Surface-coated inorganic particles and their manufacturing methods, surface modifiers, cosmetics, and surface modification methods

TWI945362BActive Publication Date: 2026-11-11KAO CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW111149913
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-12-27
Filing Date
2022-12-26
Publication Date
2026-11-11
Estimated Expiration
2042-12-25

AI Technical Summary

Technical Problem

There is a need for touch-enhancing particles that can replace synthetic polymer microparticles in cosmetics and fragrances, as synthetic polymers are difficult to decompose and pose environmental concerns.

Method used

Surface-coated inorganic particles are developed, where the surface of inorganic particles like silica or silicate minerals are coated with modified polysiloxanes and water-soluble cationic polymers, enhancing tactile feel and environmental compatibility.

Benefits of technology

The surface-coated inorganic particles provide a good tactile feel, reducing dynamic friction and stickiness, and are environmentally friendly substitutes for synthetic polymer microparticles, improving the touch of cosmetics and fragrances.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The inorganic particles coated in this invention are inorganic particles (A) whose surface is partially or entirely coated with a surface treatment agent (B). The inorganic particles (A) include silica particles or silicate mineral particles. The surface treatment agent (B) includes at least one of modified polysiloxane (b1) which is liquid at 25°C and a water-soluble cationic polymer (b2). The modified polysiloxane (b1) includes at least one of polyether-modified polysiloxane, polyglycerol-modified polysiloxane, branched polyglycerol-modified polysiloxane, and alkyl glycerol ether-modified polysiloxane.
Need to check novelty before this filing date? Find Prior Art

