AI Technical Summary
Next-generation power semiconductor devices require aluminum bonding wires or ribbons with improved high-speed temperature cycling reliability to withstand rapid temperature changes and extended cycle counts, as conventional methods fail to maintain strength under stringent high-speed temperature cycle tests, especially with silicon carbide semiconductors.
Aluminum bonding wires or ribbons containing 3.0 to 20.0 mass% silicon, with specific crystal orientation ratios and silicon phase distributions, enhance thermal strain management and crack suppression, ensuring reliability even in high-speed temperature cycling tests.
The proposed aluminum bonding wires or ribbons exhibit excellent high-speed temperature cycling reliability, extending the life of semiconductor devices to 20,000 cycles by mitigating thermal stress and crack growth, suitable for next-generation silicon carbide power semiconductors.
Smart Images

Figure TWG2TB001920360_001 
Figure TWG2TB001920360_002 
Figure TWG2TB001920360_003
Abstract
Description
Aluminum bonding wire or aluminum bonding tape The present invention relates to an aluminum bonding wire or an aluminum bonding ribbon and further relates to a semiconductor device obtained by using the aluminum bonding wire or the aluminum bonding ribbon. In semiconductor devices, electrodes formed on a semiconductor wafer are connected to electrodes on a lead frame or substrate via bonding wires (wires) or bonding tapes (ribbons). In power semiconductor devices, bonding wires or bonding tapes made primarily of aluminum (Al) are used. The diameter of aluminum bonding wires typically ranges from 100 μm to 600 μm, while the width of aluminum bonding tapes typically ranges from 100 μm to 3000 μm, and the thickness typically ranges from 50 μm to 600 μm. Herein, aluminum bonding wires and aluminum bonding tapes are collectively referred to as aluminum connecting materials. In power semiconductor devices, silicon (Si) is often used as the material for semiconductor wafers, and aluminum-silicon alloys or aluminum-copper alloys are often used as the materials for electrodes formed on the semiconductor wafers. Furthermore, power semiconductor devices using aluminum bonding wire or aluminum bonding ribbon are often used in high-power equipment such as air conditioners and solar power generation systems, as well as in automotive semiconductor devices. The bonding methods for aluminum bonding wire or ribbon include a first bonding method with an electrode on a semiconductor wafer and a second bonding method with an electrode on a lead frame or substrate, both of which utilize wedge bonding. Wedge bonding refers to a method in which ultrasonic vibrations and loads are applied to the aluminum bonding wire or ribbon using a metal jig (tool), breaking the surface oxide film between the wire or ribbon and the electrode material, exposing a new surface and performing solid-phase diffusion bonding. This bonding method is characterized by the solid-phase bonding without melting the bonding material, distinguishing it from welding techniques that melt the bonding material. The next generation of power semiconductor devices is required to operate stably for a longer period of time than general power semiconductor devices. Power semiconductor devices operate by repeatedly connecting and disconnecting current. If current is supplied to a silicon semiconductor chip through an aluminum bonding wire or an aluminum bonding ribbon, the temperature of the first bonding portion rises. On the other hand, if the current supply is stopped, the temperature of the first bonding portion drops. In this way, the first bonding portion repeatedly heats up and cools down when the power semiconductor is in operation. In this way, the first bonding portion repeatedly bears the thermal stress generated by the thermal expansion difference between the aluminum bonding wire or the aluminum bonding ribbon and the semiconductor chip. When a connecting material containing only high-purity aluminum is used, the aluminum bonding wire or the aluminum bonding ribbon will break in a relatively short period of time due to the thermal stress, making it difficult to meet the performance required by the next generation of power semiconductor devices. Therefore, the next generation of power semiconductors is required to improve the life of the bonding portion (hereinafter also referred to as "temperature cycle reliability") as the first bonding portion heats up and cools down. To meet the requirements for temperature cycling reliability, aluminum bonding wires have been proposed that focus on improving mechanical strength. As a method to improve the mechanical properties of aluminum bonding wires, a method has been proposed to add specific elements to aluminum. Patent Document 1 discloses a bonding wire comprising an aluminum alloy containing at least magnesium (Mg) and silicon (Si), wherein the total content of magnesium and silicon is 0.03 mass % or more and 0.3 mass % or less. According to this patent document, the high strength effect obtained by solid solution strengthening of magnesium or silicon or the high strength effect obtained by precipitation of magnesium silicide (Mg 2Si) The crack progression inhibition effect obtained was that the bonding strength of the first bonding portion decreased with delay in the cold temperature cycle test in the temperature range of 70°C to 120°C. Patent Document 2 discloses a bonding wire characterized by a microstructure comprising an alloy containing 0.01-0.2 mass% iron (Fe), 1-20 massppm silicon (Si), and the remainder being aluminum with a purity of 99.997 mass% or greater. The solid solution content of iron is 0.01-0.06%, the amount of iron precipitated is no more than seven times the solid solution content of iron, and the average grain size is 6-12 μm. This patent document discloses that uniformly dispersing intermetallic compound particles of iron and aluminum in the aluminum enhances the mechanical strength of the matrix and further refines the recrystallized grains, thereby suppressing a decrease in the bond strength of the first bond during thermal shock testing in the temperature range of -50°C to 200°C. Patent Document 3 discloses a bonding wire formed by melting an aluminum-silicon alloy containing 0.1 to 5% silicon (Si) by mass, with the remainder consisting of aluminum and impurities, ejecting the melt, rapidly cooling it, and forming it into a thin wire. This patent document discloses that by rapidly cooling the molten aluminum-silicon alloy and finely and evenly dispersing the silicon, mechanical strength is improved. [Prior Art Document] [Patent Document] [Patent Document 1] Japanese Patent Application Publication No. 2014-131010 [Patent Document 2] Japanese Patent Application Publication No. 2014-129578 [Patent Document 3] Japanese Patent Application Publication No. 59-57440 [Problem to be solved by the invention] As described above, the next generation of power semiconductor devices is required to withstand longer use time than general power semiconductor devices. When the power semiconductor device is in operation, the temperature of the first bonding portion repeatedly rises and falls. As a result, since the linear expansion coefficient of the aluminum bonding wire or aluminum bonding tape is greater than that of the semiconductor chip, there is a possibility that thermal stress is generated in the first bonding portion due to the difference in linear expansion coefficient between the two, and eventually the aluminum bonding wire or aluminum bonding tape is fatigue-damaged. One of the tests for accelerating the evaluation of the life (temperature cycle reliability) of the bonding portion accompanied by such a rise and fall in temperature of the first bonding portion is a temperature cycle test. The aluminum bonding wire or aluminum bonding tape used for the next generation of power semiconductors needs to show excellent temperature cycle reliability in the temperature cycle test. However, when using aluminum bonding wires that have been strengthened by the addition of silicon, etc., as disclosed in Patent Documents 1 to 3, the present inventors have confirmed that, in temperature cycling tests assumed to be used in next-generation power semiconductor devices, cracks develop at a relatively rapid rate within aluminum alloy electrodes, which have lower strength than the aluminum bonding wires, making it difficult to stably obtain good temperature cycling reliability. On the other hand, the previous temperature cycle test (hereinafter also referred to as "TCT (Temperature Cycle Test)") can be easily tested using commercially available test equipment. However, since the temperature change rate in TCT is relatively slow, there is a concern that a deviation from the faster temperature change rate will occur during the operation of the power semiconductor device. Therefore, in order to approach the conditions of actual use, a high-speed temperature cycle test (hereinafter also referred to as "high-speed TCT") with a higher temperature change rate has recently been studied. Regarding the temperature change rate, compared to the previous TCT, which is about 10°C / minute, in the high-speed TCT, the temperature changes rapidly, for example, at about 200°C / minute. Regarding the reliability evaluation of the joints of aluminum bonding wires or aluminum bonding strips, the inventors of the present invention have confirmed the following: Even if the reliability of the aluminum bonding wires or aluminum bonding strips is not reduced when evaluated in the previous TCT, if they are evaluated in the high-speed TCT, there is a situation where the bonding strength is reduced and the bonding life is shortened. Therefore, there is a demand for aluminum bonding wires or ribbons that demonstrate good joint reliability even in high-speed TCT, a more stringent test close to actual use conditions, and offer excellent temperature cycling reliability. Hereinafter, temperature cycling reliability in high-speed TCT will sometimes be referred to as "high-speed temperature cycling reliability." Furthermore, for the next generation of power semiconductor elements that will replace the previously mainstream silicon (Si), it is predicted that silicon carbide (SiC), which has higher heat resistance, will be further used. In the connection of silicon carbide power semiconductors, high-speed temperature cycle tests are required to be more stringent than at present. For example, the number of cycles of the high-speed temperature cycle test for silicon semiconductors is about 10,000 times, and the number of cycles for silicon carbide semiconductors is required to be extended to about 20,000 times. In addition, regarding the upper limit temperature, the condition of about 150°C, which is also strict for silicon semiconductors, is required. However, if it is for silicon carbide semiconductors, it is required to exhibit excellent high-speed temperature cycle reliability under more stringent conditions, such as conditions exceeding 175°C. The inventors have discovered that even aluminum bonding wires or ribbons that exhibit excellent high-speed temperature cycling reliability at approximately 10,000 cycles experience a decrease in strength at the bonding site of the aluminum bonding wire or ribbon when the number of cycles in high-speed temperature cycling tests on silicon carbide semiconductors is increased to 20,000, leading to a decrease in high-speed temperature cycling reliability. This is believed to be due to the fact that increasing the number of temperature cycles changes the morphology, location, and growth behavior of cracks that develop at the bonding site of the aluminum bonding wire or ribbon. Therefore, increasing the number of cycles from 10,000 to 20,000 increases the rate of cracks that develop within the aluminum bonding wire or ribbon, which is believed to accelerate a decrease in reliability. The present invention was completed in response to the above-mentioned problems, and its purpose is to provide an aluminum bonding wire or aluminum bonding ribbon that exhibits excellent high-speed temperature cycling reliability even in high-speed temperature cycling tests with a large number of cycles, as required by next-generation silicon carbide power semiconductors. [Technical Means for Solving the Problem] The present inventors conducted intensive research on the above-mentioned problems and discovered that the following aluminum bonding wire or aluminum bonding ribbon can solve the above-mentioned problems: the aluminum bonding wire or aluminum bonding ribbon contains 3.0 mass% to 20.0 mass% of silicon, and the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction in the L cross-section (a cross-section in the central axis direction including the central axis) of the aluminum bonding wire or aluminum bonding ribbon, and the ratio of the number of silicon phases with an equivalent circle diameter of 0.5 μm to 0.8 μm in the L cross-section are within specific ranges. Based on this understanding, further repeated research led to the completion of the present invention. That is, the present invention includes the following: <1> An aluminum bonding wire or aluminum bonding ribbon containing 3.0 mass% to 20.0 mass% silicon; wherein, when measuring the crystal orientation of the aluminum phase in an L-section (a cross section in the central axis direction including the central axis) of the aluminum bonding wire or aluminum bonding ribbon, the ratio of the <100> crystal orientation having an angular difference of 15° or less with respect to a direction parallel to the central axis (RD direction) is 15% to 50%; and, where the number of silicon phases having an equivalent circle diameter of 0.5 μm to 0.8 μm in the L-section is Ns and the number of silicon phases having an equivalent circle diameter of 0.5 μm or greater in the L-section is Nc, the ratio of Ns to Nc [Ns / Nc × 100 (%)] is 30% to 95%. <2> The aluminum bonding wire or ribbon according to <1>, wherein the ratio of Ns to Nc [Ns / Nc × 100 (%)] is 40% or more. <3> The aluminum bonding wire or ribbon according to <1> or <2>, wherein, when the crystal orientation of the silicon phase in the L-section is measured, the total ratio of the <100> crystal orientation and the <111> crystal orientation with an angle difference of 15° or less relative to the direction perpendicular to the central axis (ND direction) is 20% or more and 60% or less. <4> The aluminum bonding wire or ribbon according to any one of <1> to <3>, wherein the average value of the ratio of the short side length e to the long side length f of the silicon phase in the L-section (e / f) is 0.20 or more and 0.70 or less. <5> The aluminum bonding wire or ribbon according to any one of <1> to <4>, further comprising a total of 10 mass ppm to 800 mass ppm of one or more of strontium, sodium, iron, and phosphorus. <6> The aluminum bonding wire or ribbon according to any one of <1> to <5>, further comprising a total of 100 mass ppm to 2000 mass ppm of one or more of titanium, nickel, magnesium, and copper. <7> The aluminum bonding wire or ribbon according to any one of <1> to <6>, wherein the total concentration of elements other than aluminum, silicon, strontium, sodium, iron, phosphorus, titanium, nickel, magnesium, and copper in the aluminum bonding wire or ribbon is 0.5 mass % or less. <8> The aluminum bonding wire or ribbon according to any one of <1> to <7>, wherein the orientation ratio of the crystal orientation, the equivalent circle diameter of the silicon phase, and the number of the silicon phases are values measured using a SEM-EDS-EBSD apparatus. <9> The aluminum bonding wire or aluminum bonding ribbon according to any one of <4> to <8>, wherein the average value of the ratio of the short side length e to the long side length f of the silicon phase (e / f) is a value measured using a SEM-EDS-EBSD device. <10> The aluminum bonding wire or aluminum bonding ribbon according to any one of <1> to <9>, which is used in a semiconductor device. <11> A semiconductor device comprising the aluminum bonding wire or aluminum bonding ribbon according to any one of <1> to <10>. [Effects of