pair of dies may include three pairs of raised alignment structures and recessed alignment structures to provide both lateral and vertical alignment. The method shown in Figure 1 may also include depositing a plurality of flip-chip bumps 231 to 234 on at least one of the first surface of the first substrate or the first surface of the second substrate and / or depositing an indium film on the protrusion alignment structure 201 and / or within the recess alignment structure 202 before positioning the protrusion alignment structure 201 and the recess alignment structure 202 relative to each other. Step 103, which positions the protrusion alignment structure 201 and the recess alignment structure 202 relative to each other, may further include bonding the first substrate to the second substrate via the flip-chip bumps or the indium film. Bonding the first substrate to the second substrate may be a thermocompression bonding process. The use of flip-chip bumps is shown in more detail in Figures 2B and 2C. When the protrusion alignment structure 201 is positioned at a set depth within the recessed alignment structure 202, the height of the deposited flip-chip bumps 231 to 234 is greater than the distance between the first surface 211 of the first substrate 210 and the first surface 221 of the second substrate 220. After compression bonding, the protrusion alignment structure 201 is positioned at a set depth within the recessed alignment structure 202. Another step of depositing a base metal layer 241 on the first substrate 210 and the raised alignment structure 201, and depositing a base metal layer 242 on the second substrate 220 and the recessed alignment structure 202, can be performed before forming flip-chip bumps. The base metal layers can form the basis for other components fabricated on the substrates 210 and 220 and are patterned before step 103 of positioning the alignment structures 201 and 202. The method may include additional steps for fabricating components on a substrate, such as forming quantum circuit components on a first substrate and / or a second substrate prior to the step of positioning the protrusion alignment structure relative to the recess alignment structure. Figure 5 illustrates examples of qubits and readout structures formed on the first substrate 510 and the second substrate 520. In another step, qubit 550 is formed on the raised alignment structure 501. The qubit can be a Josephson junction-based qubit, such as a transmon qubit, and is formed on the upper surface of the raised alignment structure. Since the upper surface of the raised alignment structure is the original polished surface of the substrate, it provides a particularly suitable location for the fabrication of sensitive superconducting components, such as Josephson junctions. In another step, a through-substrate via 560 is formed in the second substrate 520. The through-substrate via extends from the recessed alignment structure 502 through the second substrate to the second surface 522 of the second substrate 520. After the through-substrate via 560 has been formed, the sidewalls of the through-substrate via 560 are metallized. Forming a through-substrate via may include forming a hard mask or resist within the recessed alignment portion 502, and etching the through-substrate via through an opening in the hard mask or resist. The sidewall metallization is formed by chemical vapor deposition or physical vapor deposition before the hard mask or resist is removed, thereby preventing the sidewalls of the recessed alignment portion 502 from being metallized and preventing direct conductive contact between the metallization 570 and the qubit 550. After the first substrate 510 and the raised alignment structure 501 are positioned relative to the second substrate 520 and the recessed alignment structure 502, and as the raised alignment structure 501 extends within the recessed alignment structure 502, as shown in FIG5, the sidewall metallization 570 and the qubit 550 each form the electrode of a capacitor. The sidewall metallization 570 can be connected to a resonator and a readout structure fabricated on the second surface 522 of the second substrate 520. To effectively control the total capacitance of the capacitor formed between the qubit 550 and the sidewall metallization 570, a high aspect ratio trench, i.e., a depth greater than its width, can be formed in the second substrate around the through-hole 560. The sidewalls of the trench are metallized and connected to electrical ground. Alternatively, as shown in FIG6, the sidewall metallization 670 may be formed after the removal of the hard mask or resist, such that the sidewalls of the recessed alignment structure 602 are also metallized. The qubits 650 formed on the upper surface of the raised alignment structure 601 are not electrically connected to the metallization 680, which is also formed on at least the sidewalls of the raised alignment structure 601. After the first substrate 610 and the raised alignment structure 601 are positioned relative to the second substrate 620 and the recessed alignment structure 602, and as the raised alignment structure 601 extends within the recessed alignment structure 602, as shown in FIG6, the metallization 680 on the sidewall of the raised alignment structure 601 and the metallization 670 on the sidewall of the recessed alignment structure are in electrical contact, and a capacitor is formed between the metallizations 670, 680 and the qubit 650. Figure 7 illustrates an alternative solution where, when the raised alignment structure is positioned at a set depth within the recessed alignment structure, the spacing between the first substrate 710 and the second substrate 720 is