Enhanced deuterium migration
Patent Information
- Application Number
- TW114100882
- Authority / Receiving Office
- TW · TW
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2024-01-10
- Filing Date
- 2025-01-09
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2045-01-08
Smart Images

Figure TWG2TB001920417_001 
Figure TWG2TB001920417_002 
Figure TWG2TB001920417_003
Abstract
Description
[Technical Field]
[0001] This application claims the benefit and priority of U.S. Patent Application No. 18 / 408,666, filed on January 10, 2024, entitled “ENHANCED DEUTERIUM MIGRATION”, which is incorporated herein by reference in its entirety.
[0002] The present invention relates to semiconductor systems and processes. More specifically, the present invention relates to three-dimensional (3D) semiconductor devices, such as dynamic random-access memory (DRAM) devices (3D DRAM) and methods for forming such devices. [Previous Technology]
[0003] Integrated circuits can be fabricated through processes that create complex patterned material layers on the surface of a substrate. Creating patterned material on a substrate requires controlled methods for forming and removing exposed material. Material properties can affect how components operate and may also affect how films are removed relative to each other. Reducing the size of integrated circuits (ICs) leads to improved performance, increased capacity, and / or lower costs. Each reduction in size requires more sophisticated techniques to form the IC. Reducing transistor size (for example) allows for the integration of an increased number of memory or logic elements onto a chip, thereby creating products with increased capacity. However, pursuing greater capacity than ever before is not without its challenges. The need to optimize the performance of each component becomes increasingly important. For example, as component sizes continue to shrink, film modification and passivation become increasingly difficult.
[0004] Therefore, there is a need for improved systems and methods for producing high-quality components and structures. The present invention addresses these and other needs. [Summary of the Invention]
[0005] The present invention is generally directed to systems and methods for semiconductor processing (such as modifying target regions of substrates). The methods include flowing deuterium-containing precursors and silicon-containing precursors into a processing region of a processing chamber. The methods include contacting a semiconductor element disposed in the processing region with the deuterium-containing precursors and silicon-containing precursors. The methods include forming a deuterium-containing dielectric film on or over the semiconductor element at a processing temperature greater than or about 350°C. The methods include passivating the target region by deuterium from the deuterium-containing dielectric film. The methods include wherein the deuterium-containing dielectric film is spaced apart from or adjacent to the target region.
[0006] In embodiments, the deuterium-containing precursor includes one or more of D₂, D₂O, DH (deuterium hydrogen), or HDO (deuterium hydroxide). In more embodiments, the deuterium-containing precursor and the silicon-containing precursor are flowed using a plasma process, wherein the plasma further includes one or more of argon (Ar), helium (He), hydrogen (H₂), nitrogen (N₂), oxygen (O₂), ammonia (NH₃), or nitrogen fluoride (NF₃). Additionally, in the embodiments, the silicon-containing precursor includes one or more of silane (SiH₄), disilane (Si₂H₆), silicon tetrachloride (SiCl₄), trichlorosilane (SiHCl₃), dichlorosilane (SiH₂Cl₂), hexachlorodisilane (Si₂Cl₆), silicon tetrafluoride (SiF₄), silicon tetrabromide (SiBr₄), tetraethyl orthosilicate (TEOS), tris(dimethylamino)silane (TDMAS), bis(tert-butylamino)silane (BTBAS), bis(diethylamino)silane (BDEAS), or combinations thereof. In the embodiments, the deuterium-containing dielectric film is formed on or on the semiconductor device at a processing temperature greater than or about 400°C. Alternatively or concurrently, the deuterium-containing dielectric film is formed at a ratio of deuterium-containing precursor to silicon-containing precursor greater than or about 0.9:1. In a further embodiment, the ratio of deuterium-containing precursor to silicon-containing precursor is greater than or about 1.5:1. In a further embodiment, the ratio of deuterium-containing precursor to silicon-containing precursor is greater than or about 4:1. Embodiments include a deuterium-containing dielectric film containing from about 0.1 wt% to about 1 wt% deuterium based on the weight of the deuterium-containing dielectric film. In an embodiment, the target region includes a channel-gate interface. Furthermore, in an embodiment, the deuterium-containing dielectric film includes an interlayer dielectric. In a further embodiment, the plasma includes a high-frequency plasma having a plasma power greater than or about 800 watts.
[0007] The present invention is also generally directed to semiconductor processing methods. The methods include forming a semiconductor element having one or more transistors and one or more capacitors on top of the transistors in a processing region of a processing chamber. The methods include flowing a deuterium-containing precursor and a silicon-containing precursor into the processing region of the processing chamber. The methods include contacting the semiconductor element disposed in the processing region with the deuterium-containing precursor and the silicon-containing precursor. The methods include forming a deuterium-containing dielectric film on or on the semiconductor element at a processing temperature greater than or about 350°C. The methods include passivating a target region of the semiconductor element by deuterium from the deuterium-containing dielectric film. The methods include wherein the deuterium-containing dielectric film is spaced apart from or adjacent to the target region.
[0008] In embodiments, the semiconductor element includes a three-dimensional (3D) semiconductor element. In more embodiments, the three-dimensional element includes a three-dimensional dynamic random access (3D DRAM) element. Additionally, in embodiments, the target region includes a channel-gate interface, and the deuterium-containing dielectric film includes an interlayer dielectric. Alternatively or additionally, in embodiments, the silicon-containing precursor includes tetraethyl orthosilicate, and the deuterium-containing dielectric film is formed at a ratio of deuterium-containing precursor to silicon-containing precursor greater than or about 0.9:1. In embodiments, the deuterium-containing precursor and the silicon-containing precursor are flowed using a plasma process, wherein the plasma includes a high-frequency plasma having a plasma power greater than or about 800 watts.
[0009] The present invention also generally relates to a method for forming a three-dimensional dynamic random access memory (3D DRAM) device. The method includes forming a semiconductor structure comprising one or more transistors and one or more capacitors on top of the transistors in a processing region of a processing chamber, wherein the transistors contain channels and gates. The method includes flowing a deuterium-containing precursor and a silicon-containing precursor into the processing region of the processing chamber. The method includes contacting the semiconductor structure disposed in the processing region with the deuterium-containing precursor and the silicon-containing precursor. The method includes forming a deuterium-containing dielectric film on or on the semiconductor structure at a processing temperature greater than or about 350°C. The method includes using the deuterium-containing dielectric film to passivate the channel-gate interface region of the semiconductor structure. In embodiments, the deuterium-containing dielectric film is an interlayer dielectric covering one or more transistors and / or one or more capacitors.