the Invention] According to the present invention, an aluminum bonding wire or aluminum bonding ribbon that exhibits excellent high-speed temperature cycling reliability even in a high-speed temperature cycling test with a large number of cycles, which is required for next-generation silicon carbide power semiconductors, and a semiconductor device obtained using the aluminum bonding wire or aluminum bonding ribbon can be provided. The following describes preferred embodiments of the present invention in detail. While drawings are sometimes referenced during the description, each drawing merely schematically illustrates the shapes, sizes, and arrangements of the components to facilitate understanding of the invention. The present invention is not limited to the following embodiments and examples and may be arbitrarily modified and implemented without departing from the scope of the present invention and its equivalents. [Aluminum bonding wire or aluminum bonding tape] The aluminum bonding wire or aluminum bonding tape of the present invention contains silicon in an amount of not less than 3.0 mass % and not more than 20.0 mass %, and is characterized in that: when the crystal orientation of the aluminum phase in the L cross-section (a cross-section in the central axis direction including the central axis) of the aluminum bonding wire or aluminum bonding tape is measured, the orientation ratio of the <100> crystal orientation with an angle difference of not more than 15° relative to the direction parallel to the central axis (RD direction, rolling direction) (hereinafter also referred to as "the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction") is not less than 15% and not more than 50%, the number of silicon phases with an equivalent circle diameter of not less than 0.5 μm and not more than 0.8 μm in the L cross-section is set to Ns, and the number of silicon phases with an equivalent circle diameter of not less than 0.5 μm and not more than 0.8 μm in the L cross-section is set to Ns. When the number of silicon phases having a size of μm or larger is defined as Nc, a ratio of Ns to Nc [Ns / Nc×100(%)] is greater than or equal to 30% and less than or equal to 95%. As mentioned above, when a connecting material containing only high-purity aluminum is used in a temperature cycling test, cracks in the connecting material progress at a relatively fast rate, and reduced temperature cycling reliability becomes a problem. Regarding aluminum alloys with high concentrations of silicon added, it has been confirmed that the thermal expansion of the wire can be reduced, thereby improving temperature cycling reliability. In a high-speed temperature cycling test (high-speed TCT) that is close to actual use conditions and accelerates the temperature change rate, it has been confirmed that even for aluminum bonding wires or aluminum bonding strips whose reliability has not been reduced when evaluated in the previous TCT, there are cases where the bonding strength is reduced and the bonding life is shortened. Furthermore, regarding aluminum bonding wires or aluminum bonding strips that have been strengthened by adding silicon, etc., there are cases where internal cracks are generated during their manufacture. In addition, if the number of temperature cycles of the high-speed TCT increases, the bonding strength is likely to be further reduced. In order to meet the high-speed temperature cycling reliability required by the next generation of power semiconductor devices with higher heat resistance such as silicon carbide, it is necessary to further improve the high-speed temperature cycling reliability. The inventors have confirmed that the morphology and factors of defects in wire or ribbon joints change with increasing cycles in high-speed temperature cycling tests. While these variations depend on the specific conditions of the temperature history, cracks within the wire or ribbon predominate up to approximately 10,000 cycles. However, beyond 15,000 cycles, cracks at the joint interface and within the electrode develop simultaneously, leading to a decrease in reliability. While it can be difficult to distinguish cracks at the joint interface from those within the electrode when observing the joint cross-section, the inventors have discovered that classifying these cracks into two types and analyzing their relationship to the wire or ribbon structure is more effective when performing high cycle tests. High-speed TCT tends to concentrate stress at the bonding interface, resulting in an increased incidence of cracks at the bonding interface compared to conventional TCT. In addition to suppressing cracks within the wire or ribbon that occur at low cycle counts, it is crucial to address both crack suppression at the bonding interface and crack suppression within the electrodes as testing progresses to 20,000 cycles. The aforementioned cycle counts are standard values under certain high-speed TCT conditions. The required cycle count will vary depending on the high-speed TCT test conditions (temperature, time, heating and cooling rates) and the semiconductor device used. The present inventors conducted intensive research to address the aforementioned issues and discovered that by ensuring that an aluminum bonding wire or ribbon contains 3.0% to 20.0% silicon by mass, and simultaneously adjusting the <100> crystal orientation ratio of the aluminum phase in the direction parallel to the central axis (RD direction) in the L-section, and the number distribution of the silicon phase in the region with a relatively small equivalent circular diameter in the L-section (the ratio of the number of silicon phases within a specific range of equivalent circular diameter to the total number of silicon phases), reliability in high-speed TCT with a significant number of temperature cycles can be improved, contributing to longer life. By mutually controlling the structure based on the crystal orientation of the aluminum phase and the number distribution of the silicon phase, improved high-speed temperature cycling reliability can be achieved even in the strict high-speed TCT. The aluminum bonding wire or ribbon of the present invention contains silicon at a concentration of not less than 3.0% by mass and not more than 20.0% by mass. It comprises an aluminum phase in which silicon is solid-dissolved in aluminum, and a silicon phase formed by silicification or precipitation. The aluminum phase may also contain other additive elements in addition to silicon. The silicon phase is a general term for both silicification and silicon precipitates. Silicification forms from the melt during solidification and is relatively coarse, ranging in size from approximately 1 to 25 μm. In contrast, silicon precipitates form in a solid state and are relatively small, ranging in size from approximately 0.1 to several μm. In this invention, "wire" and "tape" are categorized not by shape but by their manufacturing method. Specifically, "wire" refers to a connecting material produced by a wire drawing process using an eye mold, while "tape" refers to a connecting material produced by a rolling process. Typically, a "wire" has a circular cross-section, while a "tape" has a rectangular or substantially rectangular cross-section. In the present invention, "ND direction" refers to a direction that satisfies "a direction perpendicular to the center axis" and "a direction perpendicular to the rolled surface". In the case of a wire, when an eye die is used for wire drawing, since forces are applied from all directions, the selection method of the ND direction is arbitrary, and the selection method of the L section (a section in the center axis direction including the center axis) is also arbitrary. Generally speaking, the selection method is such that the L section becomes perpendicular to the ND direction, and this selection method is also adopted in the present invention. In the case of a belt, the "ND direction" is uniquely determined by the definition of "a direction perpendicular to the rolled surface". On the other hand, in a belt, there are two selection methods for the L section: "a section perpendicular to the width W direction" and "a section perpendicular to the thickness T direction". However, in order to emphasize the ease of section grinding and EBSD analysis, the "section perpendicular to the width W direction" is set as the L section (Figure 2). Specifically, the central axis of the aluminum bonding wire, a cross-section in the central axis direction including the central axis (L cross-section), the RD direction, and the ND direction are shown in Figure 1. Figure 1 illustrates an aluminum bonding wire with a circular cross-section. However, in the case of an aluminum bonding tape with a rectangular or substantially rectangular cross-section having a width W and a thickness T, the central axis refers to the axis passing through the center of width W and the center of thickness T. Furthermore, the L cross-section refers to a cross-section in the central axis direction including the central axis, and this cross-section is perpendicular to the width W direction (Figure 2). Specifically, the central axis of the aluminum bonding tape, a cross-section in the central axis direction including the central axis (L cross-section), the RD direction, and the ND direction are shown in Figure 2. When cross-sectioning is performed to expose the L cross-section of the aluminum bonding wire, it may deviate from the central axis of the aluminum bonding wire. In this case, if the length of the L cross-section in the direction perpendicular to the central axis is at least 90% of the wire diameter of the aluminum bonding wire, it is considered to be a cross-section including the central axis. The reason why the aluminum bonding wire or aluminum bonding ribbon of the present invention can provide excellent reliability even in a high-speed temperature cycle test with a considerable number of cycles is presumably as follows. First, regarding high-speed temperature cycling reliability, it is believed that the silicon phase has a lower linear expansion coefficient than aluminum, which helps to minimize the difference in linear expansion coefficient between the aluminum bonding wire or ribbon and the semiconductor wafer, thereby reducing the thermal stress generated. Furthermore, it is believed that the particulate silicon phase inhibits crack growth within the aluminum bonding wire or ribbon. Before a high-speed temperature cycling (TCT) of approximately 10,000 cycles, adjusting the crystal orientation of the aluminum bonding wire or ribbon, which enhances this effect and effectively improves reliability, exploiting the effect of the silicon phase on reducing the linear expansion coefficient. On the other hand, as the number of temperature cycles increases and exceeds 15,000 cycles, the locations and behaviors of the internally stored thermal strain affecting the bonding interface of the aluminum bonding wire or ribbon and the electrodes being bonded to it change. Therefore, it is believed that the effects of the aluminum phase's crystal orientation and the silicon phase's particle size distribution, which influence cracks at the bonding interface of the aluminum bonding wire or ribbon and cracks within the electrodes, become stronger in joints that can withstand 20,000 cycles. Specifically, when measuring the crystal orientation of the aluminum phase in the L-section, the ratio of the <100> crystal orientation with an angle difference of 15° or less relative to the direction parallel to the central axis (RD direction) is set to 15% or more and 50% or less. This mitigates the stress increase within the aluminum bonding wire or ribbon during high-speed TCT, resulting in an enhanced effect of suppressing crack growth within the electrode. Furthermore, when the number of silicon phases with an equivalent circle diameter of 0.5 μm or more and 0.8 μm or less in the L-section is defined as Ns, and the number of silicon phases with an equivalent circle diameter of 0.5 μm or more in the L-section is defined as Nc, the ratio of Ns to Nc [Ns / Nc × 100 (%)] is set to 30% or more and 95% or less, thereby enhancing the effect of suppressing crack growth at the wire or ribbon bonding interface. The present invention is characterized by the interrelationship between the crystal orientation of the aluminum phase in the RD direction and the distribution of the equivalent circular diameter of the silicon phase, resulting in enhanced effects. However, these effects are described separately. When the ratio of the <100> crystal orientation of the aluminum phase in the RD direction is between 15% and 50%, the stress buildup within the line or band during temperature fluctuation is mitigated, suppressing its impact on adjacent electrodes and the development of cracks within the electrodes. Furthermore, by simultaneously maintaining a uniform distribution of the silicon phase with a relatively small equivalent circular diameter, the thermal strain distribution near the bonding interface is uniformed, further enhancing the effect of suppressing crack development at the bonding interface. Specifically, by combining the effects of controlling the <100> crystal orientation of the aluminum phase in the RD direction, which primarily reduces crack growth within the electrode, and controlling the distribution of the amount of silicon phase with a smaller equivalent circular diameter, which reduces crack growth at the joint interface, the time it takes for joint defects to occur can be extended under the rigorous test conditions of high-speed TCT, which can cycle approximately 20,000 cycles. While controlling the <100> orientation of the aluminum phase in the RD direction alone can suppress cracks within the wire or ribbon, and controlling the distribution of the amount of silicon phase with a smaller equivalent circular diameter alone can also suppress crack growth within the electrode, simultaneous control of both enhances the synergistic effect. There are cases where stress and strain are generated around the silicon phase with a larger equivalent circular diameter, or the silicon phase itself becomes the starting point of cracks. Compared with normal TCT, the temperature change in high-speed TCT is more intense, which leads to a greater impact of stress concentration and strain. On the other hand, it is believed that by making the silicon phase smaller, the stress concentration and strain near the bonding interface can be reduced relatively uniformly. Therefore, controlling the distribution of the number of silicon phases with a smaller equivalent circular diameter in the total number of silicon phases is effective in extending the life in high-speed temperature cycling tests. Under the condition of suppressing the progression of cracks inside the wire or strip when the number of cycles is small, the average value of the equivalent circular diameter of the silicon phase shows a certain degree of effect, but in a long cycle test such as 20,000 cycles, by controlling the distribution of the number of silicon phases with a smaller equivalent circular diameter in the total number of silicon phases, the unevenness of the test results can be suppressed, and the high-speed temperature cycling reliability can be stably improved. As described above, the aluminum bonding wire or aluminum bonding tape of the present invention helps to improve the temperature cycling reliability factor in the high-speed temperature cycling test and is appropriately controlled over a wide range of cycle numbers. As a result, it is speculated that it can bring excellent high-speed temperature cycling reliability as described above. -Silicon concentration- By setting the silicon concentration to a range of 3.0% by mass to 20.0% by mass, it helps to reduce the thermal strain of the joint and improve the high-speed temperature cycling reliability. Specifically, by setting the silicon concentration to 3.0% by mass or more, the improvement effect of the high-speed temperature cycling reliability can be increased. In addition, with the advancement and optimization of the equipment and conditions used for the manufacture or bonding of wires, etc., higher