determined by the thickness of the spacer materials 791 and 792 deposited on the raised alignment structures 703 and 705 and / or the recessed alignment structures 704 and 706. In the product shown in Figure 7, spacer materials 791 and 792 are deposited on the raised alignment structures and the recessed alignment structures 703 to 706, and the spacing between the substrates 710 and 720 is determined. The spacing can be adjusted by controlling the thickness of the spacer materials. Figure 8 illustrates an embodiment in which multiple coupled qubits and resonators (such as those shown in Figure 5 or Figure 6) formed around raised alignment structures 801, 803 are coupled via an intermediate coupler 852 formed on raised alignment structure 805. Qubits 850, 851 are coupled to coupler 852 via waveguides 855, 856. Coupler 852 may be used for selectively coupling qubits 850, 851 rather than as a transmon for qubits. 101: Step 102: Step 103: Step 201: Raised alignment structure 202: Recessed alignment structure 210: First substrate 211: First surface 220: Second substrate 221: First surface 231: Flip-chip bump 232: Flip-chip bump 233: Flip-chip bump 234: Flip-chip bump 241: Base metal layer 242: Base metal layer 501: Raised alignment structure 502: Recessed alignment structure / Recessed alignment portion 510: First substrate 520: Second substrate 522: Second surface 550: Quantum bit 560: Through-substrate via 570: Sidewall metallization 601: Raised Alignment structure 602: Recessed alignment structure 610: First substrate 620: Second substrate 650: Quantum bit 670: Sidewall metallization 680: Metallization 703: Protruding alignment structure 704: Recessed alignment structure 705: Protruding alignment structure 706: Recessed alignment structure 710: First substrate 720: Second substrate 791: Spacer material 792: Spacer material 801: Protruding alignment structure 803: Protruding alignment structure 805: Protruding alignment structure 850: Quantum bit 851: Quantum bit 852: Intermediate coupler 855: Waveguide 856: Waveguide α: Interior angle β: Interior angle B raised :length B recessed :length C raised :length C recessed :length Figure 1 is a flowchart illustrating the method according to the present invention. Figures 2A to 2D depict the steps of the method of the present invention. Figure 3 is a cross-sectional view depicting the geometry of the protruding alignment structure and the recessed alignment structure of the present invention. Figure 4 is a perspective view depicting the geometry of the raised alignment structure and the recessed alignment structure of the present invention. Figure 5 is a cross-sectional view depicting the quantum bit and resonator structure according to the first embodiment of the present invention. Figure 6 is a cross-sectional view depicting the quantum bit and resonator structure according to a second embodiment of the present invention. Figure 7 is a cross-sectional view depicting a device with adjustable substrate spacing according to the present invention. Figure 8 is a cross-sectional view depicting the coupled qubit and resonator structure according to the present invention. 210: First substrate 220: Second substrate 241: Base metal layer 242: Base metal layer
Claims
1. A wafer manufacturing method comprising: etching a first substrate to form a raised alignment structure extending above a first surface of the first substrate; etching a second substrate to form a recessed alignment structure extending below a first surface of the second substrate; and positioning the raised alignment structure and the recessed alignment structure relative to each other such that the first surface of the first substrate and the first surface of the second substrate are opposite and parallel, and such that the raised alignment structure is at least partially positioned within the recessed alignment structure; wherein the raised alignment structure and the recessed alignment structure are shaped such that the raised alignment structure extends at least partially within the recessed alignment structure to a predetermined depth, and such that when the raised alignment structure is positioned within the recessed alignment structure at the predetermined depth, the first substrate is restricted to move toward the second substrate and is restricted to move relative to the second substrate along at least one axis parallel to the first surfaces of the first substrate and the second substrate, and wherein... The cross-sections of the raised alignment structure and the recessed alignment structure along at least one plane perpendicular to one of the first surfaces of each substrate are trapezoidal, such that the cross-section of the raised alignment structure is a trapezoid extending from the first surface of the first substrate, and the cross-section of the recessed alignment structure is a trapezoid extending into the first surface of the second substrate.
2. As in the wafer manufacturing method of claim 1, wherein: Before positioning the protruding alignment structure relative to the recessed alignment structure, the method further includes depositing at least one of the following: a plurality of flip-chip bumps on at least one of the first surface of the first substrate or the first surface of the second substrate; or an indium film on the protruding alignment structure and / or within the recessed alignment structure. Positioning the protruding alignment structure relative to the recessed alignment structure further includes bonding the first substrate to the second substrate via the flip-chip bumps or the indium film.
3. The wafer manufacturing method of claim 2, wherein bonding the first substrate to the second substrate comprises thermo-press bonding.