[0010] In embodiments, this technique can provide numerous advantages over known systems and methods for forming 3D devices, such as 3D DRAM devices. For example, by forming devices as discussed herein, increased migration of one or more dopants to the target region can be achieved without increasing the overall dopant concentration. Therefore, the devices and methods discussed herein can increase retention time and thus increase device reliability. Embodiments of the invention, along with its many advantages and features, are described in more detail below in conjunction with the accompanying drawings.
Implementation Method
[0019] Three-dimensional structures (such as dynamic random access memory (DRAM) devices, including horizontal and / or vertical channel devices) involve fabricating a transistor, a capacitor, and three contacts: each contact is connected to a bit line, a word line, and a reference voltage. There is ongoing pressure to reduce the size of individual cells and increase the density of memory cells to allow more memory to be squeezed onto a single memory chip. Limitations on cell size reduction include both active and passive word lines passing through the cell, the size of the cell capacitor, and the compatibility between arrayed and non-arrayed devices. As devices scale, charge carriers experience a larger electric field, resulting in defects at the channel / gate interface and reduced drain current. In addition, device scaling can also cause a phenomenon called "oxide charge," which occurs when silicon-hydrogen bonds at the channel-gate interface break due to frequent and high-energy charge-discharge cycles. This oxide charge can form dangling silicon bonds, which can form interface trap regions, further reducing drain current across the gate / channel interface.
[0020] Attempts have been made to reduce such defects by passivating the channel before gate formation. However, such passivation leads to overdoping, resulting in channels with threshold voltages that are unsuitably high for device operation. Efforts have also been made to dope adjacent materials, such as dielectric materials, and to diffuse the dopant into the target region. Such attempts have resulted in unacceptably high dopant contents in adjacent materials and poor passivation at the channel-gate interface, as the dopant cannot effectively migrate to the target region even at high doping contents.
[0021] Surprisingly, the present invention has discovered that by carefully controlling the formation of adjacent dielectric materials (such as interlayer dielectrics), films with increased density and / or reduced defects can be formed. The resulting films with increased density and / or reduced defects provide highly efficient migration of dopants to target regions. Specifically, the present invention has discovered that by controlling deposition conditions, oxide films (such as interlayer dielectrics) can be formed that provide excellent permeability to dopant materials. Furthermore, at least in part due to the efficient permeability of the dopant, the present invention can provide a target doping concentration that allows for excellent passivation of the gate-channel interface while exhibiting virtually no reduction in threshold voltage, such as virtually no increase in instability at negative bias temperature.
[0022] After describing a general configuration of a chamber (in which plasma processing may be performed) configured to perform operations according to embodiments of the invention, specific methods and component configurations may be discussed. It will be understood that the invention is not intended to be limited to the specific films and processes discussed, as the described techniques can be used to improve many film formation processes and are applicable to various semiconductor processing chambers and operations.
[0023] Figure 1A shows a top plan view of one embodiment of a processing system 10 with deposition, processing, etching, baking, and curing chambers according to an embodiment. In this figure, a pair of front-opening wafer transfer cassettes 12 supply substrates of various sizes, which are received by a robotic arm 14 and placed in a low-pressure holding region 16 before being placed into one of the semiconductor processing chambers 18a to 18f (located in cascaded sections 19a to 19c). A second robotic arm 11 can be used to transport the substrate wafers from the holding region 16 to the semiconductor processing chambers 18a to 18f and back. Each semiconductor processing chamber 18a to 18f can be equipped to perform a variety of substrate processing operations, including plasma-enhanced chemical vapor deposition, atomic layer deposition, physical vapor deposition, etching, pre-cleaning, degassing, orientation, and other substrate processes (including plasma treatment, annealing, ashing, etc.), as well as stacking to form the semiconductor materials described herein.
[0024] Semiconductor processing chambers 18a to 18f may include one or more system components for depositing, plasma processing, curing, and / or etching dielectric or other films on a substrate. In one configuration, two pairs of semiconductor processing chambers (e.g., 18c to 18d and 18e to 18f) may be used to deposit dielectric material on the substrate, and a third pair of semiconductor processing chambers (e.g., 18a to 18b) may be used to process the deposited dielectric. In another configuration, all three pairs of chambers (e.g., 18a to 18f) may be configured to deposit and process stacks of alternating dielectric films on the substrate. Any one or more of these processes may be performed in chambers separate from the manufacturing systems shown in the different embodiments. It will be understood that system 10 is contemplated with additional configurations for chambers for the deposition, processing, etching, annealing, and curing of dielectric films.
[0025] Figure 1B shows a cross-sectional view of an exemplary processing chamber 100 according to some embodiments of the present invention. This figure illustrates an overview of a system incorporating one or more aspects of the present invention and / or configured to perform one or more operations according to embodiments of the present invention. Additional details of the chamber 100 or the performed methods are further described below. The chamber 100 can be used to form a film layer, an etch material layer, other material layers, or combinations thereof, but it will be understood that deposition and etching methods can be similarly performed in any chamber where deposition and etching processes can occur. The processing chamber 100 may include a chamber body 102, a substrate support 104 disposed within the chamber body 102, and a cover assembly 106 coupled to the chamber body 102 and enclosing the substrate support 104 in a processing volume 120. A substrate 103 may be provided to the processing volume 120 via an opening 126, which may be sealed in a conventional manner using a slit valve or door for processing. During processing, the substrate 103 may be seated on the surface 105 of the substrate support. In some embodiments, the substrate support 104 may be rotated along axis 147 (where the shaft 144 of the substrate support 104 may be located) as indicated by arrow 145, or may be stationary. Alternatively, the substrate support 104 may be lifted for rotation as needed during the deposition process.
[0026] Gas distributor 112 may define orifices 118 for distributing process precursors into processing volume 120. Gas distributor 112 may be coupled to a first power source 142 (such as an RF generator, RF power supply, DC power supply, pulsed DC power supply, pulsed RF power supply, or any other power source that may be coupled to the processing chamber). In some embodiments, the first power source 142 may be an RF power supply.
[0027] The gas distributor 112 may be a conductive gas distributor or a non-conductive gas distributor. The gas distributor 112 may also be formed of conductive and non-conductive components. For example, the body of the gas distributor 112 may be conductive, while the panel of the gas distributor 112 may be non-conductive. The gas distributor 112 may be powered, for example, by a first power source 142 as shown in Figure 1, or in some embodiments, the gas distributor 112 may be coupled to the ground.
