Manufacturing method of semiconductor chip

TWI945618BActive Publication Date: 2026-11-11廖富江
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
TW113146133
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-11-28
Publication Date
2026-11-11
Estimated Expiration
2044-11-27

AI Technical Summary

Technical Problem

Current semiconductor chip packaging materials lack effective heat dissipation properties, leading to decreased efficiency and increased manufacturing time and cost, while new processes to improve heat dissipation often enlarge the chip's size and thickness.

Method used

A semiconductor wafer fabrication method involving deposition of a metal thin film on the non-active surface and sides of the wafer, followed by attaching the active surface to a solder paste pattern on a printed circuit board and reflowing to enhance heat dissipation, while reducing manufacturing steps and costs.

Benefits of technology

Improves heat dissipation efficiency, reduces chip size and thickness, and decreases production costs by eliminating pre-packaging, suitable for chips in area-constrained products like smartphones and tablets.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure TWG2TB001920363_001
    Figure TWG2TB001920363_001
  • Figure TWG2TB001920363_002
    Figure TWG2TB001920363_002
  • Figure TWG2TB001920363_003
    Figure TWG2TB001920363_003
Patent Text Reader

Abstract

This invention provides a method for manufacturing a semiconductor wafer, comprising the following steps: providing a wafer having an active surface, a non-active surface, and four side surfaces, the active surface being opposite to the non-active surface, and the four side surfaces connecting the active surface and the non-active surface, wherein a metal thin film is provided on the non-active surface and the four side surfaces; applying solder paste to a printed circuit board to form a solder paste pattern, and the solder paste pattern defining a bonding area on the printed circuit board; attaching the active surface of the wafer to the bonding area; and reflowing the printed circuit board to which the wafer is attached.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductors, and in particular to a method for manufacturing semiconductor wafers. Prior Technology

[0002] With the advancement of chip technology, chips (e.g., power chips) can operate at higher voltages or higher current densities, which in turn leads to higher temperatures during operation. If heat dissipation is not effective, the chip's efficiency will decrease as the temperature rises, thus placing increasingly stringent requirements on chip heat dissipation.

[0003] However, current technologies involve first packaging the chip and then mounting it onto a printed circuit board (PCB) using surface mount technology (SMT). However, common packaging materials are mostly polymers and lack good heat dissipation properties, which limits the chip's heat dissipation efficiency during operation. Currently, many technologies employ new processes or structures to improve chip heat dissipation efficiency during operation; however, these new processes or structures significantly increase manufacturing time and costs, and may even increase the chip's size and thickness.

[0004] Therefore, it is necessary to provide a semiconductor wafer fabrication method to solve the problems existing in conventional technologies. Summary of the Invention

[0005] The purpose of this invention is to provide a semiconductor wafer manufacturing method that can increase the heat dissipation efficiency of the wafer, reduce the number of wafer manufacturing steps, and lower the wafer production cost.

[0006] To achieve the above objectives, the present invention provides a semiconductor wafer fabrication method comprising the following steps: providing a wafer having an active surface, a non-active surface, and four side surfaces, the active surface being opposite to the non-active surface, and the four side surfaces connecting the active surface and the non-active surface, wherein a metal thin film is provided on the non-active surface and the four side surfaces; applying solder paste to a printed circuit board to form a solder paste pattern, and the solder paste pattern defining a bonding area on the printed circuit board; attaching the active surface of the wafer to the bonding area; and reflowing the printed circuit board to which the wafer is attached.

[0007] In one embodiment of the present invention, the metal thin film comprises titanium, nickel, silver, tin, aluminum, copper, platinum, chromium, gold, cobalt and molybdenum.

[0008] In one embodiment of the present invention, providing the wafer includes: attaching a back protective film to a back side of a wafer; cutting the wafer from a front side along a plurality of dicing paths to separate the wafers on the wafer; attaching a front protective film to a front side of the wafer; removing the back protective film; grinding the wafer from the back side of the wafer to reduce a thickness of the wafer; and performing a metal deposition process on the back side of the wafer to form the metal thin film on the non-active surface and the four side surfaces of the wafer, respectively.

[0009] In one embodiment of the present invention, applying solder paste to the printed circuit board to form the solder paste pattern, and the solder paste pattern defining the bonding area on the printed circuit board includes: placing a printed stencil on the printed circuit board; applying the solder paste along the printed stencil; and removing the printed stencil such that the solder paste defines the bonding area.

[0010] In one embodiment of the present invention, attaching the active surface of the wafer to the bonding region further includes: disposing a bottom filler layer between the active surface and the bonding region.

[0011] In one embodiment of the present invention, the chip is a power chip.

[0012] In one embodiment of the invention, the solder paste thickness of the solder paste pattern is 50,000 angstroms (A).