Description

Surface coated with inorganic particles This invention relates to a surface-coated inorganic particle, a surface modifier, a fragrance, a surface modification method, and a method for manufacturing surface-coated inorganic particles. From the perspective of improving tactile feel, there are cases where polymer microparticles are formulated into cosmetics, skincare products, hygiene products, perfumes, and other fragrance products. However, since synthetic polymer microparticles are difficult to decompose in the natural environment, there are concerns about their adverse impact on the ecosystem. Therefore, a tactile feel-enhancing particle is sought as an alternative to synthetic polymer microparticles. Furthermore, as a tactile feel-enhancing particle formulated into fragrance products, inorganic particles with a surface coated with a polysiloxane compound can be cited. As for technologies related to such surface-coated inorganic particles, examples include those described in Japanese Patent Application Publication No. 9-301826 (Patent Document 1) and International Publication No. 2020 / 230650 (Patent Document 2). Patent Document 1 describes inorganic particles coated with poly(N-acetylenylimide) modified polysiloxane. Patent Document 2 describes a composite surface-treated inorganic powder, which is a substrate powder mainly composed of inorganic materials, and is surface-treated with cationic surfactants and amine-modified polysiloxane. The present invention relates to the following [1] to [5]. [1] A surface-coated inorganic particle, wherein a portion or all of the surface of an inorganic particle (A) is coated with a surface treatment agent (B), wherein the inorganic particle (A) comprises silica particles or silicate mineral particles, and the surface treatment agent (B) comprises at least one selected from modified polysiloxane (b1) which is liquid at 25°C and a water-soluble cationic polymer (b2), wherein the modified polysiloxane (b1) comprises at least one selected from polyether-modified polysiloxane, polyglycerol-modified polysiloxane, branched polyglycerol-modified polysiloxane, and alkyl glycerol ether-modified polysiloxane. [2] A surface modifier comprising the surface-coated inorganic particles as described in [1] above. [3] A fragrance comprising the surface-coated inorganic particles as described in [1] above. [4] A surface modification method comprising applying the surface-coated inorganic particles as described in [1] above, the surface modifier as described in [2] above, or the fragrance as described in [3] above to a surface of an object. [5] A method for manufacturing the surface-coated inorganic particles as described in [1] above, comprising mixing the inorganic particles (A) with a surface treatment agent solution containing the surface treatment agent (B) and a solvent. The industry is seeking a tactilely enhanced particle that has a good feel and is suitable as a substitute for synthetic polymer microparticles. One embodiment of the present invention relates to providing surface-coated inorganic particles with a good tactile feel, suitable as a substitute for synthetic polymer microparticles, surface modifiers, and cosmetics, as well as a surface modification method using the aforementioned surface-coated inorganic particles, surface modifiers, or cosmetics. Furthermore, one embodiment of the present invention relates to a method for manufacturing surface-coated inorganic particles with a good tactile feel, suitable as a substitute for synthetic polymer microparticles. According to one embodiment of the present invention, a surface-coated inorganic particle with a good tactile feel, suitable as a substitute for synthetic polymer microparticles, a surface modifier, and a fragrance / cosmetic product, as well as a surface modification method using the aforementioned surface-coated inorganic particle, the aforementioned surface modifier, or the aforementioned fragrance / cosmetic product, can be provided. Furthermore, according to one embodiment of the present invention, a method for manufacturing a surface-coated inorganic particle with a good tactile feel, suitable as a substitute for synthetic polymer microparticles, can be provided. [Surface-coated inorganic particles] The surface-coated inorganic particles of the present invention are inorganic particles (A) whose surface is partially or entirely coated with a surface treatment agent (B). The inorganic particles (A) include silica particles or silicate mineral particles. The surface treatment agent (B) includes at least one of modified polysiloxane (b1) (hereinafter also referred to as "modified polysiloxane (b1)") which is liquid at 25°C and a water-soluble cationic polymer (b2). The modified polysiloxane (b1) includes at least one of polyether-modified polysiloxane, polyglycerol-modified polysiloxane, branched polyglycerol-modified polysiloxane, and alkyl glycerol ether-modified polysiloxane. The surface-coated inorganic particles of the present invention have a pleasant tactile feel. Therefore, the surface-coated inorganic particles of the present invention, when formulated into or used in cosmetics, can improve the tactile feel of cosmetics. Furthermore, the surface-coated inorganic particles of the present invention, when used as a surface modifier, can modify the surface of skin, hair, nails, etc., to have a pleasant tactile feel. Moreover, the surface-coated inorganic particles of the present invention have inorganic particles (A) that are not equivalent to synthetic polymer microparticles as core particles, and are coated with a surface treatment agent (B) comprising at least one of modified polysiloxane (b1) and a water-soluble cationic polymer (b2) that is liquid at 25°C. Therefore, they are environmentally friendly and suitable as a substitute for synthetic polymer microparticles. In this specification, the phrase "a portion or all of the surface of an inorganic particle (A) is coated with a surface treatment agent (B)" means that at least a portion of the surface of the inorganic particle (A) is adsorbed with the surface treatment agent (B) through intermolecular forces or ionic bonds. The term "adsorption" here does not include a state where the inorganic particle (A) and the surface treatment agent (B) are covalently bonded. The determination of whether at least a portion of the surface of the inorganic particle (A) is adsorbed with the surface treatment agent (B) is performed using known methods. For example, if the adsorption amount of the surface treatment agent (B) relative to 100 parts by mass of the inorganic particle (A), calculated by the "determination of the amount of adsorption of the surface treatment agent on the inorganic particle" described in the examples, exceeds 0 parts by mass, preferably 0.1 parts by mass or more, and more preferably 0.5 parts by mass or more, it is determined that the surface of the inorganic particle (A) is adsorbed with the surface treatment agent (B). In this instruction manual, "tactile sensation" refers to the smoothness and lack of dryness of the particles when applied to skin, hair, nails, etc. A smoother texture and less dryness indicate a superior tactile sensation. "Smoothness" refers to a very smooth feel without any powdery texture, while "dryness" refers to the feeling of the fingers getting stuck when moving on skin, hair, nails, etc. Furthermore, in this instruction manual, "liquid at 25°C" means that the particles are fluid in their bulk state at 1 atmosphere of pressure and 25°C. The reason for the good tactile feel of the inorganic particles coated on the surface of the present invention is not determined, but it is believed that the reason is that by coating the inorganic particles (A) containing silica particles or silicate mineral particles with a surface treatment agent (B) containing at least one of a modified polysiloxane with excellent lubricity (b1) and a water-soluble cationic polymer (b2), the dynamic friction force and the amplitude of the dynamic friction force can be effectively reduced while maintaining the appropriate hardness of the inorganic particles (A). From the viewpoint of further improving environmental adaptability, the content of the non-water-soluble synthetic polymer in the surface-coated inorganic particles of the present invention, which is solid at 25°C, is preferably less than 1% by mass, more preferably less than 0.5% by mass, further preferably less than 0.1% by mass, and even more preferably less than 0.01% by mass. The surface-coated inorganic particles of the present invention preferably do not substantially contain the synthetic polymer. In this specification, "substantially does not contain the synthetic polymer" means that it is not intentionally added, but does not exclude the presence of a small amount of the synthetic polymer as an impurity. In this specification, "non-water-soluble synthetic polymer" refers to a synthetic polymer that, according to OECD guideline 120, dissolves less than 2 g when 10 g of the synthetic polymer is mixed in 1000 mL of water at 20°C and pH 7 and stirred for 24 hours. Furthermore, "solid at 25°C" means that it does not have flowability in a bulk state under 1 atmosphere of pressure and 25°C. From the viewpoint of further improving tactile sensation, the median particle size (D) of the inorganic particles coated on the surface of the present invention... 50 Preferably, the particle size is greater than 1 μm, more preferably greater than 2 μm, and even more preferably greater than 3 μm, and preferably less than 30 μm, more preferably less than 20 μm, even more preferably less than 15 μm, and even more preferably less than 12 μm. Here, the volume median particle size (D) of the present invention... 