[0028] The first electrode 122 may be coupled to the substrate support 104. The first electrode 122 may be embedded within the substrate support 104 or coupled to the surface of the substrate support 104. The first electrode 122 may be a plate, a perforated plate, a mesh, a wire mesh, or any other distributed arrangement of conductive elements. The first electrode 122 may be a tuning electrode and may be coupled to the tuning circuit 136 via a conduit 146 (e.g., a cable having a selected resistance (such as 50 ohms), for example, disposed in a shaft 144 of the substrate support 104). The tuning circuit 136 may have an electronic sensor 138 and an electronic controller 140, which may be a variable capacitor. The electronic sensor 138 may be a voltage or current sensor and may be coupled to the second electronic controller 140 to provide further control over the plasma conditions in the processing volume 120.
[0029] The second electrode 124 (which may be a bias electrode and / or an electrostatic clamping electrode) may be coupled to the substrate support 104. The second electrode may be coupled to the second power source 150 via a filter 148, which may be an impedance matching circuit. The second power source 150 may be a DC power supply, a pulsed DC power supply, an RF bias power supply, a pulsed RF power supply, or a bias power supply, or a combination of these or other power supplies. In some embodiments, the second power source 150 may be an RF bias power supply. The substrate support 104 may also include one or more heating elements configured to heat the substrate to a processing temperature, which may be between about 25°C and about 800°C or higher.
[0030] The cover assembly 106 and substrate support 104 of Figure 1 can be used with any processing chamber for plasma or thermal processing. In operation, the processing chamber 100 can provide immediate control of plasma conditions within the processing volume 120, such as via a system controller 101 that may be contained within the processor 107. The substrate 103 can be mounted on the substrate support 104, and process gases can flow through the cover assembly 106 via inlet 114 according to any desired flow pattern. The gases can exit the processing chamber 100 via outlet 152. A power supply can be coupled to a gas distributor 112 to establish plasma in the processing volume 120. In some embodiments, the substrate can be electrically biased using a second electrode 124.
[0031] After plasma is activated in processing volume 120, a potential difference can be established between the plasma and the first electrode 122. The flow properties of the ground path, represented by tuning circuit 136, can then be adjusted using electronic controller 140. A setpoint can be delivered to the first circuit 136 to provide independent control over the deposition rate and the uniformity of plasma density from center to edge. In embodiments where the electronic controller may be a variable capacitor, the electronic sensor can independently adjust the variable capacitor to maximize the deposition rate and minimize thickness non-uniformity.
[0032] The tuning circuit 136 may have a variable impedance, which can be adjusted using the electronic controller 140. In the case where the electronic controller 140 is a variable capacitor, the capacitance range of each of the variable capacitors can be selected to provide an impedance range. This range may depend on the frequency and voltage characteristics of the plasma, and may have a minimum value within the capacitance range of each variable capacitor. Therefore, when the capacitance of the electronic controller 140 is at its minimum or maximum value, the impedance of the tuning circuit 136 may be high, resulting in a plasma shape with minimal air or lateral coverage over the substrate support. When the capacitance of the electronic controller 140 approaches a value that minimizes the impedance of the tuning circuit 136, the air coverage of the plasma may increase to its maximum value, effectively covering the entire operating area of the substrate support 104. When the capacitance of the electronic controller 140 deviates from the minimum impedance setting, the plasma shape may shrink from the chamber wall, and the air coverage of the substrate support may decrease.
[0033] Electronic sensor 138 can be used to tune circuit 136 in a closed loop. A setpoint for current or voltage (depending on the type of sensor used) can be installed in each sensor, and the sensor can have control software that determines adjustments to the corresponding electronic controller 140 to minimize deviation from the setpoint. Therefore, plasma shape can be selected and dynamically controlled during processing. It will be understood that while the foregoing discussion is based on electronic controller 140 (which may be a variable capacitor), any electronic component with adjustable characteristics can be used to provide tuning circuit 136 with adjustable impedance.
[0034] Figure 2 illustrates a perspective view of an exemplary 3D element that can utilize the methods and processes discussed herein. However, it should be understood that the techniques of this invention are applicable to other 3D elements, as well as elements that include channel-gate defects and can utilize one or more dielectric materials as discussed herein. Nevertheless, for illustrative purposes only, Figure 2 may illustrate a vertical 3D DRAM element according to an embodiment of this disclosure. Figure 2 depicts two 3D DRAM cells, each including a vertical channel element (e.g., a transistor). To avoid unnecessarily obscuring the appearance of the figures, one DRAM cell is labeled with an element symbol, and those skilled in the art will readily understand the common components in the other DRAM cell of Figure 2. Furthermore, the structures illustrated in Figure 2 may omit various components to more clearly illustrate the various features. Those skilled in the art will readily understand other components that may be included in similar structures.
[0035] The DRAM cell includes a transistor 222 and a capacitor 224. The transistor 222 includes a semiconductor material 230 disposed on and extending perpendicularly from a bit line contact 226. The semiconductor material 230 forms an active region of the transistor 222 and includes a channel region of the transistor 222. A drain region 232 and a source region 234 are disposed in the semiconductor material 230, wherein the channel region between the drain region 232 and the source region 234 is in the semiconductor material 230. In an embodiment, the drain region 232 may be disposed close to and / or adjacent to the bit line contact 226, and the source region 234 may be spaced apart from the bit line contact 226. A gate dielectric layer 236 is disposed on the semiconductor material 230 (e.g., on the sidewall surface of the semiconductor material 230), and a gate electrode 238 is disposed on the gate dielectric layer 236. Figure 2 illustrates a cross-section of the access transistor 222 to illustrate the semiconductor material 230. It will be readily understood from the following description that the gate dielectric layer 236 may be laterally disposed around the semiconductor material 230, and the gate electrode 238 may be laterally disposed around the gate dielectric layer 236, or the gate dielectric layer 236 and the gate dielectric layer may extend vertically on opposite sides of the semiconductor material 230, and other configurations known in the art exist.
[0036] The capacitor 224 includes an outer plate 240, a capacitor dielectric layer 242, and an inner plate 244. The outer plate 240 is a conductive material, such as a metal or a metal-containing material. The outer plate 240 typically has a single-cap vertical cylinder, a single-cap rectangular prism, or a similar shape. The outer plate 240 typically extends vertically from the access transistor 222 and has a contacting source region 234 of the access transistor 222 to electrically connect the source region 234 to the capped end of the capacitor 224. The capacitor dielectric layer 242 is a dielectric material disposed along the inner surface of the outer plate 240. The dielectric material of the capacitor dielectric layer 242 may be a high dielectric constant dielectric material (e.g., having a dielectric constant value greater than 4.0). The inner plate 244 may be a conductive material, such as a metal or a metal-containing material, and is disposed on the capacitor dielectric layer 242 and fills the remaining interior portion of the outer plate 240. Power supply contacts 246 (e.g., ground contacts) are laterally positioned and contact the inner plate 244 of capacitor 224. Furthermore, interlayer dielectric 248 may encapsulate all or part of the DRAM cell and may include one or more dielectric materials, which will be discussed in more detail below.
