Description
Polymer Mixtures, Crosslinkable Compositions, and Articles The present invention relates to polymer mixtures, crosslinkable compositions, and articles. Patent Document 1 describes an emulsion mixture that is a microemulsion containing the composition of the following (1) and a microemulsion of the following (2). The microemulsion of the composition of (1) contains a crosslinkable fluororubber terpolymer "substantially composed of tetrafluoroethylene (TFE), perfluoroalkyl vinyl ether (PAVE), and perfluorocyanoether (CNVE) monomer units". The microemulsion of (2) contains a functionalized polytetrafluoroethylene (PTFE) polymer, and the functionalized polytetrafluoroethylene contains 0.1 to 3 mol% of perfluorocyanoether (CNVE); moreover, the particle diameter of the above functionalized PTFE polymer is about 10 nm to 100 nm. Furthermore, Patent Document 1 describes a crosslinkable composite containing the composition of the following (1) and the composition of the following (2). The composition of (1) contains a crosslinkable fluororubber terpolymer "substantially composed of tetrafluoroethylene (TFE), perfluoromethyl vinyl ether (PMVE), and perfluorocyanoether (CNVE)". The composition of (2) contains a functionalized polytetrafluoroethylene (PTFE) polymer, and the functionalized polytetrafluoroethylene has a particle diameter of 10 nm to 100 nm and contains a crosslinkable part. The above crosslinkable fluororubber terpolymer has a metal content of less than about 3000 ppb. Furthermore, when crosslinking the above PTFE and the fluororubber terpolymer to form a crosslinked composite, when tested at 150 °C, the crosslinked composite has a compression set of less than 50%. [Prior Art Documents] [Patent Documents] [Patent Document 1] Japanese Patent Application Laid-Open No. 2009-500459 [Problems to be Solved by the Invention] In the present invention, an object is to provide a polymer mixture containing a fluororubber and a crystalline fluoropolymer, and an article that can obtain "appropriate hardness, small compression set at high temperature, and furthermore, even after use under severe conditions, the compression set is not likely to increase significantly". [Technical Means for Solving the Problems] According to the present invention, a polymer mixture can be provided, which contains a fluororubber (a) and a crystalline fluoropolymer (b). The fluororubber (a) contains tetrafluoroethylene units, fluoroalkyl vinyl ether units, and a nitrogen-containing crosslinking site. The crystalline fluoropolymer (b) contains tetrafluoroethylene units and a nitrogen-containing crosslinking site; the melting point of the above polymer mixture is 310 to 320 °C, and the content of the crystalline fluoropolymer (b) in the above polymer mixture is: 4.0 to 15.0% by mass based on the total mass of the fluororubber (a) and the crystalline fluoropolymer (b). [Effects of the Invention] According to the present invention, a polymer mixture can be provided, which contains a fluororubber and a crystalline fluoropolymer, and an article having "appropriate hardness, small compression set at high temperature, and furthermore, even after use under severe conditions, the compression set is not likely to increase" can be obtained. Hereinafter, specific embodiments of the present invention will be described in detail, but the present invention is not limited to the following embodiments. The polymer mixture of the present invention contains a fluororubber (a) and a crystalline fluoropolymer (b). Patent Document 1 describes that by using the above crosslinkable composite material, a composite material having a compression set of less than 50% when tested at 150°C can be obtained. However, it has now been found that such a conventional composite material has a problem that "even when the compression set is small before use, if it is used under severe conditions, the compression set is likely to increase". In contrast, since the polymer mixture of the present invention has the above configuration, by using the polymer mixture of the present invention, not only an article having appropriate hardness and small compression set at high temperature can be obtained, but also an article in which the compression set is not likely to increase even after use under severe conditions can be obtained. Although the reason is not yet clear, it is speculated that: not only both the fluororubber (a) and the crystalline fluoropolymer (b) in the polymer mixture have nitrogen-containing crosslinking sites, but also the melting point of the polymer mixture and the content of the crystalline fluoropolymer (b) are appropriately adjusted, whereby the nitrogen-containing crosslinking site of the fluororubber (a) in the polymer mixture and the nitrogen-containing crosslinking site of the crystalline fluoropolymer (b) are co-crosslinked, and a co-crosslinked structure is formed in the article in an appropriate proportion. (Fluororubber (a)) The polymer mixture of the present invention contains a fluororubber (a). In the present invention, the fluororubber refers to an amorphous fluoropolymer. "Amorphous" means that the size of the melting peak (ΔH) exhibited by the fluoropolymer in differential scanning calorimetry [DSC] (heating rate 10°C / minute) or differential thermal analysis [DTA] (heating rate 10°C / minute) is 4.5 J / g or less. The fluororubber exhibits elastomeric properties by crosslinking. The elastomeric properties mean the following properties, that is, the polymer can be stretched, and when the force necessary to stretch the polymer is no longer applied, it can still maintain its original length. As the fluororubber, it can be a partially fluorinated elastomer or a perfluorinated elastomer. The perfluorinated elastomer is preferred because an article having a smaller compression set at high temperature can be obtained, and furthermore, an article in which the increase in compression set after use under severe conditions is more suppressed can be obtained. In the present invention, a partially fluorinated elastomer is a fluoropolymer containing fluoromonomer units, with the content of perfluoromonomer units being less than 90 mol% relative to the total monomer units, and having a glass transition temperature of 20°C or lower and a melting peak (ΔH) size of 4.5 J / g or lower. In the present invention, a perfluoroelastomer is a fluoropolymer in which the content of perfluoromonomer units is 90 mol% or more, preferably 91 mol% or more, relative to the total monomer units, and has a glass transition temperature of 20°C or lower and a melting peak (ΔH) size of 4.5 J / g or lower. Further, it is a polymer in which the concentration of fluorine atoms contained in the fluoropolymer is 71 mass% or more, preferably 71.5 mass% or more. In the present invention, regarding the concentration of fluorine atoms contained in the fluoropolymer, the concentration (mass%) of fluorine atoms contained in the fluoropolymer is calculated based on the types and contents of the respective monomers constituting the fluoropolymer. In the present invention, a perfluoromonomer refers to a monomer that does not contain a carbon atom-hydrogen atom bond in its molecule. The above perfluoromonomer may be a monomer in which several fluorine atoms bonded to a carbon atom are replaced by chlorine atoms in addition to carbon atoms and fluorine atoms, or may also have a nitrogen atom, an oxygen atom, a sulfur atom, a phosphorus atom, a boron atom, or a silicon atom in addition to carbon atoms. As the above perfluoromonomer, a monomer in which all hydrogen atoms are replaced by fluorine atoms is preferred. The above perfluoromonomer does not include a monomer that imparts a crosslinking site. A monomer that imparts a crosslinking site refers to a monomer having a "crosslinking group that imparts a crosslinking site for forming a crosslink to a fluoropolymer" (cure site monomer). In the present invention, the content of each monomer constituting the fluoroelastomer (a), the crystalline fluoropolymer (b), and the polymer mixture can be calculated by appropriately combining NMR, FT-IR, elemental analysis, fluorescent X-ray analysis, and other known methods according to the type of monomer. Regarding the Mooney viscosity ML(1+20) of the fluoroelastomer (a) at 170°C, in terms of being able to impart an appropriate hardness to an article, obtaining an article with a smaller compression set at high temperatures, and further obtaining an article in which the increase in compression set after use under severe conditions is more suppressed, it is preferably 30 or more, more preferably 50 or more, further preferably 60 or more, still more preferably 70 or more, preferably 150 or less, more preferably 130 or less, and further preferably 120 or less. The Mooney viscosity of the fluoroelastomer (a) can be adjusted to the above range by adjusting the composition, molecular weight, etc. of the monomers constituting the fluoroelastomer (a). The Mooney viscosity can be measured at 170°C according to JIS K6300 using a Mooney viscometer model MV2000E manufactured by ALPHA TECHNOLOGIES. Regarding the glass transition temperature of the fluoroelastomer (a), in terms of being able to impart appropriate hardness to an article, obtaining an article with a smaller compression set at high temperatures, and further obtaining an article in which an increase in compression set after use under severe conditions is more suppressed, it is preferably -30°C or higher, more preferably -20°C or higher, still more preferably -10°C or higher, preferably 10°C or lower, more preferably 5°C or lower, and still more preferably 0°C or lower. The glass transition temperature can be determined as follows: Using a differential scanning calorimeter (manufactured by Hitachi High-Tech Science Corporation, X-DSC7000), heating a 3 mg sample at 20°C / min to obtain a DSC curve, and taking the temperature representing "the midpoint of two intersection points of the extension line of the baseline before and after the second transition of the DSC curve and the tangent line at the inflection point of the DSC curve" as the glass transition temperature. The fluoroelastomer (a) contained in the polymer mixture of the present invention contains tetrafluoroethylene (TFE) units, fluoroalkyl vinyl ether (FAVE) units, and a nitrogen-containing crosslinking site. As the FAVE forming the FAVE unit, in terms of being able to obtain an article with a smaller compression set at high temperatures, and further obtaining an article in which an increase in compression set after use under severe conditions is more suppressed, it is preferably at least one selected from the group consisting of fluoro monomers represented by the following general formulae: General formula (11): CF 2 =CF-ORf 13 (wherein, Rf 13 represents a perfluoroalkyl group having 1 to 8 carbon atoms) represented fluoro monomer, General formula (12): CF 2 =CFOCF 2 ORf 14 (wherein, Rf 14 is a linear or branched perfluoroalkyl group having 1 to 6 carbon atoms, a cyclic perfluoroalkyl group having 5 to 6 carbon atoms, a linear or branched perfluorooxyalkyl group having 2 to 6 carbon atoms containing 1 to 3 oxygen atoms) represented fluoro monomer, and General formula (13): CF 2 =CFO(CF 2 CF(Y 15 )O) m (CF 2 ) n F (wherein Y 15 represents a fluorine atom or a trifluoromethyl group. m is an integer from 1 to 4. n is an integer from 1 to 4) the fluorine monomer represented. Among them, as the FAVE, the fluorine monomer represented by the general formula (11) is preferably used, and more preferably selected from CF 2 =CF-OCF 3 (perfluoro(methyl vinyl ether) (PMVE)), CF 2 =CF-OCF 2 CF 3 and CF 2 =CF-OCF 2 CF 2 CF 3 at least one selected from the group consisting of, and more preferably CF 2 =CF-OCF 3 . The fluorine elastomer (a) contained in the polymer mixture of the present invention contains a nitrogen-containing crosslinking site. The nitrogen-containing crosslinking site is a site containing at least one nitrogen atom and is the site where the fluorine elastomer (a) forms crosslinks. As the nitrogen-containing crosslinking site, a nitrogen-containing crosslinking group is preferably used. As the nitrogen-containing crosslinking group, as long as it contains at least one nitrogen atom and is a crosslinking group that imparts a crosslinking site for forming crosslinks to the fluoropolymer, there is no particular limitation, and examples thereof include: a cyano group, an azide group, a sulfonyl azide group, a carbonyl azide group, an amidino group, etc. As the nitrogen-containing crosslinking group, in terms of obtaining an article with a smaller compression set at high temperature and further obtaining an article in which the increase in compression set after use under severe conditions is more suppressed, a cyano group is preferred. When the fluorine elastomer (a) has a cyano group as the nitrogen-containing crosslinking site, the cyano group can form a tri ring by cyclotrimerization to crosslink, or a tetraamine compound can be used as a crosslinking agent to form an imidazole ring to crosslink. By forming crosslinks in this way, appropriate hardness and excellent compression set characteristics can be imparted to the article. A nitrogen-containing crosslinking site can be introduced into a fluororubber, for example, by copolymerizing a monomer having a nitrogen-containing crosslinkable group during the production of the fluororubber. Further, a nitrogen-containing crosslinking site can be introduced into the fluororubber, for example, by polymerizing a monomer in the presence of a nitrogen-containing chain transfer agent during the production of the fluororubber. Examples of the nitrogen-containing chain transfer agent include compounds represented by I(CF 2 ). n CN (n is an integer from 1 to 15). Furthermore, a nitrogen-containing crosslinking site can be introduced into the fluororubber, for example, by reacting a functional group (e.g., -COF, -COOH, etc.) generated at the end of the fluororubber with ammonia after the production of the fluororubber. In one embodiment of the fluororubber (a), it contains a monomer unit having a nitrogen-containing crosslinkable group. As the monomer having a nitrogen-containing crosslinkable group, a monomer having a cyano group is preferred. Examples of the monomer having a cyano group (-CN group) include monomers represented by the following formulae: Formula: CY 1 2 =CY 1 (CF 2 ). n -CN (wherein Y 1 are each independently a hydrogen atom or a fluorine atom, and n is an integer from 1 to 8) Formula: CF 2 =CFCF 2 Rf 8 -CN (wherein Rf 8 is -(OCF 2 ). n - or -(OCF(CF 3 ). n -, and n is an integer from 0 to 5) Formula: CF 2 =CFCF 2 (OCF(CF 3 )CF 2 ) m (OCH 2 CF 2 CF 2 ) n OCH 2 CF 2 - CN (where m is an integer from 0 to 5 and n is an integer from 0 to 5) Formula: CF 2 = CFCF 2 (OCH 2 CF 2 CF 2 ) m (OCF(CF 3 )CF 2 ) n OCF(CF 3 ) - CN (where m is an integer from 0 to 5 and n is an integer from 0 to 5) Formula: CF 2 = CF(OCF 2 CF(CF 3 )) m O(CF 2 ) n - CN (where m is an integer from 0 to 5 and n is an integer from 1 to 8) Formula: CF 2 = CF(OCF 2 CF(CF 3 )) m - CN (where m is an integer from 1 to 5) Formula: CF 2 = CFOCF 2 (CF(CF 3 )OCF 2 ) n CF(−CN)CF 3 (where n is an integer from 1 to 4) Formula: CF 2 =CFO(CF 2 ) n OCF(CF 3 )−CN (where n is an integer from 2 to 5) Formula: CF 2 =CFO(CF 2 ) n −(C 6 H 4 )−CN (where n is an integer from 1 to 6) Formula: CF 2 =CF(OCF 2 CF(CF 3 )) n OCF 2 CF(CF 3 )−CN (where n is an integer from 1 to 2) Formula: CH 2 =CFCF 2 O(CF(CF 3 )CF 2 O) n CF(CF 3 )−CN (where n is an integer from 0 to 5), Formula: CF 2 =CFO(CF 2 CF(CF 3 )O) m (CF 2 ) n -CN (where m is an integer from 0 to 5 and n is an integer from 1 to 3) Formula: CH 2 =CFCF 2 OCF(CF 3 )OCF(CF 3 )-CN Formula: CH 2 =CFCF 2 OCH 2 CF 2 -CN Formula: CF 2 =CFO(CF 2 CF(CF 3 )O) m CF 2 CF(CF 3 )-CN (where m is an integer of 0 or more) Formula: CF 2 =CFOCF(CF 3 )CF 2 O(CF 2 ) n -CN (where n is an integer of 1 or more) Formula: CF 2 =CFOCF 2 OCF 2 CF(CF 3 )OCF 2 -CN Formula: CF 2 =CFO(CF 2 ) 3 CN formula: CF 2 =CFO(CF 2 ) 5 CN, which can be used separately or in any combination. Among the above, preferably the formula: CF 2 =CF(OCF 2 CF(CF 3 )) m O(CF 2 ) n -CN (where m is an integer from 0 to 5 and n is an integer from 1 to 8) represented by the monomer, more preferably CF 2 =CFOCF 2 CF(CF 3 )OCF 