50 The 50% median diameter is determined by a particle size distribution measuring machine using laser diffraction / scattering method. Specifically, it can be determined using the method described in the examples. From the viewpoint of further improving the tactile feel, the surface-coated inorganic particles of the present invention preferably have a surface treatment agent (B) adsorbed on the surface of the inorganic particles (A) via intermolecular forces or ionic bonds. In this specification, whether the adsorption of the inorganic particles (A) and the surface treatment agent (B) based on intermolecular forces or ionic bonds exists can be confirmed by known methods, such as the change in the amount of adsorption after washing the surface-coated inorganic particles with a solvent that can dissolve the surface treatment agent (B). Specifically, it can be confirmed by the methods described in the examples. The components of the surface-coated inorganic particles constituting the present invention and the manufacturing method of the surface-coated inorganic particles will be described in sequence below. <Inorganic Particles (A)> The inorganic particles (A) comprise silica particles or silicate mineral particles. From the viewpoint of further improving the tactile feel of the surface-coated inorganic particles, the inorganic particles (A) preferably comprise at least one particle selected from silica particles, talc particles, and mica particles, and more preferably comprise at least one particle selected from silica particles and mica particles. From the viewpoint of further suppressing the stickiness of the semi-dry state, it is further preferably comprised of silica particles, and more preferably comprised of porous silica particles. From the viewpoint of further improving the tactile feel of the surface-coated inorganic particles, the silicate mineral particles preferably comprise at least one selected from talc particles, mica particles, sericite particles, bentonite particles, montmorillonite particles, bentonite particles, and kaolinite particles, more preferably comprise at least one selected from talc particles and mica particles, and more preferably comprised of mica particles. When the inorganic particles (A) include porous silica particles, from the viewpoint of suppressing the disintegration of the porous silica particles and further improving the tactile feel of the surface-coated inorganic particles, the specific surface area of ​​the porous silica particles is preferably 5 m². 2 / g or more, preferably 10 m 2 / g or more, and preferably 1000 m 2 / g or less, preferably 900 m 2 / g or less. The above specific surface area is based on the BET (Brunauer-Emmett-Teller) specific surface area determined according to JIS Z 8830:2013. When the inorganic particles (A) include porous silica particles, from the viewpoint of suppressing the disintegration of the porous silica particles and further improving the tactile feel of the surface-coated inorganic particles, the pore volume of the porous silica particles is preferably 0.1 mL / g or more, more preferably 0.3 mL / g or more, and even more preferably 0.5 mL / g or more, and preferably 5 mL / g or less, more preferably 3 mL / g or less, and even more preferably 2 mL / g or less. Furthermore, from the viewpoint of eliminating dryness, the pore volume is preferably 0.3 mL / g or more, more preferably 0.5 mL / g or more, and even more preferably 0.7 mL / g or more, and even more preferably 5 mL / g or less, more preferably 3 mL / g or less, even more preferably 2 mL / g or less, and even more preferably 1.5 mL / g or less. The aforementioned pore volume can be determined by gas adsorption. As a gas adsorption method, examples include JIS Z 8831-2:2010 (Powder (Solid) Pore Size Distribution and Pore Characteristics - Part 2: Method for Determination of Micropores and Macropores by Gas Adsorption) and JIS Z 8831-3:2010 (Powder (Solid) Pore Size Distribution and Pore Characteristics - Part 3: Method for Determination of Micropores by Gas Adsorption). From the viewpoint of further improving the tactile feel of the surface-coated inorganic particles, the content of at least one particle selected from silica particles and silicate mineral particles in the inorganic particles (A) is preferably 50% by mass or more, more preferably 60% by mass or more, further preferably 70% by mass or more, further preferably 80% by mass or more, further preferably 90% by mass or more, further preferably 95% by mass or more, and preferably less than 100% by mass. The shape of the inorganic particles (A) can be spherical, plate-like, sheet-like, or irregular. Among these, from the viewpoint of further improving the tactile feel of the surface coated with inorganic particles, spherical, plate-like, or sheet-like shapes are preferred, and spherical or sheet-like shapes are even more preferred. More specifically, when the inorganic particles (A) are silicon dioxide particles, spherical shapes are preferred, and when the inorganic particles (A) are silicate mineral particles, sheet-like shapes are even more preferred. From the perspective of further improving the tactile feel of surface-coated inorganic particles, the median particle size (D) of the inorganic particles (A) is... 50Preferably, it is 1 μm or more, more preferably 2 μm or more, further preferably 3 μm or more, and preferably 30 μm or less, more preferably 20 μm or less, further preferably 15 μm or less, further preferably 12 μm or less. <Surface Treatment Agent (B)> The surface treatment agent (B) comprises at least one selected from modified polysiloxane (b1) which is liquid at 25°C and a water-soluble cationic polymer (b2). From the viewpoint of further suppressing the stickiness of the semi-dry state, it is more preferable that it comprises modified polysiloxane (b1) which is liquid at 25°C. From the viewpoint of further improving the tactile feel and environmental adaptability of the surface-coated inorganic particles, the surface treatment agent (B) preferably comprises at least 50% by mass of at least one selected from the above-mentioned modified polysiloxane (b1) and the above-mentioned water-soluble cationic polymer (b2), more preferably at least 70% by mass, more preferably at least 80% by mass, more preferably at least 90% by mass, more preferably at least 95% by mass, and more preferably at least 100% by mass. From the viewpoint of improving the tactile feel of the inorganic particles coated on the surface, the modified polysiloxane (b1), which is liquid at 25°C, includes at least one selected from polyether modified polysiloxane, polyglycerol modified polysiloxane, branched polyglycerol modified polysiloxane, and alkyl glycerol ether modified polysiloxane. From the perspective of improving the tactile feel of the inorganic particles coated on the surface, the HLB (hydrophilicity-oleophilicity balance) of the modified polysiloxane (b1) is preferably 1.0 or higher, more preferably 2.0 or higher, and even more preferably 2.5 or higher, and preferably 20.0 or lower, more preferably 18.0 or lower, even more preferably 16.0 or lower, even more preferably 15.5 or lower, even more preferably 15.0 or lower, even more preferably 10.0 or lower, even more preferably 5.0 or lower, even more preferably 4.0 or lower, even more preferably 3.5 or lower. Here, the HLB value represents the affinity of the modified polysiloxane (b1) for water and oil, which can be calculated by the Griffin method using the following formula. HLB = 20 × [(Molecular weight of hydrophilic groups contained in modified polysiloxane (b1)) / (Molecular weight of modified polysiloxane (b1))] Examples of hydrophilic groups include hydroxyl groups and ethoxyl groups. The viscosity of the modified polysiloxane (b1) at 25°C is preferably 50 mPa·s or higher, more preferably 100 mPa·s or higher, even more preferably 200 mPa·s or higher, even more preferably 400 mPa·s or higher, and preferably 500,000 mPa·s or lower, even more preferably 100,000 mPa·s or lower, even more preferably 80,000 mPa·s or lower. The above viscosity can be measured at 25°C using a Brookfield viscometer based on JIS Z 8803:2011 "Method for determination of viscosity of liquids". The polyether-modified polysiloxane is a structure in which the side chains and / or terminal hydrocarbon groups of polysiloxane oil are replaced with polyether groups. The polyether group of the polyether-modified polysiloxane is preferably a polyetheroxy group formed by the block or random addition of polyetheroxy, polyetherpropoxy, polyetheroxy (EO), and polyetherpropoxy (trimethyleneoxy or propane-1,2-dioxy; PO), and more preferably a polyetheroxy group. The polyether-modified polysiloxane can be used in compounds formed by branching polyether groups onto a polysiloxane backbone, and in compounds formed by block bonding of polysiloxane and polyether groups. From the viewpoint of improving the tactile feel of the inorganic particles coated on the surface, the viscosity of polyether-modified polysiloxane at 25°C is preferably 50 mPa·s or higher, more preferably 100 mPa·s or higher, further preferably 150 mPa·s or higher, further preferably 400 mPa·s or higher, further preferably 450 mPa·s or higher, further preferably 500 mPa·s or higher, further preferably 540 mPa·s or higher, and preferably 3000 mPa·s or lower, more preferably 2000 mPa·s or lower, further preferably 1000 mPa·s or lower, further preferably 750 mPa·s or lower, further preferably 600 mPa·s or lower. The above viscosity can be measured at 25°C using a Brookfield viscometer based on JIS Z 8803:2011 "Method for determination of viscosity of liquids". Specific examples of polyether-modified polysiloxane include: PEG (Polyethylene Glycol)-3 dimethyl polysiloxane, PEG-9 dimethyl polysiloxane, PEG-9 methyl ether dimethyl polysiloxane, PEG-10 dimethyl polysiloxane, PEG-11 methyl ether dimethyl polysiloxane, PEG-12 dimethyl polysiloxane, and PEG / PPG (Polypropylene) Glycol (polypropylene glycol)-20 / 22 butyl ether dimethyl polysiloxane, PEG-32 methyl ether dimethyl polysiloxane, PEG-9 polydimethylsiloxane, lauryl PEG-9 polydimethylsiloxane, cetyl PEG / PPG-10 / 1 dimethyl polysiloxane, PEG / PPG-30 / 10 dimethyl polysiloxane, and linear polyether-modified polysiloxanes formed by alternating copolymerization of dimethyl polysiloxane units and polyether units. Commercially available examples of polyether-modified polysiloxanes include: Shin-Etsu Chemical Industry Co., Ltd.'s KF series (e.g., KF-6004, KF-6011, KF-6012, KF-6013, KF-6015, KF-6016, KF-6017, KF-6028, KF-6038, KF-6043, KF-6048), and Dow Chemical Japan Co., Ltd.'s DOWSIL series (BY25-339, SH3775M, FZ-2203), etc. Polyglycerol-modified polysiloxane refers to polysiloxanes with a monovalent polyglycerol group in their structure. Examples include: polyglycerol-3-disiloxane dimethicone, polyglycerol-3-polydimethylsiloxane, and lauryl polyglycerol-3-polydimethylsiloxane. In this specification, branched polyglycerol-modified polysiloxanes and self-modified polyglycerol polysiloxanes are excluded. Commercially available polyglycerol-modified polysiloxanes include, for example, the KF series manufactured by Shin-Etsu Chemical Industry Co., Ltd. (e.g., KF-6100, KF-6104, KF-6106, KF-6105). From the viewpoint of improving the tactile feel of the inorganic particles coated on the surface, the viscosity of polyglycerol-modified polysiloxane at 25°C is preferably 500 mPa·s or higher, more preferably 1,000 mPa·s or higher, further preferably 2,000 mPa·s or higher, further preferably 3,000 mPa·s or higher, and preferably 20,000 mPa·s or lower, more preferably 10,000 mPa·s or lower, further preferably 5,000 mPa·s or lower, further preferably 4,000 mPa·s or lower. The above viscosity can be measured at 25°C using a Brookfield viscometer based on JIS Z 8803:2011 "Method for determination of viscosity of liquids". As a branched polyglycerol modified polysiloxane, for example, the compound represented by the following formula (1) can be listed, which has a structure in which branched polyglycerol chains are bonded to both ends of dimethyl polysiloxane via linkers containing oxyphenyl groups. [Chemistry 1] (In equation (1), R) 12 Each branched polyglycerol chain can be represented independently, where m represents an integer between 0 and 10000. In formula (1), the oxygen atom in the extended phenyl group reacts with the trimethylene (-C) group. 