values can be allowed while suppressing abnormalities such as wire breakage or deterioration of surface properties during processing, reduction in initial bonding strength due to hardening, or damage to semiconductor chips. However, by setting the silicon concentration to 20.0% by mass or less, these defects can be well suppressed and the required high-speed temperature cycling reliability can be achieved. From the perspective of obtaining good high-speed temperature cycling reliability, the silicon concentration in the aluminum bonding wire or aluminum bonding ribbon of the present invention is 3.0 mass% or more, preferably 3.5 mass% or more, more preferably 4.0 mass% or more, and further preferably 4.2 mass% or more, 4.4 mass% or more, 4.5 mass% or more, 4.6 mass% or more, 4.8 mass% or more, or 5.0 mass% or more. Furthermore, to effectively suppress abnormalities such as a decrease in initial bonding strength or damage to the semiconductor wafer due to hardening, while achieving the required high-speed temperature cycling reliability, the silicon concentration in the aluminum bonding wire or aluminum bonding ribbon of the present invention is 20.0 mass% or less, preferably 19.0 mass% or less, 18.0 mass% or less, 17.0 mass% or less, 16.0 mass% or less, 15.0 mass% or less, 14.5 mass% or less, 14.0 mass% or less, 13.5 mass% or less, 13.0 mass% or less, or 12.5 mass% or less. Furthermore, if the hardness of the aluminum bonding wire or aluminum bonding ribbon is high, damage to the semiconductor wafer may occur more easily during the initial bonding process, depending on the bonding conditions of ultrasonic vibration and load. From the perspective of obtaining good bonding strength under a wider range of bonding conditions, the silicon concentration in the aluminum bonding wire or aluminum bonding ribbon of the present invention is preferably 12.0 mass % or less, further preferably 11.5 mass % or less or 11.0 mass % or less, and particularly preferably 10.8 mass % or less, 10.6 mass % or less, 10.5 mass % or less, 10.4 mass % or less, 10.2 mass % or less, or 10.0 mass % or less. The concentration of elements contained in the aluminum bonding wire or ribbon of the present invention can be analyzed using, for example, an ICP (Inductively Coupled Plasma) emission spectrometer or an ICP mass spectrometer. If elements such as oxygen or carbon, which are atmospheric pollutants, are adsorbed on the surface of the aluminum bonding wire or ribbon, it is effective to remove the adsorbed substances using an acid or base before analysis. - Crystallographic Orientation of the Aluminum Phase in the L-Cross-Section - To achieve excellent high-speed temperature cycling reliability even in high-speed TCT with a large number of cycles, when measuring the crystallographic orientation of the aluminum phase in the L-cross-section of the aluminum bonding wire or aluminum bonding ribbon, the orientation ratio of the <100> crystal orientation with an angle difference of 15° or less relative to the direction parallel to the central axis (RD direction) is 15% or more, preferably 20% or more, more preferably 22% or more, 24% or more, 26% or more, or 28% or more, further preferably 30% or more, and further preferably 35% or more. The upper limit of the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction is 50% or less, preferably 48% or less or 45% or less, further preferably 42% or less, and further preferably 40% or less, to achieve excellent high-speed temperature cycling reliability even in high-speed TCT with a large number of cycles. Here, by setting the ratio of the <100> crystal orientation of the aluminum phase in the RD direction to 15% or more, the length of cracks within the electrode during the high-speed temperature cycling test was dramatically reduced. Furthermore, by setting the ratio of the <100> crystal orientation of the aluminum phase in the RD direction to 50% or less, a good metal bond with the electrode was achieved during bonding. Due to these two effects, when the ratio of the <100> crystal orientation of the aluminum phase in the RD direction was set between 15% and 50%, the decrease in bonding strength after 20,000 cycles in the high-speed temperature cycling test was significantly suppressed. Aluminum Phase Crystallographic Orientation Measurement Method: The crystallographic orientation ratio of the aluminum phase in the L-section of an aluminum bonding wire or ribbon can be measured using a SEM-EDS-EBSD system. Specifically, a method is used that combines information on aluminum and silicon concentrations obtained using SEM-EDS (Scanning Electron Microscope-Energy Dispersive X-ray Spectroscopy) with information on crystallographic orientation obtained using electron backscatter diffraction (EBSD). More specifically, within the measurement area, which serves as the inspection surface for the L-section of the aluminum bonding wire or ribbon, aluminum and silicon concentrations are measured using EDS and crystallographic orientation analysis using EBSD is performed simultaneously. The analysis software included with the system then separates and extracts the aluminum and silicon phases from the EDS measurement results. Specifically, it is appropriate to utilize the Chi Scan function of the analysis software OIM Data Collection or OIM Analysis (both manufactured by TSL Solution) attached to the FE-SEM (Field Emission-Scanning Electron Microscope) device. Then, for a specific area of the aluminum phase, the analysis software attached to the device can be used to calculate the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction. When calculating the orientation ratio, a partial ratio (Partial Ratio) is used as the total area of the crystal orientation that can be identified based on a certain reliability within the measurement area. With respect to the crystal orientation of the aluminum phase, the area ratio of the <100> crystal orientation in the RD direction is set as the orientation ratio of the <100> crystal orientation in the RD direction. Therefore, in one embodiment, the orientation ratio of the crystal orientation of the aluminum phase in the L-section of the aluminum bonding wire or aluminum bonding tape of the present invention is calculated by the following steps (1) to (3). (1) In the measurement area where the L-section of the aluminum bonding wire or aluminum bonding tape is used as the inspection surface, the concentration of aluminum and silicon is measured using EDS, and the crystal orientation is measured using EBSD. (2) The Chi Scan function is used to separate and extract aluminum and silicon. Specifically, based on the measurement results of silicon EDS, a tolerance equivalent to the threshold of silicon is set, thereby separating and identifying aluminum and silicon. The crystal orientation can be analyzed using the crystal information of aluminum and silicon in the material file. (3) For the area specifically containing the aluminum phase, the crystal orientation is analyzed and the orientation ratio of the <100> crystal orientation in the RD direction is calculated. In step (2) above, the tolerance (%) setting can be selected within the range of 20 to 40%. In the standard analysis of the L-section of the aluminum bonding wire or aluminum bonding ribbon, it is preferably compared at approximately 30%. A supplementary explanation is provided regarding the step of adjusting the tolerance. It is preferred that the tolerance value be selected or confirmed in such a manner that the shape and size of the silicon phase extracted and identified using the Chi Scan function are equivalent to the shape and size of the silicon phase identified based on the EDS map that represents the silicon element concentration in a two-dimensional manner through EDS analysis. In the present invention, the orientation ratio of the <110> crystal orientation of the aluminum phase in the RD direction of the L-section is the average (arithmetic mean) of the orientation ratios measured at three or more locations. When selecting the measurement region, to ensure the objectivity of the measurement data, it is preferred to collect measurement samples at intervals of 50 cm or more relative to the central axis of the aluminum bonding wire or aluminum bonding tape to be measured and subject them to measurement. Furthermore, in the present invention, the region for crystal orientation measurement using the EBSD method is preferably 300 μm or longer and less than 800 μm in length in the direction of the central axis of the aluminum bonding wire or aluminum bonding tape, and should include the entire aluminum bonding wire or aluminum bonding tape in a direction perpendicular to the central axis. However, if the wire or aluminum bonding tape is large and measurement of the entire area is difficult, the region can be adjusted to a length less than 600 μm. - Distribution of Equivalent Circle Diameter of Silicon Phase in L-Section - To achieve excellent high-speed temperature cycling reliability even in high-speed TCT with a large number of cycles, assuming Ns is the number of silicon phases with an equivalent circle diameter of 0.5 μm or more and Nc is the number of silicon phases with an equivalent circle diameter of 0.5 μm or more in the L-section of an aluminum bonding wire or aluminum bonding ribbon, the ratio of Ns to Nc [Ns / Nc × 100 (%)] (hereinafter also referred to as the "small diameter ratio of the silicon phase") is 30% or more and 95% or less. The lower limit of the ratio [Ns / Nc × 100 (%)] is preferably 32% or more, 35% or more, 38% or more, 40% or more, 42% or more, or 45% or more, more preferably 48% or more, still more preferably 50% or more or 52% or more, and even more preferably 55% or more or 60% or more. The upper limit of the ratio [Ns / Nc×100(%)] is preferably 92% or less, 90% or less, 88% or less, or 85% or less, more preferably 82% or less, or 80% or less, further preferably 78% or less, or 75% or less, and particularly preferably 72% or less, or 70% or less. In one embodiment, the ratio [Ns / Nc×100(%)] is preferably 40% or more and 90% or less. The reasons why the ratio of silicon phases with an equivalent circular diameter of 0.5 μm or more and 0.8 μm or less is considered to be more important are as follows. That is, the silicon phase with an equivalent circular diameter of 0.5 μm or more can fully obtain the effect of reducing thermal expansion because its volume is large enough. In addition, from the perspective of the analysis accuracy of current EDS and EBSD analysis equipment, it is also appropriate to target silicon phases with an equivalent circular diameter of 0.5 μm or more. On the other hand, for silicon phases with an equivalent circular diameter of 0.8 μm or less, the stress and strain near the bonding interface will become sufficiently uniform due to the silicon phase. In addition, the reasons why it is considered that by making the range of the small diameter ratio of the silicon phase [Ns / Nc×100(%)] be 30% or more and 95% or less, even in high-speed TCT with a large number of cycles, excellent high-speed temperature cycle reliability can be obtained are as follows. Specifically, if the silicon phase's minor diameter ratio is 30% or greater, the silicon phase with a small equivalent circle diameter is abundantly present, resulting in a uniform distribution of thermal strain and stable high-speed temperature cycling reliability. On the other hand, if the silicon phase's minor diameter ratio is 95% or less, the total volume of the silicon phase increases, maintaining a high level of thermal expansion reduction across the entire bonding area and significantly enhancing the effect of improving high-speed temperature cycling reliability. Here, each silicon phase is formed in a particle-like form, and it has been confirmed that the number of silicon phase particles significantly influences the thermal strain at the bonding interface. Therefore, the ratio of silicon phase particles can be used to determine high-speed temperature cycling reliability. On the other hand, the impact of coarse particles is overestimated when considering particle area, making it difficult to accurately assess their correlation with high-speed temperature cycling reliability. -Average Diameter of Silicon Phase in L-Section- The aluminum bonding wire or aluminum bonding ribbon of the present invention preferably has an average diameter of the silicon phase in its L-section of 0.8 μm or more and 4.0 μm or less. The average diameter of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding ribbon of the present invention is more preferably 3.8 μm or less or 3.5 μm or less, further preferably 3.4 μm or less, 3.2 μm or less, or 3.0 μm or less. The lower limit is more preferably 1.0 μm or more or 1.1 μm or more, further preferably 1.2 μm or more or 1.5 μm or more. -Method for Measuring the Equivalent Circular Diameter of the Silicon Phase and Calculating the Minor Diameter Ratio- This section describes a method for measuring the equivalent circular diameter of the silicon phase in the L-section of an aluminum bonding wire or aluminum bonding ribbon. The equivalent circular diameter of the silicon phase in the L-section can be measured using a SEM-EDS-EBSD device. Specifically, similar to the measurement of the orientation ratio of the aluminum phase's crystal orientation described above, a method can be used that combines the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. A more detailed procedure can be the same as that described above for measuring the orientation ratio of the aluminum phase's crystal orientation, i.e., the crystal orientation of a region specifically designated as the silicon phase can be analyzed using the analysis software included with the device. If the orientation difference between the measurement points is 15° or greater, it is determined to be a grain boundary, and the equivalent circular diameter is calculated. The average value of the equivalent circular diameter of each silicon phase is defined as the average diameter of the silicon phase. In the process of calculating the minor diameter ratio of the silicon phase and the average diameter of the silicon phase, the parts where the crystal orientation cannot be determined, or even if the measurement is completed, the parts where the reliability of the orientation analysis is low are excluded from the calculation. Therefore, in one embodiment, the minor diameter ratio of the silicon phase and the average diameter of the silicon phase in the L cross section of the aluminum bonding wire or aluminum bonding tape of the present invention are calculated by the following steps (1) to (3). (1) The L cross section of the aluminum bonding wire or aluminum bonding tape is used as the inspection surface, and the concentration of aluminum and silicon is measured using EDS, and the crystal orientation is measured using EBSD. (2) Aluminum and silicon are separated and extracted using the Chi Scan function. Specifically, based on the measurement results of EDS of silicon, a tolerance equivalent to the threshold of silicon is set, thereby separating and identifying aluminum and silicon. The crystallization information of aluminum and silicon in the material file can be used to analyze the crystal orientation. (3) For the area specifically identified as the silicon phase, the crystal orientation is analyzed. If the orientation difference between the measurement points is 15° or more, it is judged to be a grain boundary, and the equivalent circle diameter of each crystal grain is calculated. The number of crystal grains identified as the silicon phase is totaled to calculate the total number of silicon phase particles Nc. Here, the silicon phase with an equivalent circle diameter of 0.5 μm or more is set as the target. Considering the analysis accuracy of current ESD and EBSD analysis equipment, fine particles less than 0.5 μm are excluded. In addition, the number Ns of silicon phases with an equivalent circle diameter of 0.5 μm or more and 0.8 μm or less is totaled. Then, the ratio of Ns to Nc [Ns / Nc×100(%)] (the ratio of the smaller diameter of the silicon phase) is calculated. The average diameter of the silicon phase is calculated