[0037] Figure 3 illustrates exemplary operations in a method 300 for forming a semiconductor structure according to an embodiment of the present invention. Method 300 may include one or more operations prior to the initiation of the method, including front-end processing, deposition, etching, polishing, cleaning, or any other operations that may be performed prior to said operations. For example, the method may begin after deposition and / or formation of a plurality of layers (such as for the production of 3D DRAM structures) or any one or more of the 3D structures discussed above. However, as explained above, it should be understood that the figures only illustrate one exemplary process (in which an embodiment of the present invention may be employed), and the description is not intended to limit the technology to this process or structure. Some or all of the operations may be performed in the chambers or system tools as described above, or may be performed in different chambers on the same system tool, such different chambers including chambers in which the operations of method 300 may be performed.
[0038] Method 300 may include additional operations prior to the commencement of the listed operations. For example, additional processing operations may include forming a structure on the substrate, which may include forming and removing material. The previous processing operations may be performed in a chamber in which method 300 may be performed, or processing may be performed in one or more other semiconductor processing chambers before delivering the substrate to a semiconductor processing chamber in which method 300 may be performed. In any case, method 300 may, as appropriate, include delivering the substrate to a processing region of a semiconductor processing chamber, such as the semiconductor processing chamber 100 described above, or other chambers that may include the components described above. The substrate may be deposited on a substrate support, which may be a base, such as substrate support 104, and the substrate support may reside in a processing region of the chamber, such as the processing volume 120 described above.
[0039] As illustrated in Figure 4, a substrate 402 is provided to a processing chamber (such as processing chamber 100). The substrate 402 can be any number of materials (such as a substrate wafer or substrate made of silicon or silicon-containing materials, germanium, other substrate materials), and one or more materials that can be formed by overlaying the substrate during semiconductor processing. In embodiments, the substrate 402 may include a bulk substrate, an epitaxial growth substrate, and / or a silicon wafer on an insulating layer. As used herein, the term "semiconductor substrate" means a substrate in which the entire substrate is formed of a semiconductor material. A semiconductor substrate may include any suitable semiconducting material and / or combination of semiconducting materials to form a semiconductor structure. For example, the semiconducting layer may comprise one or more materials, such as crystalline silicon (e.g., Si<100> or Si<111>), silicon oxide, strained silicon, silicon-germanium, doped or undoped polycrystalline silicon, doped or undoped silicon wafers, patterned or unpatterned wafers, doped silicon, germanium, gallium arsenide, or other suitable semiconducting materials. In one embodiment, the semiconductor material is silicon (Si). In one or more embodiments, the semiconductor substrate 402 comprises a semiconductor material, such as silicon (Si), carbon (C), germanium (Ge), silicon-germanium (SiGe), germanium-tin (GeSn), other semiconductor materials, or any combination thereof. In one or more embodiments, the substrate 402 comprises one or more of silicon (Si), germanium (Ge), gallium (Ga), arsenic (As), or phosphorus (P). Although several examples of materials that can form substrates are described herein, any material that can serve as the basis for constructing passive and active electronic components (e.g., transistors, memory, capacitors, inductors, resistors, switches, integrated circuits, amplifiers, optoelectronic components, or any other electronic components) is within the spirit and scope of this disclosure.
[0040] In embodiments, the semiconductor material may be a doped material, such as n-type doped silicon (n-Si) or p-type doped silicon (p-Si). In embodiments, the substrate may be doped using any suitable process, such as an ion implantation process. As used herein, the term "n-type" refers to a semiconductor formed during manufacturing by doping an electron donor element into an intrinsic semiconductor. The term n-type derives from the negative charge of electrons. In an n-type semiconductor, electrons are the majority carriers and holes are the minority carriers. As used herein, the term "p-type" refers to the positive charge of a well (or hole). In contrast to an n-type semiconductor, a p-type semiconductor has a hole concentration that is greater than the electron concentration. In a p-type semiconductor, holes are the majority carriers and electrons are the minority carriers.
[0041] In embodiments, the prior processing may form one or more materials on the substrate 402. For example, the illustrated embodiment may include one or more transistor 222 features formed at operation 305. For example, in embodiments, a film stack may be deposited on the substrate 402. In embodiments, the film stack may include a first barrier layer 404, a conductive layer 406, and / or a second barrier layer 408, as well as other layers known in the art, or may not utilize a film stack. The first barrier layer 404 may be deposited on the substrate 402. The conductive layer 406 may be deposited on the first barrier layer 404. The second barrier layer 408 may be deposited on the conductive layer 406. Semiconductor material may be deposited on the second barrier layer 408. The first barrier layer 404, the conductive layer 406, and / or the second barrier layer 408 can be deposited and / or doped using any suitable deposition process, such as chemical vapor deposition (CVD), plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), physical vapor deposition (PVD), or the like. In embodiments, the first barrier layer 404 and / or the second barrier layer 408 are each titanium nitride (TiN), tantalum nitride (TaN), or the like. In embodiments, the conductive layer 406 is a metal or a metal-containing material, such as tungsten (W), or the like. The first barrier layer 404, the conductive layer 406, and / or the second barrier layer 408 can form all or part of the bitline contacts.
[0042] Nevertheless, as illustrated, one or more channels 438 formed of one or more semiconductor materials may be disposed on the second barrier layer 408. The semiconductor material of the channel 438 may extend vertically from the second barrier layer 408, or may extend horizontally as discussed above (e.g., forming cell pairs of horizontally extending channel elements). Each channel 438 may contain opposing source / drain regions 436, which may be doped regions of the semiconductor material of the channel 438. In embodiments, the channel 438 may be formed of silicon or one or more of the semiconductor materials discussed above.
[0043] Regardless of the material of the channel 438 selected, the gate dielectric 420 and the gate electrode 422 may be formed around or along all or part of the channel 438, separated from the second barrier layer 408 via spacer 418. Although not shown in Figure 4, the spacer 418 may contact the substrate 402 between adjacent patterned features (e.g., between corresponding bit lines). In embodiments, the gate dielectric 420 may be any dielectric material and may be deposited using one or more processes (such as PECVD, ALD, CVD, or another deposition process). Nevertheless, in embodiments, the gate dielectric may be silicon oxide.