2 CF 2 CN. Regarding the content of the nitrogen-containing crosslinking site in the fluororubber (a), when the total monomer units constituting the fluororubber (a) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the nitrogen-containing crosslinking site can be measured by infrared spectroscopy (IR). Regarding the content of the nitrogen-containing crosslinking group in the fluororubber (a), when the total monomer units constituting the fluororubber (a) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the nitrogen-containing crosslinking group can be measured by infrared spectroscopy (IR). Regarding the content of the cyano group in the fluororubber (a), when the total monomer units constituting the fluororubber (a) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the cyano group can be measured by infrared spectroscopy (IR). Regarding the content of the monomer unit having a nitrogen-containing crosslinkable group in the fluoroelastomer (a), when the total monomer units constituting the fluoroelastomer (a) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the monomer unit having a nitrogen-containing crosslinkable group can be measured by infrared spectroscopy (IR). Regarding the content of the monomer unit having a cyano group in the fluoroelastomer (a), when the total monomer units constituting the fluoroelastomer (a) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the monomer unit having a cyano group can be measured by infrared spectroscopy (IR). As the fluoroelastomer (a), a copolymer containing TFE units, FAVE units and monomer units having a nitrogen-containing crosslinkable group is preferred, a copolymer containing TFE units, FAVE units and monomer units having a cyano group is more preferred, and a copolymer containing TFE units, PMVE units and monomer units having a cyano group is still more preferred. Regarding the content of TFE units and FAVE units in the fluoroelastomer (a), when the total monomer units constituting the fluoroelastomer (a) are set to 100 mol%, it is preferably 97.0 to 99.5 mol%, more preferably 98.0 mol% or more, and still more preferably 98.5 mol% or more. In the copolymer containing TFE units, FAVE units and monomer units having a nitrogen-containing crosslinkable group, the content ratio (mol%) of TFE units / FAVE units / monomer units having a nitrogen-containing crosslinkable group is preferably 44.0 to 89.9 / 9.6 to 54.9 / 0.5 to 3.0, more preferably 50.0 to 78.0 / 20.0 to 49.5 / 0.5 to 2.0, and still more preferably 55.0 to 69.5 / 30.0 to 44.5 / 0.5 to 1.5. (Crystalline fluoropolymer (b)) The polymer mixture of the present invention contains a crystalline fluoropolymer (b). In the present invention, the crystalline fluoropolymer refers to a partially crystalline fluoropolymer, which is a fluoroplastic. The crystalline fluoropolymer has a melting point, has thermoplasticity, and can be melt-processable or non-melt-processable. In the present invention, melt-processability means that the polymer can be melted and processed using conventional processing machines such as an extruder and an injection molding machine. The melting point of the crystalline fluoropolymer (b) is 310 to 320 °C. The melting point is preferably 311 °C or higher, more preferably 312 °C or higher, still more preferably 313 °C or higher, preferably 319 °C or lower, and more preferably 318 °C or lower. If the melting point of the crystalline fluoropolymer (b) is too low, there is a risk that it will be difficult to obtain an article with a small compression set at high temperatures. If the melting point of the crystalline fluoropolymer (b) is too high, there is a risk that it will be difficult to obtain an article whose compression set does not easily increase even after use under severe conditions. The melting point of the crystalline fluoropolymer (b) can be adjusted to the above range, for example, by adjusting the composition of the monomers constituting the crystalline fluoropolymer (b). If the content of tetrafluoroethylene units increases, the melting point of the crystalline fluoropolymer (b) tends to increase, and if the content of tetrafluoroethylene units decreases, the melting point of the crystalline fluoropolymer (b) tends to decrease. Regarding the melting point of the crystalline fluoropolymer (b), it can be measured as follows: accurately weigh about 10 mg of the crystalline fluoropolymer (b) that has not been heated to a temperature above 300 °C and has no heating history, and place it in a special aluminum pan, and use TG / DTA (differential thermal thermogravimetric simultaneous measurement device) for measurement. In an atmospheric environment, the aluminum pan is heated from 25 °C to 600 °C at a rate of 10 °C / min to obtain a DTA curve, and the temperature corresponding to the peak in the obtained DTA curve is defined as the melting point of the polymer mixture. Regarding the melting point of the crystalline fluoropolymer (b), when the substance showing the melting point in the polymer mixture is only the crystalline fluoropolymer (b), it can be regarded as the same as the melting point of the polymer mixture. Therefore, by measuring the melting point of the polymer mixture, the melting point of the crystalline fluoropolymer (b) can also be grasped. The crystalline fluoropolymer (b) contained in the polymer mixture of the present invention contains tetrafluoroethylene (TFE) units and nitrogen-containing crosslinked sites. The crystalline fluoropolymer (b) may also contain other monomer units formed by other monomers copolymerizable with TFE (wherein, TFE units and monomer units having nitrogen-containing crosslinkable groups are not included). As other monomers (wherein, TFE and monomers having nitrogen-containing crosslinkable groups are not included), as long as they are copolymerizable with TFE, there is no particular limitation, and examples include: perfluoroolefins such as hexafluoropropylene [HFP]; chlorofluoroolefins such as chlorotrifluoroethylene [CTFE]; hydrogen-containing fluoroolefins such as trifluoroethylene and vinylidene fluoride [VDF]; perfluoroethyl vinyl ether; perfluoroalkyl ethylene; ethylene, etc. Regarding the content of other monomer units in the crystalline fluoropolymer (b), relative to the total monomer units constituting the crystalline fluoropolymer (b), it is preferably 0 to 0.10 mol%, more preferably 0.06 mol% or less, still more preferably 0.02 mol% or less, and may also be 0 mol%. The crystalline fluoropolymer (b) contained in the polymer mixture of the present invention contains a nitrogen-containing crosslinking site. The nitrogen-containing crosslinking site is a site containing at least one nitrogen atom and is the site where the crystalline fluoropolymer (b) forms a crosslink. As the nitrogen-containing crosslinking site, a nitrogen-containing crosslinkable group is preferred. As the nitrogen-containing crosslinkable group, as long as it contains at least one nitrogen atom and is a crosslinkable group that can impart a crosslinking site for the fluoropolymer to form a crosslink, there is no particular limitation. For example, it can be exemplified by a cyano group, an azide group, a sulfonyl azide group, a carbonyl azide group, an amidino group, etc. As the nitrogen-containing crosslinkable group, in terms of obtaining an article with a smaller compression set at high temperatures, and further obtaining an article in which the increase in compression set after use under severe conditions is more suppressed, a cyano group is preferred. When the fluoroelastomer (b) has a cyano group as the nitrogen-containing crosslinking site, the cyano group can form a triazine ring through cyclotrimerization to crosslink, or a tetraamine compound can be used as a crosslinking agent to form an imidazole ring to crosslink. By forming a crosslink in this way, appropriate hardness and excellent compression set characteristics can be imparted to the article. The nitrogen-containing crosslinking site can be introduced into the crystalline fluoropolymer, for example, by copolymerizing a monomer having a nitrogen-containing crosslinkable group when manufacturing the crystalline fluoropolymer. Also, the nitrogen-containing crosslinking site can be introduced into the crystalline fluoropolymer, for example, by polymerizing a monomer in the presence of a nitrogen-containing chain transfer agent when manufacturing the crystalline fluoropolymer. As the nitrogen-containing chain transfer agent, a compound represented by I(CF)nCN (n is an integer from 1 to 15) can be exemplified. Further, the nitrogen-containing crosslinking site can be introduced into the crystalline fluoropolymer, for example, by reacting a functional group (such as -COF, -COOH, etc.) generated at the end of the crystalline fluoropolymer with ammonia after manufacturing the crystalline fluoropolymer. In one embodiment of the crystalline fluoropolymer (b), it contains a monomer unit having a nitrogen-containing crosslinkable group. 2 ) n CN (n is an integer from 1 to 15). Further, the nitrogen-containing crosslinking site can be introduced into the crystalline fluoropolymer, for example, by reacting a functional group (such as -COF, -COOH, etc.) generated at the end of the crystalline fluoropolymer with ammonia after manufacturing the crystalline fluoropolymer. In one embodiment of the crystalline fluoropolymer (b), it contains a monomer unit having a nitrogen-containing crosslinkable group. As the monomer having a nitrogen-containing crosslinkable group, a monomer having a cyano group is preferred. As the monomer having a cyano group (-CN group), for example, monomers represented by the following formula can be exemplified: Formula: CY 1 2 =CY 1 (CF 2 ) n -CN (where Y 1 are each independently a hydrogen atom or a fluorine atom, and n is an integer from 1 to 8) Formula: CF 2 =CFCF 2 Rf 8 -CN (where Rf 8 is -(OCF 2 ) n - or -(OCF(CF 3 )) n -, and n is an integer from 0 to 5) Formula: CF 2 =CFCF 2 (OCF(CF 3 )CF 2 ) m (OCH 2 CF 2 CF 2 ) n OCH 2 CF 2 -CN (where m is an integer from 0 to 5 and n is an integer from 0 to 5) Formula: CF 2 =CFCF 2 (OCH 2 CF 2 CF 2 ) m (OCF(CF 3)CF 2 ) n OCF(CF 3 )-CN (where m is an integer from 0 to 5 and n is an integer from 0 to 5) Formula: CF 2 =CF(OCF 2 CF(CF 3 )) m O(CF 2 ) n -CN (where m is an integer from 0 to 5 and n is an integer from 1 to 8) Formula: CF 2 =CF(OCF 2 CF(CF 3 )) m -CN (where m is an integer from 1 to 5) Formula: CF 2 =CFOCF 2 (CF(CF 3 )OCF 2 ) n CF(-CN)CF 3 (where n is an integer from 1 to 4) Formula: CF 2 =CFO(CF 2 ) n OCF(CF 3 )-CN (where n is an integer from 2 to 5) Formula: CF 2 =CFO(CF 2 ) n -(C 6 H 4 ) - CN (wherein, n is an integer from 1 to 6) formula: CF 2 =CF(OCF 2 CF(CF 3 )) n OCF 2 CF(CF 3 ) - CN (wherein, n is an integer from 1 to 2) formula: CH 2 =CFCF 2 O(CF(CF 3 )CF 2 O) n CF(CF 3 ) - CN (wherein, n is an integer from 0 to 5), formula: CF 2 =CFO(CF 2 CF(CF 3 )O) m (CF 2 ) n -CN (wherein, m is an integer from 0 to 5, n is an integer from 1 to 3) formula: CH 2 =CFCF 2 OCF(CF 3 )OCF(CF 3 )-CN formula: CH 2 =CFCF 2 OCH 2 CF 2 -CN formula: CF 2 =CFO(CF 2 CF (CF 3 ) O) m CF 2 CF (CF 3 ) - CN (where m is an integer of 0 or more) Formula: CF 2 =CFOCF (CF 3 ) CF 2 O (CF 2 ) n - CN (where n is an integer of 1 or more) Formula: CF 2 =CFOCF 2 OCF 2 CF (CF 3 ) OCF 2 - CN Formula: CF 2 =CFO (CF 2 ) 3 CN Formula: CF 2 =CFO (CF 2 ) 5 CN, and these can be used separately alone or in any combination. Among the above, preferably the formula: CF 2 =CF (OCF 2 CF (CF 3 )) m O (CF 2 ) n - CN (where m is an integer from 0 to 5 and n is an integer from 1 to 8) monomer represented by, more preferably CF 2=CFOCF 2 CF (CF 3 ) OCF 2 CF 2 CN. Regarding the content of the nitrogen-containing crosslinked sites in the crystalline fluoropolymer (b), when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the nitrogen-containing crosslinked sites can be measured by infrared spectroscopy (IR). Regarding the content of the nitrogen-containing crosslinkable groups in the crystalline fluoropolymer (b), when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the nitrogen-containing crosslinkable groups can be measured by infrared spectroscopy (IR). Regarding the content of the cyano groups in the crystalline fluoropolymer (b), when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the cyano groups can be measured by infrared spectroscopy (IR). Regarding the content of the monomer units having nitrogen-containing crosslinkable groups in the crystalline fluoropolymer (b), when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the monomer units having nitrogen-containing crosslinkable groups can be measured by infrared spectroscopy (IR). Regarding the content of the monomer units having cyano groups in the crystalline fluoropolymer (b), when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and still more preferably 1.5 mol% or less. The content of the monomer units having cyano groups can be measured by infrared spectroscopy (IR). As the crystalline fluoropolymer (b), a copolymer containing TFE units and monomer units having nitrogen-containing crosslinkable groups is preferred, and a copolymer containing TFE units and monomer units having cyano groups is more preferred. Regarding the content of TFE units in the crystalline fluoropolymer (b), when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 97.0 to 99.5 mol%, more preferably 98.0 mol% or more, and still more preferably 98.5 mol% or more. (Polymer mixture) The polymer mixture of the present invention has a melting point of 310 to 320 °C. The melting point of the polymer mixture is preferably 311 °C or higher, more preferably 312 °C or higher, still more preferably 313 °C or higher, preferably 319 °C or lower, and more preferably 318 °C or lower. If the melting point of the polymer mixture is too low, there is a risk that it will be difficult to obtain an article with a small compression set at high temperatures. If the melting point of the polymer mixture is too high, there is a risk that it will be difficult to obtain an article whose compression set does not easily increase even after use under severe conditions. If a polymer mixture that does not show a clear melting point is used, there is a risk that it will be difficult to obtain an article with appropriate hardness. The melting point of the polymer mixture can be adjusted to the above range, for example, by adjusting the melting point of the crystalline fluoropolymer (b) and the content of the crystalline fluoropolymer (b). Regarding the melting point of the polymer mixture, it can be measured in the following manner: accurately weigh about 10 mg of the polymer mixture that has not been heated to a temperature above 300 °C and has no heating history, and place it in a special aluminum pan. Use TG / DTA (differential thermal thermogravimetric simultaneous measurement device) for measurement. In an atmospheric environment, heat the aluminum pan from 25 °C to 600 °C at a rate of 10 °C / minute to obtain a DTA curve, and define the temperature corresponding to the peak in the obtained DTA curve as the melting point of the polymer mixture. Regarding the Mooney viscosity ML(1+20) of the polymer mixture at 170 °C, in terms of being able to impart appropriate hardness to the article, obtaining an article with a smaller compression set at high temperatures, and further obtaining an article in which the increase in compression set after use under severe conditions is more suppressed, it is preferably 30 to 150, more preferably 50 or more, still more preferably 60 or more, even more preferably 70 or more, preferably 130 or less, and still more preferably 120 or less. The Mooney viscosity of the polymer mixture can be adjusted to the above range, for example, by adjusting the Mooney viscosity of the fluoroelastomer (a) and the content of the fluoroelastomer (a). The Mooney viscosity can be measured at 170 °C in accordance with JIS K6300 using a Mooney viscometer model MV2000E manufactured by ALPHA TECHNOLOGIES. Regarding the glass transition temperature of the polymer mixture, in terms of being able to impart appropriate hardness to an article, obtaining an article with less compression set at high temperatures, and further obtaining an article in which an increase in compression set after use under severe conditions is more suppressed, it is preferably -30°C or