3H The bonding pattern for 6-) is not particularly limited and can be adjacent, intermediate, or opposite. m represents an integer from 0 to 10,000, preferably from 1 to 300. R 12 The branched polyglycerol chain comprises glycerol units represented by the following structural formulas (2) to (5), having at least one glycerol unit with a branched structure represented by structural formula (2), and the end being a glycerol unit represented by structural formula (5). Furthermore, the average total number of bonds of the glycerol units in the branched polyglycerol chain is 3 or more and 200 or less, preferably 3 or more and 30 or less. [Chemistry 2] From the viewpoint of improving the tactile feel of the inorganic particles coated on the surface, the viscosity of branched polyglycerol-modified polysiloxane at 25°C is preferably 10,000 mPa·s or higher, more preferably 20,000 mPa·s or higher, even more preferably 40,000 mPa·s or higher, even more preferably 60,000 mPa·s or higher, even more preferably 70,000 mPa·s or higher, and preferably 500,000 mPa·s or lower, even more preferably 100,000 mPa·s or lower, even more preferably 80,000 mPa·s or lower. The above viscosity can be measured at 25°C using a Brookfield viscometer based on JIS Z 8803:2011 "Method for determination of viscosity of liquids". The branched polyglycerol-modified polysiloxane represented by formula (1) can be manufactured, for example, by the method described in Japanese Patent Application Publication No. 2004-339244, and other commonly known methods. The method described in Japanese Patent Application Publication No. 2004-339244 involves graft polymerization of modified polysiloxane with hydroxyl-substituted phenyl groups at both ends by adding 2,3-epoxy-1-propanol in the presence of an acidic or alkaline catalyst. Furthermore, commercially available products of branched polyglycerol-modified polysiloxane include, for example, Sofcare GS-G (manufactured by Kao Corporation). As alkyl glycerol ether modified polysiloxanes, examples can be listed as represented by the following formula (6). [Chemistry 3] In formula (6), Q represents a divalent hydrocarbon group with 3 to 20 carbon atoms, and R 1 ~R 9 They can be the same or different, representing a hydrogen atom, a straight-chain or branched hydrocarbon group or phenyl group with 1 to 32 carbon atoms, R 10 and R 11 They can be the same or different, representing multiple R's in the same molecule, consisting of hydrogen atoms or straight-chain or branched hydrocarbon groups with 1 to 32 carbon atoms. 10 and R 11 Alternatively, they can be different. p represents a number between 1 and 500, and q represents a number between 1 and 50. Furthermore, p and q are preferably used to represent the alkyl glycerol ether group [-Q-OCH] in the molecule. 2-CH(OR 10 )-CH 2(OR 11The content of [ ] is more than 1% by mass and less than 50% by mass. In formula (6), the divalent hydrocarbon group represented by Q, having 3 to 20 carbon atoms, is preferably a straight-chain or branched alkyl group with 3 to 20 carbon atoms. More specifically, examples include: straight-chain alkyl groups such as trimethylene, tetramethylene, pentamethylene, hexamethylene, heptamethylene, octamethylene, nonamethylene, decamethylene, undecamethylene, dodecamethylene, tetradecamethylene, hexadecylethylene, and octadecylethylene; and branched alkyl groups such as propenyl, 2-methyltrimethylene, 2-methyltetramethylene, 2-methylpentamethylene, and 3-methylpentamethylene. Also, R 1 ~R 11 In the definition, a straight-chain or branched hydrocarbon group with 1 to 32 carbon atoms can be listed as: methyl, ethyl, propyl, butyl, pentyl, hexyl, octyl, decyl, undecyl, dodecyl, tetradecyl, hexadecyl, octadecyl, eicosyl, dodecyl, tetradecyl, hexadecyl, octadecyl, triacontyl, etc., straight-chain alkyl groups; isopropyl, dibutyl, tributyl, neopentyl, 1-ethylpropyl, 1-heptyldecyl, etc., branched alkyl groups, etc. In this specification, R 1 ~R 9 Preferably, it is a straight-chain or branched alkyl group having 1 to 25 carbon atoms (part of which may also be hydrogen atoms), more preferably a straight-chain or branched alkyl group having 1 to 22 carbon atoms (part of which may also be hydrogen atoms). Also, R 10 R 11 Preferably, it is a hydrogen atom or an alkyl group having 1 to 5 carbon atoms, and even more preferably, it is a hydrogen atom. Furthermore, p and q are preferably alkyl glycerol ether groups [-Q-OCH] 2-CH(OR 10 )-CH 2(OR 11 The content of [] is between 1% and 50% by mass, more preferably between 5% and 40% by mass, and even more preferably between 10% and 30% by mass. Specifically, in terms of the ease of obtaining the organopolysiloxane used as a raw material and the operability during manufacturing, p is in the range of 1 to 500, more preferably in the range of 10 to 30, and q is in the range of 1 to 50, more preferably in the range of 1 to 30. From the viewpoint of improving the tactile feel of the inorganic particles coated on the surface, the viscosity of alkyl glycerol ether modified polysiloxane at 25°C is preferably 1,000 mPa·s or higher, more preferably 2,000 mPa·s or higher, further preferably 3,000 mPa·s or higher, further preferably 4,000 mPa·s or higher, further preferably 5,000 mPa·s or higher, further preferably 6,000 mPa·s or higher, and preferably 20,000 mPa·s or lower, more preferably 10,000 mPa·s or lower, further preferably 8,000 mPa·s or lower, further preferably 7,000 mPa·s or lower. The above viscosity can be measured at 25°C using a Brookfield viscometer based on JIS Z 8803:2011 "Method for determination of viscosity of liquids". This type of alkyl glycerol ether modified polysiloxane can be manufactured by reacting an organohydrogen polysiloxane having at least one silicon-hydrogen bond with a corresponding alkenyl glycerol ether, according to the methods described in Japanese Patent Application Publication No. 4-134013 or Japanese Patent Application Publication No. 2005-194523. Furthermore, commercially available alkyl glycerol ether modified polysiloxanes include, for example, SI-UGE and Sofcare RS-U (both manufactured by Kao Corporation). These modified polysiloxanes (b1) can be a single type or a combination of two or more types. From the viewpoint of further improving the tactile feel and environmental adaptability of the surface-coated inorganic particles, the water-soluble cationic polymer (b2) preferably includes at least one selected from cationic polymers with a cellulose backbone, cationic vinyl polymers, chitin-chitosans, and hyaluronic acid halides; more preferably, it includes at least one selected from cationic polymers with a cellulose backbone, cationic vinyl polymers, chitin-chitosans, hyaluronic acid bromide, and hyaluronic acid chloride; even more preferably, it includes at least one selected from cationic polymers with a cellulose backbone, cationic vinyl polymers, and chitin-chitosans; further preferably, it includes at least one selected from cationic polymers with a cellulose backbone and cationic vinyl polymers; and even more preferably, it includes cationic vinyl polymers. In this specification, "water-soluble polymer" refers to a polymer that dissolves more than 2 g when 10 g of the polymer is mixed in 1000 mL of water at 20°C and pH 7 and allowed to stand for 24 hours. The water-soluble cationic polymer (b2) preferably has basic groups such as primary to tertiary amine groups, quaternary ammonium groups, and hydrazine groups, and more preferably has tertiary amine groups or quaternary ammonium groups. Furthermore, the basic groups include those neutralized by acids such as hydrochloric acid, sulfuric acid, nitric acid, acetic acid, formic acid, maleic acid, fumaric acid, citric acid, tartaric acid, adipic acid, and lactic acid. Also, in this specification, water-soluble cationic polysiloxane polymers (b2) such as water-soluble amine-modified polysiloxane are excluded. From the viewpoint of improving the tactile feel of the inorganic particles coated on the surface, the weight-average molecular weight (Mw) of the water-soluble cationic polymer (b2) is preferably 3,000 or more, more preferably 5,000 or more, further preferably 15,000 or more, further preferably 50,000 or more, and further preferably 100,000 or more. It is also preferably 5 million or less, more preferably 3 million or less, and further preferably 2 million or less. The aforementioned weight-average molecular weight (Mw) can be determined by gel filtration chromatography (GPC) using polyethylene glycol as a standard. For example, the weight-average molecular weight (Mw) of cationic hydroxyethyl cellulose (b2), a water-soluble cationic polymer, was determined by GPC under the following conditions. <GPC Determination Conditions> Sample Concentration: 1 mg / mL Column: 2 TSKgel α-M tubes (Tosoh) Dissociation Solution: 0.15 mol / L sodium sulfate aqueous solution (containing 1% acetic acid) Flow Rate: 1.0 mL / min Column Temperature: 40℃ Detector: Differential refractometer In this specification, the term "cationic polymer having a cellulose backbone" refers to a polymer having cationic groups and a cellulose backbone, and being cationic in overall charge. Furthermore, the term "cationic group" refers to a cationic group or a group that can be ionized to become a cationic group, such as primary amino groups, secondary amino groups, tertiary amino groups, and quaternary ammonium groups. Examples of cationic polymers having a cellulose backbone include cationized cellulose and cationized cellulose derivatives, specifically including: cationized cellulose, cationized hydroxyethyl cellulose, cationized hydroxypropyl cellulose, and cationized carboxymethyl cellulose. A preferred cationic polymer having a cellulose backbone is cationized hydroxyethyl cellulose, and more preferably a polymer of the quaternary ammonium salt obtained by the addition of glycidyltrimethylammonium chloride to p-hydroxyethyl cellulose (INCI name: polyquaternary ammonium salt-10). Examples of cationic vinyl polymers include: vinylpyrrolidone / dimethylaminoethyl methacrylate copolymer diethyl sulfate, vinylpyrrolidone / dimethylaminopropyl methacrylate / lauryl dimethylaminopropyl methacrylate copolymer, vinylpyrrolidone / N,N-dimethylaminoethyl methacrylate / alkyl acrylate / tripropylene glycol diacrylate copolymer, polydimethylmethylenepiperidinium chloride, dimethyldiallylammonium chloride / acrylamide copolymer, trimethylammonium propyl acrylamide chloride / dimethylacrylamide copolymer, and alkylacrylamide / acrylate / alkylaminoalkylpropylene. Acrylamide / polyethylene glycol methacrylate copolymer, tert-butylacrylamide / dimethacrylamide / dimethylaminopropylacrylamide / methoxypolyethylene glycol methacrylate copolymer, vinylpyrrolidone / N,N-dimethylaminoethyl methacrylate copolymer diethyl sulfate, vinylpyrrolidone / dimethylaminoethyl methacrylate copolymer, N,N-dimethylaminoethyl methacrylate diethyl ester sulfate / N,N-dimethylacrylamide / polyethylene glycol dimethacrylate copolymer, ammonium-modified hydroxyethyl cellulose, acrylamide / DMAPA acrylate / methoxyPEG methacrylate copolymer, etc. Among these, (meth)acrylic acid polymers containing tertiary amino groups are preferred, and acrylamide / DMAPA acrylate / methoxyPEG methacrylate copolymer is even more preferred. Examples of chitin-chitosan derivatives include hydroxypropyl chitosan, carboxymethyl chitin, and carboxymethyl chitosan, as well as chitin, chitosan, etc., with chitosan being the preferred choice. These water-soluble cationic polymers (b2) can be a single type or a combination of two or more types. The surface treatment agent (B) may also include surface treatment agents other than modified polysiloxane (b1) and water-soluble cationic polymer (b2). Examples of surface treatment agents other than modified polysiloxane (b1) and water-soluble cationic polymer (b2) include surface treatment agents applied to particles used in fragrances. From the viewpoint of further improving the tactile feel of the inorganic particles coated on the surface and further improving environmental adaptability, the content of at least one of the modified polysiloxane (b1) and water-soluble cationic polymer (b2) selected from the surface treatment agent (B) which are liquid at 25°C is preferably 50% by mass or more, more preferably 60% by mass or more, further preferably 70% by mass or more, further preferably 80% by mass or more, further preferably 90% by mass or more, further preferably 95% by mass or more, and preferably less than 100% by mass. From the viewpoint of further improving environmental adaptability, the content of the synthetic polymer that is solid at 25°C and is non-water-soluble in the surface treatment agent (B) is preferably less than 10% by mass, more preferably less than 5% by mass, and even more preferably less than 1% by mass, even more preferably less than 0.1% by mass, and even more preferably less than 0.01% by mass. The surface treatment agent (B) preferably does not substantially contain the synthetic polymer. Regarding the adsorption amount of the surface treatment agent (B) on the inorganic particles (A) in the surface-coated inorganic particles of the present invention, from the viewpoint of further improving the tactile feel, the adsorption amount relative to 100 parts by mass of the inorganic particles (A) is preferably 0.1 parts by mass or more, more preferably 0.5 parts by mass or more, further preferably 0.7 parts by mass or more, further preferably 0.9 parts by mass or more, further preferably 1.0 parts by mass or more, further preferably 1.5 parts by mass or more, further preferably 2.0 parts by mass or more, further preferably 2.5 parts by mass or more, and preferably 50 parts by mass or less, more preferably 30 parts by mass or less, further preferably 20 parts by mass or less, further preferably 15 parts by mass or less, further preferably 13 parts by mass or less, further preferably 10 parts by mass or less, further preferably 8 parts by mass or less. The adsorption amount of the surface treatment agent (B) can be determined using the method described in the examples. [Method for Manufacturing Surface-Coated Inorganic Particles] The surface-coated inorganic particles of the present invention can be obtained by coating inorganic particles (A) with a surface treatment agent (B). Specifically, from the viewpoint of coating the inorganic particles (A) with the surface treatment agent (B), the method for manufacturing surface-coated inorganic particles preferably includes the step of mixing the inorganic particles (A) with a surface treatment agent solution containing the surface treatment agent (B) and a solvent, and more preferably includes the step of mixing an inorganic particle dispersion containing the inorganic particles (A) and solvent A with a surface treatment agent solution containing the surface treatment agent (B) and solvent B. As the solvent, water or an organic solvent can be used. As an organic solvent, there is no particular limitation, for example, methanol, ethanol, 1-propanol, 2-propanol and other alcohols can be used. Among the alcohols, it is more preferably selected from at least one of ethanol and 2-propanol, and more preferably ethanol. Solvent A and solvent B can be the same, or they can be different as long as they are miscible. From the viewpoint of the dispersibility of inorganic particles (A), solvent A used in the inorganic particle dispersion is preferably selected from at least one of water and ethanol. When the surface treatment agent (B) contains modified polysiloxane (b1), from the viewpoint of the solubility of modified polysiloxane (b1), the solvent used in the surface treatment agent solution is preferably an organic solvent, and from the viewpoint of miscibility with solvent A, ethanol is more preferred. When the surface treatment agent (B) contains a water-soluble cationic polymer (b2), from the viewpoint of the solubility of the water-soluble cationic polymer (b2), the solvent used in the surface treatment agent solution is preferably selected from at least one of water and ethanol, and more preferably water. Furthermore, from the viewpoint of improving the solubility of the water-soluble cationic polymer (b2), organic acids such as lactic acid can also be added to the surface treatment agent solution. When using the above-mentioned inorganic particle dispersion, from the viewpoint of enabling the surface treatment agent (B) to be efficiently adsorbed onto the surface of the inorganic particles (A), the concentration of the inorganic particles (A) in the above-mentioned inorganic particle dispersion is preferably 0.5% by mass or more, more preferably 1.0% by mass or more, and more preferably 40% by mass or less, more preferably 30% by mass or less, further preferably 20% by mass or less, and further preferably 10% by mass or less. When using the above-mentioned surface treatment agent solution, from the viewpoint of enabling the surface treatment agent (B) to be efficiently adsorbed onto the surface of the inorganic particles (A), the concentration of the surface treatment agent (B) in the above-mentioned surface treatment agent solution is preferably 0.5% by mass or more, more preferably 1.0% by mass or more, and more preferably 40% by mass or less, more preferably 30% by mass or less, further preferably 20% by mass or less, and further preferably 10% by mass or less. From the viewpoint of efficiently adsorbing the surface treatment agent (B) onto the surface of the inorganic particles (A), the temperature at which the inorganic particles (A) or the aforementioned inorganic particle dispersion is mixed with the aforementioned surface treatment agent solution is preferably 5°C or higher, more preferably 10°C or higher; and from the viewpoint of suppressing solvent evaporation, it is preferably 70°C or lower, more preferably 50°C or lower. Furthermore, from the viewpoint of fully adsorbing the surface treatment agent (B) onto the surface of the inorganic particles (A), the mixing time of the inorganic particles (A) or the aforementioned inorganic particle dispersion with the aforementioned surface treatment agent solution is preferably 5 minutes or higher, more preferably 10 minutes or higher; and from the viewpoint of manufacturing efficiency, it is preferably 12 hours or lower, more preferably 6 hours or lower. A known stirring device can be used in the step of mixing the inorganic particles (A) or the aforementioned inorganic particle dispersion with the aforementioned surface treatment agent solution. The surface-coated inorganic particles can be recovered by separating the mixture obtained through the above steps using known methods such as centrifugation, filtration, decantation, and drying. The obtained surface-coated inorganic particles can also be classified using sieves to adjust the particle size. [Surface Modifier] The surface-coated inorganic particles of the present invention can be applied to surface modifiers. That is, the surface modifier of the present invention contains the surface-coated inorganic particles of the present invention. In this specification, "surface modifier" refers to something that can improve the tactile feel of the surface of skin, hair, nails, etc. The content of the surface-coated inorganic particles of the present invention