4. The wafer manufacturing method of claim 3, wherein when the bump alignment structure is positioned within the recess alignment structure at the set depth, the height of the deposited flip-chip bump is greater than the distance between the first surface of the first substrate and the first surface of the second substrate, and wherein after compression bonding, the bump alignment structure is positioned within the recess alignment structure at the set depth.
5. A wafer manufacturing method according to any one of claims 1 to 4, wherein the longest base of the raised alignment structure trapezoid is longer than the longest base of the recessed alignment structure trapezoid, and wherein when the first surface of the first substrate is parallel to the first surface of the second substrate, each waist of the raised alignment structure trapezoid is parallel to the adjacent waist of the recessed alignment structure trapezoid.
6. The wafer manufacturing method of claim 5, wherein the protrusion alignment structure and the recess alignment structure are isosceles trapezoids.
7. The wafer manufacturing method of claim 6, wherein when the raised alignment structure extends to the set depth within the recessed alignment structure, the distance between the first surface of the first substrate and the first surface of the second substrate is given by the following equation: where is the interior angle between the isosceles side and the longest base of each trapezoid, is the length of the longest base of the raised alignment structure, and is the length of the longest base of the recessed alignment structure.
8. The wafer manufacturing method of claim 1, wherein the cross-sections of the raised alignment structure and the recessed alignment structure along two vertical planes perpendicular to the first surfaces of each substrate are trapezoidal, such that the raised alignment structure is a square or rectangular frustum extending from the first surface of the first substrate, and the recessed alignment structure is a square or rectangular frustum hollow extending to the first surface of the second substrate.
9. The wafer manufacturing method of claim 8, wherein the dimensions of the raised alignment structure and the recessed alignment structure conform to the following equation: Wherein, when the protruding alignment structure extends to the set depth within the recessed alignment structure, the distance between the first surface of the first substrate and the first surface of the second substrate is the interior angle between the equal waist side and the longest base side of the trapezoids parallel to one of the first axes of the first surfaces of the first substrate and the second substrate, the length of the longest base side of the trapezoid along the first axis of the protruding alignment structure, and the length of the longest base side of the trapezoid along the first axis of the recessed alignment structure, the interior angle between the equal waist side and the longest base side of the trapezoids parallel to the first surfaces of the first substrate and the second substrate and perpendicular to one of the first axes, the length of the longest base side of the trapezoid along the second axis of the protruding alignment structure, and the length of the longest base side of the trapezoid along the second axis of the recessed alignment structure.
10. The wafer manufacturing method of claim 7, wherein etching the first substrate to form a bump alignment structure comprises: forming a hard mask or resist on a first region of the first substrate; etching the first substrate anisotropically; and removing the hard mask or resist.
11. The wafer manufacturing method of claim 10, wherein the size, etching time and / or etchant concentration of the first region on which the hard mask or resist is formed are controlled in order to control the dimensions of the trapezoidal / frustum shape of the protrusion alignment structure.
12. The wafer manufacturing method of claim 7, wherein etching the second substrate to form a recessed alignment structure comprises: forming a hard mask or resist on an upper surface of one of the second substrates, the hard mask or resist including at least one opening defining an open region of one of the second substrates; anisotropically etching the second substrate through the opening in the hard mask or resist; and removing the hard mask or resist.
13. The wafer manufacturing method of claim 12, wherein the size of the open area on the second substrate, the etching time and / or the etchant concentration are controlled in order to control the dimensions of the trapezoidal / frustum shape of the recessed alignment structure.
14. The wafer manufacturing method of claim 1 above, wherein etching a first substrate to form a raised alignment structure includes forming a plurality of raised alignment structures on the first substrate, and the step of etching a second substrate to form a recessed alignment structure includes forming a plurality of recessed alignment structures on the second substrate.
15. The wafer manufacturing method as described in claim 14, wherein: The first substrate is a die on a first wafer containing a plurality of dies; the second substrate is a die on a second wafer containing a plurality of dies; etching the first substrate to form a plurality of raised alignment structures includes etching the first wafer to form a plurality of raised alignment structures on each die on the first wafer; and etching the second substrate to form a plurality of recessed alignment structures includes etching the second wafer to form a plurality of recessed alignment structures on each die on the second wafer.
16. The wafer manufacturing method as described in claim 15, wherein: The first wafer is etched to form a plurality of raised alignment structures, one raised alignment structure being formed in each quadrant of each die on the first wafer; and / or the second wafer is etched to form a plurality of recessed alignment structures, one recessed alignment structure being formed in each quadrant of each die on the second wafer.