higher, more preferably -20°C or higher, still more preferably -10°C or higher, preferably 10°C or lower, more preferably 5°C or lower, and still more preferably 0°C or lower. The glass transition temperature can be determined as follows: Using a differential scanning calorimeter (manufactured by Hitachi High-Tech Science Corporation, X-DSC7000), heating a 3 mg sample at 20°C / min to obtain a DSC curve, and taking the temperature representing "the midpoint of two intersection points of the extension line of the baseline before and after the secondary transition of the DSC curve and the tangent line at the inflection point of the DSC curve" as the glass transition temperature. The polymer mixture of the present invention contains a fluororubber (a) and a crystalline fluoropolymer (b). Regarding the content of the crystalline fluoropolymer (b) in the polymer mixture, it is 4.0 to 15.0% by mass based on the total mass of the fluororubber (a) and the crystalline fluoropolymer (b). Regarding the content of the crystalline fluoropolymer (b) in the polymer mixture, it is preferably 4.2% by mass or more, more preferably 4.4% by mass or more, still more preferably 4.6% by mass or more, preferably 14.0% by mass or less, more preferably 13.0% by mass or less, and still more preferably 12.0% by mass or less. If the content of the crystalline fluoropolymer (b) in the polymer mixture is too small, it becomes difficult to impart appropriate hardness to the article. If the content of the crystalline fluoropolymer (b) in the polymer mixture is too large, the hardness of the article becomes too high, or it becomes difficult to obtain an article with a small compression set at high temperatures, or it becomes difficult to obtain an article in which the compression set does not easily increase even after use under severe conditions. Regarding the content of the crystalline fluoropolymer (b) in the polymer mixture, it can be measured as follows: Accurately weigh about 10 mg of the polymer mixture that has no heating history to a temperature above 300°C, and place it in a special aluminum pan, and measure it using TG / DTA (differential thermal thermogravimetric simultaneous measurement device). In an air atmosphere, heat the aluminum pan in the temperature range from 25°C to 600°C at a rate of 10°C / min to obtain a TG curve, and calculate the weight loss rate based on the obtained TG curve to define it. Usually, the fluororubber (a) in the polymer mixture decomposes thermally at a lower temperature than the crystalline fluoropolymer (b), so the weight loss rates caused by the thermal decomposition of the fluororubber (a) and the crystalline fluoropolymer (b) can be respectively grasped from the TG curve. Further, regarding the content of the crystalline fluoropolymer (b) in the polymer mixture, when the production conditions of the polymer mixture can be controlled, the content of the crystalline fluoropolymer (b) in the polymer mixture can be determined by calculation based on the usage amount of the raw materials. The polymer mixture of the present invention contains a fluoroelastomer (a) and a crystalline fluoropolymer (b). Further, the fluoroelastomer (a) contains tetrafluoroethylene units, fluoroalkyl vinyl ether units, and a nitrogen-containing crosslinking site, and the crystalline fluoropolymer (b) contains tetrafluoroethylene units and a nitrogen-containing crosslinking site. As the FAVE that forms the FAVE unit, in terms of obtaining an article with a smaller compression set at high temperatures and further obtaining an article in which an increase in compression set after use under severe conditions is more suppressed, it is preferably at least one selected from the group consisting of fluoromonomers represented by the following general formula, namely: General formula (11): CF 2 =CF-ORf 13 (In the formula, Rf 13 represents a perfluoroalkyl group having 1 to 8 carbon atoms) the fluoromonomer represented by, General formula (12): CF 2 =CFOCF 2 ORf 14 (In the formula, Rf 14 is a linear or branched perfluoroalkyl group having 1 to 6 carbon atoms, a cyclic perfluoroalkyl group having 5 to 6 carbon atoms, or a linear or branched perfluorooxyalkyl group having 2 to 6 carbon atoms containing 1 to 3 oxygen atoms) the fluoromonomer represented by, and General formula (13): CF 2 =CFO(CF 2 CF(Y 15 )O) m (CF 2 ) n F (In the formula, Y 15 represents a fluorine atom or a trifluoromethyl group. m is an integer from 1 to 4. n is an integer from 1 to 4) the fluoromonomer represented by. Among them, as the FAVE, the fluoromonomer represented by the general formula (11) is preferred, and more preferably selected from CF 2 =CF-OCF 3 (perfluoro(methyl vinyl ether) (PMVE)), CF 2 =CF-OCF 2 CF 3 and CF 2 =CF-OCF 2 CF 2 CF 3 at least one selected from the group consisting of, and more preferably CF 2 =CF-OCF 3 . Regarding the content ratio of tetrafluoroethylene units and fluoroalkyl vinyl ether units in the polymer mixture, in terms of molar ratio (tetrafluoroethylene units / fluoroalkyl vinyl ether units), it is preferably 50 / 50 to 70 / 30, more preferably 51 / 49 or more, still more preferably 52 / 48 or more, still more preferably 53 / 47 or more, more preferably 69 / 31 or less, still more preferably 68 / 32 or less. Also, regarding the content ratio of tetrafluoroethylene units and fluoroalkyl vinyl ether units in the polymer mixture, in terms of molar ratio (tetrafluoroethylene units / fluoroalkyl vinyl ether units), it can be 54 / 46 or more, or can be 65 / 35 or less or 60 / 40 or less. If the molar ratio (tetrafluoroethylene units / fluoroalkyl vinyl ether units) is too high, there is a risk that it becomes difficult to impart appropriate hardness to the article. If the molar ratio is too low, there is a risk that the hardness of the article becomes too high, and it becomes difficult to obtain an article with a small compression set at high temperatures, or it becomes difficult to obtain an article whose compression set does not easily increase even after use under severe conditions. The fluororubber (a) and the crystalline fluoropolymer (b) contain nitrogen-containing crosslinking sites. The nitrogen-containing crosslinking site is a site containing at least one nitrogen atom, and is the site where the fluororubber (a) and the crystalline fluoropolymer (b) in the polymer mixture are used for crosslinking. As the nitrogen-containing crosslinking site, a nitrogen-containing crosslinkable group is preferred. As the nitrogen-containing crosslinkable group, as long as it contains at least one nitrogen atom and is a crosslinkable group capable of imparting a crosslinking site for the fluoropolymer to form a crosslink, there is no particular limitation. For example, it may include: cyano group, azide group, sulfonyl azide group, carbonyl azide group, amidino group, etc. As the nitrogen-containing crosslinkable group, in terms of obtaining an article with a smaller compression set at high temperature and further obtaining an article in which the increase in compression set after use under severe conditions is more suppressed, a cyano group is preferred. When the fluororubber (a) and the crystalline fluoropolymer (b) have a cyano group as the nitrogen-containing crosslinking site, the cyano group can form a triazine ring through cyclotrimerization to carry out crosslinking, or use a tetraamine compound as a crosslinking agent to form an imidazole ring for crosslinking. By forming crosslinks in this way, appropriate hardness and excellent compression set characteristics can be imparted to the article. The nitrogen-containing crosslinking site can be introduced into the crystalline fluoropolymer, for example, by copolymerizing a monomer having a nitrogen-containing crosslinkable group when manufacturing the fluororubber and the crystalline fluoropolymer. Also, the nitrogen-containing crosslinking site can be introduced into the fluororubber and the crystalline fluoropolymer, for example, by polymerizing a monomer in the presence of a nitrogen-containing chain transfer agent when manufacturing the fluororubber and the crystalline fluoropolymer. As the nitrogen-containing chain transfer agent, compounds represented by I(CF 2 ) n CN (n is an integer from 1 to 15) can be cited. Furthermore, the nitrogen-containing crosslinking site can be introduced into the fluororubber and the crystalline fluoropolymer, for example, by reacting a functional group (for example, -COF, -COOH, etc.) generated at the end of the fluororubber and the crystalline fluoropolymer with ammonia after manufacturing the fluororubber and the crystalline fluoropolymer. In one embodiment of the fluororubber (a) and the crystalline fluoropolymer (b), a monomer unit having a nitrogen-containing crosslinkable group is contained. As the monomer having a nitrogen-containing crosslinkable group, a monomer having a cyano group is preferred. As the monomer having a cyano group (-CN group), for example, monomers represented by the following formula can be cited: Formula: CY 1 2 =CY 1 (CF 2 ) n -CN (wherein Y 1 are each independently a hydrogen atom or a fluorine atom, and n is an integer from 1 to 8) Formula: CF 2 =CFCF 2 Rf 8 -CN (wherein, Rf 8 is -(OCF 2 ) n - or -(OCF(CF 3 )) n -, n is an integer from 0 to 5) formula: CF 2 =CFCF 2 (OCF(CF 3 )CF 2 ) m (OCH 2 CF 2 CF 2 ) n OCH 2 CF 2 -CN (wherein, m is an integer from 0 to 5, n is an integer from 0 to 5) formula: CF 2 =CFCF 2 (OCH 2 CF 2 CF 2 ) m (OCF(CF 3 )CF 2 ) n OCF(CF 3 )-CN (wherein, m is an integer from 0 to 5, n is an integer from 0 to 5) formula: CF 2=CF(OCF 2 CF(CF 3 )) m O(CF 2 ) n -CN (where m is an integer from 0 to 5 and n is an integer from 1 to 8) formula: CF 2 =CF(OCF 2 CF(CF 3 )) m -CN (where m is an integer from 1 to 5) formula: CF 2 =CFOCF 2 (CF(CF 3 )OCF 2 ) n CF(-CN)CF 3 (where n is an integer from 1 to 4) formula: CF 2 =CFO(CF 2 ) n OCF(CF 3 )-CN (where n is an integer from 2 to 5) formula: CF 2 =CFO(CF 2 ) n -(C 6 H 4 )-CN (where n is an integer from 1 to 6) formula: CF 2 =CF(OCF 2 CF(CF 3 )) nOCF 2 CF (CF 3 ) - CN (where n is an integer from 1 to 2) Formula: CH 2 =CFCF 2 O(CF(CF 3 )CF 2 ) n CF(CF 3 ) - CN (where n is an integer from 0 to 5), Formula: CF 2 =CFO(CF 2 CF(CF 3 )O) m (CF 2 ) n - CN (where m is an integer from 0 to 5 and n is an integer from 1 to 3) Formula: CH 2 =CFCF 2 OCF(CF 3 )OCF(CF 3 ) - CN Formula: CH 2 =CFCF 2 OCH 2 CF 2 - CN Formula: CF 2 =CFO(CF 2 CF(CF 3 )O) m CF 2 CF(CF 3) - CN (where m is an integer of 0 or more) formula: CF 2 =CFOCF(CF 3 )CF 2 O(CF 2 ) n -CN (where n is an integer of 1 or more) formula: CF 2 =CFOCF 2 OCF 2 CF(CF 3 )OCF 2 -CN formula: CF 2 =CFO(CF 2 ) 3 CN formula: CF 2 =CFO(CF 2 ) 5 CN, and they can be used separately or in any combination. Among the above, preferably the formula: CF 2 =CF(OCF 2 CF(CF 3 )) m O(CF 2 ) n -CN (where m is an integer of 0 to 5 and n is an integer of 1 to 8) monomer represented, more preferably CF 2 =CFOCF 2 CF(CF 3 )OCF 2 CF 2 CN. Regarding the content of the nitrogen-containing crosslinking sites in the polymer mixture, when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, it is 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and even more preferably 1.5 mol% or less. The content of the nitrogen-containing crosslinking sites can be measured by infrared spectroscopy (IR). Regarding the content of the nitrogen-containing crosslinkable groups in the polymer mixture, when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and even more preferably 1.5 mol% or less. The content of the nitrogen-containing crosslinkable groups can be measured by infrared spectroscopy (IR). Regarding the content of the cyano groups in the polymer mixture, when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and even more preferably 1.5 mol% or less. The content of the cyano groups can be measured by infrared spectroscopy (IR). Regarding the content of the monomer units having nitrogen-containing crosslinkable groups in the polymer mixture, when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and even more preferably 1.5 mol% or less. The content of the monomer units having nitrogen-containing crosslinkable groups can be measured by infrared spectroscopy (IR). Regarding the content of the monomer units having cyano groups in the polymer mixture, when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 0.5 to 3.0 mol%, more preferably 2.0 mol% or less, and even more preferably 1.5 mol% or less. The content of the monomer units having cyano groups can be measured by infrared spectroscopy (IR). Regarding the content of the TFE units and the FAVE units in the polymer mixture, when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, it is preferably 97.0 to 99.5 mol%, more preferably 98.0 mol% or more, and even more preferably 98.5 mol% or more. (Method for manufacturing the polymer mixture) The polymer mixture of the present invention can be manufactured by a manufacturing method of mixing the fluororubber (a) and the crystalline fluoropolymer (b), a manufacturing method of producing the fluororubber (a) and the crystalline fluoropolymer (b) by two-stage polymerization, etc. The polymer mixture of the present invention is preferably produced by the following method: preparing an aqueous dispersion containing a fluororubber (a) and a crystalline fluoropolymer (b), and aggregating the fluororubber (a) and the crystalline fluoropolymer (b) in the aqueous dispersion. When using a polymer mixture obtained by a production method of mixing the solids of the fluororubber (a) and the solids of the crystalline fluoropolymer (b), an article having appropriate hardness, a small compression set at high temperature, and further, even after use under severe conditions, the compression set is not likely to increase can be obtained. However, it has now been found that a polymer mixture obtained by a production method of aggregating the fluororubber (a) and the crystalline fluoropolymer (b) in an aqueous dispersion has a smaller compression set at high temperature than a polymer mixture obtained by a production method of mixing the solids of the fluororubber (a) and the solids of the crystalline fluoropolymer (b), and further, an article in which an increase in the compression set after use under severe conditions is further suppressed can be obtained. The reason is not clear yet, but it is speculated that it is because the reaction of forming a co-crosslinked structure between the nitrogen-containing crosslinked sites of the fluororubber (a) and the nitrogen-containing crosslinked sites of the crystalline fluoropolymer (b) proceeds smoothly. As a method for preparing an aqueous dispersion containing a fluororubber (a) and a crystalline fluoropolymer (b), examples include: a method of mixing an aqueous dispersion containing a fluororubber (a) and an aqueous dispersion containing a crystalline fluoropolymer (b), a method of mixing a powder of the fluororubber (a) and an aqueous dispersion containing a crystalline fluoropolymer (b), a method of mixing an aqueous dispersion containing a fluororubber (a) and a powder of the crystalline fluoropolymer (b), etc. Among them, a method of mixing an aqueous dispersion containing a fluororubber (a) and an aqueous dispersion containing a crystalline fluoropolymer (b) is preferred. As a method for aggregating the fluororubber (a) and the crystalline fluoropolymer (b) in the aqueous dispersion, examples include: a method of mixing the aqueous dispersion and a flocculant or a method of freezing the aqueous dispersion. As the flocculant, known flocculants such as acids can be used. For example, aluminum salts, calcium salts, or magnesium salts can be cited. As organic flocculants, ammonium acetate, ammonium carbonate, etc. can be cited. As inorganic acid flocculants, hydrochloric acid, nitric acid, hydrofluoric acid, sulfuric acid, trifluoroacetic acid, etc. can be cited. The aggregate obtained by aggregation can also be washed with water, and after removing impurities such as a small amount of buffer solution or salt present in the aggregate, the washed aggregate can be dried using a hot air furnace or a vacuum dryer, etc., thereby preparing a polymer mixture. The form of the polymer mixture obtained after aggregation is not particularly limited and may be gum, crumb, powder, granules, etc., preferably gum or crumb. Gum is a granular lump composed of