by averaging the equivalent circle diameters of the individual grains. The average calculation uses an average value obtained by area averaging (area weighted averaging) that can be selected in the software included with the device. Figure 4 shows an example of the measurement results. The horizontal axis represents the equivalent circular diameter of the silicon phase, with each interval shown as 0.25 μm wide. The vertical axis represents the number of particles. The range between 0.5 μm and 0.8 μm is indicated by two arrows. The particle number ratio [Ns / Nc × 100%) in this interval is 50%. In high-speed temperature cycling testing of this aluminum bonding wire, even after 20,000 cycles, strength degradation remained low, confirming excellent high-speed temperature cycling reliability. - Crystal orientation of silicon phase in L cross section - If the bonding strength of multiple aluminum bonding wires or aluminum bonding ribbons is evaluated in a high-speed TCT, it is confirmed that multiple bonding parts do not deteriorate at the same time, and there is uneven degradation of the bonding strength. That is, even when the number of cycles of the high-speed temperature cycle test increases and the average value of the bonding strength is roughly maintained, the bonding parts of a small number of aluminum bonding wires or aluminum bonding ribbons begin to lose strength, resulting in uneven degradation of the bonding strength. Even for a small number of aluminum bonding wires or aluminum bonding ribbons, if the degradation of the bonding strength progresses, there is a concern that the load on other aluminum bonding wires or aluminum bonding ribbons will increase under high current, causing a sudden defect. In order to achieve the reliability required by the next generation of power semiconductor devices, it is required not only to manage the life based on the average value of the bonding strength in a high-speed TCT, but also to control the unevenness of the bonding strength. From the perspective of obtaining further improved high-speed temperature cycle reliability in high-speed TCT with a large number of cycles and from the perspective of suppressing uneven bonding strength, when measuring the crystal orientation of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding tape, the total orientation ratio of the <100> crystal orientation and the <111> crystal orientation with an angle difference of less than 15° relative to the vertical direction (ND direction, normal direction) of the central axis (hereinafter also referred to as the "total ratio of <100> + <111> of the silicon phase in the ND direction") is preferably in the range of more than 20% and less than 60%. In addition to controlling the <100> crystal orientation ratio of the aluminum phase in the RD direction and the minor diameter ratio of the silicon phase, by maintaining the combined <100> + <111> ratio of the silicon phase in the ND direction within the aforementioned range, local stress concentration is dispersed, reducing crack propagation at the bond interface. Consequently, shear strength variations after rigorous high-speed TCT (TCT) cycles exceeding 20,000 cycles can be mitigated. Furthermore, by aligning the <100> and <111> crystal orientations of the silicon phase in the ND direction with the <100> crystal orientation of the aluminum phase in the RD direction, it is believed that this can suppress local delamination at the bond interface even with increased cycles in high-speed TCT, where the temperature changes rapidly. The total ratio of <100> + <111> of the silicon phase in the ND direction is preferably 25% or greater, and more preferably 26% or greater, 28% or greater, or 30% or greater, from the perspective of achieving superior high-speed temperature cycling reliability in high-speed TCT with a large number of cycles and suppressing variation in bonding strength. The total ratio of <100> + <111> of the silicon phase is more preferably 58% or less, and more preferably 55% or less, 52% or less, 50% or less, 48% or less, or 45% or less, from the perspective of achieving superior high-speed temperature cycling reliability in high-speed TCT with a large number of cycles and suppressing variation in bonding strength. -Method for Determining the Crystallographic Orientation of the Silicon Phase- The orientation ratio of the silicon phase in the L-section of an aluminum bonding wire or aluminum bonding ribbon can be measured using a SEM-EDS-EBSD system. Specifically, similar to the determination of the orientation ratio of the aluminum phase, information on the aluminum and silicon concentrations obtained by SEM-EDS and information on the crystal orientation obtained by EBSD can be combined. The detailed procedure is the same as that described above for determining the orientation ratio of the aluminum phase. Specifically, for a region specifically containing the silicon phase, the analysis software included with the system is used to calculate the orientation ratio of the silicon phase in the ND direction, including the ratio of the <100> crystal orientation to the <111> crystal orientation, and their sum. This orientation ratio is calculated using a partial ratio, which is a measure of the area within the measurement region where only the crystal orientations that can be identified with a certain degree of reliability are considered as the total. Therefore, in one embodiment, the orientation ratio of the crystal orientation of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding tape of the present invention is calculated by the following steps (1) to (3). (1) In the measurement area with the L-section of the aluminum bonding wire or aluminum bonding tape as the inspection surface, the concentration of aluminum and silicon is measured using EDS and the crystal orientation analysis is performed using EBSD. (2) Aluminum and silicon are separated and analyzed using the Chi Scan function. Specifically, based on the measurement results of EDS of silicon, a tolerance equivalent to the threshold of silicon is set, thereby separating and identifying aluminum and silicon. The crystal orientation is analyzed using the crystal information of aluminum and silicon in the material file. (3) The crystal orientation is analyzed for the area specifically containing the silicon phase, and the orientation ratio of the <100> crystal orientation and the orientation ratio of the <111> crystal orientation of the silicon phase in the ND direction are calculated. In the present invention, the <100> crystal orientation ratio and the <111> crystal orientation ratio of the silicon phase in the ND direction in the L-section are the arithmetic averages of the values of the orientation ratios obtained by measuring at least three locations. The tolerance setting range, the method for obtaining the measurement sample, or the area for measuring the crystal orientation using the EBSD method in step (2) above are the same as those described above for the measurement of the crystal orientation ratio of the aluminum phase. -Shape of the Silicon Phase in the L-Section- When bonding aluminum bonding wire or aluminum bonding ribbon to electrodes on a conductive wafer, lead frame, or substrate, bonding defects, such as peeling of the aluminum bonding wire or aluminum bonding ribbon from the electrodes, can lead to product defects and reduced manufacturing yields. Therefore, good bonding strength is required at each bonding point. In this regard, applying strong ultrasonic vibration or load to achieve good bonding strength in the first bonding point can sometimes damage the semiconductor wafer. In particular, when using aluminum bonding wire or aluminum bonding ribbon that has been strengthened by the addition of silicon or other materials, its hardness can easily damage the semiconductor wafer during the first bonding. Adjusting the ultrasonic vibration or load to minimize this damage makes it impossible to stably secure the bonding area due to the high or low deformation resistance or instability of the deformation direction, and thus, sufficient bonding strength in the first bonding point (hereinafter referred to as "first bonding strength") cannot be achieved. Problems in the initial bonding of these first bonding portions may in turn lead to reduced or unstable reliability during high-speed temperature cycling. Therefore, aluminum bonding wires or aluminum bonding ribbons that are strengthened by adding silicon or the like are more ideal in order to exhibit excellent first bonding strength. The present inventors have discovered that by controlling the shape of the silicon phase (the ratio (e / f) of the short side length e to the long side length f of the silicon phase in its L-section), the following effects can be achieved: The adhesion of the interface between the silicon phase and the aluminum phase in the central axis direction is improved, which controls interfacial slip when ultrasonic vibration and load are applied, thereby improving the initial shear strength (first bond strength) immediately after bonding. Furthermore, as part of the effect of increasing initial shear strength, advantages such as stabilization of the failure time (lifespan) during high-speed temperature cycling testing are also achieved. Specifically, the present inventors studied aluminum bonding wires or aluminum bonding ribbons containing 3.0% to 20.0% silicon by mass, with a <100> ratio of the aluminum phase in the RD direction and a minor diameter ratio of the silicon phase in the L-section within specific ranges. They discovered that the shape of the silicon phase in the L-section affects the primary bonding strength. Specifically, by setting the average value of the ratio (e / f) of the short side length e to the long side length f of the silicon phase in the L-section to a range of 0.20 to 0.70, they found that in addition to suppressing the deterioration of bonding strength after high-speed TCT, the primary bonding strength was improved and even the unevenness of bonding strength was reduced. The numerical value of this ratio (e / f) represents an indicator of flatness. This is further explained with reference to FIG3 . Figure 3 schematically illustrates the silicon phase in an L-section of an aluminum bonding wire or ribbon. The central axis of the aluminum bonding wire or ribbon corresponds to the horizontal direction (left-right direction) in Figure 3, and the direction perpendicular to the central axis corresponds to the vertical direction (up-down direction) in Figure 2. Regarding the silicon phase in the L-section, the "short side length e" described above corresponds to the dimension indicated by the symbol e in Figure 3. Furthermore, regarding the silicon phase in the L-section, the "long side length f" described above corresponds to the dimension indicated by the symbol f in Figure 3. Hereinafter, the ratio (e / f) of the short side length e to the long side length f of the silicon phase in the L-section is also referred to as the "silicon phase aspect ratio (e / f)." The value of the silicon phase aspect ratio (e / f) can be calculated using the analysis software included with the device as the grain shape aspect ratio. The reason why the first bonding strength can be improved by controlling the average value of the silicon phase aspect ratio (e / f) in the aluminum bonding wire or aluminum bonding ribbon of the present invention is presumed to be as follows. The reason for the reduction in first bonding strength is that cracks develop along the central axis of the aluminum bonding wire or aluminum bonding ribbon or in a direction close thereto within the aluminum bonding wire or aluminum bonding ribbon or at the bonding interface. Here, due to the plastic working performed by wire drawing, the silicon phase tends to be arranged so that the direction of its long side length f is in the direction of the central axis of the aluminum bonding wire or aluminum bonding ribbon or in a direction close thereto. If the average value of the silicon phase aspect ratio (e / f) is within the range of 0.20 to 0.70, it is believed that the silicon phase takes on an elliptical or columnar shape, which acts to alleviate thermal stress in the direction of the central axis of the aluminum bonding wire or aluminum bonding ribbon, thereby suppressing the development of cracks along the central axis of the aluminum bonding wire or aluminum bonding ribbon or in a direction close thereto. Furthermore, to enhance the primary bonding strength, it is sufficient that the average aspect ratio (e / f) of the silicon phase in the L-section is within the aforementioned preferred range. It is not necessary for the average aspect ratio (e / f) of all silicon phases to be within the range of 0.20 to 0.70. For example, a silicon phase with an aspect ratio (e / f) less than 0.20 may be included, or a silicon phase with an aspect ratio (e / f) exceeding 0.70 may be included. From the perspective of improving primary bond strength, even reducing bond strength variation during high-speed TCT, and achieving the further improved reliability required of next-generation power semiconductor devices, the average value of the aspect ratio (e / f) of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding ribbon of the present invention is preferably 0.25 or greater, more preferably 0.30 or greater, and particularly preferably 0.32 or greater, 0.34 or greater, or 0.35 or greater. From the perspective of improving primary bond strength, the upper limit of the average value of the aspect ratio (e / f) of the silicon phase is more preferably 0.65 or less or 0.60 or less, and more preferably 0.58 or less, 0.56 or less, or 0.55 or less. -Method for measuring the aspect ratio (e / f) of the silicon phase- The method for measuring the aspect ratio (e / f) of the silicon phase in the L-section of an aluminum bonding wire or aluminum bonding ribbon is described. First, the measurement can be performed using an SEM-EDS-EBSD device, similar to the measurement of the crystal orientation and the measurement of the equivalent circular diameter of the silicon phase described above. Specifically, a method can be used that combines the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. A more detailed procedure can be set to be the same as that described above for the measurement of the orientation ratio of the crystal orientation, that is, for the region specifically designated as the silicon phase, the crystal orientation can be analyzed using the analysis software included with the device. If the orientation difference between the measurement points is 15° or more, it is determined to be a grain boundary, and the aspect ratio (e / f) is calculated. The average value of the shape ratio (e / f) of each silicon phase is defined as the average value of the shape ratio (e / f) of the silicon phase. In the process of calculating the shape ratio (e / f) of the silicon phase, the portion where the crystal orientation cannot be determined, or the portion where the reliability of the orientation analysis is low even if the determination is completed, is excluded from the calculation. Therefore, in one embodiment, the average value of the shape ratio (e / f) of the silicon phase in the L cross section of the aluminum bonding wire or aluminum bonding tape of the present invention is calculated by the following steps (1) to (3). (1) The L cross section of the aluminum bonding wire or aluminum bonding tape is used as the inspection surface, and the concentration of aluminum and silicon is measured using EDS and the crystal orientation is measured using EBSD at the same time. (2) Aluminum and silicon are separated and extracted using the Chi Scan function. Specifically, based on the measurement results of the EDS of silicon, a tolerance equivalent to the threshold value of silicon is set, thereby separating and identifying aluminum and silicon. The crystallization information of aluminum and silicon in the material file can be used to analyze the crystal orientation. (3) For the area specifically designated as the silicon phase, the crystal orientation is analyzed. If the orientation difference between the measurement points is 15° or more, it