17. A wafer manufacturing method according to any one of claims 14 to 16, wherein the plurality of bump alignment structures are disposed on the first substrate and the plurality of recess alignment structures are disposed on the second substrate, such that positioning the bump alignment structure relative to the recess alignment structure includes positioning each bump alignment structure relative to the recess alignment structures such that each bump alignment structure extends at least partially within the opposing recess alignment structure to the predetermined depth.
18. The wafer manufacturing method of claim 1 above, wherein the method further includes forming a quantum circuit assembly on the first substrate and / or the second substrate prior to the step of positioning the protrusion alignment structure relative to the recess alignment structure.
19. The wafer manufacturing method of claim 18, wherein forming a quantum circuit assembly comprises: forming a qubit on the raised alignment structure; forming a through-substrate via in the second substrate, the through-substrate via extending from the recessed alignment structure through the second substrate to a second surface of the second substrate; and metallizing the sidewalls of the through-substrate via.
20. The wafer manufacturing method of claim 19, wherein the raised alignment structure and the recessed alignment structure are positioned opposite each other to form a capacitor between the sidewall metallization of the through-hole in the substrate and the qubit formed on the raised alignment structure.
21. The wafer manufacturing method of claim 19 or 20, wherein forming the qubit on the bump alignment structure includes forming the qubit on the upper surface of the bump alignment structure.
22. The wafer manufacturing method of claim 19, wherein forming the through-substrate via comprises forming a hard mask or resist within the recessed alignment portion and etching the through-substrate via an opening in the hard mask or resist.
23. The wafer manufacturing method of claim 19, wherein the sidewall metallization is formed by chemical vapor deposition or physical vapor deposition before the hard mask or resist is removed.
24. The wafer manufacturing method of claim 19, further comprising: forming a plurality of bump alignment structures and a plurality of recessed alignment structures; forming a qubit on the bump alignment structure including forming a qubit on a first subset of one of the bump alignment structures; forming a through-substrate via including forming a through-substrate via extending from the first subset of one of the recessed alignment structures, the first subset of the recessed alignment structures including the recessed alignment structures positioned relative to the bump alignment structures in the first subset of the bump alignment structures during a positioning step; and depositing a spacer material layer on a second subset of one of the bump alignment structures and / or the second subset of the recessed alignment structures before positioning the bump alignment structure relative to the recessed alignment structure.
25. The wafer manufacturing method of claim 24, wherein after the raised alignment structures and the recessed alignment structures are positioned relative to each other, the distance between the first substrate and the second substrate is determined at least in part by the thickness of the spacer material layer deposited on the second subset of the raised alignment structures and / or the second subset of the recessed alignment structures.
26. The wafer manufacturing method of claim 19, wherein the method further comprises forming a metallization around the qubit at least on the sidewall of the raised alignment structure, and wherein positioning the raised alignment structure relative to the recessed alignment structure further comprises making the metallization on the sidewall of the through-hole in the substrate electrically contact the metallization on the sidewall of the raised alignment structure.
27. The wafer manufacturing method of claim 19, further comprising: forming a plurality of raised alignment structures and a plurality of recessed alignment structures; forming a qubit on the raised alignment structure including forming a qubit on at least two of the raised alignment structures and forming a coupler on at least one of the raised alignment structures; forming a connection element connecting at least two qubits to at least one coupler; forming a through-substrate via including forming a through-substrate via extending from a subset of the recessed alignment structures, the subset of the recessed alignment structures including the recessed alignment structures positioned relative to the raised alignment structures on which the qubits are formed.
28. The wafer manufacturing method of claim 19, wherein the qubit is a Josephson junction-based qubit, such as a transmon qubit.
29. A wafer product comprising: a first substrate including at least one raised alignment structure extending above a first surface of one of the first substrates; and a second substrate including at least one recessed alignment structure extending below a first surface of one of the second substrates. The raised alignment structure and the recessed alignment structure are positioned relative to each other such that the first surface of the first substrate is opposite to and parallel to the first surface of the second substrate, and the raised alignment structure is at least partially positioned within the recessed alignment structure; wherein the raised alignment structure and the recessed alignment structure are shaped such that the raised alignment structure extends at least partially within the recessed alignment structure to a predetermined depth, and the first substrate is restricted to move toward the second substrate and is restricted to move relative to the second substrate along at least one axis parallel to the first surfaces of the first substrate and the second substrate; and wherein the cross-section of the raised alignment structure and the recessed alignment structure along at least one axis parallel to the first surfaces of each substrate is trapezoidal, such that the cross-section of the raised alignment structure is a trapezoid extending from the first surface of the first substrate, and the cross-section of the recessed alignment structure is a trapezoid extending to the first surface of the second substrate.