the polymer mixture, and crumb refers to a blocky form with no fixed shape formed by the fluororubber (a) in the polymer mixture adhering to each other because it cannot maintain a small granular shape in the form of gum at room temperature. In the method for producing the polymer mixture of the present invention, as a method for producing the fluororubber (a) and the crystalline fluoropolymer (b) by mixing, the following production method is preferred, that is: (1-1) In the presence of an aqueous medium, tetrafluoroethylene, fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing the fluororubber (a); (1-2) In the presence of an aqueous medium, tetrafluoroethylene and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing the crystalline fluoropolymer (b); (1-3) The aqueous dispersion containing the fluororubber (a) is mixed with the aqueous dispersion containing the crystalline fluoropolymer (b) to prepare an aqueous dispersion containing the fluororubber (a) and the crystalline fluoropolymer (b); (1-4) The fluororubber (a) and the crystalline fluoropolymer (b) in the aqueous dispersion are aggregated to obtain a polymer mixture. The preparation of the aqueous dispersion containing the fluororubber (a) and the aqueous dispersion containing the crystalline fluoropolymer (b) can be carried out by a known polymerization method. In the method for producing the polymer mixture of the present invention, as a method for producing the fluororubber (a) and the crystalline fluoropolymer (b) by two-stage polymerization, the following production method is preferred, that is: (2-1) In the presence of an aqueous medium, tetrafluoroethylene and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing the crystalline fluoropolymer (b), and then, (2-2) In the presence of the crystalline fluoropolymer (b) and the aqueous medium, tetrafluoroethylene, fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing the fluororubber (a) and the crystalline fluoropolymer (b); (2-3) The fluororubber (a) and the crystalline fluoropolymer (b) in the aqueous dispersion are aggregated. In the above production method, the polymerization in step (2-1) and the polymerization in step (2-2) can be carried out in the same reaction vessel or in different reaction vessels. Also, when carried out in the same reaction vessel, the polymerization in step (2-2) can be started after stopping the polymerization in step (2-1), or the polymerization in step (2-2) can be started without stopping the polymerization in step (2-1). In one embodiment of the above manufacturing method, (2-1) after preparing an aqueous dispersion containing a crystalline fluoropolymer (b) in a reaction vessel, (2-2) while continuously carrying out the polymerization reaction in the above reaction vessel, a fluoroalkyl vinyl ether is introduced into the above reaction vessel to polymerize tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group. By manufacturing a polymer mixture using such a continuous polymerization reaction, an article having an appropriate hardness and a smaller compression set at high temperatures can be obtained, and further, a polymer mixture for manufacturing an article in which an increase in compression set after use under severe conditions is more suppressed can be manufactured. The polymerization in step (2-1) and the polymerization in step (2-2) can be carried out using an appropriate emulsion polymerization method. In one embodiment, the polymerization is carried out in the presence of a polymerization initiator, a surfactant, and an aqueous medium. Examples of the polymerization initiator include: an oil-soluble radical polymerization initiator or a water-soluble radical initiator. Examples of the oil-soluble radical polymerization initiator may be known oil-soluble peroxides, such as dialkyl peroxydicarbonates such as diisopropyl peroxydicarbonate and di-sec-butyl peroxydicarbonate; peroxyesters such as tert-butyl peroxyisobutyrate and tert-butyl peroxypivalate; dialkyl peroxides such as di-tert-butyl peroxide, etc. Also, the following representative ones may be mentioned: bis(ω-hydro-perfluorohexanoyl) peroxide, bis(ω-hydro-dodecafluoroheptanoyl) peroxide, bis(ω-hydro-tetradecafluorooctanoyl) peroxide, bis(ω-hydro-hexadecafluorononanoyl) peroxide, bis(perfluorobutanoyl) peroxide, bis(perfluoropentanoyl) peroxide, bis(perfluorohexanoyl) peroxide, bis(perfluoroheptanoyl) peroxide, bis(perfluorooctanoyl) peroxide, bis(perfluorononanoyl) peroxide, bis(ω-chloro-hexafluorobutanoyl) peroxide, bis(ω-chloro-decafluorohexanoyl) peroxide, bis(ω-chloro-tetradecafluorooctanoyl) peroxide, ω-hydro-dodecafluoroheptanoyl-ω-hydro-hexadecafluorononanoyl-peroxide, ω-chloro-hexafluorobutanoyl-ω-chloro-decafluorohexanoyl-peroxide, ω-hydro-dodecafluoroheptanoyl-perfluorobutanoyl-peroxide, bis(dichloropentafluorobutanoyl) peroxide, bis(trichlorooctafluorohexanoyl) peroxide, bis(tetrachloroundecafluorooctanoyl) peroxide, bis(pentachlorotetradecafluorodecanoyl) peroxide, bis(undecachlorotritriacontadifluorodocosanoyl) peroxide, etc., bis[perfluoro(or fluorochloro)acyl] peroxides, etc. As a water-soluble free radical polymerization initiator, known water-soluble peroxides can be used, for example: ammonium salts, potassium salts, sodium salts of persulfuric acid, perboric acid, perchloric acid, perphosphoric acid, percarbonic acid, etc., t-butyl permaleate, t-butyl hydroperoxide, etc. A reducing agent such as a sulfite may also be included, and its usage amount can be 0.1 to 20 times that of the peroxide. The addition amount of the polymerization initiator is not particularly limited, as long as it is added once, successively, or continuously at the initial stage of polymerization in an amount such that the polymerization rate does not significantly decrease (for example, a concentration relative to water of several ppm) or more. The upper limit is within the range where the heat of the polymerization reaction can be removed from the device surface. As the surfactant, nonionic surfactants, anionic surfactants, cationic surfactants, etc. can be used, and fluorine-based surfactants used in, for example, International Publication No. 2000 / 029479, or the specification of U.S. Patent Application Publication No. 2007 / 0015865, or Japanese Patent Application Laid-Open No. 2014-540475 can also be used. The addition amount (relative to the solvent) is preferably 10 mass ppm to 20 mass%, more preferably 10 mass ppm to 10 mass%, still more preferably 10 mass ppm to 7 mass%, and particularly preferably 50 mass ppm to 5 mass%. Furthermore, a reactive emulsifier can be used as the surfactant. The reactive emulsifier is not particularly limited as long as it is a compound having one or more unsaturated bonds and a hydrophilic group each, for example: CH 2 =CFCF 2 OCF(CF 3 )CF 2 OCF(CF 3 )COONH 4 、CH 2 =CFCF 2 CF(CF 3 )OCF 2 CF 2 COONH 4 、CF 2 =CFOCF 2 CF(CF 3 )OCF (CF 3 )COONH 4 . The addition amount (relative to the solvent) is preferably 10 to 5000 mass ppm, more preferably 50 to 5000 mass ppm. Furthermore, a polymer of a compound having one or more unsaturated bonds and a hydrophilic group can also be used to replace the surfactant. Examples of such polymers include: CH 2 =CFCF 2 OCF (CF 3 )CF 2 OCF (CF 3 )COONH 4 、CH 2 =CFCF 2 CF (CF 3 )OCF 2 CF 2 COONH 4 、CF 2 =CFOCF 2 CF (CF 3 )OCF (CF 3 )COONH 4 and other homopolymers of compounds. The addition amount (relative to the solvent) is preferably 10 mass ppm to 10 mass%, more preferably 50 mass ppm to 5 mass%, and still more preferably 50 mass ppm to 2 mass%. As the aqueous medium, a medium without chain transferability is preferred. Examples of the aqueous medium include: water, a mixture of water and a water-soluble organic solvent, or a mixture of water and a water-insoluble organic solvent. Furthermore, the polymerization can be carried out in the presence of a chain transfer agent. As the chain transfer agent, in addition to the above nitrogen-containing chain transfer agent, an iodine compound or a bromine compound can also be used. As a polymerization method using an iodine compound or a bromine compound, for example, there can be mentioned: a method of carrying out emulsion polymerization in a water medium under pressure and simultaneously in the presence of an iodine compound or a bromine compound in a substantially oxygen-free state (iodine transfer polymerization method). As a representative example of the iodine compound or bromine compound used, for example, there can be mentioned a compound represented by the general formula: R 21 I x Br y (wherein x and y are each an integer from 0 to 2, and satisfy 1 ≦ x + y ≦ 2, and R 21 is a saturated or unsaturated fluorohydrocarbon group or chlorofluorohydrocarbon group having 1 to 16 carbon atoms, or a hydrocarbon group having 1 to 3 carbon atoms, and may also contain an oxygen atom). By using an iodine compound or a bromine compound, an iodine atom or a bromine atom is introduced into the polymer, thereby functioning as a crosslinking point. As the iodine compound and the bromine compound, for example, there can be mentioned: 1,3-diiodoperfluoropropane, 2-iodoperfluoropropane, 1,3-diiodo-2-chloroperfluoropropane, 1,4-diiodoperfluorobutane, 1,5-diiodo-2,4-dichloroperfluoropentane, 1,6-diiodoperfluorohexane, 1,8-diiodoperfluorooctane, 1,12-diiodoperfluorododecane, 1,16-diiodoperfluorohexadecane, diiodomethane, 1,2-diiodoethane, 1,3-diiodo-n-propane, CF 2 Br 2 , BrCF 2 CF 2 Br, CF 3 CFBrCF 2 Br, CFClBr 2 , BrCF 2 CFClBr, CFBrClCFClBr, BrCF 2 CF 2 CF 2 Br, BrCF 2 CFBrOCF 3 , 1-bromo-2-iodoperfluoroethane, 1-bromo-3-iodoperfluoropropane, 1-bromo-4-iodoperfluorobutane, 2-bromo-3-iodoperfluorobutane, 3-bromo-4-iodoperfluorobutene-1, 2-bromo-4-iodoperfluorobutene-1, monoiodo monobromo substituents of benzene, diiodo monobromo substituents, and (2-iodoethyl) and (2-bromoethyl) substituents, etc. These compounds can be used alone or in combination with each other. Among them, in terms of polymerization reactivity, crosslinking reactivity, ease of acquisition, etc., it is preferable to use 1,4-diiodoperfluorobutane, 1,6-diiodoperfluorohexane, and 2-iodoperfluoropropane. The polymerization temperature, polymerization pressure, and polymerization time vary depending on the type of solvent or polymerization initiator, and can be -15 to 150 °C, atmospheric pressure to 12 MPa, and 1 to 24 hours. As the polymerization initiator, when using an oil-soluble radical polymerization initiator, the polymerization temperature is preferably 30 to 95 °C. When using a water-soluble radical polymerization initiator as the polymerization initiator, the polymerization temperature is preferably 0 to 100 °C, more preferably 10 to 95 °C. (Crosslinkable composition) By mixing the above polymer mixture with at least one selected from the group consisting of inorganic nitrides, organotin compounds, ammonia-generating compounds, and crosslinking agents, a crosslinkable composition can be prepared. Crosslinking a crosslinkable composition containing the above polymer mixture and at least one selected from the group consisting of inorganic nitrides, organotin compounds, ammonia-generating compounds, and crosslinking agents can obtain an article (crosslinked product). As the inorganic nitride, there is no particular limitation, and examples thereof include: silicon nitride (Si 3 N 4 ), lithium nitride, titanium nitride, aluminum nitride, boron nitride, vanadium nitride, zirconium nitride, etc. Among them, in terms of supplying nanoparticles, silicon nitride is preferable. As the organotin compound, examples thereof include: tetraphenyltin, triphenyltin, etc. As the ammonia-generating compound, it is preferably a compound that generates ammonia at 40 to 330 °C. As the ammonia-generating compound, urea or its derivatives and ammonium salts are preferable, more preferably urea or ammonium salts, and even more preferably urea. As the ammonium salt, it can be an organic ammonium salt or an inorganic ammonium salt. Also, as the ammonia-generating compound, it can also be one that reacts with a small amount of water to generate ammonia. As the derivatives of urea, examples thereof include: biurea, thiourea, urea hydrochloride, biuret, etc. As the organic ammonium salt, examples thereof include: ammonium salts of non-fluorine carboxylic acids or sulfonic acids such as ammonium benzoate, ammonium adipate, and ammonium phthalate. Examples of the inorganic ammonium salts include compounds described in JP-A-9-111081, such as ammonium sulfate, ammonium carbonate, ammonium nitrate, and ammonium phosphate. Examples of the ammonia-generating compounds also include acetaldehyde ammonia, hexamethylenetetramine, formamidine, formamidine hydrochloride, formamidine acetate, tert-butyl carbamate, benzyl carbamate, phthalimide, and the like. Examples of the crosslinking agent include crosslinking agents used in peroxide crosslinking, polyol crosslinking, polyamine crosslinking, tri azole crosslinking, imidazole crosslinking, and thiazole crosslinking. The crosslinking agent used in peroxide crosslinking may be any organic peroxide that can easily generate peroxy radicals in the presence of a heat or redox system. Specifically, examples include: 1,1-bis(tert-butylperoxy)-3,5,5-trimethylcyclohexane, 2,5-dimethylhexane-2,5-dihydroperoxide, di-tert-butyl peroxide (PERBUTYL D), tert-butylcumyl peroxide (PERBUTYL C), dicumyl peroxide (Percumyl D, Percumyl D-40, Percumyl D-40MB(T)), α,α-bis(tert-butylperoxy)-p-diisopropylbenzene, 2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane (Perhexa 25B, Perhexa 25B-40), 2,5-dimethyl-2,5-bis(tert-butylperoxy)-3-hexyne (Perhexyne 25B, Perhexyne 25B-40), benzoyl peroxide, tert-butyl peroxybenzoate, 2,5-dimethyl-2,5-bis(benzoylperoxy)hexane (Perhexa 25Z), tert-butyl maleate peroxide (t-Butyl MA), tert-butyl isopropylcarbonate peroxide (PERBUTYL I-75), methyl ethyl ketone peroxide (Permek D(DR), Permek H(HR, HY), Permek N(NR, NY), Permek S(SR), Permek F(FR), Permek G(GR, GY)), cyclohexanone peroxide (Perhexa H), acetylacetone peroxide (Percure AH, AL), 1,1-bis(tert-hexylperoxy)-3,3,5-trimethylcyclohexane (Perhexa TMH), 1,1-bis(tert-hexylperoxy)cyclohexane (Perhexa HC), 1,1-bis(tert-butylperoxy)-2-methylcyclohexane (Perhexa MC), 1,1-bis(tert-butylperoxy)cyclohexane (Perhexa C-80(S), Perhexa C-75(EB), Perhexa C(C), Perhexa C-40, Perhexa C-40MB(S)), 2,2-bis(tert-butylperoxy)butane (Perhexa 22), 4,4-bis-(tert-butylperoxy)butyl valerate (Perhexa V, Perhexa V-40(F)), 2,2-bis(4,4-bis-(tert-butylperoxy)cyclohexyl)propane (PERTETRA A), p-menthane hydroperoxide (PERMENTA H), diisopropylbenzene hydroperoxide (Percumyl P), 1,1,3,3-Tetramethylbutyl hydroperoxide (PEROCTA H), cumene hydroperoxide (Percumyl H-80), tert-butyl hydroperoxide (PERBUTYL H-69), bis(2-tert-butylperoxyisopropyl)benzene (PERBUTYL P, PERBUTYL P-40, Peroxymon F-40, PERBUTYL P-40MB(K)), di-tert-hexyl peroxide (Perhexyl D), diisobutyryl peroxide (PEROYL IB), bis(3,5,5-trimethylhexanoyl) peroxide (PEROYL 355(S)), dilauroyl peroxide (PEROYL L), disuccinic peroxide (PEROYL SA), a polymeric mixture of di-(3-methylbenzoyl) peroxide, benzoyl(3-methylbenzoyl) peroxide, and dibenzoyl peroxide (Nyper BMT-K40, Nyper BMT-M), dibenzoyl peroxide (Nyper BW, Nyper BO, Nyper FF, Nyper BS, Nyper E, Nyper NS), bis(4-methylbenzoyl) peroxide (Nyper PMB), di-n-propyl peroxydicarbonate (PEROYL NPP-50M), diisopropyl peroxydicarbonate (PEROYL IPP-50, PEROYL IPP-27), di(4-tert-butylcyclohexyl) peroxydicarbonate (PEROYL TCP), di(2-ethylhexyl) peroxydicarbonate (PEROYL OPP), di-sec-butyl peroxydicarbonate (PEROYL SBP), cumyl neodecanoate (Percumyl ND, Percumyl ND-50E), 1,1,3,3-tetramethylbutyl neodecanoate (PEROCTA ND, PEROCTA ND-50E), tert-hexyl neodecanoate (PERHEXYL ND, PERHEXYL ND-50E), tert-butyl neodecanoate (PERBUTYL ND, PERBUTYL ND-50E), tert-butyl neodecanoate (PERBUTYL NHP), tert-hexyl pivalate (PERHEXYL PV, PERHEXYL PV-50E), tert-butyl pivalate (PERBUTYL PV, PERBUTYL PV-40E), 1,1,3,3-tetramethylbutyl 2-ethylhexanoate (PEROCTA O), 2,5-dimethyl-2,5-bis(2-ethylhexanoylperoxy)hexane (Perhexa 25O), tertiary hexyl 2-ethylhexanoate peroxide (PERHEXYL O, Percure HO(N)), tertiary butyl 2-ethylhexanoate peroxide (PERBUTYL O, Percure O), tertiary hexyl isopropyl monocarbonate peroxide (PERHEXYL I), tertiary butyl 3,5,5-trimethylhexanoate peroxide (PERBUTYL 355), tertiary butyl laurate