is determined to be a grain boundary. The shape ratio (e / f) of each grain is calculated. The shape ratio (e / f) of each grain is averaged to calculate the average value of the shape ratio (e / f) of the silicon phase. Here, the average value of the shape ratio (e / f) of the silicon phase is calculated using the value of the Grain Shape Aspect Ratio (hereinafter referred to as "grain shape aspect ratio") in the analysis software. This value is obtained by averaging the grain shape aspect ratios of each grain and calculating the average value. In addition, regarding the calculation method of the grain shape aspect ratio, the ratio (e / f) of the short side length (e) (Grain Shape Minor Axis) and the long side length (f) (Grain Shape Major Axis) of one grain is calculated. In addition, regarding the average calculation, an average value obtained based on the area average (area weighted average) selectable in the software included with the device is used.By using the average value calculated by area averaging, it is possible to accurately measure and determine whether the average value of the silicon phase aspect ratio (e / f) meets the conditions. This is suitable for reducing the unevenness of bonding strength in high-speed temperature cycling tests with a large number of cycles, thereby achieving further improvement in the high-speed temperature cycling reliability required by next-generation power semiconductor devices. When measuring the average value of the aspect ratio (e / f) of the silicon phase in the L cross-section, the setting range of the tolerance in the above step (2) and the area for determining the crystal orientation using the EBSD method are the same as described above for the determination of the orientation ratio of the crystal orientation of the aluminum phase. Furthermore, in addition to the above-mentioned methods, there are also some methods for measuring the equivalent circular diameter of the silicon phase or the shape ratio (e / f) of the silicon phase, including binarization processing of the observation image from the L cross-section. However, in the present invention, based on the multiple characteristics such as the above-mentioned crystal orientation, the equivalent circular diameter of the silicon phase or the shape ratio (e / f) of the silicon phase obtained by a single measurement with multiple measurement functions, automatic analysis can be achieved, and the equipment and analysis technology are relatively popular and easy to measure, it is preferable to use the method of combining the information on aluminum concentration and silicon concentration obtained by SEM-EDS and the information on crystal orientation obtained by EBSD as described above. -Addition of Strontium, Sodium, Iron, and Phosphorus- The aluminum bonding wire or aluminum bonding ribbon of the present invention may further contain one or more of strontium, sodium, iron, and phosphorus (hereinafter also referred to as the "first element group"). The total concentration of the first element group may be 0 mass ppm, preferably 1 mass ppm or more, more preferably 3 mass ppm or more, further preferably 5 mass ppm or more, and particularly preferably 8 mass ppm or more or 10 mass ppm or more. The upper limit of the total concentration of the first element group is preferably 10,000 mass ppm or less or 8,000 mass ppm or less, more preferably 5,000 mass ppm or less or 3,000 mass ppm or less, further preferably 2,000 mass ppm or less or 1,000 mass ppm or less, and particularly preferably 900 mass ppm or less or 800 mass ppm or less. In one embodiment, the total concentration of the first element group is preferably 10 mass ppm or more and 800 mass ppm or less. The aluminum bonding wire or aluminum bonding ribbon of the present invention further contains a total of 10 to 800 mass ppm of at least one of strontium, sodium, iron, and phosphorus, thereby reducing the frequency of wire breakage during the wire drawing process. Aluminum alloys containing silicon at high concentrations of 3.0 to 20.0 mass % tend to experience increased wire breakage during the wire drawing process. This is believed to be due to stress concentration caused by silicon phase particles that crystallize during solidification, leading to wire breakage. It is speculated that the addition of the first element group can uniformly distribute the particulate silicon phase and inhibit the growth and coarsening of the silicon phase. These effects can alleviate stress concentration during the wire drawing process and reduce wire breakage. It is believed that by controlling the orientation ratio of the aluminum phase's crystallographic orientation in the RD direction of the L-section and the minor diameter ratio of the silicon phase, while adding the first element group, the effect of alleviating stress concentration during the wire drawing process can be enhanced. From the perspective of reducing the frequency of wire breakage during wire drawing, the total concentration of the first element group in the aluminum bonding wire or aluminum bonding tape of the present invention is preferably 20 mass ppm or more, and further preferably 30 mass ppm or more, 40 mass ppm or more, or 50 mass ppm or more. The upper limit is preferably 750 mass ppm or less, more preferably 740 mass ppm or less, 720 mass ppm or less, or 700 mass ppm or less, and further preferably 680 mass ppm or less, 650 mass ppm or less, 620 mass ppm or less, or 600 mass ppm or less, and particularly preferably 580 mass ppm or less, 550 mass ppm or less, 520 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains at least one element from the first element group, it may contain any one element from the first element group, any two elements from the first element group, any three elements from the first element group, or all four elements from the first element group. Furthermore, when the aluminum bonding wire or aluminum bonding ribbon of the present invention contains at least one element from the first element group, it may also contain strontium, sodium, iron, or phosphorus. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains strontium from the first element group, the strontium concentration can be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, or 8 mass ppm or higher. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the strontium concentration is more preferably 10 mass ppm or higher, and even more preferably 20 mass ppm or higher, 30 mass ppm or higher, 40 mass ppm or higher, or 50 mass ppm or higher. The upper limit of the strontium concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, 3,000 mass ppm or lower, 2,000 mass ppm or lower, 1,000 mass ppm or lower, or 900 mass ppm or lower. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the strontium concentration is preferably 800 mass ppm or less, and further preferably 750 mass ppm or less, 740 mass ppm or less, 720 mass ppm or less, 700 mass ppm or less, 680 mass ppm or less, 650 mass ppm or less, 620 mass ppm or less, 600 mass ppm or less, 580 mass ppm or less, 550 mass ppm or less, 520 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains sodium from the first element group, the sodium concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, or 8 mass ppm or higher. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the sodium concentration is more preferably 10 mass ppm or higher, and even more preferably 20 mass ppm or higher, 30 mass ppm or higher, 40 mass ppm or higher, or 50 mass ppm or higher. The upper limit of the sodium concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, 3,000 mass ppm or lower, 2,000 mass ppm or lower, 1,000 mass ppm or lower, or 900 mass ppm or lower. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the sodium concentration is preferably 800 mass ppm or less, and further preferably 750 mass ppm or less, 740 mass ppm or less, 720 mass ppm or less, 700 mass ppm or less, 680 mass ppm or less, 650 mass ppm or less, 620 mass ppm or less, 600 mass ppm or less, 580 mass ppm or less, 550 mass ppm or less, 520 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains iron from the first element group, the iron concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, or 8 mass ppm or higher. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the iron concentration is more preferably 10 mass ppm or higher, and even more preferably 20 mass ppm or higher, 30 mass ppm or higher, 40 mass ppm or higher, or 50 mass ppm or higher. The upper limit of the iron concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, 3,000 mass ppm or lower, 2,000 mass ppm or lower, 1,000 mass ppm or lower, or 900 mass ppm or lower. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the iron concentration is preferably 800 mass ppm or less, and further preferably 750 mass ppm or less, 740 mass ppm or less, 720 mass ppm or less, 700 mass ppm or less, 680 mass ppm or less, 650 mass ppm or less, 620 mass ppm or less, 600 mass ppm or less, 580 mass ppm or less, 550 mass ppm or less, 520 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains phosphorus from the first element group, the phosphorus concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, or 8 mass ppm or higher. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the phosphorus concentration is more preferably 10 mass ppm or higher, and even more preferably 20 mass ppm or higher, 30 mass ppm or higher, 40 mass ppm or higher, or 50 mass ppm or higher. The upper limit of the phosphorus concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, 3,000 mass ppm or lower, 2,000 mass ppm or lower, 1,000 mass ppm or lower, or 900 mass ppm or lower. Furthermore, from the perspective of reducing the frequency of wire breakage during wire drawing, the phosphorus concentration is preferably 800 mass ppm or less, and further preferably 750 mass ppm or less, 740 mass ppm or less, 720 mass ppm or less, 700 mass ppm or less, 680 mass ppm or less, 650 mass ppm or less, 620 mass ppm or less, 600 mass ppm or less, 580 mass ppm or less, 550 mass ppm or less, 520 mass ppm or less, or 500 mass ppm or less. - Addition of Titanium, Nickel, Magnesium, and Copper - The aluminum bonding wire or aluminum bonding ribbon of the present invention may further contain one or more of titanium, nickel, magnesium, and copper (hereinafter also referred to as the "second element group"). The total concentration of the second element group may be 0 mass ppm, preferably 1 mass ppm or more or 3 mass ppm or more, more preferably 5 mass ppm or more or 8 mass ppm or more, further preferably 10 mass ppm or more or 30 mass ppm or more, and particularly preferably 50 mass ppm or more, 80 mass ppm or more, or 100 mass ppm or more. The upper limit of the total concentration of the second element group is preferably 10,000 mass ppm or less, more preferably 8,000 mass ppm or less, further preferably 5,000 mass ppm or less, and particularly preferably 3,000 mass ppm or less or 2,000 mass ppm or less. In one embodiment, the total concentration of the second element group is preferably 100 mass ppm or more and 2,000 mass ppm or less. The aluminum bonding wire or ribbon of the present invention further contains a total of 100 to 2000 mass ppm of one or more of titanium, nickel, magnesium, and copper. This prevents damage and scratches on the surface of the aluminum bonding wire or ribbon, resulting in a smooth surface. Aluminum alloys containing silicon at high concentrations of 3.0 to 20.0 mass percent can cause surface damage and scratches during wire drawing due to surface hardening or shedding of silicon phases and aluminum oxide on the surface, resulting in significant surface irregularities in the aluminum bonding wire or ribbon. It is speculated that the addition of the second element group stabilizes the aluminum oxide on the surface of the aluminum bonding wire or ribbon, refines the aluminum grain structure, and hardens it, thereby reducing damage and scratches during wire drawing. It is believed that by controlling the orientation ratio of the crystal orientation of the aluminum phase in the RD direction in the L cross-section and the diameter ratio of the silicon phase while adding the second element group, the effect of suppressing the damage and scratches on the surface of the aluminum bonding wire or aluminum bonding tape can be improved, thereby forming a smooth surface. From the perspective of suppressing the occurrence of surface damage and scratches and forming an aluminum bonding wire or aluminum bonding tape with a smooth surface, the total concentration of the second element group in the aluminum bonding wire or aluminum bonding tape of the present invention is preferably 150 mass ppm or more, further preferably 200 mass ppm or more, 250 mass ppm or more, or 300 mass ppm or more, and the upper limit is preferably 1800 mass ppm or less, more preferably 1600 mass ppm or less, 1500 mass ppm or less, or 1200 mass ppm or less, further preferably 1000 mass ppm or less, 900 mass ppm or less, or 800 mass ppm or less, and particularly preferably 700 mass ppm or less, 600 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains at least one element from the second element group, it may contain any one element from the second element group, any two elements from the second element group, any three elements from the second element group, or all four elements from the second element group. Furthermore, when the aluminum bonding wire or aluminum bonding ribbon of the present invention contains at least one element from the second element group, it may contain titanium, nickel, magnesium, or copper. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains titanium from the second element group, the titanium concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, 8 mass ppm or higher, 10 mass ppm or higher, 30 mass ppm or higher, 50 mass ppm or higher, or 80 mass ppm or higher. Furthermore, from the perspective of suppressing surface damage and scratches, thereby forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the titanium concentration is more preferably 100 mass ppm or higher, and even more preferably 150 mass ppm or higher, 200 mass ppm or higher, 250 mass ppm or higher, or 300 mass ppm. The upper limit of the titanium concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, or 3,000 mass ppm or lower. Furthermore, from the perspective of suppressing the occurrence of surface damage and scratches and forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the titanium concentration is preferably 2000 mass ppm or less, and further preferably 1800 mass ppm or less, 1600 mass ppm or less, 1500 mass ppm or less, 1200 mass ppm or less, 1000 mass ppm or less, 900 mass ppm or less, 800 mass ppm or less, 700 mass ppm or less, 600 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains nickel from the second element group, the nickel concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, 8 mass ppm or higher, 10 mass ppm or higher, 30 mass ppm or higher, 50 mass ppm or higher, or 80 mass ppm or higher. Furthermore, from the perspective of suppressing surface damage and scratches, thereby forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the nickel concentration is more preferably 100 mass ppm or higher, and even more preferably 150 mass ppm or higher, 200 mass ppm or higher, 250 mass ppm or higher, or 300 mass ppm. The upper limit of the nickel concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, or 3,000 mass ppm or lower. Furthermore, from the perspective of suppressing the occurrence of surface damage and scratches and forming an aluminum bonding wire or aluminum bonding tape with a smooth surface, the nickel concentration is preferably 2000 mass ppm or less, and further preferably 1800 mass ppm or less, 1600 mass ppm or less, 1500 mass ppm or less, 1200 mass ppm or less, 1000 mass ppm or less, 900 mass ppm or less, 800 mass ppm or less, 700 mass ppm or less, 600 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains magnesium from the second element group, the magnesium concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, 8 mass ppm or higher, 10 mass ppm or higher, 30 mass ppm or higher, 50 mass ppm or higher, or 80 mass ppm or higher. Furthermore, from