[0044] Gate electrodes 422 may be formed along the surface of the gate dielectric layer 420. Each of the formed gate electrodes 422 may be disposed on a portion of the gate dielectric layer 420, which is located on the sidewall of the corresponding channel 438, such that the corresponding gate electrode 422 extends laterally around the channel 438 or along the opposite side of the channel 438. The material of the gate electrode 422 may be deposited by PECVD, ALD, CVD or another deposition process known in the art. The material of the gate electrode 422 may be a single material or multiple different materials (e.g., in multiple different layers). In some instances, the gate electrode 122 is a metal or a metal-containing material, such as tungsten (W) or the like.
[0045] In an embodiment, dielectric layer 428 is deposited on gate dielectric layer 420 and gate electrode 422. Dielectric layer 428 may be any dielectric layer, such as silicon oxide, borosilicate glass (BPSG), silicon phosphorus glass (PSG), or the like.
[0046] Nevertheless, at operation 310, one or more capacitors 224 or features thereof may be formed on the transistor 222. For example, an etch barrier layer 450 and contact pads 452 may be formed on the transistor 222 such that the contact pads 452 contact the source / drain regions 436 of the transistor. The conductive pads 452 may include a barrier layer, such as titanium nitride (TiN), tantalum nitride (TiN), or the like; and a metal or metal-containing material, such as tungsten (W), aluminum (Al), copper (Cu), or the like, on the barrier layer. The conductive pads 452 may form ohmic contacts with the corresponding channels 438.
[0047] In an embodiment, at operation 315, an interlayer dielectric (ILD) layer 454 is formed on the etch stop layer 450 and the conductive pad 452. The ILD layer 454 may be or contain one or more dielectric materials and may be deposited by one or more deposition processes, as will be discussed in more detail. The ILD layer 454 may be patterned to have openings leading to the respective conductive pads 452.
[0048] A capacitor 224 may be formed in a corresponding opening through the ILD layer 454. The capacitor includes an outer plate 460, a capacitor dielectric layer 462, and an inner plate 464. The outer plate 460 may be formed along the surface of the opening through the ILD layer 454. The capacitor dielectric layer 462 may be formed on the inner surface of the corresponding outer plate 460. The capacitor dielectric layer 462 may extend between openings on the top surface of the ILD layer 454. The inner plate 464 may be formed on the outer plate 460 and may form terminals of corresponding elements, which are electrically connected to power supply nodes (e.g., ground nodes), as discussed in Figure 3. In embodiments, the outer plate 460 and / or the inner plate 464 may be any conductive material, such as a metal or a metal-containing material, such as titanium nitride (TiN). In embodiments, the capacitor dielectric layer 462 may be any dielectric material, and further, may be a high dielectric constant dielectric material (e.g., having a dielectric constant value greater than 4.0).
[0049] Although capacitor 224 is formed, interlayer dielectric 454 can still be carefully formed according to the technique of the present invention. That is, as discussed above, the present invention surprisingly discovers that improved dopant migration can be achieved, alone or in combination with the very precise target dopant level at the channel-gate interface, due to the target doping concentration during layer formation. Without wishing to be limited by theory, it is believed that by forming interlayer dielectric 454 according to the technique of the present invention, an interlayer dielectric with almost no film change is formed, thereby allowing improved migration, at least in part, due to the reduction of getter sites in interlayer dielectric 454. As discussed above, in previous devices, dielectric layers (such as interlayer dielectrics) contain high-level getter sites (also referred to as "interface traps"), which prevent dopant migration across the dielectric layer because the dopant is "trapped" in the getter sites. Therefore, by utilizing target temperature and deposition conditions, such as high HF concentration, due to the homogeneous and dense material, improved mobility across the dielectric layer can be achieved.
[0050] In an embodiment, the deuterium (D) doping of the interlayer dielectric 454 during its formation advantageously allows deuterium to act as a passivating agent, stabilizing and increasing the reliability of the channel-gate interface. Without intending to be limited by theory, it is believed that films containing deuterium and / or hydrogen achieve chemical passivation of unsatisfied valence bonds on fixed atoms in the solid matrix. That is, compared to chemical passivation with hydrogen, deuterium can form stronger and more stable chemical passivation for many atomic elements. For example, in solid-state materials and solid-state interfaces formed with common silicon-based solid-state materials (such as crystalline silicon, polycrystalline silicon, amorphous silicon, silicon oxide, silicon nitride, and silicon carbide), the chemical bonds formed by deuterium with silicon atoms are stronger than those formed by hydrogen with silicon atoms. Compared to hydrogen-passivated silicon materials and interfaces, deuterium-passivated silicon materials and interfaces have been found to be more electrically stable and reliable under higher applied voltages, higher applied currents, shorter wavelength and higher intensity electromagnetic radiation exposure, and at higher temperatures. Nevertheless, in the embodiments, other dopants (such as tritium), or other dopants with properties similar to hydrogen but with increased bond strength and / or reduced desorption rates, are conceivable.
[0051] In embodiments, in other common material systems, it is possible to improve material and interface reliability through deuterium chemical passivation, such as (but not limited to) group III-V and II-VI semiconductors: gallium arsenide, aluminum arsenide, aluminum gallium arsenide, gallium nitride, aluminum nitride, aluminum gallium nitride, zinc oxide, cadmium oxide, cadmium telluride, cadmium selenide, magnesium oxide, and oxide and nitride derivatives of group III-V and II-VI semiconductors. Therefore, although silicon and silicon oxide have been referenced herein, it should be understood that the methods and systems discussed herein are also suitable for passivating other semiconductor materials.
[0052] Nevertheless, in embodiments, deuterium may be incorporated into one or more dielectric layers, such as interlayer dielectric 454. The one or more dielectric layers may comprise any dielectric material known in the art, such as electrically insulating materials that can be polarized by an applied electric field. In one or more embodiments, the dielectric material includes (but is not limited to) oxides (e.g., SiO₂, Ta₂O₅, Al₂O₃), nitrides (e.g., Si₃N₄), and barium strontium titanate (BST). In one or more embodiments, the dielectric material may include silicon dioxide (SiO₂). In embodiments, the film composition may be non-stoichiometric relative to an ideal molecular formula. For example, in some embodiments, the dielectric material includes (but is not limited to) oxides (e.g., silicon oxide, tantalum oxide, aluminum oxide), nitrides (e.g., silicon nitride (SiN)), carbides (e.g., silicon carbide (SiC), silicon carbide nitride (SiCN)), oxycarbides (e.g., silicon carbide (SiOC)), oxynitrocarbides (e.g., silicon carbide (SiNCO)), and barium strontium titanate (BST). However, as discussed above, in embodiments, the dielectric material (such as interlayer dielectric 454) may be or include silicon dioxide. Furthermore, while the methods and systems discussed herein relate to interlayer dielectric 454, it should be understood that the incorporation of dopants as discussed herein can be used in other dielectric layers in one or more devices. As will be discussed in more detail below, it may be necessary to dope interlayer dielectric 454 to achieve a high diffusion level without negatively affecting the film properties of the channel. That is, as noted above, when the channel is directly doped, an unacceptably high threshold voltage is exhibited, a situation that does not occur or occurs to a significantly lower degree when the adjacent material is doped.