in the surface modifier of the present invention is appropriately set according to the type of surface modifier, and therefore is not particularly limited. For example, it is 0.1% by mass or more, preferably 1% by mass or more, and for example, 50% by mass or less, preferably 30% by mass or less, and more preferably 10% by mass or less. The surface modifier of this invention may appropriately contain any component used according to the type of surface modifier, within a range that does not impair the effects of this invention. Examples of components other than the inorganic particles used for surface coating in this invention include: ultraviolet absorbers, oils, surfactants, water-soluble polymers, thickeners, neutralizers, sprays, pH adjusters, bactericides, anti-inflammatory agents, preservatives, colorants, chelating agents, whitening agents, blood flow promoters, cooling agents, antiperspirants, insecticides, physiologically active ingredients, salts, humectants, antioxidants, fragrances, plant extracts, etc. Examples of the forms of the surface modifier of this invention include: liquid, emulsion, cream, paste, gel, wax, and solid forms. The surface modifier of this invention can also be applied to tablets, sprays, mousses, etc. The surface modifier of this invention can be applied to skin (including lips), hair, nails, etc., preferably by coating. From the viewpoint of further improving environmental adaptability, the content of synthetic polymer microparticles in the surface modifier of the present invention is preferably less than 0.01% by mass, more preferably less than 0.005% by mass, and even more preferably less than 0.001% by mass. In this specification, synthetic polymer microparticles refer to synthetic polymers that are solid at 25°C and non-water-soluble, comprising 1% or more by mass of such polymers and have a median particle size (D). 50 () refers to microparticles with a diameter of 0.1 μm or larger and a diameter of 5 mm or smaller. There are no particular limitations on the manufacturing method of the surface modifier of the present invention. For example, it can be manufactured by stirring and mixing the components using a known device. [Fragrance Products] The inorganic particles coated on the surface of this invention can be formulated or applied to various fragrance products. That is, the fragrance products of this invention contain the inorganic particles coated on the surface of this invention. The content of the inorganic particles coated on the surface of this invention in the fragrance products of this invention is appropriately set according to the type of fragrance product, and therefore is not particularly limited. For example, it is 0.1% by mass or more, preferably 1% by mass or more, and for example, 50% by mass or less, preferably 30% by mass or less. In this specification, "fragrant products" refers to cosmetics, skin care products, hygiene products, perfumes, and other products that come into direct contact with the human body. The cosmetic products of this invention may appropriately contain any ingredients used according to the type of cosmetic product, within the scope that does not impair the effects of this invention. Examples of any ingredients other than the inorganic particles coated on the surface of this invention include: ultraviolet absorbers, oils, surfactants, water-soluble polymers, thickeners, neutralizers, sprays, pH adjusters, bactericides, anti-inflammatory agents, preservatives, colorants, chelating agents, whitening agents, blood flow promoters, cooling agents, antiperspirants, insecticides, physiologically active ingredients, salts, moisturizers, antioxidants, fragrances, plant extracts, etc. Examples of the forms of the cosmetic products of this invention include: liquid, lotion, cream, paste, gel, wax, and solid. The cosmetic products of this invention can also be applied to tablets, sprays, mousses, etc. The cosmetic products of this invention can be applied to skin (including lips), hair, nails, etc., preferably by application. From the viewpoint of further improving environmental adaptability, the content of synthetic polymer microparticles in the fragrance cosmetics of the present invention is preferably less than 0.01% by mass, more preferably less than 0.005% by mass, and even more preferably less than 0.001% by mass. The manufacturing method of the cosmetic product of the present invention is not particularly limited. For example, it can be manufactured by stirring and mixing the ingredients using a known device. [Surface Modification Method] The surface modification method of the present invention includes the step of applying the surface-coated inorganic particles of the present invention, the surface modifier of the present invention, or the fragrance of the present invention to a surface of a target object. Examples of target surfaces include skin, hair, and nails, with skin being preferred. Methods for applying the surface-coated inorganic particles, surface modifier, or fragrance of the present invention to a target surface include, for example, coating, spraying, or casting them onto the target surface, or immersing the target object in the surface-coated inorganic particles, surface modifier, or fragrance of the present invention. [Example] The present invention will now be described with reference to examples, but the invention is not limited to the scope of the examples. Furthermore, in these examples and comparative examples, various measurements and evaluations were performed using the following methods. [Determination and Evaluation Methods] (1) Determination of the Adsorption Amount of Surface Treatment Agent on Inorganic Particles The adsorption amount of the surface treatment agent was determined by thermogravimetric-differential calorimetry (TG-DTA) analysis of the sample using a thermal analysis apparatus (Thermo plus EVO2 TG-DTA8122) from Rigaku Corporation. The determination conditions are as follows. Sample preparation: Surface-coated inorganic particles and inorganic particles before surface coating (approximately 30 mg (accurately weighed)) obtained from the Examples and Comparative Examples Heating rate: 10℃ / min Measurement temperature range: 35~800℃ Measurement atmosphere: Air (180 mL / min) The adsorption amount of the surface treatment agent relative to 100 parts by mass of inorganic particles was calculated from the obtained TG-DTA curve using the following formula. Here, the adsorption amount of the surface treatment agent in the surface-coated inorganic particles is set as x mass% (the total amount of surface-coated inorganic particles is set as 100 mass%). The adsorption capacity (parts by mass) of the surface treatment agent relative to 100 parts by mass of inorganic particles is calculated as follows: x / (100 - x) × 100. x is calculated using the following formula: A × x / 100 + A × (1 - x / 100) × y = BA: Mass of the sample containing the surface-coated inorganic particles (mg); B: Mass reduction of the surface-coated inorganic particles from 100℃ to 800℃ (mg); y: Mass reduction rate of the inorganic particles before surface coating from 100℃ to 800℃ (= Mass reduction of the inorganic particles before surface coating from 100℃ to 800℃ / Mass of the sample containing the inorganic particles before surface coating). (2) The median particle size (D) of inorganic particles and surface-coated inorganic particles 50 The particle size distribution of inorganic particles and surface-coated inorganic particles was determined using a laser diffraction / scattering particle size analyzer LA-960 manufactured by Horiba Manufacturing Co., Ltd. Distilled water was added to the measuring tank, and the particle size distribution of inorganic particles and surface-coated inorganic particles was measured separately at a concentration where the absorbance was within an appropriate range. The median volume diameter (D) of both inorganic particles and surface-coated inorganic particles was calculated from the obtained particle size distribution. 50 ). (3) Functional Evaluation (3-1) Degree of No Dryness and Slipperyness: Under an environment of 20-25°C and 25-40%RH, 0.2 g of the particles obtained by the Examples and Comparative Examples were evenly coated onto the inner side of the forearm with a finger and the coating was rubbed with the finger to evaluate the degree of no dryness and slipperyness. Scoring was performed according to the following criteria. Three professional functional inspectors were assigned to each sample shown in the table below, and compared with the reference sample (lauryl methacrylate-ethylene glycol dimethacrylate-sodium methacrylate copolymer particles, median particle size (D)). 50 (2 μm, manufactured according to Example 1 of Japanese Patent Application Publication No. 2006-8980) The degree of "non-dryness" and "smoothness" of each tactile sensation were evaluated in comparison. A score of "5" was given for samples that were considered equivalent to the reference sample, with excellent non-dryness and smoothness; a score of "4" was given for samples that were slightly inferior to the reference sample but still had good non-dryness and smoothness; a score of "3" was given for samples that were inferior to the reference sample but still had average non-dryness and smoothness; a score of "2" was given for samples that were inferior to the reference sample but still had poor non-dryness and smoothness; and a score of "1" was given for samples that were significantly inferior to the reference sample but still had very poor non-dryness and smoothness. The average score from all evaluators was used. Furthermore, each evaluator scored using a 0.5 scale that included the median score. Here, the lauryl methacrylate-ethylene glycol dimethacrylate-sodium methacrylate copolymer particles mentioned above are equivalent to polymer particles commonly used as tactile enhancement particles. (3-2) Durability of tactile sensation: Under an environment of 20-25°C and 25-40%RH, 0.2 g of the particles obtained in the examples and comparative examples were evenly applied to the inner side of the forearm with a finger, and the entire coated area was rubbed 10 times with the finger. Subsequently, the degree of dryness and smoothness were evaluated by rubbing the coated material with the finger, and the scores were made according to the same criteria as in (3-1) above. (3-3) For the semi-dry stickiness, at a temperature of 20-25°C and a humidity of 25-40%RH, 0.1 mL of a 5% by mass water / ethanol dispersion (particles / water / ethanol = 5 / 70 / 25 by mass) of the particles obtained in the examples and comparative examples was applied to the inner side of the forearm in a pattern with a diameter of approximately 5 cm. The application was allowed to spread for 10 seconds, and the stickiness in the semi-dry state was evaluated. Scoring was performed according to the following criteria. Three professional functional inspectors were assigned to each sample shown in the table below, comparing it with the reference sample (lauryl methacrylate-ethylene glycol dimethacrylate-sodium methacrylate copolymer particles, median particle size (D...)). 