[0013] As described above, this invention involves depositing metal thin films on the non-active side and all four sides of a chip, and attaching the active side of the chip to a bonding area defined by a solder paste pattern on a printed circuit board (PCB). The PCB with the chip attached is then reflowed. During the reflow process, solder paste adheres to the metal thin films on the non-active side and all four sides of the chip. The large area of ​​the metal thin films effectively improves the chip's heat dissipation efficiency. Furthermore, this invention eliminates the need for pre-packaging the chip, reducing manufacturing steps and production costs, and also decreasing the chip's size and thickness. Therefore, this invention can be used to produce chips for products with area requirements or portable devices with strict space constraints (e.g., smartphones or tablets). Simple Explanation of the Diagram

[0014] Figure 1 is a flowchart of one step of a semiconductor wafer fabrication method according to an embodiment of the present invention. Figure 2 is a flowchart of a detailed step in an embodiment of the present invention. Figure 3 is a flowchart of a detailed step in an embodiment of the present invention. Figures 4a to 4d are application diagrams of embodiments of the present invention. Implementation

[0015] To make the above and other objects, features and advantages of the present invention more apparent and understandable, preferred embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0016] Please now refer to Figures 1 through 3. Figure 1 is a flowchart of one step of a semiconductor wafer fabrication method according to an embodiment of the present invention. Figure 2 is a flowchart of a detailed step in an embodiment of the present invention. Figure 3 is a flowchart of a detailed step in an embodiment of the present invention. This embodiment provides a semiconductor wafer fabrication method 100, which includes the following steps:

[0017] Step S110: A wafer is provided, the wafer having an active surface, a non-active surface, and four side surfaces. The active surface is opposite to the non-active surface, and the four side surfaces connect the active surface and the non-active surface. A metal thin film is provided on both the non-active surface and the four side surfaces. Specifically, step S110 may include: step S111, attaching a back protective film to a back surface of a wafer; step S112, cutting the wafer along a plurality of dicing paths on a front surface of the wafer to separate the wafers on the wafer; step S113, attaching a front protective film to a front surface of the wafer; step S114, removing the back protective film; step S115, grinding the wafer from the back surface to reduce its thickness; and step S116, performing a metal deposition process on the back surface of the wafer to form the metal thin film on both the non-active surface and the four side surfaces of the wafer. The metal thin film may contain a conductive metal. The metal thin film can contain one or more metals such as titanium, nickel, silver, tin, aluminum, copper, platinum, chromium, gold, cobalt, and molybdenum. For example, the metal thin film may contain titanium, nickel, silver, and tin. It should be noted that the composition of the metal thin film can be adjusted according to the chip's function or usage requirements. Forming the metal thin film on the five surfaces of the chip, including the non-active surface and the four side surfaces, can also shield electromagnetic waves, thereby preventing external electromagnetic interference with the chip's operation. It should be noted that the metal thin film can be formed on the non-active surface and the four side surfaces through deposition, sputtering, or other feasible process methods. It should be noted that the metal thickness can be adjusted according to different requirements. In some embodiments, the chip can be a power chip, a diode, or an insulated-gate bipolar transistor (IGBT). It should be understood that the chip can also be a chip with high heat dissipation requirements, such as a central processing unit (CPU), a graphics processing unit (GPU), or other chips with high-speed computing capabilities.

[0018] Step S120 involves applying solder paste to a printed circuit board to form a solder paste pattern, and the solder paste pattern defining a bonding area on the printed circuit board. Specifically, step S120 may include: step S121, placing a printed stencil on the printed circuit board; step S122, applying the solder paste along the printed stencil; and step S123, removing the printed stencil, so that the solder paste defines the bonding area. In some embodiments, the thickness of the solder paste pattern can be 50,000 angstroms (Å). It should be noted that the thickness of the solder paste pattern can also be adjusted to the required thickness as needed, for example, according to the chip function or chip specifications.

[0019] Step S130 involves attaching the active surface of the wafer to the bonding region. In some embodiments, step S130 further includes: depositing a bottom filler layer between the active surface and the bonding region. The bottom filler layer prevents the active surface from becoming conductive with the solder paste pattern.

[0020] Step S140: Reflow the printed circuit board with the chip attached. In some embodiments, the printed circuit board with the chip attached is sent to a reflow oven for reflow.