[0053] Regardless of the material or layers(s) selected, operation 315 may include forming a dielectric layer, such as an interlayer dielectric 454, in the presence of a deuterium-containing precursor. In embodiments, the deuterium-containing precursor may be pulsed or co-flowed into the processing chamber with a flowing gas or carrier gas. In other embodiments, the deuterium-containing precursor is pulsed into the processing chamber in the absence of a carrier gas. As used herein, the term "carrier gas" refers to a fluid (gas or liquid) that can move precursor molecules from one location to another. For example, a carrier gas may be a liquid that moves molecules from a solid precursor in an ampoule to an aerosolizer. In some embodiments, the carrier gas is an inert gas. In one or more embodiments, the carrier gas is one or more of argon (Ar), helium (He), xenon (Xe), or nitrogen (N2). In embodiments, the deuterium-containing precursor may include one or more of molecular deuterium (D₂), deuterated water (D₂O), DH (deuterium hydrogen), or HDO (deuterium hydroxide). Furthermore, in embodiments, the plasma may also include one or more of argon (Ar), helium (He), hydrogen (H₂), nitrogen (N₂), oxygen (O₂), ammonia (NH₃), or nitrogen trifluoride (NH₃).
[0054] In embodiments, chemical precursors and inert gases can be used to deposit films and / or layers containing deuterium and silicon, and / or one or more other materials discussed above, via plasma-enhanced chemical vapor deposition (PECVD), chemical vapor deposition (CVD), or atomic layer deposition (ALD), and other methods known in the art. In one or more embodiments, the deposition method passivates dangling silicon bonds by introducing a dopant (such as deuterium) into the film, which allows deuterium to migrate to target regions (e.g., the channel-gate interface in the illustrated example). Thus, the present invention provides a targeted dopant content while preventing changes in film quality. For example, in one or more embodiments, films including (but not limited to) SiH YD Z, SiO X1H YD Z, SiN X2H YD Z, SiC X3H YD Z, and SiO X1N X2C X3H YD are deposited on a substrate surface. In one or more embodiments, the deuterium-containing precursor includes one or more of D₂, D₂O, SiD₄, and Si₂D₆. In one or more embodiments, the deuterium-containing precursor may be combined with or co-flowed with one or more silicon precursors selected from one or more of SiH₄, Si₂H₆, SiCl₄, SiHCl₃, SiH₂Cl₂, SiHCl₃, Si₂Cl₆, SiF₄, SiBr₄, TEOS, TDMAS, BTBAS, BDEAS, and the like. Nevertheless, in embodiments, the deuterium-containing precursor may be combined with or flowed with tetraethyl orthosilicate (TEOS) alone or together with one or more precursors.
[0055] In one or more embodiments, the deuterium-containing precursor may be combined with or co-flushed with one or more of oxygen (O2), ozone (O3), or water (H2O). In one or more embodiments, the deuterium-containing precursor may be combined with or co-flushed with one or more of nitrogen (N2) or ammonia (NH3) to form a deuterium-containing nitride film. In one or more embodiments, the deuterium-containing precursor may be combined with or co-flushed with one or more of methane (CH4) or ethane (C2H2) to form a deuterium-containing carbon film. In one or more embodiments, the deuterium-containing precursor may be combined with or co-flushed with hydrogen (H2). In one or more embodiments, the deuterium-containing precursor may be combined with or co-flushed with one or more inert gases (including but not limited to argon (Ar) or helium (He)) to form a deuterium-containing film. In one or more embodiments, the deposition process may include a heat source, a plasma source, and / or a light source to activate the precursor and control the chemical reaction rate.
[0056] Nevertheless, in embodiments, the interlayer dielectric 454 can be formed at relatively high temperatures. That is, the present invention has found that increased temperature during deposition may result in a reduction in the number of getter sites and / or an increase in their density in the interlayer dielectric 454. Therefore, in embodiments, the interlayer dielectric 454 can be formed at temperatures greater than or about 325°C, such as greater than or about 330°C, such as greater than or about 335°C, such as greater than or about 340°C, such as greater than or about 345°C, such as greater than or about 350°C, such as greater than or about 355°C, such as greater than or about 360°C, such as greater than or about 365°C, such as greater than or about 370°C, such as greater than or about 375°C, such as greater than or about 380°C, such as greater than or about 385°C, such as greater than or about 390°C, such as greater than or about 395°C, such as up to about 400°C or higher, or any range or value therein.
[0057] Furthermore, the present invention has surprisingly discovered that the presence of getter sites in the interlayer dielectric 454 and / or the allowable density increase can also be improved by using high-frequency RF plasma at a customized power level. Therefore, in embodiments, the plasma processes discussed above (such as the flow of silicon-containing precursors, deuterium-containing precursors, and additional process gases) can be generated at high frequencies using a high-frequency generator (such as a generator operating at a frequency greater than or about 13.56 MHz or other high frequencies known in the art). Furthermore, high-frequency RF plasma can be generated at plasma powers greater than or about 800 watts, such as greater than or about 850 watts, such as greater than or about 900 watts, such as greater than or about 950 watts, such as greater than or about 1000 watts, such as greater than or about 1050 watts, such as greater than or about 1100 watts, such as greater than or about 1150 watts, such as greater than or about 1200 watts, or any range or value between these values.
[0058] The pressure within the semiconductor processing chamber can also affect the performed operation. In an embodiment, the pressure may be maintained at less than about 100 Torr. Therefore, the pressure may be maintained at less than or about 50 Torr, less than or about 40 Torr, less than or about 30 Torr, less than or about 25 Torr, less than or about 20 Torr, less than or about 18 Torr, less than or about 16 Torr, less than or about 14 Torr, less than or about 12 Torr, less than or about 10 Torr, less than or about 8 Torr, less than or about 6 Torr, less than or about 4 Torr, less than or about 2 Torr or less, or any range or value therebetween. The pressure may also be maintained at any pressure within these ranges, within a smaller range encompassed by these ranges, or between any ranges of these ranges.