peroxide (PERBUTYL L), tertiary butyl 2-ethylhexyl monocarbonate peroxide (PERBUTYL E), tertiary hexyl benzoate peroxide (PERHEXYL Z), tertiary butyl acetate peroxide (PERBUTYL A), polymer mixture of tertiary butyl 3-methylbenzoate peroxide and tertiary butyl benzoate peroxide (PERBUTYL ZT), tertiary butyl benzoate peroxide (PERBUTYL Z), tertiary butyl allyl monocarbonate peroxide (Peromer AC), 3,3',4,4'-tetra(tertiary butylperoxycarbonyl)benzophenone (BTTB-25), 2,3-dimethyl-2,3-diphenylbutane (Nofmer BC-90), etc. Among them, the dialkyl type is preferred. Further, 2,5-dimethyl-2,5-bis(tertiary butylperoxy)hexane is particularly preferred. Usually, the type and amount of the organic peroxide are selected in consideration of the amount of active -O-O- and the decomposition temperature, etc., Also, as the crosslinking aid that can be used in this case, any compound that is reactive with peroxy radicals and polymer radicals can be used. For example, those having -CH=CH 2 、-CH 2 CH=CH 2 、-CF=CF 2 、-C(CF 3 )=CF 2 、-C(CH 3 )=CF 2 、-CF=CF(CF 3 )、-CF=CF(CH 3 )、-C(C 6 H 5 )=CF 2 , -CF=CF(C 6 H 5 ), -CH=CF 2 , -CF=CHF, -C(CF 3 )=CHF, -CF=CH(CF 3 ), -CH=CF(CF 3 ) and other polyfunctional compounds having functional groups (in each formula, "C 6 H 5 " represents a phenyl group). Specifically, for example, triallyl cyanurate, triallyl isocyanurate (TAIC), triallyl formal, triallyl trimellitate, N,N'-p-phenylene bismaleimide, dipropargyl terephthalate, diallyl phthalate, tetraallyl terephthalamide, triallyl phosphate, bismaleimide, fluorinated triallyl isocyanurate (1,3,5-tris(2,3,3-trifluoro-2-propenyl)-1,3,5-tri 2,4,6-trione), tris(diallylamine)-S-tri , triallyl phosphite, N,N-diallylacrylamide, 1,6-divinyldodecafluorohexane, etc. Further, as a crosslinking aid used in combination with a peroxide crosslinking agent, examples include the general formula (31): (In the formula, six Rs 31 are each independently H, a halogen atom, or an optionally halogenated group having 1 to 5 carbon atoms that can insert an ether bond, and Z 31 is an optionally halogenated linear or branched alkylene group, cycloalkylene group, or (per)fluoropolyoxyalkylene group having 1 to 18 carbon atoms that optionally contains a hetero atom) represented by the compound. As the compound represented by the general formula (31), examples include the general formula (32): (In the formula, j is an integer from 2 to 10, preferably an integer from 4 to 8, and four Rs 32 are each independently H, F, or an alkyl group or (per)fluoroalkyl group having 1 to 5 carbon atoms) represented by the compound, the general formula (33): (In the formula, Y 31Independently of each other, they are F, Cl or H, Y 32 Independently of each other, they are F, Cl, H or OR 33 (Here, R 33 is a branched or straight-chain alkyl group that may be partially substantially or completely fluorinated or chlorinated), Z 33 is an optionally fluorinated divalent group having 2 to 10 carbon atoms that may insert an ether bond, preferably Z 33 is an integer of m being 3 to 5 of -(CF 2 ) m -group, the compound represented by the general formula (33) is preferably F 2 C=CF-O-(CF 2 ) 5 -O-CF=CF 2 )-represented compound, general formula (34): (In the formula, Y 31 , Y 32 and Z 33 are as described above, R 34 Independently of each other, they are H, F or an alkyl or (per)fluoroalkyl group having 1 to 5 carbon atoms) -represented compounds, etc. As a crosslinking aid used in combination with a crosslinking agent or a peroxide crosslinking agent, those having at least one general formula (35) can be exemplified: (In the formula, R 35 ~R 37 Independently of each other, they are a hydrogen atom, a fluorine atom, an alkyl group, a fluorinated alkyl group, or a substituted or unsubstituted aryl group, R 35 ~R 37 At least one of them is a fluorine atom or a group containing a fluorine atom. m is an integer of 1 to 5. When m is 2 or more, m R 35 ~R 37They may be the same or different. The hydrogen atoms of the benzene ring may be substituted) a compound having the structure represented. In the case where m is 1, it is preferably to have two or more of such structures. As a compound having the structure represented by the general formula (36), examples include: General formula (36): (In the formula, R 35 ~R 37 As described above. p is an integer from 0 to 2, and n is an integer from 2 to 6) a compound represented, General formula (37): (In the formula, R 35 ~R 37 As described above. R 38 is a single bond, -SO 2 -, -O-, -S-, -CO-, a heteroatom-containing group, a substituted or unsubstituted alkylene group, a substituted or unsubstituted cycloalkylene group, or a substituted or unsubstituted arylene group. m is an integer from 1 to 5. These groups may be partially or fully fluorinated) a compound represented, etc. As a heteroatom-containing group, there is no particular limitation as long as it is a divalent group containing a heteroatom. As heteroatoms, examples include: an oxygen atom, a nitrogen atom, a sulfur atom, a boron atom, a phosphorus atom. As a crosslinking agent for polyol crosslinking, examples include polyol compounds such as bisphenol A and bisphenol AF. As a crosslinking agent for polyamine crosslinking, examples include: polyamine compounds such as hexamethylene diisocyanate carbamate, N,N'-diphenylallylidene-1,6-hexanediamine, 4,4'-bis(aminocyclohexyl)methane carbamate. As used for azole crosslinking, imidazole crosslinking, thiazole crosslinking crosslinking agent, for example, examples include: General formula (41): (In the formula, R 41 is -SO 2 -, -O-, -CO-, an alkylene group having 1 to 6 carbon atoms, a perfluoroalkylene group having 1 to 10 carbon atoms or a single bond, or the group represented, R 42 and R 43 one of which is -NH 2 , the other is -NHR 44 、-NH 2 , -OH or -SH, R 44 is a hydrogen atom, a fluorine atom or a monovalent organic group, preferably R 42 is -NH 2 and R 43 is -NHR 44 . As preferred specific examples of the alkylene group having 1 to 6 carbon atoms, examples include: methylene, ethylene, propylene, butylene, pentylene, hexylene, etc. As the perfluoroalkylene group having 1 to 10 carbon atoms, examples include: etc. Furthermore, these compounds are known as examples of bis(diaminophenyl) compounds in Japanese Patent Publication No. 2-59177, Japanese Unexamined Patent Publication No. 8-120146, etc.) bis(diaminophenyl)-type crosslinking agents, bis(aminophenol)-type crosslinking agents, bis(aminobenzenethiol)-type crosslinking agents represented by; General formula (42): (R 41 As described above, R 45 are each independently any one of the following groups) bisamidrazone-type crosslinking agents represented by; General formula (43): (In the formula, Rf 41 is a perfluoroalkylene group having 1 to 10 carbon atoms) amidrazone-type crosslinking agents represented by; or General formula (44): (In the formula, n is an integer from 1 to 10) bisamidoxime-type crosslinking agents represented by; and General formula (45): HN=CR 45 R 46 (In the formula, R 45 is selected from the group consisting of H, NH 2 , and NHR 47 The group consisting of, R 46 is selected from the group consisting of Ph, SO 2 H, NR 48 R 49 , 2-pyridine, and CH 2CONH 2 the group consisting of, R 47 is selected from the group consisting of Ph, NH 2 , and CN, R 48 is selected from the group consisting of H, NHPh, CH 2 CONH 2 , a linear alkyl group having 1 to 8 carbon atoms, and a branched alkyl group having 1 to 8 carbon atoms, and R 49 is selected from the group consisting of Ph, COOC(CH 3 ) 3 , NH 2 , CH 2 COOH, CSNH 2 , CNHNH 3 + Cl - , p-phenyl CN, and compounds represented by the group consisting of COPh). Furthermore, as a crosslinking agent, the general formula (46): X 41 -(CH 2 ) n -R 50 -(CH 2 ) m -X 41 (wherein X 41 are each independently an alkynyl group, a nitrile group or Y 41 P N 3 (Y 41 is SO, SO 2 , C 6 H 4 or CO, p is 0 or 1), n and m are independently integers from 1 to 4, R 50 selected from the group consisting of: i) a fluoroalkylene group having 3 to 10 carbon atoms, ii) a fluoroalkoxy group having 3 to 10 carbon atoms, iii) a substituted arylene group, iv) an oligomer containing copolymerized units of vinylidene fluoride and perfluoro(methyl vinyl ether), v) an oligomer containing copolymerized units of vinylidene fluoride and hexafluoropropylene, vi) an oligomer containing copolymerized units of tetrafluoroethylene and perfluoro(methyl vinyl ether), and vii) an oligomer containing copolymerized units of tetrafluoroethylene and olefin), the crosslinking agent represented by As a particularly preferred crosslinking agent, examples include: a compound having plural 3-amino-4-hydroxyphenyl groups, or 3-amino-4-mercaptophenyl groups, or the general formula (47): (wherein R 41 , R 42 and R 43 as described above), specifically, for example: 2,2-bis(3-amino-4-hydroxyphenyl)hexafluoropropane (common name: bis(aminophenol) AF), 2,2-bis(3-amino-4-mercaptophenyl)hexafluoropropane, tetraaminobenzene, bis-3,4-diaminophenylmethane, bis-3,4-diaminophenyl ether, 2,2-bis(3,4-diaminophenyl)hexafluoropropane, 2,2-bis[3-amino-4-(N-phenylamino)phenyl]hexafluoropropane, 2,2-bis[3-amino-4-(N-methylamino)phenyl]hexafluoropropane, 2,2-bis[3-amino-4-(N-ethylamino)phenyl]hexafluoropropane, 2,2-bis[3-amino-4-(N-propylamino)phenyl]hexafluoropropane, 2,2-bis[3-amino-4-(N-perfluorophenylamino)phenyl]hexafluoropropane, 2,2-bis[3-amino-4-(N-benzylamino)phenyl]hexafluoropropane, etc. Among them, as the crosslinking agent, in terms of heat resistance, steam resistance, amine resistance, and good crosslinking property, 2,2-bis[3-amino-4-(N-phenylamino)phenyl]hexafluoropropane is preferred. Regarding the content of at least one selected from the group consisting of inorganic nitrides, organotin compounds, ammonia-generating compounds, and crosslinking agents, relative to 100 parts by mass of the polymer mixture, it is preferably 0.05 part by mass or more, more preferably 0.1 part by mass or more, still more preferably 0.2 part by mass or more, particularly preferably 0.3 part by mass or more, and preferably 10 parts by mass or less, more preferably 5.0 parts by mass or less, still more preferably 2.0 parts by mass or less, particularly preferably 1.0 part by mass or less. (Other components) The crosslinkable composition may also contain other components other than the crosslinking agent. As other components, for example, fillers can be cited. As fillers, examples include: imide-based fillers having an imide structure such as polyimide, polyamideimide, and polyetherimide; organic fillers made of engineering plastics such as polyarylate, polysulfone, polyethersulfone, polyphenylene sulfide, polyetheretherketone, polyetherketone, and polyoxybenzoate; metal oxide fillers such as silicon oxide, aluminum oxide, and yttrium oxide; metal carbides such as silicon carbide and aluminum carbide; metal nitride fillers such as silicon nitride and aluminum nitride; and inorganic fillers such as carbon black, aluminum fluoride, and carbon fluoride. Among them, in terms of the shielding effect against various plasmas, carbon black, aluminum oxide, silicon oxide, yttrium oxide, silicon carbide, silicon nitride, polyimide, and carbon fluoride are preferred. Also, the above-mentioned inorganic fillers and organic fillers can be blended alone or two or more of them can be combined and blended. Especially in fields where high purity and non-pollution are not required, common additives such as processing aids, plasticizers, and colorants can be blended into the composition as needed, and one or more common crosslinking agents or crosslinking aids different from the above can also be blended. The crosslinkable composition may also contain an organic basic compound. As the organic basic compound, examples include: the formula: CH 3 (CH 2 ) 17 -NH 2 of octadecylamine; the formula: H 2 N-C(O)-(CH 2 ) 11 -CH=CH-(CH 2 ) 7 CH 3Erucamide; formula: H 2 N-C(O)-(CH 2 ) 7 -CH=CH-(CH 2 ) 7 CH 3 Oleamide; formula: H 2 N-(CH 2 ) 6 -NH 2 Hexamethylenediamine; formula: 1,8 - Diazabicycloundec - 7 - ene (DBU), etc. The above cross - linkable composition can be prepared by mixing a polymer mixture and other components such as a cross - linker. The mixing can be carried out using ordinary polymer processing machines, such as open rolls, Banbury mixers, kneaders, closed mixers, etc. The above cross - linkable composition can preferably be used as a molding material for obtaining an article by cross - link molding. (Article) The article of the present invention can be obtained by cross - linking the above cross - linkable composition. The article of the present invention has appropriate hardness, a small compression set at high temperature, and furthermore, even after use under severe conditions, the compression set is not likely to increase significantly. Also, according to the present invention, an article can be provided, the compression set of which measured after being placed at 300 °C for 70 hours is 50% or less, the compression set of which measured after being placed at 200 °C for 70 hours and then at 70 °C for 70 hours is less than 50%, and the hardness measured according to ASTM D2240 is 65 or more. The article of the present invention has appropriate hardness, a small compression set at high temperature, and furthermore, even after use under severe conditions, the compression set is not likely to increase significantly. The article of the present invention having the characteristics of compression set and hardness preferably contains a polymer. As the polymer, the above polymer mixture is preferred. Hereinafter, both the article obtained by cross - linking the above cross - linkable composition and the article having the characteristics of compression set and hardness will be described. The hardness (Shore A, peak value) of the article is preferably 65 or more, more preferably 67 or more. The upper limit of the hardness is not particularly limited and may be 90 or less, or may be 80 or less. The hardness of the article can be measured according to JIS K6253. As described above, the article of the present invention has appropriate hardness. Therefore, for example, when the article of the present invention is used as a sealing material, even when tightly sealed, the article is not easily damaged, and even when used at high temperatures, cracks are not easily generated. If the hardness of the article is too low, it becomes difficult to tightly seal, or cracks are likely to occur when used at high temperatures. If the hardness is too high, it becomes difficult to compress the article, and thus there is a risk of becoming difficult to obtain excellent sealing performance. The compression set (300 °C) of the article measured after being placed at 300 °C for 70 hours is preferably 50% or less, more preferably 45% or less, still more preferably 40% or less, and even more preferably 35% or less. The compression set (300 °C) can be calculated by the following method: After the article is compressed at a compression rate of 25% and placed at 300 °C for 70 hours, the compression is released, and after being placed at 23 °C for 30 minutes, the thickness of the article before and after compression is measured, and then the compression set is calculated. As described above, even when the article of the present invention is used at a high temperature exceeding 300 °C, the compression set is small. The compression set (200 °C) of the article measured after being placed at 200 °C for 70 hours and then at 70 °C for 70 hours is preferably less than 50%, more preferably 45% or less, and still more preferably 40% or less. The compression set (200 °C) can be calculated by the following method: After the article is compressed at a compression rate of 25% and placed at 200 °C for 70 hours, and then at 70 °C for 70 hours, the compression is released, and after being placed at 20 °C for 30 minutes, the thickness of the article after compression is measured, and then the compression set is calculated. Thus, even after the article of the present invention is used under severe conditions, the compression set is not likely to increase. For example, when the article of the present invention is used as a sealing material for a semiconductor manufacturing apparatus, during the operation of the semiconductor manufacturing apparatus, there is a situation where the sealing material is used at a temperature of 