30. The wafer product of claim 29, wherein the product further comprises: a plurality of flip-chip bumps connecting the first surface of the first substrate and the first surface of the second substrate; and / or an indium film on the raised alignment structure and / or within the recessed alignment structure.
31. The chip product of claim 29, wherein the longest base of the raised alignment trapezoid is longer than the longest base of the recessed alignment trapezoid, and wherein each side of the raised alignment trapezoid is parallel to the adjacent side of the recessed alignment trapezoid.
32. The chip product of claim 31, wherein the raised alignment structure and the recessed alignment structure are isosceles trapezoids.
33. The wafer product of claim 32, wherein when the raised alignment structure extends to the set depth within the recessed alignment structure, the spacing between the first substrate and the second substrate is given by the following equation: where is the interior angle between the isosceles side and the longest base side of each trapezoid, is the length of the longest base side of the raised alignment structure, and is the length of the longest base side of the recessed alignment structure.
34. A wafer product of any one of claims 29 to 33, wherein the cross-sections of the raised alignment structure and the recessed alignment structure along two vertical axes parallel to the first surfaces of each substrate are trapezoidal, such that the raised alignment structure is a square or rectangular frustum extending from the first surface of the first substrate, and the recessed alignment structure is a square or rectangular frustum hollow extending to the first surface of the second substrate.
35. The wafer product of claim 34, wherein the dimensions of the raised alignment structure and the recessed alignment structure conform to the following equation: Wherein d represents the distance between the first surface of the first substrate and the first surface of the second substrate when the protruding alignment structure extends to the set depth within the recessed alignment structure, which is the interior angle between the equal waist side and the longest base side of the trapezoids parallel to the first axis of one of the first surfaces of the first substrate and the second substrate, which is the length of the longest base side of the trapezoid along the first axis of the protruding alignment structure, and the length of the longest base side of the trapezoid in the recessed alignment structure along the first axis, which is the interior angle between the equal waist side and the longest base side of the trapezoids parallel to the first surfaces of the first substrate and the second substrate and perpendicular to the first axis, which is the length of the longest base side of the trapezoid along the second axis of the protruding alignment structure, and the length of the longest base side of the trapezoid in the recessed alignment structure along the second axis.
36. The chip product of claim 29, wherein the product includes a plurality of raised alignment structures and a plurality of recessed alignment structures, such that each raised alignment structure extends at least partially within the opposite recessed alignment structure to the predetermined depth.
37. The wafer product of claim 36, wherein at least one raised alignment structure and at least one recessed alignment structure are present in each quadrant of the substrate.
38. The chip product as described in claim 29, wherein: The product further includes a qubit on the raised alignment structure; a through-substrate via extending from the recessed alignment structure to a second surface of the second substrate; and the sidewalls of the through-substrate via are metallized.
39. The wafer product of claim 38, wherein the qubit and the through-substrate sidewall metallization are electrodes of a capacitor.
40. The chip product of claim 39, wherein the qubit is positioned on the upper surface of the protrusion alignment structure.
41. A wafer product as claimed in any one of claims 38 to 40, wherein the product comprises a plurality of bump alignment structures and a plurality of recessed alignment structures; a qubit is positioned on each of the bump alignment structures in a first subset of the bump alignment structures; a through-substrate via extends from the first subset of the recessed alignment structures, the first subset of the recessed alignment structures comprising the recessed alignment structures positioned relative to the bump alignment structures in the first subset of the bump alignment structures; and a spacer layer is positioned on a second subset of the bump alignment structures and / or the second subset of the recessed alignment structures.
42. The wafer product of claim 41, wherein the distance between the first substrate and the second substrate is determined by the thickness of the spacer material layer located on the second subset of the raised alignment structure and / or the second subset of the recessed alignment structure.
43. The wafer product of claim 29, wherein the product further comprises a metallization surrounding the qubit at least on the sidewall of the protrusion alignment structure, and wherein the metallization on the sidewall of the through-hole in the substrate is in electrical contact with the metallization on the sidewall of the protrusion alignment structure.
44. The wafer product of claim 29, wherein the product includes a plurality of raised alignment structures and a plurality of recessed alignment structures; a qubit is positioned on at least two of the raised alignment structures and a coupler is positioned on at least one of the raised alignment structures; a connecting element connects at least two qubits to at least one coupler; a through-substrate via extends from a subset of the recessed alignment structures, the subset of the recessed alignment structures including the recessed alignment structures positioned relative to the raised alignment structures on which the qubits are positioned.
Citation Information
Patent Citations
Passive alignment using slanted wall pedestal
US20010010743A1