the perspective of suppressing surface damage and scratches, thereby forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the magnesium concentration is more preferably 100 mass ppm or higher, and even more preferably 150 mass ppm or higher, 200 mass ppm or higher, 250 mass ppm or higher, or 300 mass ppm. The upper limit of the magnesium concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, or 3,000 mass ppm or lower. Furthermore, from the viewpoint of suppressing the occurrence of surface damage and scratches and forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the magnesium concentration is more preferably 2000 mass ppm or less, and further preferably 1800 mass ppm or less, 1600 mass ppm or less, 1500 mass ppm or less, 1200 mass ppm or less, 1000 mass ppm or less, 900 mass ppm or less, 800 mass ppm or less, 700 mass ppm or less, 600 mass ppm or less, or 500 mass ppm or less. When the aluminum bonding wire or aluminum bonding ribbon of the present invention contains copper from the second element group, the copper concentration may be 0 mass ppm, but is preferably 1 mass ppm or higher, 3 mass ppm or higher, 5 mass ppm or higher, 8 mass ppm or higher, 10 mass ppm or higher, 30 mass ppm or higher, 50 mass ppm or higher, or 80 mass ppm or higher. Furthermore, from the perspective of suppressing surface damage and scratches, thereby forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the copper concentration is more preferably 100 mass ppm or higher, and even more preferably 150 mass ppm or higher, 200 mass ppm or higher, 250 mass ppm or higher, or 300 mass ppm. The upper limit of the copper concentration is preferably 10,000 mass ppm or lower, 8,000 mass ppm or lower, 5,000 mass ppm or lower, or 3,000 mass ppm or lower. Furthermore, from the viewpoint of suppressing the occurrence of surface damage and scratches and forming an aluminum bonding wire or aluminum bonding ribbon with a smooth surface, the copper concentration is more preferably 2000 mass ppm or less, and further preferably 1800 mass ppm or less, 1600 mass ppm or less, 1500 mass ppm or less, 1200 mass ppm or less, 1000 mass ppm or less, 900 mass ppm or less, 800 mass ppm or less, 700 mass ppm or less, 600 mass ppm or less, or 500 mass ppm or less. When manufacturing the aluminum bonding wire or aluminum bonding ribbon of the present invention, aluminum with a purity of 4N (aluminum: 99.99% by mass or greater) is preferably used, and aluminum with a purity of 5N (aluminum: 99.999% by mass or greater) or greater, which has a lower amount of impurities, is more preferably used. Furthermore, in one embodiment, aluminum with a purity of 3N (aluminum: 99.9% by mass or greater) can also be used. The aluminum bonding wire or ribbon of the present invention may further contain elements other than aluminum, silicon, the first element group, and the second element group (hereinafter referred to as "other elements"), within a range that does not impair the effects of the present invention. Specifically, "other elements" refer to elements other than aluminum, silicon, strontium, sodium, iron, phosphorus, titanium, nickel, magnesium, and copper. The aluminum bonding wire or ribbon of the present invention may further contain elements other than aluminum, silicon, strontium, sodium, iron, phosphorus, titanium, nickel, magnesium, and copper. The total concentration of other elements in the aluminum bonding wire or ribbon is not particularly limited, as long as it does not impair the effects of the present invention. The total concentration of the other elements may be, for example, 0.5 mass % or less, 0.4 mass % or less, 0.3 mass % or less, 0.2 mass % or less, 0.15 mass % or less, 0.1 mass % or less, 0.08 mass % or less, 0.06 mass % or less, 0.05 mass % or less, 0.04 mass % or less, 0.03 mass % or less, 0.025 mass % or less, 0.02 mass % or less, 0.018 mass % or less, 0.016 mass % or less, 0.015 mass % or less, 0.014 mass % or less, 0.012 mass % or less, or 0.01 mass %. The lower limit of the total concentration of the other elements is not particularly limited and may be 0 mass %. In one embodiment, the remainder of the aluminum bonding wire or ribbon of the present invention comprises aluminum and other elements. Thus, in one preferred embodiment, the aluminum bonding wire or ribbon of the present invention comprises aluminum, silicon, and other elements. In another preferred embodiment, the aluminum bonding wire or ribbon of the present invention comprises aluminum, silicon, one or more elements from the first element group, and other elements. In yet another preferred embodiment, the aluminum bonding wire or ribbon of the present invention comprises aluminum, silicon, one or more elements from the second element group, and other elements. In yet another preferred embodiment, the aluminum bonding wire or ribbon of the present invention comprises aluminum, silicon, one or more elements from the first element group, one or more elements from the second element group, and other elements. In one embodiment, the remainder of the aluminum bonding wire or aluminum bonding ribbon of the present invention comprises aluminum and inevitable impurities. Therefore, in one suitable embodiment, the aluminum bonding wire or aluminum bonding ribbon of the present invention comprises aluminum, silicon, and inevitable impurities. In another suitable embodiment, the aluminum bonding wire or aluminum bonding ribbon of the present invention comprises aluminum, silicon, one or more elements of the first element group, and inevitable impurities. In yet another suitable embodiment, the aluminum bonding wire or aluminum bonding ribbon of the present invention comprises aluminum, silicon, one or more elements of the second element group, and inevitable impurities. In yet another suitable embodiment, the aluminum bonding wire or aluminum bonding ribbon of the present invention comprises aluminum, silicon, one or more elements of the first element group, one or more elements of the second element group, and inevitable impurities. In one preferred embodiment, the aluminum bonding wire or ribbon of the present invention does not have a coating primarily composed of a metal other than aluminum on its outer periphery. Here, "a coating primarily composed of a metal other than aluminum" refers to a coating containing a metal other than aluminum at a content of 50% by mass or greater. The aluminum bonding wire or aluminum bonding tape of the present invention can be an aluminum bonding wire or an aluminum bonding tape. In the case of the aluminum bonding wire of the present invention, the wire diameter is not particularly limited, and can be, for example, 50 μm or more, 60 μm or more, 80 μm or more, 100 μm or more, 120 μm or more, 140 μm or more, 150 μm or more, 180 μm or more, or 200 μm or more. The upper limit of the wire diameter is not particularly limited, and can be, for example, 600 μm or less, 550 μm or less, 500 μm or less, 450 μm or less, or 400 μm or less. In one embodiment, the wire diameter of the aluminum bonding wire of the present invention can be in the range of 100 to 600 μm, preferably 200 to 400 μm. In the case of an aluminum bonding tape of the present invention, the size of its rectangular or substantially rectangular cross section (width W×thickness T) is not particularly limited. For example, W may be 100-3000 μm, and T may be 50-600 μm. The aluminum bonding wire or ribbon of the present invention exhibits excellent high-speed temperature cycling reliability even in high-cycle high-speed temperature cycling tests. Therefore, the aluminum bonding wire or ribbon of the present invention is suitable for use as an aluminum bonding wire or ribbon for semiconductor devices. The aluminum bonding wire or ribbon of the present invention is particularly suitable for use as an aluminum bonding wire or ribbon for power semiconductor devices, and is even more suitable for use as an aluminum bonding wire or ribbon for silicon carbide power semiconductor devices. -Method for Manufacturing Aluminum Bonding Wire or Aluminum Bonding Ribbon- An example of a method for manufacturing an aluminum bonding wire or an aluminum bonding ribbon according to the present invention will be described. Hereinafter, the manufacturing of an aluminum bonding wire will be described as an example. Aluminum and alloying elements used as raw materials are preferably of high purity. Aluminum preferably has a purity of 99.5% by mass or greater, with the remainder consisting of unavoidable impurities, more preferably 99.9% by mass or greater, and even more preferably 99.99% by mass or greater. Silicon, the first group of elements, the second group of elements, and other elements used as alloying elements preferably have a purity of 99.9% by mass or greater, with the remainder consisting of unavoidable impurities, more preferably 99.99% by mass or greater. Aluminum alloys used for aluminum bonding wire can be manufactured by placing aluminum and alloying element raw materials into a graphite or alumina crucible processed to obtain a cylindrical ingot, and then melting the raw materials in an electric furnace or high-frequency heating furnace. The diameter of the cylindrical ingot is preferably set to 6 mm or greater and less than 8 mm to consider workability in subsequent processing steps. The atmosphere within the furnace during melting is preferably an inert or reducing atmosphere to prevent excessive oxidation of the aluminum or silicon, the first group of elements, the second group of elements, and other elements that constitute the wire. The maximum temperature limit of the melt during melting is preferably set to 800°C or greater and less than 1050°C to ensure fluidity and facilitate control of the shape and size of the silicon phase during solidification. Cooling methods after melting can include water cooling, furnace cooling, and air cooling. The cylindrical ingot obtained by melting is subjected to a solution treatment at high temperature, followed by repeated wire drawing using an eye die to produce wire of the desired diameter. The drawn wire undergoes a final heat treatment in an electric furnace and can be used as aluminum bonding wire. To control the crystal orientation of the aluminum phase in the L-section, the minor diameter ratio of the silicon phase, the average diameter of the silicon phase, and the crystal orientation of the silicon phase, it is effective to control the heat treatment conditions such as the solution treatment, homogenization treatment, and final heat treatment, as well as the wire drawing process conditions. During the wire drawing process, the use of a lubricant is effective to ensure lubricity at the contact interface between the wire and the eye mold. An example of manufacturing conditions for controlling the <100> crystal orientation ratio of the aluminum phase in the RD direction in the L cross section within a range of 15% to 50% and for controlling the small diameter ratio of the silicon phase within a range of 30% to 95% is shown below. <Control of the <100> Crystal Orientation of the Aluminum Phase in the RD Direction> Regarding wire drawing conditions, it is effective to set the wire reduction ratio per eye die used during wire drawing to a range of 10% or greater and less than 20%. Here, if the wire reduction ratio per eye die is defined as P1, P1 is expressed by the following formula. P1={(R 2 2 -R 1 2 ) / R 2 2}×100 Where, R 2 represents the diameter of the wire before processing (mm), R 1 represents the diameter of the wire after processing (mm). By controlling the average eye mold reduction ratio within a range of 10% to 20% to control the processing strain, the <100> crystal orientation of the aluminum phase in the RD direction can be adjusted. For example, increasing the processing strain by increasing the reduction ratio helps control the ratio of the <100> crystal orientation of the aluminum phase in the RD direction, which forms the recrystallized structure during heat treatment. Adjusting the conditions of the intermediate heat treatment makes it easier to adjust the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction. The intermediate heat treatment is a heat treatment performed during the process from ingot processing to the final wire diameter. The number of intermediate heat treatments is preferably in the range of 3 to 4 times, and the wire diameter for which the intermediate heat treatment is performed can be selected. Among them, the intermediate heat treatment (intermediate annealing) with a temperature range of 250°C or more and less than 400°C and a time of 1 hour or more and less than 48 hours is performed at least once in the range of 4.0 to 5.5 times the final wire diameter and at least once in the range of 2.0 to 3.5 times the final wire diameter. This helps to adjust the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction under the final wire diameter to a range of 15% or more and 50% or less. By performing the intermediate heat treatment under these conditions, the processing strain in the aluminum phase is reduced, causing mild recrystallization, thereby reducing the processed structure of the aluminum phase at the final wire diameter. The subsequent heat treatment increases the degree of recrystallization of the aluminum phase or promotes the rotation of the crystal orientation, making it easier to adjust the <100> crystal orientation ratio of the aluminum phase in the RD direction. On the other hand, if the intermediate heat treatment temperature is set above 400°C, there is a concern that the <100> crystal orientation ratio of the aluminum phase in the RD direction may become unstable. <Control of the Small Diameter Ratio of the Silicon Phase> To control the small diameter ratio of the silicon phase, it is effective to adapt the intermediate heat treatment conditions to the final heat treatment conditions as a set. Specifically, if the temperature of the intermediate heat treatment for the wire diameter closest to the final wire diameter (final) is set to Tm (°C), and the temperature of the final heat treatment below the final wire diameter is set to Tc (°C), then the intermediate heat treatment temperature Tm is at least 50°C higher than the final heat treatment temperature Tc, thereby making it easier to adjust the small diameter ratio of the silicon phase to between 30% and 95%. Specifically, by increasing the intermediate heat treatment temperature, the silicon dissolved in the aluminum phase can be homogenized, and by lowering the temperature of the final heat treatment step, the solid solution concentration of silicon in the aluminum phase can be reduced. By combining these temperatures, the number of micro-silicon phases is increased, thereby increasing the small diameter ratio of the silicon phase. A more effective method is to adjust the temperature of the last intermediate heat treatment among multiple intermediate heat treatments, and utilize the increased dislocation in the subsequent processing steps, which is believed to help increase the number of tiny silicon phases. Regarding the final heat treatment conditions, it is effective to adjust them within the temperature range of 200°C or more and less than 360°C and the time range of 2 hours or more and less than 20 hours. While the aluminum phase is being restored and recrystallized by the final heat treatment, the amount of silicon dissolved in the aluminum phase will change due to the heat treatment temperature, resulting in a change in the recrystallization temperature. By adjusting the progress of recrystallization by the final heat treatment, it becomes easy to control the diameter ratio of the silicon phase. For example, by adjusting the final heat treatment at a low temperature or for a short time, there is a tendency for the diameter ratio of the silicon phase to increase. In addition, by adjusting the final heat treatment conditions, it also becomes easy to control the average value of the equivalent circular diameter of the silicon phase (the average diameter of the silicon phase). <Control of the Aspect Ratio of Silicon Phase (e / f)> To adjust the aspect ratio (e / f) of the silicon phase in the L-section, it is effective