200 °C or higher in a compressed state. After that, if the operation of the semiconductor manufacturing apparatus is stopped, the sealing material remains in a compressed state, slowly cools to room temperature, and is then placed at room temperature. Therefore, the sealing material is required to have the characteristics to withstand use under such severe conditions. The article of the present invention is excellent in both high-temperature sealing performance and low-temperature sealing performance and can withstand use under such severe conditions. As a method for obtaining an article from a self-crosslinkable composition, the following methods can be cited: after obtaining a preform by shaping the crosslinkable composition as a molding material, crosslink the preform. The method for obtaining the preform from the composition can be a common method and can be carried out by the following known methods, namely: a method of hot compression using a mold, a method of pressing into a heated mold, a method of extrusion using an extruder, etc. In the case of extruded products such as hoses or electric wires, an article can be obtained by heat-crosslinking using steam or the like after extrusion. The above crosslinking is called primary crosslinking and can be carried out in the order of primary crosslinking and secondary crosslinking. The primary crosslinking is preferably carried out at 150 to 250 °C for 5 to 120 minutes, more preferably at 170 to 200 °C for 5 to 60 minutes. As the crosslinking means, any known crosslinking means can be used, and for example, pressure crosslinking etc. can be cited. The secondary crosslinking is preferably carried out at 250 to 320 °C for 2 to 48 hours, more preferably at 280 to 310 °C for 5 to 24 hours. Also, the secondary crosslinking can also be carried out at 180 to 320 °C for 2 to 24 hours, and can also be carried out at 190 to 310 °C for 5 to 20 hours. The temperature change can also be maintained within this temperature range. As the crosslinking means, any known crosslinking means can be used, and for example, oven crosslinking etc. can be cited. Regarding crosslinking, for example, it can be carried out in an air environment or a nitrogen environment. The article of the present invention can be suitably used as a sealing material for a semiconductor manufacturing apparatus that particularly requires heat resistance, especially a sealing material for a semiconductor manufacturing apparatus that performs high-density plasma irradiation. As the above sealing material, the following can be cited: O-rings, angular rings, gaskets, liners, oil seals, bearing seals, end seals, etc. In addition, it can also be used as various polymer products used in semiconductor manufacturing apparatuses, such as diaphragms, tubes, hoses, various rubber rollers, belts, etc. Also, it can be used as a coating material and a lining material. Furthermore, the semiconductor manufacturing apparatus in the present invention is not particularly limited to an apparatus for manufacturing semiconductors, and broadly includes apparatuses for manufacturing liquid crystal panels or plasma panels, etc., and the entire manufacturing apparatus used in the semiconductor field that requires a high degree of cleanliness. For example, the following can be cited. (1) Etching apparatus Dry etching apparatus Plasma etching apparatus Reactive ion etching apparatus Reactive ion beam etching apparatus Sputtering etching apparatus Ion beam etching apparatus Wet etching apparatus Ashing apparatus (2) Cleaning apparatus Dry etching cleaning apparatus UV / O 3Cleaning device, ion beam cleaning device, laser beam cleaning device, plasma cleaning device, gas etching cleaning device, extraction cleaning device, Soxhlet extraction cleaning device, high-temperature and high-pressure extraction cleaning device, microwave extraction cleaning device, supercritical extraction cleaning device, (3) Exposure device, stepper, coater, developer, (4) Polishing device, CMP device, (5) Film forming device, CVD device, sputtering device, (6) Diffusion, ion implantation device, oxidation diffusion device, ion implantation device The article of the present invention exhibits excellent performance as a sealing material for, for example, a CVD device, a plasma etching device, a reactive ion etching device, an ashing device, or an excimer laser exposure machine. As described above, the embodiments have been described, but it should be understood that various changes in form or details can be made without departing from the gist and scope of the patent application. <1> According to the first aspect of the present invention, a polymer mixture can be provided, which contains a fluororubber (a) and a crystalline fluoropolymer (b). The fluororubber (a) contains tetrafluoroethylene units, fluoroalkyl vinyl ether units, and a nitrogen-containing crosslinking site. The crystalline fluoropolymer (b) contains tetrafluoroethylene units and a nitrogen-containing crosslinking site. The melting point of the above polymer mixture is 310 to 320 °C. The content of the crystalline fluoropolymer (b) in the above polymer mixture is 4.0 to 15.0% by mass based on the total mass of the fluororubber (a) and the crystalline fluoropolymer (b). <2> According to the second aspect of the present invention, a polymer mixture as in the first aspect can be provided, wherein the Mooney viscosity of the above polymer mixture at 170 °C is 70 to 120. <3> According to the third aspect of the present invention, a polymer mixture as in the first or second aspect can be provided, wherein when the total monomer units constituting the fluororubber (a) and the crystalline fluoropolymer (b) are set to 100 mol%, the content of the nitrogen-containing crosslinking site in the above polymer mixture is 0.5 to 3.0 mol%. <4> According to the fourth aspect of the present invention, a polymer mixture as in any one of the first to third aspects can be provided, wherein the content ratio of the tetrafluoroethylene units to the fluoroalkyl vinyl ether units in the above polymer mixture, in terms of molar ratio (tetrafluoroethylene units / fluoroalkyl vinyl ether units), is 50 / 50 to 70 / 30. <5> According to the fifth aspect of the present invention, a polymer mixture as in any one of the first to fourth aspects can be provided, wherein the above fluoroalkyl vinyl ether unit in the fluororubber (a) is a perfluoro(methyl vinyl ether) unit. <6> According to the sixth aspect of the present invention, a polymer mixture as in any one of the first to fifth aspects can be provided, wherein the fluororubber (a) and the crystalline fluoropolymer (b) contain monomer units having a nitrogen-containing crosslinkable group. <7> According to the seventh aspect of the present invention, a polymer mixture as in any one of the first to sixth aspects can be obtained by the following production method, which is to prepare an aqueous dispersion containing the fluororubber (a) and the crystalline fluoropolymer (b), and coagulate the fluororubber (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion.<8> According to the 8th aspect of the present invention, a polymer mixture according to any one of the 1st to 7th aspects can be provided, which is obtained by the following production method. The production method is as follows: (1-1) In the presence of an aqueous medium, tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing a fluororubber (a). (1-2) In the presence of an aqueous medium, tetrafluoroethylene and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing a crystalline fluoropolymer (b). (1-3) The aqueous dispersion containing the fluororubber (a) is mixed with the aqueous dispersion containing the crystalline fluoropolymer (b) to prepare an aqueous dispersion containing the fluororubber (a) and the crystalline fluoropolymer (b). (1-4) The fluororubber (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion are aggregated to obtain the above polymer mixture. <9> According to the 9th aspect of the present invention, a polymer mixture according to any one of the 1st to 8th aspects can be provided, wherein when the total monomer units constituting the fluororubber (a) are set to 100 mol%, the content of the nitrogen-containing crosslinking site in the fluororubber (a) is 0.5 to 3.0 mol%. <10> According to the 10th aspect of the present invention, a polymer mixture according to any one of the 1st to 9th aspects can be provided, wherein when the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, the content of the nitrogen-containing crosslinking site in the crystalline fluoropolymer (b) is 0.5 to 3.0 mol%. <11> According to the 11th aspect of the present invention, a polymer mixture according to any one of the 1st to 7th aspects can be provided, which is obtained by the following production method. The production method is as follows: (2-1) In the presence of an aqueous medium, tetrafluoroethylene and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing a crystalline fluoropolymer (b). Then, (2-2) In the presence of the crystalline fluoropolymer (b) and an aqueous medium, tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group are polymerized to prepare an aqueous dispersion containing a fluororubber (a) and a crystalline fluoropolymer (b). (2-3) The fluororubber (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion are aggregated. <12> According to the 12th aspect of the present invention, a crosslinkable composition can be provided, which contains the polymer mixture according to any one of the 1st to 11th aspects and at least one selected from the group consisting of inorganic nitrides, organotin compounds, ammonia-generating compounds, and crosslinking agents. <13> According to the 13th aspect of the present invention, an article obtained by crosslinking the crosslinkable composition can be provided. The above crosslinkable composition is the crosslinkable composition according to the 12th aspect.<14>According to the 14th aspect of the present invention, an article as in the 13th aspect can be provided, wherein the compression set measured after being placed at 300°C for 70 hours is 50% or less, the compression set measured after being placed at 200°C for 70 hours and then at 70°C for 70 hours is less than 50%, and the hardness measured according to ASTM D2240 is 65 or more. <15>According to the 15th aspect of the present invention, a method for producing a polymer mixture according to any one of the 1st to 10th aspects is provided, which includes the following steps: (1-1) Polymerize tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group in the presence of an aqueous medium to prepare an aqueous dispersion containing a fluororubber (a). (1-2) Polymerize tetrafluoroethylene and a monomer having a nitrogen-containing crosslinkable group in the presence of an aqueous medium to prepare an aqueous dispersion containing a crystalline fluoropolymer (b). (1-3) Mix the aqueous dispersion containing the fluororubber (a) with the aqueous dispersion containing the crystalline fluoropolymer (b) to prepare an aqueous dispersion containing the fluororubber (a) and the crystalline fluoropolymer (b). (1-4) Coagulate the fluororubber (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion to obtain the above polymer mixture. <16>According to the 16th aspect of the present invention, a method for producing a polymer mixture according to any one of the 1st to 7th and 11th aspects is provided, which includes the following steps: (2-1) Polymerize tetrafluoroethylene and a monomer having a nitrogen-containing crosslinkable group in the presence of an aqueous medium to prepare an aqueous dispersion containing a crystalline fluoropolymer (b), and then, (2-2) Polymerize tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group in the presence of the crystalline fluoropolymer (b) and the aqueous medium to prepare an aqueous dispersion containing a fluororubber (a) and a crystalline fluoropolymer (b). (2-3) Coagulate the fluororubber (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion to obtain the above polymer mixture. <17>According to the 17th aspect of the present invention, a production method as in the 16th aspect is provided, wherein, (2-1) After preparing an aqueous dispersion containing a crystalline fluoropolymer (b) in a reaction vessel, (2-2) While continuously carrying out the polymerization reaction in the above reaction vessel, a fluoroalkyl vinyl ether is introduced into the above reaction vessel to polymerize tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinkable group. <18>According to the 18th aspect of the present invention, an article having the following characteristics is provided, wherein the compression set measured after being placed at 300°C for 70 hours is 50% or less, the compression set measured after being placed at 200°C for 70 hours and then at 70°C for 70 hours is less than 50%, and the hardness measured according to ASTM D2240 is 65 or more. [Examples]. Next, examples will be given to describe the embodiments of the present invention, but the present invention is not limited to the related examples. The respective numerical values of the examples were measured by the following methods. (Mooney viscosity) The Mooney viscosity (ML(1+20)) of the polymer mixture and the fluororubber was measured at 170 °C in accordance with JIS K6300 using a Mooney viscometer type MV2000E manufactured by ALPHA TECHNOLOGIES. (Monomer composition) The monomer composition of the polymer mixture, the fluororubber, and the crystalline fluoropolymer was determined by 19 F-NMR analysis. Among them, the content of the cyano group-containing monomer unit was determined by the following method (IR). (Content of cyano group and cyano group-containing monomer unit) The content of the cyano group and the cyano group-containing monomer unit in the polymer mixture, the fluororubber, and the crystalline fluoropolymer was measured by infrared spectroscopy (IR). (Glass transition temperature) The glass transition temperature of the polymer mixture can be determined as follows: Using a differential scanning calorimeter (manufactured by Hitachi High-Tech Science, X-DSC7000), heating a 3 mg sample at 20 °C / min to obtain a DSC curve, and taking the temperature representing "the midpoint of the two intersection points of the extension line of the baseline before and after the secondary transition of the DSC curve and the tangent line at the inflection point of the DSC curve" as the glass transition temperature. (Content of crystalline fluoropolymer (b)) Regarding the content of the crystalline fluoropolymer (b) in the polymer mixture, it can be measured as follows: Accurately weigh about 10 mg of the polymer mixture that has no heating history to a temperature above 300 °C, and place it in a dedicated aluminum pan, and measure it using TG / DTA (differential thermal thermogravimetric simultaneous measurement device). In an atmospheric environment, heat the aluminum pan in the temperature range of 25 °C to 600 °C at a rate of 10 °C / min to obtain a TG curve, and calculate the weight loss rate based on the obtained TG curve to make a determination. The content of the crystalline fluoropolymer (b) in the polymer mixture relative to the total mass of the fluororubber (a) and the crystalline fluoropolymer (b) is shown in Table 1. (Melting Point) Regarding the melting point of the polymer mixture, it can be measured in the following manner: accurately weigh approximately 10 mg of the polymer mixture that has not been heated to a temperature above 300 °C and has no heating history, and place it in a special aluminum pan. Use TG / DTA (Differential Thermal and Thermogravimetric Simultaneous Measurement Device) for measurement. Under an atmospheric environment, heat the aluminum pan from 25 °C to 600 °C at a rate of 10 °C per minute to obtain a DTA curve, and define the temperature corresponding to the peak in the obtained DTA curve as the melting point of the polymer mixture. Regarding whether the fluororubber has a melting point, the measurement method for the melting point of the polymer mixture is also used for confirmation. In Table 1, "N.D" indicates that no distinct peak can be confirmed in the DTA curve. (Hardness (Shore A) Peak) Using an article with a thickness of 2 mm, measure the hardness (Shore A) (peak) according