50 The "stickiness in the semi-dry state" was evaluated by comparing samples (2 μm, manufactured according to Example 1 of Japanese Patent Application Publication No. 2006-8980). Samples deemed to have the same level of stickiness as the reference sample and excellent in the semi-dry state were rated "5"; samples deemed slightly worse than the reference sample but still exhibiting good stickiness in the semi-dry state were rated "4"; samples deemed worse than the reference sample but exhibiting average stickiness in the semi-dry state were rated "3"; samples deemed worse than the reference sample and exhibiting poorer stickiness in the semi-dry state were rated "2"; and samples deemed significantly worse than the reference sample and exhibiting very poor stickiness in the semi-dry state were rated "1". The average score from all evaluators was used. Furthermore, each evaluator scored using a 0.5 scale that included the median score. [Preparation of Inorganic Particles for Surface Coating] Example 1: 2 g of polyether-modified polysiloxane 1 (PEG-10 dimethicone, Shin-Etsu Chemical Industry Co., Ltd.'s "KF-6017", HLB: 4.5, viscosity at 25°C: 490 mPa·s) and 98 g of ethanol were added to a 500 mL beaker as surface treatment agents to prepare a polyether-modified polysiloxane solution. In a separate 500 mL beaker, silica 1 (porous silica particles, Nippon Chemi-Conducting Chemical Co., Ltd.'s "HCS 160M5") was added as inorganic particles, with a median particle size (D...). 50 (5 μm, pore volume: 0.7 mL / g) 2 g of ethanol and 98 g of ethanol were homogenized using an ultrasonic homogenizer (ULTRASONIC HOMOGENIZER US-600E, Nippon Seiki Co., Ltd.) at 200 W for 5 minutes to obtain a particle dispersion. The above-mentioned polyether-modified polysiloxane solution was added to the obtained particle dispersion, and the mixture was stirred at 600 rpm for 1 hour at room temperature using a magnetic stirrer. The resulting mixture was centrifuged at 3000 rpm for 30 minutes using a HITACHI CR21G III centrifuge to separate the particles (dispersion phase) and solution (dispersion medium). After removing the supernatant, the precipitate was dried overnight under reduced pressure at 50°C to obtain surface-coated inorganic particles. The obtained surface-coated inorganic particles were evaluated. The results are shown in the table below. Examples 2-6 and 9-11 involved changing the types of inorganic particles and surface treatment agents to those listed in the table below, while obtaining surface-coated inorganic particles using the same method as in Example 1. The obtained surface-coated inorganic particles were evaluated. The results are shown in the table below. Examples 7, 12, and 14: The types of inorganic particles and surface treatment agents were changed to those listed in the table below, and "98 g of ethanol" was changed to "98 g of water." Otherwise, surface-coated inorganic particles were obtained using the same method as in Example 1. The obtained surface-coated inorganic particles were evaluated. The results are shown in the table below. In Examples 8 and 13, the types of inorganic particles and surface treatment agents were changed to those listed in the table below, and "98 g of ethanol" was changed to "98 g of water." Furthermore, 40 mg of 90% lactic acid (product name: Musashino Lactic Acid 90, manufactured by Musashino Chemical Research Institute Co., Ltd.) was added to the resulting cationic ethylene polymer 1 solution. Otherwise, surface-coated inorganic particles were obtained using the same method as in Example 1. The obtained surface-coated inorganic particles were evaluated. The results are shown in the table below. Examples 15-19: The mixing amount of the surface treatment agent was varied such that the adsorption amount of the surface treatment agent became the value described in the table below. Otherwise, surface-coated inorganic particles were obtained using the same method as in Example 1. The obtained surface-coated inorganic particles were evaluated. The results are shown in the table below. Comparative Example 1: 2 g of ethanol was used instead of 2 g of polyether-modified polysiloxane. Otherwise, the inorganic particles were obtained using the same method as in Example 1. The resulting inorganic particles were evaluated. The results are shown in the table below. [Table 1] [Table 2] [Table 3] [Table 4] [Table 5] The ingredients listed in the table are as follows. (Inorganic particles) • Silicon dioxide 1 (Porous silicon dioxide particles, "HCS 160M5" manufactured by Nichibukai Catalyst Chemical Co., Ltd., with a volume median particle size (D) 50 ): 5 μm, pore volume: 0.7 mL / g, spherical) ・Silica 2 (porous silica particles, "Sunsphere H-51" manufactured by AGC SI-TECH Co., Ltd., with a volume median particle size (D 50 5 μm, pore volume: 1 mL / g, specific surface area: 800 m² 2 / g, spherical) ・Talc 1 (talc particles, "JA-13R" manufactured by Asada Flour Co., Ltd., median particle size (D 50 ): 6 μm, flake-like) ・Mica 1 (mica particles, "Y-1800" manufactured by YAMAGUCHI MICA Co., Ltd., with a volume median particle size (D 50 (10 μm, sheet-like) (Surface Treatment Agents) • Polyether-modified polysiloxane 1 (PEG-10 dimethicone, Shin-Etsu Chemical Co., Ltd.'s "KF-6017", HLB: 4.5, viscosity at 25°C: 490 mPa·s) • Polyether-modified polysiloxane 2 (PEG-11 methyl ether dimethicone, Shin-Etsu Chemical Co., Ltd.'s "KF-6011", HLB: 14.5, viscosity at 25°C: 130 mPa·s) • Polyether-modified polysiloxane 3 (Lauryl PEG-9 polydimethylsiloxyethyl dimethicone, Shin-Etsu Chemical Co., Ltd.'s "KF-6038", HLB: 3.0, viscosity at 25°C: 550 mPa·s) • Polyglycerol-modified polysiloxane 1 (polyglycerol-3-dimethylsiloxyethyl dimethoxysilane, manufactured by Shin-Etsu Chemical Industry Co., Ltd., "KF-6104", viscosity at 25°C: 3300 mPa·s) • Branched polyglycerol-modified polysiloxane 1 (bis(polyglycerol-3-oxyphenylpropyl)dimethoxysilane, manufactured by Kao Corporation, "Sofcare GS-G", viscosity at 25°C: 77000 mPa·s) • Alkyl glycerol ether-modified polysiloxane 1 (dialkyl(C16-18)glycerol-undecyl dimethoxysilane, manufactured by Kao Corporation, "Sofcare RS-U", viscosity at 25°C: 6200 mPa·s) • Cationic hydroxyethyl cellulose 1 (polytetraammonium salt-10, manufactured by Kao Corporation, "Poiz C-150L (Mw: 1,500,000) • Cationic vinyl polymer 1 (acrylamide / DMAPA acrylate / methoxyPEG methacrylate copolymer, manufactured according to manufacturing example 1 below) • Hymebromium bromide (HCS 160M5 manufactured by FUJI FILM Wako Pure Chemical Co., Ltd., Mw: 5,000~10,000) Example 1: A four-necked flask equipped with a reflux condenser, a liquid delivery device, a thermometer, a nitrogen inlet tube, and a stirrer was heated to 50°C in an oil bath. 100 parts by mass of monomer (monomer mass ratio: N-tert-butylacrylamide / N,N-dimethylacrylamide / methoxy polyethylene glycol monomethacrylate / N-(3-dimethylaminopropyl)acrylamide = 55 / 23 / 20 / 2) was dissolved in 75 parts by mass of ethanol to obtain a monomer solution. Additionally, 0.2 mol% of an initiator (V-65B) was dissolved in ethanol at a concentration of 5% by mass relative to the monomer to obtain an initiator solution. Under a nitrogen atmosphere, the obtained monomer solution and initiator solution were simultaneously added dropwise to the flask over 130 minutes, and the reaction was carried out at 50°C for 130 minutes, followed by a period of 80°C for 120 minutes. After polymerization, the polymer's ethanol solution was injected into n-hexane for reprecipitation purification, followed by vacuum drying at 80°C to obtain a solid cationic ethylene polymer 1. (Reagents used) ・N-tert-butylacrylamide (manufactured by Shin-Ling Co., Ltd.) ・N,N-dimethylacrylamide (manufactured by KJ Chemicals Co., Ltd.) ・Methoxy polyethylene glycol monomethacrylate (average addition mole number of ethylene oxide: 9 (manufactured by Shin-Nakamura Chemical Industry Co., Ltd., NK ESTER M-90G)) ・N-(3-dimethylaminopropyl)acrylamide (manufactured by KJ Chemicals Co., Ltd.) ・V-65B: 2,2'-azobis-(2,4-dimethylpentanonitrile) (manufactured by FUJI FILM Wako Pure Chemical Co., Ltd.) ・Ethanol (manufactured by FUJI FILM Wako Pure Chemical Co., Ltd.) ・n-Hexane (manufactured by FUJI FILM Wako Pure Chemical Co., Ltd.) As shown in the table above, the surface-coated inorganic particles of the embodiments exhibit excellent slipperiness, a lack of dryness, and consistent tactile feel, resulting in a pleasant tactile experience. Furthermore, it is evident that the surface-coated inorganic particles of the embodiments possess inorganic particles as core particles that are not equivalent to synthetic polymer microparticles, and the surface treatment agent does not contain synthetic polymers that are solid at 25°C and are non-water-soluble. Therefore, it is environmentally friendly and suitable as a substitute for synthetic polymer microparticles. [Industrial Applicability] According to one embodiment of the present invention, a surface-coated inorganic particle with a good tactile feel, suitable as a substitute for synthetic polymer microparticles, a surface modifier, and a fragrance / cosmetic product, as well as a surface modification method using the aforementioned surface-coated inorganic particle, the aforementioned surface modifier, or the aforementioned fragrance / cosmetic product, can be provided. Furthermore, according to one embodiment of the present invention, a method for manufacturing a surface-coated inorganic particle with a good tactile feel, suitable as a substitute for synthetic polymer microparticles, can be provided.