to control the conditions of the above-mentioned two-stage heat treatment (solution treatment and homogenization treatment) and the final heat treatment. It is preferred that the solution treatment temperature of the ingot be set to a range of 400°C to less than 550°C, for a duration of 1 hour to less than 6 hours, and the subsequent homogenization treatment be set to a temperature of 250°C to less than 350°C, for a duration of 2 hours to less than 6 hours. The solution treatment causes the separation and growth of the crystallized silicon phase during solidification, while the homogenization treatment causes the dissolution and precipitation of silicon at the silicon phase interface, thereby controlling the shape of the silicon phase. For example, if the solution treatment is performed at a high temperature, the aspect ratio (e / f) of the silicon phase tends to decrease. <Control of the Crystallographic Orientation of the Silicon Phase in the ND Direction> In order to adjust the crystallographic orientation of the silicon phase in the ND direction, it is effective to control the area reduction ratio during wire drawing while performing two-stage heat treatment (solution treatment and homogenization treatment) on the ingot. It is effective to perform the solution treatment at a temperature range of 450°C to less than 550°C, and for a time of 1 hour to less than 6 hours. After the solution treatment, it is effective to perform a homogenization treatment at a temperature of 250°C to less than 350°C, and for a time of 2 hours to less than 6 hours. This promotes the separation and growth of the crystallized silicon phase during solidification, and adjusts the crystallographic orientation of the silicon phase in the ND direction to either a <100> or <111> orientation. It is also effective to incorporate a wire drawing assembly with a high eye mold reduction ratio (between 20% and 30%) into the wire drawing step to increase processing strain and control the crystal orientation of the silicon phase. When the wire drawing step is performed two or more times, the eye mold reduction ratio can be set to between 20% and 30% in at least one of the wire drawing steps. By adjusting the wire reduction ratio within the aforementioned range, the entire aluminum bonding wire or aluminum bonding ribbon is significantly deformed during eye mold processing, increasing processing strain within the aluminum bonding wire or aluminum bonding ribbon. Then, while the silicon phase is aligned along the central axis of the aluminum bonding wire or aluminum bonding ribbon, the processing strain within the silicon phase is adjusted. When the crystal orientation of the silicon phase cannot be simply adjusted by the above-mentioned two-stage heat treatment of the ingot (solution treatment and homogenization treatment), it is also possible to adjust the orientation ratio of the <100> crystal orientation and the <111> crystal orientation of the silicon phase in the ND direction by incorporating an operation of adjusting the eye mold reduction rate within the above-mentioned range. The above description uses the production of aluminum bonding wire as a wire material as an example, serving as a representative example of aluminum bonding wire or aluminum bonding tape. Aluminum bonding tape as a strip material can also be produced using essentially the same steps. The heat treatment temperature and time conditions described above can be used. Furthermore, when producing aluminum bonding tape by rolling, the reduction ratio of the eye die can be adjusted by replacing it with the rolling reduction ratio. [Semiconductor Device] A semiconductor device can be manufactured by connecting electrodes on a semiconductor wafer to external electrodes on a lead frame or substrate using the aluminum bonding wire or aluminum bonding ribbon of the present invention. Specifically, the semiconductor device of the present invention includes the aluminum bonding wire or aluminum bonding ribbon of the present invention. As described above, both the first bond to the electrode on the semiconductor wafer and the second bond to the electrode on the lead frame or substrate can be made using wedge bonding. In one embodiment, the semiconductor device of the present invention is characterized by including a circuit substrate, a semiconductor chip, and an aluminum bonding wire or aluminum bonding ribbon for conducting electricity between the circuit substrate and the semiconductor chip, and the aluminum bonding wire or aluminum bonding ribbon is the aluminum bonding wire or aluminum bonding ribbon of the present invention. In the semiconductor device of the present invention, the circuit substrate and semiconductor wafer are not particularly limited, and any known circuit substrate and semiconductor wafer that can be used to construct a semiconductor device can be used. Alternatively, a lead frame can be used in place of the circuit substrate. For example, as in the semiconductor device described in Japanese Patent Application Laid-Open No. 2020-150116, a semiconductor device can be constructed that includes a lead frame and a semiconductor wafer mounted on the lead frame. Examples of semiconductor devices include various semiconductor devices used in electrical products (e.g., computers, mobile phones, digital cameras, televisions, air conditioners, solar power generation systems, etc.) and vehicles (e.g., motorcycles, cars, trains, ships, and airplanes, etc.). Among them, semiconductor devices for electric power (power semiconductor devices) are particularly preferred. [Examples] The present invention will be described in detail below with reference to Examples. However, the present invention is not limited to the following Examples. (Sample) The method for producing the sample is described. Aluminum used as a raw material has a purity of 4N (99.99% by mass or more), and the remainder is composed of unavoidable impurities. Silicon, the first group of elements (strontium, sodium, iron, phosphorus), the second group of elements (titanium, nickel, magnesium, copper), and other elements (manganese, zinc) used as alloying elements have a purity of 99.99% by mass or more, and the remainder is composed of unavoidable impurities. The aluminum alloy used for aluminum bonding wire or aluminum bonding ribbon is manufactured by charging aluminum raw materials and alloying element raw materials into an alumina crucible and melting them in a high-frequency heating furnace. The atmosphere in the furnace during melting is set to an argon atmosphere, and the maximum limit temperature of the melt during melting is set to be above 800°C and below 1050°C. The cooling method after melting is air cooling in the atmosphere or water cooling in water. A Φ6 mm cylindrical ingot is obtained by melting. After solution treatment and homogenization treatment, the ingot is subjected to wire drawing using an eye die and intermediate heat treatment to produce a Φ300 μm aluminum bonding wire. In addition, using the Φ300 μm aluminum bonding wire as the starting material, an aluminum bonding strip with a thickness of 100 μm and a width of 600 μm is produced by two-stage roller rolling. The temperature range of the solution treatment is set to be above 500°C and below 550°C, and the time is set to be above 2 hours and below 4 hours. After the solution treatment is completed, homogenization treatment is continuously performed during the cooling process. The temperature range of the homogenization treatment is set to be above 250°C and below 350°C, and the time is set to be above 2 hours and below 5 hours. The cooling method after the homogenization treatment adopts air cooling in the atmosphere. The number of intermediate heat treatments is between three and four. Regarding the wire diameter after intermediate heat treatment, the first intermediate annealing is performed at a wire diameter of 6.5 to 7.0 times the final wire diameter. The second intermediate annealing is performed at a wire diameter of 4.0 to 5.0 times the final wire diameter. The third intermediate annealing is performed at a wire diameter of 2.0 to 3.0 times the final wire diameter. When the intermediate annealing is performed four times, the wire diameter is 7.5 to 8.5 times the final wire diameter. Regarding the temperature range for the intermediate heat treatments, the first and second intermediate annealings are adjusted to a temperature of 300°C to 370°C and a time of 1 hour to 3 hours. The third and fourth intermediate annealings are adjusted to a temperature of 250°C to 400°C and a time of 2 hours to 40 hours. Commercially available lubricant is used during wire drawing. The wire reduction ratio for each eye mold during wire drawing is set to 10.0% or higher and less than 30.0%. The wire reduction ratio is adjusted based on the wire diameter of the eye mold. The final heat treatment temperature range is set to 200°C or higher and less than 350°C, and the final heat treatment time is set to 2 hours or longer and less than 20 hours. The final heat treatment temperature (Tc) is selected within a temperature range 50-100°C lower than the temperature (Tm) of the third or fourth intermediate annealing process described above. In some embodiments, an eye mold with an eye mold angle of greater than 14° and less than 18° is used for wire drawing processing. (Method for Determining Element Content) The concentration of elements contained in the aluminum bonding wire or aluminum bonding ribbon is analyzed using an ICP-OES (Inductively Coupled Plasma-Optical Emission Spectrometer) ("PS3520UVDDII" manufactured by Hitachi High-Tech Science Co., Ltd.) or an ICP-MS (Inductively Coupled Plasma-Mass Spectrometer) ("Agilent 7700x ICP-MS" manufactured by Agilent Technologies Co., Ltd.) as an analytical device. (Method for measuring the orientation ratio of the crystal orientation of the aluminum phase and the silicon phase) The L-section (a section in the center axis direction including the center axis) of the aluminum bonding wire or the aluminum bonding ribbon is used as the inspection surface to measure the crystal orientation of the aluminum phase and the silicon phase. The measurements were performed using a FE-SEM (SU-70, manufactured by Hitachi High-Technologies Corporation) and TSL Solutions' APEX (for data acquisition), OIM Data Collection (for Chi Scan), and OIM Anaysis (for data analysis). Three measurement areas were randomly selected at intervals of at least 50 cm relative to the central axis of the aluminum bonding wire or ribbon, and measurements were performed on these three areas. The measurement area was defined as being at least 300 μm and less than 800 μm in the direction of the central axis of the aluminum bonding wire or ribbon, and encompassing the entire aluminum bonding wire or ribbon perpendicular to the central axis. The key conditions for EDS and EBSD measurements were an acceleration voltage of 15 kV, a measurement magnification of 350x, a scanning speed of 30 to 120 points / second, and a measurement interval of 0.1 to 0.3 μm. While faster scanning speeds can shorten measurement time, there is a concern that EDS measurement accuracy may be reduced. Ideally, a scanning speed within the above range should be selected. -Crystal Orientation of Aluminum Phase- In the measurement of the orientation ratio of the crystal orientation of the aluminum phase in the L-section of an aluminum bonding wire or an aluminum bonding ribbon, the following method is used, namely, using an SEM-EDS-EBSD device and combining the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. More specifically, the measurement is performed in the following sequence of steps (1) to (3). (1) In the measurement area using the L-section of the aluminum bonding wire or the aluminum bonding ribbon as the inspection surface, the concentrations of aluminum and silicon are measured using EDS and the crystal orientation is measured using EBSD simultaneously. (2) Aluminum and silicon are separated and extracted using the Chi Scan function of the EBSD analysis software. Specifically, based on the measurement results of the EDS of silicon, a tolerance equivalent to the threshold value of silicon is set to separate and identify aluminum and silicon. The crystal information of aluminum and silicon in the material file is used for analyzing the crystal orientation. Here, the tolerance condition is mainly set to 30% and adjusted as needed. (3) For the area specifically containing the aluminum phase, the crystal orientation is analyzed and the orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction is calculated. As the crystal orientation to be investigated, at least three representative crystal orientations of aluminum metal, <111>, <110>, and <100>, are selected, as well as a crystal orientation with a higher ratio as needed. Here, the partial ratio is used for the orientation ratio of the crystal orientation. The orientation ratio of the <100> crystal orientation of the aluminum phase in the RD direction is the average value (arithmetic mean) of the values obtained by the above steps (1) to (3) for three measurement areas. -Crystal Orientation of Silicon Phase- In the measurement of the crystal orientation ratio of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding ribbon, the following method is used, similar to the measurement of the crystal orientation ratio of the aluminum phase, that is, using a SEM-EDS-EBSD device, and combining the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. Specifically, after performing the above steps (1) and (2), the measurement is performed according to the following step (3). (3) For the region specifically containing the silicon phase, the crystal orientation is analyzed, and the orientation ratio of the <100> crystal orientation and the orientation ratio of the <111> crystal orientation of the silicon phase in the ND direction are calculated. Regarding the orientation ratio of the crystal orientation, the partial ratio (Partial Ratio) is used. The orientation ratio of the <100> crystal orientation and the orientation ratio of the <111> crystal orientation of the silicon phase in the ND direction are the average values (arithmetic mean) of the values obtained by the above steps (1) to (3) for the three measurement areas. (Small diameter ratio of silicon phase [Ns / Nc×100(%)]) In the measurement of the small diameter ratio [Ns / Nc×100(%)] of the silicon phase in the L cross section, the following method is used, similar to the measurement of the orientation ratio of the crystal orientation of the aluminum phase, that is, using a SEM-EDS-EBSD device, and combining the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. In detail, after implementing the above steps (1) and (2), the measurement is carried out according to the following step (3). (3) For the region specifically identified as the silicon phase, the crystal orientation is analyzed. If the orientation difference between the measurement points is 15° or more, it is judged to be a grain boundary and the equivalent circle diameter of each grain is calculated. The number of grains identified as the silicon phase is totaled to calculate the total number of silicon phase particles Nc. Here, the analysis targets silicon phases with an equivalent circle diameter of 0.5 μm or greater. Considering the analytical accuracy of current EDS and EBSD analysis equipment, fine phases less than 0.5 μm are excluded. Next, the number Ns of silicon phases with an equivalent circle diameter between 0.5 μm and 0.8 μm is totaled. The ratio of Ns to Nc (small diameter ratio of the silicon phase) is then calculated [Ns / Nc × 100%). The minor diameter ratio of the silicon phase is calculated as the average value (arithmetic mean) of the values obtained by the above steps (1) to (3) for the three measurement areas. (Method for measuring the average diameter of the silicon phase) In the measurement of the average diameter of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding ribbon, the following method is used, similar to the measurement of the crystal orientation of the aluminum phase, that is, using a SEM-EDS-EBSD device, and combining the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. In