to JIS-K6253. (Compression Set (300 °C)) The compression set is measured according to the method described in ASTM D395 or JIS K6262. Using a compression device, at room temperature, compress the O-rings produced in the examples and comparative examples to a compression ratio of 25% (compress an O-ring with a thickness (wire diameter) of 3.5 mm to a thickness of 2.625 mm). Then, place the compression device with the compressed O-ring fixed in an electric furnace and leave it at 300 °C for 70 hours, and then remove the compression device from the electric furnace. Remove the O-ring from the compression device, place the removed O-ring in a constant temperature chamber at 23 °C for 30 minutes, and measure the thickness of the O-ring (t 2 ). Calculate the compression set using the following formula. Furthermore, the closer the compression set is to 0%, the more excellent the compression set characteristics of the article. Compression Set (%) = (t 0 - t 2 ) / (t 0 - t 1 ) × 100 t 0 : The original thickness (mm) of the O-ring t 1 : The thickness (mm) of the spacer t 2 : The thickness (mm) of the O-ring after the compression test In the above test, t 0 = 3.5 mm, t 1 = 2.625 mm. (Compression set (200°C → 70°C)) The compression set was measured according to the method described in ASTM D395 or JIS K6262. Using a compression device, at room temperature, the O-rings produced in the examples and comparative examples were compressed to a compression ratio of 25% (the O-ring with a thickness (wire diameter) of 3.5 mm was compressed to a thickness of 2.625 mm). Subsequently, the compression device with the compressed O-ring fixed was left stationary in an electric furnace and placed at 200°C for 70 hours, and then the compression device was removed from the electric furnace. Then, the compression device with the compressed O-ring fixed was left stationary in another electric furnace and placed at 70°C for 70 hours. The O-ring was removed from the compression device, and the removed O-ring was placed in a thermostatic chamber at 23°C for 30 minutes, and the thickness of the O-ring (t 2 ) was measured. The compression set was calculated by the following formula. Compression set (%) = (t 0 −t 2 ) / (t 0 −t 1 ) × 100 t 0 : The original thickness of the O-ring (mm) t 1 : The thickness of the spacer (mm) t 2 : The thickness of the O-ring after the compression test (mm) In the above test, t 0 = 3.5 mm, t 1 = 2.625 mm. Example 1 After adding 43 g of ammonium perfluorocaproate and 0.08 g of ammonium carbonate to a 2 L SUS autoclave, 790 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5°C, and 0.33 g of CF 2 =CFOCF 2 CF(CF 3 )OCF 2 CF 2After CN (CNVE), TFE was added to make the pressure reach 0.29 MPa, and the pressure and the temperature in the tank were maintained. 3.0 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.27 g of CNVE was continuously added until 25.0 g of TFE was added additionally. Finally, after the addition of TFE was completed, the pressure in the tank was reduced to 0.19 MPa, and then 40.4 g of PMVE was added. After the addition of PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 56.0 / 44.0 mol% was introduced into the reaction vessel in such a way that the pressure became 0.85 MPa. Then, the additional gas of TFE / PMVE = 56.0 / 44.0 mol% of 185.0 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 4.7 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuum at 70 °C for 24 hours to obtain 218 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 317.7 °C, and the content of the crystalline fluoropolymer (b) was 10.6 wt% according to the weight reduction rate. Also, according to DSC measurement, the glass transition temperature was -4.6 °C. Also, according to NMR analysis, TFE / PMVE = 55.2 / 44.8 mol%, and according to IR analysis, CNVE was 0.57 mol%. Also, the Mooney viscosity was 72. Example 2 After adding 43 g of ammonium perfluorohexanoate and 0.08 g of ammonium carbonate into a 2-L SUS autoclave, 790 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.16 g of CNVE, TFE was added to make the pressure 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 1.6 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.38 g of CNVE was continuously added until 20.0 g of TFE was added additionally. After finally adding TFE, the pressure inside the tank was reduced to 0.19 MPa, and then 40.4 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 54.0 / 46.0 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 54.0 / 46.0 mol% of 185.0 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 4.7 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 213 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 316.5 °C, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 9.4 wt%. Also, from DSC measurement, the glass transition temperature was -5.0 °C. Also, from NMR analysis, TFE / PMVE = 53.5 / 46.5 mol%, and from IR analysis, CNVE was 0.56 mol%. Also, the Mooney viscosity was 86. Example 3: After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate into a 6-L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.65 g of CNVE, TFE was added to make the pressure reach 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 8.5 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.65 g of CNVE was continuously added until 34.0 g of TFE was additionally added. Finally, after adding TFE was completed, the pressure inside the tank was reduced to 0.19 MPa, and then 145 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 14.3 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 718 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 313.7 °C, and from the weight reduction rate, the content of the crystalline fluoropolymer (b) was found to be 5.5 wt%. Also, according to DSC measurement, the glass transition temperature was -5.3 °C. Also, according to NMR analysis, TFE / PMVE = 58.6 / 41.4 mol%, and according to IR analysis, CNVE was 0.55 mol%. Also, the Mooney viscosity was 90. Example 4: After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate into a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.54 g of CNVE, TFE was added until the pressure reached 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 5.4 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.65 g of CNVE was continuously added until 34.0 g of TFE was added additionally. After finally adding TFE, the pressure inside the tank was reduced to 0.19 MPa, and then 145 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 58.0 / 42.0 mol% of 660 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 14.3 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 700 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 314.3 °C, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 5.0 wt%. Also, according to DSC measurement, the glass transition temperature was -5.3 °C. Also, according to NMR analysis, TFE / PMVE = 58.9 / 41.1 mol%, and according to IR analysis, CNVE was 0.57 mol%. Also, the Mooney viscosity was 115. Example 5 After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate into a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.54 g of CNVE, TFE was added until the pressure reached 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 9.2 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.97 g of CNVE was continuously added until 51.0 g of TFE was additionally added. Finally, after adding TFE was completed, the pressure inside the tank was reduced to 0.19 MPa, and then 145 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 58.0 / 42.0 mol% of 660 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 14.3 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 730 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 314.4 °C, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 7.6 wt%. Also, from DSC measurement, the glass transition temperature was -5.5 °C. Also, from NMR analysis, TFE / PMVE = 58.1 / 41.9 mol%, and from IR analysis, CNVE was found to be 0.53 mol%. Also, the Mooney viscosity was 87. Example 6: After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate into a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.54 g of CNVE, TFE was added to make the pressure 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 7.2 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.97 g of CNVE was continuously added until 51.0 g of TFE was added additionally. After finally adding TFE and completing the addition, the pressure inside the tank was reduced to 0.19 MPa, and then 124 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 62.5 / 37.5 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of 720 g of TFE / PMVE = 62.5 / 37.5 mol% was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 14.3 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 700 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 312.9 °C, and from the weight reduction rate, the content of the crystalline fluoropolymer (b) was found to be 5.9 wt%. Also, according to DSC measurement, the glass transition temperature was -4.1 °C. Also, according to NMR analysis, TFE / PMVE = 63.5 / 36.5 mol%, and according to IR analysis, CNVE was 0.55 mol%. Also, the Mooney viscosity was 111. Example 7: After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate into a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 67.5 °C, and after adding 0.54 g of CNVE, TFE was added to make the pressure 0.36 MPa, and the pressure and the temperature in the tank were maintained. 1.1 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.36 MPa, and a total of 0.45 g of CNVE was continuously added until 42.0 g of TFE was added additionally. After finally adding TFE and completing, the pressure in the tank was reduced to 0.26 MPa, and then 115 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 64.5 / 35.5 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 64.5 / 35.5 mol% of 724 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 17.4 g of CNVE was continuously added. Also, when the polymerization rate started to decrease, an aqueous solution of 2 mass% of APS was appropriately added. The total amount of the aqueous solution of 2 mass% of APS added after the start of polymerization was 20 mL. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 730 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 317.5 °C, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 5.2 wt%. Also, according to DSC measurement, the glass transition temperature was -2.6 °C. Also, according to NMR analysis, TFE / PMVE = 66.2 / 33.8 mol%, and according to IR analysis, CNVE was 0.61 mol%. Also, the Mooney viscosity was 111. Example 8 After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate into a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 67.5 °C, and after adding 0.54 g of CNVE, TFE was added to make the pressure 0.36 MPa, and the pressure and the temperature inside the tank were maintained. 1.1 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.36 MPa, and a total of 0.97 g of CNVE was continuously added until 51.0 g of TFE was additionally added. After finally adding TFE and completing, the pressure inside the tank was reduced to 0.26 MPa, and then 115 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 64.5 / 35.5 mol% was introduced into the reaction vessel in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 64.5 / 35.5 mol% of 724 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 17.4 g of CNVE was continuously added. Also, when the polymerization rate started to decrease, an aqueous solution of 2 mass% of APS was appropriately added. The total amount of the aqueous solution of 2 mass% of APS added after the start of polymerization was 20 mL. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 742 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 316.2 °C, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 7.2 wt%. Also, from DSC measurement, the glass transition temperature was -2.8 °C. Also, from NMR analysis, TFE / PMVE = 66.6 / 33.4 mol%, and from IR analysis, CNVE was found to be 0.59 mol%. Also, the Mooney viscosity was 108. Comparative Example 1 After adding 43 g of ammonium perfluorohexanoate and 0.08 g of ammonium carbonate into a 2-L SUS autoclave, 790 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, 0.16 g of CNVE was added, then TFE was added to make the pressure 0.29 MPa, and the pressure and the temperature inside the vessel were maintained. 1.6 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.19 g of CNVE was continuously added until 10.0 g of TFE was added additionally. After the final addition of TFE was completed, the pressure inside the vessel was reduced to 0.19 MPa, and then 40.4 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 54.0 / 46.0 mol% was introduced into the reaction vessel in such a way that the pressure became 0.85 MPa. Then, the additional gas of TFE / PMVE = 54.0 / 46.0 mol% was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 5.0 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out of the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 213 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, no observation was possible. From the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 3.6 wt%. Also, from DSC measurement, the glass transition temperature was -5.4 °C. Also, from NMR analysis, TFE / PMVE = 54.4 / 45.6 mol%, and from IR analysis, CNVE was found to be 0.56 mol%. Also, the Mooney viscosity was 96. Comparative Example 2 After adding 155 g of ammonium perfluorohexanoate and 0.28 g of ammonium carbonate into a 6 L SUS autoclave, 2880 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 2.24 g of CNVE, a mixed gas of TFE / PMVE = 24.0 / 76.0 mol% was added to make the pressure 0.85 MPa, and the pressure and the temperature inside the tank were maintained. 15.0 g of ammonium persulfate (APS) was added as a polymerization initiator. 810 g of an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was continuously introduced while keeping the reaction pressure constant at 0.85 MPa. At the same time, a total of 25.6 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 828 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, no melting point was observed, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 0 wt%. Also, from DSC measurement, the glass transition temperature was -5.2 °C. Also, from NMR analysis, TFE / PMVE = 58.0 / 42.0 mol%, and from IR analysis, CNVE was found to be 1.20 mol%. Also, the Mooney viscosity was 80. Comparative Example 3 After adding 43 g of ammonium perfluorohexanoate and 0.08 g of ammonium carbonate to an SUS autoclave with an internal volume of 2 L, 790 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.64 g of CNVE, TFE was added to a pressure of 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 2.2 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.49 g of CNVE was continuously added until 17.0 g of TFE was additionally added. After finally adding TFE, the pressure inside the tank was reduced to 0.19 MPa, and then 40.4 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was introduced into the reaction vessel and introduced in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 58.0 / 42.0 mol% of 198.0 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 4.7 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out of the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 217 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 304.0 °C, and from the weight reduction rate, the content of the crystalline fluoropolymer (b) was found to be 8.0 wt%. Also, from DSC measurement, the glass transition temperature was -5.0 °C. Also, from NMR analysis, TFE / PMVE = 58.0 / 42.0 mol%, and from IR analysis, CNVE was found to be 0.58 mol%. Also, the Mooney viscosity was 92. Comparative Example 4 After adding 43 g of ammonium perfluorohexanoate and 0.08 g of ammonium carbonate into a 2 L SUS autoclave, 790 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.16 g of CNVE, TFE was added to make the pressure 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 1.8 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.08 g of CNVE was continuously added until 22.0 g of TFE was added additionally. After finally adding TFE, the pressure inside the tank was reduced to 0.19 MPa, and then 40.4 g of PMVE was added. After adding PMVE, the pressure was reduced to 0.735 MPa, and then an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was introduced into the reaction vessel in such a way that the pressure became 0.85 MPa. Then, an additional gas of TFE / PMVE = 58.0 / 42.0 mol% of 188.0 g was continuously introduced in such a way that the pressure was kept constant at 0.85 MPa. At the same time, a total of 4.8 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. The obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours to obtain 213 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 328.0 °C, and from the weight loss rate, the content of the crystalline fluoropolymer (b) was found to be 10.0 wt%. Also, from DSC measurement, the glass transition temperature was -5.0 °C. Also, from NMR analysis, TFE / PMVE = 58.0 / 42.0 mol%, and from IR analysis, CNVE was found to be 0.58 mol%. Also, the Mooney viscosity was 86. Synthesis Example of Fluoroelastomer (a) 155 g of ammonium perfluorohexanoate and 0.28 g of ammonium carbonate were added to a 6 L SUS autoclave, and then 2880 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, 1.21 g of CNVE was added, and then a mixed gas of TFE / PMVE = 24.0 / 76.0 mol% was added to make the pressure reach 0.85 MPa, and the pressure and the temperature inside the tank were maintained. 