[0059] The flow rate of one or more of the silicon-containing precursor, deuterium-containing precursor, plasma process precursor, or combinations thereof may be between 1 sccm and 10,000 sccm, for example, from about 400 sccm to about 2,000 sccm. The processing time may be between 1 minute and 10 minutes, such as 3 minutes. During the vapor phase process, the pressure in the processing chamber may vary. For example, the pressure may vary between 50 Torr and 500 Torr.
[0060] Furthermore, the present invention has surprisingly discovered that by carefully customizing the ratio of deuterium-containing precursor to silicon-containing precursor, a high percentage of deuterium can migrate to the channel-gate region without exhibiting a significant increase in deuterium in the interlayer dielectric 454. Therefore, in embodiments, the deuterium-containing precursor can be introduced into the processing region at a ratio to the silicon-containing precursor (such as TEOS in the embodiments) greater than or about 0.9:1, such as greater than or about 1:1, such as greater than or about 1.1:1, such as greater than or about 1.2:1, such as greater than or about 1.3:1, such as greater than or about 1.4:1, such as greater than or about 1.5:1, such as greater than or about 1.6:1, such as greater than or about 1.7:1, such as greater than or about 1.8:1, such as greater than or about 1.9:1, such as greater than or about 2:1, such as greater than or about 2.2. :1, such as greater than or approximately 2.4:1, such as greater than or approximately 2.6:1, such as greater than or approximately 2.8:1, such as greater than or approximately 3:1, such as greater than or approximately 3.2:1, such as greater than or approximately 3.4:1, such as greater than or approximately 3.6:1, such as greater than or approximately 3.8:1, such as greater than or approximately 4:1, such as greater than or approximately 4.2:1, such as greater than or approximately 4.4:1, such as greater than or approximately 4.5:1, such as greater than or approximately 4.6:1, such as greater than or approximately 4.8:1, such as up to about 5:1 or greater, or any range or value therein. By utilizing these ratios, excellent stress and deposition rate can be maintained, while also maintaining the desired deuterium level in the interlayer dielectric 454.
[0061] By utilizing these ratios, the amount of deuterium in the interlayer dielectric 454, by weight, can be from about 0.1% to about 1% of the interlayer dielectric, such as greater than or about 0.15% by weight, such as greater than or about 0.2% by weight, such as greater than or about 0.25% by weight, such as greater than or about 0.3% by weight, such as greater than or about 0.35% by weight, such as greater than or about 0.4% by weight, such as greater than or about 0.45% by weight, such as greater than or about 0.5% by weight, such as greater than or about 0.55% by weight, such as greater than or about 0.6% by weight, such as greater than or about 0.65% by weight, such as greater than or about 0.7% by weight, such as greater than or about 0.75% by weight, such as greater than or about 0.8% by weight, such as greater than or about 0.85%, such as greater than or about 0.9% by weight, such as greater than or about 0.95% by weight, or any range or value therein.
[0062] In an embodiment, optional operation 320 may include thermally treating or annealing the semiconductor structure after forming the deuterium-containing dielectric to facilitate the migration of deuterium to the target region. However, in an embodiment, passivation of the target region may be achieved during processing, and a separate annealing or thermal treatment operation may not be required.
[0063] In the foregoing description, numerous details have been set forth for illustrative purposes in order to provide an understanding of various embodiments of the present invention. However, it will be apparent to those skilled in the art that certain embodiments may be practiced without some of these details or with additional details.
[0064] In disclosing several embodiments, those skilled in the art will recognize that various modifications, alternative constructions, and equivalents can be used without departing from the spirit of the embodiments. Furthermore, many well-known processes and components have not been described to avoid unnecessarily obscuring the technical scope of the invention. Therefore, the above description should not be considered as a limitation on the scope of the technology. In addition, methods or processes may be described as sequential or step-by-step, but it should be understood that they may be performed simultaneously or in a different order than those listed.
[0065] If a range of values is provided, it should be understood, unless the context explicitly specifies otherwise, that each intermediate value (up to the smallest unit fraction of the lower limit) between the upper and lower limits of that range is also specifically disclosed. Any narrower range between any stated or unstated intermediate value within the range and any other stated or intermediate value within that range is included. The upper and lower limits of those smaller ranges may be independently included or excluded from the range, and each range that includes any limit, excludes any limit, or includes two limits within a smaller range is also included in this art and is subject to any explicitly excluded limit in the range. If the range includes one or both of the limits, then the range that excludes any one or both of the included limits is also included. As used herein and in the claims of the appended patent applications, the terms "about" and / or "approximately" when referring to measurable values (such as quantities, durations of time, and the like) encompass variations of ±20%, ±10%, ±5%, or +0.1% from the specified value, because such variations are appropriate in the context of the systems, components, circuits, methods, and other embodiments described herein. Similarly, as used herein and in the claims of the appended patent applications, the term "substantially" when referring to measurable values (such as quantities, durations of time, physical properties (such as frequencies), and the like) also encompass variations of ±20%, ±10%, ±5%, or ±0.1% from the specified value, because such variations are appropriate in the context of the systems, components, circuits, methods, and other embodiments described herein.
[0066] As used herein and in the appended claims, the singular forms “a(a)”, “an”, and “the” include a plurality of references unless the context clearly requires otherwise. Thus, for example, a reference to “a precursor” includes a plurality of such precursors, and a reference to “the layer” includes a reference to one or more layers and their equivalents known to those skilled in the art, and so on.
[0067] Furthermore, the terms “comprise(s)”, “comprising”, “contain(s)”, “containing”, “include(s)” and “including” are used in this specification and the following claims to indicate the presence of the said feature, integer, component or operation, but do not exclude the presence or addition of one or more other features, integers, components, operations, actions or groups. [Simplified Explanation of the Diagram]
[0011] A further understanding of the nature and advantages of the disclosed technology can be achieved by referring to the rest of this specification and the figures.
[0012] Figure 1A shows a top plan view of an exemplary processing system according to an embodiment of the present invention.
[0013] Figure 1B shows a schematic cross-sectional view of an exemplary processing system according to an embodiment of the present invention.
[0014] Figure 2 shows a schematic diagram of an exemplary unit cell according to an embodiment of the present invention.
[0015] Figure 3 illustrates the operation of an exemplary semiconductor processing method according to some embodiments of the present invention.