detail, after implementing the above steps (1) and (2), the measurement is carried out according to the following step (3). (3) For the region specifically identified as the silicon phase, the crystal orientation is analyzed. If the orientation difference between the measurement points is 15° or more, it is judged to be a grain boundary and the equivalent circle diameter of each grain is calculated. Then, the equivalent circle diameter of each grain is averaged to calculate the average diameter of the silicon phase. Here, for the average calculation, the average value obtained by area average (area weighted average) is used. Furthermore, when calculating the average diameter of the silicon phase in the L-section, only silicon phases having a diameter (equivalent circle diameter) of 0.5 μm or more were considered. The average diameter of the silicon phase is the average value (arithmetic mean) of the values obtained by the above steps (1) to (3) for three measurement areas. (Method for measuring the shape of the silicon phase) In the measurement of the shape ratio (e / f) of the silicon phase in the L-section of the aluminum bonding wire or aluminum bonding ribbon, the following method is used, similar to the measurement of the orientation ratio of the crystal orientation of the aluminum phase, that is, using a SEM-EDS-EBSD device, and combining the information on the aluminum concentration and silicon concentration obtained by SEM-EDS with the information on the crystal orientation obtained by EBSD. Specifically, after performing the above steps (1) and (2), the measurement is performed according to the following step (3). (3) For the region specifically identified as the silicon phase, the crystal orientation is analyzed. If the orientation difference between the measurement points is 15° or more, it is determined to be a grain boundary and the shape ratio (e / f) of each grain is calculated. Then, the shape ratio (e / f) of each grain is averaged to calculate the average value of the shape ratio (e / f) of the silicon phase. The average value of the silicon phase aspect ratio (e / f) is calculated using the Grain Shape Aspect Ratio value ("grain shape aspect ratio") from the analysis software. The grain shape aspect ratio is calculated automatically by the software as the ratio (e / f) of the short side length (e) (Grain Shape Minor Axis) to the long side length (f) (Grain Shape Major Axis) of a single grain. The average calculation uses the area average (area-weighted average). The aspect ratio (e / f) of the silicon phase is calculated as the average value (arithmetic mean) of the values obtained by the above steps (1) to (3) for the three measurement areas. (Evaluation method for aluminum bonding wire or aluminum bonding tape) The following describes the evaluation method for aluminum bonding wire. The aluminum bonding wire used for evaluation has a wire diameter of 300 μm. A silicon wafer is used as the semiconductor wafer, and an aluminum-0.5% copper alloy having a thickness of 4 μm is used as the electrode on the semiconductor wafer. A 5 μm nickel film is formed on an aluminum alloy as the substrate. The aluminum bonding wire is bonded using a commercially available wire bonder (manufactured by Ultrasonic Industries), with both the first bond (bonding to the electrodes on the semiconductor wafer) and the second bond (bonding to the substrate) being wedge-type bonds. The aluminum bonding tape is bonded using the Hesse BJ955 fully automatic bonder equipped with a tape bonding head. (Evaluation method for high-speed temperature cycle reliability) A commercially available high-speed thermal shock tester is used in the high-speed temperature cycle test (high-speed TCT). In the high-speed TCT, hot air is blown onto the sample to perform rapid heating. The sample for the high-speed TCT adopts a structure in which a semiconductor chip is mounted on a substrate, and the electrodes on the semiconductor chip and the electrodes on the substrate are connected by aluminum bonding wires or aluminum bonding tapes. For the sample placed in the sample chamber of the high-speed thermal shock tester, a heat load is repeatedly applied with heating and cooling as one cycle. The minimum temperature during cooling is set to -50°C, and the maximum temperature during heating is set to 175°C. The heating time including the heating time is set to 20 seconds, and the cooling time including the cooling time is set to 40 seconds. After the test starts, the sample is taken out after 20,000 cycles, and a shear strength test of the first joint is performed. The value of the shear strength (shear strength) of the first joint used to evaluate the high-speed temperature cycle reliability is the average value of the shear strength of 10 randomly selected first joints. The ratio (percentage) of the average shear strength after high-speed TCT to the average shear strength before the test is defined as the strength maintenance rate. The higher the strength maintenance rate, the better the reliability of the joint. If the strength maintenance rate is 85% or more, it is judged as excellent and indicated by "3", if it is 75% or more and less than 85%, it is judged as excellent and indicated by "2", if it is 70% or more and less than 75%, it is judged as requiring improvement and indicated by "1", and if it is less than 70%, practical problems arise and indicated by "0". "3" and "2" are judged as qualified, and "1" and "0" are judged as unqualified. The evaluation results are recorded in the "High-speed temperature cycle reliability" column in the table. The requirement for high-speed temperature cycle reliability in next-generation silicon carbide semiconductors is equivalent to 20,000 cycles. (Method for Evaluating Bond Strength Variation in High-Speed Temperature Cycle Testing) In the aforementioned high-speed TCT, after 20,000 cycles, the shear strength of the first bond was measured at 20 locations. To evaluate the bond strength variation in the high-speed TCT, the unbiased standard deviation (σ) of the shear strength was calculated. The unbiased standard deviation of the shear strength of the first bond is largely unaffected by the conditions of the first bond and can therefore be used as an indicator for appropriately evaluating the properties of aluminum bonding wire or aluminum bonding ribbon. If σ is less than 30 gf, the variation in joint strength is extremely small, and the stability is judged to be excellent and evaluated as "3". If σ is 30 gf or more and less than 50 gf, the variation in joint strength is small and the stability is judged to be excellent and evaluated as "2". If σ is 50 gf or more and less than 70 gf, the variation in joint strength is within the allowable range and the stability is judged to be good and evaluated as "1". If σ is 70 gf or more, the variation in joint strength is large and is judged to be practically problematic and recorded as "0". The evaluation results are recorded in the "High-Speed TCT Joint Strength Variation" column in the table. (Evaluation method of the first bonding strength) The evaluation method of the first bonding strength is described. The first bonding strength is evaluated by a shear strength test. 10 first bonds are performed under bonding conditions suitable for the reliability test, and the shear strength of the first bonding portion is measured. Under the bonding conditions, the ultrasonic output is set slightly higher to ensure the bonding area. In the shear strength measurement, a commercially available micro shear strength tester (4000-PLUS manufactured by Nordson) is used. The shear speed is set to 200 μm / second, and the height of the shear tool is set to 10 μm from the electrode surface. The shear strength is measured by fixing the substrate bonded with an aluminum bonding wire or an aluminum bonding tape using a jig. If the average shear strength of the ten first joints is 1500 gf or greater, it is considered excellent and rated "3." If it is 1300 gf or greater but less than 1500 gf, it is considered practically sound and rated "2." If it is 1000 gf or greater but less than 1300 gf, it is considered necessary for improvement and rated "1." If it is less than 1000 gf, it is considered practically problematic and rated "0." The evaluation results are recorded in the "First Joint Strength" column of the table. (Evaluation Method for Wire Breakage During Processing) The evaluation method for wire breakage during processing is described below. Wire drawing was performed with wire diameters ranging from 6 mmφ to 0.3 mmφ, and the number of wire breakages was determined. Wire drawing conditions, such as feed speed and area reduction ratio, were selected from the conditions described above, and appropriate manufacturing conditions were adjusted and varied for each wire. The length of the drawn aluminum bonding wire ranged from 100 to 200 m, and the number of wire breakages was calculated per 100 m. A zero breakage was considered good and scored "3." A single breakage was considered manageable by improving manufacturing conditions and scored "2." A breakage of 2 to 4 times indicated a decrease in productivity and was scored "1." A breakage of 5 or more times was considered impractical and scored "0." The evaluation results are recorded in the "Wire Breakage During Processing" column of the table. (Evaluation method for surface damage and scratches) Regarding the surface properties of aluminum bonding wires or aluminum bonding tapes, evaluation is performed focusing on damage and scratches. The wire diameter of the aluminum bonding wire is set to Φ300 μm. The aluminum bonding tape is set to have a thickness of 100 μm and a width of 600 μm. Three measurement areas are randomly selected at intervals of more than 1 m relative to the central axis direction of the aluminum bonding wire or aluminum bonding tape, and three samples with a length of approximately 2 cm are collected at each of the three locations, and a total of nine samples are observed. Specifically, an SEM is used to observe the surface at a magnification range of 50 to 500 times. Damage of more than 50 μm in length and scratches of more than 30 μm in length are judged as defective. The number of scratches and abrasions was counted. If there were no scratches or abrasions, the surface was judged to be good and acceptable, and the evaluation was "3." If there were one or more but two or fewer scratches, the surface was judged to be practically acceptable, and the evaluation was "2." If there were three to seven scratches or abrasions, the surface was judged to be poor, and the evaluation was "1." If there were eight or more scratches or abrasions, the surface was judged to be practically unacceptable, and the evaluation was "0." The evaluation results are recorded in the "Surface Properties" column of the table. The evaluation results of the examples and comparative examples are shown in Tables 1 to 4. Examples 1 to 44 and Comparative Examples 1 to 10 in Tables 1 to 3 are the results for aluminum bonding wires, and Examples B1 to B3 and Comparative Example B1 in Table 4 are the results for aluminum bonding tapes. [Table 1] (Table 1) [Table 2] (Table 2) [Table 3] (Table 3) [Table 4] (Table 4) 1: Aluminum bonding wire 2: Aluminum bonding strip 3: Aluminum bonding wire or aluminum bonding strip 10: Central axis 11: L-section 20: Central axis 21: L-section 31: Silicon phase 32: Central axis direction of the aluminum bonding wire or aluminum bonding strip e: Short side length of the silicon phase f: Long side length of the silicon phase ND: Direction perpendicular to the central axis RD: Direction parallel to the central axis W: Width T: Thickness Figure 1 is a schematic diagram illustrating the measurement target surface (inspection surface), RD direction, and ND direction when measuring the crystal orientation of the aluminum and silicon phases, the minor diameter ratio of the silicon phase, and the shape of the silicon phase in an aluminum bonding wire. The measurement target surface is a cross-section (L cross-section) of the aluminum bonding wire in the direction of the central axis, including the central axis. Figure 2 is a schematic diagram illustrating the measurement target surface (inspection surface), RD direction, and ND direction when measuring the crystal orientation of the aluminum and silicon phases, the minor diameter ratio of the silicon phase, and the shape of the silicon phase in an aluminum bonding ribbon. The measurement target surface is a cross-section (L cross-section) of the aluminum bonding ribbon in the direction of the central axis, including the central axis. Figure 3 is a schematic diagram illustrating the short side length (e) and long side length (f) of the silicon phase in the L cross-section. Figure 4 is an example of a graph showing the number distribution of equivalent circular diameters of the silicon phase in the L cross-section. 1: Aluminum bonding wire 10: Center axis 11: L section ND: Vertical direction of the central axis RD: Direction parallel to the central axis
Claims
1. An aluminum connector, comprising an aluminum bonding wire or aluminum bonding strip, containing 3.0% by mass and 20.0% by mass of silicon, wherein when measuring the crystal orientation of the aluminum phase in the L-section (a section including the central axis direction) of the aluminum bonding wire or aluminum bonding strip, the orientation ratio of <100> crystal orientations with an angle difference of 15° or less relative to the direction parallel to the central axis (RD direction) is 15% to 50%, and when the number of silicon phases with an equivalent circle diameter of 0.5 μm or more and 0.8 μm or less in the L-section is defined as Ns, and the number of silicon phases with an equivalent circle diameter of 0.5 μm or more in the L-section is defined as Nc, the ratio of Ns to Nc [Ns / Nc×100(%)] is 30% to 95%.
2. The aluminum connector as requested in item 1, wherein the ratio of Ns to Nc [Ns / Nc×100(%)] is 40% or more.
3. For the aluminum connector of claim 1, when measuring the crystal orientation of the silicon phase in the L section, the total ratio of the orientation of the <100> crystal orientation and the <111> crystal orientation with an angle difference of less than 15° relative to the direction perpendicular to the central axis (ND direction) is more than 20% and less than 60%.
4. For the aluminum connector as requested in item 1, the average value of the ratio (e / f) of the short side length e to the long side length f of the silicon phase in section L is 0.20 or more and 0.70 or less.
5. The aluminum connector material as claimed in claim 1 further contains strontium, sodium, iron, or phosphorus in aggregate amounts of 10 ppm to 800 ppm.
6. The aluminum connector material as claimed in claim 1 further contains one or more of titanium, nickel, magnesium, and copper in aggregates of 100 ppm to 2000 ppm.
7. The aluminum connector material as claimed in claim 5 further contains one or more of titanium, nickel, magnesium, and copper in aggregates of 100 ppm to 2000 ppm.
8. The aluminum connector as requested in any of items 1 to 7, wherein the total concentration of elements other than aluminum, silicon, strontium, sodium, iron, phosphorus, titanium, nickel, magnesium and copper in the aluminum connector is less than 0.5% by mass.
9. For any of the aluminum connectors requested in items 1 to 7, the orientation ratio of the crystal orientation, the equivalent circle diameter of the silicon phase, and the number thereof are values measured using a SEM-EDS-EBSD device.
10. For the aluminum connectors of claim 4, the average value of the ratio (e / f) of the short side length e to the long side length f of the silicon phase is a value measured using a SEM-EDS-EBSD device.
11. The aluminum connector as claimed in any of claims 1 to 7, used in a semiconductor device.
12. A semiconductor device comprising an aluminum connector as claimed in any one of claims 1 to 11.
Citation Information
Patent Citations
Bonding structure, semiconductor package and semiconductor device
CN111316425A
Aluminium alloy wire for bonding applications
TW201425596A
Al bonding wire for semiconductor devices
WO2022168787A1