[0021] Please now refer to Figures 4a to 4d, which are application diagrams of embodiments of the present invention. In the application scenarios shown in Figures 4a to 4d, a wafer 10 is first provided, wherein the wafer 10 has an active surface 11, a non-active surface 12, and four side surfaces 13. The active surface 11 is opposite to the non-active surface 12, and the four side surfaces 13 are respectively connected to the active surface 11 and the non-active surface 12. In some examples, the active surface 11 may be provided with a source 11a and a gate 11b, and the non-active surface 12 may be provided with a drain, wherein the drain is not shown. A metal thin film 14 is provided on the non-active surface 12 and the four side surfaces 13, as shown in Figure 4a. Solder paste is applied to a printed circuit board 20 to form a solder paste pattern 30, and the solder paste pattern 30 defines a bonding region A on the printed circuit board 20, as shown in Figure 4b. The active surface 11 of the wafer 10 is attached to the bonding area A of the printed circuit board 20, as shown in Figure 4c. Specifically, the active surface 11 of the wafer 10 is attached to the bonding area A surrounded by the solder paste pattern 30. It should be noted that the active surface 11 may be provided with metal contacts (e.g., by deposition or sputtering), which facilitates the electrical connection of the wafer 10 to the printed circuit board 20. In addition, the active surface 11 facing the printed circuit board 20 and being directly electrically connected to the printed circuit board 20 can reduce the electrical connection distance, thereby reducing the resistance (also known as internal resistance) of the connection between the wafer 10 and the printed circuit board 20, and such an electrical connection method also helps to increase heat dissipation. After the chip 10 is attached to the printed circuit board 20, the printed circuit board 20 with the chip 10 attached is sent to a reflow oven, for example, at 230 °C to 260 °C. During the reflow, the solder paste pattern 30 liquefies and attaches to the non-active surface 12 and the metal film 14 of the four side surfaces 13 of the chip 10. It should be noted that the reflow temperature can be adjusted as needed.

[0022] As described above, this invention involves depositing a metal thin film (such as a titanium-nickel-silver-tin film) on the non-active side and all four sides of the chip, and attaching the active side of the chip to the bonding area defined by the solder paste pattern on a printed circuit board. The printed circuit board with the chip attached is then reflowed. During the reflow process, solder paste adheres to the metal thin film (such as a titanium-nickel-silver-tin film) on the non-active side and all four sides of the chip. The large area of ​​the metal thin film effectively improves the chip's heat dissipation efficiency. Furthermore, this invention eliminates the need for pre-packaging the chip, reducing manufacturing steps and production costs, and also reducing the chip's size and thickness. Therefore, this invention can be used to produce chips for products with area requirements or portable devices with strict space requirements (e.g., smartphones or tablets).

[0023] Although the present invention has been disclosed with reference to preferred embodiments, it is not intended to limit the invention. Any person skilled in the art may make various modifications and alterations without departing from the spirit and scope of the invention. Therefore, the scope of protection of the present invention shall be determined by the appended claims.

[0024] 10: Chips 11: Proactive Side 11a: Source 11b: Gate 12: Non-active surface 13: Side surface 14:Metal film 20: Printed Circuit Board 30: Solder paste pattern 100: Semiconductor wafer manufacturing methods S110: Steps S111: Steps S112: Steps S113: Steps S114: Steps S115: Steps S116: Steps S120: Steps S121: Steps S122: Steps S123: Steps S130: Steps S140: Steps A: Joint area

Claims

1. A method for manufacturing a semiconductor wafer, comprising the following steps: providing a wafer having an active surface, a non-active surface, and four side surfaces, the active surface being opposite to the non-active surface, the four side surfaces connecting the active surface and the non-active surface, wherein a metal thin film is provided on the non-active surface and the four side surfaces, wherein the metal thin film comprises tin; applying solder paste to a printed circuit board to form a solder paste pattern, the solder paste pattern defining a bonding region on the printed circuit board; attaching the active surface of the wafer to the bonding region surrounded by the solder paste pattern; and reflowing the printed circuit board on which the wafer is attached, such that the solder paste pattern is attached to the metal thin film on the non-active surface and the four side surfaces.

2. The semiconductor wafer fabrication method as described in claim 1, wherein the metal thin film comprises titanium, nickel, silver, aluminum, copper, platinum, chromium, gold, cobalt, and molybdenum.

3. A method for manufacturing a semiconductor wafer as described in claim 1 or 2, wherein providing the wafer comprises: attaching a back protective film to a back side of a wafer; cutting the wafer from a front side along a plurality of dicing paths to separate the wafers on the wafer; attaching a front protective film to a front side of the wafer; removing the back protective film; grinding the wafer from the back side of the wafer to reduce a thickness of the wafer; and performing a metal deposition process on the back side of the wafer to form the metal thin film on the non-active surface and the four side surfaces of the wafer.

4. The semiconductor wafer fabrication method as claimed in claim 1, wherein applying the solder paste to the printed circuit board to form the solder paste pattern, and the solder paste pattern defining the bonding area on the printed circuit board comprises: placing a stencil on the printed circuit board; applying the solder paste along the stencil; and removing the stencil such that the solder paste defines the bonding area.

5. The semiconductor wafer manufacturing method as described in claim 1, wherein attaching the active surface of the wafer to the bonding region further comprises: disposing a bottom filler layer between the active surface and the bonding region.

6. The method for manufacturing a semiconductor wafer as described in claim 1, wherein the wafer is a power wafer.

7. The semiconductor wafer fabrication method as described in claim 1, wherein the thickness of a solder paste pattern is 50,000 angstroms (Å).

Citation Information

Patent Citations

  • Integrated circuit packaging structure and packaging method thereof

    TW201041110A

  • Circuit package with internal and external shielding

    US10141268B2

  • Wafer processing method

    US20170330799A1