[0016] Figure 4 shows a schematic cross-sectional view of an exemplary unit cell according to an embodiment of the present invention.
[0017] Some of the figures are included as schematic diagrams. It should be understood that the figures are for illustrative purposes and should not be considered to be drawn to scale unless specifically stated otherwise. Furthermore, as schematic diagrams, the figures are provided to aid understanding and may not include all appearances or information compared to actual representations, and may include exaggerated material for illustrative purposes.
[0018] In the accompanying figures, similar parts and / or features may have the same reference labels. Furthermore, various parts of the same type may be distinguished by having the reference label followed by letters used to distinguish similar parts. If only a first reference label is used in this specification, the description applies to any of the similar parts having the same first reference label, regardless of the letters. [Biomaterial Storage]
[0069] Domestic Deposit Information (Please note in order of deposit institution, date, and number) None
[0070] Overseas Deposit Information (Please note in the order of deposit country, institution, date, and number) None
Claims
1. A method for modifying a target region, comprising the steps of: flowing a deuterium-containing precursor and a silicon-containing precursor into a processing region of a processing chamber; contacting a semiconductor element disposed in the processing region with the deuterium-containing precursor and the silicon-containing precursor; forming a deuterium-containing dielectric film on or over the semiconductor element at a processing temperature greater than or about 350°C, wherein the deuterium-containing dielectric film is formed at a ratio of the deuterium-containing precursor to the silicon-containing precursor greater than or about 0.9:1; and passivating the target region by deuterium from the deuterium-containing dielectric film; wherein the deuterium-containing dielectric film is spaced apart from or adjacent to the target region.
2. The method as described in claim 1, wherein the deuterium-containing precursor comprises one or more of D2, D2O, DH (deuterium hydrogen) or HDO (deuterium hydroxide).
3. The method as claimed in claim 1, wherein the deuterium-containing precursor and the silicon-containing precursor flow using a plasma process, wherein the plasma further comprises one or more of argon (Ar), helium (He), hydrogen (H2), nitrogen (N2), oxygen (O2), ammonia (NH3) or nitrogen fluoride (NF3).
4. The method as claimed in claim 1, wherein the silicon-containing precursor comprises one or more of silane (SiH4), disilane (Si2H6), silicon tetrachloride (SiCl4), trichlorosilane (SiHCl3), dichlorosilane (SiH2Cl2), hexachlorodisilane (Si2Cl6), silicon tetrafluoride (SiF4), silicon tetrabromide (SiBr4), ethyl silicate (TEOS), tris(dimethylamino)silane (TDMAS), bis(tert-butylamino)silane (BTBAS), bis(diethylamino)silane (BDEAS), or a combination thereof.
5. The method as claimed in claim 1, wherein the deuterium-containing dielectric film is formed on or on the semiconductor element at a processing temperature greater than or about 400°C.
6. The method as described in claim 1, wherein the ratio of the deuterium-containing precursor to the silicon-containing precursor is greater than or about 1.5:
1.
7. The method as described in claim 6, wherein the ratio of the deuterium-containing precursor to the silicon-containing precursor is greater than or about 4:
1.
8. The method as described in claim 1, wherein the deuterium-containing dielectric film contains from about 0.1% by weight to about 1% by weight of deuterium, based on the weight of the deuterium-containing dielectric film.
9. The method as described in claim 1, wherein the target region includes a channel-gate interface.
10. The method as described in claim 1, wherein the deuterium-containing dielectric film comprises an intercalary dielectric layer.
11. The method as described in claim 3, wherein the plasma comprises a high-frequency plasma and a plasma power of greater than or about 800 watts.
12. A semiconductor processing method comprising the steps of: forming a semiconductor element comprising one or more transistors and one or more capacitors on the one or more transistors in a processing region of a processing chamber; flowing a deuterium-containing precursor and a silicon-containing precursor into the processing region of the processing chamber; contacting the semiconductor element disposed in the processing region with the deuterium-containing precursor and the silicon-containing precursor; forming a deuterium-containing dielectric film on or on the semiconductor element at a processing temperature greater than or about 350°C, wherein the deuterium-containing dielectric film is formed at a ratio of the deuterium-containing precursor to the silicon-containing precursor greater than or about 0.9:1; and passivating a target region of the semiconductor element by deuterium from the deuterium-containing dielectric film; wherein the deuterium-containing dielectric film is spaced apart from or adjacent to the target region.
13. The semiconductor processing method as described in claim 12, wherein the semiconductor element comprises a three-dimensional (3D) semiconductor element.
14. The semiconductor processing method as described in claim 13, wherein the three-dimensional element comprises a three-dimensional dynamic random access memory (3D DRAM) element.
15. The semiconductor processing method as claimed in claim 12, wherein the target region includes a channel-gate interface and the deuterium-containing dielectric film includes an interlayer dielectric.
16. The semiconductor processing method as claimed in claim 12, wherein the silicon-containing precursor comprises ethyl orthosilicate.
17. The semiconductor processing method of claim 12, wherein the deuterium-containing precursor and the silicon-containing precursor are flowed using a plasma process, wherein the plasma comprises a high-frequency plasma and a plasma power of greater than or about 800 watts.
18. A method of forming a three-dimensional dynamic random access memory (3D DRAM) device, comprising the steps of: forming a semiconductor structure comprising one or more transistors and one or more capacitors on the one or more transistors in a processing region of a processing chamber, wherein the one or more transistors comprise a channel and a gate; flowing a deuterium-containing precursor and a silicon-containing precursor into the processing region of the processing chamber; contacting the semiconductor structure disposed in the processing region with the deuterium-containing precursor and the silicon-containing precursor; forming a deuterium-containing dielectric film on or on the semiconductor structure at a processing temperature greater than or about 350°C, wherein the deuterium-containing dielectric film is formed at a ratio of the deuterium-containing precursor to the silicon-containing precursor greater than or about 0.9:1; and passivating a channel-gate interface region of the semiconductor structure by deuterium from the deuterium-containing dielectric film.
19. The method as described in claim 18, wherein the deuterium-containing dielectric film is an interlayer dielectric layer covering the one or more transistors and / or the one or more capacitors.
Citation Information
Patent Citations
Method of semiconductor technology
CN110600370A
Structures having boron and gallium doped silicon germanium
CN116978776A
Memory device and method of manufacturing memory device charge storing structure
CN1763930A
Method of Depositing Polysilicon Gate Using Tetra Deuterium Silicon Gas
KR1020000067657A
Enhancing transistor performance and reliability by incorporating deuterium into a strained capping layer
US9401423B2