Claims

1. A surface-coated inorganic particle, wherein part or all of the surface of the inorganic particle (A) is coated with a surface treatment agent (B), wherein the inorganic particle (A) comprises silicon dioxide particles or mica particles, and the surface treatment agent (B) comprises a modified polysiloxane (b1) selected from those that are liquid at 25°C, wherein the modified polysiloxane (b1) comprises a polyether-modified polysiloxane, and wherein the polyether-modified polysiloxane is selected from PEG-3 dimethyl polysiloxane, PEG-9 dimethyl polysiloxane, PEG-9 methyl ether dimethyl polysiloxane, PEG-10 dimethyl polysiloxane, PEG-11 methyl ether dimethyl polysiloxane, PEG-12 dimethyl polysiloxane, PEG / PPG-20 / 22 butyl ether dimethyl polysiloxane, PEG-32 methyl ether dimethyl polysiloxane, PEG The surface treatment agent (B) is one or more of the following groups: polydimethylsiloxane-9, lauryl PEG-9, cetyl PEG / PPG-10 / 1, PEG / PPG-30 / 10, and linear polyether-modified polysiloxanes copolymerized by alternating dimethyl polysiloxane units and polyether units. The surface treatment agent (B) is adsorbed by intermolecular forces or ionic bonds, and the amount of surface treatment agent (B) adsorbed on the inorganic particles (A) is 0.1 parts by mass or more relative to 100 parts by mass of the inorganic particles (A).

2. The surface of the surface-coated inorganic particles as claimed in claim 1, wherein the amount of the surface treatment agent (B) adsorbed by the inorganic particles (A) is more than 0.1 parts by mass and less than 50 parts by mass relative to 100 parts by mass of the inorganic particles (A).

3. The surface of the surface coated with inorganic particles as claimed in claim 1 or 2, wherein the surface treatment agent (B) comprises more than 50% by mass of the modified polysiloxane (b1).

4. The surface of the inorganic particles (A) of the claimed item 1 or 2 is coated with inorganic particles, wherein the median particle size (D50) of the inorganic particles (A) is more than 1 μm and less than 30 μm.

5. The surface-coated inorganic particles of claim 1 or 2, wherein the volume median particle size (D50) of the surface-coated inorganic particles is greater than 1 μm and less than 30 μm.

6. The surface-coated inorganic particles of claim 1 or 2, wherein the content of the synthetic polymer that is solid at 25°C and non-water-soluble in the surface-coated inorganic particles is less than 1% by mass.

7. The surface of the surface of claim 1 or 2 is coated with inorganic particles, wherein the amount of the surface treatment agent (B) adsorbed by the inorganic particles (A) is more than 2.5 parts by mass and less than 8 parts by mass relative to 100 parts by mass of the inorganic particles (A).

8. The surface of the inorganic particles as claimed in claim 1 or 2, wherein the modified polysiloxane (b1) comprises polyether-modified polysiloxane with a viscosity of 130 mPa·s or more and 3,000 mPa·s or less.

9. A surface modifier comprising surface-coated inorganic particles as claimed in any one of claims 1 to 8.

10. A fragrance product comprising inorganic particles coated on the surface as claimed in any one of claims 1 to 8.

11. The fragrance product of claim 10, wherein the content of synthetic polymer microparticles in the aforementioned fragrance product does not reach 0.01 by mass.

12. A surface modification method comprising the steps of applying surface-coated inorganic particles as claimed in any one of claims 1 to 8, a surface modifier as claimed in claim 9, or a fragrance or cosmetic as claimed in claim 10 or 11 to a surface of an object.

13. The surface modification method of claim 12, wherein the surface of the object is skin.

14. A method for manufacturing surface-coated inorganic particles as claimed in any one of claims 1 to 8, comprising the step of mixing the inorganic particles (A) with a surface treatment agent solution containing the surface treatment agent (B) and a solvent.

Citation Information

Patent Citations

  • Powder treated by hydrophilicizing treatment and composition comprising it

    JP2004155978A

  • Powder composition, powder dispersion in oil and cosmetic containing them

    JP2004169015A