15.0 g of ammonium persulfate (APS) was added as a polymerization initiator. 810 g of an additional gas of TFE / PMVE = 58.0 / 42.0 mol% was continuously introduced while keeping the reaction pressure constant at 0.85 MPa. At the same time, a total of 19.8 g of CNVE was continuously added. When all the additional gas and CNVE were added, stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. A part of the obtained aqueous dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours. As a result of performing TG / DTA measurement on the obtained fluoroelastomer (a), no melting point was observed, and according to the weight loss rate, the content of the crystalline fluoropolymer (b) was 0 wt%. Also, according to NMR analysis, TFE / PMVE = 58.0 / 42.0 mol%, and according to IR analysis, CNVE was 0.60 mol%. Also, the Mooney viscosity was 74. Synthesis Example of Crystalline Fluoropolymer (b1) 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate were added to a 6 L SUS autoclave, and then 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, 0.54 g of CNVE was added, and then TFE was added to make the pressure reach 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 5.4 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added while keeping the reaction pressure constant at 0.29 MPa, and a total of 0.65 g of CNVE was continuously added until 34.0 g of TFE was added additionally. After adding TFE finally, the pressure inside the tank was reduced to 0.19 MPa, then stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out from the reaction vessel and cooled. A part of the obtained dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours. As a result of IR analysis of the obtained crystalline fluoropolymer (b1), CNVE was 0.90 mol%. Synthesis Example of Crystalline Fluoropolymer (b2) After adding 145 g of ammonium perfluorohexanoate and 0.26 g of ammonium carbonate to a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.1 g of CNVE, TFE was added until the pressure reached 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 5.4 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 0.04 g of CNVE was continuously added until 34.0 g of TFE was added additionally. After finally adding TFE, the pressure inside the tank was reduced to 0.19 MPa, then stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out of the reaction vessel and cooled. A part of the obtained dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours. From IR analysis of the obtained crystalline fluoropolymer (b2), it was found that CNVE was 0.10 mol%. Synthesis Example of Crystalline Fluoropolymer (b3) After adding 145 g of ammonium perfluorohexanoate and 2.16 g of ammonium carbonate to a 6 L SUS autoclave, 2660 g of deionized and degassed water was added. The reaction vessel was sealed, and the inside of the system was purged with nitrogen to remove oxygen. The reaction vessel was heated to 54.5 °C, and after adding 0.54 g of CNVE, TFE was added until the pressure reached 0.29 MPa, and the pressure and the temperature inside the tank were maintained. 5.4 g of ammonium persulfate (APS) was added as a polymerization initiator. TFE was added in such a way that the reaction pressure was kept constant at 0.29 MPa, and a total of 1.71 g of CNVE was continuously added until 34.0 g of TFE was added additionally. After finally adding TFE, the pressure inside the tank was reduced to 0.19 MPa, then stirring was stopped, the reaction vessel was depressurized to atmospheric pressure, and the aqueous dispersion was taken out of the reaction vessel and cooled. A part of the obtained dispersion was coagulated with nitric acid water, washed with water, and dried in vacuo at 70 °C for 24 hours. From IR analysis of the obtained crystalline fluoropolymer (b3), it was found that CNVE was 3.20 mol%. Example 9: 995 g of an aqueous dispersion of fluororubber (a) and 846 g of an aqueous dispersion of fluoropolymer (b1) were previously introduced into a container equipped with a stirrer to prepare a mixed aqueous dispersion. The prepared mixed aqueous dispersion was coagulated with nitric acid water, washed with water, and dried under vacuum at 70°C for 24 hours to obtain 220 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 318°C, and from the weight reduction rate, the content of crystalline fluoropolymer (b) was found to be 4.7 wt%. Also, according to DSC measurement, the glass transition temperature was -5.0°C. Also, the Mooney viscosity was 86. Example 10: 942 g of an aqueous dispersion of fluororubber (a) and 1692 g of an aqueous dispersion of fluoropolymer (b1) were previously introduced into a container equipped with a stirrer to prepare a mixed aqueous dispersion. The prepared mixed aqueous dispersion was coagulated with nitric acid water, washed with water, and dried under vacuum at 70°C for 24 hours to obtain 220 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 318°C, and from the weight reduction rate, the content of crystalline fluoropolymer (b) was found to be 11.2 wt%. Also, according to DSC measurement, the glass transition temperature was -5.0°C. Also, the Mooney viscosity was 92. Comparative Example 5: 890 g of an aqueous dispersion of fluororubber (a) and 2538 g of an aqueous dispersion of fluoropolymer (b1) were previously introduced into a container equipped with a stirrer to prepare a mixed aqueous dispersion. The prepared mixed aqueous dispersion was coagulated with nitric acid water, washed with water, and dried under vacuum at 70°C for 24 hours to obtain 220 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 318°C, and from the weight reduction rate, the content of crystalline fluoropolymer (b) was found to be 15.7 wt%. Also, according to DSC measurement, the glass transition temperature was -4.8°C. Also, the Mooney viscosity was 92. Comparative Example 6: 953 g of an aqueous dispersion of fluororubber (a) and 1523 g of an aqueous dispersion of fluoropolymer (b2) were previously introduced into a container equipped with a stirrer to prepare a mixed aqueous dispersion. The prepared mixed aqueous dispersion was coagulated with nitric acid water, washed with water, and dried under vacuum at 70°C for 24 hours to obtain 220 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 328°C, and from the weight reduction rate, the content of crystalline fluoropolymer (b) was found to be 10.2 wt%. Also, according to DSC measurement, the glass transition temperature was -4.8°C. Also, the Mooney viscosity was 82. Comparative Example 7: 963 g of an aqueous dispersion of a fluororubber (a) and 1353 g of an aqueous dispersion of a fluoropolymer (b2) were previously introduced into a container equipped with a stirrer to prepare a mixed aqueous dispersion. The prepared mixed aqueous dispersion was coagulated with nitric acid water, washed with water, and dried under vacuum at 70 °C for 24 hours to obtain 220 g of a polymer mixture. As a result of performing TG / DTA measurement on the obtained polymer mixture, the melting point was shown to be 299 °C, and from the weight reduction rate, the content of the crystalline fluoropolymer (b) was found to be 8.2 wt%. Also, according to DSC measurement, the glass transition temperature was -4.9 °C. Further, the Mooney viscosity was 87. With respect to 100 parts by mass of the fluororubber (a) in the polymer mixture prepared in the Examples and Comparative Examples, 0.9 part by mass of the crosslinking agent 2,2-bis[3-amino-4-(N-phenylamino)phenyl]hexafluoropropane was introduced, and kneading was carried out using an open roll, followed by crosslinking by pressing at 180 °C for 30 minutes, and further oven crosslinking in an air oven at 290 °C for 18 hours to prepare a sheet with a thickness of 2 mm and an O-ring of size P24. The hardness of the obtained sheet was measured, and the compression set of the obtained O-ring was measured. The results are shown in Tables 1 to 3. [Table 1] [Table 2-1] Table 2-1 Composition of Fluororubber (a) [Table 2-2] Table 2-2 Composition of Crystalline Fluoropolymer (b) [Table 3] None None
Claims
1. A polymer mixture comprising a fluoroelastomer (a) and a crystalline fluoropolymer (b), wherein the fluoroelastomer (a) comprises tetrafluoroethylene units, fluoroalkyl vinyl ether units, and nitrogen-containing crosslinking sites, and the crystalline fluoropolymer (b) comprises tetrafluoroethylene units and nitrogen-containing crosslinking sites; the polymer mixture has a melting point of 310–320°C, and the content of the crystalline fluoropolymer (b) in the polymer mixture is 4.0–15.0% by mass relative to the total mass of the fluoroelastomer (a) and the crystalline fluoropolymer (b).
2. The polymer mixture as claimed in claim 1, wherein, The Menner viscosity of the above polymer mixture at 170°C is 70–120.
3. The polymer mixture as claimed in claim 1 or 2, wherein, When the total monomer units constituting the fluoroelastomer (a) and the crystalline fluoropolymer (b) are set to 100 mol%, the content of the nitrogen-containing crosslinked portion in the above polymer mixture is 0.5 to 3.0 mol.
4. A polymer mixture as claimed in claim 1 or 2, wherein, The ratio of tetrafluoroethylene units to fluoroalkyl vinyl ether units in the above polymer mixture, expressed in molar ratio (tetrafluoroethylene units / fluoroalkyl vinyl ether units), is 50 / 50 to 70 / 30.
5. A polymer mixture as claimed in claim 1 or 2, wherein, The fluoroalkyl vinyl ether unit in the fluoroelastomer (a) is a perfluoro (methyl vinyl ether) unit.
6. A polymer mixture as claimed in claim 1 or 2, wherein, Fluoroelastics (a) and crystalline fluoropolymers (b) contain monomer units with nitrogen-containing crosslinking groups.
7. The polymer mixture of claim 1 or 2 is obtained by the following manufacturing method: preparing an aqueous dispersion containing a fluoroelastomer (a) and a crystalline fluoropolymer (b), and causing the fluoroelastomer (a) and the crystalline fluoropolymer (b) in the aqueous dispersion to aggregate.
8. The polymer mixture of claim 1 or 2 is obtained by the following manufacturing method: (1-1) polymerizing tetrafluoroethylene, fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinking group in the presence of an aqueous medium to prepare an aqueous dispersion containing a fluoroelastomer (a); (1-2) polymerizing tetrafluoroethylene and a monomer having a nitrogen-containing crosslinking group in the presence of an aqueous medium to prepare an aqueous dispersion containing a crystalline fluoropolymer (b); (1-3) mixing the aqueous dispersion containing the fluoroelastomer (a) with the aqueous dispersion containing the crystalline fluoropolymer (b) to prepare an aqueous dispersion containing both the fluoroelastomer (a) and the crystalline fluoropolymer (b); (1-4) agglomerating the fluoroelastomer (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion to obtain the above polymer mixture.
9. A polymer mixture as claimed in claim 1 or 2, wherein, When the total monomer units constituting the fluoroelastomer (a) are set to 100 mol%, the content of nitrogen-containing crosslinked parts in the fluoroelastomer (a) is 0.5 to 3.0 mol.
10. A polymer mixture as claimed in claim 1 or 2, wherein, When the total monomer units constituting the crystalline fluoropolymer (b) are set to 100 mol%, the content of nitrogen-containing crosslinked sites in the crystalline fluoropolymer (b) is 0.5 to 3.0 mol.
11. The polymer mixture of claim 1 or 2 is obtained by the following manufacturing method: (2-1) polymerizing tetrafluoroethylene and a monomer having a nitrogen-containing crosslinking group in the presence of an aqueous medium to prepare an aqueous dispersion containing a crystalline fluoropolymer (b); then, (2-2) polymerizing tetrafluoroethylene, fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinking group in the presence of the crystalline fluoropolymer (b) and an aqueous medium to prepare an aqueous dispersion containing a fluoroelastomer (a) and a crystalline fluoropolymer (b); and (2-3) causing the fluoroelastomer (a) and the crystalline fluoropolymer (b) in the above aqueous dispersion to aggregate.
12. A crosslinkable composition comprising a polymer mixture of any one of claims 1 to 11, and at least one selected from the group consisting of inorganic nitrides, organotin compounds, ammonia-generating compounds, and crosslinking agents.
13. An article obtained by crosslinking a crosslinking composition, wherein the crosslinking composition is the crosslinking composition of claim 12.
14. The article of claim 13, whose compression set is less than 50% after being placed at 300°C for 70 hours, whose compression set is less than 50% after being placed at 200°C for 70 hours and then at 70°C for 70 hours, and whose hardness is greater than 65 according to ASTM D2240.
15. A method for manufacturing a polymer mixture according to any one of claims 1 to 10, comprising the following steps: (1-1) polymerizing tetrafluoroethylene, fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinking group in the presence of an aqueous medium to prepare an aqueous dispersion containing a fluoroelastomer (a); (1-2) polymerizing tetrafluoroethylene and a monomer having a nitrogen-containing crosslinking group in the presence of an aqueous medium to prepare an aqueous dispersion containing a crystalline fluoropolymer (b); (1-3) mixing the aqueous dispersion containing the fluoroelastomer (a) with the aqueous dispersion containing the crystalline fluoropolymer (b) to prepare an aqueous dispersion containing both the fluoroelastomer (a) and the crystalline fluoropolymer (b); and (1-4) agglomerating the fluoroelastomer (a) and the crystalline fluoropolymer (b) in the aqueous dispersion to obtain the polymer mixture.
16. A method for manufacturing a polymer mixture according to any one of claims 1 to 7 and 11, comprising the following steps: (2-1) polymerizing tetrafluoroethylene and a monomer having a nitrogen-containing crosslinking group in the presence of an aqueous medium to prepare an aqueous dispersion containing a crystalline fluoropolymer (b); then, (2-2) polymerizing tetrafluoroethylene, a fluoroalkyl vinyl ether, and a monomer having a nitrogen-containing crosslinking group in the presence of the crystalline fluoropolymer (b) and an aqueous medium to prepare an aqueous dispersion containing a fluoroelastomer (a) and a crystalline fluoropolymer (b); and (2-3) causing the fluoroelastomer (a) and the crystalline fluoropolymer (b) in the aqueous dispersion to agglomerate to obtain the polymer mixture.
17. The manufacturing method as described in claim 16, wherein, (2-1) After preparing an aqueous dispersion containing crystalline fluoropolymer (b) in a reaction vessel, (2-2) while continuing the polymerization reaction in the reaction vessel, fluoroalkyl vinyl ether is added to the reaction vessel to polymerize tetrafluoroethylene, fluoroalkyl vinyl ether, and monomers with nitrogen-containing crosslinking groups.
Citation Information
Patent Citations
High purity perfluoroelastomer composites and a processes to produce the same
US20060270780A1